结合工业化生产的无取向硅钢,探讨了氧硫交互作用对钢中夹杂物生成的影响。借助非水溶液电解+扫描电镜法,研究了不同O、S含量下钢中夹杂物的变化规律。结果表明,本实验条件下,提高O含量、降低S含量,会劣化热轧组织再结晶效果。在劣化效果上,O的作用大于S;低Si、无Al硅钢中,应尽可能降低O含量、适当提高S含量,以粗化钢中微细夹杂物,减少尺寸小于1.0μm的夹杂物的数量;O、S含量与钢中夹杂物数量不具有关联性。生产过程中,不仅要严格控制O、S含量,还要严格控制生产工艺,以免生成较多的有害夹杂物。 Based on the industrial production of non-oriented silicon steel,the effects of interaction between oxygen and sulfur on the formation of inclusions were discussed.The change of non-metallic inclusions in steel sheets was investigated by means of electrolysis with non-aqueous solution under different oxygen and sulfur content.Results show that the recrystallization microstructure of hot rolled sheets will be deteriorated with the increase of oxygen content and the decrease of sulfur content.The ... 
2012-04-28 134 5.8

选用Q235和Q345钢,在纯锌浴和含钛量分别为0.05%、0.10%、0.15%、0.20%(质量分数)的合金浴中浸镀0.5、1、3、5、8 min。利用扫描电子显微镜和能谱仪研究了钛对热浸镀锌组织和生长动力学的影响,并提出钛对含硅钢铁锌反应抑制作用的机理。结果表明:钛的加入缩短了Γ的孕育期,促进了合金层中δ的生长和ζ的消失,δ的生长依然受扩散控制,呈抛物线生长规律;Zn-0.05%Ti锌浴可以很好的抑制高硅钢的硅反应性;含硅钢热浸镀锌钛合金浴时,在锌浴中会形成锌铁钛三元T相,该相能吸收ζ晶界处富集的硅,从而抑制了铁锌反应。 Both Q235 and Q345 steels were immersed for 0.5 to 8 min in Zn bath with different amount of Ti,ranging from 0 to 0.20 mass%,for galvanization.The effect of Ti in Zn bath on microstructure and growth kinetics of hot-dip galvanizing coatings on the two steels were investigated by means of SEM and EDS analysis.Base on the experiment,the mechanism of Ti additions in controlling Fe-Zn reaction was proposed.The results show that addition of Ti in the zinc bath decreases the incubation time of Γ phase... 
2013-09-28 135 5.8

本实用新型涉及一种堆叠定子硅钢片复位装置,主要包括气动按压装置与弹簧悬架,弹簧悬架中设有的硅钢片放置板,硅钢片放置板中心部位嵌入式连接有滑动杆,滑动杆的一侧设有固定顶针,且滑动杆的顶部还设有弧形倒角,滑动杆一端套接有硅钢片,另一端与固定板连接;固定板两侧上套接有轴套,轴套内滑动设置有定位滑轴,定位滑轴的外部套接有螺旋弹簧组成弹簧减震器,且螺旋弹簧设置在轴套上底面与硅钢片放置板下底面之间;这种结构的设置通过硅钢片放置板上设置的固定顶针,使得硅钢片与硅钢片放置板之间的连接更加稳定,同时通过弹簧减震器的设置可以降低机器手下压的压力,从而增强硅钢片的承受力。
2021-09-30 122 6.8

本实用新型提供了一种带有可回收再利用功能的冷轧硅钢卷捆扎装置,底座上设有安装块一,加紧装置一安装在安装块一上,加紧装置一包括外壳,外壳内设有凹槽一,凹槽一内设有通口,凹槽一内设有气缸,气缸一端设有夹块,气缸一侧设有挡板,挡板安装在凹槽一上,外壳上设有凸块,硅钢卷进行捆扎,可以重复利用,加紧装置一与加紧装置二可以把硅钢卷两端进行固定吗,里面安装的气缸可以加紧硅钢卷,安装的吸盘可把加紧装置二的位置提高,方便进行固定上端,安装的承重块可以起到防止倾斜的作用,在不使用的时候加紧装置一与加紧装置二之间可以通过卡扣之间的连接进行固定。
2021-09-09 128 6.8

借助电子背散射(EBSD)技术对AlN为主抑制剂的Hi-B取向硅钢常化工艺的中间冷却制度进行了研究。结果表明:常化后试样均发生了完全再结晶,在60℃/s冷速下组织最均匀;在合适的冷却制度下常化板表层保留了强的Goss织构,它深入到1/4厚度处,并且形成对Goss织构有利的强{554}<225>织构。 The intermediate cooling system of Hi-B oriented silicon steel with AlN main inhibitor in normalizing process was studied by means of electron back diffraction(EBSD) technique. The results show that:the specimens after normalizing are fully recrystallization, and the microstructure is most uniform under the intermediate cooling rate of 60℃/s; under suitable cooling system, normalized plate surface retains strong Goss texture, it penetrates into the 1/4 thickness of the plate and forming strong {... 
2014-11-28 134 5.8

