压下率对取向硅钢热轧板织构的影响
采用X-射线衍射分析技术测定了取向硅钢热轧板在不同压下率下不同厚度处的织构。结果表明,在压下率低于80%的情况下,几乎所有试样的不同厚度处的织构均为旋转立方织构类型{100}<011>,但不同压下率、不同厚度处的织构强度存在很大差异;在压下率大于80%的情况下,不同试样的不同厚度处的织构类型发生了变化,其织构类型为旋转立方织构或高斯织构{011}<100>,且当织构类型为旋转立方织构时,织构强度存在很大差异,而当织构类型为高斯织构时,织构强度差异相对较小。 The texture of the grain oriented silicon steel hot rolled plate at different compressibility has been measured.The experimental results have shown that the texture of all samples at different thickness is {100}<011> when the compressibility is below 80%,and its intensity at different compressibility and thickness is difference.The texture of all samples at different thickness is variable when the compressibility is above 80%,it is {100}<011> or {011}<100>,and the intensity of ...
晶界位向对硅钢立方/旋转立方取向双晶轧制取向变化的影响
晶界和{100}柱状晶在硅钢生产过程中对织构的遗传和演变有关键作用,因此本文利用晶体塑性有限元方法进行立方和旋转立方取向双晶在晶界不同位向时晶体取向演变的全场模拟。模拟显示,三种晶界位向下,晶界都具有诱发晶内产生S形状形变不均匀和缓解局部形变不均匀区取向转动的特点,立方和旋转立方取向双晶在带有剪切作用的轧制条件下都显示明显的取向稳定性。GB⊥RD(表示晶界垂直于轧向)晶界位向时,旋转立方取向晶粒优先在晶界中心位置发生取向转动,而立方取向则优先在远离晶界的端部发生取向转动。GB⊥TD(表示晶界垂直于横向)的晶界位向下,其晶界阻碍作用最小,双晶内产生的取向漫散度大,织构强度较低;除绕TD转动外,也具有复杂的绕RD、ND的取向转动。GB⊥ND(表示晶界垂直于法向)的晶界位向下,取向转动与GB⊥RD时相近,但有少量取向绕ND转动。 Grain boundaries and initial{100}columnar grains play a key role in the inheritance and evolution of texture in the production of electrical steels.In this paper,the crystal plasticity finite element method was used to simulate the grain orientation evolution of cube and rotated-cube oriented bicrystals when grain boundary was set to different orientations.It was shown that the grain boundary in three grain boundary orientations demonstrated the characteristics of inducing Sshape deformation inh...
CN202110667000.7一种用于风力发电机定子铁芯扇形硅钢片的保护工装
本发明公开了一种用于风力发电机定子铁芯扇形硅钢片的保护工装,包括第一防护罩和第二防护罩,第一防护罩、第二防护罩均为扇形罩体,其由弧形底板和两个扇形侧板构成,第一防护罩的两端连接有能够折叠收纳的柔性罩;第一防护罩滑动套设在扇形硅钢的外侧,第二防护罩滑动套设在第一防护罩的外侧。本发明提供的保护工装主要有两个功能,当扇形硅钢片处于运输过程中时,利用第一防护罩、第二防护罩、柔性罩协同配合为其防刮伤防护;当扇形硅钢片装配后,利用第一防护罩内部的冷却散热系统提供散热防护,防止出现高温过热现象;通过这种方式,本发明保护工装满足大规格定子铁芯扇形硅钢片的防护需求。
轧制复合法制备硅浓度梯度高硅钢薄带的织构演变
采用\"热轧复合+冷轧减薄+退火\"方法成功制备了0.20mm厚的硅浓度梯度高硅钢薄带,并采用SEM和X射线衍射技术对制备过程中组织和织构演变进行了研究。热轧复合板微观组织呈明显层状分布,复合界面为紧密冶金结合且经过83%的大冷轧变形未开裂。热轧和冷轧复合板带中均形成强α和γ织构,再结晶退火后形成强γ织构。冷轧和退火织构沿板厚呈显著的梯度分布特征,其主要来自于复合界面两侧硅浓度和初始热轧织构的差异性以及冷变形的不均匀性。 Gradient high silicon steel thin sheets with thickness of 0.20 mm were successfully produced by the rolling and annealing method,including hot rolling bonding,cold rolling,and annealing.Microstructure and texture evolution was investigated by means of SEM and X-ray diffraction.Microstructure of hot-rolling-bonding shows obviously layered distribution,the composite interface was closely metallurgical bonding and no cracking appears even after 83%cold rolling.Strongαandγfibers develop in the hot a...
