钢厂
微合金元素对冷轧取向电工钢再结晶行为的影响
以取向电工钢成分为基础,制备了含C或Mn和S的4种实验钢。观察了接近平衡析出状态实验钢经60%冷轧后在600~1000℃范围再结晶退火过程中微观组织演变,统计分析了再结晶体积分数随退火时间的变化规律,进而计算了各实验钢静态再结晶的激活能。观察了高含C实验钢退火初期再结晶晶粒优先出现的部位。结果表明900~1000℃范围内各实验钢铁素体的化学成分相似,因而其再结晶激活能基本一致。在600~800℃范围内铁素体内会有阻碍再结晶进程的三次渗碳体析出,从而使再结晶激活能明显提高。高C含量实验钢中还会有从奥氏体转变而来的粗大珠光体或渗碳体,轧制过程中其附近形成的变形区会促进600~800℃加热时该区域附近率先发生再结晶形核、降低再结晶激活能。固溶的Mn、S元素可微弱提高再结晶激活能,但高Mn、S含量会改变粗渗碳体从奥氏体析出时的形态。 Four experimental steels based on grain oriented electrical steel containing C,or Mn and S were prepared.Microstructure evolution of the steels close to a state of equilibrium precipitation were observed during annealing processes at 600-1000 ℃after 60% cold rolling,the changes of recrystallization volume fraction were analyzed statistically as the annealing was prolonged,and the activation energy for static recrystallization of the steels were calculated.The locations,where the recrystallizatio...
CN202123158104.X一种变压器铁芯加工用硅钢片裁剪装置
本实用新型涉及变压器铁芯加工的技术领域,特别是涉及一种变压器铁芯加工用硅钢片裁剪装置,其可提高下料的便利性,同时提升工作效率;包括操作台、集料板、气缸、底架、两组立板、电机、从动轴、传送带、缓冲座、两组高弹簧和两组低弹簧,操作台底端设有四组支腿,操作台顶端设有送料组件和裁剪机,操作台上设有下料口,集料板转动安装在下料口内,气缸顶端和操作台底端固定连接,集料板底端滑动设有铰接座,气缸的输出端和铰接座铰接,立板通过两组立板固定安装在操作台底端,电机固定安装在底架前端,电机的输出端设有主动轴,主动轴转动安装在底架内,从动轴转动安装在底架内,主动轴和从动轴之间通过传送带传动连接。
CN202180015376.8无取向性电磁钢板用钢板
提供一种如下的无取向性电磁钢板用钢板:含有:C:0.0040%以下、Si:1.9%以上3.5%以下、Al:0.10%以上3.0%以下、Mn:0.10%以上2.0%以下、P:0.09%以下、S:0.005%以下、N:0.0040%以下、B:0.0060%以下;剩余部分由Fe和杂质构成;分别从板宽方向的两端部向板宽中央10mm的各位置的板厚方向截面组织的重结晶率不足50%;将板宽记为W时,分别距板宽方向的两端部1/4W的位置的板厚方向截面组织的重结晶率在50%以上。
退火温度对2%Si无取向电工钢磁性能的影响
研究了传统工艺流程生产的2%Si无取向电工钢在不同退火温度下的磁性能。研究结果表明,随着退火温度的升高,显微组织均匀性提高且晶粒尺寸增大;有利织构组分{100}<0vw>、α、η增强,不利织构组分减弱;成品的铁损P1.5/50先下降后略有上升,磁感B50上升平缓;在890℃×2 min的退火工艺条件下,成品电工钢的磁性能最佳,对应的铁损P1.5/50小于3.2 W/kg,磁感B50高于1.74 T。 In this paper,the effect of annealing temperature on magnetic properties of non-oriented electrical steel with 2% silicon was studied.Results show that the uniformity of microstructure and the average grain size increase with the rise of annealing temperature.The texture components of annealing can be improved by enhancing {100} <0vw>,α,η fiber textures and weakening {111} <112> fiber texture.The tendency of core loss P1.5/50 shows that it decreases first and then increases,while the...
