CN202110758995.8一种中温普通取向硅钢及其制备方法
本申请涉及一种中温普通取向硅钢及其制备方法,依次包括加热、除鳞、控制轧制、控制冷却、卷取;加热、控制轧制、控制冷却、卷取过程中分别控制硅钢边部组织类型、边部脱碳宽度、边部晶粒大小,从而降低了后续冷轧工序的裂口率和提高了成材率。本申请提供的一种中温普通取向硅钢的制备方法,通过改善加热炉气氛、优化控制轧制工艺、优化控制冷却工艺以及调整板坯的装钢间距。制备后的硅钢边部硬度明显降低,在后续冷轧工序中,严重裂口率显著降低。
云边一体化系统架构下硅钢制造管理业务数字化融合应用
提出以“云边一体化架构”构建硅钢智慧决策系统,来解决原硅钢制造L1~L5系统架构模式下的数字信息孤岛、业务功能割裂等问题。在此基础上,开发了云边协同的自学习型控制模型及业务决策模型,构建起硅钢“智慧大脑”,形成了以研发、制造、服务等核心业务数字化融合的智能化决策支持新模式,探索出一条钢铁制造业数字化、智能化转型之路。 SIDS(Silicon-steel Intelligent Decision-making System)based on \"cloud-edge integration architecture\" was proposed to solve the problems of data silos and business function fragmentation in the original L1~L5 system architecture.On this basis,the self-learning control model and decision-making model of cloud-edge collaboration were developed,the \"smart brain\" of silicon steel department was constructed,and a new intelligent decision-making support model of digital integration of core businesses s...
CN202023246581.7硅钢冷轧用厚壁套筒
本实用新型涉及硅钢生产设备技术领域,具体公开了硅钢冷轧用厚壁套筒,包括外筒和内筒,所述外筒与内筒之间固定有若干连接板,所述外筒上开设有插缝槽,所述外筒的内壁上设有靠近插缝槽设置的限位件,所述限位件包括锁止板和弹性件,弹性件一端固定在外筒的内壁上,另一端固定在锁止板的顶部,所述锁止板上设有朝向插缝槽的斜面。本专利中通过外筒与内筒设置,既提高了整个套筒的厚度,使其能够承受硅钢带卷绕时的压力,同时也减少因提高套筒厚度使得套筒的重量增加的问题,这样设置整个套筒的质量较轻。
CN202123325575.5一种带连接筋的硅钢盘
本实用新型提供了一种带连接筋的硅钢盘,包括多个周向间隔排列的硅钢块,任意相邻的两所述硅钢块之间连接至少两连接筋,以将相邻的两所述硅钢块之间的空间分割为分设在所述硅钢盘轴向两侧的转子槽,及位于两所述转子槽之间的若干个收纳孔。多个所述硅钢块通过连接筋连接,并形成一整体的硅钢盘,相对现有技术独立成型多个硅钢块来说,不仅避免硅钢块丢失,还有效提升硅钢盘装配为转子盘的成型效率,以及保证各硅钢块在转子盘上的位置一致性,并且增加所述连接筋的数量,有效增强相邻两硅钢块的连接性能,从而大幅增强转子盘的机械可靠性。
节能电机用无取向电工钢带退火工艺的试验与应用
针对节能电机对无取向电工钢在磁性能方面的特殊要求,采用普通W600牌号的热轧板为原料,通过大量的现场工艺试验,研究总结出了\"超低张力\"的运行工艺、\"先快后慢\"的加热工艺、\"先湿后干\"的退火脱碳工艺、\"先缓后急\"的冷却工艺,生产出P1.5/50≤4.0 W/kg、B50≥1.70 T的冷轧电工钢产品,满足了节能电机的要求。 Based on the special requirements of no-oriented electrical steel for saving energy motor in magnetic aspects,using common W600 brand of hot rolled plate as raw material,through a large number of real tests,an ultra-low tension process,heating process which was quick at first and then slow,annealing decarburization process which was dry after the first wet,and a cooling technology of \"slow after the first urgent\" were concluded.Electrical steel product with P1.5/50≤4.0W/kg,B50≥1.70T was produced...
取向硅钢初次再结晶退火工艺正交试验
以试验室模拟CSP工艺生产的Fe-3Si热轧钢带为研究对象,采用正交试验及方差分析的方法,研究了取向硅钢初次再结晶退火工艺对高温退火后获得锋锐的高斯织构的影响。结果表明:取向硅钢两段式初次再结晶脱碳退火工艺参数加热段保温时间及加热温度是高温退火后获得锋锐高斯织构的主要影响因素,其可信度分别在90%和85%以上;在本试验条件下,通过正交试验获得的最佳退火工艺为:冷硬板经600℃保温3 min和850℃保温6 min。 Fe-3Si hot rolled strip was produced by simulating CSP technology in the laboratory.Orthogonal experiment and analysis of variance were carried out to investigate the influence of primary recrystallization on the sharp Goss texture of the oriented silicon steel.The results show that holding time of the heating section and the heating temperature for a sharp Goss texture of the samples annealed has important implications in this experiment conditions,the two-step decarburization annealing process...
