所有分类
  • 所有分类
  • 未分类

介绍了普通取向硅钢(CGO)和高磁感取向硅钢(Hi-B)铸坯高温加热两次冷轧、一次冷轧和铸坯低温加热两次冷轧、一次冷轧法4种成熟生产工艺的主要技术参数,取向硅钢理论研究(Goss晶核和抑制剂)和生产技术现状。取向钢的发展趋势为:提高(110)[001]晶粒取向度,降低取向硅钢铁损,发展铸坯低温加热(≤1 300℃)和薄板坯连铸连轧流程生产取向硅钢工艺。 Main technology parameters of four developed process:cast bloom higher temperature heating-double cold rolling or single cold rolling,lower temperature heating-double cold rolling or single rolling process for production of common grain oriented silicon steel(CGO) and high magnetic induction grain oriented silicon steel(Hi-B),theory research on grain oriented steel(Goss nucleus and inhibitor) and present situation of process are summarized in this paper.The development trend of grain oriented si... 
2013-05-28 129 5.8

为了优化激光刻痕降低取向硅钢铁损的工艺,寻找刻痕速度、脉冲能量、扫描间距等重要刻痕参数的最佳匹配关系,提出了一种基于人工神经网络与遗传算法的优化模型,并利用这种模型对30Q130取向硅钢材料的刻痕工艺进行了优化实验,结果表明,这种模型稳定可靠,可以作为取向硅钢刻痕工艺优化的一种有效的措施。 A laser is often considered to scribe the grain-oriented silicon steel surfaces after cold-rolling and annealing to reduce the core loss.It is necessary to select the best scribing parameters to maximize the reduction in this process.This paper proposes an optimization method of genetic algorithm during laser scribing of 30Q130 steel,by developing an artificial neural network prediction model using a database form a designed orthogonal experiment.The objective is to determine the best combinatio... 
2011-08-28 100 5.8

借助于EBSD对比研究了常化退火对高牌号无取向电工钢热轧组织和织构演变的影响,分析了常化退火对热轧板各厚度层织构的演变规律。结果表明,常化退火改善了热轧组织的均匀性,并弱化了热轧变形的γ纤维织构。升高常化退火温度,可增大热轧板的晶粒尺寸,提高{100}和{110}织构组分占有率,有利于提高无取向电工钢成品板的磁性能。 Effects of normalizing annealing on microstructure and texture of high-grade non-oriented electrical steel hot-rolled sheet were investigated by EBSD. Emphasis was put on the effects of normalizing annealing on texture evolution in the sheet thickness. The results show that the hot-rolled microstructure homogeneity is improved and the γ-fiber texture is weakened by normalizing annealing treatment. The grain size of hot-rolled sheet and intensity of the {100} and {110} favorable texture can be in... 
2014-02-28 103 5.8

研究了CSP流程试制50W270高牌号无取向硅钢热轧→常化→冷轧→退火过程中织构的演变.利用电子背散射衍射技术对全流程织构进行测量和分析.发现热轧板织构在厚度方向上存在较大差异,表层主要为铜型、黄铜和高斯织构,1/4层存在微弱的高斯织构和旋转立方织构,中心层以γ纤维织构和旋转立方织构为主,还含有较弱的α纤维织构.与热轧板相比,常化板表层和1/4层织构变化不大,中心层旋转立方织构和α纤维织构增强.冷轧板各层均具有α纤维织构和γ纤维织构.与冷轧板相比,成品板各层中α纤维织构基本消失,还出现了立方织构和高斯织构. This article focuses on texture evolution in 50W270 high-brand non-oriented silicon steel produced by CSP in hot rolling,normalizing,cold rolling,and annealing processes.The texture in the whole process was measured and analyzed by electron back-scatter diffraction.It is found that the texture along the thickness direction in hot-rolled strips changes obviously;there are mainly copper,brass,and Goss textures in the surface layer;the 1/4 layer has weak Goss texture and rotating cube texture;γ-fib... 
2014-09-28 124 5.8

研究了冷轧95%变形量无取向硅钢不同退火温度(710~1 050℃)下再结晶织构特征.再结晶刚完成时(710℃退火),呈现强γ({111<112>~<134>)与弱{114}<481>织构特征;随退火温度升高至900℃,γ明显减弱,{114}<481>组分持续增强,形成典型的{h,1,1}<1/h,1,2>织构;进一步升温至1 050℃,再结晶织构不再发生明显变化.基于EBSD分析,{114}<481>组分的持续强化可归因于其明显的尺寸优势以及较高频率的高能晶界(取向差角为20°~45°). A non-oriented silicon steel was heavily rolled to 95% reduction and subsequently annealed at 710~1 050 ℃ to investigate recrystallization texture evolution.When annealed at 710 ℃ with complete recrystallization,the texture is characterized by a strong partial γ fiber spreading from {111}<112> to {111}<134> and a weak {114}<481> component.As annealing at 900 ℃,γ fiber is decreased significantly while {114}<481> is increased consistently,producing a typical {h,1,1}<1/h,... 
2013-05-28 133 5.8

