研究了铝和铬元素在无取向电工钢晶粒长大过程中对织构及晶界变化的影响规律。试验结果表明:电工钢在晶粒长大过程中的主要织构组分均为{111}<112>。在晶粒生长期间,不加铝的1号试样中,{111}<112>、{111}<110>织构组分强化,而{100}<001>织构组分弱化;与1号试样相比,在加入0.2%的铝(质量分数,下同)的2号试样中,{111}<112>、{111}<110>织构组分强化(增加)的速率下降,{100}<001>织构组分变化不明显,甚至稍有增加。在含铝的试样中再加入0.3 5%的铬之后(3号试样),{111}<112>{、111}<110>和{100}<001>织构组分的变化规律与1号试样相似,但当电工钢中加入0.72%的铬之后(4号试样),上述3种织构组分的变化规律与2号试样相似。对于在晶粒生长期间持续变化的3种织构组分而言,1号试样的{1 1 1}<112>和{111}<110>织构组分的高(低)取向差角度晶界频率下降(... The effect rule of Aluminm and Chromium on texture and grain boundary transformation in the nonoriented electrical steel during grain growth was investigated.The experimental result shows that the main texture component is {111}<112> in the electrical steel.The {111}<112> and {111}<110> components in specimen 1 without Alumium were strengthened during grain growth whereas {100}<001> component was weakened.But the growth rate of {111}<112> and {111}<110> compon... 
2011-06-28 110 5.8

电工钢反复弯曲次数是电工钢性能检验的重要指标之一,直接影响到用户在使用电工钢过程的机加工性能。主要分析了试样宽度、试样张力、晶粒取向、反复弯曲设备等因素对电工钢反复弯曲试验的影响,并对各个因素的影响程度进行量化以及原因探讨,从而归纳形成各影响因素的基本规律,以便为电工钢实际生产、用户使用提供科学指导。结果表明:试样宽度增加,反复弯曲次数也会不断增加,晶粒位向对取向电工钢的反复弯曲次数影响较大,当支座顶部到拨杆底部的距离减小或拉紧力增加时,反复弯曲次数会不断减小,但当拉紧力达到60N以上时,对反复弯曲次数影响不大,试样经退火后,反复弯曲次数略有上升。 The reverse bend number is an important performance of electrical steels′capabilities,affecting the machining performance directly when the customers used.It investigated some factors,such as sample′s width,sample′s tension load,grain orientation and equipment,how to effect the reverse bend test for electrical steel,measured the influence degree,and discussed the reason,in order to form basic rules which could be guided the manufacturing and using for electrical steel.Results showed that the rev... 
2014-07-28 118 5.8

电动汽车电机在高速旋转时承受离心力和电磁力的作用,在进行电机转子设计时,既要考虑电磁性能,还要考虑机械性能。对电机转子受力情况进行了综述,分析了转子用电工钢疲劳性能参数的重要性,详细阐述了试样抛光、表面处理、试样的对中和安装对测试结果的影响。 The motor of electric vehicle bears big force for high speed rotors,mainly including centrifugal and electromagnetic forces.The magnetic and mechanical aspects of the electrical steel are crucial to machine design.In this paper,the forces applied on the motor were summarized and importance of fatigue properties was analyzed.The influence of specimen polish,surface treatment,alignment and installation on fatigue testing result were represented in detail. 
2014-10-28 115 5.8

本发明提出一种预判取向硅钢冷轧脆断发生的方法,将酸洗带头20‑30cm进行剪切取样,在取到的样板上面注明工作侧和传动侧;将取好的样板送至焊缝检测冲压机处,通过冲压机对样板进行冲压,根据不同钢带厚度,设定不同冲孔机压力,对样板进行冲压后,通过观察裂纹形貌,预判常化卷在冷轧轧制过程中是否会发生脆断,本发明使带钢在冷轧前能够制定相应的对策措施,从而降低冷轧断带所产生的损失。
2021-03-05 97 6.8

