钢厂
无取向电工钢HW600高温变形抗力的研究
在Gleeble-3500热/力模拟试验机上对HW600钢进行高温压缩试验,研究在不同试验条件下的变形抗力。试验结果表明:变形温度对变形抗力的影响最为显著,在相同的变形速率下,随着变形温度的升高,变形抗力降低;在同一变形温度下,变形速率增大,变形抗力增加;在同一变形温度、变形速率下,随着变形程度的增加,变形抗力急剧增大,真应变达到0.1后,变形抗力增加趋势变缓。 The high-temperature compression test is done for HW600 steel with Gleeble-3500 thermal simulation testing machine to research its resistance to deformation under different test conditions.It is showed from result that deformation temperature has greatest effect on the resistance,and along with the temperature getting higher the resistance lowered under same deformation rate;the resistance increases along with deformation rate getting greater under same temperature;and under same deformation tem...
CN202123098360.4一种铁芯硅钢片卷料的上料装置
本实用新型公开了一种铁芯硅钢片卷料的上料装置,包括升降机构、固定座、转动执行机构和转动平台,所述固定座固定设置在地面上,所述升降机构相邻设置在固定座的一侧,所述固定座对立于升降机构的一侧设置有转动平台,所述转动平台的一端铰接设置在固定座上,且所述转动平台的另一端为自由端,所述转动平台在竖向面内朝向或远离于升降机构偏转,所述固定座上设置有转动执行机构,所述转动执行机构驱动转动平台转动;所述转动平台上的物料通过转动可位移至固定座和升降机构上,能够安全的、快速的将卷料转移至升降机构上,从而便于上料。
CN202123154347.6一种变压器铁芯制备用硅钢片涂漆设备
本实用新型涉及变压器铁芯制备的技术领域,特别是涉及一种变压器铁芯制备用硅钢片涂漆设备,其满足不同身高的操作人员对装置的操作要求,提高装置的实用性;包括工作台、喷涂机构和输送机构,喷涂机构和输送机构均安装在工作台顶端,输送机构上设置有烘干机构;还包括固定板、支腿、连接板和升降机构,四组支腿呈四角分布安装在固定板底端,连接板横向安装在四组支腿之间,升降机构安装在固定板上;升降机构包括电机、电机座、支杆、第一连接杆、滑套、限位板、丝杆螺母、丝杠和花键轴,电机安装在电机座上,电机座安装在连接板顶端,四组支杆呈四角分布安装在工作台底端,四组第一连接杆呈四角分布安装在固定板顶端。
双辊连铸无取向硅钢铸带特征及常化作用研究
双辊连铸技术是冶金及材料领域内的一项前沿技术,对于生产高品质硅钢具有独特优势.本实验研究了一种双辊铸轧w[Si]=4.5%的无取向硅钢,考察其铸态和常化处理后样品的组织、织构及析出相尺寸特征.结果表明:铸带组织以与铸带法向成5~20(°)倾角的柱状晶为主,晶内存在少量0.3~0.4μm的AlN析出相,铸带织构以λ(<001>//ND)织构为主,表层织构漫散.950℃/10 min常化处理后,析出相尺寸增大,表层λ织构增强. As an advanced technique of metallurgy and material science,twin- roll strip casting has unique advantages for producing high quality silicon steel. The present study was aimed at a 4. 5% Si non- oriented electrical steel for analyzing the structure,texture and the size of precipitates at the initial and normalized state. The results revealed that the initial structure mainly consisted of columnar grains with 5 ~ 20( °) angle to the normal of cast strip,and some AlN precipitates of 0. 3 ~ 0. 4 μ...
