钢厂
硅钢氧化镁的制备进展
介绍了硅钢氧化镁制备方法及高质量硅钢氧化镁制备技术的研究进展,并对利用我国丰富的卤水资源制备硅钢氧化镁进行了展望。 The preparation methods of silicon steel magnesium oxide and research progress of high quality silicon steel magnesium oxide preparation technology were introduced.The use of abundant brine resources in the preparation of silicon steel magnesium oxide was prospected.
CN202110729402.5一种硅钢氧化镁废水回用处理与污泥资源化工艺
本发明公开了一种硅钢氧化镁废水回用处理与污泥资源化工艺,包括:预过滤:氧化镁废水进入过滤容器,过滤得到的水,返回调节池中,直至预过滤澄清;过滤过程:氧化镁废水在预过滤阶段逐渐澄清后进入过滤程序,产生的过滤水满足要求后,自流入产水箱;滤饼干燥:停止过滤后,将过滤容器中的水排空至调节池,之后按照与过滤相同的方向通压缩空气,通过压缩使滤饼干燥;反吹排泥:滤饼干燥完成后,通反向的压缩空气,之后进入下一个过滤周期;经过处理后,过滤阶段产生的合格水循环利用;滤饼干燥后进一步进行资源化处理。本发明实现了废水回用;产生的沉淀污泥经处理后可分别作为钛白粉的生产原料和土壤改良剂,具有良好的社会效益和环境效益。
PDSOFT在硅钢退火炉管道设计中的应用
结合硅钢退火炉项目中应用PDSOFT软件进行三维配管设计的案例,描述PDSOFT软件的应用过程,总结其使用要点,分析其优缺点,并提出了推广三维设计软件的思路,对今后PDSOFT在相似项目中的推广应用有参考和借鉴价值。 Combining the case of using PDSOFT software to design the three-dimensional piping,the application process of the PDSOFT software is described,the using points are summarized,the advantages and disadvantages are analyzed,and the ideas of promoting the three-dimensional design software are put forward,which have a strong reference value for the promotion and application of PDSOFT in similar projects in the future.
CN202110396796.7一种高压电机用无取向硅钢50SBW600的制备方法
本发明涉及一种高压电机用无取向硅钢50SBW600的制备方法,包括,S1,将装有精炼钢水的钢包运至回转台,回转台转到浇铸位置后,将钢水注入中间包;S2,中间包通过水口将所述钢水分配至若干个结晶器中,所述结晶器中设置有浸入式水口,S3,钢水在结晶器内生成晶核,结晶器将带有晶核的钢水下放至通道;S4,通道上设有第二电磁搅拌器,第二电磁搅拌器对通道内钢水进行电磁搅拌,所述钢水在通道中逐步转换为钢坯;S5,拉矫辊将的所述钢坯拉出通道并对钢坯进行形态矫正;S6,切断装置所述钢坯进行切割。本发明通过在无取向硅钢50SBW600制备过程中设置双电磁搅拌装置,充分保证连铸过程中钢坯中的等轴晶数量,保障了产品表面缺陷质量。
脉冲电场对取向硅钢磁性能及织构的影响
采用硅钢自动测量装置及X射线衍射仪检测出样品在实验前后的磁性能参数和织构强度.结果表明:较低的电压、9 Hz、较长的处理时间以及退火温度为650℃有利于增高铁损降低比例;较低的电压、较高的频率以及退火温度为650℃有利于增加磁感应强度增高比例.最佳的提高磁性能的实验参数是:频率为9 Hz,电压为500 V,处理时间为6 min,退火温度为650℃.通过织构分析可以验证:取向硅钢磁感应强度的变化取决于{110}<001>晶粒取向度值,而{110}<001>取向度值可看成是一个反映总体平均偏离角大小情况的综合值. An automatic measurement system for silicon steel and an X-ray diffraction meter were used for measuring the magnetic property parameters and texture of ex-processed samples and processed samples.It is shown that under the condition of a lower voltage,9Hz,a longer processed time and an annealing temperature of 650℃,the decrease rate of iron loss can be increased;a lower voltage,a higher frequency and an annealing temperature of 650℃ are in favor of improving the increase rate of magnetic inducti...
