对两种硅钢水溶性极厚绝缘涂层进行了不同温度的热老化实验。通过TG-DTA,GDS,FT-IR,SEM和光泽度仪等测试方法对老化的涂层进行分析表征,提出了评估硅钢水溶性极厚绝缘涂层热老化性能的合理温度区间,探讨了涂层热老化行为,并分析了两种涂层热老化性能的差异。结果表明,涂层附着性随着老化时间的延长逐渐下降。FT-IR表征结果显示,热老化过程中,涂料交联形成的化学键未发生断裂,交联剂氨基树脂的三嗪环被破坏是聚合物三维网络结构坍塌的主要原因。 Thermal aging expriments at different temperature were carried out on two types of water-soluble and extra-thick insulation coatings for non-oriented silicon steel,and a series of test methods such as glossmeters,TG-DTA,FT-IR,GDS,SEM were applied in analysis.For evaluating the thermal aging effect of this kind of insulation coating,the proper temperature range was proposed.The difference of aging performance between two coatings was been investigated and the related behaviors were been discussed... 
2011-04-28 308 5.8

【作者】 陈迪安; 李春生; ...
2023-05-09 255 5.8

本实用新型公开了一种硅钢底辊套管生产用防氧化处理装置,包括一种硅钢底辊套管生产用防氧化处理装置,包括底板和打磨箱,所述底板的顶面固定安装有打磨箱,且打磨箱的背立面焊接有安装架,且安装架的一侧表面固定安装有驱动电机,所述驱动电机的输出端通过联轴器贯穿打磨箱的表面并延伸至内部固定安装有转动轴,且转动轴的表面设有打磨辊。有益效果:通过设置吸尘管、吸尘孔、管道和吸尘器的相互配合使用,吸尘器的进气端能够将打磨过程中的灰尘通过管道从吸尘管表面的多个吸尘孔内吸出,防止灰尘四处飘散,降低灰尘对工作人员身体造成的伤害,同时减少灰尘对环境造成的污染,且减轻工作人员清理飘散后灰尘时的劳动量。
2021-10-13 289 6.8

【作者】 卢鹏; ...
2014-03-28 176 5.8

冷轧无取向硅钢(/%:0.003C,2.35Si,0.22Mn,0.011P,0.002S,0.36A1,0.003 0N)经890℃或940℃3 min常化的2.3 mm热轧板冷轧成0.35 mm薄板。研究了常化温度和800920℃3 min退火对该钢高频(400Hz)磁性能和抗拉强度的影响。结果表明,830920℃退火时高频铁损P10/400值最低,随退火温度增加,晶粒尺寸增大,钢的抗拉强度降低;该钢的最佳热处理工艺为常化温度940℃,退火温度830℃,其抗拉强度Rm、高频铁损P10/400和磁感应强度J50分别为565 MPa,21.5 W/kg和1.69 T。 The cold-rolled non-oriented silicon steel(/%:0.003C,2.35Si,0.22Mn,0.011P,0.002S,0.36A1,0.003 0N) is cold-rolled to 0.35 mm sheet from 2.3 mm hot-rolled plate normalized at 890 ℃ or 940℃ for 3 min.The effect of normalizing temperature and annealing process at 800 920 °C for 3 min on high frequency(400 Hz) magnetic properties and tensile strength of the steel has been tested and studied.Results show that with annealing at 830 920 ℃the high frequency iron loss value P10... 
2014-03-28 559 5.8

本发明公开一种硅钢片叠片装置,涉及硅钢片叠加领域,包括:上料机构,其包括第一定位装置,第一定位装置包括多个第一轴向定位柱,第一轴向定位柱与周向开孔一一对应,多个第一轴向定位柱分别穿过不同位置的周向开孔;精定位机构,其周向定位硅钢片;下料机构,其包括第二定位装置,第二定位装置包括用于与硅钢片的中心孔相配合的中心定位柱;用于将设置于第一轴向定位柱上的硅钢片移动至精定位机构的移载机构;摄像装置;机器臂,摄像装置与机器臂通信连接,机器臂根据摄像装置拍的键槽方口特征调整硅钢片的角度、并将硅钢片移动至中心定位柱。该硅钢片叠片装置能够有效降低人工劳动强度,并提高叠放效率。
2021-07-12 413 6.8

本实用新型公开了一种硅钢卷上料装置,包括两支撑台和设置在两支撑台之间的输送组件,所述输送组件包括轨道和设置在轨道上的输送件,所述输送件包括滑板、支撑板、承重板和气缸,所述轨道平行于两支撑台设置在两支撑台之间,所述滑板可滑动设置在轨道上,所述支撑板通过气缸可升降设置在滑板上,所述承重板设置在支撑板上,所述承重板的截面呈U型,其上设置有第二缓冲条。其可实现硅钢卷的轻松上料,省时省力的同时,安全性大大提高。
2021-12-20 308 6.8

