钢厂
硅钢高温退火环形炉炉壳制作与安装技术
硅钢高温退火环形炉炉壳制作与安装精度要求较高,施工时通过对壳体原材料矫正、炉壳板拼焊、下料切割、型钢骨架组装及焊接、骨架及炉壳板矫正、骨架与炉壳板组装及焊接、炉壳矫正、零配件装置、定位钻孔、报验检查、出厂、内侧板安装、外侧板安装、顶板安装等环节的工艺技术控制,能保质高效地完成硅钢高温退火环形炉炉壳制作与安装,为以后同类工程的施工提供可借鉴经验。 The required precision of manufacture and installation technique of the silicon steel high temperature annealing annular-furnace shell is high.During construction , manufacture and installation of the silicon steel high temperature annealing annular-furnace shell could be finished high efficiently through correcting the raw materials of shell , furnace shell plate welding , material cutting , steel frame assembly and welding , skeleton and shell plate correction , skeleton and furnace shell asse...
热处理工艺对含Mn高硅钢热轧带的组织及硬度的影响
研究了热处理工艺(退火温度、保温时间、冷却方式)对含Mn的Fe-6.5wt%Si高硅钢热轧带的显微组织及硬度的影响。结果表明,退火温度对Fe-6.5wt%Si合金的组织和显微硬度均有较大影响,随退火温度升高,平均晶粒尺寸和显微硬度均明显增大。小于1 h退火时,晶粒长大缓慢,而长时间(>1 h)退火时,一些次表层晶粒将发生异常长大。水冷组织比空冷组织略细小,但水冷显著降低了显微硬度。Mn含量提高能抑制850℃退火时晶粒的长大,并且促进退火后高硅钢的软化。 The influences of heat treatment process(annealing temperature,heating time,cooling methods) on the microstructure and microhardness of Fe-6.5wt%Si high silicon steel containing manganese for hot rolled strip were studied.The results show that the annealing temperature has a great effect on the microstructure and microhardness of Fe-6.5wt%Si alloy,and as the annealing temperature increases,the average grain sizes and microhardness will significantly increase.When annealing time for less than 1 h...
脉冲磁场退火对取向硅钢磁性能的影响
通过对取向硅钢进行脉冲磁场退火实验,发现在相同的退火时间(6.0 min)内,低于1 T的脉冲磁场可以在一定程度上提高取向硅钢的磁感(B8),而高于1 T的脉冲磁场则会使取向硅钢的磁性能急剧恶化.同时发现,脉冲直流电加热方式会使取向硅钢的磁性能恶化.研究表明,脉冲磁场退火有望成为一种调控材料微观结构的有效手段. We have carried out experiments of annealing by pulse magnetic field.The results show that a pulse magnetic field with intensity lower than 1 T can promote magnetic induction density(B8) of grain-oriented silicon steel,while the magnetic properties deteriorate sharply when intensity is higher than 1 T.It has also been found that heating by using pulse direct current can cause the magnetic properties to deteriorate,in contrast to the traditional heating using resistance furnace.Our research shows...
卷取工艺对新型冷轧无取向电工钢组织性能的影响
研究了卷取工艺对一种新型含铜无取向电工钢晶粒尺寸、织构演变、铁损和磁感应强度的影响。结果表明,试样织构组分主要为{111}、{112}、{100}和高斯织构,在550℃卷取、保温2~3h,{100}织构有增强趋势,磁感应强度较高,铁损较低。 The effects of coiling process on grain size,texture,core loss and magnetic induction of a new cold rolled non-oriented electrical steel with copper were investigated.The results show that there are mainly {111},{112},{100} and {110}<001> texture.Coiling at 550℃and keeping for 2~3 hours,the {100} texture is enhanced,magnetic induction is higher and core loss is lower.
B元素对高牌号无取向硅钢热轧板组织和性能的影响
借助实验室设备研究了B元素对高牌号无取向硅钢热轧板组织和磁性能的影响。结果表明,与无硼钢相比,含硼钢的热轧板晶粒尺寸略小,析出物的类型和尺寸没有区别,主要是AlN和(AlN+MnS)复合析出物,少量的MnS析出物,尺寸集中在1.0~2.5μm范围内。未发现BN析出物。在力学性能方面,B对钢的软化作用不明显。在磁性能方面,含硼钢的铁损为3.215W/kg,磁感为1.710T,综合磁性能比无硼钢差。 Influences of boron on microstructure and properties of hot rolled band in high-grade non-oriented silicon steel are researched in this paper by experimental equipments.Compared with boron-free steel,the result shows that boron-bearing steel has smaller grain size,but the type and size of precipitations have no differences.The main precipitates are AlN,(MnS + AlN) composite precipitate and few MnS,the range of which are between 1.0 μm and 2.5 μm.BN precipitation is not found.With reward to mecha...