介绍了微合金元素锡、铌、稀土对无取向硅钢性能的影响,并扼要分析了这些元素对硅钢性能的影响机理:晶界偏聚元素Sn可细化晶粒提高硅钢磁性能;微合金元素Nb细化铁素体晶粒,提高硅钢的强度、韧性和塑性及磁性能;稀土元素(RE)在硅钢中的主要作用包括净化钢液、变质夹杂物、改善铸态组织和性能及微合金化,减少晶界上出现偏析的几率。 The influence of micro-alloy elements on properties of non-oriented silicon steel and the mechanism for effect of the micro-alloy elements including Sn、Nb and RE on the properties of steel are presented and analyzed in this paper.Grain boundary segregation elements Sn in steel can grain refinement and improve the magnetic properties;Micro-alloy elements Nb can refine the ferrite grain,increase the silicon steel strength,toughness and plastic;The main role of the RE in the silicon steel including... 
2013-03-28 117 5.8

本发明公开了一种基于硅钢服役特性的立体卷铁心单框损耗测量方法及系统,根据硅钢片在立体卷铁心中的服役特性,获得测量铁心单框所需的非正弦励磁电压波形,通过所述立体卷铁心的心柱绕组电压和单框绕组电压之间的关系,确定所述被测立体卷铁心单框所需的电压有效值,再通过计算机、数据采集卡D/A转换器、功率放大器、隔离变压器和示波器,直接在所述立体卷铁心单框上加载励磁电压,利用功率表测量立体卷铁心单框损耗。本发明利用硅钢的服役特性,获得测量立体卷铁心单框所需的非正弦励磁电压波形和电压有效值,再将励磁电压直接加载到被测立体卷铁心单框,测量立体卷单框铁心损耗。
2021-08-31 121 6.8

本实用新型涉及一种摩托车点火器线圈用硅钢片,包括E型件和I型件,所述E型件和I型件可组合成日字形;所述E型件包括竖边和设置在竖边三个横边,所述竖边与三个横边接触的位置设置孔眼;所述孔眼内径从为变径结构;位于E型件正面设置散热线槽,所述散热线槽一端与孔眼贯通,另一端指向凸部;位于E型件背面在散热线槽正对位置设置外凸线,所述I型件一侧设置与凸部匹配的凹部,在所述凹部之间凸台;所述凸台与凹台重叠;在凸台与凹部之间设置凸棱,所述凸棱位于I型件外侧。本实用新型设计新颖,改进巧妙,由于E型件具有弧形边可以有利于拾取,方便工作操作,同时采用采用接触的方式接触,增加了组合体的稳定性。
2021-08-20 98 6.8

本发明公开了一种硅钢高温加热炉用铬基高氮合金垫块及其制备方法,所述合金垫块含有Cr、Mo、N、La、Ce和Fe,不含有钨;所述合金垫块在高温抗氧化性能和高温抗蠕变性能上,优于现有技术的铬铁合金;本发明可以优化替代现有的硅钢高温加热炉用铬铁合金垫块,满足硅钢在加热炉中的加热需求,大规模工厂化生产,拥有极高的使用价值和广阔的应用市场。
2021-07-08 97 6.8

采用化学气相沉积(CVD)渗硅处理工艺连续制备6.5%Si高硅钢,具有优质的软磁性能,通过理论研究化学反应并且用简单的试验设备做进一步的探讨。根据试验的结果对连续制备6.5%Si高硅钢的CVD工艺构造提出全面、有效的建议,实现制备6.5%Si高硅钢系统。 CVD method for continuously manufacturing 6.5%Si Steel Sheet has excellent soft magnetic.Carried out a theoretical study of related chemical reaction and performing basic research with a simple test apparatus.Based on the results,finally proposed an overall process configuration to realize such a production-CVD method for continuously manufacturing 6.5%Si Steel Sheet. 
2011-12-28 114 5.8

本发明涉及冶金技术领域,具体涉及一种硅锰镇静无取向硅钢的生产方法及浸入式水口。本发明提供的硅锰镇静无取向硅钢的生产方法,包括如下步骤:1)转炉出钢:转炉出钢后对钢水进行真空抽渣,抽渣结束后向钢水中加入石灰、萤石造渣,待渣料熔化后将钢水运至RH工位处理;2)RH真空精炼:将运至RH工位的钢水通过RH真空精炼处理后进行破空、出钢,出钢后在钢包渣面加入渣面脱氧剂以对炉渣进行扩散脱氧;3)连铸浇注:对加入渣面脱氧剂的钢水采用浸入式水口进行浇注。本发明提供的生产方法可有效改善浸入式水口的侵蚀状况,提高浸入式水口的使用寿命,增加连浇炉数,进而提高连铸坯质量稳定性,降低生产成本。
2021-08-05 89 6.8

本发明涉及一种含磷高磁感无取向硅钢的生产方法,工艺路线:铁水脱硫-转炉冶炼-RH精炼-连铸-热轧-酸洗-冷轧-连续炉退火-涂层-性能检验-包装,具体步骤包括:1)将钢水冶炼至目标成分后采用连铸方式将钢水铸成坯;2)热轧板坯加热炉均热段板坯温度950~1050℃,终轧温度控制在780~830℃,卷取温度600~680℃;3)酸洗后冷轧,控制冷轧整体压下率80%以上,至成品厚度,增加剪切带组织;4)连续退火炉快速加热段温度设定1000~1150℃,增加有利织构组织形核;均热段温度设定750~830℃,全氮气干气氛保护,退火工艺速度110~150m/min,满足晶粒度8~4级。本发明在减少硅、铝、锰合金添加量的情况下,改善铁损提高磁感性能,提高机械性能。
2021-08-19 108 6.8