钢厂
CN202080089018.7取向电工钢板及其磁畴细化方法
根据本发明的一个实施例的取向电工钢板,其中存在于电工钢板表面的沟槽以及与沟槽底部相连的再结晶和其他再结晶的平均取向度差为0.5°至10°。
硅钢氧化镁的制备进展
介绍了硅钢氧化镁制备方法及高质量硅钢氧化镁制备技术的研究进展,并对利用我国丰富的卤水资源制备硅钢氧化镁进行了展望。 The preparation methods of silicon steel magnesium oxide and research progress of high quality silicon steel magnesium oxide preparation technology were introduced.The use of abundant brine resources in the preparation of silicon steel magnesium oxide was prospected.
CN202111200887.5一种改善表面麻点缺陷的薄规格中低牌号无取向硅钢及其生产方法
本发明提供一种改善表面麻点缺陷的薄规格中低牌号无取向硅钢及其生产方法,成分C≤0.0025%,1.2≤Si≤1.65%,0.25%≤Mn≤0.35%,0.06%≤P≤0.11%,0.1%≤Als≤0.2%,S≤0.0025%、N≤0.0025%,Ti≤0.0025%,其余为Fe及不可避免的杂质。与现有技术相比,本发明采用较低氢气浓度,防止炉内氧化铁皮还原,减轻碳套辊的腐蚀程度,减少碳套辊结瘤率,改善带钢表面质量;采用合理合金成分设计,提高带钢的力学强度,降低碳套辊结瘤对带钢表面的影响程度,改善带钢表面质量。产品厚度为0.35mm,板面麻点发生率降低,无手感,且辊身周长周期范围内麻点个数≤5个。
双辊连铸3%Si无取向硅钢铸带特征
针对传统工艺生产硅钢周期长、能耗大等缺点,采用双辊连铸工艺制备3%Si无取向硅钢连铸薄带,利用MEM,SEM和TEM观察了铸带的组织、织构及析出物,同时对比了Al的质量分数为0.6%和0.9%的连铸薄带在组织、织构及析出物特征方面的异同.结果表明:双辊连铸工艺生产的3%Si无取向硅钢铸带的组织为均匀等轴晶粒,平均晶粒尺寸约为300μm;织构组成随Al质量分数的不同具有明显差别,Al质量分数为0.9%的铸带中{100}织构强度是随机织构的7倍;铸带中的析出物为AlN和MnS,最大尺寸分别为500和50 nm左右. Given the lengthy production cycle,high energy consumption,and other shortcomings of the traditional process for producing silicon steel,a twin-roll casting process was used to produce 3%Si non-oriented silicon steel casting strips. MEM,SEM,and TEM were used to compare micro-structure,texture,and precipitate characteristics of a casting strip containing 0.6%Al with another containing 0.9%Al.The structure of 3%Si non-oriented silicon steel produced by the twin-roll casting process was a uniform i...
无取向硅钢铬酸镁绝缘涂层高温固化工艺
为了确保硅钢铬酸盐涂料的环保性,需要严格控制涂料的固化工艺,保证涂料固化过程中涂料中的六价铬充分转化为三价铬。对涂料及原料进行热重分析(TG)及差示扫描量热法分析(DSC)。结果表明,MgO与铬酐混合转化为MgCrO4,使六价铬稳定性增强,其中大部分Cr6+转变为Cr3+发生在620~700℃,在450~500℃高于铬酐发生大量失重,因此必须加入还原剂保证涂料中六价铬被充分还原;超过360℃后树脂会发生分解,因此实际板温不能超过360℃;加入了还原剂的整体涂料的失重温度区间主要在260~320℃,因此涂料固化时钢板的实际温度最佳区间为320~360℃。 Because of the silicon steel chromate coating’s environmental requirements,the paint curing process must be controlled strictly to ensure all Cr( Ⅵ) transforms to Cr( Ⅲ). The TG and DSC analyses of the paint are studied. The reaction of MgO and CrO3 would generate MgCrO4,enhancing the stability of Cr( Ⅵ). The most r( Ⅵ) in MgCrO4 changes to Cr( Ⅲ) at 620-700 ℃,while the CrO3 has a large weight loss at 450-500 ℃. The reductant must be added in the paint to make sure the Cr( Ⅵ) could transform suf...
电工钢反复弯曲试验的影响因素
电工钢反复弯曲次数是电工钢性能检验的重要指标之一,直接影响到用户在使用电工钢过程的机加工性能。主要分析了试样宽度、试样张力、晶粒取向、反复弯曲设备等因素对电工钢反复弯曲试验的影响,并对各个因素的影响程度进行量化以及原因探讨,从而归纳形成各影响因素的基本规律,以便为电工钢实际生产、用户使用提供科学指导。结果表明:试样宽度增加,反复弯曲次数也会不断增加,晶粒位向对取向电工钢的反复弯曲次数影响较大,当支座顶部到拨杆底部的距离减小或拉紧力增加时,反复弯曲次数会不断减小,但当拉紧力达到60N以上时,对反复弯曲次数影响不大,试样经退火后,反复弯曲次数略有上升。 The reverse bend number is an important performance of electrical steels′capabilities,affecting the machining performance directly when the customers used.It investigated some factors,such as sample′s width,sample′s tension load,grain orientation and equipment,how to effect the reverse bend test for electrical steel,measured the influence degree,and discussed the reason,in order to form basic rules which could be guided the manufacturing and using for electrical steel.Results showed that the rev...
