钢厂
碳化法制备硅钢氧化镁过程中杂质脱除研究
以轻烧氧化镁粉为原料,经消化、碳化制得重镁水,在热解反应前采用络合剂对重镁水中的杂质钙、铁进行络合掩蔽,再经热解得到碱式碳酸镁,碱式碳酸镁经煅烧可制得钙、铁杂质含量较低的氧化镁。在重镁水络合除杂过程中,考察了络合剂三乙醇胺、柠檬酸、草酸单独和复合使用的除铁、除钙效果。以三乙醇胺为络合剂时,在200 mL重镁水中加10 mL三乙醇胺(1∶1),氧化镁产品中w(氧化镁)=99.3%、w(氧化钙)=0.31%、w(氧化铁)=0.042%;使用草酸和柠檬酸作为复合络合剂时,在200 mL重镁水中加入1.0 g柠檬酸和2.0 g草酸,氧化镁产品中w(氧化镁)=98.2%、w(氧化钙)=0.24%、w(氧化铁)=0.030%。 Light-burned magnesia as a raw material was hydrated and carbonated to obtain magnesium bicarbonate liquor.Before the pyrolyzing of magnesium bicarbonate liquor,complexants were used to cover Fe and Ca impurities.Then the treated liquid was pyrolyzed to obtain basic magnesium carbonate which was calcined to magnesium oxide with low calcium and iron content.During the complexing purification of magnesium bicarbonate liquor,the Fe and Ca removing effects of single or compound complexing agents,suc...
CN202121979677.6一种摩托车点火器线圈用硅钢片
本实用新型涉及一种摩托车点火器线圈用硅钢片,包括E型件和I型件,所述E型件和I型件可组合成日字形;所述E型件包括竖边和设置在竖边三个横边,所述竖边与三个横边接触的位置设置孔眼;所述孔眼内径从为变径结构;位于E型件正面设置散热线槽,所述散热线槽一端与孔眼贯通,另一端指向凸部;位于E型件背面在散热线槽正对位置设置外凸线,所述I型件一侧设置与凸部匹配的凹部,在所述凹部之间凸台;所述凸台与凹台重叠;在凸台与凹部之间设置凸棱,所述凸棱位于I型件外侧。本实用新型设计新颖,改进巧妙,由于E型件具有弧形边可以有利于拾取,方便工作操作,同时采用采用接触的方式接触,增加了组合体的稳定性。
CN202120773168.1一种具有低应力隔磁桥的硅钢片和电机转子
本实用新型涉及电机技术领域,具体涉及一种具有低应力隔磁桥的硅钢片和电机转子。包括硅钢片、开设在硅钢片上的若干个磁钢槽组和永磁体,若干个磁钢槽组沿所述硅钢片周向分布,每个磁钢槽组均至少包括一对沿径向对称分布的磁钢槽,永磁体嵌设于磁钢槽内,磁钢槽朝向硅钢片内侧的一端设有空腔,一对磁钢槽的空腔之间通过隔磁桥隔离,隔磁桥的空腔上壁面与空腔侧壁面之间通过第一椭圆弧过渡连接,隔磁桥的空腔下壁面与空腔侧壁面之间通过第二椭圆弧过渡连接。有效降低该处隔磁桥在拐角处所受应力,进而提高该隔磁桥的强度,避免磁钢和铁芯产生形变而断裂。
CN202120300684.2一种用于硅钢片叠装的工装
本实用新型公开了一种用于硅钢片叠装的工装,包括安装底座,所述安装底座上设置有限位装置,所述限位装置包括多个水平限位柱和多个竖直限位柱;各个水平限位柱之间的缝隙的尺寸等于其对应放置的硅钢片的宽度,各个竖直限位柱与安装底座的底边之间的距离等于其对应放置的硅钢片的总长度;所述各个竖直限位柱设置在各个水平限位柱之间的缝隙所正对的位置;采用多个水平限位柱和多个竖直限位柱进行水平和竖直方向上均对硅钢片进行定位;使用此工装叠装出来的成品,长短一致,侧面相当整齐;本实用新型,结构简单,操作方便。
取向硅钢含铬无机绝缘涂层的研究进展
绝缘涂层可以有效提高硅钢片的耐蚀、耐腐、磁、绝缘等性能,因此取向硅钢涂装绝缘涂层是取向硅钢生产过程中重要的一环。本文对取向硅钢含铬无机绝缘涂层以及氮化铬涂层的性能优缺点进行了介绍,并对国内无机含铬取向硅钢绝缘涂层及氮化铬涂层的研究现状进行了综述。最后对未来含铬无机绝缘涂层的研发方向进行了展望。 Insulation coating can effectively improve the corrosion resistance of silicon steel sheet, such as corrosion, magnetic, insulation performance, thus oriented silicon steel insulation coating is the important part of oriented silicon steel production process. In this paper, the inorganic insulation coating oriented silicon steel containing chromium and chromium nitride coating performance advantages and disadvantages are introduced.In addition, the research status of insulation coating and chrom...
