本实用新型公开了一种取向硅钢毛刷辊损耗检测装置及钢带刷洗机构。该取向硅钢毛刷辊损耗检测装置包括:固定基座,设置于刷辊的辊面侧方;压力测试元件,用于与刷辊的刷毛相顶压并测试刷毛对测力件的压力;接近机构,连接压力测试元件与固定基座,驱动测力件朝向或者背向刷辊运动。该取向硅钢毛刷辊损耗检测装置中的接近机构带动压力测试元件向刷辊一侧运动,直至刷毛与压力测试元件相顶压,当压力值至预定范围后,获得接近机构带动压力测试元件朝向刷辊的运动量,进而获得刷毛的损耗量;保证钢带刷洗清洁效果的同时,降低刷辊维护成本。
2021-03-19 153 6.8

采用火花源原子发射光谱分析测定电工钢中超低C,研究试样制备方法、Ar纯度和压力等条件对分析结果的影响,并对工作曲线进行了优化,实现了一次分析同时测定电工钢的多种元素,满足炉前和精炼在线分析的要求。 Ultra-low carbon in electrical steel is determined with spark-source atom emission spectrum.It is researched the influence of sample making method,purity of Ar,and pressure on analysis result.The work curve is optimized.The determination of many elements in electrical steel only in one analysis is realized.It meets demands of on-line analysis for blast furnace and refining. 
2011-09-28 143 5.8

抑制回硅是低硅品种钢冶炼的重点和难点,南钢中厚板卷厂通过转炉出钢弱脱氧操作,精炼炉弱脱氧升温,脱氧、脱硫造渣,连铸严格的保护浇注及吹氩塞棒、吹氩浸入式上水口的应用等一系列工艺优化和操作的改进,使整个冶炼过程钢水回硅量稳定控制在200×10-6以内,钢水终点成分完全满足低硅钢要求。 Control of increasing silicon is the emphasis and difficulty in low silicon varieties steel smelting.The Nisco Wide Plate/Coil Plant can control the silicon content in molten steel keeping within 200×10-6 through whole steelmaking process by using oxygen residual operation in converter tapping,oxygen residual and increasing temperature,deoxidation,desulfurization,slag refining,protection cast,blowing argon by plugged nozzle,blowing argon by submerged entry nozzle in continuous casting,and other ... 
2013-05-28 140 5.8

本实用新型公开了一种变压器用硅钢板滑石丸粘接加工设备,用于对变压器用硅钢片进行贴片,其结构包括:机械臂、抓取头、分道排序机构,所述抓取头位于机械臂的末端,用于抓取滑石丸,在抓取头上能够同时抓取多个滑石丸,配合机械视觉系统,就能够更精确的确定贴片位置,并完成贴片,提高了生产效率;所述分道排序机构包括:振动盘、排料板,振动盘中储存有一定的滑石丸,振动盘顶部的出料口与排料板连接,工作时振动盘中的滑石丸依次从出料口进入排料板中,在排料板上的物料通道中运动,物料通道的末端是多条分支,且末端向外敞开,抓取头能够在物料通道末端同时抓取多个滑石丸。
2021-03-09 161 6.8

本发明公开了一种轻便电动自行车轮毂电机用无取向电工钢及制造方法,属于无取向钢领域。针对现有小型电机无取向钢加工难度大,效率低的问题,本发明提供一种轻便电动自行车轮毂电机用无取向电工钢,包括如下重量百分比的各组分:Si:1.50%~3.00%;Als:0.50%~2.00%;Mn:0.20%~1.00%;P:0.01%~0.20%;C:≤0.005%S:≤0.03%;N:≤0.03%;Ti:≤0.005%,其余为铁和不可避免的杂质;其中C、S、N和Ti的重量百分比满足下式:C%+S%+N%+Ti%≤0.01%。本发明通过合理控制元素含量提高硅钢的延塑性,便于加工。本发明提供的制造方法降低卷绕铁芯中的涡流和磁滞损耗,同时能够避免钢卷表面氧化和表面氮化物析出,降低铁芯损耗,与现有同铁损级别无取向硅钢相比延伸率较高,后续冷加工性能更加优异。在保证优良性能的同时便于加工。
2021-03-29 145 6.8

本实用新型公开了一种防溢出的无取向硅钢绝缘涂液存储装置,涉及无取向硅钢绝缘涂液技术领域,为解决现有无取向硅钢绝缘涂液存储设备在存储过程中存在涂液过满,导致液体溢出产生浪费现象的问题。所述绝缘涂液存储机构本体上方的一侧设置有液位监测器,所述液位监测器的下端设置有监测杆,所述液位监测器的输出端设置有单片机,且液位监测器的输出端与单片机电性连接,所述绝缘涂液存储机构本体的内壁设置有压力传感器,且压力传感器设置有若干个,所述压力传感器的输出端与单片机的输入端电性连接,所述绝缘涂液存储机构本体的内部设置有泵体,且泵体设置有两个,所述泵体的一端设置有溢流输送管。
2021-09-02 172 6.8