CN202123355538.9变压器铁芯用硅钢片成型铁测量平台及其定位台
本实用新型公开了一种变压器铁芯用硅钢片成型铁测量平台,包括游标测量尺及定位台;定位台包括基架、操作台及至少两根的定位销,操作台I及操作台II分别设置于基架的横向两端,且操作台I及操作台II之间留有宽度a的间距区,操作台II上设置有至少一组的沿横向均匀分布的定位孔组,且至少两根的定位销能够与该定位孔组的定位孔配合,游标测量尺设置于基架上间距区处。在操作台II上设置有至少一组的沿横向均匀分布的定位孔组,且至少两根的定位销能够与定位孔配合,以将该硅钢片成型铁定位区域限定在操作台II台面上,采用多个定位孔和定位销配合结构,同时能够沿横向调整硅钢片成型铁定位位置,以便测量各个区域尺寸。
CN202123198150.2一种取向硅钢全氢式高温罩式炉外罩
本实用新型涉及一种取向硅钢高温退火设备,尤其涉及一种取向硅钢全氢式高温罩式炉外罩,从外至内包括圆柱形外壳和耐火保温层,所述耐火保温层内壁铺设有电阻带;所述圆柱形外壳上部设有外罩顶盖;所述耐火保温层由陶瓷纤维模块堆砌而成,所述电阻带通过钉子铺设在陶瓷纤维模块上;电阻带头一端通过接线棒引出炉壳外,另一端中性点在炉内短接。本实用新型保温层内层采用模块化的高纯度陶瓷纤维代替耐火砖,该材料具有重量轻、蓄热少,低导热性能带来高的节能效果,具有抵抗热冲击的能力,加上模块化的结构,安装快捷,衬体无需烘干和养护,所以安装好以后便可立即投入使用。
CN202123144024.9转盘式硅钢片转运装置
本实用新型公开了转盘式硅钢片转运装置,属于硅钢片转运领域,包括本体,所述本体的顶部设置有收纳箱,所述本体的内部水平设置有横板,所述横板的两侧分别与本体内腔的两侧固定连接,所述横板的底部设置有平移机构,所述横板横向活动套接在连接杆,所述连接杆顶端与收纳箱的底部固定连接,所述连接杆的底端固定连接有转动盘,所述转动盘的底部固定连接有固定杆,所述固定杆上活动套接有套筒,通过设置平移机构,平移机构带动铰接杆,铰接杆拉动固定杆,固定杆带动转动盘,转动盘通过连接杆带动收纳箱,使得收纳箱可以进行旋转,将远离工作人员的一侧,调整至靠近工作人员的一侧,从而方便进行安放硅钢片。
CN202111448726.8一种硅钢生产线上的牵引装置
一种硅钢生产线上的牵引装置,包含有底座(1)、支架(2)、平移机构(3)、上压板(4)、下托板(5)、气缸(6)、转向辊(7)和对中摄像头(8);所述的平移机构(3)包含有长条齿轮(14)、齿轮(15)、电机(16)和滚轮轴承(17);其特征在于:所述的齿轮(15)固定在电机(16)的输出轴上,并且与长条齿轮(14)啮合;使得平移机构(3)可以由电机(16)驱动在导轨(10)上左右滑动。本发明通过气缸(6)驱动上压板(4)和下托板(5)夹紧钢带(9),由平移机构(3)带动钢带(9)进行左右平移,避免了原先夹送辊刮伤钢带(9)表面涂层,减少了带头的浪费。
CN202111369195.3一种电力变压器硅钢片自动叠片生产设备
本发明公开了一种电力变压器硅钢片自动叠片生产设备,包括支撑板和叠片立板,其中一组所述支撑板的表面安装有叠片立板,另一组所述支撑板的顶部安装有检测立板;所述叠片立板的背面安装有连杆,所述连杆的尾端连接有限位环,所述限位环的内部等距贯穿安装有第一电动伸缩杆,所述第一电动伸缩杆的尾端表面套接有橡胶套,所述叠片立板的背面设有滑槽,所述滑槽的底壁安装有缓冲弹簧,所述滑槽的顶壁安装有第二电动伸缩杆,所述第二电动伸缩杆的尾端连接有拦截条,两组所述支撑板的顶部均安装有立块。本发明通过设置有叠片立板、限位环、拦截条以及缓冲弹簧的配合,可简化本叠片设备的整体占地面积,简化叠片加工程序。
CN202111249559.4一种基于全流程数据的冷轧硅钢厚度控制方法、装置
本发明涉及一种基于全流程数据的冷轧硅钢厚度控制方法、装置,该方法包括:针对某个冷轧钢卷,首道次默认使用监控AGC,在进入冷轧机工序生产之前,获取其前序全流程的生产工艺和质量数据,并进行预鉴定,若发现硅钢性能波动,则首道次额外再使用秒流量AGC;若发现硅钢厚度波动不剧烈,则首道次额外再使用前馈AGC。本发明无需人工干涉,采用上述规则在生产前就能自动确定最优的AGC生产模式,保证了硅钢产品厚度精度,避免硅钢厚度指标上的缺陷。