钢厂
“双碳”大背景下的中国电工钢走势
阐述了电工钢在\"双碳\"中的作用,强调了电工钢的生产工艺技术及在减少碳排放、降低能耗中的作用,对下游能效升级带来明显的节能及降碳成果。同时,分析了2021年电工钢的生产运行情况,介绍了电工钢的未来发展,并针对如何减少碳排放以及生产更多的更低铁损、更高磁感的电工钢谈了几点启示。 The effects of electrical steels on carbon peak and carbon neutralization were expounded,especially on the achievements of obvious energy saving and carbon reduction to the downstream energy efficiency upgrading bringing from the production technology of electrical steels and their effects to reducing carbon emission and energy consumption.Meanwhile the production situation of electrical steels in 2021 was analyzed,and the future development of electrical steels was introduced,and some advices w...
CN202111083171.1一种高强型高频电磁性能优异的硅钢薄带板及生产工艺
一种高强型高频电磁性能优异的硅钢薄带板,钢中化学成分按重量百分比计为:C≤0.0027%、Si3.10%~3.35%、Als0.80%~1.2%、Mn0.20%~0.85%、P≤0.050%、S≤0.0020%、N≤0.0020%、Ti≤0.0020%、V≤0.0020%、Nb0.0050%~0.080%,其余为Fe和不可避免的杂质。本发明的无取向硅钢薄带产品用于新能源汽车驱动电机的制造,其强度高,中高频电磁特性优异。
CN202120558972.8一种硅钢片横剪线裁切设备
本实用新型公开了一种硅钢片横剪线裁切设备,包括:本体,所述本体包括工作台、挡屑罩和裁切装置,所述挡屑罩内水平固定安装有横杆,所述裁切装置与横杆下表面滑动连接;两个定位机构,所述定位机构包括第一螺纹杆、第一滑块和压板,所述挡屑罩内壁开设有两个安装槽,两根所述第一螺纹杆分别转动安装在两个安装槽内,两个所述第一滑块分别螺纹套设在两根第一螺纹杆上,两个所述压板分别与两个第一滑块远离安装槽槽底的一端水平固定链接;两个驱动机构,所述驱动机构用于控制第一螺纹杆发生转动。通过驱动装置控制定位机构中压板在垂直方向上的位置便可快速实现对硅钢片的定位工作和解除工作,方便快捷,提高了裁切工作的效率。
CN202110274559.3一种基于冷轧全流程数据的硅钢铁损预测方法
本发明一种基于冷轧全流程数据的硅钢铁损预测方法,其对冷轧硅钢进行全流程物料跟踪,以基于聚类算法分类,并选取代表性工艺作为神经网络的训练集来对冷轧硅钢铁损进行预测,以探明冷轧各机组工艺对冷轧硅钢铁损的影响。
中低牌号无取向电工钢轧制工艺研究
热轧轧制工艺对产品性能和轧制稳定性影响很大,对中低牌号无取向电工钢,当在两相区轧制时,热轧塑性明显降低,板形变坏,易出现边裂等情况。以50W1000为例,通过对其变形抗力进行研究,得出把两相区控制在F4与F5之间为最佳轧制工艺的结论。在此基础上制定了一套较为合理的热轧工艺制度。采用新的轧制工艺后,50W1000热轧精轧的稳定性明显改善,热轧产品合格率由开发初期的40%左右提高到95%以上。 The hot rolling process has great influence on product′s performance and rolling stability.For the low medium grade non-oriented electrical steel,when non-oriented electrical steel is rolled in tow phase region,the hot rolling plasticity reduces obviously,the shape of strip goes bad and easily to crack at the edge.The deformation resistance of 50W1000 steel was investigated.The results show that the optimal rolling process is to control the two phase region between F4 and F5.Based on the results...