分析了电感耦合等离子体发射光谱法(ICP-AES)测定硅钢中铌的检测过程,讨论了该检测过程中不确定度的主要来源,建立了该方法的定量的数学模型,并根据这一模型计算出了检测结果的合成标准不确定度和扩展不确定度。 The measurement of niobium content in silicon steel by inductively coupled plasma atomic emission spectrometry(ICP-AES) was analyzed,by which the main factors affecting the uncertainty of the measurement were ascertained and the calculation formula was given.Finally,according to the formula the combined uncertainty and expanded uncertainty were obtained. 
2023-05-12 1.25k 5.8

采用X-射线衍射分析技术测定了取向硅钢热轧板在不同压下率下不同厚度处的织构。结果表明,在压下率低于80%的情况下,几乎所有试样的不同厚度处的织构均为旋转立方织构类型{100}<011>,但不同压下率、不同厚度处的织构强度存在很大差异;在压下率大于80%的情况下,不同试样的不同厚度处的织构类型发生了变化,其织构类型为旋转立方织构或高斯织构{011}<100>,且当织构类型为旋转立方织构时,织构强度存在很大差异,而当织构类型为高斯织构时,织构强度差异相对较小。 The texture of the grain oriented silicon steel hot rolled plate at different compressibility has been measured.The experimental results have shown that the texture of all samples at different thickness is {100}<011> when the compressibility is below 80%,and its intensity at different compressibility and thickness is difference.The texture of all samples at different thickness is variable when the compressibility is above 80%,it is {100}<011> or {011}<100>,and the intensity of ... 
2011-04-28 111 5.8

【作者】 王爱华; ...
2013-10-28 70 5.8

本发明公开了一种高磁感取向硅钢高效脱碳退火工艺,主要工艺流程为:炼钢连铸→热轧→酸洗常化→冷轧→脱碳和初次再结晶退火→渗氮处理(低温Hi‑B)→涂覆氧化镁隔离剂→高温退火→拉伸平整退火→涂覆绝缘涂层→精整,低温HiB不同于高温Hi‑B的工艺流程主要是在脱碳退火后增加了渗氮段。本发明在保证产品实物质量不低于现有水平(国内领先水平)的前提下,使Hi‑B钢退火效率达到世界领先,制造成本大幅降低。
2021-09-26 100 6.8

【机构】 武汉钢铁学院轧钢七二级电工钢结业小组; ...
2023-05-12 199 5.8

阐述了电工钢在\"双碳\"中的作用,强调了电工钢的生产工艺技术及在减少碳排放、降低能耗中的作用,对下游能效升级带来明显的节能及降碳成果。同时,分析了2021年电工钢的生产运行情况,介绍了电工钢的未来发展,并针对如何减少碳排放以及生产更多的更低铁损、更高磁感的电工钢谈了几点启示。 The effects of electrical steels on carbon peak and carbon neutralization were expounded,especially on the achievements of obvious energy saving and carbon reduction to the downstream energy efficiency upgrading bringing from the production technology of electrical steels and their effects to reducing carbon emission and energy consumption.Meanwhile the production situation of electrical steels in 2021 was analyzed,and the future development of electrical steels was introduced,and some advices w... 
2022-01-28 138 5.8

【机构】 武钢研究院; ...
2013-06-28 77 5.8

本发明涉及取向硅钢制造技术领域,公开了一种快速判断取向硅钢初次再结晶晶粒直径的方法,包括如下步骤:选取取向硅钢热轧来料,进行生产,对产出的钢板在同部位各取若干个拉伸试样,加工拉伸和分析,取得屈服强度,在拉伸试样部位两侧连续制取金相试样,计算对应拉伸试样的平均晶粒直径D,将性能数据和平均晶粒直径进行统计分析,建立屈服强度与晶粒直径的对应关系,实际生产时,在产出的钢板上取判断试样,取得判断试样的屈服强度,进而取得判断试样的晶粒直径。本发明快速判断取向硅钢初次再结晶晶粒直径的方法,通过机械性能检验,来间接指示初次晶粒的大小,检测速度快,评价更准确。