CN202122099636.4一种防溢出的无取向硅钢绝缘涂液存储装置
本实用新型公开了一种防溢出的无取向硅钢绝缘涂液存储装置,涉及无取向硅钢绝缘涂液技术领域,为解决现有无取向硅钢绝缘涂液存储设备在存储过程中存在涂液过满,导致液体溢出产生浪费现象的问题。所述绝缘涂液存储机构本体上方的一侧设置有液位监测器,所述液位监测器的下端设置有监测杆,所述液位监测器的输出端设置有单片机,且液位监测器的输出端与单片机电性连接,所述绝缘涂液存储机构本体的内壁设置有压力传感器,且压力传感器设置有若干个,所述压力传感器的输出端与单片机的输入端电性连接,所述绝缘涂液存储机构本体的内部设置有泵体,且泵体设置有两个,所述泵体的一端设置有溢流输送管。
CN202023181223.2一种无取向硅钢厚涂层涂层液生产用纯水制水机
本实用新型公开了一种无取向硅钢厚涂层涂层液生产用纯水制水机,包括底板,底板顶端的两侧分别固定设有固定座和存水筒,固定座顶端的中部设有蒸馏组件,蒸馏组件包括球形釜,球形釜设置在固定座的顶部,球形釜的外部固定套设有导热层,导热层的内部固定嵌设有电热丝,导热层的外部固定套设有隔热层,本实用新型的有益效果是:通过设置的电热丝通过导热层对球形釜内部的水进行加热,球形釜提供更加均匀的受热效果,水蒸气通过V形管进入L形管,通过设置的环状冷却管内部的液氮对水蒸气进行冷却,便于提供更高效的蒸馏处理,通过设置的防腐蚀磁铁网格滤板、无纺布滤层、活性炭滤层和高密度滤网层,便于提供更好的过滤效果。
初次再结晶退火工艺对3%Si取向硅钢组织和织构的影响
试验研究了0.3 mm取向硅钢冷轧板(/%:0.046C,3.07Si,0.09Mn,0.029P,0.004S,0.005A1)的退火温度(760~880℃7 min)和退火时间(820℃3~9 min)对该钢的晶粒尺寸,再结晶和织构的影响。结果表明,最佳初次再结晶退火工艺为820℃5 min,该钢的平均晶粒尺寸为14.20μm,完全再结晶率为92%,不利{111}<110>结构含量为3.16%,有利织构{111}<112>,{012}<001>和高斯织构含量分别0.40%,4.73%和2.46%。 The effect of annealing temperature(at 760 ~ 880 X.for 7 min) and time(at 820℃ for 3~9 min) on grain size,recrystallization rate and texture of 0.3 mm cold-rolled sheet of oriented silicon steel(/%:0.046C,3.07Si,0.09Mn,0.029P,0.004S,0.005Al) has been tested and studied.Results show that with optimum recrystallized annealing at 820℃ for 5 min,the silicon steel average grain size is 14.20 fun,the complete recrystaUization rate is 92%,the unfavourable-texture {111}< 110 > content in steel is ...
