钢厂
退火温度和时间对用电沉积法制备的高硅钢性能的影响
研究了退火温度和退火时间对电沉积硅钢试样中的断面层组织、硅在试样中的分布情况、织构分布和磁性能的影响。结果表明:退火温度为1000℃、退火时间为210 min时得到的试样晶粒分布均匀、硅在试样中分布均匀、硅平均浓度为6.3715%(接近6.5%)。试样的织构分析及磁性能检测的结果表明,在较高温度下延长退火时间可增加{100}和{110}面织构,降低铁损,所得试样的磁性能较为良好。 The effect of annealing temperature and time on the microstructure, distribution of silicon,texture and magnetism of the high silicon steel prepared by electrodeposition was investigated. The results showed that after annealing at 1000℃ for 210 min, the mean grain size of steel was about 190 μm with a uniform grain size distribution, and the silicon is also uniformly distributed on the entire cross section with an average Si concentration 6.3715%(close to 6.5%); With the increasing annealing tim...
资源节约型高强度电工钢SXRC的开发
日本住友金属成功地开发了一种资源节约型高强度无取向电工钢SXRC,这种电工钢是通过固溶铌适度抑制位错的合并对消而得到一种特殊的微观组织,因此兼具很高的力学性能和磁性,特别适用于HEV、EV驱动电机转子。而且,不使用昂贵的镍就可以达到期望的强度,合金成本可控,是一种优越的资源节约型产品。 Sumitomo metal industries ltd of Japan successfully developed a type of high strength non-orientation electrical steel SXRC of resources-saving.The steel has both high mechanical performance and good magnetic property thanks to the special microstructure produced by the formation of Nb solid solution serving to appropriately inhibit the combination and cancellation of dislocations.The material is,in particular,suitable for manufacturing rotors of HEV and EV driving motors.Besides,expected streng...
CN202111195012.0高硅无取向电工钢及其生产方法
本发明揭示了一种高硅无取向电工钢及其生产方法。该方法包括:1)钢水冶炼并连铸成坯;2)加热并保温,之后热轧得到热轧卷板,其中粗轧出口温度940±20℃,精轧终轧温度840±20℃,卷取温度650±20℃;3)常化,常化温度((732~742)+3000[Si])℃,常化时长4min~5min;4)常化后直接进行冷轧,而后连续退火和涂层,退火温度940℃~990℃且退火时长1.5min~3min;5)涂层处理后的钢板加工成型,而后进行去应力退火,退火温度为((761~766)+3000[Si])℃。如此,在保证磁性能的同时,解决了冷轧难度大的问题。
CN202110591803.9一种用于取向硅钢的无铬无机绝缘涂料及其制备方法
本发明属于涂料技术领域,具体公开了一种用于取向硅钢的无铬无机绝缘涂料,包括以下重量份配比的原料:小颗粒硅溶胶10‑50份、大颗粒硅溶胶10‑50份、磷酸二氢铝溶液5‑50份、助剂0.1‑10份及水10‑100份。本发明还提供了一种用于取向硅钢的无铬无机绝缘涂料的制备方法,通过将小颗粒硅溶胶和大颗粒硅溶胶混合均匀成硅溶胶混合液后加水得到混合硅溶胶水溶液;再依次向其中加入磷酸二氢铝和助剂并持续拌至均匀,得到用于取向硅钢的无铬无机绝缘涂料。本发明提供的无铬无机绝缘涂料适用于取向硅钢,使取向硅钢环保无害的同时具有与含铬取向硅钢相当的耐腐蚀时效,从而实现取向硅钢产业绿色化并大大改善取向硅钢的综合性能。
Al含量对2.2%Si无取向硅钢组织、织构和磁性能的影响
通过实验室25 kg真空感应炉冶炼和锻轧研究了0.26%~0.95%Al含量对0.5 mm 2.2%Si无取向硅钢冷轧板组织、织构和磁性能的影响。试验结果表明,0.26%~0.81%Al含量时,随钢中Al含量的增加,成品退火钢板的晶粒尺寸增加同时铁损减少;当Al含量大于0.81%时,随Al含量增加,钢板的晶粒尺寸减小,同时铁损增加。Al含量对硅钢板磁感的影响没有明显的规律。2.2%Si无取向硅钢的合适Al含量为0.48%~0.81%。 The effect of 0.26%~0.95%Al content on structure,texture and magnetic performance of 0.5 mm cold rolled sheet of 2.2%Si non-oriented silicon steel has been studied by a 25 kg vacuum induction furnace smelting,and forging -rolling in laboratory.Results show that as 0.26%~0.81%Al,with increasing Al content in steel the grain size of annealed finished sheet increases while iron loss of sheet decreases,and as Al content in steel is more than 0.81%,the grain size of sheet decreases while iron loss in...
