钢厂
双辊薄带连铸3.98%Si-0.71%Al无取向硅钢的组织、织构和磁性能
采用双辊薄带连铸工艺制备了厚度为2.4mm的3.98%Si-0.71%Al无取向硅钢带,经常化、冷轧、不同温度退火后,对其显微组织、析出物、织构和磁性能进行了检测分析。结果表明:随着退火温度的提高,退火板晶粒尺寸增大,组织均匀性提高;退火板析出物主要是AlN和MnS与AlN复合析出物,尺寸较粗大,达0.5~2.5μm;退火板织构沿厚度方向变化明显,表层和1/2层存在较强的{100}织构,1/2层还存在较强的{111}织构,1/4层主要是{112}织构;随退火温度的升高相应的铁损和磁感应强度均降低。 Using twin roll thin strip continuous casting technique,the 3.98%Si-0.71%Al no-oriented silicon steel strip in thickness of 2.4mm was produced.The microstructure,precipitates,texture,and magnetic properties of the sheet after normalizing,cold rolling and annealing at different temperatures were studied.The results show that with annealing temperature increase,the grain size and uniformity of annealed sheet increased.The main precipitates in coarse size of 0.5-2.5μm in annealed sheet were AlN and...
CN202110041772.X一种酸洗低牌号无取向硅钢的方法
本发明公开了一种酸洗低牌号无取向硅钢的方法,从酸洗线前拉矫机的延伸率设定、酸液浓度、酸液温度、酸洗槽内液位的控制、酸液中铁离子的含量等方面入手,解决酸洗低牌号无取向硅钢的问题。
宝钢无取向电工钢发展历程及生产技术进步
简要介绍了宝钢无取向电工钢的发展历程、产品大纲、电磁性能控制情况,以及高附加值新产品的开发、应用情况。概述了近年来宝钢无取向电工钢生产技术进步,主要包括夹杂物控制技术、连轧机高牌号硅钢制造技术、同板差控制技术、环保涂层开发技术等。 This paper briefly summarizes the development history, product catalogue, and magnetic properties of non-oriented electrical steel sheets at Baosteel, as well as the development and application of high-value-added steel grades. Recent advances in manufacturing electrical steel sheets are also introduced, including technologies for controlling inclusion, producing high-grade steel strips by a tandem rolling mill, and controlling the transverse thickness difference of steel sheets, as well as the ...
无取向电工钢边部减薄控制技术研究
叠片系数是冷轧无取向电工钢的重要质量指标。为了提高叠片系数,必须保证无取向电工钢板形良好以及横向厚差小。针对攀钢冷轧厂4机架HC轧机轧制无取向电工钢的边部减薄问题,以无取向电工钢横向厚差最小作为目标函数,建立了一套针对无取向电工钢边部减薄控制的辊型曲线优化数学模型,开发了无取向电工钢专用辊型曲线,使无取向电工钢横向厚差从25μm降低到10μm以下,取得了良好的控制效果。 The lamination factor is an important quality index of non-oriented silicon steel strip.Considering the lamination factor,the non-oriented silicon steel must have a good shape and a smaller transverse thickness difference.In order to solve the edge thinning of non-oriented silicon steel strip in Panzhihua Steel,a mathematic model for designing the roll shape is built.In the model,the transverse thickness difference of non-oriented silicon steel strip is taken as the objective function.Based on t...
CN202111121077.0一种耐热刻痕型取向硅钢涂层用涂液、取向硅钢板及其制造方法
本发明公开了一种耐热刻痕型取向硅钢涂层用涂液,其溶剂为水,其含有:磷酸盐、胶态二氧化硅、铬酐和乙醇。本发明还公开了一种耐热刻痕型取向硅钢板,其包括基板,所述基板表面具有采用上述的耐热刻痕型取向硅钢涂层用涂液涂覆在基板上而形成的涂层。相应地,本发明还公开了上述取向硅钢板的制造方法,其包括步骤:在基板表面涂覆所述涂液,基板的刻痕沟槽涂液填充率>95%;进行烧结处理,其中烧结处理中的板温为780‑900℃。本发明的耐热刻痕型取向硅钢涂层用涂液具有良好的流动性,其可以涂覆于耐热刻痕取向硅钢基板的表面中,涂覆后,能有效填充基板的刻痕沟槽,且可以在其表面形成涂层,保证耐热刻痕取向硅钢在具有低铁损的同时具备更高的安全性。
微量Sn对0.4%Si无取向硅钢组织和磁性能的影响
结合实际生产0.4%Si无取向硅钢,统计了不含Sn和0.025%Sn无取向硅钢的磁性能变化,利用金相显微镜、X射线衍射仪观察分析不同成分下试样的显微组织和微观织构。试验结果表明:Sn元素可以显著降低无取向硅钢的晶粒尺寸,0.025%Sn试样的平均晶粒尺寸比不含Sn减小28.4%;加入Sn元素后抑制了无取向硅钢中不利于磁性能的{111}面织构组分强度,提高了对磁性能有利的{100}面织构组分强度,0.025%Sn与不含Sn相比磁感均值从1.756 T提升至1.768 T,铁损均值从5.476 W/kg降低至5.204 W/kg,明显改善了无取向硅钢磁性能。 In this paper combined with the actual production of 0.4% Si non oriented silicon steel, the magnetic properties of non oriented silicon steel without Sn and 0.025% Sn were counted. The microstructure and microtexture of samples with different compositions were observed and analyzed by metallographic microscope and X-ray diffraction. The results show that: Sn can significantly reduce the grain size of non oriented silicon steel, and the average grain size of 0.025% Sn sample is 28.4% smaller tha...
