CN202123227418.0一种铁芯硅钢片卷材的自动放卷上料装置
本实用新型公开了一种铁芯硅钢片卷材的自动放卷上料装置,包括放卷机、导向平台和防折组件,所述导向平台间距设置在放卷机的下方,所述导向平台与放卷机之间构成供料带缓冲的缓冲空间,所述料带在缓冲空间内呈U型状走向,所述导向平台的上方间距设置有防折组件,所述防折组件与导向平台之间构成供所述料带通过的导向通道,所述防折组件设置在料带的内弯侧。通过防折组件对料带的内弯侧进行支撑,能够有效的防止料带被过度弯折,能够对料带进行缓冲和缓冲保护,保证料带放卷上料的稳定性。
配分温度对碳-锰-硅钢显微组织与力学性能的影响
对碳-锰-硅钢进行不同配分温度的Q&P(Quenching and Partitioning)处理,测试了热处理后不同钢的力学性能和残余奥氏体含量,并用扫描电子显微镜和透射电镜观察其显微组织,分析了配分温度对显微组织和力学性能的影响。结果表明:试验钢显微组织基本由低碳板条状马氏体、块状铁素体和条状残余奥氏体组成;随配分温度的升高,试验钢的抗拉强度呈下降趋势,伸长率与奥氏体含量的变化趋势相同,但变化规律不确定;提高锰含量能稳定残余奥氏体,从而提高试验钢的伸长率,并使伸长率对配分温度不敏感。 The C-Mn-Si steel was quenched and partitioned at different partitioning temperatures,the mechanical properties and residual austenite contents were investigated,the microstructure was observed by SEM and TEM,and the effect of partitioning temperature on microstructure and mechanical properties was analyzed.The results show that the microstructure of the tested steel consisted of lath martensite with low carbon,nubby ferrite and banded residual austenite.The tensile strength of the tested steel ...
CN202122485286.5一种硅钢片生产用冲压机构
本实用新型公开了一种硅钢片生产用冲压机构,包括安装底板,所述安装底板的侧壁设置有固定件,安装底板的上表面设置有工位调节机构,工位调节机构包括固定连接在安装底板上表面的四个安装块,每两个安装块为一组,两组安装块的相对面均转动连接有往复丝杠,正面两个安装块的正面均固定连接有驱动往复丝杠转动的伺服电机,往复丝杠的表面螺纹连接有工位安装板。该硅钢片生产用冲压机构,在冲压加工过程中,通过伺服电机带动往复丝杠转动,能够带动两个工位安装板移动,从而使冲压母模沿往复丝杠进行移动,在加工过程中,通过对两个冲压母模进行交换,能够节省硅钢片上料与下料的时间,从而提高冲压加工的效率,且能够提高生产的安全性。
CN202111670012.1一种电机定子硅钢片激光焊接装置
本发明涉及一种电机定子硅钢片激光焊接装置,其包括底座;工作台,其安装于所述底座;下压旋转组件,其包括:焊接支座,其安装于所述底座上;用于压紧定子硅钢片的下压组件,所述下压组件位于所述工作台的上方,且可沿垂直于所述工作台的板面的方向移动;用于驱动所述定子硅钢片旋转的旋转组件,其安装于所述下压组件靠近所述工作台的一端,所述旋转组件可绕所述下压组件的轴线旋转;以及激光焊接头组件,其固定于所述底座。通过在焊接工作台上设置下压旋转组件,下压组件可以驱动下压使定子硅钢片压紧,旋转组件可以驱动定子硅钢片旋转,进行下一道焊缝焊接,直到该定子硅钢片所有焊缝焊接完成,使用方便,省时省力。
CN202110555870.5一种电化学评价取向硅钢氧化层的装置及方法
本发明公开了一种电化学评价取向硅钢氧化层的装置及方法,包括电解池、设于电解池一侧的磁铁组、设于电解池上的饱和甘汞电极和铂电极以及与电解池连接的电化学工作站;磁铁组包括固定在电解池上的固定磁铁和与固定磁铁磁性连接的移动磁铁,移动磁铁设于电解池侧面的出口上;参比电极设于磁铁组与辅助电极之间;参比电极和辅助电极与电化学工作站连接。本发明的评价方法通过电化学测量取向硅钢试样的电位‑时间曲线,计算出取向硅钢氧化层各分层的溶解电量,实现了对取向硅钢氧化层各分层的快速、准确测定,可以区分出Mg2SiO4玻璃膜底层、SiN层、SiO2层、FeO及铁橄榄石层等分层性能,为取向硅钢生产工艺参数的控制提供指导。
取向硅钢中含铜抑制剂的固溶析出行为
含铜抑制剂作为取向硅钢的主抑制剂或辅助抑制剂不仅可以抑制初次晶粒的长大,促进二次再结晶,还可以降低铸坯的加热温度。取向硅钢中主要抑制剂为10~50 nm Cu2S,在钢的铸坯、热轧、冷轧、脱碳等工艺过程均可析出;(Cu,Mn)1.8S、Cu1.8S、ε-Cu等主要作为辅助抑制剂,尺寸一般为30~50 nm(或大于50 nm),主要在热轧阶段析出。总结了国内外有关取向硅钢中含铜抑制剂析出行为的研究进展,当前主要研究不同生产流程和工序中含铜抑制剂的析出行为和作用机理。 As main inhibitor or auxiliary inhibitor for grain-oriented silicon steel,the particles of inhibitor bearing copper not only inhibit the primary crystal growing and promote the secondary recrystallization,but also decrease the heat temperature of casting slab.The main inhibitor for grain-oriented silicon steel is 10~50 nm Cu2S,which precipitate in process and procedure including steel casting slab,hot rolling,cold rolling and decarburizing process,while the 30~50 nm or more than 50 nm...
