树脂含量对半无机型无铬无取向硅钢涂层性能的影响
本文研究了丙烯酸树脂含量对以Al(H2PO4)3为基料的无铬无取向硅钢绝缘涂层各项性能的影响.用盐雾实验、动电位极化及交流阻抗等试验手段研究了不同树脂含量对硅钢绝缘涂层的耐盐雾性能和电化学行为的影响,同时采用SEM对涂层的表面形貌和附着性进行研究.结果表明,树脂含量为19.9~29.4%时,涂层的耐蚀性和附着性最好;树脂含量过多时,涂层的耐蚀性和附着性均较差. This paper studies the influence of acrylic resin on the performance of insulating coating of aluminum dihydrogen phosphate on chromium-free non-oriented silicon steel.Salt spray experiment,potentiodynamic polarization and electrochemical impedance spectroscopy were used to study the influence of acrylic resin content on the salt spray resistance and electrochemical behavior of the insulation coating of nonoriented silicon steel.The surface morphologys and adhesion of coating were tested by SEM....
CN202180023598.4无取向性电磁钢板、铁芯、冷轧钢板、无取向性电磁钢板的制造方法及冷轧钢板的制造方法
此无取向性电磁钢板具有预定的化学组成,所述化学组成满足(2×[Mn]+2.5×[Ni]+[Cu])-([Si]+2×[sol.Al]+4×[P])≧1.50%,以SEM-EBSD测定距表面1/2板厚深度的与轧制面平行的面时,将{hkl}<uvw>取向的晶粒相对于全部视野的面积率记为Ahkl-uvw时,A411-011在15.0%以上,且平均晶体粒径为50μm~150μm。
CN202122860692.5硅钢片叠压精准定位设备
本实用新型涉及一种硅钢片叠压精准定位设备,包括压台、压板和仿形燕尾键,所述压台上开有与仿形燕尾键下端相对的限位槽,所述压板设置与压台上方,所述压板上开有与仿形燕尾键上端相对的限位孔。本技术方案当硅钢片叠放压合之后,仿形燕尾键可以去除,并能够在硅钢片组成的铁芯上形成燕尾槽,用于后期燕尾键的组装,且能够保证燕尾槽内的结构规则,便于后期燕尾键组装。
CN202120638252.2无取向硅钢蠕变性能测试装置
本实用新型涉及一种无取向硅钢蠕变性能测试装置,包括基座,基座的顶部和侧面设有开口;试样夹持装置,试样夹持装置安装在基座的顶部,用于夹持硅钢蠕变试样;转换力杆,转换力杆安装在基座的侧面,与试样夹持装置连接;可调节式砝码盘,可调节式砝码盘安装在转换力杆上,可调节式砝码盘上能够放置不同重量的砝码,转换力杆将砝码的重力转换成水平力,以实现对硅钢蠕变试样不同应力水平的加载;可调节式灯座,设置在试验腔内并与基座的侧面插接;加热装置,放置到可调节式灯座上,用于给硅钢蠕变试样加热。本实用新型具有解决无法实现不同应力和温度下硅钢材料的蠕变研究的问题的效果。
CN202110311664.X一种取向硅钢高温退火底板
本发明公开了一种取向硅钢高温退火底板,涉及钢卷生产技术领域,解决了钢卷的尺寸变形导致钢卷切边量过大的技术问题。包括应变诱导板,应变诱导板的板面开设有若干凹槽,相邻凹槽之间于应变诱导板的板面形成凸楞,钢卷放置于应变诱导板的板面上,其中部分的钢卷端面支撑于凸楞上,其余的钢卷端面悬置于凹槽上。本发明通过在应变诱导板上设置凹槽与凸楞,钢卷在高温退火过程中同样受重力产生蠕变变形,但蠕变变形按照凸楞所设定的方向进行,从而将产生的不均匀的“大浪”分割成碎化均匀的“细浪”,使得钢卷边部的变形细小、均匀、可控,从而降低了大象脚变形的缺陷影响程度,减小了钢卷的切边量,提高了成材率,同时能够获得良好的边部板形。
硅钢连续退火生产线设备改造
针对硅钢连续生产线设备存在的故障、隐患以及精度等影响产品质量的问题进行分析及改造,实现保证生产线设备稳定运行、提高设备精度及硅钢产品质量的目的。 This paper analyzes and transforms the electrical equipment failures, risks existed in slicon continuous production line, and the effect of accuracy to product quality, in order to ensure stable operation of equipment in production line and improve the accuracy of device, quality of silicon.
