西安重型机械研究所为武钢开发了目前国内第一台自动化水平较高的先进可靠的硅钢热轧试验轧机。本文介绍了该轧机的工艺参数、设备组成,技术特点及轧制流程,该轧机在规定的终轧温度范围内,实现了2.5 m/s的快速轧制速度,保证了控制系统准确及时的采集到轧件进出轧辊时的信号,缩短道次间隙时间,实现了自动控制,保证了产品板形及精度的高水平要求,对于硅钢尤其是对其取向硅钢新产品、新工艺的开发具有深远意义。 An experimental prototype of 400 mm silicon steel hot rolling mill was developed by Xi’an Heavy Machinery Research Institue for Wu Gang.The technological parameters,configuration and characteristic of advanced control system in the experimental prototype are introduced in detail.The experimental prototype was realized the fast rolling of 2.5 m/s in the range of specified rolling temperature.Its automatic rolling control system can acquisite the signals that a rolled piece enters in and exits fro... 
2011-04-28 177 5.8

简要介绍了宝钢无取向电工钢的发展历程、产品大纲、电磁性能控制情况,以及高附加值新产品的开发、应用情况。概述了近年来宝钢无取向电工钢生产技术进步,主要包括夹杂物控制技术、连轧机高牌号硅钢制造技术、同板差控制技术、环保涂层开发技术等。 This paper briefly summarizes the development history, product catalogue, and magnetic properties of non-oriented electrical steel sheets at Baosteel, as well as the development and application of high-value-added steel grades. Recent advances in manufacturing electrical steel sheets are also introduced, including technologies for controlling inclusion, producing high-grade steel strips by a tandem rolling mill, and controlling the transverse thickness difference of steel sheets, as well as the ... 
2014-05-28 178 5.8

本实用新型公开了一种电工钢自粘涂层液生产用搅拌釜,包括釜体,釜体的内部通过两个第一隔板分隔成第一安装腔、第二安装腔和搅拌腔,釜体的内部设有传动组件,传动组件包括伺服电机、主动轴和两个从动轴,伺服电机固定安装在釜体顶端的中部,伺服电机的输出轴与主动轴的顶端固定连接,本实用新型的有益效果是:通过设有八个与十二个搅拌叶片相交错的挡板,避免搅拌轴在搅拌过程中产生离心力造成漩涡,使自粘内外侧的涂层液得到充分搅拌,通过设有循环泵机、第二隔板和流通槽使搅拌釜内的自粘涂层液处于流通的状态,使底部不易被搅拌的涂层液能够得到充分搅拌,在提高搅拌釜的灵活性的同时,保留其原有的稳定性。
2020-12-25 173 6.8

两炉次无取向硅钢XG800WR(/%:0.003~0.004C、0.71~0.75Si、0.32~0.33Mn、0.004~0.007S、0.016P)的炼钢流程为铁水预处理(KR)-210 t顶底复吹转炉-钢包吹氩-RH脱碳精炼-230mm×1220 mm板坯连铸。53 t中间包钢水过热度为25~30℃,钢包到中间包采用长水口全程吹氩保护浇铸,中间包至结晶器采用浸入式水口浇铸。结果表明,在RH、中间包、结晶器过程中钢中总氧以及夹杂物数量和尺寸均明显降低;但在钢包到中间包过程T[O]、[N]和钢中夹杂物数量增加,说明长水口浇铸过程存在二次氧化。连铸坯中T[O]、[N]平均他分别为11×10-6和30×10-6,显微夹杂物数量平均为4个/mm2。铸坯中的显微夹杂物主要为3~5μm的AlN,同时存在少量的MnS、Al2O3·AlN和Al2O3·MgO·MnS。 The steelmaking flow sheet for two heats non-oriented silicon steel XG800WR(/%:0.003~0.004C. 0.71~0.75Si,0.32~0.33Mn,0.004~0.007S,0.016P) is hot metal pretreatment(KR)-210 t top and bottom combined blown converter-ladle argon blowing-RH decarburization refining-230 mm×1 220 mm slab casting.The superheating extent of liquid in 53 t tundish is 25~30℃,whole casting is shielded by blowing argon with long nozzle from ladle to tundish and the submerged nozzle is adopted in casting from tundish to mold... 
2011-05-28 170 5.8

采用自主研发的脉冲磁场退火装置,在取向硅钢脱碳退火过程中分别施加不同强度的磁场,并采用光学显微镜和X射线衍射仪研究了脉冲磁场脱碳退火后试样的显微组织和宏观织构。结果表明,脱碳退火过程中施加脉冲磁场后取向硅钢的平均晶粒尺寸均增加,当磁场强度为40 mT时,平均晶粒尺寸最大,为13.06μm。此外,取向硅钢试样的立方织构{001}<100>强度减弱,高斯织构{110}<001>和{111}<112>织构增强,有利于获得更好的成品织构和磁性能。 Self-developed pulsed magnetic field annealing device was used to apply magnetic field of different intensities during decarburization annealing of an oriented silicon steel, and microstructure and macro-texture of the specimens after decarburization annealing in a pulsed magnetic field were studied by using optical microscope and X-ray diffractometer. The results show that the average grain size of the oriented silicon steel increases with the application of pulsed magnetic field during decarbu... 
2022-02-28 197 5.8

