  • 未分类

本实用新型公开了用于变压器铁芯硅钢片的叠片翻转支架,包括槽板,所述槽板内部卡装有转板,转板两侧对称安装有卡杆,槽板底部安装有风扇;所述转板另外两侧对称安装有放置槽,放置槽底部卡装有电磁铁,转板两侧皆设置有两组开关;在开关不受到压力时,此时开关所在电路处于通电状态,开关与电磁铁为电性连接,每个开关独立控制一组电磁铁,电磁铁处于工作状态,电磁铁正常运行产生的磁吸力,使得铁芯硅钢片固定在放置槽内,在使用机械臂取用铁芯硅钢片时,机械臂底部连接的触发条持续压迫开关,此时开关所在电路处于断路状态,开关所控制的相应电磁铁不产生磁力,机械臂可以较为容易的取用铁芯硅钢片。
2021-12-28 211 6.8

以取向电工钢成分为基础,制备了含C或Mn和S的4种实验钢。观察了接近平衡析出状态实验钢经60%冷轧后在600~1000℃范围再结晶退火过程中微观组织演变,统计分析了再结晶体积分数随退火时间的变化规律,进而计算了各实验钢静态再结晶的激活能。观察了高含C实验钢退火初期再结晶晶粒优先出现的部位。结果表明900~1000℃范围内各实验钢铁素体的化学成分相似,因而其再结晶激活能基本一致。在600~800℃范围内铁素体内会有阻碍再结晶进程的三次渗碳体析出,从而使再结晶激活能明显提高。高C含量实验钢中还会有从奥氏体转变而来的粗大珠光体或渗碳体,轧制过程中其附近形成的变形区会促进600~800℃加热时该区域附近率先发生再结晶形核、降低再结晶激活能。固溶的Mn、S元素可微弱提高再结晶激活能,但高Mn、S含量会改变粗渗碳体从奥氏体析出时的形态。 Four experimental steels based on grain oriented electrical steel containing C,or Mn and S were prepared.Microstructure evolution of the steels close to a state of equilibrium precipitation were observed during annealing processes at 600-1000 ℃after 60% cold rolling,the changes of recrystallization volume fraction were analyzed statistically as the annealing was prolonged,and the activation energy for static recrystallization of the steels were calculated.The locations,where the recrystallizatio... 
2011-12-28 206 5.8

本发明公开了一种自主学习的高硅钢软磁复合铁芯智能化生产系统及生产方法,属于软磁复合铁芯智能化生产技术领域。本发明的生产系统包括数据输入模块、数据分析模块、数据输出模块、通信模块、数据修正模块;生产方法为:用户通过输入模块选择目标性能参数及生产控制模式,系统生成生产过程关键参数,并由输出模块输出给用户;用户确认后形成控制指令,并发送至生产设备进行生产。本发明的系统不仅能够根据高硅钢铁芯产品的目标性能参数自动生成合理的操作条件,还能根据历史数据和产品检化结果对系统内置的关系模型不断进行优化、完善,能够有效提高产品产量和质量、减少浪费、降低成本。
2021-03-26 212 6.8

根据本发明的一个实施例的无取向电工钢板,以重量%计,所述钢板包含Si:2.1至3.8%、Mn:0.001至0.6%、Al:0.001至0.6%、Bi:0.0005至0.003%和Ge:0.0003至0.001%,余量包含Fe和不可避免的杂质。
2020-12-17 255 6.8

【作者】 安斌; ...
2014-09-28 206 5.8

6.5%Si电工钢是一种优异的软磁材料,织构对其磁性能影响很大。利用温轧工艺对6.5%Si电工钢热轧板进行不同压下率轧制,研究了温轧板织构随压下率的变化规律。实验结果显示,随着压下率的增大,{100}〈110〉、{110}〈100〉和γ纤维织构在薄板表层中的强度先增强后减弱,当压下率达到75%时,沿板厚方向形成3个组织区域:表层细晶粒区({110}〈100〉取向为主)、过渡层({111}〈110〉和{111}〈112〉变形晶粒区)和中心层(以拉长的γ纤维织构和{100}〈110〉取向晶粒为主),这种组织和织构不均性对后期织构的发展有重大影响。 6.5wt% Si electric steel has excellent soft magnetic properties,on which texture play important role.In this experiment,warm rolling technique was employed to investigate the effect of rolling reduction on texture.It was found that the density of {100}〈110〉,{110}〈100〉 and γ-fiber textures first increased and then decreased with increasing of the rolling reduction.At 75% reduction,the microstructure along the thickness of the sheet formed three zones,containing surface layer with {110}〈100〉 orien... 
2023-05-09 250 5.8

本实用新型公开了一种硅钢片加工装置,涉及硅钢片加工领域,包括底板,所述底板的上方左右两端固定连接有液压伸缩杆,所述液压伸缩杆的顶部固定连接有连接板。该硅钢片加工装置,可灵活调节两组打孔机之间的距离,可使用该加工装置加工出不同孔距的硅钢片,也即可加工出所需不同种类的硅钢片,加工灵活性强,使用范围广泛,通过开启电机,最终可使得两组打孔机同时进行向内侧或外侧进行移动,实现调节硅钢片两组打孔的位置。
2021-04-21 163 6.8