双辊连铸无取向硅钢铸带特征及常化作用研究
双辊连铸技术是冶金及材料领域内的一项前沿技术,对于生产高品质硅钢具有独特优势.本实验研究了一种双辊铸轧w[Si]=4.5%的无取向硅钢,考察其铸态和常化处理后样品的组织、织构及析出相尺寸特征.结果表明:铸带组织以与铸带法向成5~20(°)倾角的柱状晶为主,晶内存在少量0.3~0.4μm的AlN析出相,铸带织构以λ(<001>//ND)织构为主,表层织构漫散.950℃/10 min常化处理后,析出相尺寸增大,表层λ织构增强. As an advanced technique of metallurgy and material science,twin- roll strip casting has unique advantages for producing high quality silicon steel. The present study was aimed at a 4. 5% Si non- oriented electrical steel for analyzing the structure,texture and the size of precipitates at the initial and normalized state. The results revealed that the initial structure mainly consisted of columnar grains with 5 ~ 20( °) angle to the normal of cast strip,and some AlN precipitates of 0. 3 ~ 0. 4 μ...
CN202111317124.9一种宽频率低铁损无取向电工钢及其制备方法
本发明公开了一种宽频率低铁损无取向电工钢及其制备方法,属于无取向电工钢生产制造技术领域。它从电工钢表面向内依次包括0.005mm~0.1mm的渗透层和钢材内芯;所述渗透层是由硅原子向电工钢内渗透形成,渗透层中的硅元素含量为3wt%~8wt%;所述钢材内芯包括2.0wt%~5.5wt%的硅元素和不少于93.2wt%的铁元素。本发明能保证无取向电工钢具有低频低铁损性能同时有效降低高频条件下的铁损,具体铁损性能为:铁损P1.5/50≤2.35W/kg,铁损P1.0/400≤13.8W/kg。
CN202122736197.3水性硅钢绝缘涂料制备用袋式过滤机
本实用新型公开了水性硅钢绝缘涂料制备用袋式过滤机,包括下壳体,所述下壳体顶部铰接有一对上壳体,一对所述上壳体均具有连接板,一对所述连接板通过若干个吊环连接,所述上壳体外侧壁面设有上固定座,所述下壳体后壁面设有出液管,所述下壳体内部设有弹出支撑板机构,所述上壳体内部设有上壳体清洁机构,所述下壳体内部设有下壳体清洁机构。本实用新型涉及袋式过滤器技术领域,本装置结构紧凑,通过一对第一气缸铰接于一对上壳体两侧,使上壳体实现向自动两侧打开的功能,取出支撑板时较为方便,上壳体内壁面的挤压销能够对支撑板进行挤压,当上壳体被打开时,支撑板失去挤压销的限位作用时就会从限位槽中弹出,给人们带来了方便。
CN202121910597.5硅钢冲压片质量筛查分拣装置
本实用新型涉及一种硅钢冲压片质量筛查分拣装置,包括:第一组传送带机构,第一摄像头,设置于第一组传送带机构的上方,用于对硅钢冲压片的第一表面的残损进行检测;第一机械手机构,设置于第一组传送带机构的上方且位于所述第一摄像头的后方;翻转装置,设置第一组传送带机构的后方,用于对第一组传送带机构传输的初检良品进行翻面并将翻面后的初检良品传输给第二组传送带机构;第二组传送带机构,设置于翻转装置的后方;第二摄像头,设置于第二组传送带机构的上方,用于对硅钢冲压片的第二表面的残损进行检测;第二机械手机构,设置于第二组传送带机构的上方且位于第二摄像头的后方。本实用新型可高效的检测每一个产品的外观质量。
CN202122999248.1一种无取向硅钢喷涂用即时干燥装置
本实用新型公开了一种无取向硅钢喷涂用即时干燥装置,包括干燥箱,所述干燥箱内滑动连接有加热台,所述干燥箱顶部设置有加热箱,所述加热箱左右两侧分别设置有进风管和出风管,所述进风管和出风管均与干燥箱连通,所述加热箱内部从左到有依次固定连接有风机和加热网,所述干燥箱内设有带式传送机,通过带式传送机使喷涂过后的硅钢在干燥箱中移动,首先经过加热台加热,使涂层表面干燥硬化,不会变形,然后再经过加热箱吹出的风对硅钢表面的涂层进行进一步的烘干,从而保证干燥过程中涂层不会起褶皱。
CN202111146383.X一种电磁屏蔽用1050铝/50W800无取向电工钢钢板生产方法
本发明提供一种电磁屏蔽用1050铝/50W800无取向电工钢钢板生产方法,包括S1)、将轧制好的铝卷和钢卷分别放置在两个开卷机上开卷;S2)、开卷后分别采用HCl、NaOH溶液清洗;S3)、用旋转钢丝刷法对铝板、钢板待结合面进行机械处理10‑15s;S4)、将铝板、钢板置于丙酮溶液中超声波清洗2‑3min;S5)、将表面处理后的铝板、钢板进行预拉伸或者预压缩,S6)、将预应力处理的铝板、钢板边部进行焊接;S7)、将焊接好的钢铝板进行轧前的预热处理;S8)、然后进行连续退火炉中进行退火处理,本发明将金属铝板、钢板通过热轧轧制复合化结合在一起,界面剪切强度≥100MPa,反复弯曲次数≥10次。