钢厂
电工钢显微结构和疲劳性能的研究
研究了电工钢SXRC的显微结构和疲劳性能,并与DP钢进行了比较。结果表明,退火温度低温化能够有效的抑制电工钢的再结晶。该钢在固溶铌的作用下,能够在保证电机磁性的同时具有一定的强度。与DP钢相比,SXRC钢的抗疲劳性能更好。 The microstructures and fatigue properties of the electrical steel SXRC we re investigated, and the properties were also compared with the steel DP. The results show that the recrystallization of the electrical steel can be suppressed at lower annealing temperature. The steel presents favorable motor magnetic and also a compatible strength with the help of solid-solution Nb. Compared with the steel DP, the fatigue resistance of the steel SXRC is preferable.
冷轧压下量对取向硅钢极薄带显微组织的影响
观察了取向硅钢极薄带经冷轧至不同厚度,并经过不同工艺热处理后的显微组织及亚结构。结果表明:冷轧压下量越大,显微组织中位错密度越高,冷变形组织越多,等轴晶粒越少;增加冷轧压下量可以使试样的再结晶温度降低,当钢带厚度为0.08 mm时,在650℃退火时就能发生明显的再结晶。 Microstructure and substructure of the grain oriented ultra-thin silicon steel sheets is analyzed,which are rolled down to different thickness and treated with different heat treatment process.The result shows that there are higher dislocation density,more cold deformation structure and less equiaxed crystal grain in microstructure of the steel sheets with more cold rolled reduction.Increase of cold rolled reduction will decrease recrystallization temperature,and when thickness of the steel shee...
纳米TiO_2轧制液对硅钢冷轧性能的影响
分别采用传统冷轧轧制液和纳米TiO2的冷轧轧制液,对无取向硅钢板进行了四辊冷轧实验.重点研究两种冷轧轧制液的轧制润滑性能和对轧后硅钢薄带表面质量和耐蚀性能的影响.通过场发射电子显微镜和能谱仪对使用两种轧制液轧后得到的硅钢薄带表面形貌和成分进行了分析.给出了轧制液中TiO2纳米粒子在轧制过程中的抗磨减摩机理.在轧制载荷较高时,纳米TiO2轧制液具有优良的轧制润滑性能并能显著改善轧后硅钢薄带的表面质量.同时在高载荷作用下,TiO2纳米粒子被压入硅钢薄带基体,形成一个滑动系来支撑载荷,从而使润滑膜的耐磨性提高. Non-oriented silicon steel strips were rolled on a four-high cold rolling mill lubricated by a traditional cold rolling liquid and a nano-TiO2 cold rolling liquid,with emphasis on studying the rolling lubrication performance of both the liquids and their effect on the surface quality and corrosion resisting property of the silicon steel strips.The surface micrograph and composition of the silicon steel strips after being rolled with both the liquids were characterized by field emissio...
CN202111385527.7硅钢片叠压设备
本发明涉及一种硅钢片叠压设备,包括加压机构,加压机构包括压台和压板,压台四角均设置导向柱,导向柱下端与压台固定连接,上端垂直向上延伸且穿透压板四角,压板上方设置有加力机构,加力机构包括固定板、活动板和挤压弹簧,固定板、活动板和压板平行设置,固定板设置与最上方且与导向柱上端固定连接,活动板设置于固定板和压板之间,固定板上穿透有多个螺杆,螺杆下端抵靠活动板顶面;活动板与压板之间均匀分布有多个挤压弹簧。本技术方案压台和压板构成了用于挤压叠放的硅钢片,通过转动螺杆可以将活动板向下推动,进而使活动板通过挤压弹簧将压板向下推动对叠放的硅钢片进行施压,装置结构简单、操作简单方便。
钇元素对6.5%Si无取向硅钢组织、高温拉伸及断裂机制的影响
通过微观组织表征、高温拉伸和断口形貌分析,研究了钇(Y)元素对6.5%Si无取向硅钢组织、高温拉伸及断裂机制的影响。研究结果表明,添加Y元素可以在钢液中形成YS和YP的复合析出。YS和YP可以充当异质形核基底,提高形核率,细化凝固组织。热轧组织不均匀,由表层至芯部分别形成等轴晶、等轴晶/拉长晶和拉长晶的混合组织。退火后,热轧变形组织转变为等轴晶,含Y实验钢的退火组织得到明显细化。500℃时效处理后,含Y实验钢具备较低的有序度,300℃的拉伸断口呈现韧性断裂特征,断后伸长率达到20.2%。相反,无Y实验钢发生脆性断裂,断后伸长率仅为2.1%。研究结果证实,Y元素可以通过组织细化和降低有序度提高6.5%Si无取向硅钢的中温塑性。 The effects of yttrium(Y)on microstructure,elevated-temperature tensile properties and fracture mechanism of 6.5% Si non-oriented electrical steel were investigated by means of microstructure characterization,high-temperature tensile test and fracture analysis.The results showed that the doping of Y introduced composite Y-rich precipitates(YS/YP)in the melt.YS and YP precipitates were qualified for heterogeneous nucleation agents,which thus raised the nucleation rate and refined the solidificati...
热轧组织对无取向硅钢织构的影响
采用X射线衍射仪分析无取向硅钢冷轧织构和再结晶退火织构的演化,研究了热轧组织对无取向硅钢织构以及磁性能的影响。结果表明,具有均匀、粗大晶粒组织的热轧板,冷轧形成更多的剪切带,导致成品板形成高的高斯织构组分,并提高了{100}织构强度,降低了γ纤维织构,最终导致成品磁感应强度升高,铁损下降。 The texture evolution of non-oriented silicon steel during cold-rolling and recrystallization annealing was investigated by X-ray diffractometer.The effects of hot band microstructure on the texture and magnetic properties of non-oriented silicon steel were analyzed.The results show that more shear bands appear during cold rolling due to homogeneous coarse grain in hot band.So strong{110}<001> texture after recrystallization annealing forms.At the same time,the {100} texture components inc...
