本发明公开了一种硅钢片横剪线裁切设备,包括:本体,所述本体包括工作台、挡屑罩和裁切装置,所述挡屑罩内水平固定安装有横杆,所述裁切装置与横杆下表面滑动连接;两个定位机构,所述定位机构包括第一螺纹杆、第一滑块和压板,所述挡屑罩内壁开设有两个安装槽,两根所述第一螺纹杆分别转动安装在两个安装槽内,两个所述第一滑块分别螺纹套设在两根第一螺纹杆上,两个所述压板分别与两个第一滑块远离安装槽槽底的一端水平固定链接;两个驱动机构,所述驱动机构用于控制第一螺纹杆发生转动。通过驱动装置控制定位机构中压板在垂直方向上的位置便可快速实现对硅钢片的定位工作和解除工作,方便快捷,提高了裁切工作的效率。
2021-03-18 122 6.8

6.5%Si硅钢具有优异的磁学性能和广泛的应用前景。本文综述了6.5%Si硅钢的物理、机械及磁学特性,讨论了传统轧制、温轧、薄带连铸、快速凝固、CVD、粉末轧制等不同制备工艺的关键技术及特点,概括了6.5%Si硅钢在高效节能电机、汽车马达及磁屏蔽等领域中的主要应用,介绍了硅钢的制备技术取得的研究进展,并指出了其广阔的发展前景。 6.5% Si silicon steel has good magnetic properties and wide applications.In this paper physical and mechanical magnetic properties were summarized,and key technology and characteristic of several preparation methods,such as traditional rolling,warm rolling,thin strip continuous casting,rapid solidification,CVD and powder rolling,were discussed.Main applications of 6.5% Si steel in the fields of high-efficiency electrical motors,automobile motors,transformer cores and magnetic shielding were gene... 
2012-06-28 150 5.8

【摘要】 <正>由西电集团、保定天威集团使用迁钢公...
2013-10-28 129 5.8

本发明公开了一种硅钢片激光曲线开料机,本发明涉及电力设备技术领域,目前现有的硅钢立体三角形卷铁芯的机械式斜度开料机在开料过程中精度差、效率低,且在硅钢片送料的过程中,长时间后硅钢片容易发生松散情况,同时只能对单一厚度的硅钢片进行输送工作,包括放料组件和开料组件以及收料组件,所述放料组件用于对硅钢片的放料工作,所述开料组件用于对硅钢片的开料工作,所述收料组件用于对硅钢片的收料工作。该硅钢片激光曲线开料机,通过利用高速激光曲线开料,效率高精度好,且硅钢片在输送的过程中,能够自动调整导向辊的位置,进而能够对硅钢片起到很好的导向作用,使其表面时刻为张紧状态,进而保证硅钢片的开料效果。
2021-12-28 191 6.8

本发明提供一种无取向硅钢低温无铬环保绝缘涂层立式干燥固化工艺,冷轧无取向硅钢在镀锌机组经过退火后,通过涂层机涂覆低温无铬环保绝缘涂层,再经过立式干燥炉完成干燥固化,生产冷轧无取向硅钢产品。低温无铬环保绝缘涂层厚度0.8~1.0μm;立式干燥炉各段炉温:加热一段炉温420~450℃,加热二段炉温460~490℃,加热三段炉温500~530℃,加热三段出口板温200~240℃,冷却段出口板温60~65℃;立式干燥炉各段加热时间:加热一段、加热二段、加热三段的加热时间均为3.5~4s。采用本发明工艺不仅能保证钢带涂层均匀,使最终产品的涂层具有优异的绝缘性、耐蚀性、附着性、冲片性、焊接性和耐热性,满足下游工序要求,还可提高产品合格率,减少废品,保证生产顺行。
2020-12-23 161 6.8

