钢厂
辉光放电发射光谱法测定电工钢中8种元素
通过对辉光放电发射光谱法分析电工钢样品光谱行为的研究,分析其工作参数如:电压、电流、预溅射时间和积分时间对光谱强度和稳定性的影响,并以铁为内标元素,优化了工作参数。确定了直流辉光放电光谱法测定电工钢中碳、硅、锰、磷、硫、铬、镍、铜共8种元素的定量分析方法,并对该方法分析的精密度和准确度进行验证,结果表明,各元素的测定结果与认定值和其他方法测定值一致,测量元素结果RSD值小于2%。 Based on research on analyzing the spectrum behavior of the sample taken from the electrical steel by glow discharge optical emission spectrometry,the effect of its operational parameters such as current,voltage,pre-sputtering time and integrating time on the spectral intensity and spectral stability is analyzed.Taking the Fe as an element applied by internal standard method,these operational parameters are optimized,and therefore the quantitative analysis method for testing eight kinds of eleme...
Al含量对2.2%Si无取向硅钢组织、织构和磁性能的影响
通过实验室25 kg真空感应炉冶炼和锻轧研究了0.26%~0.95%Al含量对0.5 mm 2.2%Si无取向硅钢冷轧板组织、织构和磁性能的影响。试验结果表明,0.26%~0.81%Al含量时,随钢中Al含量的增加,成品退火钢板的晶粒尺寸增加同时铁损减少;当Al含量大于0.81%时,随Al含量增加,钢板的晶粒尺寸减小,同时铁损增加。Al含量对硅钢板磁感的影响没有明显的规律。2.2%Si无取向硅钢的合适Al含量为0.48%~0.81%。 The effect of 0.26%~0.95%Al content on structure,texture and magnetic performance of 0.5 mm cold rolled sheet of 2.2%Si non-oriented silicon steel has been studied by a 25 kg vacuum induction furnace smelting,and forging -rolling in laboratory.Results show that as 0.26%~0.81%Al,with increasing Al content in steel the grain size of annealed finished sheet increases while iron loss of sheet decreases,and as Al content in steel is more than 0.81%,the grain size of sheet decreases while iron loss in...
CN202210229033.8一种半无机硅钢片漆
本发明公开了一种硅钢片漆,该硅钢片漆采用特定的聚酰胺酰亚胺乳液制备,通过使偏苯三酸酐与组合形式的双端氨基化合物反应,添加三乙胺进一步提升反应进行的程度,并赋予整体更好的柔性和韧性,而磷酸三丁酯能够进一步通过物理改性改善体系的韧性,之后蒸出全部的有机溶剂,并添加一定量的水溶性有机溶剂,然后加入组合形式的活化剂,混合,再滴入水,形成稳定的乳液,最后添加双马来酰亚胺封端剩余的活性基团,该硅钢片漆不仅可以采用水作为主体溶剂,提升了环保型,而且还兼具耐高温、高粘结强度、电气性能强等优点,并有好的环境抗性与施工性能。
冷轧工艺对取向硅钢初次再结晶织构的影响
研究了取向硅钢制备过程中常见的两种冷轧工艺,主要研究了一阶段冷轧与两阶段冷轧+中间退火工艺对初次再结晶组织及织构的影响.结果表明:采用两阶段冷轧+中间退火工艺制备以Cu2S为主抑制剂的取向硅钢,其初次再结晶平均晶粒尺寸为18.1μm,高斯晶粒的体积分数为0.6%,迁移性强的重位点阵晶界(Σ5+Σ9)和高能晶界(20°~45°取向偏差角)所占比例分别为1.8%和50.4%.与一阶段冷轧工艺相比,其初次再结晶晶粒较细,且高斯晶核与特征晶界所占的比例较高,有利于高斯晶粒发生二次再结晶. Two common cold-rolling processes of grain oriented silicon steel and the effects of the single stage cold rolling and tw o-stage cold rolling w ith intermediate annealing processes on the primary recrystallization microstructure and texture w ere investigated. The results revealed that for the grain oriented silicon steel prepared under the tw o-stage cold rolling process w ith intermediate annealing w ith Cu 2 S as the main inhibitor,the average grain size of the primary recrystallization micr...
