钢厂
低温取向硅钢热轧态组织及织构的研究
利用热模拟试验机、光学显微镜和X射线衍射仪对Fe-3.2%Si低温取向硅钢热轧工艺参数对组织及织构的影响进行了研究。结果表明,Fe-3.2%Si硅钢在1110℃粗轧、880℃终轧,轧后以10℃/s的速度冷却到550℃卷取,然后空冷到室温,热轧硅钢板沿板厚方向的显微组织不均匀性显著,对后续发展完善的二次再结晶有重要作用。无论是热轧板,常化板还是冷轧板,它们的织构集中分布在γ取向线上,γ取向线的织构除取向密度不同外,织构种类是一致的,这说明γ取向线上织构是有继承性的。从热轧到常化,织构取向密度显著减小,经二次冷轧后,织构密度又显著升高,可见,轧制变形有助于织构的形成并使织构强度升高。 The influence of hot-rolled process parameters on the microstructure and texture of Fe-3.2%Si low temperature hot rolled grain-oriented silicon steel were researched by hot simulation experiment machine,light microscope and X-ray diffractometer.The results show that,Fe-3.2%Si silicon steel is rolled by the technology with a temperature of rough rolling of1110℃,finish rolling of 880℃,coiling with the speed of 10℃ /s,and then cooled to room temperature with air.The microstructure of hot-rolled sil...
CN202110137389.4一种强磁性取向高硅钢极薄带及其制备方法
本发明提供了一种强磁性取向高硅钢极薄带及其制备方法,属于电工钢制造领域,所述强磁性取向高硅钢极薄带包括以下质量百分比的元素:C:0.0045%~0.0060%、Si:4.5%~5.0%、Mn:0.23%~0.32%、S:0.02%~0.03%、Bi:0.03%~0.08%、Als:0.027%~0.035%、Cu:0.02%~0.03%,N:0.008%~0.010%,P<0.005%,其余为铁,其中所述Cu、S、N元素在熔炼时以含硫氮和铜的多核配位化合物的方式加入所述高硅钢;本发明通过对取向高硅钢的原料组分进行设计,采用含硫氮和铜的多核配位化合物和Bi元素作为合金抑制剂,所制得的强磁性取向高硅钢极薄带晶粒细小,组织均匀,具有高磁感应强度,低铁损的优良磁性能。
CN202110203335.3硅钢含铬涂层废液处理过程中六价铬浓度在线监控方法
本发明公开了一种硅钢含铬涂层废液处理过程中六价铬浓度在线监控方法,提出一种准确检测废液中六价铬含量的方法和检测时间的确定,实现了含铬废水原液中六价铬含量预测和焦亚硫酸溶液添加量的确定及六价铬在线检测预处理系统的启动时间的确定,确保处理装置安全高效运行。在酸化还原罐上安装氧化还原电位检测仪,实时检测含铬废液在整个处理过程中ORP的变化,推测含铬涂层废液中六价铬还原情况,初步判断还原过程的终点,为在线六价铬自动检测仪的启动提供依据,最终实现解毒后废液六价铬的含量低于0.05mg/L,达到六价铬含量超低处理的要求。
CN202111081530.X硅钢冷连轧轧制过程温度获取方法、装置及电子设备
本发明公开了一种硅钢冷连轧轧制过程温度获取方法、装置及电子设备,通过获取硅钢冷连轧生产过程的工业参数数据以及各机架间硅钢的实际温度测试数据,然后基于工业参数数据以及预设初始模型,确定硅钢冷连轧生产过程的温度预测模型,接着基于硅钢轧制前的预热温度以及温度预测模型,得到硅钢冷连轧轧制过程各机架变形区出口与下一机架变形区入口之间的预测温度数据,再将预测温度数据与实际温度测试数据进行对比,并根据对比结果中的温度差异值对相应机架间的乳化液参数进行修正,直至温度差异值小于预设阈值,得到修正后的温度预测模型,能够用于实现硅钢冷连轧轧制过程中,任意采样点硅钢温度的获取。
CN202110332173.3一种轻便电动自行车轮毂电机用无取向电工钢及制造方法
本发明公开了一种轻便电动自行车轮毂电机用无取向电工钢及制造方法,属于无取向钢领域。针对现有小型电机无取向钢加工难度大,效率低的问题,本发明提供一种轻便电动自行车轮毂电机用无取向电工钢,包括如下重量百分比的各组分:Si:1.50%~3.00%;Als:0.50%~2.00%;Mn:0.20%~1.00%;P:0.01%~0.20%;C:≤0.005%S:≤0.03%;N:≤0.03%;Ti:≤0.005%,其余为铁和不可避免的杂质;其中C、S、N和Ti的重量百分比满足下式:C%+S%+N%+Ti%≤0.01%。本发明通过合理控制元素含量提高硅钢的延塑性,便于加工。本发明提供的制造方法降低卷绕铁芯中的涡流和磁滞损耗,同时能够避免钢卷表面氧化和表面氮化物析出,降低铁芯损耗,与现有同铁损级别无取向硅钢相比延伸率较高,后续冷加工性能更加优异。在保证优良性能的同时便于加工。
预退火温度对高磁感取向硅钢初次再结晶织构的影响
对高磁感取向硅钢冷轧板分别进行800、950、1050和1120℃不脱碳的预退火处理,在800℃预退火,成品的磁性能较好。织构分析的结果表明,随着预退火温度升高,初次再结晶后有利织构组分{111}<112>与不利织构组分(118)[110]的比值f(111)/f(118)逐渐降低,初次再结晶织构的变化是成品磁性的影响因素之一。 Preliminary annealing process at different temperatures for cold-rolled strips of a high permeability grain-oriented silicon steel was investigated to study the effect of the annealing temperature on microstructure and magnetic performance of the steel.Results show that the magnetic performances of the products annealed at 800 ℃ are best.Analysis of primary recrystallization texture indicates that with rising temperature,f(111)/f(118) which is the ratio of the favorable component {111}<112>...
