  • 未分类

利用背散射衍射技术(EBSD)和XRD,研究了两段式脱碳退火工艺对取向硅钢纵截面初次再结晶的微区取向、取向差分布、特殊晶界(CSL)及高温退火试样高斯织构。分析了初次再结晶晶界特征对取向硅钢高温退火后宏观织构的影响。结果表明:初次再结晶的纵截面基体中Σ3和Σ5晶界使得高斯晶粒有着较高的迁移率,在高温退火时借助20o~45°的大角度晶界的界面能吞并周围{111}<112>晶粒迅速长大,形成密度水平较高的高斯织构。 Micro area orientation of primary recrystallization,the misorientation distribution,special boundaries under different two-stage decarburization annealing and the Goss texture under high temperature annealing the longitudinal section of grain-oriented silicon steel were detected by electron back scattering diffraction(EBSD) and X-ray diffraction(XRD).The effect of primary recrystallization grain boundary on macrotexture after high temperature annealing was analyzed.The results show that the Σ3 a... 
2023-05-11 247 5.8

本发明提供的一种耐热型低损耗取向硅钢,取向硅钢的单面采用激光刻痕形成平行线状沟槽;所述激光刻痕为取向硅钢制备工艺中的渗氮步骤之后和在涂覆MgO涂层步骤之前实施;在渗氮步骤之后和在涂覆MgO涂层步骤之前进行激光刻痕加工不会破坏高温退火后形成的硅酸镁底层,底层完整性好,刻痕形成的沟槽位于取向硅钢带材金属基体表面,在高温退火过程中沟槽内直接反应生成硅酸镁底层,最终取向硅钢带材表面涂覆张应力涂层后光滑、平整、无凹凸,取向硅钢带材损耗低、叠片系数高、耐热,成品取向硅钢带材既可用于制备立体卷铁心变压器也可用于制备叠片铁心变压器。
2021-11-23 159 6.8

对高磁感取向硅钢冷轧板分别进行800、950、1050和1120℃不脱碳的预退火处理,在800℃预退火,成品的磁性能较好。织构分析的结果表明,随着预退火温度升高,初次再结晶后有利织构组分{111}<112>与不利织构组分(118)[110]的比值f(111)/f(118)逐渐降低,初次再结晶织构的变化是成品磁性的影响因素之一。 Preliminary annealing process at different temperatures for cold-rolled strips of a high permeability grain-oriented silicon steel was investigated to study the effect of the annealing temperature on microstructure and magnetic performance of the steel.Results show that the magnetic performances of the products annealed at 800 ℃ are best.Analysis of primary recrystallization texture indicates that with rising temperature,f(111)/f(118) which is the ratio of the favorable component {111}<112>... 
2013-03-28 148 5.8

本实用新型公开了一种薄带取向电工钢的热处理炉板,炉板的中心设置有气流循环通孔,炉板的硅钢卷预定压接面设置有通气槽,炉板内设置有进气孔,进气孔的第一孔口设置于通气槽中,进气孔的第二孔口设置于炉板的侧壁上。该薄带取向电工钢的热处理炉板在设置通气槽的基础上,进一步设置进气孔,通过向进气孔中导入气流,增加通气槽的进气量,有助于硅钢卷与炉板压接侧边处水蒸气的及时排出,进一步提高卷内硅钢的热处理品质。本实用新型还公开了一种包含热处理炉板的薄带取向电工钢罩式炉。
2021-08-28 159 6.8

为了确定普通冷轧取向硅钢最优的中间完全脱碳退火工艺,在其一次冷轧后进行5种不同工艺的脱碳退火处理,借助扫描电镜及电子背散射衍射技术研究了不同工艺脱碳退火后的组织、织构和脱碳效果。结果表明:经5种工艺脱碳退火处理后,初次再结晶的平均晶粒尺寸均约为19μm,且不随退火温度和时间的变化而变化;经840℃×10min工艺退火后的晶粒最均匀,高斯织构位向更准确,高斯织构面积分数最多,为3.1%,可将碳脱至0.003 5%。 In order to determine the optimal intermediate complete decarburizing annealing processes for common grain-oriented(CGO)silicon steel,five kinds of intermediate decarburizing annealing processes were conducted,the microstructure,texture and decarbonization after different decarburizing annealing processes were studied by scanning electron microscopy and electro back-scattered diffraction(EBSD)technology.The results show that the average grains sizes of primary recrystallization were about 19μm a... 
2013-11-28 160 5.8

采用化学气相沉积(CVD)渗硅处理工艺连续制备6.5%Si高硅钢,具有优质的软磁性能,通过理论研究化学反应并且用简单的试验设备做进一步的探讨。根据试验的结果对连续制备6.5%Si高硅钢的CVD工艺构造提出全面、有效的建议,实现制备6.5%Si高硅钢系统。 CVD method for continuously manufacturing 6.5%Si Steel Sheet has excellent soft magnetic.Carried out a theoretical study of related chemical reaction and performing basic research with a simple test apparatus.Based on the results,finally proposed an overall process configuration to realize such a production-CVD method for continuously manufacturing 6.5%Si Steel Sheet. 
2011-12-28 161 5.8