CN202111182553.X一种多组分{100}织构无取向电工钢的制备方法
本发明涉及冶金技术领域,具体涉及一种多组分{100}织构无取向电工钢的制备方法。本发明通过控制薄带连铸参数制备1.5~2.5mm厚的无取向电工钢铸带,直接冷轧至厚度为0.35~0.50mm后,先进行预回复退火,再进行成品退火,此过程中控制退火温度、时间以及升降温速率。本发明所制备的无取向电工钢具有多组分{100}织构,包括{100}&lt;001&gt;、{100}&lt;012&gt;和{100}&lt;011&gt;,{100}织构组分体积分数达到25~39%,其轧向磁感值1.71~1.78T,横向磁感值1.70~1.76T,板面45°方向磁感值达到1.65~1.67T。本发明通过优化退火工艺,利用{100}变形组织的强回复与再结晶协同作用,从而显著增强{100}退火织构,方法简单有效。
CN202011640274.9一种叠片装置以及硅钢片收料设备
本发明公开了叠片装置,以及采用该叠片装置的硅钢片收料设备,包括分料装置和本发明第一方面实施例的叠片装置,分料装置包括有分料件、上分料传送带和下分料传送带,上分料传送带的一端和下分料传送带的一端与分料件连接,分料件用于将硅钢片分别输送至上分料传送带和下分料传送带,本发明第一方面实施例的叠片装置,叠片装置的数量为两个,两个叠片装置上下平行设置,并且分别与上分料传送带和下分料传送带的远离分料件的一端连接。根据本发明的叠片装置,以及采用该叠片装置的硅钢片收料设备,可实现硅钢片的自动叠片,提高生产效率。
CN202121016000.2一种冷轧取向硅钢带整平装置
本实用新型公开了一种冷轧取向硅钢带整平装置,包括两个上下对称分布的保护罩,所述保护罩的内部均转动连接有展平辊,且展平辊的一端均延伸至保护罩的外部,所述保护罩的外壁设置有传动罩,且传动罩的外壁设置有动力箱,所述动力箱与展平辊传动连接,上下两个所述展平辊之间设置有其,特征在于,所述保护罩的两侧外壁均固定连接有支撑架,且支撑架的一侧外壁均设置有延展机构,两个所述延展机构之间设置有连接架,且连接架的一侧外壁设置有吸水布,所述吸水布的内部设置有胶板。本实用新型吸水布与硅钢带本体的外壁滑动接触,以此将展平时涂抹在硅钢带本体表面的水溶性润滑剂刮抹掉,减少硅钢带本体表面上的水分。
高硅钢薄板退火过程中的织构演变
采用传统的轧制和退火工艺制备了0.30mm厚的6.5%(质量分数)Si高硅电工钢薄板,采用X射线衍射技术对退火过程中的再结晶织构进行了研究。冷轧高硅钢薄板700℃退火形成以{111}〈112〉为峰值的γ织构(〈111〉∥ND)和以{001}〈210〉为峰值的{001}织构;而900℃以上温度退火则形成强{001}〈210〉织构。进一步的研究表明是在晶粒长大过程中{001}〈210〉发展成为主要再结晶织构组分。 High silicon steel thin sheets with thickness of 0.3mm were successfully produced by conventional rolling and annealing methods.Recrystallization texture was investigated by means of X-ray diffraction.It is found that recrystallization texture is mainly composed of γ fiber(〈111〉∥ND)with peak at {111}〈112〉 and {001} fiber with peak at {001}〈210〉 after annealing at 700℃,while strong {001}〈210〉 component dominates recrystallization texture after annealing above 900℃.It is during grain growth that {...