树脂含量对半无机型无铬无取向硅钢涂层性能的影响
本文研究了丙烯酸树脂含量对以Al(H2PO4)3为基料的无铬无取向硅钢绝缘涂层各项性能的影响.用盐雾实验、动电位极化及交流阻抗等试验手段研究了不同树脂含量对硅钢绝缘涂层的耐盐雾性能和电化学行为的影响,同时采用SEM对涂层的表面形貌和附着性进行研究.结果表明,树脂含量为19.9~29.4%时,涂层的耐蚀性和附着性最好;树脂含量过多时,涂层的耐蚀性和附着性均较差. This paper studies the influence of acrylic resin on the performance of insulating coating of aluminum dihydrogen phosphate on chromium-free non-oriented silicon steel.Salt spray experiment,potentiodynamic polarization and electrochemical impedance spectroscopy were used to study the influence of acrylic resin content on the salt spray resistance and electrochemical behavior of the insulation coating of nonoriented silicon steel.The surface morphologys and adhesion of coating were tested by SEM....
CN202121871279.2一种便于操作的硅钢板带加工用打标装置
本实用新型公开了一种便于操作的硅钢板带加工用打标装置,包括工作台,所述工作台的下端固定连接有多个支撑地脚,所述工作台的两端上下侧均转动连接有限位辊筒。本实用新型在进行打标时,速度监测仪会对不锈钢带的移动速度进行监测,位移机构会带动打标机构以与不锈钢带位移方向相同、与不锈钢带移动速度相等的状态进行移动,在打标机构移动的过程中,激光打标头对不锈钢带进行打标,打标结束后,位移机构带动打标机构反向位移,回到起始点,再进行下一次打标,从而可以使得不锈钢带在保持移动的状态下,使用打标机构对不锈钢带进行打标,提高打标效率,且打标机构可以对激光打标头的位置和高度进行调节,可以对不同尺寸的不锈钢带进行打标。
取向硅钢生产工艺技术分析和发展趋势
介绍了普通取向硅钢(CGO)和高磁感取向硅钢(Hi-B)铸坯高温加热两次冷轧、一次冷轧和铸坯低温加热两次冷轧、一次冷轧法4种成熟生产工艺的主要技术参数,取向硅钢理论研究(Goss晶核和抑制剂)和生产技术现状。取向钢的发展趋势为:提高(110)[001]晶粒取向度,降低取向硅钢铁损,发展铸坯低温加热(≤1 300℃)和薄板坯连铸连轧流程生产取向硅钢工艺。 Main technology parameters of four developed process:cast bloom higher temperature heating-double cold rolling or single cold rolling,lower temperature heating-double cold rolling or single rolling process for production of common grain oriented silicon steel(CGO) and high magnetic induction grain oriented silicon steel(Hi-B),theory research on grain oriented steel(Goss nucleus and inhibitor) and present situation of process are summarized in this paper.The development trend of grain oriented si...
高温硅钢加热炉双蓄热燃烧技术的探讨
介绍了双蓄热燃烧技术的特点和高温硅钢加热炉的特点,探讨了双蓄热燃烧技术在高温硅钢加热炉中使用的技术难点,分析了双蓄热燃烧技术在高温硅钢加热炉上使用的可能性。 Introduced characteristics of double regenerative combustion technology and high temperature silicon steel reheating furnace,discussed technical difficulties for using double regenerative combustion technology,analyzed the possibility of double regenerative combustion technology applied to high temperature silicon steel reheating furnace.
CN202123127843.2硅钢片生产用上料装置
本实用新型公开了硅钢片生产用上料装置,属于硅钢片生产领域,包括本体,所述本体包括侧板和U型板,所述侧板固定连接在U型板的一侧,所述本体的顶部横向设置有平移机构,所述平移机构上安装有气缸,所述气缸的底部安装有吸盘,所述U型板内腔的底部竖向固定连接有弹簧,所述弹簧远离U型板的一端水平固定连接有升降板,所述平移机构包括电机、螺纹杆、限位板和移动块,所述电机安装在侧板的顶部,所述电机的输出轴与螺纹杆的一端固定连接,通过设置弹簧,在第一个物料从上料装置移出后弹簧的弹力推动剩余物料,使得剩余物料进行上升,避免吸盘触碰不到物料的问题,简化吸盘移动轨迹,加快上料速度。