制备{100}织构无取向电工钢方法综述
{100}织构因具有两个易磁化方向能够明显的提高磁性能,因此如何在表面获得具有{100}织构一直是无取向电工钢研究焦点。本文主要介绍了获得{100}织构的主要工艺方法及其基本原理,并结合实际生产过程对各工艺方法的优缺点进行了分析;一方面,优化无取向电工钢的成分,降低碳、锰元素含量以避免脱碳退火和真空退火,简化生产工艺;另一方面,调节升温速度、降温速度和退火气氛,使{100}晶面的表面能或弹性应变能最低,制备具有{100}织构柱状晶组织的无取向电工钢是今后的发展方向。 Because { 100} texture has two easy magnetization directions,which can significantly improve magnetization properfies,how to develop { 100} texture is a focus for researchers and manufactures. In the paper,main manufacturing processes and basic principle are introdued,and their advantages and disadvantages in practical production are analyzed. On the one hand,the production process can be simplified by optimizing chemical compositions,such as reducing the content of C and Mn,which can avoid deca...
CN202122014099.9一种用于硅钢板带的表面清理装置
本实用新型公开了一种用于硅钢板带的表面清理装置,包括机体,所述机体的内部设置有转动机构,所述转动机构的内部安装有固定机构,所述机体的外表面一侧固定连接有驱动电机,所述驱动电机的输出端固定连接有螺杆,所述螺杆的外部设置有螺纹套,且螺纹套在螺杆上螺纹转动连接,所述螺纹套的底部固定连接有电动推杆,所述电动推杆的输出端固定连接有连接板。本实用新型,利用转动机构可很好的进行翻转,便于对两面进行清理,从而提高了一定的工作效率,相比人工翻转清理时效果更好,具有一定的实用性,利用固定机构可很好对于成硅钢板带进行固定,可方便进行清理,提高清理时的工作效率,实用性较强。
CN202123048227.8一种硅钢前处理铁泥泵反冲洗装置
本实用新型公开了一种硅钢前处理铁泥泵反冲洗装置,包括污泥处理组件,所述污泥处理组件包括置放于污泥池的泵体、与泵体相连的传动轴管、设于传动轴管远离泵体一端的驱动电机以及与泵体相连的污泥管道,所述污泥管道的另一端穿过污泥池与排污管路连通;反冲洗组件,所述反冲洗组件包括与污泥管道相连的冲洗管道以及与冲洗管道相连的冲洗水泵,所述冲洗水泵的另一端与自来水供水管路相连;开关组件,所述开关组件包括设于污泥管道与排污管路连接处的第一阀门以及设于冲洗管道与冲洗水泵连接处的第二阀门。本实用新型减少了因铁泥堵死管道,所造成的电机过载烧坏,提高了生产效率,降低了维修维护成本。
本钢薄板坯连铸机生产无取向电工钢的工艺优化
针对本钢薄板坯铸机在生产无取向电工硅钢的过程中存在的铸坯拉断、中包增碳、增氮等问题,进行了连铸工艺优化。通过采用新型无碳中间包覆盖剂、环保中间包干式料及专用结晶器保护渣后,降低了铸坯增碳量;通过控制钢包到中间包的增氮环节,降低钢水增氮;适当增大二冷水量,控制钢水过热度,防止铸坯拉断等生产事故的发生。改进工艺后,精炼后到成品铸坯的平均增碳量能控制在10×10-6以内,平均增氮量能控制在4×10-6以内。 The technology optimization has been adopted for preventing nitrogen increasing and carbon increasing in Benxi thin slab producing non-oriented silicon steel.Measures accordingly were adopted and satisfactory results were achieved.
无取向硅钢磷酸盐型杂化涂层性能测试
以质量分数为25%的丙烯酸乳液MC-102、15%Al(H2PO4)3溶液、0.01%H3BO3、0.01%Zn(Ac)2·2H2O和2%二乙二醇丁醚组分,在不同固化工艺下制备涂层。极化曲线和电导率测试发现300℃处理60 s得到的涂层具有良好的耐腐蚀性和绝缘性;水煮实验证明该涂层具有良好的耐水性;断口线扫描发现涂层具有良好的附着性。 A formula comprising MC-102 acrylic emulsion 25%,aluminium dihydrogen phosphate15%,boric acid 0. 01%,zinc acetate dihydrate 0. 01% and diethylene glycol monobutyl ether 2% was used to prepare coatings via different treatment process. The conductivity test and polarization curves revealed that a coating cured at 300 ℃ for 60 s showed good insulative and anticorrosive properties. The water boiling test indicated that the said coating had good water resistance. A cross section of the coating was in...
CN202122562844.3一种电工钢切片用辅助定位装置
一种电工钢切片用辅助定位装置,涉及电工钢加工技术领域,包括加工台、支撑腿、定位块、侧板、滑杆、移动板、顶板、滑动架、伸缩杆、切片装置、定位杆和挡板;支撑腿设置在加工台底部;定位块设置有两组,两组定位块均设置在加工台上,两组定位块沿横向分布,每组定位块设置有两个,每组的两个定位块沿纵向分布;侧板设置有两个,两个侧板均设置在加工台纵向一侧,两个侧板沿横向分布;滑杆设置在两个侧板之间;移动板沿横向滑动设置在滑杆上;顶板设置在移动板靠近加工台的纵向一侧,顶板位于移动板上端。本实用新型能够方便工作人员切割出一定尺寸的电工钢切片,且切割精度很高。
电工钢检测方法及标准综述
综述了电工钢从生产到成品过程中涉及到的检测项目、检测方法及仪器,并通过对电工钢标准的发展改进,详细阐述了我国现有的电工钢技术标准体系,同时对代表企业的电工钢重点指标进行了摘录对比,为综合应用电工钢检测方法并促进电工钢的发展提供了一定的参考。 This article summarizes the testing items,methods,and instruments involved in the process from manufacturing to finished products of electric steel. The current electric steel technical standards system in our country is also elaborated in detail,along with the development and improvement of electric steel standards. Meanwhile,by comparison of electric steel KPI in representitive companies,this article provides references for comprehensive application of electric steels testing methods and promo...