脱碳温度和脱碳时间对CGO取向硅钢碳含量控制的试验研究
通过测试取向硅钢不同工艺条件下的碳含量,探讨了CGO取向硅钢碳含量控制的最优处理条件,研究了脱碳温度和脱碳时间对相同初始碳含量取向硅钢的脱碳效果的影响。结果表明,在气氛为(15%~20%)H2+(75%~80%)N2,炉压差为10~20 Pa的条件下,CGO取向硅钢合适的脱碳温度为1 073 K~1 123 K,脱碳时间为10~20 min。在该处理条件下,能取得较好的脱碳效果。 By means of testing carbon content of oriented silicon steel below the distinct technical conditions,inquires the excellent handle terms of carbon content controlling for CGO oriented silicon steel,studies effects of decarburization annealing temperature and decarburization annealing time to the oriented silicon steel decarburization efficiency in same initial carbon content.The results show that,under the condition of atmosphere(15% ~ 20%) H2+(75% ~ 80%)N2 and furnace pressure difference 10 ~ 2...
CN202110176053.9一种常化后免酸洗生产取向硅钢的方法
本发明涉及一种常化后免酸洗生产取向硅钢的方法,取向硅钢的生产工艺路线为:冶炼→连铸→热轧→常化退火→拉伸矫直→抛丸→冷轧→脱碳退火→渗氮→涂MgO→高温退火→热拉伸平整及涂绝缘膜;本发明在常化退火后通过物理方法去除带钢表面的氧化铁皮,且效率高、效果好、操作简单、易于控制;与常规工艺相比,省去了酸洗及后续废酸处理工作,排除了酸雾对环境的污染,消除了取向硅钢带因酸洗而产生的潜在缺陷,产品质量更加稳定可靠。
CN202110496191.5一种中高牌号无取向硅钢无焊丝焊接的方法
一种中高牌号无取向硅钢无焊丝焊接的方法,属于无取向硅钢激光焊接技术领域,该焊接的方法,包括1)将低牌号无取向硅钢的带尾与中高牌号无取向硅钢的带头对中接触相连;2)激光焊接前对引带和母材之间的焊缝进行预热处理,然后采用激光焊机焊接,焊接完成后对焊缝高温回火处理;3)焊接完成后,将中高牌号无取向硅钢和低牌号无取向硅钢按照上述步骤交替焊接,本发明的有益效果是,本发明通过合理选择引带、在焊接前预加热和焊接后回火处理的工艺、适当调整连轧机组的轧制参数,实现了中高牌号无取向硅钢的无焊丝焊接,提高了焊缝的质量,降低了断带率,保证了焊缝的可连续轧制,提高了轧制的效率。
CN202122954252.6一种冷轧硅钢无压回水自动控制设备
本实用新型属于冷轧硅钢技术领域的一种冷轧硅钢无压回水自动控制设备,包括底座,底座外表面的上端固定连接有工作台,工作台外表面上端的两侧分别固定连接有固定柱和压辊主体,工作台外表面上端的中部滑动连接有移动架,压辊主体的下端设置有集水槽,集水槽的内表面设置有浮球液位传感器。液压杆工作推动移动架位移到合适的位置,再通过气缸使伸缩管发生位移,使出水口接近钢板,设置的水箱高于出水口所以水可以在重力的作用下流淌,流出的水流到集水槽内,水流在集水槽内聚集,水流使浮球液位传感器的浮球上升,上升到合适的位置时,浮球液位传感器通过电缆发生电信号至控制器,此设置可以实现设备的自动控制,省去人工进行操作。
CN202123198150.2一种取向硅钢全氢式高温罩式炉外罩
本实用新型涉及一种取向硅钢高温退火设备,尤其涉及一种取向硅钢全氢式高温罩式炉外罩,从外至内包括圆柱形外壳和耐火保温层,所述耐火保温层内壁铺设有电阻带;所述圆柱形外壳上部设有外罩顶盖;所述耐火保温层由陶瓷纤维模块堆砌而成,所述电阻带通过钉子铺设在陶瓷纤维模块上;电阻带头一端通过接线棒引出炉壳外,另一端中性点在炉内短接。本实用新型保温层内层采用模块化的高纯度陶瓷纤维代替耐火砖,该材料具有重量轻、蓄热少,低导热性能带来高的节能效果,具有抵抗热冲击的能力,加上模块化的结构,安装快捷,衬体无需烘干和养护,所以安装好以后便可立即投入使用。