钢厂
CN202120320747.0一种实验室模拟硅钢带连续常化退火炉
本实用新型公开了一种实验室模拟硅钢带连续常化退火炉,属于热处理技术领域。该退火炉包括:炉膛,沿退火炉本体的长度方向贯通,所述炉膛的两端的开口处设有炉门,炉门上设有透气孔,炉膛内自左向右依次分为多个加热区;滑轨,沿炉膛的长度方向设于所述炉膛的底部;移动机构,设在滑轨上且能沿滑轨移动;牵引绳,由耐高温材料制成,其一端与移动机构连接,另一端延伸至退火炉本体的外部;牵引绳收放机构,设于退火炉本体的外部,并与牵引绳的外端连接,用于收放牵引绳。本实用新型的退火炉采用三段加热区域,独立控温,能够模拟硅钢带预热、加热、均热、冷却等连续常化工艺,实验条件更接近工业生产。
新钢1580取向硅钢宽度窄尺原因分析
取向硅钢因其高磁导率、低矫顽力和大电阻系数等特性,被广泛应用于大中型变压器和大型电动机铁芯的制造。因取向硅钢性能和成分控制严格,生产工艺复杂,故其产品代表了钢铁企业特殊钢生产的最高水平。本文介绍了新钢公司卷板厂1580热连轧线生产取向硅钢过程中出现的窄尺问题,研究了取向硅钢产品的特点,分析了热轧过程中的组织转变,并结合生产实际提出了改进措施。通过对加热炉钢坯加热模式、粗轧轧制策略、精轧轧制工艺、二级模型等方面的优化和改进,取向硅钢窄尺情况明显好转,提高了产品的成材率和市场口碑。 The oriented silicon steel is widely used in the iron core manufacture of large and mediumsized transformers and large motors because of its high permeability, low coercivity and large resistance coefficient. Due to the performance and composition control of oriented silicon steel is strict, the production process is complex,therefore, its products represent the highest level of special steel production in iron and steel enterprises. This paper introduces the problem of narrow gauge in the produ...
CN202122627090.5一种变压器铁芯硅钢板的剪切装置
本实用新型涉及硅钢片切割设备领域,具体涉及一种变压器铁芯硅钢板的剪切装置,包括操作台,操作台的顶部安装有传送辊,传送辊的侧部安装有限位装置,限位装置的侧部依次安装有送料装置和切割装置,切割装置包括固定座,固定座的顶部固定连接有底板,底板的两侧固定连接有导向柱,导向柱的顶部安装有顶板,导向柱上且位于顶板的下方滑动设置有刀架,刀架上安装有切割刀,顶板上安装有液压缸,液压缸的自由端的端部与刀架的顶部固定连接;解决现有的硅钢片切割效率低的问题。
CN202111385527.7硅钢片叠压设备
本发明涉及一种硅钢片叠压设备,包括加压机构,加压机构包括压台和压板,压台四角均设置导向柱,导向柱下端与压台固定连接,上端垂直向上延伸且穿透压板四角,压板上方设置有加力机构,加力机构包括固定板、活动板和挤压弹簧,固定板、活动板和压板平行设置,固定板设置与最上方且与导向柱上端固定连接,活动板设置于固定板和压板之间,固定板上穿透有多个螺杆,螺杆下端抵靠活动板顶面;活动板与压板之间均匀分布有多个挤压弹簧。本技术方案压台和压板构成了用于挤压叠放的硅钢片,通过转动螺杆可以将活动板向下推动,进而使活动板通过挤压弹簧将压板向下推动对叠放的硅钢片进行施压,装置结构简单、操作简单方便。
CN202110291809.4一种提高无取向硅钢铁损均匀性的方法