CN202110879636.8一种高强度碳化硅钢球及其制备方法
本发明公开了一种高强度碳化硅钢球,所述高强度碳化硅钢球包括以下重量份的原料:碳化硅20‑30份、铬1‑2份、氮化硼3‑5份、铁10‑20份、钼2‑3份、锰钢30‑40份、镍5‑8份、钛6‑8份、磷2‑3份、硫2‑3份;一种高强度碳化硅钢球制备方法,包括如下步骤S1、熔融;S2、模锻成球;S3、打磨;S4、二次加热;S5、高温淬火;S6、机油回火;S7、检测成品。本发明制备的高强度碳化硅钢球具有抗折强度高、洛氏硬度高及抗压强度高等优异的机械性能,并且使用寿命长,运转精确度高,并且其工艺简单,生产耗能低,无“三废”产生,环保性高。
6.5%Si硅钢的制备技术和发展前景
6.5%Si硅钢具有优异的磁学性能和广泛的应用前景。本文综述了6.5%Si硅钢的物理、机械及磁学特性,讨论了传统轧制、温轧、薄带连铸、快速凝固、CVD、粉末轧制等不同制备工艺的关键技术及特点,概括了6.5%Si硅钢在高效节能电机、汽车马达及磁屏蔽等领域中的主要应用,介绍了硅钢的制备技术取得的研究进展,并指出了其广阔的发展前景。 6.5% Si silicon steel has good magnetic properties and wide applications.In this paper physical and mechanical magnetic properties were summarized,and key technology and characteristic of several preparation methods,such as traditional rolling,warm rolling,thin strip continuous casting,rapid solidification,CVD and powder rolling,were discussed.Main applications of 6.5% Si steel in the fields of high-efficiency electrical motors,automobile motors,transformer cores and magnetic shielding were gene...
高磁感取向硅钢涂层技术
涂层技术在高磁感取向硅钢生产中起着重要的作用.根据生产实践,介绍了高磁感取向硅钢生产中涂层的种类和作用、涂料的成分和对产品性能的影响、涂层工艺质量控制要点和检验方法等,并提出了通过优化涂层工艺改善高磁感取向硅钢性能和外观质量的方法. Surface coating technique plays an important role in producing high magnetic inductivity grain-oriented silicon steel.Based on production practice,this paper describes the types and function of the coating,the composition of the coating and its effect on the product performance,the quality control and inspection method for the coatings,as well as proposes ways to improve the magnetic property and surface quality of the steel by optimizing the coating process.
CN202111183528.3一种取向硅钢实验室轧机二次冷轧方法
本发明公开了一种取向硅钢实验室轧机二次冷轧方法,包括取样→制样→冷轧轧制规程制定→实验轧机二次冷轧。本发明所要解决的技术问题是提供一种取向硅钢实验室轧机二次冷轧方法,本发明提供的方法轧制出来的取向硅钢二次冷轧试样,对于开展后续研究提供了更加可靠的试样和条件。
硅钢在连续退火机组浪形缺陷的控制
为了消除硅钢在连续退火机组产生的浪形缺陷,对浪形缺陷产生的主要原因进行了分析。制定了相应控制措施,对炉内带钢张力、冷却段输出、碳套辊与带钢的同步性、无氧化炉燃烧状态等参数进行了调整;在生产组织上安排高低牌号宽窄规格穿插生产、定期更换碳套辊等,实施后效果明显。 The main cause leading to waviness defects of silicon steel is analyzed in order to eliminate the waviness defects of silicon steel in continuous annealing line.And thus corresponding measures for controlling these defects are made by means of adjusting these parameters such as the tension of silicon steel coils in continuous annealing furnace,the output in cooling section and the combusting condition of the non-oxidation furnace as well as keeping the synchronization between carbon sleeved roll...
CN202123201562.7一种取向硅钢氧化镁涂层线用冷涂辊
本实用新型涉及一种取向硅钢氧化镁线涂层装置,尤其涉及一种取向硅钢氧化镁涂层线用冷涂辊,具有涂层辊本体及包覆在涂层辊本体外层的橡胶涂层;涂层辊本体内部为空腔结构,空腔结构内通有循环冷冻液。本实用新型涂层辊内部设计成空腔结构,并通过循环冷冻液对涂层辊进行冷却降温,既可以达到通过涂层辊对氧化镁进行降温的目的,从而满足工艺要求,防止质量缺陷的产生,还可延缓涂层辊因反复摩擦生热造成橡胶层老化,从而延缓涂层辊使用寿命。