研究了CSP工艺生产≤0.005%C-1.1%Si的2.2mm无取向电工钢热轧板在800~1000℃常化对0.5mm冷轧板840℃退火后组织和磁性能的影响。结果表明,热轧板常化温度升高,冷轧板退火后的再结晶晶粒增大,铁损降低,磁感增加;热轧板常化温度超过900℃,因第二相固溶而后弥散析出,退火后冷轧晶粒细化,铁损增加,因此该无取向电工钢热轧板最佳常化温度为900℃。 The effect of normalizing at 800-1000℃ of CSP produced plate(≤0.005%C-1.1%Si) on the microstructure and magnetic properties of downstream cold-rolled non-oriented electrical steel annealed at 840℃ was studied.Results show that with increasing normalizing temperature of hot-rolled material the recrystallized grain size of annealed sheet increases,iron loss reduced and magnetic induction increases.As normalizing temperature excesses 900℃,grain is refined and iron loss increases after annealing due... 
2012-03-28 144 5.8

本实用新型公开了一种硅钢炉底辊套管生产用专用夹具,包括工作台,所述工作台的顶端表面设置有旋转云台,所述旋转云台的顶端表面设置有固定柱,所述固定柱通过转轴安装有固定杆,且转轴的端部通过联轴器安装有第一电机,所述固定杆的端部通过转轴转动连接有安装杆,所述转轴的端部通过联轴器安装有第二电机。本实用新型中,通过旋转云台、固定柱、第一电机、固定杆、第二电机、安装杆、第三电机、连接杆和机械爪的相互配合使用下,实现了对炉底辊套管的全自动夹取,有效的降低现场工作人员的劳动负荷,避免操作人员通过夹具在夹取可能出现的意外事件,极大的提高了夹取效率。
2021-10-13 138 6.8

本实用新型公开了一种变压器铁芯硅钢片叠装对齐工装,包括叠装平台、定位板、推齐板和下压板;定位板和推齐板分别位于叠装平台的两侧,下压板位于叠装平台的上方;定位板用于对铁芯长度或宽度侧进行定位;推齐板平推铁芯使各硅钢片抵靠定位板而对齐;下压板下压铁芯使各硅钢片叠装紧密。本实用新型提供的一种变压器铁芯硅钢片叠装对齐工装,能够提高铁芯生产精度,并提高硅钢片叠装效率。
2021-12-22 238 6.8

针对本钢薄板坯铸机在生产无取向电工硅钢的过程中存在的铸坯拉断、中包增碳、增氮等问题,进行了连铸工艺优化。通过采用新型无碳中间包覆盖剂、环保中间包干式料及专用结晶器保护渣后,降低了铸坯增碳量;通过控制钢包到中间包的增氮环节,降低钢水增氮;适当增大二冷水量,控制钢水过热度,防止铸坯拉断等生产事故的发生。改进工艺后,精炼后到成品铸坯的平均增碳量能控制在10×10-6以内,平均增氮量能控制在4×10-6以内。 The technology optimization has been adopted for preventing nitrogen increasing and carbon increasing in Benxi thin slab producing non-oriented silicon steel.Measures accordingly were adopted and satisfactory results were achieved. 
2011-05-28 178 5.8

本发明是改善硅钢边缘裂边的工艺,包括:S1:对普通取向硅钢卷进行放卷、活套、清洗、加热、冷却;S2:对硅钢进行收卷,收卷张力系数为3‑9kg/mm2;S3:对硅钢卷用收紧带收紧打包,打包带张力为3‑8kg;S4:罩式炉进行炉底板检测,炉底板不平度<2mm;S5:将收紧打包后的硅钢卷送入罩式炉内进行高温退火处理;本发明的优点:通过调整取向硅钢材料生产过程中对CA线收卷张力的控制、CA收紧带的使用与控制、罩式炉炉底板的平整度,实现1200mm以上宽度材料平均不良切边宽度≤45mm,边部裂边尺寸减少40%。有效提高了加工材料成材率,提高了纵剪材料使用率,降低了吨钢成本,减少了纵剪生产停顿,提高了效率。
2021-04-23 149 6.8