本发明提供了一种提高无取向硅钢铁损均匀性的方法,所述方法包括,对无取向硅钢板坯进行加热和粗轧,获得中间坯;将所述中间坯精轧后以620‑750℃的温度进行卷取,获得热轧卷;将所述热轧卷进行酸洗和冷轧,获得冷轧卷;对所述冷轧卷升温至900‑960℃的温度保温50‑90s的时间,进行退火,获得铁损均匀性良好的无取向硅钢。本发明提供的方法,其铁损P1.0/50为1.379‑2.721W/kg,P1.5/50为2.751‑5.438W/kg,B5000为1.706‑1.741T,在线P1.0/50极差为0.062‑0.188W/kg,无取向硅钢的铁损更均匀。
CN202110009935.6一种甩带法制备高磁性能含磷硅钢薄带的方法
一种甩带法制备高磁性能含磷硅钢薄带的方法,属于合金材料领域。本发明以硅钢(Fe‑(3‑6.5)wt.%Si)块体为母合金,并添加一定量的硅铁合金及磷铁合金,放置于中频感应炉中,熔融后经快速凝固‑甩带、冷轧、热处理工艺,得到具有优异性能的含磷硅钢薄带。对于硅钢而言,P元素的少量加入能够有效的提升电阻率从而显著降低铁损,且具备优化软磁性能的作用。而采用甩带法能够充分利用其快速凝固的特征,从根本上避免了P元素在传统熔炼冷却过程中严重偏析的缺陷,极佳地保证了产品的组织优势与软磁性能。本发明具有操作简单、生产效率高、产品精度高、工艺流程短、无污染与夹杂、性能优异等优点。
CN202121007099.X一种电工钢生产高温处理用上料装置
本实用新型公开了一种电工钢生产高温处理用上料装置,包括工作台和底板,所述工作台的顶部外壁固定有对称分布的两个第一侧板,且第一侧板的相对侧外壁通过轴承转动连接有等距分布的第一转辊,两个所述第一侧板的顶端转动连接有对称分布的两个活动框,且活动框的一侧转动连接有等距分布的第二转辊,所述活动框的顶部外壁固定有安装杆,且安装杆的顶端转动连接有转块,所述转块的内部开有螺纹孔。本实用新型双向螺纹杆带动两个转块相向移动,使两个活动框转动,一端相互靠近,将第一转辊上的电工钢向中间推动,从而使电工钢落在传送带中间位置,向上运输到正确的位置,解决了电工钢偏移输送路线,无法输送到准确的位置,发生脱落的问题。
高硅FeSi合金层对普通取向硅钢磁性能的影响
目的提高硅钢的磁性能。方法采用多弧离子镀技术,在普通取向硅钢薄板两面沉积高硅FeSi合金层制得高硅梯度硅钢,并进行热处理,观察其显微组织,测量磁性能。结果退火态高硅梯度硅钢表面的高硅FeSi合金层与基底结合紧密,均匀致密。高硅梯度硅钢中硅含量呈梯度分布,最表层硅质量分数为11.0%,随着深度增加,硅含量逐渐降低,在距表面20μm处硅质量分数仍能达到6.5%。沉积态高硅梯度硅钢的电阻率ρ、低频铁损P10/50、高频铁损P10/1k及磁感应强度B8分别为68.6μΩ·cm,0.82W/kg,83.3 W/kg和1.73 T,退火后分别为63.1μΩ·cm,0.44 W/kg,54.38 W/kg和1.89 T。结论由于表层高硅FeSi合金层的存在,梯度高硅钢的低频磁学性能良好,但高频损耗需进一步改善。 Objective To improve the magnetic properties of silicon steel. Methods FeSi alloy coatings with high-silicon content were deposited on the surface of common grain-oriented silicon steel by cathodic arc plasma evaporation,and then a kind of high silicon gradient steel was prepared. The morphologies,content and magnetic properties of the samples were tested. Results FeSi alloy coatings were featured with compact microstructures and excellent adhesive quality with the substrates. The silicon conten...
