所有分类
  • 所有分类
  • 未分类

【作者】 朱传芳; 潘恒韬; ...
2023-05-12 304 5.8

取向硅钢成品的晶粒尺寸非常大,其易磁化方向[001]晶向对于轧向的偏差角度对其磁性能影响极大。本文介绍了取向硅钢二次再结晶后成品晶粒位向的几种测定方法,包括侵蚀法、劳厄法、OIM法、极图法和非对称X射线衍射法等,并对这几种测量方法进行了比较。 The finished product of grain-oriented silicon steel has immense grain size ranging from millimeters to centimeters and the deviation angles of easy magnetization direction from rolling direction plays a remarkable role in magnetic properties of grain-oriented silicon steel.The methods in common use for determining the deviation angles of crystal direction are introduced,which include the etch-figure method,the Laue method,the OIM method,the pole figure method and the asymmetrical X-Ray diffract... 
2011-04-28 184 5.8

本实用新型公开了一种硅钢板带运输使用的固定设备,所述壳体的侧壁固定连接有多个第一放置轴,所述壳体的侧壁固定连接有多个第一限位套,且第一限位套与第一放置轴同轴心,所述第一限位套的内部设置有第一压板,所述壳体的内部设置有第一滑槽及第二滑槽,所述壳体的一侧设置有滑板。本实用新型通过将硅钢板带卷起后用绑线绑紧后,放入第一放置轴外表面后推入第一限位套内部,放好一行成硅钢板带后将将第一个滑板底部的滑杆放入第一滑槽内,推动滑板进入壳体内,使插杆插入凹槽内,再对下一列的硅钢板带进行放置,安装完成后,将挡板放入第二滑槽内,推动滑板向壳体内移动,将挡板向壳体内移动。
2021-08-18 188 6.8

对3层高硅电工钢复合板铸坯进行热轧及温轧变形加工后,采用正火、退火两种热处理方式处理,并观察轧制过程中产生的裂纹,研究不同状态下复合板的磁性能。对不同状态下的试样进行扩散退火处理,研究复合板中裂纹变化及其对磁性能的影响。结果表明:不同热处理工艺下合金内部的裂纹尺寸差异明显,裂纹尺寸对复合板的磁性能影响显著,相对于深裂纹,其他因素的影响较小;温轧变形加工后,复合板内层出现有序组织,但该有序组织在合金存在深裂纹的前提下并不能从本质上提高合金的磁性能;扩散退火工艺可以消除复合板内部的浅裂纹及微裂纹,但不能消除尺寸较大的裂纹,故而不能显著提高存在深裂纹的复合板的磁性能。 After hot rolling and warm rolling deformation processing of casting billet for three-layer high silicon electrical steel composite plate, it was normalized and annealed for heat treatment. Then, the cracks produced during the rolling process were observed, and the magnetic properties of composite plate in different states were also investigated. Furthermore, the samples in different states were subjected to diffusion annealing treatment, and the changes of crack in composite plate and their eff... 
2022-02-28 227 5.8

本发明公开了一种高磁感取向硅钢实验室轧机一次冷轧方法,包括:1)取样,实验室冷轧材料选取经过常化酸洗后的厚度为2.3mm的取向硅钢试样;2)制样,利用取向硅钢专用剪板机,裁剪试样尺寸为轧向600mm×横向150mm;将试样表层轻涂一层薄薄的轧制油;3)冷轧轧制规程制定,轧前厚度为2.3mm;其中:轧制总道次为6次时轧后厚度为0.35mm,轧制总道次为7次时轧后厚度为0.27mm,轧制总道次为8次时轧后厚度为0.23mm。本发明的目的是提供一种高磁感取向硅钢实验室轧机一次冷轧方法,为工业试制提供一定的技术参考,以及后续工艺研究提供了更加可靠的试样和条件。
2021-11-25 232 6.8

本实用新型涉及电机技术领域,具体涉及一种具有低应力结构的硅钢片、转子和电机。包括硅钢片、开设在硅钢片上的磁钢槽和嵌设在所述磁钢槽内的磁钢组件,所述磁钢组件包括多个磁钢组,所述磁钢组包括靠近转子边缘的一对小永磁体和靠近转子内侧的一对大永磁体,所述硅钢片在转子轭部沿周向分布有径向开槽,且所述径向开槽从硅钢片的中心向边缘延伸。其通过在转子轭部沿周向分设置从硅钢片的中心向边缘延伸的径向开槽,能降低大永磁体左右两侧铁芯刚度差距,从而有效降低隔磁桥处的应力,防止磁钢和铁芯产生形变而断裂。其无需改变电机转子外圆结构,在保证转矩输出的前提下,防止高速旋转时带来空气啸叫声。
2021-04-15 193 6.8