CN202111332457.9一种无取向硅钢用涂层溶液及其制备方法和应用
本发明提供一种无取向硅钢用涂层溶液及其制备方法和应用,以所述无取向硅钢用涂层溶液的总质量为基础计,所述无取向硅钢用涂层溶液包括如下质量百分含量的原料组分:磷酸盐溶液55%~60%;树脂溶液20%~25%;二乙二醇丁醚2%~4%;改性剂3%~5%;余量为水。由本发明所述无取向硅钢用涂层溶液形成的绝缘涂层厚度均匀,表面光滑,具有优良的绝缘性、耐腐蚀性、附着性,而且硅钢片的冲片性能好、叠片系数高。
50W600无取向硅钢钙处理的热力学分析及实验研究
通过热力学计算及实验室研究,对钙处理前后50W600无取向硅钢退火冷轧板中夹杂物的类型、数量及尺寸进行了系统分析。结果表明,50W600无取向硅钢经钙处理后(w(Ca)=0.002 6%),钙在1 600℃的钢液中主要以固态的CaO·2Al2O3、CaO·6Al2O3及溶解钙的形式存在。在钢液的凝固过程中,钢中的溶解钙和硫反应生成了CaS和CaS-MnS复合夹杂,有效抑制了MnS的弥散析出,减少了钢中微细夹杂物的数量。同时钙处理促进了钢中微细夹杂物的聚合长大,导致显微夹杂物的数量增加。 Based on thermodynamic calculation and laboratory experiment,the type,quantity and size of inclusions in annealed cold-rolled steel sheets of 50W600 non-oriented silicon steel before and after calcium treatment were systematically studied.Results showed that after calcium treatment(w(Ca) = 0.002 6%),calcium was mainly in the form of CaO·2Al2O3,CaO·6Al2O3 and dissolved calcium in steel at 1 600 ℃.Dissolved calcium could combine with sulfur to form CaS inclusions and compound CaS-MnS inclusions du...
高温硅钢加热炉双蓄热燃烧技术的探讨
介绍了双蓄热燃烧技术的特点和高温硅钢加热炉的特点,探讨了双蓄热燃烧技术在高温硅钢加热炉中使用的技术难点,分析了双蓄热燃烧技术在高温硅钢加热炉上使用的可能性。 Introduced characteristics of double regenerative combustion technology and high temperature silicon steel reheating furnace,discussed technical difficulties for using double regenerative combustion technology,analyzed the possibility of double regenerative combustion technology applied to high temperature silicon steel reheating furnace.
低铁损高磁通密度无取向硅钢的应用与生产技术进展
分析了高转矩和高转速条件下高效驱动马达铁芯材料对无取向硅钢磁性能要求,讨论了无取向硅钢的高磁通密度和低铁损对电机转矩和效率的影响,介绍了国内外高磁感无取向硅钢发展情况。在生产工艺上,提高钢质纯净度,弱化夹杂物和第二相粒子对畴壁移动和再结晶晶粒长大的钉扎作用,添加微量晶界和带钢表面的偏析元素促使有利织构发展等技术可提高无取向硅钢的磁通密度。 The requirements of high efficient drive motor core materials under the conditions of high torque and high speed were analyzed.The effects of high magnetic flux density of non-oriented silicon steel on the torque and efficiency of the motor were discussed.The development of non-oriented silicon steel with high magnetic was introduced.The magnetic flux density of non-oriented silicon steel sheet can be obviously improved by some production technologies,such as purification steel,weakening the pin...
CN202123048227.8一种硅钢前处理铁泥泵反冲洗装置
本实用新型公开了一种硅钢前处理铁泥泵反冲洗装置,包括污泥处理组件,所述污泥处理组件包括置放于污泥池的泵体、与泵体相连的传动轴管、设于传动轴管远离泵体一端的驱动电机以及与泵体相连的污泥管道,所述污泥管道的另一端穿过污泥池与排污管路连通;反冲洗组件,所述反冲洗组件包括与污泥管道相连的冲洗管道以及与冲洗管道相连的冲洗水泵,所述冲洗水泵的另一端与自来水供水管路相连;开关组件,所述开关组件包括设于污泥管道与排污管路连接处的第一阀门以及设于冲洗管道与冲洗水泵连接处的第二阀门。本实用新型减少了因铁泥堵死管道,所造成的电机过载烧坏,提高了生产效率,降低了维修维护成本。
CN202122238301.6一种硅钢片用叠压装置
本实用新型公开了一种硅钢片用叠压装置,包括机架,机架上设有工作平台,工作平台的顶面上沿轴向并排设有定位块和可远离或者靠近定位块的抵紧块,定位块的水平截面呈L状,且其与定位块之间形成叠压区,叠压区的上方水平设有可竖直移动的传动板,传动板上竖向滑动穿设有若干均匀分布的导杆,导杆的两端均伸出传动板,且顶端设有限位块,底端共同安装有水平设置的压板,导杆上套设有位于压板和传动板之间的弹簧,机架上还设有与传动板和抵紧块均相连的可编程控制器。本实用新型解决了如何能高效且保质地对硅钢片进行叠压的技术问题,具有工人劳动强度低、叠压效率高且叠压质量好等优点。
EBSD技术在硅钢织构研究中的应用
运用电子背散射衍射(EBSD)和X射线衍射(XRD)技术对硅钢热轧板的织构在板厚方向的分布进行了研究,并分析了两种织构测量方法的特点。EBSD技术能直观给出板厚方向的微观织构,XRD能得到钢板的宏观统计织构信息,结合两种技术的分析,能更直观更精确的研究不同织构在板厚方向的分布。 The texture distribution along the thickness of the silicon steel has been investigated by electron backscatter diffraction(EBSD) and X-ray diffraction(XRD) technique.The characteristics of two technique of texture analysis have been investigated.Combined the two techniques,the texture distribution along the thickness of the silicon steel could be realized distinctly and accurately.