我国硅钢发展现状及发展趋势
硅钢是钢铁产品中的\"工艺品\",是高附加值产品,通过对我国主要硅钢生产厂家的工艺设备,市场情况分析,简要介绍了我国硅钢生产消费现状,未来生产能力预测及硅钢未来发展趋势。 Silicon steel is the \"crafts\" of steel products,also is high value-added product.By analyzing process equipment and market condition of major silicon steel-making plant of China,it briefly introduces our current production consumption status,future production capacity prediction and future development trend of silicon steel.
优化脱氧工艺改善低碳低硅钢钢水可浇性
介绍了重庆钢铁股份有限公司炼钢厂生产低碳低硅钢的脱氧工艺,对连铸过程中水口结瘤的原因进行分析,并提出了优化措施。生产实践表明:钢水中的活性氧质量分数控制在10×10-6~30×10-6时,单中包浇铸炉数由6~7炉提高到11~12炉,同时能保证连铸顺行和减少铸坯气孔。 The deoxidation process of low-carbon and low-silicon steel in steel plant of Chongqing Steel was introduced.The nuzzle clogging was analyzed and some measures were put forward.Production experiments showed that when the active oxygen was controlled between 10×10-6~30×10-6,the amount of furnaces would rise from 6~7 to 11~12,which will make the casting process work well and reduce casting holes.
CN202110627061.0电工钢及其制备方法
本申请提供一种电工钢及其制备方法,制备方法包括:将电工钢的板坯进行热轧获得钢卷;将热轧后的钢卷进行酸洗冷轧;将酸洗冷轧后的钢卷进行第一次罩式退火;将第一次罩式退火后的钢卷进行平整;将平整后的钢卷进行第二次罩式退火;将第二次罩式退火后的钢卷进行重卷,以获得电工钢。本申请提供的电工钢的制备方法采用两次罩式退火,退火的主要目的是消除酸洗冷轧工序产生的加工硬化,使钢板充分再结晶,获得理想的铁损及磁感应强度。而采用两次罩式退火,相对于一次罩式退火工序来说,能够进一步降低铁损,提高电工钢的磁性能。
取向硅钢初次再结晶退火工艺正交试验
以试验室模拟CSP工艺生产的Fe-3Si热轧钢带为研究对象,采用正交试验及方差分析的方法,研究了取向硅钢初次再结晶退火工艺对高温退火后获得锋锐的高斯织构的影响。结果表明:取向硅钢两段式初次再结晶脱碳退火工艺参数加热段保温时间及加热温度是高温退火后获得锋锐高斯织构的主要影响因素,其可信度分别在90%和85%以上;在本试验条件下,通过正交试验获得的最佳退火工艺为:冷硬板经600℃保温3 min和850℃保温6 min。 Fe-3Si hot rolled strip was produced by simulating CSP technology in the laboratory.Orthogonal experiment and analysis of variance were carried out to investigate the influence of primary recrystallization on the sharp Goss texture of the oriented silicon steel.The results show that holding time of the heating section and the heating temperature for a sharp Goss texture of the samples annealed has important implications in this experiment conditions,the two-step decarburization annealing process...
CN202122492040.0一种硅钢片快速叠片装置
本实用新型公开了一种硅钢片快速叠片装置,包括模具箱,所述模具箱的上表面开设有放置槽,放置槽的内底壁开设有滑动调节槽,滑动调节槽的内侧壁转动连接有调节丝杆,调节丝杆的外表面螺纹连接有滑动块,滑动块的上表面分别固定连接有第一电动伸缩杆和支撑板,第一电动伸缩杆的顶端固定连接有固定板,固定板的上表面开设有滑槽。该硅钢片快速叠片装置,通过设置支撑板、放置板、第二电动伸缩杆与缓冲橡胶块,能方便将硅钢片进行叠放,通过设置第一电动伸缩杆、固定板、支架板、滚动轮与复位弹簧,便于对已经放置好的硅钢片进行固定,从而使整个装置具有方便快速自动叠片的效果,降低工作人员的劳动强度,提高硅钢片叠片的效率。