采用光学显微镜、X射线衍射仪等分析了宁波钢铁有限公司生产的取向硅钢不同工序下的组织及织构演变规律。结果表明:铸坯经过热轧后,沿着厚度方向组织不均匀;一次冷轧并经脱碳退火后,组织由条状纤维状变成等轴状的初次再结晶晶粒,初次再结晶平均晶粒尺寸为18.17μm,织构主要以α织构和γ织构为主;在二次冷轧后,晶粒再次被压缩,转变为纤维状,织构主要为γ织构;经过高温退火后,发生二次再结晶,晶粒异常长大,晶粒尺寸达到厘米级,织构成分为单一且锋锐的Goss织构。 The microstructure and texture evolution of oriented silicon steel produced by Ningbo Iron and Steel Co.,Ltd.were analyzed by optical microscope and X-ray diffraction.The results showed that the microstructure of the slab was inhomogenous along the thickness direction after hot rolling.After first cold rolling and decarburizing annealing,the microstructure changed from strip fibrous to equiaxed primary recrystallized grains,and the average grain size of the primary recrystallization microstructu... 
2022-01-28 189 5.8

本发明涉及电机技术领域,具体涉及一种具有低应力结构的硅钢片、转子和电机。包括硅钢片、开设在硅钢片上的磁钢槽和嵌设在所述磁钢槽内的磁钢组件,所述磁钢组件包括多个磁钢组,所述磁钢组包括靠近转子边缘的一对小永磁体和靠近转子内侧的一对大永磁体,所述硅钢片在转子轭部沿周向分布有径向开槽,且所述径向开槽从硅钢片的中心向边缘延伸。其通过在转子轭部沿周向分设置从硅钢片的中心向边缘延伸的径向开槽,能降低大永磁体左右两侧铁芯刚度差距,从而有效降低隔磁桥处的应力,防止磁钢和铁芯产生形变而断裂。其无需改变电机转子外圆结构,在保证转矩输出的前提下,防止高速旋转时带来空气啸叫声。
2021-04-15 175 6.8

提供一种如下的无取向性电磁钢板用钢板:含有:C:0.0040%以下、Si:1.9%以上3.5%以下、Al:0.10%以上3.0%以下、Mn:0.10%以上2.0%以下、P:0.09%以下、S:0.005%以下、N:0.0040%以下、B:0.0060%以下;剩余部分由Fe和杂质构成;分别从板宽方向的两端部向板宽中央10mm的各位置的板厚方向截面组织的重结晶率不足50%;将板宽记为W时,分别距板宽方向的两端部1/4W的位置的板厚方向截面组织的重结晶率在50%以上。
2021-02-19 146 6.8

本实用新型公开了一种新型取向硅钢薄板,所述硅钢薄板包括薄板主体,薄板主体呈方形,薄板主体的内部具有硅钢基板,所述薄板主体的上部具有耐磨层,耐磨层底部还具有抗压层,耐磨层具有若干均匀分布的耐磨条,耐磨层之间分别等距间隔布置,间隔的耐磨条之间形成透气槽,透气槽具有两个侧边,透气槽底部具有透气通孔,所述透气槽两侧具有导风侧凸条,导风侧凸条具有根部和端部,根部分布在透气槽的底部左侧和右侧位置,所述端部延向透气槽两侧边部上部,所述耐磨条为均匀排列的若干双V型结构,双V型结构纵向排列,耐磨条和抗压层之间具有硬质包覆层,在不影响耐磨作用的前提下能够起到透气通风的效果,不需要增加硅钢薄板的厚度。
2021-06-24 154 6.8

本实用新型公开了一种变压器铁芯硅钢片板材滚切后打磨装置,包括机体、导向机构、隔板、前端打磨体和后端打磨体,所述导向机构设置在机体上,且所述导向机构导向若干料带的位移,所述导向机构之间设置有若干隔板,所述前端打磨体设置在料带传送方向上的前端,所述后端打磨体设置在料带传送方向上的后端,且所述前端打磨体、后端打磨体分别设置在两两相邻的料带之间;传送状态下的料带切割边缘相对于前端打磨体、后端打磨体打磨。在料带传动的同时,通过前端打磨体和后端打磨体的相对运动同时对两个料带的边缘进行打磨,结构简单,成本低,且能够提升料带外观质量。
2021-12-13 185 6.8

6.5%Si硅钢具有优异的磁学性能和广泛的应用前景。本文综述了6.5%Si硅钢的物理、机械及磁学特性,讨论了传统轧制、温轧、薄带连铸、快速凝固、CVD、粉末轧制等不同制备工艺的关键技术及特点,概括了6.5%Si硅钢在高效节能电机、汽车马达及磁屏蔽等领域中的主要应用,介绍了硅钢的制备技术取得的研究进展,并指出了其广阔的发展前景。 6.5% Si silicon steel has good magnetic properties and wide applications.In this paper physical and mechanical magnetic properties were summarized,and key technology and characteristic of several preparation methods,such as traditional rolling,warm rolling,thin strip continuous casting,rapid solidification,CVD and powder rolling,were discussed.Main applications of 6.5% Si steel in the fields of high-efficiency electrical motors,automobile motors,transformer cores and magnetic shielding were gene... 
2012-06-28 161 5.8

本发明涉及一种超纯净无取向冷轧硅钢中非金属夹杂物形貌的原位观察方法,包括如下步骤:制备无取向冷轧硅钢样品,将待测试面用打磨至1000#,使样品表面平整光滑,并进行机械抛光和表面清洗。对处理好的样品在电化学工作站上进行电化学腐蚀,电解液为:1~8wt%氯化物MCl溶液,余量为去离子水,通入CO2气体至饱和,加入适量NaHCO3和三乙醇胺作为稳定剂调节pH值将其稳定在6.0~6.5之间。电化学设定参数:开路:0.5~2h,动电位极化测试:扫描速率:0.1mV/S~1.0mV/S,测试区间:VS.SCE‑0.8V~0.2V,测试温度为:10~25℃。取不同区间内做完电化学腐蚀的样品用去离子水冲洗,吹干。通过扫描电子显微镜+能谱仪对非金属夹杂物的形貌进行原位观察和成分分析。
2021-06-11 168 6.8