为了提升新能源车用驱动电机的功率密度,各大电机厂商都在不断地提升电机转速,随之而来的问题就是电机的铁耗也在不断增高,如何降低电机铁耗成为了电机厂商必须要解决的难题。本文讨论了电机铁耗的组成部分及影响因素,并对1台8极48槽的永磁同步电机分别使用3种不同厚度的材料进行仿真,对比其效率及铁耗分布,推导出驱动电机中硅钢厚度、铁耗及成本的关系,最后对驱动电机选材提出建议。 In order to increase the power density of traction motor for new energy vehicles,major motor manufacturers have been constantly increasing the motor speed.The following problem that manufacturers have to solve is how to reduce the increasing iron loss when the motor speed is increased.The components and influencing factors of motors’ iron loss were discussed in this paper,and an 8-pole 48-slot permanent magnet synchronous motor using three different thickness materials was simulated.To compare i... 
2022-01-28 194 5.8

本发明涉及一种低耗高效硅钢常化酸洗工艺及酸洗设备,其有效利用常化炉出口余温作为加热带钢的介质,使带钢与低温的酸液接触表面发生强烈的物理化学反应,快速酸洗剥离表层粗大的氧化铁皮,降低酸洗系统的酸液温度,通过调控溶液氧化还原特性提高酸洗效率去除残留的铁橄榄石,节约了能耗,同时取消了高投资高运行成本的抛丸工艺,实现了低耗高效硅钢常化酸洗的目的。
2021-07-23 149 6.8

本发明公开了一种电力变压器硅钢片自动叠片生产设备,包括支撑板和叠片立板,其中一组所述支撑板的表面安装有叠片立板,另一组所述支撑板的顶部安装有检测立板;所述叠片立板的背面安装有连杆,所述连杆的尾端连接有限位环,所述限位环的内部等距贯穿安装有第一电动伸缩杆,所述第一电动伸缩杆的尾端表面套接有橡胶套,所述叠片立板的背面设有滑槽,所述滑槽的底壁安装有缓冲弹簧,所述滑槽的顶壁安装有第二电动伸缩杆,所述第二电动伸缩杆的尾端连接有拦截条,两组所述支撑板的顶部均安装有立块。本发明通过设置有叠片立板、限位环、拦截条以及缓冲弹簧的配合,可简化本叠片设备的整体占地面积,简化叠片加工程序。
2021-11-18 168 6.8

一种高磁感低铁损取向硅钢生产用修复装置,包括:工作台,工作台上方设有放置板,放置板两端均设有L形夹板,放置板两侧位于两个L形夹板相对位置均开设有驱动槽,两个驱动槽内底部均水平设有一号螺杆,本实用新型具有以下优点:通过一号电机带动一号螺杆进行转动,使两个L形夹板相互靠近,便于对放置板上的取向硅钢片进行夹持固定,提高其修复过程的稳定性,避免其修复过程中发生移动;通过风机组将修复过程中产生的残渣吹至收集口,并落入收集箱内,提高工作台表面的清洁度;通过电动滑轨以及二号电机带动二号螺杆进行转动,便于使修复装置主体对准取向硅钢片修复部位,降低时间和劳动力的消耗,提高工作效率。
2021-12-23 202 6.8

【作者】 陶永根; ...
2011-01-28 180 5.8

对西昌钢钒炼钢厂200 t BOF(顶底复吹)-RH-CC工艺生产50PRW800无取向硅钢RH精炼过程中主要成份进行了分析。找出了目前工艺中影响钢液质量的主要因素是钢水脱氧处理不彻底,造成加入的部分硅元素烧损。操作工艺改为铝的脱氧即合金化操作一步完成,保证了钢水中氧处于一个较低的范围,从而减少对硅元素的烧损,提高合金收得率。 The factors of BOF-RH-CC process affecting the compositions of liquid steel were systematically investigated and studied of Xichang Steel and Vanadium Company. The main factors affecting the steel cleanliness were picked out. All results showed that the loss of silicon elements resulting from the deoxidization of liquid steel was not completely. It was suggested that the addition of aluminum for deoxidizing and alloying of molten steel was executed as one step in order to lower the oxygen potent... 
2014-03-28 174 5.8

