采用CVD法制备6.5%Si高硅钢,介绍了具体的制备工艺过程,研究了温度对渗硅速率和试样质量减轻的影响,同时分析了扩散时间对高硅钢中硅分布的影响。结果表明:在CVD反应过程中,反应温度高于1050℃将大大提高渗硅速率,但当温度大于1200℃后,渗硅速率趋于稳定;渗硅后,试样会减轻、减薄,随着温度升高,试样质量减轻的速率逐渐增大,在1200℃左右趋于稳定;扩散时间越长,硅分布越均匀,结合制备效率进行考虑,满足Δw表-中/b≤5的时间为适宜的扩散时间。 6.5%Si high silicon steel was manufactured by using CVD method and the process was introduced,the influence of temperature on the siliconizing rate and quality reducing rate,diffusion time on silicon distribution were investigated.Results as follows: the siliconizing rate will increase quickly when the temperature is higher than 1050 ℃,but the siliconizing rate will become steadily as the temperature up to 1200 ℃;The quality reducing rate will increase with the elevating of temperature and the r... 
2013-01-28 280 5.8

本发明公开了一种风电磁钢粘接包角专用装置,其包括:工作台;磁钢限位台,其设置于所述工作台上,所述磁钢限位台上设置有多个挡块,用以在风电磁钢放置于磁钢限位台上时,围挡风电磁钢有包角粘附的左右侧面及无包角粘附的后侧面;三个抵压机构,三个抵压机构设置于工作台上,且分别位于磁钢限位台左右两侧及正前方,所述抵压机构包括伸缩元件和连接于伸缩元件上的压块,用以在粘附有包角的风电磁钢放置于磁钢限位台上时,伸缩元件驱动压块抵压住包角,使包角粘实。本发明能够将风电磁钢和包角快速定位粘接,节约人力,保证产品粘接的一致性。
2021-12-30 617 6.8

变压器D21硅钢铁芯片采用冲压工艺生产。首先对其工艺进行了分析,确定了冲压方案。对产品进行了排样设计,计算了冲压力,确定了压力中心。然后,设计了单工序落料模具,完成了模具装配图。 D21 silicon steel chips for transformer are produced by stamping.First,its stamping process was analyzed and the scheme of the stamping process was determined.The product layout was designed,the punching pressure was calculated,the pressure center was determined.Then,the blanking die with single procedure was designed,the die assembly drawing was completed. 
2013-07-28 446 5.8

采用X-射线衍射分析技术测定了取向硅钢热轧板在不同压下率下不同厚度处的织构。结果表明,在压下率低于80%的情况下,几乎所有试样的不同厚度处的织构均为旋转立方织构类型{100}<011>,但不同压下率、不同厚度处的织构强度存在很大差异;在压下率大于80%的情况下,不同试样的不同厚度处的织构类型发生了变化,其织构类型为旋转立方织构或高斯织构{011}<100>,且当织构类型为旋转立方织构时,织构强度存在很大差异,而当织构类型为高斯织构时,织构强度差异相对较小。 The texture of the grain oriented silicon steel hot rolled plate at different compressibility has been measured.The experimental results have shown that the texture of all samples at different thickness is {100}<011> when the compressibility is below 80%,and its intensity at different compressibility and thickness is difference.The texture of all samples at different thickness is variable when the compressibility is above 80%,it is {100}<011> or {011}<100>,and the intensity of ... 
2011-04-28 390 5.8

一种高磁感低铁损取向硅钢生产用修复装置,包括:工作台,工作台上方设有放置板,放置板两端均设有L形夹板,放置板两侧位于两个L形夹板相对位置均开设有驱动槽,两个驱动槽内底部均水平设有一号螺杆,本实用新型具有以下优点:通过一号电机带动一号螺杆进行转动,使两个L形夹板相互靠近,便于对放置板上的取向硅钢片进行夹持固定,提高其修复过程的稳定性,避免其修复过程中发生移动;通过风机组将修复过程中产生的残渣吹至收集口,并落入收集箱内,提高工作台表面的清洁度;通过电动滑轨以及二号电机带动二号螺杆进行转动,便于使修复装置主体对准取向硅钢片修复部位,降低时间和劳动力的消耗,提高工作效率。
2021-12-23 236 6.8

通过固溶度积公式计算及热模拟实验,对不同热装和加热温度条件下的无取向硅钢铸坯中析出相进行了研究.在低于950℃热装时,铸坯中AlN的析出量和尺寸不再变化,但MnS和AlN-MnS的数量及平均尺寸随着热装温度降低而进一步增加,并在温度低于600℃时达到最大值后保持不变.与1200℃相比,1100℃加热的铸坯中AlN、MnS的总固溶量相对更少.相比850℃热装,600℃热装再加热到1100℃的铸坯中AlN和MnS的总固溶量更少,且AlN和MnS尺寸更大.合适的热装温度和加热温度分别为600℃和1100℃. Based on solubility product calculation and thermal simulation experiments,precipitated phases in continuous casting slabs of non-oriented silicon steel were systematically studied at different hot charging and heating temperatures.When the hot charging temperature is below 950 ℃,the content and size of AlN remain unchanged,but the quantity and size of MnS and AlN-MnS increase when the hot charging temperature decreases,reach maximum and remain unchanged when the hot charging temperature is belo... 
2013-08-28 214 5.8