以取向电工钢成分为基础,制备了含C或Mn和S的4种实验钢。观察了接近平衡析出状态实验钢经60%冷轧后在600~1000℃范围再结晶退火过程中微观组织演变,统计分析了再结晶体积分数随退火时间的变化规律,进而计算了各实验钢静态再结晶的激活能。观察了高含C实验钢退火初期再结晶晶粒优先出现的部位。结果表明900~1000℃范围内各实验钢铁素体的化学成分相似,因而其再结晶激活能基本一致。在600~800℃范围内铁素体内会有阻碍再结晶进程的三次渗碳体析出,从而使再结晶激活能明显提高。高C含量实验钢中还会有从奥氏体转变而来的粗大珠光体或渗碳体,轧制过程中其附近形成的变形区会促进600~800℃加热时该区域附近率先发生再结晶形核、降低再结晶激活能。固溶的Mn、S元素可微弱提高再结晶激活能,但高Mn、S含量会改变粗渗碳体从奥氏体析出时的形态。 Four experimental steels based on grain oriented electrical steel containing C,or Mn and S were prepared.Microstructure evolution of the steels close to a state of equilibrium precipitation were observed during annealing processes at 600-1000 ℃after 60% cold rolling,the changes of recrystallization volume fraction were analyzed statistically as the annealing was prolonged,and the activation energy for static recrystallization of the steels were calculated.The locations,where the recrystallizatio... 
2011-12-28 275 5.8

针对某厂DMS森吉米尔轧机生产无取向硅钢表面麻面缺陷的问题,根据生产实际,对其形成原因从乳化液及工作辊两方面因素进行了分析。结果表明:乳化液对麻面缺陷的产生有一定影响,但不是主要因素,主要原因是由于二十辊森吉米尔轧机工作辊辊径较小,轧制相同长度带钢轧辊运转周期较大,容易产生疲劳失效而导致。为此,提出通过调整冷轧工序成品轧制道次的压下率以减小轧制力,从而减小工作辊的磨损疲劳;通过对轧制乳化液浓度、温度的合理控制,以改善润滑效果、提高轧制速度,而进一步缓解轧辊疲劳的改进措施,使该钢厂无取向硅钢麻面缺陷发生率由原来的18%降至0.8%,带钢表面质量明显改善。 For the problem of surface pockmarks of non-oriented silicon steel strip produced by a DMS Sendzimir mill, based on the production practice, the formation causes were analyzed from two aspects of emulsion and working roll. The results show that the emulsion has a certain effect on the formation of surface pockmarks defects, but it is not the main factor. The main reason is that the working roll diameter of the 20-high Sendzimir mill is small, and the running period of the roll rolling the same l... 
2022-01-28 469 5.8

综述了国内外大钢铁企业与研究机构采用获得抑制剂法生产低温高磁感取向硅钢的开发及应用情况,分析了以该法生产高磁感取向硅钢过程中抑制剂的控制技术,包括固有抑制剂组成方案、气态渗氮方式与工艺及高温退火工艺的制定.研究表明,固有抑制剂组成方案的设计思路大体一致,化合物抑制剂以AlN为主、硫化物为辅,同时添加少量Sn,Sb等单元素抑制剂,但组成元素含量存在一定差别;在脱碳退火后用NH3进行非平衡渗氮处理已成为气态渗氮的主要方式,但最佳方式仍未明确,具体选择需依据实际生产条件,相应脱碳及渗氮工艺的控制条件差别较大;高温退火工艺中升温制度差别不大,升温阶段退火气氛中N2含量的选择存在差别.此外,分析了抑制剂控制技术目前存在的关键问题,并指出了进一步的研究方向. The current application and exploitation on production of low-temperature high magnetic induction grain-oriented silicon steel with acquired inhibitor method at both iron and steel enterprises and research institutions in the world are reviewed. The control techniques of inhibitors, which include the composition design for inherent inhibitors, nitriding method and process, and secondary recrystallization annealing, are thoroughly analyzed and proposed. It is indicated that the design ideas for i... 
2014-01-28 438 5.8

对高牌号无取向电工钢国内生产情况、工艺技术、产品性能及应用领域等进行了阐述,并探讨了高牌号无取向电工钢产品的发展趋势。 This paper introduces basic facts on the production status,process technology and products’ properties and their applications of non-oriented electrical steel with high grade at home,and then discusses the development trend on technology for producing the non-oriented electrical steel with high grade. 
2011-02-28 218 5.8

简要介绍了宝钢无取向电工钢的发展历程、产品大纲、电磁性能控制情况,以及高附加值新产品的开发、应用情况。概述了近年来宝钢无取向电工钢生产技术进步,主要包括夹杂物控制技术、连轧机高牌号硅钢制造技术、同板差控制技术、环保涂层开发技术等。 This paper briefly summarizes the development history, product catalogue, and magnetic properties of non-oriented electrical steel sheets at Baosteel, as well as the development and application of high-value-added steel grades. Recent advances in manufacturing electrical steel sheets are also introduced, including technologies for controlling inclusion, producing high-grade steel strips by a tandem rolling mill, and controlling the transverse thickness difference of steel sheets, as well as the ... 