本实用新型提供了一种硅钢叠铁芯线圈吊装夹具,属于变压器的技术领域,缓解了现有技术中存在的线圈吊装夹具单次只能进行单个垫块装配,效率较低的技术问题。所述夹具包括:中心盘、吊环、连接杆、吊臂、勾具;连接杆一端连接中心盘,所述连接杆的数量为3个,且两两之间的夹角为120°;所述吊环设置于中心盘上方;每个所述连接杆另一端连接一个吊臂;每个吊臂上设置有勾具。
2021-04-21 137 6.8

本发明公开了一种硅钢与碳钢混合生产条件下提高钢带表面清洁度的方法,硅钢与碳钢混合冷轧轧制条件下,通过控制冷轧乳化液指标,轧机工作辊表面粗糙度,退火工序氢气吹扫流量,平整及重分卷工序钢带涂油量等措施,能够提高钢带表面清洁度。
2021-11-18 179 6.8

利用本钢技术中心试验厂技术手段,并与北京钢铁研究院合作,试制了用作家电用电机、微电机、小电机或部分中型电机铁芯的冷轧无取向电工钢。试制钢硅含量小于0.5%,钢板表面平滑,公称厚度0.5mm,且厚度均匀偏差小,性能测定结果表明,产品的磁性能、力学性能满足其使用要求。 BX STEELTechnology Center pilot plant using technical means,and with Beijing Iron and Steel Research Institute,trial cold rolled non-oriented electrical steel that has been used as appliance motor core,micro motor core,small motor core,or part of the medium-sized motor core。Trial steel of silicon content is less than 0.5%,steel plate surface is smooth,the nominal thickness of 0.5mm,and the thickness deviation is small,performance measurement results show that the magnetic properties,mechanical p... 
2011-01-28 214 5.8

针对陶瓷辊表面结瘤清除时间长、清除效果差等缺陷,研究正反转陶瓷辊除瘤法,以缩短除瘤时间,增强除瘤效果。 The general removal of ceramic roller surface tumor costs a long time and the effect is poor.This paper probed into the ceramic roller tumor removal in order to shorten time and enhance the effect of eliminating. 
2013-05-28 174 5.8

采用拉伸试验和显微组织观测的方法确定了GTN损伤模型中的9个损伤参数,运用GTN损伤模型对冷轧硅钢薄板边部缺陷的扩展及边裂的产生进行了有限元模拟,并与预置缺口的钢板轧制试验进行对比。结果表明:轧制过程中边部缺陷是造成钢板边部裂纹萌生和扩展的一个重要原因,GTN损伤模型可用来预测含边部缺陷硅钢薄板在冷轧过程中边裂的产生;预测结果与试验结果基本一致。 The crack initiation and propagation of silicon steel strip with edge defect during cold rolling process was studied by using GTN damage model in this paper.Nine damage parameters in GTN model were identified by tensile testing and microstructure observing,and then the FE simulation of edge defect evolution of silicon steel strip during rolling process was conducted on the base of GTN damage model,and then the results were compared with rolling experimental results.The results show that the edge... 
2013-01-28 171 5.8

本发明提供一种超低铝无取向硅钢夹杂物控制方法。该钢种化学成分质量百分比为C≤0.005%,Si:0.25%‑1.50%,Mn:0.15%‑0.55%,P:0.02%‑0.06%,S≤0.005%,Als≤0.005%,余量为Fe及不可避免的杂质。工艺流程为:KR→BOF→RH→连铸。转炉出钢严格控制下渣量,出钢结束加石灰、渣面脱氧剂调渣;RH脱碳结束后,先加低碳低硫硅铁、金属铝或铝钙铁合金复合脱氧,最后加入金属锰、磷铁进行合金化,然后净循环6‑10min,破空出钢运至连铸浇注。得到钢水中主要为SiO2‑Al2O3系夹杂,避免了生成低熔点SiO2‑MnO系夹杂,轧制延展变长,影响晶粒长大;同时也避免了生成高SiO2组分类酸性夹杂,导致耐材的侵蚀。可显著改善钢中非金属夹杂物类型,提高无取向硅钢的性能,并提高了钢水浇注性能。
2021-01-21 185 6.8