CN202111157344.X一种适用于无取向硅钢极薄带表面涂覆的涂液及其制备方法与应用
本发明公开了一种适用于无取向硅钢极薄带表面涂覆的涂液,它由水溶性丙烯树脂、成膜助剂、耐盐雾助剂、流平剂、纳米氢氧化锆、消泡剂、水按质量比100:(2~8):(1~3):(1~5):(0~1):(0.1~0.5):(70~130)组成。将该涂液在无取向硅钢极薄带表面可表现出良好的涂覆性,经烘烤固化后形成的绝缘涂层表面透明光滑,附着性和绝缘性能优良,可有效提升无取向硅钢极薄带的综合性能,适合推广应用。
固溶处理对高牌号无取向硅钢磁性能的影响
对商用50W330型无取向硅钢成品在930℃下保温2 h固溶并以不同方式冷却处理,利用磁性检测仪检测分析了处理前后的磁感和铁损变化,应用光学显微镜、扫描电子显微镜、X射线衍射仪观测分析了显微组织结构的演变。考察了平均晶粒尺寸、织构组分比及第二相粒子状态对磁性能的影响规律,结果表明:固溶处理前后平均晶粒尺寸的变化对硅钢磁性能的影响非常显著;当平均晶粒尺寸相差不大时,织构组分比[Goss+{100}]/{111}越大,磁感会越高;固溶处理会将细小弥散的第二相粒子重新回溶到基体中,减小了其对磁畴壁的钉扎作用,铁损随之下降。 The commercial 50W330 non-oriented silicon steel samples were heat treated at 930℃ for 2 h and cooled in different ways,then the iron loss and the magnetic induction of the samples before and after solution treatment were measured with a magnetic detector.The evolution of microstructural texture was analyzed by optical microscopy,scanning electron microscopy and X-ray diffractometry.The effects of average grain size,texture composition ratio and the second phase particles on the magnetic propert...
常化温度对热轧无取向硅钢组织与磁性能的影响
为研究常化温度对热轧无取向硅钢组织与织构的影响,采用光学显微镜、背电子散射衍射技术研究了不同常化温度对其影响。结果表明,实验硅钢板在700~850℃温度下常化时,随常化温度的升高,晶粒尺寸增大,有利组分α织构增强,不利组分γ织构降低。对比研究了800℃和850℃常化热轧板CSL晶界分布图与取向差分布图,在本文研究条件下,Goss织构易在Σ=3,9的CSL晶界及晶粒取向差为30°~55°处形成。 The hot strips normalized at different temperatures were investigated by optical microscope and EBSD to study the effect of normalizing temperature on microstructure and texture of hot-rolled non-oriented silicon steel sheets.The results show that the grain size increases,the intensity of α-fibre texture increases,and the γ-fibre texture decreases when the hot strips are normalized at the 700-850 ℃.And CSL boundaries of Σ=3 and 15,and misorientation angles between 30° and 55° are more likely rel...
CN202023342355.9一种硅钢片铁芯叠片机构
本实用新型公开了硅钢片铁芯叠片机构,包括送料装置和叠片装置,送料装置包括有磁性传送带、送料件和第一定位杆,磁性传送带用于将已剪切的硅钢片传送至送料件,送料件安装于磁性传送带的下方,并且可沿磁性传送带的正交方向平行伸出,第一定位杆安装于送料件上,用于定位硅钢片,叠片装置设置于送料件的伸出的一方,包括有叠放台、第二定位杆和机械手,叠放台用于叠放硅钢片,第二定位杆用于定位硅钢片,机械手用于将送料件的硅钢片搬运至叠放台上,机械手包括有转动臂和取料单元,取料单元安装于转动臂的端部,包括有电永磁铁,电永磁铁用于吸取硅钢片。根据本实用新型的硅钢片铁芯叠片机构,可有效提高叠片速度,降低能耗,提高生产效率。
硅钢在连续退火机组浪形缺陷的控制
为了消除硅钢在连续退火机组产生的浪形缺陷,对浪形缺陷产生的主要原因进行了分析。制定了相应控制措施,对炉内带钢张力、冷却段输出、碳套辊与带钢的同步性、无氧化炉燃烧状态等参数进行了调整;在生产组织上安排高低牌号宽窄规格穿插生产、定期更换碳套辊等,实施后效果明显。 The main cause leading to waviness defects of silicon steel is analyzed in order to eliminate the waviness defects of silicon steel in continuous annealing line.And thus corresponding measures for controlling these defects are made by means of adjusting these parameters such as the tension of silicon steel coils in continuous annealing furnace,the output in cooling section and the combusting condition of the non-oxidation furnace as well as keeping the synchronization between carbon sleeved roll...
无取向硅钢冶炼过程中的夹杂物遗传变化
研究表明,硅钢中的夹杂物对成品带钢的磁性能有显著影响。为研究冶炼过程硅钢中的夹杂物遗传变化,进而提出更有效的控制措施加以去除,本文结合典型的无取向硅钢生产炉次,采用非水溶液电解提取+扫描电镜观察方法分析冶炼过程中上述炉次典型试样的夹杂物。结果表明:转炉冶炼结束、RH精炼开始时,钢的氧化物夹杂总量最大,约为0.23%;RH精炼过程中,氧化物夹杂总量不断降低,并在脱碳结束时达到最低,约为0.02%;连铸过程中,氧化物夹杂总量仍有不断降低趋势,但夹杂物的平均尺寸变化不大。本试验条件下,中间包试样的夹杂物数量约为1.59×104个/mm3。 As we all know, the non-metallic inclusion effects magnetic properties of silicon steel sheets obviously. The article aims to study the heredity of non-metallic inclusion in non-oriented silicon steels during the steel making process, and then provides a more effective controlling measure to remove the inclusions. Based on the typical non-oriented silicon steel charges, the non-aqueous solution extraction and SEM observation were adopted to analyze the non-metallic inclusions. Results show that,...