钢厂
低牌号无取向电工钢磁时效行为分析
选取了三种50W 800无取向电工钢,分析了化学成分、晶粒尺寸、织构、以及200℃时效处理48 h前后的磁性能和第二相粒子析出状态的变化。结果表明,钢板中第二相粒子的分布密度对钢板铁损有最重要的影响。降低钢中C、N元素含量,或改进钢板热加工参数以降低成品钢板中第二相粒子形成元素的过饱和度均有利于明显降低钢板磁时效过程中的铁损增幅。钢板中对磁性能有利的织构也有利于降低钢板铁损的时效幅度。 The evolution of chemical composition,grain size,texture,as well as magnetic property after aging treatment at 200 ℃ for 48 h and distribution of second phase particles precipitation in three selected 50W800 non-oriented electrical steels were analyzed.The results show that the distribution density of second phase particles has great influence on core loss.Reducing C and N content,or improving hot-working parameters to reduce the supersaturation of elements forming second phase particles in prod...
CN202123098360.4一种铁芯硅钢片卷料的上料装置
本实用新型公开了一种铁芯硅钢片卷料的上料装置,包括升降机构、固定座、转动执行机构和转动平台,所述固定座固定设置在地面上,所述升降机构相邻设置在固定座的一侧,所述固定座对立于升降机构的一侧设置有转动平台,所述转动平台的一端铰接设置在固定座上,且所述转动平台的另一端为自由端,所述转动平台在竖向面内朝向或远离于升降机构偏转,所述固定座上设置有转动执行机构,所述转动执行机构驱动转动平台转动;所述转动平台上的物料通过转动可位移至固定座和升降机构上,能够安全的、快速的将卷料转移至升降机构上,从而便于上料。
CN202123248776.X一种变压器铁芯硅钢片叠装对齐工装
本实用新型公开了一种变压器铁芯硅钢片叠装对齐工装,包括叠装平台、定位板、推齐板和下压板;定位板和推齐板分别位于叠装平台的两侧,下压板位于叠装平台的上方;定位板用于对铁芯长度或宽度侧进行定位;推齐板平推铁芯使各硅钢片抵靠定位板而对齐;下压板下压铁芯使各硅钢片叠装紧密。本实用新型提供的一种变压器铁芯硅钢片叠装对齐工装,能够提高铁芯生产精度,并提高硅钢片叠装效率。
低铁损高磁通密度无取向硅钢的应用与生产技术进展
分析了高转矩和高转速条件下高效驱动马达铁芯材料对无取向硅钢磁性能要求,讨论了无取向硅钢的高磁通密度和低铁损对电机转矩和效率的影响,介绍了国内外高磁感无取向硅钢发展情况。在生产工艺上,提高钢质纯净度,弱化夹杂物和第二相粒子对畴壁移动和再结晶晶粒长大的钉扎作用,添加微量晶界和带钢表面的偏析元素促使有利织构发展等技术可提高无取向硅钢的磁通密度。 The requirements of high efficient drive motor core materials under the conditions of high torque and high speed were analyzed.The effects of high magnetic flux density of non-oriented silicon steel on the torque and efficiency of the motor were discussed.The development of non-oriented silicon steel with high magnetic was introduced.The magnetic flux density of non-oriented silicon steel sheet can be obviously improved by some production technologies,such as purification steel,weakening the pin...
CN202111652218.1一种高硅钢材料及其制备方法
一种高硅钢材料的制备方法,步骤包括靶材、金属基材表面清理;排除密闭容器内空气、通保护气;双辉光等离子预轰击靶材和基材,净化表面;等离子溅射、加热、保温;缓慢冷却取出。预轰击靶材、基材,去除表面吸附层、活化基材,交替升高基材电压、靶材电压,使靶材中的合金元素被离子轰击而溅射出来、扩散进入基材内部形成表面高硅钢层。“双辉光等离子表面冶金技术”制备高硅钢的工艺简单易行、可控性高、成本低、无污染且基体和表面的结合力高,适合大规模产业化生产;更重要的是该方法采用交替离子轰击、扩渗速度快,结合强度高,得到硅含量均匀分布或呈梯度分布的高硅钢材料,为制备更高品质的无噪音、低铁损的高硅钢产业化奠定基础。
无取向硅钢铬酸镁绝缘涂层高温固化工艺
为了确保硅钢铬酸盐涂料的环保性,需要严格控制涂料的固化工艺,保证涂料固化过程中涂料中的六价铬充分转化为三价铬。对涂料及原料进行热重分析(TG)及差示扫描量热法分析(DSC)。结果表明,MgO与铬酐混合转化为MgCrO4,使六价铬稳定性增强,其中大部分Cr6+转变为Cr3+发生在620~700℃,在450~500℃高于铬酐发生大量失重,因此必须加入还原剂保证涂料中六价铬被充分还原;超过360℃后树脂会发生分解,因此实际板温不能超过360℃;加入了还原剂的整体涂料的失重温度区间主要在260~320℃,因此涂料固化时钢板的实际温度最佳区间为320~360℃。 Because of the silicon steel chromate coating’s environmental requirements,the paint curing process must be controlled strictly to ensure all Cr( Ⅵ) transforms to Cr( Ⅲ). The TG and DSC analyses of the paint are studied. The reaction of MgO and CrO3 would generate MgCrO4,enhancing the stability of Cr( Ⅵ). The most r( Ⅵ) in MgCrO4 changes to Cr( Ⅲ) at 620-700 ℃,while the CrO3 has a large weight loss at 450-500 ℃. The reductant must be added in the paint to make sure the Cr( Ⅵ) could transform suf...