CN202121345062.8一种硅钢片钢卷原料拆包装置
本实用新型涉及拆包装置技术领域,且公开了一种硅钢片钢卷原料拆包装置,解决了现有的硅钢片钢卷原料拆包装置不具备便捷移动功能的问题,其包括装置本体,所述装置本体的底部设有安装块,安装块顶部的两端均安装有螺纹销,安装块的两端均安装有稳定机构,安装块底部的两端均固定连接有支撑板,安装块底部的两侧均安装有连接板,两个连接板底部的两端均安装有移动轮,安装块底部的中部安装有一对气缸;使本装置能够在需要时便捷的进行移动,并且能够有效的保持连接板的稳定,同时能够有效的对插板进行固定,使置物板能够有效的保持稳定,从而能够在需要时便捷的搬运本装置,进而提高了本装置的实用性。
CN202110958410.7一种硅钢片压装工装
本发明公开了一种硅钢片压装工装,其涉及电机生产技术领域。其技术方案要点包括下压板,所述下压板上设置有限位结构,所述限位结构用于在硅钢片压装过程中对硅钢片进行限位;所述限位结构包括能够转动调节的限位挡块,所述限位挡块包括多个分别用于对不同尺寸规格的硅钢片进行限位的限位面,且该多个所述限位面与限位挡块的转动轴线之间的最小距离均不相同。本发明能够适用于多种规格的硅钢片,而且操作方便,稳定性好。
CN202111672979.3一种双取向硅钢薄带及其制备方法
本发明属于双取向硅钢技术领域,公开了一种双取向硅钢薄带及其制备方法,包括:选取具有Si、Al、Mn、C和Fe,且具有一定取向的硅钢薄带;将其进行冷轧;将冷轧板在N2、H2保护气氛中进行退火处理。本发明通过合理的轧制和退火工艺搭配,使具有Goss取向的硅钢薄带转变为具有旋转立方取向的硅钢薄带,将单取向硅钢转变为双取向硅钢。本发明具有工艺简单和便于利用钢铁企业现有设备的特点,所制备的双取向硅钢薄带具有双向铁损低和磁感高的性能。本发明制备的双取向硅钢薄带在与轧向成45°的两个方向上具有优异的双向磁性能,解决了现有双取向硅钢薄带的制备工艺复杂、设备要求高、不利于工业生产的问题。
CN202080097191.1电工钢板粘接涂料组合物、电工钢板层叠体及其制造方法
根据本发明的一个实施例的粘接涂料组合物,其包含聚乙烯丙烯酸酯100重量份和无机颗粒3至25重量份,所述聚乙烯丙烯酸酯包含由以下化学式1表示的重复单元和由以下化学式2表示的重复单元,所述聚乙烯丙烯酸酯包含75至95重量%的由以下化学式1表示的重复单元、5至25重量%的由以下化学式2表示的重复单元。
CN202122845310.1一种用于硅钢片的焊接工装夹具
本实用新型公开了一种用于硅钢片的焊接工装夹具,它包括底座,所述底座包括底板(1)、固设于底板(1)顶表面上的左挡板(2)和右挡板(3),左挡板(2)与右挡板(3)之间固设有位于底板(1)上的挡条(4),挡条(4)的前端面上设置有止口(5),左挡板(2)的前端部铰接有压杆(6),所述底板(1)的顶表面上且位于其左侧放置有压条(7),底板(1)的顶表面上且位于其右侧固设有限位条(8),压条(7)与限位条(8)之间设置有多个紧靠于一起的定位块(9),每个定位块(9)均放置于底板(1)的顶表面上。本实用新型的有益效果是:结构紧凑、提高硅钢片组件焊接质量、提高硅钢片组件生产效率、操作简单。
热轧加热时间对稀土取向硅钢抑制剂固溶行为的影响
借助OM、激光共聚焦显微镜、质谱仪和电解萃取等设备和方法,研究了添加微量稀土La(质量分数0.001 1%)的取向硅钢在轧制前采用不同加热保温时间对抑制剂固溶行为的影响。结果表明:当稀土取向硅钢在1 250℃分别保温10、20、30 min后,试验钢晶粒尺寸随保温时间延长有先快后慢的长大趋势;三种抑制剂元素Mn、Cu和Al均发生固溶,保温时间对Mn和Cu两种元素的固溶影响明显,固溶量分别由69.8%和43.7%增加至84.2%和85.2%;随着保温时间的延长,稀土取向硅钢中抑制剂的小尺寸未溶物逐渐减少直至消失,较大尺寸未溶物(300~600 nm)逐渐转变为小尺寸未溶物逐步溶入基体中,数量减少且未溶物的类型由复杂逐渐转变为单一。 In this paper the solid solution behavior of the inhibitor under various holding time in 0.001 1 %La oriented silicon steel during reheating had been investigated by using OM, LM, methods of electrolytic extraction and mass spectrometer. The results showed that grain size of the test steel increased significantly with the holding time prolonging when the rare earth oriented silicon steel was heated to1 250 ℃ and held for 10, 20 min and 30 min respectively, and the growth trend slowed down after ...