抑制回硅是低硅品种钢冶炼的重点和难点,南钢中厚板卷厂通过转炉出钢弱脱氧操作,精炼炉弱脱氧升温,脱氧、脱硫造渣,连铸严格的保护浇注及吹氩塞棒、吹氩浸入式上水口的应用等一系列工艺优化和操作的改进,使整个冶炼过程钢水回硅量稳定控制在200×10-6以内,钢水终点成分完全满足低硅钢要求。 Control of increasing silicon is the emphasis and difficulty in low silicon varieties steel smelting.The Nisco Wide Plate/Coil Plant can control the silicon content in molten steel keeping within 200×10-6 through whole steelmaking process by using oxygen residual operation in converter tapping,oxygen residual and increasing temperature,deoxidation,desulfurization,slag refining,protection cast,blowing argon by plugged nozzle,blowing argon by submerged entry nozzle in continuous casting,and other ... 
2013-05-28 156 5.8

采用双辊薄带连铸工艺制备了厚度为2.4mm的3.98%Si-0.71%Al无取向硅钢带,经常化、冷轧、不同温度退火后,对其显微组织、析出物、织构和磁性能进行了检测分析。结果表明:随着退火温度的提高,退火板晶粒尺寸增大,组织均匀性提高;退火板析出物主要是AlN和MnS与AlN复合析出物,尺寸较粗大,达0.5~2.5μm;退火板织构沿厚度方向变化明显,表层和1/2层存在较强的{100}织构,1/2层还存在较强的{111}织构,1/4层主要是{112}织构;随退火温度的升高相应的铁损和磁感应强度均降低。 Using twin roll thin strip continuous casting technique,the 3.98%Si-0.71%Al no-oriented silicon steel strip in thickness of 2.4mm was produced.The microstructure,precipitates,texture,and magnetic properties of the sheet after normalizing,cold rolling and annealing at different temperatures were studied.The results show that with annealing temperature increase,the grain size and uniformity of annealed sheet increased.The main precipitates in coarse size of 0.5-2.5μm in annealed sheet were AlN and... 
2014-01-28 171 5.8

通过对3%Si CGO硅钢进行恒变形速率、不同变形温度下的单道次压缩实验,结合Thermal-Calc软件,金相分析,SEM及EBSD技术,研究了取向硅钢热变形过程中组织和微观织构的变化规律。结果表明:实验钢是在双相区变形,变形后组织主要是铁素体和少量的珠光体。随变形温度的升高,晶粒由长条状变为等轴状,尺寸逐渐变大;CGO硅钢在热变形过程中立方{100}<001>取向是较为稳定存在的。随着变形温度的提高,{111}<110>等取向逐渐转向{110}<1 10>取向,且{110}<1 10>取向逐渐变得锋锐。 3% Si CGO silicon steel was studied at constant strain rate and different deformation temperatures by single-pass compression deformation experiments to reveal the evolution of microstructure and texture during thermal deformation in oriented silicon steel,and the Thermal-Calc software,metallurgical,SEM and EBSD technique was used in the experiment. The results show that experimental steel is deformed at the temperatures of two-phase zone. The microstructure of the deformed steel consists of fer... 
2014-05-28 212 5.8

本发明公开了一种硅钢片宽度偏差检测装置及其检测方法,属于硅钢片检测领域。一种硅钢片宽度偏差检测装置,包括检测装置上的第一输送机体,还包括:多个均匀分布的隔板,均固定安装在第一输送机体的皮带表面;开槽,设置在所述第一输送机体的侧壁;装置盒,通过上下滑动机构与所述第一输送机体连接,其中,所述装置盒内通过顶紧机构滑动安装有滚轮;第一支架,固定安装在第一输送机体的侧壁;装置板,通过转轴转动连接在第一支架的侧壁,所述转轴位于装置板的侧壁中部,所述装置板两端设有自动推料机构;本发明中的硅钢片宽度偏差检测装置不仅可以更高精度的检测硅钢片的宽度,并且还能将不达标的硅钢片自动筛选出来,使用更加的方便。
2021-06-28 206 6.8

本发明涉及取向硅钢高温连续退火炉领域,尤其涉及一种取向硅钢高温连续退火炉隔离装置,包括安装在炉壳上的隔离炉门及设置在隔离炉门四周的密封井;隔离炉门顶部两侧安装有水冷却装置;水冷却装置上部设有隔离炉门动力牵引装置;密封井包括固定密封井和伸缩密封井,伸缩密封井位于固定密封井内部并与固定密封井滑动连接,伸缩密封井与固定密封井端部连接处设有密封装置。本发明可以确保隔离炉门升降过程中实现无缝全密封状态,提高密封效果,且采用伸缩密封井实际降低了密封井的高度,间接降低了水冷却装置连接管道上升至最高点的净空标高,与传统固定式密封井高度相比可以降低高度50%~80%,从而降低厂房净空标高,节省厂房基建投资。
2021-12-18 201 6.8