介绍了微合金元素锡、铌、稀土对无取向硅钢性能的影响,并扼要分析了这些元素对硅钢性能的影响机理:晶界偏聚元素Sn可细化晶粒提高硅钢磁性能;微合金元素Nb细化铁素体晶粒,提高硅钢的强度、韧性和塑性及磁性能;稀土元素(RE)在硅钢中的主要作用包括净化钢液、变质夹杂物、改善铸态组织和性能及微合金化,减少晶界上出现偏析的几率。 The influence of micro-alloy elements on properties of non-oriented silicon steel and the mechanism for effect of the micro-alloy elements including Sn、Nb and RE on the properties of steel are presented and analyzed in this paper.Grain boundary segregation elements Sn in steel can grain refinement and improve the magnetic properties;Micro-alloy elements Nb can refine the ferrite grain,increase the silicon steel strength,toughness and plastic;The main role of the RE in the silicon steel including... 
2013-03-28 140 5.8

本发明公开了非晶与硅钢卷绕机用恒张力一体式纠偏机构,包括放卷结构和收卷结构,所述放卷结构和收卷结构间依次连接张力装置和纠偏装置,所述纠偏装置下方设置有纠偏张力控制系统;所述纠偏张力控制系统包括放卷张力程序模块、速度张力闭环反馈程序模块和纠偏定位程序模块;所述放卷张力程序模块与张力装置电信号连接;所述速度张力闭环反馈程序模块与放卷结构和收卷结构电信号连接;所述纠偏定位程序模块与纠偏装置电信号连接。通过集纠偏控制与张力控制于一体,并设置了纠偏张力控制系统,提高了卷绕精度,降低了设备制造成本,并有效解决了设备占用空间较大的问题。
2021-12-14 165 6.8

本实用新型涉及一种硅钢冲压片质量筛查分拣装置,包括:第一组传送带机构,第一摄像头,设置于第一组传送带机构的上方,用于对硅钢冲压片的第一表面的残损进行检测;第一机械手机构,设置于第一组传送带机构的上方且位于所述第一摄像头的后方;翻转装置,设置第一组传送带机构的后方,用于对第一组传送带机构传输的初检良品进行翻面并将翻面后的初检良品传输给第二组传送带机构;第二组传送带机构,设置于翻转装置的后方;第二摄像头,设置于第二组传送带机构的上方,用于对硅钢冲压片的第二表面的残损进行检测;第二机械手机构,设置于第二组传送带机构的上方且位于第二摄像头的后方。本实用新型可高效的检测每一个产品的外观质量。
2021-08-16 111 6.8

【作者】 姚昌国; ...
2011-05-28 130 5.8

本实用新型公开了一种电工钢自粘涂层液生产用搅拌釜,包括釜体,釜体的内部通过两个第一隔板分隔成第一安装腔、第二安装腔和搅拌腔,釜体的内部设有传动组件,传动组件包括伺服电机、主动轴和两个从动轴,伺服电机固定安装在釜体顶端的中部,伺服电机的输出轴与主动轴的顶端固定连接,本实用新型的有益效果是:通过设有八个与十二个搅拌叶片相交错的挡板,避免搅拌轴在搅拌过程中产生离心力造成漩涡,使自粘内外侧的涂层液得到充分搅拌,通过设有循环泵机、第二隔板和流通槽使搅拌釜内的自粘涂层液处于流通的状态,使底部不易被搅拌的涂层液能够得到充分搅拌,在提高搅拌釜的灵活性的同时,保留其原有的稳定性。
2020-12-25 147 6.8

研究了CSP工艺生产≤0.005%C-1.1%Si的2.2mm无取向电工钢热轧板在800~1000℃常化对0.5mm冷轧板840℃退火后组织和磁性能的影响。结果表明,热轧板常化温度升高,冷轧板退火后的再结晶晶粒增大,铁损降低,磁感增加;热轧板常化温度超过900℃,因第二相固溶而后弥散析出,退火后冷轧晶粒细化,铁损增加,因此该无取向电工钢热轧板最佳常化温度为900℃。 The effect of normalizing at 800-1000℃ of CSP produced plate(≤0.005%C-1.1%Si) on the microstructure and magnetic properties of downstream cold-rolled non-oriented electrical steel annealed at 840℃ was studied.Results show that with increasing normalizing temperature of hot-rolled material the recrystallized grain size of annealed sheet increases,iron loss reduced and magnetic induction increases.As normalizing temperature excesses 900℃,grain is refined and iron loss increases after annealing due... 
2012-03-28 125 5.8

该电磁钢板用涂布组合物含有环氧树脂、酚类固化剂(A)、以及从芳香族胺和双氰胺中选择的一种以上的胺类固化剂(B),所述酚类固化剂(A)的含量相对于所述环氧树脂100质量份为1~40质量份,所述胺类固化剂(B)的含量相对于所述环氧树脂100质量份为0.5~5质量份。