取向硅钢的晶体衍射花样特征研究
广泛应用于电子电力行业的取向硅钢材料的磁性能与其晶体取向密切关联,对取向硅钢晶体衍射花样的研究非常重要.采用理论计算的方式研究了取向硅钢的晶体衍射花样特征,并绘制了取向硅钢的高斯织构理论极图、理论单晶透射电子衍射斑点花样和理论电子背散射衍射(Electron backscatter diffraction, EBSD)菊池花样.取向硅钢理论单晶衍射花样不仅可以为以后标定样品实测晶体衍射花样提供一种简单快捷的方法,也可以为样品检测提供一种标准.这种研究方法不仅限于取向硅钢,也被期待应用于其他材料晶体衍射花样研究. The magnetic properties of oriented silicon steels which are widely used in electronic and power industries are closely related to their crystal orientations, so it is very important to study the crystal diffraction patterns of oriented silicon steels. The characteristics of crystal diffraction patterns of oriented silicon steels are studied by means of theoretical calculation. The theoretical pole figures, theoretical single crystal transmitted electron diffraction patterns and theoretical elec...
CN202110334955.0一种变压器硅钢片智能叠片机械及叠片方法
本发明涉及一种变压器硅钢片智能叠片机械及叠片方法,包括工作台、叠片机构、交替机构、放置机构和交换机构,所述的工作台上方设置有叠片机构,叠片机构上右方设置有交替机构,叠片机构左右对称设置有放置机构,放置机构前方设置有交换机构,本发明采用放置机构放置待叠片的硅钢片,一号电动气缸与二号电动气缸分别交替带动连接板上的一号电磁铁与连板上的二号电磁铁吸附二号水平板上弧形杆内的硅钢片到一号数片板上的圆弧挡板内,当二号水平板上弧形杆内的硅钢片吸附完时,推动放置硅钢片的三号水平板在前后两个导向板之间,然后再将待叠片的硅钢片放在二号水平板上的弧形杆内,这种交换方式节约了叠放时间,提高了工作效率。
CN202011484349.9一种用于取向硅钢卷的焊缝切除方法
本发明公开了一种用于取向硅钢卷的焊缝切除方法,包括在焊接机组完成钢卷焊接后,在距离焊缝预设距离位置处冲孔;而后,钢卷到达成品退火工序时,利用孔洞检测装置检测焊缝冲孔,并根据焊缝冲孔得到焊缝位置,并记录该焊缝位置;并在分卷工序中,根据记录得到的焊缝位置对焊缝进行切除。这样,该方法利用焊缝冲孔,结合孔洞检测装置,将焊缝位置信息传递到分切工序,使得焊缝识别切除率较高,有效解决了取向硅钢焊缝无法精准定位切除的问题,实现了卷中焊缝多工序结合精准切除。
微合金元素对冷轧取向电工钢再结晶行为的影响
以取向电工钢成分为基础,制备了含C或Mn和S的4种实验钢。观察了接近平衡析出状态实验钢经60%冷轧后在600~1000℃范围再结晶退火过程中微观组织演变,统计分析了再结晶体积分数随退火时间的变化规律,进而计算了各实验钢静态再结晶的激活能。观察了高含C实验钢退火初期再结晶晶粒优先出现的部位。结果表明900~1000℃范围内各实验钢铁素体的化学成分相似,因而其再结晶激活能基本一致。在600~800℃范围内铁素体内会有阻碍再结晶进程的三次渗碳体析出,从而使再结晶激活能明显提高。高C含量实验钢中还会有从奥氏体转变而来的粗大珠光体或渗碳体,轧制过程中其附近形成的变形区会促进600~800℃加热时该区域附近率先发生再结晶形核、降低再结晶激活能。固溶的Mn、S元素可微弱提高再结晶激活能,但高Mn、S含量会改变粗渗碳体从奥氏体析出时的形态。 Four experimental steels based on grain oriented electrical steel containing C,or Mn and S were prepared.Microstructure evolution of the steels close to a state of equilibrium precipitation were observed during annealing processes at 600-1000 ℃after 60% cold rolling,the changes of recrystallization volume fraction were analyzed statistically as the annealing was prolonged,and the activation energy for static recrystallization of the steels were calculated.The locations,where the recrystallizatio...