高强无取向硅钢组织演变与强化机制
针对新能源汽车的发展,制备了含Ni固溶强化、含Cu析出强化以及含Ni+Cu复合强化3%Si无取向硅钢,研究了强化方式对无取向硅钢组织、织构和性能的影响。结果表明:固溶强化型无取向硅钢热轧板中形成了粗大{221}<221>晶粒,冷轧过程中剪切变形明显并在退火后形成良好再结晶织构。析出强化型无取向硅钢热轧板中心层形成γ取向粗大晶粒,在后续的加工中γ织构逐渐增强并最终得到相对细小的再结晶晶粒。复合强化型无取向硅钢热轧板中保留了强λ取向带状组织,退火后形成了有益的Goss织构和λ织构。固溶强化型与复合强化型无取向硅钢磁感应强度B50分别达到1.742、1.688 T,高于析出强化型无取向硅钢的1.645 T。同时,复合强化型无取向硅钢高频铁损最低,其P1.0/400和P1.0/1 000分别低至20.97、82.69 W/kg,这与其较小的晶粒尺寸和织构改善有关。强度计算结果表明:Ni元素固溶强化对强度的提高有限,屈服强度为468 MPa,纳米Cu析出可显著提高屈服强度(强度增量约200 MPa),且主要来自于模量强... For the development of new energy vehicles, 3%Si non-oriented silicon steel were processed by solid solution strengthening with Ni, precipitation strengthening with Cu, and composite strengthening with Ni and Cu. The effects of different strengthening methods on the microstructure, texture and properties of high-strength non oriented silicon steel were studied.The results show that coarse {221}<221> grains are formed in the hot rolled sheet of solution strengthened non-oriented silicon ste...
电工钢中柱状晶尺寸及退火工艺对{100}织构的影响
利用EBSD技术研究了电工钢中不同的柱状晶尺寸及退火工艺下{100}织构的演变规律。结果表明,初始晶粒尺寸的影响最显著。细小柱状晶热轧后经过常化处理,组织已均匀,但中心层有强{100}织构。粗大柱状晶中{100}织构的遗传性强,常化及中间退火后,中心层仍有粗大的以{100}取向为主的晶粒;脱碳退火后才能完成组织均匀化和织构梯度的弱化。常化时的升温速度也对织构演变存在影响,低的升温速度有利于{100}织构的保留,但升温速度的影响没有初始晶粒尺寸及退火次数的影响显著。细小柱状晶样品经过热轧及三次退火工艺适合制备取向电工钢。 Evolution of {100} texture of different columnar grains and annealing process was investigated in electrical steels with the help of EBSD technique.The results show that the effect of initial grain size is the strongest.The initial fine-grained specimen shows uniform microstructure after the normalizing process,while {100} grains appear preferentially in the central layer of sheets.The heredity of {100} texture in the initial coarse-grained specimen is more significant.{100} mainly-oriented coar...
CN202121977192.3一种硅钢片堆叠移送装置
本实用新型涉及硅钢片堆叠输送技术领域,具体涉及一种硅钢片堆叠移送装置,本实用新型的硅钢片堆叠移送装置在底座上形成用于堆叠硅钢片的叠置区,叠置区内设置有可上下移动的托料部,推料部设置在叠置区的一侧,若干个硅钢片堆叠到托料部上,托料部上下移动至其与挡部之间的高度为预设高度后,推料部将托料部和挡部之间的若干个硅钢片推出,实现定量堆叠硅钢片,移料机械手再将推出的硅钢片移送至传送带上,托料部可托举剩余的硅钢片朝上移动,方便推料部复位,本实用新型的硅钢片堆叠移送装置能够代替人工分拣堆叠硅钢片,提高工作效率,并且通过设定托料部与挡部之间的高度实现固定数量的硅钢片堆叠分拣,精确度高。
50W600无取向硅钢钙处理的热力学分析及实验研究
通过热力学计算及实验室研究,对钙处理前后50W600无取向硅钢退火冷轧板中夹杂物的类型、数量及尺寸进行了系统分析。结果表明,50W600无取向硅钢经钙处理后(w(Ca)=0.002 6%),钙在1 600℃的钢液中主要以固态的CaO·2Al2O3、CaO·6Al2O3及溶解钙的形式存在。在钢液的凝固过程中,钢中的溶解钙和硫反应生成了CaS和CaS-MnS复合夹杂,有效抑制了MnS的弥散析出,减少了钢中微细夹杂物的数量。同时钙处理促进了钢中微细夹杂物的聚合长大,导致显微夹杂物的数量增加。 Based on thermodynamic calculation and laboratory experiment,the type,quantity and size of inclusions in annealed cold-rolled steel sheets of 50W600 non-oriented silicon steel before and after calcium treatment were systematically studied.Results showed that after calcium treatment(w(Ca) = 0.002 6%),calcium was mainly in the form of CaO·2Al2O3,CaO·6Al2O3 and dissolved calcium in steel at 1 600 ℃.Dissolved calcium could combine with sulfur to form CaS inclusions and compound CaS-MnS inclusions du...