钢厂
大压下率冷轧无取向硅钢再结晶织构演变
研究了冷轧95%变形量无取向硅钢不同退火温度(710~1 050℃)下再结晶织构特征.再结晶刚完成时(710℃退火),呈现强γ({111<112>~<134>)与弱{114}<481>织构特征;随退火温度升高至900℃,γ明显减弱,{114}<481>组分持续增强,形成典型的{h,1,1}<1/h,1,2>织构;进一步升温至1 050℃,再结晶织构不再发生明显变化.基于EBSD分析,{114}<481>组分的持续强化可归因于其明显的尺寸优势以及较高频率的高能晶界(取向差角为20°~45°). A non-oriented silicon steel was heavily rolled to 95% reduction and subsequently annealed at 710~1 050 ℃ to investigate recrystallization texture evolution.When annealed at 710 ℃ with complete recrystallization,the texture is characterized by a strong partial γ fiber spreading from {111}<112> to {111}<134> and a weak {114}<481> component.As annealing at 900 ℃,γ fiber is decreased significantly while {114}<481> is increased consistently,producing a typical {h,1,1}<1/h,...
CN202121387289.9一种硅钢片横剪线用转运系统
本实用新型涉及一种硅钢片横剪线用转运系统,包括一暂存组件,所述暂存组件包括一暂存支架,在暂存支架上安装有若干存放条料卷用的凸台;一转运组件,包括一转运底座,该转运底座由第一水平移动机构驱动进行往复移动,在转运底座上安装有一转运支架,所述转运支架由一旋转机构驱动进行转动,且转运支架由第二水平移动机构驱动进行水平移动,在转运支架上安装有一转运托架,所述转运托架由一升降机构驱动上下升降。本实用新型的优点在于:通过暂存组件与转运组件之间的相互配合,实现了条料卷的竖直存放,方便了后续人员选用所需宽度的条料卷,也实现了条料卷的自动流转,有效的降低了人工劳动强度,对于人力资源的消耗也减少了。
无取向电工钢RH脱硫渣系的研究
在15 kg真空感应炉上,用CaO-Al2O3-SiO2-MgO渣系进行脱硫试验,探讨了脱硫渣系碱度、MI、Al2O3、CaF2对脱硫效果的影响。研究结果表明,随脱硫渣系碱度、MI、Al2O3和CaF2含量的增加,脱硫率都呈现先增加后减少的趋势。初始硫含量为0.009 33%~0.010 73%,加入脱硫渣系4 min时间内表观脱硫速率为(0.000 96~0.001 49)%/min,平均脱硫率为81.2%,最高达86.8%。当脱硫渣中w(CaO)=58.15%、w(SiO2)=4.85%、w(Al2O3)=25%、w(MgO)=6%、w(CaF2)=6%,脱硫效果最好,此时钢液中硫为0.001 33%。 Experiments on desulfurization of molten steel using CaO-Al2O3-SiO2-MgO based desulfurization slag was carried out in a 15 kg vacuum induction furnace. The effects of desulfurization slag basicity,MI, Al2O3and CaF2on desulfurization of molten steel were studied. The results show that with the increase of basicity,MI,Al2O3or CaF2in desulfurization slag,the desulfurization rate rises initially and then decreases. In addition,as the initial sulfur content is 0. 009 33% ~ 0. 010 73%,the apparent des...
CN202110041772.X一种酸洗低牌号无取向硅钢的方法
本发明公开了一种酸洗低牌号无取向硅钢的方法,从酸洗线前拉矫机的延伸率设定、酸液浓度、酸液温度、酸洗槽内液位的控制、酸液中铁离子的含量等方面入手,解决酸洗低牌号无取向硅钢的问题。
高温退火气氛对硅钢表面硅酸镁底层形貌的影响
对取向硅钢在不同气氛下的高温退火工艺进行实验室模拟,利用X射线衍射仪(XRD)分析了硅钢退火至900℃和1170℃时的样品表面氧化层和底层的物相组成,采用场发射扫描电镜(SEM)观察了样品表面氧化层和底层在截面方向上的微观形貌特征,并计算了高温退火一次升温阶段氧化反应的吉布斯自由能以及900℃时退火气氛的氧分压。结果表明:当退火气氛的露点温度保持一定时,较高的氢气含量有利于生成完整连续的底层;当退火气氛的水氢分压比保持一定时,在露点温度与氢气含量两者较低的条件下,底层附着性不佳易脱落,较高条件下,底层中夹杂着较多的铁单质;当氧化层中无FeO时,底层完整连续但易脱落,当FeO层较薄时,底层下方存在部分未反应的SiO2,当FeO层较厚时,底层不完整连续且有分层。 The high temperature annealing process of grain-oriented silicon steel in different atmospheres was simulated in the laboratory. X-ray diffractometer(XRD) was used to analyze the phase compositions of the surface oxide layer and forsterite film of the silicon steel annealed to 900 ℃ and 1170 ℃. Field-emission scanning electron microscopy(SEM) was used to observe the micro morphology characteristics of the surface oxide layer and forsterite film of the samples in the cross section direction. The ...
无取向硅钢铬酸镁绝缘涂层结构与耐蚀性能研究
采用扫描电镜、原子力显微镜研究了铬酸镁半无机绝缘涂层的微观结构。结果表明,涂层厚度为数微米,涂层中的有机树脂乳液颗粒均匀分布在无机涂层的表面,从而保证了涂层具有良好的冲片性能。采用极化曲线研究了涂层的耐蚀性能,发现铬酸镁与铬酸锌绝缘涂层的耐蚀性能相当。 In this paper,the microstructure and anti-corrosion property of magnesium chromate coating on non-oriented silicon steel were studied.The microstructure was observed by SEM and AFM.The anti-corrosion properties were evaluated by polarization curves.The results show that the thickness of coating is several microns and the polymer particles were scattered on the surface of inorganic coating,which is the guarantee for lamination property.The corrosion resistance of the magnesium chromate film was e...
