研究了CSP工艺流程生产的硅含量为1.5%的无取向电工钢在不同常化温度下对磁性能的变化。研究结果表明:随着常化温度的提高,热轧板的晶粒尺寸增大,且组织均匀性提高;此外成品的有利织构组分{100}<0vw>、α、η增强,不利织构组分减弱;铁损P1.5/50呈下降趋势,磁感B50上升平缓。在常化工艺为970℃×2.5min下,对应的铁损P1.5/50<3.4W/kg,磁感B50>1.74T。 The effect of normalizing temperature on the magnetic properties of non-oriented electrical steel containing 1.5%silicon produced by CSP process was studied.The results show that with increasing normalizing temperature,the average grain size of hot-rolled plate increases and the microstructure uniformity is improved.Furthermore,the texture components of finished products are improved through enhancing of{100}<0vw>,αandηtextures and weakening of{111}<112>texture;the core loss P1.5/50 ... 
2014-03-28 120 5.8

通过金相分析和电子背散射衍射技术研究了一种新型含铜无取向电工钢在950℃退火不同时间(3~180s)空冷后的组织和织构取向的演变。结果表明:该钢在退火3s时的主要织构为α和γ线织构,{100}<110>织构最强;退火20s时织构以<111><112>、{111}<110>、{112}<110>、高斯织构和立方织构为主,随着退火时间的延长,高斯织构和立方织构强度呈减弱趋势;合理控制保温时间有利于提高{100}、{110}面织构的占有率。 Evolution of microstructure and texture oriented of a new non-oriented electrical steel during annealing at 950℃for different times(3-180) s and air cooling was studied by metallography and electron back-scattering diffraction analysis.The results show that after annealing for 3 s most of the texture oriented alongα-fibre andγ-fibre,the intensity of {100}〈110〉was the strongest.{111}〈112〉,{111}〈110〉,{112}〈110〉,Gauss texture and cube texture were the main texture after annealing for 20 s,with the ... 
2011-09-28 120 5.8

采用SEM、EDS和XRD对不同加热温度下W470连铸坯氧化铁皮的微观形貌及相结构进行研究。结果表明,W470氧化铁皮难以除去的原因是氧化铁皮熔化,液相包裹着FeO,凝固时发生共晶反应,生成FeO/Fe2SiO4共晶混合物,并深嵌入基体。降低加热炉的加热温度,使连铸坯全程在FeO/Fe2SiO4共晶混合物熔点(1177℃)以下加热,可降低氧化铁皮与基体的结合力,能够有效解决W470除鳞困难问题。 The microstructure and phase structure of iron scale of W470 continuous casting billet at different heating temperatures were investigated by SEM,EDS,and XRD.The results show that the reason why the iron scale of W470 removes hardly is that iron scale is melted and the FeO is surrounded by the liquid phase,which forms FeO / Fe2SiO4eutectic mixture and is embedded into the matrix after solidification.Lowering the heating temperature and keeping the continuous casting billet heating under the melt... 
2014-04-28 120 5.8

本发明涉及一种硅钢片叠压设备,包括加压机构,加压机构包括压台和压板,压台四角均设置导向柱,导向柱下端与压台固定连接,上端垂直向上延伸且穿透压板四角,压板上方设置有加力机构,加力机构包括固定板、活动板和挤压弹簧,固定板、活动板和压板平行设置,固定板设置与最上方且与导向柱上端固定连接,活动板设置于固定板和压板之间,固定板上穿透有多个螺杆,螺杆下端抵靠活动板顶面;活动板与压板之间均匀分布有多个挤压弹簧。本技术方案压台和压板构成了用于挤压叠放的硅钢片,通过转动螺杆可以将活动板向下推动,进而使活动板通过挤压弹簧将压板向下推动对叠放的硅钢片进行施压,装置结构简单、操作简单方便。
2021-11-22 120 6.8

一种在取向硅钢中获得沿晶断口的方法:将取向硅钢样品加工成俄歇电子能谱仪标准试样;对标准试样进行表面清理;充氢:将标准试样所设定的预设断口处放入充氢装置的含硫脲溶液中,并使取向硅钢样品为阴极;将铂片置入并作为阳极;阴极充氢电流为1.25~1.35A,充氢电流密度在0.1~0.8A/m2,充氢时间在12~50h,充氢电压为36~39V;进行表面分析。本发明不仅工艺简单,便于操作,用时短,所用毒化剂是硫脲,从而避免了采用剧毒的三氧化二砷作为毒化剂,对人体健康有极大威胁的问题,且所获得的取向硅钢断口均为典型沿晶断口,适用于取向硅钢晶界偏聚行为以及晶界微区成分分析。
2020-12-29 120 6.8