对硅钢板材分别进行异步和同步轧制,研究了轧制参数包括速比、压下量和道次对板材表面显微组织的演变的作用.结果表明,异步轧制硅钢板材表面形成了晶粒尺寸为10~50 nm,取向接近随机分布的纳米晶,而同步轧制板材的表面只形成了位错胞,证明异步轧制可以诱发表面纳米化.异步轧制板材表面纳米晶的形成过程为:在剪切力的反复作用下,高密度位错形成、滑移、湮灭和重组形成亚微米尺度的亚微晶/位错胞.随着压下量和轧制道次增加,高密度位错重复以上过程使晶粒尺寸减小、取向差增大,最终形成取向接近随机分布的纳米晶组织.大压下量和多道次是异步轧制诱发板材表面纳米化的关键,而速比的增加可以加快纳米化进程. Surface nanocrystallization(SNC) can effectively enhance the surface and global properties of the metallic materials,such as microhardness,intensity,fatigue,wear and corrosion resistances,therefore provides more promising practical industrial applicability.Up to now,several SNC treatment methods were developed based either on the principles of ball impactions or friction sliding,however,difficulty still exists for the surface treatment of large-dimensional samples with high efficiency.Recently,m... 
2014-09-28 194 5.8

本实用新型公开了一种变压器铁芯硅钢片的堆叠装置,包括底座、摆动机构、摆动板和垫高倾板,所述底座上设置有摆动机构,所述摆动板的一端铰接设置在底座上,且所述摆动板间距于摆动轴线的板体与摆动机构对应设置,所述摆动机构驱动摆动板在竖向面内进行往复摆动,所述垫高倾板间距于摆动板设置在底座上,且所述垫高倾板与摆动板之间构成用于叠放硅钢片的叠放区,所述叠放区的底部呈高低倾斜设置,且所述叠放区的低端侧朝向于摆动板,能够使得硅钢片的收集简单,且十分整齐。
2021-12-30 298 6.8

作为一种具有优异高频铁磁性能的合金,Fe-6.5%Si(质量分数)高硅钢在高频工况条件下降损效果明显,对电气行业应用器件高频化、小型化、节能等具有十分重要的意义。通过与取向硅钢测量B-P数据对比,验证了高硅钢高频超低损特性,且轧制高硅钢与日本CVD法生产高硅钢存在基本相同的铁损值。采用国标Epstein Square法对0.30mm高硅钢薄板进行单片测试,并对由0.30mm高硅钢薄板首次装配成的电感器进行铁损测试,对比测试结果表明,元件测试与单片测试数据基本吻合,高磁感应强度条件下,元件测试结果略低于单片测试,分析原因为:线圈引起励磁压降;元件叠片间出现短路,电流增大,损耗增加;气隙板厚度过大。 As one core material with excellent high-frequency ferromagnetism,Fe-6.5%Si performs obviously reduction on core loss in high field frequency which means much to high frequency,minimization,energy conservation in electric industry.Super low loss was verified by drawing B-P curves based on detected experimental data,and which went equal to Fe-6.5%Si thin strip fabricated by CVD in Japan.Fe-6.5%Si was firstly fabricated as inductor in this research,and its core loss was determined for comparison w... 
2023-05-09 204 5.8

本实用新型属于冷轧硅钢技术领域的一种冷轧硅钢无压回水自动控制设备,包括底座,底座外表面的上端固定连接有工作台,工作台外表面上端的两侧分别固定连接有固定柱和压辊主体,工作台外表面上端的中部滑动连接有移动架,压辊主体的下端设置有集水槽,集水槽的内表面设置有浮球液位传感器。液压杆工作推动移动架位移到合适的位置,再通过气缸使伸缩管发生位移,使出水口接近钢板,设置的水箱高于出水口所以水可以在重力的作用下流淌,流出的水流到集水槽内,水流在集水槽内聚集,水流使浮球液位传感器的浮球上升,上升到合适的位置时,浮球液位传感器通过电缆发生电信号至控制器,此设置可以实现设备的自动控制,省去人工进行操作。
2021-11-29 169 6.8

本实用新型涉及变压器铁芯装配技术领域,具体公开了一种硅钢片铁芯的装配工装,包括底座、对称设于底座上的两个承压条以及快速装夹机构;所述快速装夹机构包括设于两个承压条一侧的安装框架、安装于安装框架两侧的侧挡板、紧固组件以及将安装框架和承压条之间定位的卡接组件;所述卡接组件包括安装于安装框架一侧的定位块、以及开设于承压条一侧的定位槽,所述定位块的内部开设有安装槽,本实用新型通过快速装夹机构能够实现安装框架的快速定位,从而便于安装框架的安装,有效的提高了安装框架的拆装效率,有助于硅钢片铁芯的快速装配,可提高硅钢片铁芯的装配效率,增加硅钢片铁芯的生产效益。
2021-09-09 180 6.8

站点公告

网站试运行,请大家关注本站公众号,多提宝贵意见!

显示验证码
没有账号?注册  忘记密码?