CN202120320747.0一种实验室模拟硅钢带连续常化退火炉
本实用新型公开了一种实验室模拟硅钢带连续常化退火炉,属于热处理技术领域。该退火炉包括:炉膛,沿退火炉本体的长度方向贯通,所述炉膛的两端的开口处设有炉门,炉门上设有透气孔,炉膛内自左向右依次分为多个加热区;滑轨,沿炉膛的长度方向设于所述炉膛的底部;移动机构,设在滑轨上且能沿滑轨移动;牵引绳,由耐高温材料制成,其一端与移动机构连接,另一端延伸至退火炉本体的外部;牵引绳收放机构,设于退火炉本体的外部,并与牵引绳的外端连接,用于收放牵引绳。本实用新型的退火炉采用三段加热区域,独立控温,能够模拟硅钢带预热、加热、均热、冷却等连续常化工艺,实验条件更接近工业生产。
新能源车电机用硅钢选材分析
为了提升新能源车用驱动电机的功率密度,各大电机厂商都在不断地提升电机转速,随之而来的问题就是电机的铁耗也在不断增高,如何降低电机铁耗成为了电机厂商必须要解决的难题。本文讨论了电机铁耗的组成部分及影响因素,并对1台8极48槽的永磁同步电机分别使用3种不同厚度的材料进行仿真,对比其效率及铁耗分布,推导出驱动电机中硅钢厚度、铁耗及成本的关系,最后对驱动电机选材提出建议。 In order to increase the power density of traction motor for new energy vehicles,major motor manufacturers have been constantly increasing the motor speed.The following problem that manufacturers have to solve is how to reduce the increasing iron loss when the motor speed is increased.The components and influencing factors of motors’ iron loss were discussed in this paper,and an 8-pole 48-slot permanent magnet synchronous motor using three different thickness materials was simulated.To compare i...
电工钢反复弯曲试验的影响因素
电工钢反复弯曲次数是电工钢性能检验的重要指标之一,直接影响到用户在使用电工钢过程的机加工性能。主要分析了试样宽度、试样张力、晶粒取向、反复弯曲设备等因素对电工钢反复弯曲试验的影响,并对各个因素的影响程度进行量化以及原因探讨,从而归纳形成各影响因素的基本规律,以便为电工钢实际生产、用户使用提供科学指导。结果表明:试样宽度增加,反复弯曲次数也会不断增加,晶粒位向对取向电工钢的反复弯曲次数影响较大,当支座顶部到拨杆底部的距离减小或拉紧力增加时,反复弯曲次数会不断减小,但当拉紧力达到60N以上时,对反复弯曲次数影响不大,试样经退火后,反复弯曲次数略有上升。 The reverse bend number is an important performance of electrical steels′capabilities,affecting the machining performance directly when the customers used.It investigated some factors,such as sample′s width,sample′s tension load,grain orientation and equipment,how to effect the reverse bend test for electrical steel,measured the influence degree,and discussed the reason,in order to form basic rules which could be guided the manufacturing and using for electrical steel.Results showed that the rev...
CN202110670657.9无取向硅钢及其生产方法
本发明揭示了一种无取向硅钢及其生产方法。所述生产方法包括:按照Si0.8~1.1%、Mn0.2~0.4%、不添加Sn和Sb进行炼钢,并制坯;将铸坯加热到1060~1120℃并保温150min以上,而后轧成厚度40~45mm的中间坯,再经精轧、卷取得到厚度为3.00±0.25mm的热轧卷板,精轧开轧温度≤872℃+1000*(11*[Si]‑14*[Mn]+21*[Al]);精轧终轧温度≤820℃,卷取温度≤560℃;常化、酸连轧,得到厚度为0.500±0.005mm的冷硬卷,常化温度850~900℃;成品退火温度820~880℃,退火后经冷却、涂层和精整,得到无取向硅钢。
CN202111082830.X一种取向硅钢边浪的控制方法、装置、设备和存储介质
本发明涉及取向硅钢技术领域,尤其涉及一种取向硅钢边浪的控制方法、装置、设备和存储介质,该方法包括:在将通过脱碳退火阶段的取向硅钢的带钢进行卷取过程中,在带钢的下端侧上刻上刻痕线,其中,下端侧为带钢与高温退火炉的承托底板接触的一侧,刻痕线平行于带钢轧制的方向;控制卷取后的带钢通过高温退火阶段和热拉伸平整阶段后至精整阶段时,沿着刻痕线,切除带刚的边浪;其中,边浪为在带钢的刻痕线至下端侧的边的部分。该控制方法可显著改善高温退火后取向硅钢边部浪形,有效降低精整切边量,提高取向硅钢的板形质量及成材率,降低生产成本。