取向硅钢成品的晶粒尺寸非常大,其易磁化方向[001]晶向对于轧向的偏差角度对其磁性能影响极大。本文介绍了取向硅钢二次再结晶后成品晶粒位向的几种测定方法,包括侵蚀法、劳厄法、OIM法、极图法和非对称X射线衍射法等,并对这几种测量方法进行了比较。 The finished product of grain-oriented silicon steel has immense grain size ranging from millimeters to centimeters and the deviation angles of easy magnetization direction from rolling direction plays a remarkable role in magnetic properties of grain-oriented silicon steel.The methods in common use for determining the deviation angles of crystal direction are introduced,which include the etch-figure method,the Laue method,the OIM method,the pole figure method and the asymmetrical X-Ray diffract... 
2011-04-28 120 5.8

本实用新型提供一种硅钢片模具产品的吸料装置,包括固定架、电动伸缩杆、微型吸气泵、操作台、吸气机构以及放置机构,所述固定架上表面设有电动伸缩杆,所述固定架上表面设有微型吸气泵,所述微型吸气泵右端面设有吸气口,所述吸气口右端设有气管,所述电动伸缩杆底部设有吸气机构,所述吸气机构底部设有操作台,所述操作台上表面设有固定柱,所述固定柱前表面设有放置机构,与现有技术相比,本实用新型具有如下的有益效果:通过设置的橡胶套,代替手进行硅钢片的取料,通过设置固定杆,实现橡胶套的自动放料,更安全,通过设置的放置机构,实现硅钢片倾斜放置,方便进行硅钢片的拿取进行变压器装配。
2021-01-05 120 6.8

本实用新型公开了一种大型硅钢片生产用输送装置,包括支撑座,所述支撑座的顶部安装有第一支架和第二支架,且第一支架位于第二支架的上方,所述第二支架的一端伸出支撑座的底部,其中,所述第一支架的外部套设有多组第一皮带,所述第一支架的内部安装有多组气缸,且气缸的一侧安装有感应器;所述第二支架的外部套设有两组第二皮带以及两组第三皮带,且两组第二皮带分别位于第二支架的两侧,两组所述第三皮带位于两组第二皮带之间,且第三皮带的长度小于第二皮带的长度。本实用新型所述的一种大型硅钢片生产用输送装置,通过对第一皮带增加磁性,并对调整第三皮带之间间距,能够轻松将转子和定子进行分类堆叠,节省机械手运行的时间。
2021-11-25 120 6.8

一种硅钢厂调功器故障报警自动复位的方法,包括:通过人机界面对炼钢炉温度进行设定,并在炼钢过程中实时获取炼钢炉温度;将炼钢炉实时温度与设定温度进行对比,当炼钢炉实时温度低于设定温度时,启动调节器;调节器输出功率使电阻带加热,使炼钢炉实时温度达到设定温度;当调节器发生故障时,调节器将故障信号发送给后台服务器,后台服务器根据故障指令,按预设规则控制与调节器连接的继电器,控制继电器按压复位按钮,使调节器自动复位。本发明解决了现有技术中通过电气人员来通过复位消除故障状态,耽误时间长,容易产生废品的问题。
2021-03-29 120 6.8

本实用新型涉及硅钢轧制油反应设备技术领域,尤其是一种硅钢轧制油专用反应装置,它包括反应罐,所述反应罐的内底部焊接有导热板,所述导热板的底面安装有安装壳,所述安装壳的内部固定安装有电热盘,所述反应罐的右侧面底部固定安装有温度传感器,所述反应罐内设置有搅拌机构,本实用新型通过设有温度传感器、电热盘和控制器,能够有效控制反应罐内部的温度,使其内部的温度能够达到设定的温度值,防止因温度过高而爆炸,提高了安全性,而且,通过由搅拌电机、搅拌轴、主搅拌叶、分搅拌叶和螺旋搅拌杆组成的新型搅拌机构,该搅拌机构的搅拌覆盖率大,搅拌效果较好,能够进一步加快物料间化学反应的速率,提高生产效率。
2021-03-04 120 6.8

本实用新型公开了一种基于取向电工钢用收卷组件及其固定结构,包括主体,所述主体的后侧中部固定安装有固定杆,所述固定杆的侧面活动安装有活动机构,所述活动机构包括活动块,活动区,弹簧,主动块,连接孔,连接杆,齿轮,卷筒,挡板。该种基于取向电工钢用收卷组件及其固定结构,活动块会带动活动区内部的主动块在其内部移动,可以通过连接杆带动齿轮进行转动,因齿轮侧面啮合连接有齿口,从而会顺着主体的侧面进行移动,当齿轮移动到主体的一角时,会带动活动区内部的弹簧收缩,弹簧可根据齿轮到主体中心的距离长短进行伸缩,物料会通过卷筒落到卷块的表面,从而可以对物料进行收卷,最后达到了便于收卷,降低物体损害的目的。
2021-05-31 120 6.8

本发明提供了一种取向硅钢制作的电机凸极转子,包括由取向硅钢一体制作而成的凸极极身、轭部与极靴,整个转子的易磁方向为径向,通过对轭部厚度、相邻凸极根部中心点距离、凸极极身宽度和极靴尺寸等进行特殊结构设计,能够提高电机功率密度与效率,且无二次气隙与额外的工艺需求。