高性能取向硅钢生产过程中的节能降耗
从取向硅钢生产路线的选择、工艺技术的改进和生产设备的改造三方面进行了生产取向硅钢的节能降耗技术改造.通过完善多元抑制剂配方生产低温取向硅钢,通过加抛丸的酸洗、带面超声波清洗、改进连续退火炉以及余热循环利用等技术改造,使2012年取向硅钢的产量与未进行技术改造前的2009年相比提高了2.5倍,产品磁性上升了一个半牌号,能耗下降了8.9%,成材率提高了6.4%,生产成本下降了22%,综合效益显著. Energy saving technological transformation was carried out in the production of grain oriented silicon steel from three aspects of the oriented silicon steel production process route selection,technology improvement and equipment renovation.Through the improvement of multiple inhibitor formulations for producing low-temperature grain-oriented silicon steel,and by adding the blasting pickling,the belt surface ultrasonic cleaning,improvement of continuous annealing furnace,waste heat recycling tec...
CN202111012116.3无取向电工钢以及制造方法
本发明提供了一种无取向电工钢,包括:C0.001~0.010%,Si0.5~4.0%,Mn0.05~0.8%,Al0.2~1.5%,P≤0.002%,S≤0.0015%,O≤0.002%,N≤0.0015%,各成分均为质量百分比;还提供一种无取向电工钢制造方法,包括:冶炼钢水、薄带连铸、常化酸洗、冷轧以及退火涂层。本发明中,在冶炼钢水时,控制钢水中C、Si、Mn、Al、P、S、O以及N几种成分的含量,且通过常化工艺,可以有效控制无取向电工钢成品的产品质量,具有较低的铁损以及较高的电磁性能,另外整体制造流程比较短,能够达到节能环保的目的,而通过冷连扎,有利于提高产品的质量、成材率和生产效率。
Fe-6.5%Si高硅钢铁芯与Epstein Square标准单片铁损检测结果对比及数据差异分析
作为一种具有优异高频铁磁性能的合金,Fe-6.5%Si(质量分数)高硅钢在高频工况条件下降损效果明显,对电气行业应用器件高频化、小型化、节能等具有十分重要的意义。通过与取向硅钢测量B-P数据对比,验证了高硅钢高频超低损特性,且轧制高硅钢与日本CVD法生产高硅钢存在基本相同的铁损值。采用国标Epstein Square法对0.30mm高硅钢薄板进行单片测试,并对由0.30mm高硅钢薄板首次装配成的电感器进行铁损测试,对比测试结果表明,元件测试与单片测试数据基本吻合,高磁感应强度条件下,元件测试结果略低于单片测试,分析原因为:线圈引起励磁压降;元件叠片间出现短路,电流增大,损耗增加;气隙板厚度过大。 As one core material with excellent high-frequency ferromagnetism,Fe-6.5%Si performs obviously reduction on core loss in high field frequency which means much to high frequency,minimization,energy conservation in electric industry.Super low loss was verified by drawing B-P curves based on detected experimental data,and which went equal to Fe-6.5%Si thin strip fabricated by CVD in Japan.Fe-6.5%Si was firstly fabricated as inductor in this research,and its core loss was determined for comparison w...
CN202011597301.9一种在取向硅钢中获得沿晶断口的方法
一种在取向硅钢中获得沿晶断口的方法:将取向硅钢样品加工成俄歇电子能谱仪标准试样;对标准试样进行表面清理;充氢:将标准试样所设定的预设断口处放入充氢装置的含硫脲溶液中,并使取向硅钢样品为阴极;将铂片置入并作为阳极;阴极充氢电流为1.25~1.35A,充氢电流密度在0.1~0.8A/m2,充氢时间在12~50h,充氢电压为36~39V;进行表面分析。本发明不仅工艺简单,便于操作,用时短,所用毒化剂是硫脲,从而避免了采用剧毒的三氧化二砷作为毒化剂,对人体健康有极大威胁的问题,且所获得的取向硅钢断口均为典型沿晶断口,适用于取向硅钢晶界偏聚行为以及晶界微区成分分析。