  • 未分类

分析了高转矩和高转速条件下高效驱动马达铁芯材料对无取向硅钢磁性能要求,讨论了无取向硅钢的高磁通密度和低铁损对电机转矩和效率的影响,介绍了国内外高磁感无取向硅钢发展情况。在生产工艺上,提高钢质纯净度,弱化夹杂物和第二相粒子对畴壁移动和再结晶晶粒长大的钉扎作用,添加微量晶界和带钢表面的偏析元素促使有利织构发展等技术可提高无取向硅钢的磁通密度。 The requirements of high efficient drive motor core materials under the conditions of high torque and high speed were analyzed.The effects of high magnetic flux density of non-oriented silicon steel on the torque and efficiency of the motor were discussed.The development of non-oriented silicon steel with high magnetic was introduced.The magnetic flux density of non-oriented silicon steel sheet can be obviously improved by some production technologies,such as purification steel,weakening the pin... 
2023-05-11 1.32k 5.8

阐述了国内外高磁感取向硅钢的生产研究水平与发展趋势,包括通过提高高斯晶粒取向度、细化磁畴、涂覆张力涂层、减薄钢片厚度进一步降低铁损以及低温加热技术和短流程技术新工艺。分析高磁感取向硅钢在我国大型电力变压器上的应用情况,结果表明,发展更薄规格高磁感、低铁损、低磁致伸缩取向硅钢可为大型变压器的安全性、节能性及环保性提供有效保障。 The research progress and development trend of high magnetic induction grain-oriented silicon steel at home and abroad are summarized,including the technology of improving the Goss alignment,refining domain wall,adding stress coating,decreasing thickness of sheet,and the new technique of reducing heating temperature of casting slab and shortening operational.Moreover,the application of high magnetic induction grain-oriented silicon in power transformer is presented.Developing grain-oriented sili... 
2014-11-28 165 5.8

本发明公开了一种低磁致伸缩取向硅钢的制造方法,其包括步骤:(1)在硅钢基板上进行单面激光刻痕,其中进行激光刻痕的表面为第一表面,第一表面的背向一侧表面为第二表面;(2)基于激光刻痕的功率确定第一表面和第二表面的挠度差;(3)基于挠度差获得第一表面和第二表面所涂覆的绝缘涂层的涂覆量差;(4)基于涂覆量差,在第一表面和第二表面上涂覆绝缘涂层,其中第二表面的绝缘涂层涂覆量大于第一表面的绝缘涂层涂覆量。相应地,本发明还公开了采用上述制造方法所制得的低磁致伸缩取向硅钢,其第一表面和第二表面的磁致伸缩偏差≤2db(A),并且所述低磁致伸缩取向硅钢的平均磁致伸缩≤55db(A)。
2021-01-11 127 6.8

运用电子背散射衍射(EBSD)和X射线衍射(XRD)技术对硅钢热轧板的织构在板厚方向的分布进行了研究,并分析了两种织构测量方法的特点。EBSD技术能直观给出板厚方向的微观织构,XRD能得到钢板的宏观统计织构信息,结合两种技术的分析,能更直观更精确的研究不同织构在板厚方向的分布。 The texture distribution along the thickness of the silicon steel has been investigated by electron backscatter diffraction(EBSD) and X-ray diffraction(XRD) technique.The characteristics of two technique of texture analysis have been investigated.Combined the two techniques,the texture distribution along the thickness of the silicon steel could be realized distinctly and accurately. 
2011-02-28 134 5.8

采用经验设计法初步确定了取向硅钢铸坯感应加热线圈设计参数,应用Ansoft仿真软件分别对36组不同线圈高度、线圈内径的感应加热炉在不同频率下的三维整体磁场和铸坯的温度场进行了数值仿真。通过对比仿真结果,确定电磁场分布最佳的一组感应加热炉设计参数为线圈高度h=1.50 m、线圈内径D1=0.575 m、电流频率f=110 Hz。在该参数下应用Ansoft仿真软件对取向硅钢铸坯感应加热炉的温度场进行了仿真,结果发现温度场分布均匀,可满足取向硅钢铸坯加热要求。 The induction heating coil design parameters for the oriented silicon steel casting blank were determined preliminary by experience design method,and 36 groups three-dimensional electromagnetic field with different height and inside diameter of coil under different frequencies of the induction heating furnace and the temperature field of the casting blank were investigated by numerical simulation using Ansoft simulation software. By comparing the simulation results of electromagnetic field distr... 
2014-01-28 117 5.8

冷轧无取向硅钢是高技术含量、高附加值产品,工艺复杂,生产周期长,过程控制难度大,被誉为钢铁产品中的\"工艺品\"。热轧生产工艺又是无取向硅钢生产的重中之重,直接决定了硅钢的铁损和电磁性等多项指标。 Cold rolled non-oriented silicon steel is high technology content 、high added value product. Its process is complex, its production cycle is of length, and its process control is difficult, which is known as the iron and steel products \" Arts and crafts\". Hot rolling production process is the top priority of non-oriented silicon steel, which directly determines iron loss of the silicon steel and electromagnetic property,as well as other many index. 
2014-02-28 158 5.8