CN202123246747.X一种变压器铁芯硅钢片叠装平台
本实用新型公开了一种变压器铁芯硅钢片叠装平台,包括支撑架、升降装置、铁芯架和硅钢片支撑板;铁芯架为硅钢片叠放形成铁芯的作业架,硅钢片支撑板用于储放构成铁芯的硅钢片,铁芯架及硅钢片支撑板均通过升降装置活动设置于支撑架上,且在叠装作业过程中,铁芯架与硅钢片支撑板通过升降装置驱动同时升降。本实用新型提供的一种变压器铁芯硅钢片叠装平台,提高铁芯叠装作业的便捷性,降低劳动强度,提高效率。
CN202180052321.4取向性电磁钢板的制造方法
本发明的取向性电磁钢板的制造方法能够稳定地制造被膜特性和磁特性优异的取向性电磁钢板。其包括:对含有规定的添加元素的钢坯进行热轧;冷轧制成最终板厚;进行脱碳退火;涂布以MgO为主剂的退火分离剂;进行最终退火,其中,上述退火分离剂的主剂的BET比表面积比率H2O/N2为0.6~1.6且浆料状态下粒径40μm以上的粒子的比例为5质量%以下。
CN202110023277.6一种无取向电工钢用绝缘涂液
本发明涉及一种无取向电工钢片绝缘涂液,它的主要有效成分包括有机树脂、水溶性磷酸二氢盐、硅溶胶、涂料助剂、和特定水溶性金属盐。上述各组分的质量组成比例为:有机树脂100份,水溶性磷酸二氢盐100‑250份,硅溶胶0‑100份、涂料助剂0‑20份,特定水溶性金属盐10‑50份,其余为水,涂液的固含量为15~40%。其中特定水溶性金属盐是指水溶性磷酸二氢盐以外的二价或多价金属盐,这种盐可以在磷酸二氢盐溶液中稳定存在,但是在电工钢涂层烧结温区会氧化或分解。本发明的绝缘涂液固化速度快且固化彻底,涂层具有优异的耐盐雾性能。
CN202120757212.X一种用于激光切割的铁芯硅钢片夹持装置
本实用新型公开了一种用于激光切割的铁芯硅钢片夹持装置,包括固定座,所述固定座的上方设置有底板,所述底板的上方设置有压板,所述压板与底板的内部且靠近前后侧边缘处均活动连接有转动辊,所述转动辊的表面活动连接有输送带,所述固定座的表面开设有排料口,所述底板的上表面开设有泄料口,所述压板的上表面开设有加工预留口,所述压板的内部且位于转动辊之间固定连接有转轴,所述转轴的表面固定连接有从动锥齿轮,所述压板的内部且靠近左侧边缘处固定连接有电机,所述电机的输出端固定连接有转动杆。本实用新型,该装置结构简单合理,能很好地解决现有技术的不足,能实现在夹持的时候进行送料工作,有利于提高硅钢片的加工效率。
CN202110137389.4一种强磁性取向高硅钢极薄带及其制备方法
本发明提供了一种强磁性取向高硅钢极薄带及其制备方法,属于电工钢制造领域,所述强磁性取向高硅钢极薄带包括以下质量百分比的元素:C:0.0045%~0.0060%、Si:4.5%~5.0%、Mn:0.23%~0.32%、S:0.02%~0.03%、Bi:0.03%~0.08%、Als:0.027%~0.035%、Cu:0.02%~0.03%,N:0.008%~0.010%,P<0.005%,其余为铁,其中所述Cu、S、N元素在熔炼时以含硫氮和铜的多核配位化合物的方式加入所述高硅钢;本发明通过对取向高硅钢的原料组分进行设计,采用含硫氮和铜的多核配位化合物和Bi元素作为合金抑制剂,所制得的强磁性取向高硅钢极薄带晶粒细小,组织均匀,具有高磁感应强度,低铁损的优良磁性能。