冷轧无取向硅钢是高技术含量、高附加值产品,工艺复杂,生产周期长,过程控制难度大,被誉为钢铁产品中的\"工艺品\"。热轧生产工艺又是无取向硅钢生产的重中之重,直接决定了硅钢的铁损和电磁性等多项指标。 Cold rolled non-oriented silicon steel is high technology content、high addedvalue product. Its process is complex, Its production cycle is of Length, and Its Process control is difficult. Which is known as the iron and steel products \" Arts and crafts\". Hot rolling production process is the top priority of non-oriented silicon steel, Which Directly determines iron loss of the silicon steel and electromagnetic property, etc many index. 
2023-05-09 233 5.8

研究了退火温度和退火时间对电沉积硅钢试样中的断面层组织、硅在试样中的分布情况、织构分布和磁性能的影响。结果表明:退火温度为1000℃、退火时间为210 min时得到的试样晶粒分布均匀、硅在试样中分布均匀、硅平均浓度为6.3715%(接近6.5%)。试样的织构分析及磁性能检测的结果表明,在较高温度下延长退火时间可增加{100}和{110}面织构,降低铁损,所得试样的磁性能较为良好。 The effect of annealing temperature and time on the microstructure, distribution of silicon,texture and magnetism of the high silicon steel prepared by electrodeposition was investigated. The results showed that after annealing at 1000℃ for 210 min, the mean grain size of steel was about 190 μm with a uniform grain size distribution, and the silicon is also uniformly distributed on the entire cross section with an average Si concentration 6.3715%(close to 6.5%); With the increasing annealing tim... 
2014-07-28 175 5.8

本发明公开了一种消除取向硅钢热轧边裂的制造方法,通过成分设计、热轧加热和轧制参数优化等方面控制方面,有效解决取向硅钢热轧板边裂缺陷,提高材料的成材率,可以有效消除取向硅钢热轧板的边裂并能保证良好的成品磁性能。
2021-09-16 156 6.8

为提高无取向硅钢导磁性能,研究了不同剪切方式对无取向硅钢剪切处磁畴结构的影响。利用纳米磁流体观测无取向硅钢剪切后边部磁畴结构。结果表明,硅钢无论在机械剪切还是线切割后的边部磁畴都会发生不同程度的改变:线切割对边部磁畴结构改变较小,边部磁畴分布均匀且连续,在距边缘0~20μm范围内出现磁畴宽度变小现象;机械剪切对磁畴的改变较为严重,剪切处磁畴零乱且不连续,在距边缘20μm处仍难以观察到完整的磁畴结构。 The effects of different shearing modes on magnetic domain structure of cold rolled non-oriented silicon steel are studied in this paper.The magnetic domain of cold rolled non-oriented silicon steel is observed by nanometer magnetic fluid pattern method.The results show that the edge magnetic domain structure will be changed by mechanical shear and wire-electrode cutting,the variation of edge magnetic domain structure wire-electrode cutting edge is very small,the magnetic domain structure is wel... 
2012-04-28 153 5.8

本实用新型公开了叠片装置,以及采用该叠片装置的硅钢片收料设备,包括分料装置和本实用新型第一方面实施例的叠片装置,分料装置包括有分料件、上分料传送带和下分料传送带,上分料传送带的一端和下分料传送带的一端与分料件连接,分料件用于将硅钢片分别输送至上分料传送带和下分料传送带,本实用新型第一方面实施例的叠片装置,叠片装置的数量为两个,两个叠片装置上下平行设置,并且分别与上分料传送带和下分料传送带的远离分料件的一端连接。根据本实用新型的叠片装置,以及采用该叠片装置的硅钢片收料设备,可实现硅钢片的自动叠片,提高生产效率。
2020-12-31 184 6.8

本实用新型涉及硅钢片铁芯性能测试技术领域,公开了CD型硅钢片铁芯性能测试工装,包括:机台,上部后侧固定有竖直向上的后侧板;托板,水平设置在所述机台上方;夹持机构,设置在所述机台上,所述夹持机构包括:第二气缸,其驱动杆端部固定套接有夹持块,夹持块外端部固定有橡胶缓冲块;橡胶垫,固定在所述托板右侧上部。本实用新型通过设置第一气缸驱动连接于托板,可以先根据硅钢片的厚度,通过操作气缸控制器控制第一气缸工作带动托板在机台上进行升降高度,从而调整托板与夹持块的高度差,提高装置的实用性和广泛性,较为实用,适合广泛推广和使用。
2021-05-14 146 6.8

站点公告

网站试运行,请大家关注本站公众号,多提宝贵意见!

显示验证码
没有账号?注册  忘记密码?