采用ZMLMC超高梯度定向凝固装置,研究了5种凝固速率(10、35、80、150和450μm/s)对定向凝固50W600无取向硅钢的固液界面稳定性转变规律和一次、二次枝晶间距的影响。研究结果表明,在特定的温度梯度下,随着凝固速率的增加,定向凝固的固液界面由胞状晶转变为胞状枝晶,再转变为细小的树枝晶。随着凝固速率的增加,定向凝固组织的枝晶形貌逐渐细化,一次和二次枝晶间距逐渐减小,且与冷却速率之间都符合指数关系:λ1=151.73×(G L·R)-0.31,λ2=22.07×(G L·R)-0.44。当冷却速率达到4.275℃/s时,一次、二次枝晶间距分别为112μm、14.1μm。 Under the conditions of certain temperature gradient and different solidification rate,the directional solidification experiment of non-oriented electrical steel 50W600 was carried out.The microstructure of 50W600 steel was also analyzed in different solidification rate.The result shows that the solid/liquid interface of the steel undergoes an evolution from cellular,cellular dendrite and finally to fine dendrite morphologies.The dendrite refines gradually and the distance between dendrites decr... 
2013-11-28 138 5.8

本发明涉及一种提高低温高磁感取向硅钢附着性的方法,该方法在现有低温高磁感取向硅钢连续式脱碳退火炉中,通过在脱碳退火前区通入氮气、氢气干式混合气,在脱碳退火后区通入氮气、氢气湿式混合气进行脱碳,在渗氮区通入氮气、氢气湿式混合气及氨气进行渗氮,解决了低温高磁感取向硅钢附着性不好的难题。本发明方法提高了钢中总氧量、增加了氧化层厚度、改善了氧化层结构,经高温退火后生成了致密的硅酸镁底层,附着性大幅提高,测试结果均在C级以上,大部分样品在B级以上。
2021-09-30 177 6.8

本实用新型公开了一种用于电机生产的硅钢片放料机构,包括用于传输硅钢片的传送机构和用于堆叠的放料机构以及用于旋转位移的旋转机构,所述传送机构出料端设置有所述放料机构,所述放料机构安装在所述旋转机构上端,所述放料机构下侧设置有推动机构。本实用新型利用传送机构、放料机构配合,保证了硅钢片的传输效果和放料效果,从而保证了硅钢片在放料堆叠过程的稳定性和安全性,提高加工效率,利用放料机构、推动机构配合,在后期放料堆叠后能够快速进行捆扎和运输。
2021-09-29 154 6.8

本发明涉及低温取向硅钢片制造领域,具体为一种重质硅钢级氧化镁的生产工艺。为提升现有取向硅钢片的表面质量,将工业氧化镁、聚乙烯醇粘结剂和水在不锈钢反应罐中水热合成氢氧化镁,经压滤、煅烧、冷却、气流粉碎、包装产物为重质硅钢级氧化镁。产品具有生产工艺独特、成本较低,能明显提高取向硅钢片的表面质量和增加磁感应强度,降低铁损,提高取向硅钢片的正品率。可针对性在取向硅钢片生产厂家推广使用。
2021-10-22 152 6.8

本实用新型公开了一种铁芯硅钢片卷料的上料装置,包括升降机构、固定座、转动执行机构和转动平台,所述固定座固定设置在地面上,所述升降机构相邻设置在固定座的一侧,所述固定座对立于升降机构的一侧设置有转动平台,所述转动平台的一端铰接设置在固定座上,且所述转动平台的另一端为自由端,所述转动平台在竖向面内朝向或远离于升降机构偏转,所述固定座上设置有转动执行机构,所述转动执行机构驱动转动平台转动;所述转动平台上的物料通过转动可位移至固定座和升降机构上,能够安全的、快速的将卷料转移至升降机构上,从而便于上料。
2021-12-10 160 6.8

采用双辊连铸工艺制备了硅的质量分数分别为0.5%,1.0%,3.0%,4.5%的硅钢薄带,用光学显微镜观察其组织,并研究了后处理工艺对薄带组织和性能的影响。结果表明:硅含量为0.5%和1.0%的薄带适合采用一次冷轧+850~950℃退火的后处理工艺,而硅含量在3.0%以上的薄带适合采用二次冷轧+950℃退火的后处理工艺;硅含量为3.0%和4.5%的薄带在冷轧并950℃退火后,其磁性能最佳,铁芯损耗约为4.30 W·kg-1,磁感应强度约为1.68T。 Silicon steel thin strips with silicon content of 0.5wt%,1.0wt%,3.0wt%and 4.5wt%were prepared by twin-roll continuous casting process,and the microstructure of the strips were observed by means of optical microscopy,and on the basis,the effect of post-treatment process on microstructure and properties of the strips was studied.The results show that the post-treatment process of one-time cold rolling and annealing between 850—950℃was suitable for the strips with silicon content of 0.5wt%and 1.0wt... 
2011-08-28 145 5.8