化学气相沉积法制备6.5%Si高硅钢的研究
采用化学气相沉积(CVD)渗硅处理工艺连续制备6.5%Si高硅钢,具有优质的软磁性能,通过理论研究化学反应并且用简单的试验设备做进一步的探讨。根据试验的结果对连续制备6.5%Si高硅钢的CVD工艺构造提出全面、有效的建议,实现制备6.5%Si高硅钢系统。 CVD method for continuously manufacturing 6.5%Si Steel Sheet has excellent soft magnetic.Carried out a theoretical study of related chemical reaction and performing basic research with a simple test apparatus.Based on the results,finally proposed an overall process configuration to realize such a production-CVD method for continuously manufacturing 6.5%Si Steel Sheet.
陶瓷辊除瘤方法在瑞致电工钢的应用
针对陶瓷辊表面结瘤清除时间长、清除效果差等缺陷,研究正反转陶瓷辊除瘤法,以缩短除瘤时间,增强除瘤效果。 The general removal of ceramic roller surface tumor costs a long time and the effect is poor.This paper probed into the ceramic roller tumor removal in order to shorten time and enhance the effect of eliminating.
CN202120876949.3一种变压器用硅钢片存放架
本实用新型公开了一种变压器用硅钢片存放架,其包括多个存放板座和多个支撑柱,多个存放板座依次呈上下间隔设置,在相邻两个存放板座之间设置若干支撑柱,支撑柱的上下两端分别与相邻两个存放板座可拆卸地连接,在存放板座四周的边沿设置有多个吊挂结构,存放架从下往上进行搭设过程中,硅钢片可依次从下往下依次叠放于多个存放板座上,提高存放量,降低存放占用的车间面积;在吊运时,从上往下依次把存放有硅钢片的存放板座吊起移动即可,实现硅钢片的快捷吊运,在不使用时或者运输时,可把支撑柱拆下,存放板座叠在一起进行存放收纳。本实用新型可应用于变压器硅钢片的存放吊运。
稀土处理无取向硅钢中的夹杂物与电磁性能变化
结合工业化生产的无取向硅钢,进行了RH精炼添加稀土合金实验。结果表明,1.15%(质量分数)Si钢的脱硫反应,主要发生在添加稀土合金之后的前5min。最佳的稀土合金添加量为0.6~0.9kg/t钢。钢液经过稀土处理后,加入的稀土总量越多,稀土氧硫化物夹杂物的尺寸就越大,但热轧带钢再结晶效果会逐渐变差,成品带钢晶粒尺寸先是快速长大,而后逐渐减小。最佳的钢中存留稀土含量与钢的化学成分有关,应严格控制在2.0×10-3%~6.0×10-3%(质量分数)。在此范围内,钢的铁损先是快速降低,而后缓慢升高,钢的磁感应强度则单调降低。 Based on the industrial production of non-oriented electrical steel,rare earth(RE) alloy treatment during the RH refining process was studied.The results showed that the effects of desulfurization and total concentration of RE remained in steel mainly depended on the chemical compositions of different steel grades.For 1.15wt% Si steel grade,the desulfurization reaction mainly focused on the initial 5min after RE alloy added during the RH refining process.The suitable RE alloy addition was 0.6-0....
基于GTN损伤模型对含边部缺陷硅钢薄板冷轧时边裂的预测
采用拉伸试验和显微组织观测的方法确定了GTN损伤模型中的9个损伤参数,运用GTN损伤模型对冷轧硅钢薄板边部缺陷的扩展及边裂的产生进行了有限元模拟,并与预置缺口的钢板轧制试验进行对比。结果表明:轧制过程中边部缺陷是造成钢板边部裂纹萌生和扩展的一个重要原因,GTN损伤模型可用来预测含边部缺陷硅钢薄板在冷轧过程中边裂的产生;预测结果与试验结果基本一致。 The crack initiation and propagation of silicon steel strip with edge defect during cold rolling process was studied by using GTN damage model in this paper.Nine damage parameters in GTN model were identified by tensile testing and microstructure observing,and then the FE simulation of edge defect evolution of silicon steel strip during rolling process was conducted on the base of GTN damage model,and then the results were compared with rolling experimental results.The results show that the edge...
CN202123186405.3一种硅钢铁芯生产用多功能卷绕机
本申请实施例公开了一种硅钢铁芯生产用多功能卷绕机,包括平台板,所述平台板底部的左侧固定连接有旋转电机,所述旋转电机的输出端固定连接有旋转杆,所述旋转杆的顶部固定连接有转盘,所述转盘的顶部固定连接有铁芯型模,所述铁芯型模的外表面活动连接有限定座,所述平台板顶部中心的左侧固定连接有第一U型板。第一弹簧和升降板的配合使用,可以让使用者下压升降板,使得升降板带动安装杆进行向下移动,继而使得安装杆脱离第二U型板所开设的轴槽,继而使得安装杆的顶部存在一定的间隙,进而可以通过间隙将带盘插入在安装杆上,该方式装卸起来简单快捷,可以有效的减少装卸带盘所消耗的时间,从而提高了设备的工作效率。