脉冲磁场热处理对CGO取向硅钢脱碳退火过程中组织和织构的影响
采用自主研发的脉冲磁场退火装置,在取向硅钢脱碳退火过程中分别施加不同强度的磁场,并采用光学显微镜和X射线衍射仪研究了脉冲磁场脱碳退火后试样的显微组织和宏观织构。结果表明,脱碳退火过程中施加脉冲磁场后取向硅钢的平均晶粒尺寸均增加,当磁场强度为40 mT时,平均晶粒尺寸最大,为13.06μm。此外,取向硅钢试样的立方织构{001}<100>强度减弱,高斯织构{110}<001>和{111}<112>织构增强,有利于获得更好的成品织构和磁性能。 Self-developed pulsed magnetic field annealing device was used to apply magnetic field of different intensities during decarburization annealing of an oriented silicon steel, and microstructure and macro-texture of the specimens after decarburization annealing in a pulsed magnetic field were studied by using optical microscope and X-ray diffractometer. The results show that the average grain size of the oriented silicon steel increases with the application of pulsed magnetic field during decarbu...
CN202121026669.XCD型硅钢片铁芯性能测试工装
本实用新型涉及硅钢片铁芯性能测试技术领域,公开了CD型硅钢片铁芯性能测试工装,包括:机台,上部后侧固定有竖直向上的后侧板;托板,水平设置在所述机台上方;夹持机构,设置在所述机台上,所述夹持机构包括:第二气缸,其驱动杆端部固定套接有夹持块,夹持块外端部固定有橡胶缓冲块;橡胶垫,固定在所述托板右侧上部。本实用新型通过设置第一气缸驱动连接于托板,可以先根据硅钢片的厚度,通过操作气缸控制器控制第一气缸工作带动托板在机台上进行升降高度,从而调整托板与夹持块的高度差,提高装置的实用性和广泛性,较为实用,适合广泛推广和使用。
CN202110781803.5一种取向硅钢的磁畴细化方法及应用
本发明提供了一种取向硅钢的磁畴细化方法,属于高磁感取向硅钢生产技术领域技术领域,包括:采用激光在带钢表面烧蚀出若干沟槽;采用腐蚀液对所述沟槽进行腐蚀,获得刻槽;其中,所述沟槽与带钢宽度方向的夹角为0‑20°;所述沟槽的深度为0.5~20μm,宽度为30~200μm;所述刻槽深度为0.5~30μm、宽度为30~300μm。该方法能够显著的细化磁畴,降低取向硅钢片单位损耗,同时细化磁畴的效果能够承受800℃‑900℃的消除应力退火。本发明还提供了一种取向硅钢的磁畴细化方法在取向硅钢生产中的应用。
CN202111220995.9一种冷轧取向硅钢EBSD用样品电解抛光制样方法
本发明公开了一种冷轧取向硅钢EBSD用样品电解抛光制样方法,包括:S1.机械抛光,切取10mm*10mm规格试样用超声仪清洗,在不同粒度的砂纸上预磨后在金相试样抛光机上抛光至镜面;S2.电解抛光,利用struerslectropol‑5型电解抛光机对机械抛光好的试样进行电解抛光;S3.EBSD检测。本发明主要解决现有设备技术条件下如何得到高质量的EBSD检测技术样品的问题,适用于大批量冷轧取向硅钢的EBSD样品制备,发明本方法后实验过程简单快捷,节约了实验时间和成本。
CN202022991890.0一种新型的去角硅钢片
本实用新型提供了一种新型的去角硅钢片,包括硅钢片本体,所述硅钢片本体包括叠放区和防护区,所述硅钢片本体设有防护结构,所述防护结构包括叠放区上设有的多个均匀分布的降噪凹槽,所述防护区上下两端分别设有多个防护条,且两两防护条之间设为连接槽,每个所述防护条皆包括与硅钢片本体连接的防护层和减震层,所述防护区底部两侧分别设有减震柱,所述防护区中间设有贯穿孔,所述贯穿孔内设有绝缘螺栓。本实用新型能降低噪音和减少震动影响,从而避免使得变压器寿命及功能性降低。
低温高磁感取向硅钢连铸与均热过程AlN与MnS析出的热力学
针对薄板坯连铸连轧流程结合\"获得抑制剂法\"所制备的低温高磁感取向硅钢,通过热力学计算研究了AlN与MnS在连铸与均热过程中的析出规律与行为。计算结果表明,连铸过程中AlN在凝固后的高温α相中便可能析出,而MnS仅可能在凝固后的α+γ两相区内析出。钢中AlN与MnS在均热过程中均处于部分固溶与部分析出的状态。后续高温渗氮处理后初次晶粒的异常长大并不明显,表明渗氮处理前钢中固有抑制剂的数量相对充足。 The precipitation behavior of MnS and AlN in low-temperature high magnetic induction grain-oriented silicon steel produced by thin slab casting and rolling process with\"acquired inhibitor method\"during continuous casting and soaking was studied by thermodynamic calculation.The calculated results show that AlN is likely to precipitate in ferrite after solidification.However,MnS can precipitate only in the two phase region of ferrite and austenite.Meanwhile,MnS and AlN in the steel can not be comp...