结合工业化生产的50A1300牌号无取向硅钢,分析了化学成分、RH精炼脱氧方式、板坯装炉温度以及热轧平整工艺等对磁性能的影响,探讨成品钢磁性能的改善。结果表明,采取改善后,50A1300牌号无取向硅钢的磁性能得到明显改善。2012年,该钢种平均铁损、磁感应强度分别达到5.26 W/kg、1.762 T,能够较好地满足用户市场需求及同行对标需要。 Based on the industrial manufacture of 50A1300 grade non-oriented silicon steel sheets,effects of chemical composition,deoxidization method in RH vacuum refining,charging temperature of steel slabs,hot rolling and flattening progress on magnetic properties are analyzed.The optimization methods of magnetic properties of steels are discussed. Results show that the magnetic properties are obviously improved by the adopted measures above. In 2012,the average core loss and the magnetic induction of 5... 
2014-02-28 228 5.8

提出了一种基于爱泼斯坦方圈族(包括标准25cm爱泼斯坦方圈、缩比的17.5cm和20cm爱泼斯坦方圈)和二级加权处理方法对爱泼斯坦测试数据,包括有效磁路长度、比损耗、励磁功率,进行处理的晶粒取向电工钢磁性能扩展模拟方法。详细地考察了励磁频率、试样剪切角度和环境温度对爱泼斯坦方圈测量结果的影响。研究结果表明,利用本文提出的爱泼斯坦方圈组合以及二级加权处理技术,可以有效地建立取向电工钢损耗模拟模型,从而更加准确地确定了取向电工钢的损耗,改善并提高了爱泼斯坦磁性能测试数据的应用价值。 The extended modeling of the magnetic properties of GO(grain oriented) electrical steel is presented in this paper which is based on a set of standard and scaled-down Epstein frames and a proposed two-level weighted processing of Epstein data, including the mean magnetic path length, specific magnetization loss and exciting power. The effects of excitation frequency, strip angle and ambient temperature on the results obtained from the Epstein frames are investigated. It is shown that using the p... 
2014-09-28 177 5.8

本发明公开了一种高效无取向硅钢极薄带的工业连续化生产方法,其包括异步轧制、脱脂、热处理、急速冷却、涂绝缘层、烘干烧结、卷取收集各工序;其中,异步轧制中的异步比为1:1.05~1:1.24;脱脂、热处理、急速冷却、涂绝缘层、烘干烧结、卷取收集工序为连续化生产工艺;热处理工序中,第一步为预热,预热温度为500℃~720℃,预热时间20秒~125秒;第二步为相变热处理,相变热处理温度为840℃~940℃,相变热处理时间100秒~600秒;急速冷却工序中,30秒内将钢带温度降温至350℃以下。优点在于:实现工业化连续生产无取向硅钢极薄带,有效提高产能,生产的无取向硅钢极薄带具备高磁感、低铁损等磁性能。
2021-07-31 187 6.8

本发明涉及一种硅钢片叠装用上料系统,包括放置板,设置于硅钢片横剪线的出料端处,用于接收硅钢片并堆放;供料板,设置于硅钢片叠装线的上料端处,用于接取放置板并对进行初定位;输送单元,设置于硅钢片横剪线的出料口处,用于放置板并实现放置板的输送;转运单元,设置于输送单元的出料口处,用于接取放置板并将放置板输送给供料板;上料单元,设置于硅钢片叠装线的上料端处,用于接取供料板并为硅钢片叠装线进行供料。本发明的优点在于:通过放置板、供料板、输送单元、转运单元、上料单元之间的相互配合,从而将硅钢片横剪线裁切好的硅钢片送至硅钢片叠装线处进行叠装,整个过程无需再由人工搬运,大大降低了人工劳动。
2021-06-09 143 6.8

本实用新型公开了一种用于硅钢片的焊接工装夹具,它包括底座,所述底座包括底板(1)、固设于底板(1)顶表面上的左挡板(2)和右挡板(3),左挡板(2)与右挡板(3)之间固设有位于底板(1)上的挡条(4),挡条(4)的前端面上设置有止口(5),左挡板(2)的前端部铰接有压杆(6),所述底板(1)的顶表面上且位于其左侧放置有压条(7),底板(1)的顶表面上且位于其右侧固设有限位条(8),压条(7)与限位条(8)之间设置有多个紧靠于一起的定位块(9),每个定位块(9)均放置于底板(1)的顶表面上。本实用新型的有益效果是:结构紧凑、提高硅钢片组件焊接质量、提高硅钢片组件生产效率、操作简单。
2021-11-19 160 6.8

本申请涉及硅钢制造技术领域,尤其涉及一种去除耐热刻痕取向硅钢中熔覆物的化学试剂及其方法。所述化学试剂的组分以质量分数计包括:强酸溶液:8%~20%;酸性氧化剂:5%~15%或助剂:5%~20%;其余为溶剂;其中,所述强酸溶液包括硫酸、盐酸和硝酸中任意一种。本申请实施例提供的该方法,通过10%~20%强酸溶液,可快速有效地去除取向硅钢刻痕处的熔融物,而酸性氧化剂:5%~15%,或助剂:5%~20%结合合适浓度的强酸溶液,可以将取向硅钢的基体破坏降到最小,两种综合作用,得到表面平整的耐热刻痕取向硅钢。