通过制备磷酸二氢铝硅钢涂层,研究了氧化锌对无铬涂层耐盐雾性能、电化学性能和附着性的影响。结果表明,硅钢表面涂层含有4.0%的氧化锌时,涂层具有最高的耐腐蚀性能和电化学性能,而且其致密表面最为平整,没有裂纹出现。 The effects of ZnO on the salt spray resistance property, electrochemical performance and adhesiveness of silicon steel insulating coating were studied. The results show that the best corrosion resistance and electrochemical properties can be obtained when the coating contains 4.0% oxide zinc, and the dense surface is smooth without cracks. 
2014-07-28 199 5.8

对w(Si)=3%无取向硅钢进行表面机械研磨处理(SMAT)和异步轧制(CSR),获得表面纳米结构,再进行550~650℃、4 h固体粉末渗硅处理,用透射电镜(TEM)、扫描电镜(SEM)和X射线衍射仪(XRD)研究表层组织演变。结果表明:经过SMAT后,w(Si)=3%无取向硅钢表面形成了等轴状、取向呈随机分布的、晶粒尺寸为10 nm的纳米晶组织;异步轧制后,表面纳米晶组织保持不变;550~650℃、4 h渗硅处理后,SMAT+CSR样品表面形成化合物层,其厚度随着温度的升高由17μm增加到52μm;化合物层由Fe3Si和FeSi相组成. Nanostructured surface layer was fabricated on a 3%(mass fraction) non-grain oriented silicon steel by means of surface mechanical attrition treatment(SMAT) and cross-shear rolling(CSR),and then a solid powder siliconizing treatment was carried out for the SMAT+CSR sample at 550~650 ℃ for 4 h.The microstructural evolution was examined by using transmission electron microscopy(TEM),scanning electron microscopy(SEM) and X-ray diffraction(XRD).Experimental results show that: equiaxed nanocrystallin... 
2011-03-28 165 5.8

为提高无取向硅钢导磁性能,研究了不同剪切方式对无取向硅钢剪切处磁畴结构的影响。利用纳米磁流体观测无取向硅钢剪切后边部磁畴结构。结果表明,硅钢无论在机械剪切还是线切割后的边部磁畴都会发生不同程度的改变:线切割对边部磁畴结构改变较小,边部磁畴分布均匀且连续,在距边缘0~20μm范围内出现磁畴宽度变小现象;机械剪切对磁畴的改变较为严重,剪切处磁畴零乱且不连续,在距边缘20μm处仍难以观察到完整的磁畴结构。 The effects of different shearing modes on magnetic domain structure of cold rolled non-oriented silicon steel are studied in this paper.The magnetic domain of cold rolled non-oriented silicon steel is observed by nanometer magnetic fluid pattern method.The results show that the edge magnetic domain structure will be changed by mechanical shear and wire-electrode cutting,the variation of edge magnetic domain structure wire-electrode cutting edge is very small,the magnetic domain structure is wel... 
2012-04-28 164 5.8

本实用新型公开了一种高磁感取向硅钢加工用拉伸装置,涉及硅钢加工技术领域,包括安装架,所述安装架的后端安装有两个驱动电机,两个所述驱动电机的输出端均连接有下输送辊,所述下输送辊的左侧设置有下调节辊,所述下调节辊和下输送辊的末端均固定有限位圈,所述下输送辊的上方设置有上输送辊,所述上输送辊的左侧设置有上调节辊,所述上调节辊和下调节辊的内部均设置有连接杆,所述连接杆的外表面设置有卡块。该高磁感取向硅钢加工用拉伸装置通过设置的驱动电机,能够带动下输送辊转动,从而对工件进行输送,通过设置的连接杆和卡块,使得下输送辊转动时能够带动下调节辊转动,提高工件的输送效率。
2021-12-12 190 6.8

【作者】 卢鹏; ...
2014-03-28 139 5.8

本实用新型公开了一种用于激光切割的铁芯硅钢片夹持装置,包括固定座,所述固定座的上方设置有底板,所述底板的上方设置有压板,所述压板与底板的内部且靠近前后侧边缘处均活动连接有转动辊,所述转动辊的表面活动连接有输送带,所述固定座的表面开设有排料口,所述底板的上表面开设有泄料口,所述压板的上表面开设有加工预留口,所述压板的内部且位于转动辊之间固定连接有转轴,所述转轴的表面固定连接有从动锥齿轮,所述压板的内部且靠近左侧边缘处固定连接有电机,所述电机的输出端固定连接有转动杆。本实用新型,该装置结构简单合理,能很好地解决现有技术的不足,能实现在夹持的时候进行送料工作,有利于提高硅钢片的加工效率。
2021-04-14 145 6.8

站点公告

网站试运行,请大家关注本站公众号,多提宝贵意见!

显示验证码
没有账号?注册  忘记密码?