【作者】 朱传芳; 潘恒韬; ...
2023-05-11 252 5.8

薄带连铸流程下取向硅钢粗大λ晶粒(〈100〉//ND,normal direction)的“遗传”会导致磁性能恶化.为解决这一问题,针对取向硅钢的热轧孪生行为开展研究,结果表明:凝固组织粗大的取向硅钢在650℃热轧时可产生大量{112}〈111〉形变孪晶,这与具有高层错能的硅钢在较高温度下难以孪生变形的传统认知不同.热轧过程中复杂的应力状态降低了变形孪晶的取向依赖性,由于具有更高的储存能,孪晶界/孪晶界及孪晶界/晶界交叉点成为再结晶形核的优先位置,大大提高了常化过程中的再结晶率,受沿孪晶界应变分布及孪晶间距离的限制,沿孪晶界形核的再结晶晶粒通常呈“饼状”,最终形成以细小且取向漫散的再结晶晶粒为主的常化组织,消除了初始凝固组织中有害的粗大λ晶粒. In strip casting grain-oriented silicon steels, the inheritance of coarse λ grains(〈100〉//ND, normal direction) can deteriorate their magnetic properties. To solve the problem, twinning behaviors in strip casting grain-oriented silicon steels during hot rolling were investigated in this work. It is found that after rolling at 650 ℃, a number of {112}〈111〉deformation twins are formed in the coarse solidification microstructure of the steels, in contrast to the well-accepted view that it is diffic... 
2022-02-28 191 5.8

介绍了一种适用于超大晶粒取向硅钢的高斯晶粒取向偏离角的X射线衍射测量方法,提出了将试探法和探测器扫描法相结合的方式进行测量。结果表明:该方法可以同时获得准确的实际衍射角度和取向偏离角度,试样制备方式简单,对设备的要求低且测量结果准确。 This paper introduces a X-ray diffraction measurement method of Gaussian grain orientation deviation angle for ultra-large grain oriented silicon steel, and puts forward a method of combining the test method with the detector scanning. The results show that this method can obtain accurate actual diffraction angle and orientation deviation angle at the same time. The sample preparation method is simple, the requirements for equipment are low, and the measurement results are accurate. 
2022-02-28 156 5.8

本实用新型属于抛丸设备技术领域,具体涉及一种防飞料的硅钢抛丸设备,包括料仓和安装在料仓内的抛丸器,料仓的相对两侧上开有对称设置的通口,抛丸室内设有穿过两通口并向料仓室外延伸的输送辊道,输送辊道包括辊架和转动连接在辊架上的多个转辊;料仓的侧壁上滑动连接有用于封堵通口的挡料板,挡料板上设有用于固定挡料板的固定件;挡料板的下部内滑动连接有一端伸出挡料板的密封板,密封板与挡料板之间连接有弹性件。使用本方案,硅钢与通口之间的缝隙能被有效封堵,有效避免钢丸通过通口与硅钢之间的缝隙排出,提高抛丸设备的密封性,防止飞料。
2020-12-31 144 6.8

本发明涉及一种常化后免酸洗生产取向硅钢的方法,取向硅钢的生产工艺路线为:冶炼→连铸→热轧→常化退火→拉伸矫直→抛丸→冷轧→脱碳退火→渗氮→涂MgO→高温退火→热拉伸平整及涂绝缘膜;本发明在常化退火后通过物理方法去除带钢表面的氧化铁皮,且效率高、效果好、操作简单、易于控制;与常规工艺相比,省去了酸洗及后续废酸处理工作,排除了酸雾对环境的污染,消除了取向硅钢带因酸洗而产生的潜在缺陷,产品质量更加稳定可靠。
2021-02-09 145 6.8

本实用新型公开了一种变压器铁芯硅钢片的收片装置,包括固定平台、硅钢片出料机构、压片机构、支撑平台和升降调节机构,所述固定平台设置在硅钢片出料机构的出料端下方,所述压片机构对应于硅钢片出料机构的出料口设置在硅钢片出料机构的上方,从所述硅钢片出料机构传送出的硅钢片通过压片机构压覆在固定平台上;所述固定平台上设置有升降调节机构,所述升降调节机构的升降端设置有支撑平台,所述支撑平台相对于固定平台在竖向方向上位移调节设置,能够对硅钢片叠放平面进行高度调节,保证出料高度的一致性,使得出料规整性较好。
2021-12-28 188 6.8

本发明公开了一种降低无取向硅钢W800头部窄尺的控制方法,步骤1、筛选板坯长度,并使板坯进入加热炉后头部均朝向轧机方向;步骤2、控制板坯头部温差小于10℃;步骤3、固定粗轧到精轧区间内的轧机机架轧制速度;步骤4、固定相变机架,使板坯的奥氏体‑铁素体相变发生在F2和F3机架中;步骤5、调整精轧机架间的负荷分配,降低F2和F3机架的压下量;步骤6、调整活套张力,降低F2和F3机架的活套单位张力补偿;步骤7、降低模型AGC增益,降低F2和F3机架的AGC补偿的辊缝波动量。本发明通过控制固定相变机架、优化相变机架的负荷分配、AGC补偿系数、活套张力等,使秒流量保持平衡,减少无取向硅钢W800头部窄尺。
2021-12-27 206 6.8