Fe-3.15%Si低温取向硅钢不同常化工艺下的组织及析出相研究
利用OM,TEM,EDS与XRD技术,对Fe-3.15%Si低温取向硅钢热轧板不同常化处理后的显微组织、析出相及最终产品的磁性能进行了分析研究,并对热轧板和常化板经过冷轧后的冷轧板织构进行了对比分析.结果表明,采用1120℃保温3 min二段式冷却的常化处理工艺,常化板表层显微组织均匀,沿板厚方向的显微组织的不均匀性显著,对后续过程中形成高取向的Goss织构最有利,取向硅钢的磁性能最高;采用二段式冷却的常化冷却工艺最优,在此冷却工艺下析出的细小的析出物数量最多,且弥散分布在基体中,抑制剂的抑制效果最好,对成品获得高磁性最有利;热轧板、常化板经过冷轧后的冷轧板织构均主要由{111}〈110〉和{111}〈112〉织构组成,但常化板较热轧板冷轧后的冷轧板γ取向线织构密度明显增高,由此可以证实常化处理有助于取向硅钢最终获得高取向的Goss织构. The decreasing of slab heating temperature for grain-oriented silicon steel will reduce the amount of precipitates in hot rolled plate,and be disadvantage to the formation of ultimate Goss texture.The aim of normalizing is to control and adjust the amount,size and distribution of precipitates.Microstructures,precipitates and magnetic characteristics of finished products with different normalizing technologies for Fe-3.15%Si low temperature hot rolled grain-oriented silicon steel are researched,a...
CN202110091324.0一种电机硅钢片加工用码垛装置
本发明涉及码垛装置技术领域,且公开了一种电机硅钢片加工用码垛装置,包括底板,所述底板的顶面活动连接有夹板,所述底板的顶面固定安装有固定板,所述固定板的中部活动连接有螺纹杆,所述螺纹杆的表面固定安装有齿轮一,所述底板的顶面固定安装有固定轴,所述固定轴的顶端活动连接有齿圈。该电机硅钢片加工用码垛装置,齿圈在旋转时带动啮合齿旋转,通过啮合齿与齿轮一的啮合带动齿轮一转动,齿轮一在转动时通过与夹板底端的啮合,可以带动三个夹板同时移动,从而可以改变三个夹板之间的面积值,从而实现装置可以对不同规格的硅钢片进行码垛,操作简单,降低了操作人员的劳动强度。
CN202123056302.5一种具有自动接料机构的变压器硅钢加工用防刮伤剪床
本实用新型公开了一种具有自动接料机构的变压器硅钢加工用防刮伤剪床,包括支撑座,所述支撑座的上端固定连接有相互对称的进料机构与出料机构,所述进料机构上设置有调节机构,所述进料机构与出料机构之间设置有切割底座,所述切割底座的两端设置有气缸,所述气缸的内侧设置有切割机构,所述切割机构上设置有卡接机构,所述出料机构的一侧设置有接料机构;本实用新型涉及剪床技术领域。该具有自动接料机构的变压器硅钢加工用防刮伤剪床,切割后的硅钢,通过出料机构输送至承接板上,挡板与侧板能够使得硅钢能够自动叠放整齐,自动叠放整齐相对于人工接料可明显节省时间,提高剪床的运行效率,减少人力成本,提高运行的安全性。
CN202023334280.X用于硅钢生产的碎边设备
本实用新型属于钢带剪切技术领域,具体涉及一种用于硅钢生产的碎边设备,包括收集斗、限位机构、输送机构和剪切机构;限位机构包括两个限位块;输送机构包括输送滚轮和驱动件;剪切机构包括连通筒、动力件和固定筒,固定筒内滑动连接有活塞;连通筒的一侧内滑动连接有第一塞座,连通筒的另一侧内滑动连接有第二塞座,第一塞座上设有第一剪切刀,第二塞座上设有第二剪切刀,第一剪切刀与第二剪切刀交错设置,第一剪切刀的侧面能与第二剪切刀的侧面接触;动力件用于驱动活塞往复运动。使用本设备,能够有效的对废钢带进行剪切、碎边,使废钢带形成尺寸规格相对较小的片状,使收集斗能够容纳更多的废钢带,有效提高收集斗的收纳能力。
常化对含硅1.6%的无取向电工钢组织和织构的影响
研究了常化对CSP流程生产的wSi=1.6%的无取向电工钢组织、织构和成品磁性能的影响。结果表明,经CSP流程生产,且在相同的冷轧及退火制度下,经1 000℃×2min常化处理的wSi=1.6%的无取向电工钢热轧板,其最终退火成品的铁损P15/50比不常化试样下降了10.5%,磁感B50比不常化试样提高了2.5%;常化使wSi=1.6%的无取向电工钢成品的平均晶粒尺寸增大,成品铁损P15/50相应减小;同时,常化使wSi=1.6%的无取向电工钢成品中高斯织构的强度增加,γ纤维织构的强度减弱,这有利于成品磁感B50的提高。 The effect of normalizing on microstructure,texture and magnetic properties of non-oriented electrical steel with wSi=1.6% produced by CSP process was investigated.The results show that,under the same cold rolling and annealing system,the iron loss(P15/50) of annealed samples whose hot bands has been normalized by 1 000 ℃×2 min process decreases by 10.5% and magnetic induction(B50) increases by 2.5% compared with the samples whose hot bands was not normalized.The average grain size of non-orient...