选用Q235和Q345钢,在纯锌浴和含钛量分别为0.05%、0.10%、0.15%、0.20%(质量分数)的合金浴中浸镀0.5、1、3、5、8 min。利用扫描电子显微镜和能谱仪研究了钛对热浸镀锌组织和生长动力学的影响,并提出钛对含硅钢铁锌反应抑制作用的机理。结果表明:钛的加入缩短了Γ的孕育期,促进了合金层中δ的生长和ζ的消失,δ的生长依然受扩散控制,呈抛物线生长规律;Zn-0.05%Ti锌浴可以很好的抑制高硅钢的硅反应性;含硅钢热浸镀锌钛合金浴时,在锌浴中会形成锌铁钛三元T相,该相能吸收ζ晶界处富集的硅,从而抑制了铁锌反应。 Both Q235 and Q345 steels were immersed for 0.5 to 8 min in Zn bath with different amount of Ti,ranging from 0 to 0.20 mass%,for galvanization.The effect of Ti in Zn bath on microstructure and growth kinetics of hot-dip galvanizing coatings on the two steels were investigated by means of SEM and EDS analysis.Base on the experiment,the mechanism of Ti additions in controlling Fe-Zn reaction was proposed.The results show that addition of Ti in the zinc bath decreases the incubation time of Γ phase... 
2013-09-28 161 5.8

本实用新型涉及硅钢片铁芯性能测试技术领域,公开了CD型硅钢片铁芯性能测试工装,包括:机台,上部后侧固定有竖直向上的后侧板;托板,水平设置在所述机台上方;夹持机构,设置在所述机台上,所述夹持机构包括:第二气缸,其驱动杆端部固定套接有夹持块,夹持块外端部固定有橡胶缓冲块;橡胶垫,固定在所述托板右侧上部。本实用新型通过设置第一气缸驱动连接于托板,可以先根据硅钢片的厚度,通过操作气缸控制器控制第一气缸工作带动托板在机台上进行升降高度,从而调整托板与夹持块的高度差,提高装置的实用性和广泛性,较为实用,适合广泛推广和使用。
2021-05-14 142 6.8

根据本发明的一个实施例的无取向电工钢板,以重量%计,所述钢板包含Si:2.1至3.8%、Mn:0.001至0.6%、Al:0.001至0.6%、Bi:0.0005至0.003%和Ge:0.0003至0.001%,余量包含Fe和不可避免的杂质。
2020-12-17 223 6.8

本发明涉及变压器硅钢片冲裁加工技术领域,具体涉及一种变压器硅钢片制造成型加工机械及加工方法,包括垫板、冲裁装置和进料装置,所述的垫板上安装有冲裁装置,冲裁装置上安装有进料装置;本发明可以解决变压器硅钢片在冲裁成型时存在的以下难题:一、在通过冲裁设备对变压器硅钢片进行冲裁作业时,由于变压器硅钢片大多没有进行稳定的定位作业,使得变压器硅钢片冲裁时产生偏差,降低了变压器硅钢片的冲裁质量,若使用定位机构进行定位处理,还会额外增加操作时间,降低了加工效率;二、需要人工进行送料作业,由于人工送料的间距难以控制,导致变压器硅钢片的冲裁位置发生偏差,造成变压器硅钢片的浪费。
2021-09-02 148 6.8

本实用新型涉及变压器材料检测技术领域,具体为一种硅钢片检测装置,包括材料检测装置主体,材料检测装置主体包括相互连接的铁损测试仪主机及磁导计,磁导计的顶端设置有清洁机构,清洁机构包括固定盒、拉块及刷块,固定盒固接于磁导计上,拉块插设于固定盒中、能够在固定盒中上下移动,固定盒的内部底面上及拉块的底端上分别安装有刷块,铁损测试仪主机上还设有束线机构。本实用新型使得用户可在检测硅钢片前,对硅钢片两面沾染的灰尘污渍进行擦拭,避免灰尘污渍影响对硅钢片的测定结果,可方便地对刷块进行清洁更换,使得用户可方便地对电源线和导线进行收纳。
2021-08-16 137 6.8

本实用新型提供了一种带有可回收再利用功能的冷轧硅钢卷捆扎装置,底座上设有安装块一,加紧装置一安装在安装块一上,加紧装置一包括外壳,外壳内设有凹槽一,凹槽一内设有通口,凹槽一内设有气缸,气缸一端设有夹块,气缸一侧设有挡板,挡板安装在凹槽一上,外壳上设有凸块,硅钢卷进行捆扎,可以重复利用,加紧装置一与加紧装置二可以把硅钢卷两端进行固定吗,里面安装的气缸可以加紧硅钢卷,安装的吸盘可把加紧装置二的位置提高,方便进行固定上端,安装的承重块可以起到防止倾斜的作用,在不使用的时候加紧装置一与加紧装置二之间可以通过卡扣之间的连接进行固定。