CN202123201670.4一种取向硅钢高温连续退火炉隔离装置
本实用新型涉及取向硅钢高温连续退火炉领域,尤其涉及一种取向硅钢高温连续退火炉隔离装置,包括安装在炉壳上的隔离炉门及设置在隔离炉门四周的密封井;隔离炉门顶部两侧安装有水冷却装置;水冷却装置上部设有隔离炉门动力牵引装置;密封井包括固定密封井和伸缩密封井,伸缩密封井位于固定密封井内部并与固定密封井滑动连接,伸缩密封井与固定密封井端部连接处设有密封装置。本实用新型可以确保隔离炉门升降过程中实现无缝全密封状态,提高密封效果,且采用伸缩密封井实际降低了密封井的高度,间接降低了水冷却装置连接管道上升至最高点的净空标高,与传统固定式密封井高度相比可以降低高度50%~80%,从而降低厂房净空标高,节省厂房基建投资。
CN202111389801.8一种硅钢级氧化镁制备方法、硅钢级氧化镁保护膜
本发明公开一种硅钢级氧化镁制备方法、硅钢级氧化镁保护膜,涉及氧化镁制备技术领域。将得到的粗氧化镁产品进行净化处理;将净化处理后的粗氧化镁产品与金属镁碳还原剂,在真空状态下,利用真空碳热还原技术进行金属镁的置换,制得金属镁;金属镁碳还原剂与粗氧化镁产品的质量比为(1~1.5):1;制得的金属镁在纯氧下制得氧化镁;将制得氧化镁根据实际需求获得不同粒径硅钢级氧化镁颗粒。本发明产品各项指标优于企业标准的硅钢级氧化镁。而且不会受原料中含有的钙等杂质的影响,产品纯度很容易达标,同时,还存在能耗较低、生产成本低等优点,解决了业在降低能耗方面的突破可应用于工业化生产。
电工钢热压缩时动、静态再结晶组织及取向分析
采用热模拟方法及EBSD技术,研究Fe-3 wt%Si电工钢在不同温度下组织的动、静态再结晶及晶粒取向特征,特别是少量奥氏体对铁素体动、静态再结晶组织及取向的影响。结果表明,不同温度形变的组织主要分三类:形变长条铁素体、珠光体和等轴细小铁素体。长条形变铁素体内发生动态回复或连续式的动态再结晶,奥氏体周围的铁素体动态再结晶加速,部分以传统的不连续方式动态再结晶。铁素体、奥氏体都可发生静态再结晶。奥氏体的静态再结晶在1050℃以上明显,铁素体的静态再结晶随温度的升高逐渐进行,最显著的再结晶发生在1050℃。不同温度形变的样品,其形变晶粒取向主要以<111>和<100>为主,小等轴铁素体晶粒除与大形变铁素体取向相近外,出现了<110>取向及其它取向。 Static and dynamic recrystallization and grain orientations in a hot-compressed Fe-3 wt% Si electrical steels were studied at different temperatures using Gleeble simulator and EBSD technique,particularly focusing on the effect of small amount of austenite on ferritic microstructure and orientations.The results show that microstructure of the compressed steel,depending on deformation temperature,consisted of elongated and deformed ferrite,pearlite and fine equal-axed ferrite.The elongated ferrit...
CN202122033237.8一种硅钢片图像采集装置
本实用新型涉及一种硅钢片图像采集装置,在固定支架上设置有工业相机,所述的工业相机可以沿垂直方向上下移动或者沿水平方向前后移动,通过上下移动或者前后移动对硅钢片的形状和尺寸、硅钢片叠积形成的铁芯进行实时图像采集。固定支架包括:固定底座、支撑杆和工作台面,一对固定底座平行对称设置,所述的固定底座上对称设置两条竖直支撑杆,竖直支撑杆的上端面固定连接工作台面,在两条竖直支撑杆的中间位置设置升降丝杆,水平支撑杆的两端分别与升降丝杆的升降螺母固定连接,相机滑台活动设置在水平支撑杆上。本实用新型通过工业相机的上下前后移动,实现了硅钢片形状尺寸和硅钢片高度即时拍照测量,较人工测量提高了测量精度及准确性。