高牌号无取向电工钢技术发展及应用
对高牌号无取向电工钢国内生产情况、工艺技术、产品性能及应用领域等进行了阐述,并探讨了高牌号无取向电工钢产品的发展趋势。 This paper introduces basic facts on the production status,process technology and products’ properties and their applications of non-oriented electrical steel with high grade at home,and then discusses the development trend on technology for producing the non-oriented electrical steel with high grade.
双辊连铸无取向硅钢铸带特征及常化作用研究
双辊连铸技术是冶金及材料领域内的一项前沿技术,对于生产高品质硅钢具有独特优势.本实验研究了一种双辊铸轧w[Si]=4.5%的无取向硅钢,考察其铸态和常化处理后样品的组织、织构及析出相尺寸特征.结果表明:铸带组织以与铸带法向成5~20(°)倾角的柱状晶为主,晶内存在少量0.3~0.4μm的AlN析出相,铸带织构以λ(<001>//ND)织构为主,表层织构漫散.950℃/10 min常化处理后,析出相尺寸增大,表层λ织构增强. As an advanced technique of metallurgy and material science,twin- roll strip casting has unique advantages for producing high quality silicon steel. The present study was aimed at a 4. 5% Si non- oriented electrical steel for analyzing the structure,texture and the size of precipitates at the initial and normalized state. The results revealed that the initial structure mainly consisted of columnar grains with 5 ~ 20( °) angle to the normal of cast strip,and some AlN precipitates of 0. 3 ~ 0. 4 μ...
CN202111108098.9一种取向硅钢实验室常化工艺方法
本发明公开了一种取向硅钢实验室常化工艺方法,采用两段式常化工艺,可以模拟现场常化生产,为现场批量生产提供有效的工艺参考,缩短现场调试工艺次数和废品率、次品率,降低制造成本。
低硅钢冶炼过程硅质量分数控制
抑制回硅是低硅品种钢冶炼的重点和难点,南钢中厚板卷厂通过转炉出钢弱脱氧操作,精炼炉弱脱氧升温,脱氧、脱硫造渣,连铸严格的保护浇注及吹氩塞棒、吹氩浸入式上水口的应用等一系列工艺优化和操作的改进,使整个冶炼过程钢水回硅量稳定控制在200×10-6以内,钢水终点成分完全满足低硅钢要求。 Control of increasing silicon is the emphasis and difficulty in low silicon varieties steel smelting.The Nisco Wide Plate/Coil Plant can control the silicon content in molten steel keeping within 200×10-6 through whole steelmaking process by using oxygen residual operation in converter tapping,oxygen residual and increasing temperature,deoxidation,desulfurization,slag refining,protection cast,blowing argon by plugged nozzle,blowing argon by submerged entry nozzle in continuous casting,and other ...
CN202111574676.8一种含铝电工钢连铸高效生产的方法
本发明公开了一种含铝电工钢连铸高效生产的方法,其中CSP连铸连轧包括以下步骤:利用普通硅铁合金中的残余钙元素进行钙处理,钢水中Al2O3夹杂物得到球化;转炉终点氧含量加入改质剂;根据连铸拉速设定结晶器电磁制动电流参数,并制定不同拉速条件下的二冷修正系数;采用低粘度低转折温度消耗量为0.30kg/t高拉速结晶器保护渣,本发明连铸拉速从最高的4.2m/min提高至5.8m/min,提升幅度达到了38%,实现了薄板坯连铸连轧工艺技术条件下含铝电工钢50W1300的高效低耗生产。