研究了取向硅钢制备过程中常见的两种冷轧工艺,主要研究了一阶段冷轧与两阶段冷轧+中间退火工艺对初次再结晶组织及织构的影响.结果表明:采用两阶段冷轧+中间退火工艺制备以Cu2S为主抑制剂的取向硅钢,其初次再结晶平均晶粒尺寸为18.1μm,高斯晶粒的体积分数为0.6%,迁移性强的重位点阵晶界(Σ5+Σ9)和高能晶界(20°~45°取向偏差角)所占比例分别为1.8%和50.4%.与一阶段冷轧工艺相比,其初次再结晶晶粒较细,且高斯晶核与特征晶界所占的比例较高,有利于高斯晶粒发生二次再结晶. Two common cold-rolling processes of grain oriented silicon steel and the effects of the single stage cold rolling and tw o-stage cold rolling w ith intermediate annealing processes on the primary recrystallization microstructure and texture w ere investigated. The results revealed that for the grain oriented silicon steel prepared under the tw o-stage cold rolling process w ith intermediate annealing w ith Cu 2 S as the main inhibitor,the average grain size of the primary recrystallization micr... 
2014-02-28 156 5.8

本实用新型公开了高磁感冷轧无取向硅钢卷,包括硅钢卷本体,所述硅钢卷本体由硅钢板、电磁屏蔽层与耐磨层组成,且硅钢板的内部包括有第一夹层与抑制剂层,所述电磁屏蔽层电镀于硅钢板的表面,所述耐磨层电镀于电磁屏蔽层的表面,所述第一夹层的内部由硅元素与锰元素组成,所述抑制剂层的内部主要由磷元素与硫元素组成,所述电磁屏蔽层为铝箔材质制成,所述耐磨层为金属铬制成。本实用新型中抑制剂层的内部主要由磷元素与硫元素组成,同时锰与硫元素形成取向硅钢中重要的抑制剂MnS,保证硅钢板中再结晶组织的完整性,能提高取向硅钢的电阻,提高硅钢板的磁性能,使电阻率变大可有效降低铁损,保证硅钢板在热轧过程中组织性更加均匀,提高硅钢板的加工质量。
2021-05-20 125 6.8

介绍在取向硅钢生产中抑制剂的作用以及多元抑制剂的机理和应用情况,分析多元抑制剂方案中各种元素对高磁感取向硅钢性能的影响,并根据生产实践提出了进一步研究的方向. The role of an inhibitor in the production of grain oriented silicon steel,and the mechanism of multiplex inhibitor in the production are described in the present article.In addition,the influence of various elements in the multiplex inhibitor on the performance of grain oriented silicon steel with high magnetic induction is elucidated.Further work needed in this research is also indicated. 
2013-01-28 136 5.8

一种取向硅钢极薄冷轧板钢带的焊接系统及方法,于该系统内设有焊轮及与焊轮电连接的焊接控制器;所述焊轮由前后呈直线布设的主焊轮、副焊轮构成;所述焊接控制器由分别与主焊轮电连接的第一焊接控制器、与副焊轮电连接的第二焊接控制器构成。所述焊接基于单排焊,仅使用一次焊接行程,通过设置的第一次焊接与第二次碾压焊接依次作业完成。本发明的一种取向硅钢极薄冷轧板钢带的焊接系统及方法,针对取向硅钢极薄钢带冷轧板焊接的问题,对传统电阻焊焊机拥有的碾压轮改造及建立的相应焊接工艺。平衡了热量积累与质量保证两者,解决了取向硅钢极薄钢带冷轧板焊接容易发生虚焊、爆焊和焊接时间长等问题。同时和传统电阻焊焊机相比焊接工艺窗口更大,焊接效率更高。
2021-09-27 126 6.8

一种无取向硅钢用轧制工作辊,属于轧机工作辊技术领域,该轧制工作辊,包括锥形曲面段和平直段,锥形曲面段包括弧形段Ⅰ和弧形段Ⅱ,弧形段Ⅰ的弧面内凹,弧形段Ⅱ的弧面外凸,弧形段Ⅱ和平直段与带钢接触,弧形段Ⅰ的一端水平向外延伸,弧形段Ⅰ的另一端与弧形段Ⅱ的一端相切,弧形段Ⅱ的另一端与平直段相切,本实用新型的有益效果是,该工作辊整体结构简单,轧制效率高,降低了辊耗,消除了工作辊边部的急剧弹性压扁、弹性变形,降低了轧制断带的风险,可有效控制钢带边部的边降和形状。
2021-05-07 120 6.8

本实用新型公开了一种适用于自动线的硅钢叠装系数性能检测装置,涉及实验仪器自动化技术领域,为解决机器人自动上样至叠装系数测量仪经常发生碰撞的问题;本实用新型包括框架、上压板、下压板、压紧驱动机构、高度探规和加载力值传感器,其中压紧驱动机构设置于框架上端,下压板固定于框架内的下端,上压板安装于下压板上方且与压紧驱动机构的输出端传动连接,加载力值传感器安装于上压板与压紧驱动机构的输出端之间,高度探规安装在上压板上,且探头向下伸出上压板下端面,框架为“C”字形一体式刚性结构,其设有上下两个水平板,以及位于一侧的竖直板;本实用新型能够避免机器人自动上样时碰撞到框架,以及下压时高度探规压到试样。