CN202121979677.6一种摩托车点火器线圈用硅钢片
本实用新型涉及一种摩托车点火器线圈用硅钢片,包括E型件和I型件,所述E型件和I型件可组合成日字形;所述E型件包括竖边和设置在竖边三个横边,所述竖边与三个横边接触的位置设置孔眼;所述孔眼内径从为变径结构;位于E型件正面设置散热线槽,所述散热线槽一端与孔眼贯通,另一端指向凸部;位于E型件背面在散热线槽正对位置设置外凸线,所述I型件一侧设置与凸部匹配的凹部,在所述凹部之间凸台;所述凸台与凹台重叠;在凸台与凹部之间设置凸棱,所述凸棱位于I型件外侧。本实用新型设计新颖,改进巧妙,由于E型件具有弧形边可以有利于拾取,方便工作操作,同时采用采用接触的方式接触,增加了组合体的稳定性。
CN202023005869.5一种取向硅钢二轧料氧化镁冷涂装置
本实用新型公开了一种取向硅钢二轧料氧化镁冷涂装置,包括主体,所述主体的中部安装有架体,且架体的右侧安装有冷涂机构,所述冷涂机构的右端一侧安装有液压气缸,且液压气缸的内壁连接有连接杆,所述架体的前后两端安装有调节架机构,所述调节架机构的表面安装有防护块,且防护块的内壁安装有橡皮套。该取向硅钢二轧料氧化镁冷涂装置设置有冷涂机构,且箱体通过安装有单独喷管和连接喷头,便于使用者两者兼合使用,可使用单独喷管也可连接喷头,使用者可根据自己使用的需求,对单独喷管和连接喷头进行针对性使用,单独喷管通过安装扣将连接喷头进行拼接使用,箱体通过旋转轴与支撑架的旋转,便于将箱体进行角度旋转。
中低牌号无取向硅钢冷轧工艺优化生产实践
无取向硅钢特别是中牌号以上的无取向硅钢,随着含硅量的提高,常温下塑性较差,冷轧过程中轧制力明显提高,如果存在原料质量问题,极易发生断带事故,影响硅钢冷轧过程的成材率和生产效率。通过优化冷轧工艺参数,可提高冷轧稳定性。生产中通过合理分配冷轧各道次压下量和轧制速度,保证了轧制过程的稳定,很大程度减少了冷轧断带事故的发生。 Non-oriented silicon steel, especially in the low and middle grade, with the increase of silicon content, plasticity is poor at room temperature, rolling force in cold rolling process significantly improved .If there is the quality defect of raw materials , easily sheet is rolling off. Affect finished product rate and production efficiency in process of cold-rolled silicon steel. Through optimization of cold rolled process parameter , improve the stability of cold-rolling process. Through reason...
CN202011557728.6一种硅钢生产线退火炉前的换热装置
一种硅钢生产线退火炉前的换热装置,包含有抽风机(1)、立柱(2)、热交换器(3)、软管(4)和热风机(5);其特征在于:所述的热交换器(3)由若干组U形不锈钢管连接而成,一端固定在轴套(8)上,另一端通过链条(10)连接在立柱(2)顶端的链条盘(9)上,当链条盘(9)转动时,链条(10)拉动热交换器(3)绕着横轴(7)抬起或放下。本发明通过抽风机(1)将清洁空气抽到热交换器(3)内进行加热,然后再通过软管(4)将热空气输送到热风机(5)内来加热硅钢板(14),有效的利用了热能,避免了凝露导致的板面发蓝现象。
CN202121672222.X一种包容产品转子硅钢片叠加公差的模具机构
本实用新型公开了一种包容产品转子硅钢片叠加公差的模具机构,包括上下设置的定模固定板和动模固定板,定模固定板下面设置有定模仁,定模仁内穿设有定模型芯,定模型芯的上端设置有定模型芯限位块,定模型芯限位块套设在导向销下端,导向销上套设有定模型芯浮动弹簧B,定模型芯底部设置有台阶面,定模型芯上套设有定模型芯浮动弹簧A,定模仁外圈设置有定模浮动型芯,定模浮动型芯与动模固定板之间设置有动模浮动板,动模固定板中心设置有动模仁,动模仁上套设有产品转子,产品转子上端与定模型芯下端接触。本实用新型提供的一种包容产品转子硅钢片叠加公差的模具机构,能够省去高度调整工序,降低成本和品质管控风险。
CN202123075500.6一种硅钢前处理高液回流装置
本实用新型属于硅钢技术领域,具体的说是一种硅钢前处理高液回流装置,包括机体;所述机体的侧端固接有一号导管;所述一号导管上安装有二号导管;所述机体的顶端固接有连接管;所述连接管上安装有入泡管;所述二号导管的内侧壁固接有电机;所述电机的输出端固接有扇叶;所述二号导管的顶端内侧壁固接有定位板;所述定位板的侧端转动连接有旋转叶轮;所述二号导管的底端固接有排泡管;通过一号导管和二号导管的配合可以把溢出的泡沫进行导向,通过扇叶和旋转叶轮的配合可以使泡沫快速流动,再通过排泡管排出进入机体的内部,可以使泡沫循环使用,避免泡沫的溢流造成环境的污染及碱液的浪费。