采用EBSD检测技术,分析了50W800无取向电工钢在重要生产工序间织构的演变以及织构沿带钢宽度方向上的差异性。结果表明:热轧板织构沿带钢宽度方向上的差异性主要体现在表层织构。带钢边部表层织构主要由旋转立方织构、α纤维织构以及少量的γ纤维织构组成,带钢宽度1/4处的表层织构主要存在高斯织构,带钢宽度1/2处的表层织构主要为(110)面织构以及少量的铜型织构。各处的带钢宽度1/4处和1/2处的织构类型基本一致,都以α纤维织构和旋转立方织构为主。冷轧后,各处的表层织构类型差异较小,均为γ纤维织构和α纤维织构。由板宽边部至中心处织构强度值逐渐降低。退火后,各处织构的组分基本一致,为较强的γ纤维织构和较弱的(100)面织构。各处织构强度值差异较小,变化趋势与冷轧板一致。 The texture of non-oriented electrical steel 50W800 was detected by EBSD technique.The evolution of the texture between important processes and the difference of texture along the width direction of strip were analyzed.The result shows that the difference along the width direction of strip of texture at the surface of hot rolled plate is most obvious.The texture at the surface of strip edge is primarily made of rotating cube texture,αfiber texture and weakγfiber texture.Goss texture is mainly co... 
2014-09-28 318 5.8

利用加热炉模拟、动态再结晶以及热模拟等试验方法以及扫描电镜、金相显微镜等分析观察手段对无取向硅钢边裂的成因进行了探讨。结果表明,长时间加热使得板坯边部晶粒异常长大,晶界氧化并脱碳,轧制过程中边部温度过低,动态再结晶过程变弱,使得板坯边部延伸性能变差,是导致硅钢边裂的主要原因。建议通过适当降低铸坯加热温度、缩短保温时间、提高终轧温度来改善硅钢边裂缺陷。 The behaviors of high temperature oxidation,dynamic recrystallization,and hot ductility,microstructure evolution were investigated on the non-oriented electrical steel sheets to discuss the formation of edge crack.The key causes of cracking was found to be the coarse as-cast microstructure,grain boundary oxidation and decarburization in reheating furnace,as well as reduced temperature at strip edge region during hot rolling process resulting in reduced hot ductility and lack of enough dynamic re... 
2013-02-28 233 5.8

针对硅钢连续退火机组的主要能源介质消耗现状,对现有生产工艺和设备研究采取机组循环用水、增加清洗段漂洗级数等措施可节约大概27 m3/h的过滤水量,并可减少78%的弱碱处理量;将炉子烟气换热系统增加一级余热回收,每年回收的余热相当于583 t标煤消耗,可节约蒸汽5 368 t。 The present situation of energy consumption for silicon steel annealing line is analyzed in this paper.In existing process and equipment conditions,increasing the number of cleaning series will lead to a saving of about 27 m3/h of filter water and reduce 78 % of weak base processing volume.For the flue gas heat-exchange system,adding a waste heat recovery device will recover waste heat equivalent to 583 tons of standard coal per year,corresponding to a saving of steam 5 368 t per year. 
2011-05-28 304 5.8

本实用新型公开了一种硅钢环形炉台车用垫片,垫片为多个陶瓷纤维高密度板拼接而成的环状,垫片的内边缘和外边缘均呈正八边形;陶瓷纤维高密度板的导热系数不大于0.15W/(m·k)。上述垫片在实际使用时,铺设于台车的底座,并在垫片上砌筑耐火砖,最后在耐火砖上浇筑耐火浇注料。因垫片的导热系数很低,因此能够减少台车底座背面热量的散失,并且能够避免高温对台车内钢卷造成影响,保证了钢卷的质量。因此,本实用新型提出的硅钢环形炉台车用垫片,对台车进行了改进,保证了钢卷的品质,解决了现阶段该领域的难题。
2020-12-26 343 6.8

【作者】 朱一知; 陈山; ...
2011-06-28 281 5.8

本实用新型公开了一种取向硅钢绝缘涂液用废液回收利用装置,涉及取向硅钢绝缘涂液技术领域,为解决现有取向硅钢绝缘涂液的废液在回收时没有进行多层热分解,导致回收利用率低的问题。所述下料筒的下端设置有调节筒,所述调节筒的下端设置有分流筒,所述分流筒的下端设置有出料筒,所述调节筒的内部设置有下料板,所述下料板的一端设置有转轴,所述转轴的一端设置有交流电机,所述下料板的侧表面设置有外接孔,所述下料筒的筒壁内设置有加热板,所述下料筒的内部设置有一级过滤网,所述分流筒的内部设置有隔挡板,所述隔挡板的一侧设置有二级过滤网。