采用X射线衍射仪分析无取向硅钢冷轧织构和再结晶退火织构的演化,研究了热轧组织对无取向硅钢织构以及磁性能的影响。结果表明,具有均匀、粗大晶粒组织的热轧板,冷轧形成更多的剪切带,导致成品板形成高的高斯织构组分,并提高了{100}织构强度,降低了γ纤维织构,最终导致成品磁感应强度升高,铁损下降。 The texture evolution of non-oriented silicon steel during cold-rolling and recrystallization annealing was investigated by X-ray diffractometer.The effects of hot band microstructure on the texture and magnetic properties of non-oriented silicon steel were analyzed.The results show that more shear bands appear during cold rolling due to homogeneous coarse grain in hot band.So strong{110}<001> texture after recrystallization annealing forms.At the same time,the {100} texture components inc... 
2023-05-09 214 5.8

本实用新型公开了一种高磁感取向硅钢用钢带纠偏装置,包括支架,所述支架的顶部外壁通过螺栓固定连接有传送电机、安装柱和固定板,所述安装柱的顶部外壁通过螺栓固定连接有侧边板,所述侧边板的两边内壁均开有滑动槽,所述滑动槽的内壁通过螺钉固定连接有滑动轨道,所述滑动轨道的内壁滑动连接有滑动板,所述侧边板的一侧内壁设有推力弹簧,所述滑动板的底部外壁通过轴承连接有抵边轮。本实用新型对带钢产生更大的推力,使得带钢归位,推力弹簧的弹性使得装置对带钢的力比较缓和,不易使得带钢形变,顶压板和防抖轮会在带钢的顶部对带钢施加一个垂直向下的压力,使得带钢在运输过程中不易上下抖动。
2021-05-12 458 6.8

以构建高磁感、低铁损、免轧制高硅电工钢铁芯为出发点,提出采用单辊甩带制备非晶铁硅合金薄带、微氧化法在铁硅合金粉末表面包覆高电阻率铁硅氧化物薄膜制备核壳异质结构高硅电工钢纳米粉末、放电等离子烧结快速成形制备颗粒间绝缘的高硅电工钢铁芯。研究了不同氧化包覆时间对SPS烧结试样密度、物相组成、微观结构和静磁性能的影响。研究表明,在氧化包覆5h烧结温度800℃工艺条件下,制备的6.5%Si高硅电工钢铁芯的静磁性能最佳,饱和磁化强度为128.84A.m2/kg、矫顽力为2.25kA/m、剩磁为3.47A.m2/kg。其饱和磁化强度与粉末压延法制备的高硅钢相当,但矫顽力降低了1/3。 The paper takes preparation 6.5%Si steel with high induction,low core loss and removing rolling as the starting point,amorphous Fe-Si ribbons was synthesized by melt spinning method,6.5%Si steel nanopowders with high resietivity core shell structure was prepared by the slight oxidation process and 6.5% Si steel iron core with evaluating internal was sintered by spark plasma sintering process(SPS).The essay focuses studies the effects of different oxidation cladding time on sample density,phase c... 
2013-10-28 136 5.8

本发明涉及一种变压器铁芯制造硅钢片绝缘涂装方法,其使用了一种涂装设备,该涂装设备包括基座、支撑架、转动装置、下降装置、滚涂装置与涂装仓,通过顺时针转动转动环,转动环转动带动齿轮转动,从而实现两个支撑弧形板展开的每个硅钢片进行内部支撑,通过向右推动推杆,从而对每个硅钢片进行阻隔,开启驱动电机,驱动电机输出端带动中心转轴转动,使滑动杆向下移送时带动匚型架向下移动,实现对匚型架内的硅钢片进行浸涂,匚型架向上移动时由于弹簧的作用力进行上下摆动,从而对硅钢片上多余的绝缘漆进行摆掉,开启电动推杆向前移动,从而对支撑弧形板外侧的多个硅钢片进行表面滚涂,避免硅钢片表面在浸涂绝缘漆时产生凸块。
2021-01-14 122 6.8

冷轧无取向硅钢是高技术含量、高附加值产品,工艺复杂,生产周期长,过程控制难度大,被誉为钢铁产品中的\"工艺品\"。热轧生产工艺又是无取向硅钢生产的重中之重,直接决定了硅钢的铁损和电磁性等多项指标。 Cold rolled non-oriented silicon steel is high technology content、high addedvalue product. Its process is complex, Its production cycle is of Length, and Its Process control is difficult. Which is known as the iron and steel products \" Arts and crafts\". Hot rolling production process is the top priority of non-oriented silicon steel, Which Directly determines iron loss of the silicon steel and electromagnetic property, etc many index. 
2023-05-09 231 5.8

本发明涉及一种永磁电机铁芯电工钢材料优化匹配方法及系统,涉及电机技术领域,包括根据永磁电机的应用场合,确定设计指标和永磁电机模型,并根据永磁电机模型确定电机性能;判断永磁电机的电机性能是否符合设计指标,若是确定第一集合、第二集合以及第三集合的交集;该交集的元素为永磁电机的电机性能满足第一指标、第二指标以及第三指标时对应的硅钢材料。本发明综合考虑了电机的电磁场、温度场、应力场性能,可以在多种电工钢材料中选出与该种转子结构匹配度最高的电工钢材料。
2021-08-24 194 6.8