CN202023147451.8一种带缓冲保护装置的硅钢片纵剪线
本实用新型公开了一种带缓冲保护装置的硅钢片纵剪线,包括工作台,工作台的顶部外壁设置有放料辊,工作台靠近放料辊的一侧设置有牵引辊,工作台靠近牵引辊的一侧设置有整平机构,工作台的内部设置有第一缓冲坑,第一缓冲坑的顶部设置有导料辊,第一缓冲坑的内部设置有第三转轴,第三转轴的外壁传动连接有皮带,皮带的内壁传动连接有第二转轴,皮带的外壁传动连接有第一转轴,第三转轴的外壁固定安装有转筒,转筒的外壁设置有伸缩杆,伸缩杆的外壁套接有弹簧,伸缩杆的底部设置有滚珠,通过设置的第一缓冲坑与第二缓冲坑结构,可防止硅钢片在进入第一缓冲坑与第二缓冲坑时弯曲程度过大导致的断裂,且双重的缓冲装置更有利于对硅钢片的保护。
CN202111127223.0高磁感取向硅钢高效脱碳退火工艺
本发明公开了一种高磁感取向硅钢高效脱碳退火工艺,主要工艺流程为:炼钢连铸→热轧→酸洗常化→冷轧→脱碳和初次再结晶退火→渗氮处理(低温Hi‑B)→涂覆氧化镁隔离剂→高温退火→拉伸平整退火→涂覆绝缘涂层→精整,低温HiB不同于高温Hi‑B的工艺流程主要是在脱碳退火后增加了渗氮段。本发明在保证产品实物质量不低于现有水平(国内领先水平)的前提下,使Hi‑B钢退火效率达到世界领先,制造成本大幅降低。
硅钢高温退火环形炉炉壳制作与安装技术
硅钢高温退火环形炉炉壳制作与安装精度要求较高,施工时通过对壳体原材料矫正、炉壳板拼焊、下料切割、型钢骨架组装及焊接、骨架及炉壳板矫正、骨架与炉壳板组装及焊接、炉壳矫正、零配件装置、定位钻孔、报验检查、出厂、内侧板安装、外侧板安装、顶板安装等环节的工艺技术控制,能保质高效地完成硅钢高温退火环形炉炉壳制作与安装,为以后同类工程的施工提供可借鉴经验。 The required precision of manufacture and installation technique of the silicon steel high temperature annealing annular-furnace shell is high.During construction , manufacture and installation of the silicon steel high temperature annealing annular-furnace shell could be finished high efficiently through correcting the raw materials of shell , furnace shell plate welding , material cutting , steel frame assembly and welding , skeleton and shell plate correction , skeleton and furnace shell asse...
CN202011487359.8一种改善取向硅钢边部变形的热处理辅助方法
本发明公开了一种改善取向硅钢边部变形的热处理辅助方法,在高温退火工序前,在钢卷的下端预设位置处放置阻热环并固定;在高温退火完成后,拆除固定件并移除所述阻热环。本发明通过施加阻热环,降低了取向硅钢卷在高温退火过程中的升温速率,降低了钢卷在升温及冷却过程中的胀缩量,有效改善了边部变形情况。同时,本发明由于采用一体式隔热材料,其装配及移除难度大幅度降低,有利于推广应用。
CN202120928437.7一种用于硅钢件的高效激光焊接机
本实用新型公开了一种用于硅钢件的高效激光焊接机,涉及激光焊接机技术领域。本实用新型包括机体、底座和控制柜,底座上表面固定安装有工作平台,机体上表面设置有转动盘,转动盘上表面设置有焊接臂,焊接臂一端设置有连接头,连接头下表面设置有焊接头,焊接头、连接头和焊接臂均与机体电性连接,焊接臂一端设置有转动轴,转动轴一端固定连接有过渡仓,过渡仓一端设置有抽风机,过渡仓另一端设置有出风口,出风口通过过渡仓与抽风机相连通。本实用新型通过在焊接臂一端设置抽风机对着工作平台,将焊接产生的浓烟进行吸收并通过出风口排出避免对人体健康产生影响,通过设置具有防火花和强光功能的防护罩对工作人员的眼睛提供保护作用。
高强度无取向电工钢的研究进展
针对宝钢集团、日本新日铁住金和JFE公司公开的相关专利等资料,总结了国内外高强度无取向电工钢的研究进展,分析了不同电工钢的化学成分、生产工艺及产品性能,指出固溶强化、细晶强化、析出强化、位错强化都有可能被用来提高无取向电工钢的强度,并阐述了四种强化方式的优缺点;指出在高强度无取向电工钢的研发过程中,需根据其具体用途确定目标性能,再采用合适的强化手段,最终实现力学性能、磁性能和生产性能之间的平衡。 The research progress of high strength non-oriented electrical steels at home and abroad is summarized according to related patents brought into the public by Baosteel,Nippon Steel & Sumitomo Metal corporation and JFE corporation.The characteristics of chemical composition,production technology and properties of products in the patents are analyzed.Each of solution strengthening method,fine-grain strengthening method, precipitation strengthening method or dislocations strengthening method ma...