薄板坯连铸连轧流程试制含钒钛取向硅钢中氮化物析出相
通过热力学计算与模拟试验研究了含钒钛取向硅钢中氮化物析出相的析出规律与析出行为,并探讨了含钒钛元素的氮化物析出相作为薄板坯连铸连轧流程制备取向硅钢中辅助抑制剂的可行性.研究表明,在所冶炼的含钒钛取向硅钢的成分范围内,Ti N在钢液凝固末期便具备析出的热力学条件,而Al N与VN只可能在凝固后的α+γ或α+Fe3C两相区内析出.含钒钛取向硅钢中氮化物析出相以成分复杂的复合析出相为主,且随着钒钛加入量的增加,钢中抑制剂析出相总的分布密度由于含钒钛元素的氮化物析出相的增加而明显提高,使抑制剂抑制初次再结晶晶粒正常长大的能力得以加强,最终成品的磁感应强度值B8由1.857 T提升至1.898 T.同时,加入不高于0.007%的Ti与不高于0.005%的V不会影响中间脱碳退火工序的脱碳效果以及高温退火净化阶段硫、氮的脱除效果,其形成的含钒钛元素的纳米级氮化物析出相适合作为薄板坯连铸连轧流程制备取向硅钢的辅助抑制剂. The precipitation behavior of nitride precipitates in grain-oriented silicon steel containing vanadium and titanium elements produced by thin slab casting and rolling process was studied by thermodynamic calculation and simulation experiment. The feasibility of nitride precipitates containing V and Ti elements as auxiliary inhibitors was also investigated. It is found that Ti N is likely to precipitate at the final stage of solidification in the grain-oriented silicon steel,but VN and Al N can p...
无取向硅钢表面环保涂层的发展
简述了无取向硅钢环保涂层发展背景,分析了硅钢环保涂层的特点及国内、外研究进展,提出了硅钢保涂层下一步的发展方向。 The back ground of environmental protection coating of non-oriented silicon steel was described in this paper.The characteristics and study progress in domestic and foreign of environmental protection coating of non-oriented silicon steel were analysised.The next development direction of environmental protection coating of non-oriented silicon steel was put forward.
CN202023331940.9硅钢片卷材加工用张力机构以及硅钢片剪切机
本实用新型公开了硅钢片卷材加工用张力机构以及硅钢片剪切机,包括安装架、转动装置和按压装置,安装架的上安装块、连接块和下安装块组成凹槽,转动装置包括下转轴和转动驱动单元,下转轴水平设置,可转动地安装于下安装块上,设置于凹槽中,按压装置包括有上转轴和按压驱动单元,上转轴水平设置于下转轴的上方,可转动地安装于上安装块上,设置于凹槽中,并且可沿上安装块上下运动,其中,上转轴可与下转轴抵接。根据本实用新型的硅钢片卷材加工用张力机构以及硅钢片剪切机,可加强硅钢片卷材输送过程中的张力,降低硅钢片卷材输送的位置偏差率,提高产品合格率,提高原材料利用率,从而提高生产效率。
压下率对6.5%Si电工钢温轧板织构的影响规律
6.5%Si电工钢是一种优异的软磁材料,织构对其磁性能影响很大。利用温轧工艺对6.5%Si电工钢热轧板进行不同压下率轧制,研究了温轧板织构随压下率的变化规律。实验结果显示,随着压下率的增大,{100}〈110〉、{110}〈100〉和γ纤维织构在薄板表层中的强度先增强后减弱,当压下率达到75%时,沿板厚方向形成3个组织区域:表层细晶粒区({110}〈100〉取向为主)、过渡层({111}〈110〉和{111}〈112〉变形晶粒区)和中心层(以拉长的γ纤维织构和{100}〈110〉取向晶粒为主),这种组织和织构不均性对后期织构的发展有重大影响。 6.5wt% Si electric steel has excellent soft magnetic properties,on which texture play important role.In this experiment,warm rolling technique was employed to investigate the effect of rolling reduction on texture.It was found that the density of {100}〈110〉,{110}〈100〉 and γ-fiber textures first increased and then decreased with increasing of the rolling reduction.At 75% reduction,the microstructure along the thickness of the sheet formed three zones,containing surface layer with {110}〈100〉 orien...
CN202111457976.8一种超低碳含钇取向硅钢及其制备方法
本发明的一种超低碳含钇取向硅钢及其制备方法,化学组成及质量百分比为Si:2.0~4.5%,C:≤0.003%,Y:0.001~0.1%,Mn:0.1~0.25%,Al:0.01~0.02%,Cu:0~0.3%,S:0.02~0.035%,N:0.009~0.011%,其余为Fe和不可避免的杂质元素。生产工艺为:连铸、铸坯加热、热轧、常化、冷轧、初次再结晶退火、二次再结晶退火。本发明采用超低碳的成分,取消了常规取向硅钢脱碳退火工艺,简化了生产流程。通过稀土微合金化解决了因超低碳成分导致的单向铁素体组织抑制剂析出困难的技术难题。本发明制备的含钇取向硅钢厚度为0.2~0.35mm,磁感应强度B8为1.85~1.94T,铁损P17/50为0.9~1.2W/kg,可以用于变压器的铁芯材料,制备流程更为简洁。
CN202110047416.9可替代高磁感取向硅钢常化退火的热处理方法
本发明公开了一种可替代高磁感取向硅钢常化退火的热处理方法。该方法包括对所述取向硅钢的铸坯依次进行热轧、酸洗和冷轧,省去了常化酸洗工序中的常化退火工艺。所述热轧工序包括加热、粗轧和精轧过程,所述精轧过程中,热轧板离开精轧机最后一个机架时的温度达到1000~1050℃;或者,所述酸洗工序后,对热轧板进行通电加热至1000~1050℃;然后,对热轧板采用短时通电加热控制冷却速度,通电加热2‑5s使热轧板的温度降至940~960℃。采用该热处理方法得到高磁感取向硅钢常化板等效织构,满足生产高磁感取向硅钢的织构组分条件,其简化了高磁感取向硅钢的制造工艺,降低了生产成本和能耗,提高了生产效率。