新日铁高强度无取向电工钢的研究进展
针对新日铁公开的相关专利,总结日本高强度无取向电工钢的研究进展,分析了各专利化学成分、生产工艺及产品性能的特点,指出固溶强化、细晶强化、析出强化、位错强化都有可能被用来提高无取向电工钢的强度。在高强度无取向电工钢的研发过程中,需要根据其具体用途确定目标性能,再采用合适的强化手段,从而实现力学性能、磁性能和生产性能之间的平衡。 Authors summarize the research progress of high strength non-oriented electrical steel in Japan by learning related patents brought into the public by Nippon Steel. Authors also analyze the characteristics of the chemical composition, production technology and properties of products in the patents and point out that any ones of solution strengthening method, fine-grain strengthening method, precipitation strengthening method or dislocations strengthening method may be used to improve the strengt...
CN202110953215.5一种含磷高磁感无取向硅钢的生产方法
本发明涉及一种含磷高磁感无取向硅钢的生产方法,工艺路线:铁水脱硫-转炉冶炼-RH精炼-连铸-热轧-酸洗-冷轧-连续炉退火-涂层-性能检验-包装,具体步骤包括:1)将钢水冶炼至目标成分后采用连铸方式将钢水铸成坯;2)热轧板坯加热炉均热段板坯温度950~1050℃,终轧温度控制在780~830℃,卷取温度600~680℃;3)酸洗后冷轧,控制冷轧整体压下率80%以上,至成品厚度,增加剪切带组织;4)连续退火炉快速加热段温度设定1000~1150℃,增加有利织构组织形核;均热段温度设定750~830℃,全氮气干气氛保护,退火工艺速度110~150m/min,满足晶粒度8~4级。本发明在减少硅、铝、锰合金添加量的情况下,改善铁损提高磁感性能,提高机械性能。
CN202110759732.9一种无机绝缘漆及其制备方法以及在极薄硅钢带中应用
本发明提出了一种无机绝缘漆,由下列物质组成,其重量百分比为:质量百分含量为50~55%的磷酸二氢铝溶液:30~70%;质量百分含量为60~70%的磷酸二氢锰溶液:10~15%;质量百分含量为80~85%的硼酸溶液:5~6%;质量百分含量为99%的硅烷偶联剂溶液:1~5%;质量百分含量为30~35%的硝酸盐溶液:0.1~0.5%;硅溶胶:10~15%;纳米硅酸铝:10~15%;纳米二氧化硅:20~30%;消泡剂:1~5%;水溶剂:适量。本发明采用磷酸二氢铝、纳米二氧化硅为主料制备了一种极薄硅钢带薄绝缘无机绝缘漆的涂层,涂层厚度均匀性好,涂层表面光亮、附着性强、绝缘电阻系数高。
剪切方式对冷轧无取向硅钢边部磁畴的影响
为提高无取向硅钢导磁性能,研究了不同剪切方式对无取向硅钢剪切处磁畴结构的影响。利用纳米磁流体观测无取向硅钢剪切后边部磁畴结构。结果表明,硅钢无论在机械剪切还是线切割后的边部磁畴都会发生不同程度的改变:线切割对边部磁畴结构改变较小,边部磁畴分布均匀且连续,在距边缘0~20μm范围内出现磁畴宽度变小现象;机械剪切对磁畴的改变较为严重,剪切处磁畴零乱且不连续,在距边缘20μm处仍难以观察到完整的磁畴结构。 The effects of different shearing modes on magnetic domain structure of cold rolled non-oriented silicon steel are studied in this paper.The magnetic domain of cold rolled non-oriented silicon steel is observed by nanometer magnetic fluid pattern method.The results show that the edge magnetic domain structure will be changed by mechanical shear and wire-electrode cutting,the variation of edge magnetic domain structure wire-electrode cutting edge is very small,the magnetic domain structure is wel...
CN202121007099.X一种电工钢生产高温处理用上料装置
本实用新型公开了一种电工钢生产高温处理用上料装置,包括工作台和底板,所述工作台的顶部外壁固定有对称分布的两个第一侧板,且第一侧板的相对侧外壁通过轴承转动连接有等距分布的第一转辊,两个所述第一侧板的顶端转动连接有对称分布的两个活动框,且活动框的一侧转动连接有等距分布的第二转辊,所述活动框的顶部外壁固定有安装杆,且安装杆的顶端转动连接有转块,所述转块的内部开有螺纹孔。本实用新型双向螺纹杆带动两个转块相向移动,使两个活动框转动,一端相互靠近,将第一转辊上的电工钢向中间推动,从而使电工钢落在传送带中间位置,向上运输到正确的位置,解决了电工钢偏移输送路线,无法输送到准确的位置,发生脱落的问题。
CN202111181650.7一种CSP流程生产高效冷轧无取向电工钢及生产方法
本发明提供了一种CSP流程生产高效冷轧无取向电工钢及生产方法,成分:C≤0.0030%、Si 1.00‑1.70%、Als≤0.0050%、Mn 0.10‑0.30%、Sn0.01‑0.3%、P≤0.050%、S≤0.0080%、N≤0.0030%、Nb≤0.0030%、V≤0.0030%、Ti≤0.0030%,其余为Fe以及不可避免的杂质。与现有技术相比,本发明CSP流程生产高效冷轧无取向电工钢的方法,通过控制钢中的化学成分,并采用合适的生产工艺,实现了表面质量优良,低铁损、高磁感、低制造成本且生产高效。