本实用新型公开了一种无取向硅钢喷涂用即时干燥装置,包括干燥箱,所述干燥箱内滑动连接有加热台,所述干燥箱顶部设置有加热箱,所述加热箱左右两侧分别设置有进风管和出风管,所述进风管和出风管均与干燥箱连通,所述加热箱内部从左到有依次固定连接有风机和加热网,所述干燥箱内设有带式传送机,通过带式传送机使喷涂过后的硅钢在干燥箱中移动,首先经过加热台加热,使涂层表面干燥硬化,不会变形,然后再经过加热箱吹出的风对硅钢表面的涂层进行进一步的烘干,从而保证干燥过程中涂层不会起褶皱。
2021-12-02 223 6.8

目前高磁感冷轧硅钢生产过程中,采用经验方法确定的乳化液流量设定值往往会造成硅钢产品的磁感性能达不到预期目标,针对此情况,基于轧机轧制机理研究了的乳化液流量数学模型,确定了乳化液流量设定值。实践表明,使用该数学模型输出的乳化液流量设定值,可提高轧制过程中乳化液流量控制精度,从而提高高磁感冷轧硅钢的轧制性能。 In view of the current production process of high magnetically inductive cold-rolled silicon steel, the mathematical model of emulsified fluid flow based on mill rolling mechanism is studied in view of the situation in which the magnetic sensing performance of silicon steel products is often not up to the expected target by using empirical method to determine the emulsified liquid flow setting. Practice shows that the emulsified fluid flow setting value output from this mathematical model improv... 
2022-01-28 193 5.8

从取向硅钢生产路线的选择、工艺技术的改进和生产设备的改造三方面进行了生产取向硅钢的节能降耗技术改造.通过完善多元抑制剂配方生产低温取向硅钢,通过加抛丸的酸洗、带面超声波清洗、改进连续退火炉以及余热循环利用等技术改造,使2012年取向硅钢的产量与未进行技术改造前的2009年相比提高了2.5倍,产品磁性上升了一个半牌号,能耗下降了8.9%,成材率提高了6.4%,生产成本下降了22%,综合效益显著. Energy saving technological transformation was carried out in the production of grain oriented silicon steel from three aspects of the oriented silicon steel production process route selection,technology improvement and equipment renovation.Through the improvement of multiple inhibitor formulations for producing low-temperature grain-oriented silicon steel,and by adding the blasting pickling,the belt surface ultrasonic cleaning,improvement of continuous annealing furnace,waste heat recycling tec... 
2013-02-28 207 5.8

采用电子背散射衍射技术测定50SW1300冷轧无取向硅钢中不同尺寸范围晶粒的含量,利用主成分回归分析法,综合研究不同尺寸范围晶粒的含量对无取向硅钢磁性能的影响。结果表明:通过主成分回归分析法能够从不同尺寸范围晶粒的含量的多个影响因素中获取主要的因素,定量研究它们对无取向硅钢磁性能的影响规律。分析表明,无取向硅钢的铁损与不同尺寸范围晶粒的含量之间存在着可靠的多元线性关系,在一定范围内,较大尺寸晶粒的含量越多,其对铁损优化的作用越明显;而无取向硅钢的磁感与不同尺寸范围晶粒的含量之间并无线性关系。 Distribution of grain size in cold rolled non-oriented silicon steel 50SW1300 was measured by EBSD.The effects of the distribution of grain size on magnetic properties of the non-oriented silicon steel were comprehensively researched by means of principal component regression method.The results indicate that the main factors influencing the magnetic properties in the distribution of grain sizes,which can be used to guantitative study the magnetlic properies of the steel,are obtained by principal... 
2014-11-28 200 5.8

本发明公开了一种取向硅钢实验室常化工艺方法,采用两段式常化工艺,可以模拟现场常化生产,为现场批量生产提供有效的工艺参考,缩短现场调试工艺次数和废品率、次品率,降低制造成本。
2021-09-22 175 6.8

针对新日铁公开的相关专利,总结日本高强度无取向电工钢的研究进展,分析了各专利化学成分、生产工艺及产品性能的特点,指出固溶强化、细晶强化、析出强化、位错强化都有可能被用来提高无取向电工钢的强度。在高强度无取向电工钢的研发过程中,需要根据其具体用途确定目标性能,再采用合适的强化手段,从而实现力学性能、磁性能和生产性能之间的平衡。 Authors summarize the research progress of high strength non-oriented electrical steel in Japan by learning related patents brought into the public by Nippon Steel. Authors also analyze the characteristics of the chemical composition, production technology and properties of products in the patents and point out that any ones of solution strengthening method, fine-grain strengthening method, precipitation strengthening method or dislocations strengthening method may be used to improve the strengt... 