无取向电工钢RH脱硫渣系的研究
在15 kg真空感应炉上,用CaO-Al2O3-SiO2-MgO渣系进行脱硫试验,探讨了脱硫渣系碱度、MI、Al2O3、CaF2对脱硫效果的影响。研究结果表明,随脱硫渣系碱度、MI、Al2O3和CaF2含量的增加,脱硫率都呈现先增加后减少的趋势。初始硫含量为0.009 33%~0.010 73%,加入脱硫渣系4 min时间内表观脱硫速率为(0.000 96~0.001 49)%/min,平均脱硫率为81.2%,最高达86.8%。当脱硫渣中w(CaO)=58.15%、w(SiO2)=4.85%、w(Al2O3)=25%、w(MgO)=6%、w(CaF2)=6%,脱硫效果最好,此时钢液中硫为0.001 33%。 Experiments on desulfurization of molten steel using CaO-Al2O3-SiO2-MgO based desulfurization slag was carried out in a 15 kg vacuum induction furnace. The effects of desulfurization slag basicity,MI, Al2O3and CaF2on desulfurization of molten steel were studied. The results show that with the increase of basicity,MI,Al2O3or CaF2in desulfurization slag,the desulfurization rate rises initially and then decreases. In addition,as the initial sulfur content is 0. 009 33% ~ 0. 010 73%,the apparent des...
取向电工钢加工过程中第二相粒子的析出行为
利用场发射扫描电镜观察了以MnS为主要抑制剂的普通取向电工钢加工过程中第二相粒子的分布状态,统计了粒子面密度、平均尺寸以及相应的尺寸分布.结果显示,热轧加工造成了大量第二相粒子弥散、细小地析出,同时基体仍保持过饱和状态.冷轧变形会造成第二相粒子的回溶行为,而基体的过饱和状态会减弱回溶现象.中间退火与脱碳退火过程中会同时存在新粒子的形核及已析出粒子的粗化两个过程,而在最终二次再结晶升温阶段则以第二相粒子明显粗化为主. The distribution of second phase particles in conventional grain-oriented electrical steels during manufacturing processes with MnS as inhibitors was observed by field emission scanning electron microscopy,while the areal particle density,the average particle size and the corresponding size distribution were statistically determined.It is indicated that hot rolling leads to dispersive precipitation of a large amount of fine second phase particles and the matrix keeps a supersaturated state furth...
CN202110778749.9硅钢产品生产方案的智能设计评估方法
本发明公开了一种硅钢产品生产方案的智能设计评估方法,包括以下步骤:1、采集数据,并集成用户数据、实验室研发数据和大生产数据;2、构建用户数据主题、实验室研发数据主题和大生产数据主题;3、输入硅钢产品的种类、规格和性能需求的需求信息,并根据需求信息生成若干个硅钢产品的生产方案,生产方案包括优化产品的生产方案和新产品的生产方案;4、多维度综合评估步骤3中生成的每个硅钢产品的生产方案,得到硅钢产品生产方案的绿色设计指数,并根据绿色设计指数推荐生产方案。本发明基于产品设计需求,融合实验研发数据和大生产数据,生成并评估产品设计方案模型,缩短研发周期,提高研发效率。
卷取工艺对新型冷轧无取向电工钢组织性能的影响
研究了卷取工艺对一种新型含铜无取向电工钢晶粒尺寸、织构演变、铁损和磁感应强度的影响。结果表明,试样织构组分主要为{111}、{112}、{100}和高斯织构,在550℃卷取、保温2~3h,{100}织构有增强趋势,磁感应强度较高,铁损较低。 The effects of coiling process on grain size,texture,core loss and magnetic induction of a new cold rolled non-oriented electrical steel with copper were investigated.The results show that there are mainly {111},{112},{100} and {110}<001> texture.Coiling at 550℃and keeping for 2~3 hours,the {100} texture is enhanced,magnetic induction is higher and core loss is lower.
CN202110667000.7一种用于风力发电机定子铁芯扇形硅钢片的保护工装
本发明公开了一种用于风力发电机定子铁芯扇形硅钢片的保护工装,包括第一防护罩和第二防护罩,第一防护罩、第二防护罩均为扇形罩体,其由弧形底板和两个扇形侧板构成,第一防护罩的两端连接有能够折叠收纳的柔性罩;第一防护罩滑动套设在扇形硅钢的外侧,第二防护罩滑动套设在第一防护罩的外侧。本发明提供的保护工装主要有两个功能,当扇形硅钢片处于运输过程中时,利用第一防护罩、第二防护罩、柔性罩协同配合为其防刮伤防护;当扇形硅钢片装配后,利用第一防护罩内部的冷却散热系统提供散热防护,防止出现高温过热现象;通过这种方式,本发明保护工装满足大规格定子铁芯扇形硅钢片的防护需求。