本实用新型涉及硅钢片铁芯性能测试技术领域,公开了CD型硅钢片铁芯性能测试工装,包括:机台,上部后侧固定有竖直向上的后侧板;托板,水平设置在所述机台上方;夹持机构,设置在所述机台上,所述夹持机构包括:第二气缸,其驱动杆端部固定套接有夹持块,夹持块外端部固定有橡胶缓冲块;橡胶垫,固定在所述托板右侧上部。本实用新型通过设置第一气缸驱动连接于托板,可以先根据硅钢片的厚度,通过操作气缸控制器控制第一气缸工作带动托板在机台上进行升降高度,从而调整托板与夹持块的高度差,提高装置的实用性和广泛性,较为实用,适合广泛推广和使用。
2021-05-14 148 6.8

双辊连铸技术是冶金及材料领域内的一项前沿技术,对于生产高品质硅钢具有独特优势.本实验研究了一种双辊铸轧w[Si]=4.5%的无取向硅钢,考察其铸态和常化处理后样品的组织、织构及析出相尺寸特征.结果表明:铸带组织以与铸带法向成5~20(°)倾角的柱状晶为主,晶内存在少量0.3~0.4μm的AlN析出相,铸带织构以λ(<001>//ND)织构为主,表层织构漫散.950℃/10 min常化处理后,析出相尺寸增大,表层λ织构增强. As an advanced technique of metallurgy and material science,twin- roll strip casting has unique advantages for producing high quality silicon steel. The present study was aimed at a 4. 5% Si non- oriented electrical steel for analyzing the structure,texture and the size of precipitates at the initial and normalized state. The results revealed that the initial structure mainly consisted of columnar grains with 5 ~ 20( °) angle to the normal of cast strip,and some AlN precipitates of 0. 3 ~ 0. 4 μ... 
2014-03-28 165 5.8

对碳-锰-硅钢进行不同配分温度的Q&P(Quenching and Partitioning)处理,测试了热处理后不同钢的力学性能和残余奥氏体含量,并用扫描电子显微镜和透射电镜观察其显微组织,分析了配分温度对显微组织和力学性能的影响。结果表明:试验钢显微组织基本由低碳板条状马氏体、块状铁素体和条状残余奥氏体组成;随配分温度的升高,试验钢的抗拉强度呈下降趋势,伸长率与奥氏体含量的变化趋势相同,但变化规律不确定;提高锰含量能稳定残余奥氏体,从而提高试验钢的伸长率,并使伸长率对配分温度不敏感。 The C-Mn-Si steel was quenched and partitioned at different partitioning temperatures,the mechanical properties and residual austenite contents were investigated,the microstructure was observed by SEM and TEM,and the effect of partitioning temperature on microstructure and mechanical properties was analyzed.The results show that the microstructure of the tested steel consisted of lath martensite with low carbon,nubby ferrite and banded residual austenite.The tensile strength of the tested steel ... 
2011-09-28 159 5.8

在50Kg氧化镁坩埚真空感应炉上进行高硅电工钢的脱氧试验。结果表明,通过控制原料的成分、高真空下的碳氧反应和炉衬分解向钢液中的供氧,可使钢液的总氧含量≤15×10-6;在维持高温高真空条件下,当钢液中的反应达到一定程度后,延长精炼时间并不能降低钢液的总氧含量;完成精炼后加入硅钙合金沉淀脱氧可进一步降低钢液的总含氧量,但脱氧效果有限。 The test of high-silicon electric steel deoxidation has been carried out in 50Kg vacuum induction furnace with magnesium oxide crucible.Results show that the total oxygen could be ≤15×10-6in molten steel by controlling material components,carbon-oxygen reaction in high vacuum and oxygen contamination from crucible materials on molten steel;And when the reaction was carried through to a certain extent,total oxygen in molten steel could not be reduced by the extension of refining period in high va... 
2011-02-28 187 5.8

结合冶炼无取向硅钢的生产实际,对钢中硫的来源,以及炉渣性质、钢水温度、底吹强度对脱硫的影响进行了分析。研究表明,转炉钢中硫的主要来源为铁水、废钢、铁水渣及石灰带入;冶炼硅钢时,终渣碱度为3.0~3.5,w((FeO))≤20%,终点钢水温度大于等于1 680℃,加大底吹搅拌强度能提高转炉脱硫效果。硅钢平均出钢硫的质量分数为0.004 8%,能满足无取向硅钢对硫含量的要求。 With the actual production of non-oriented silicon steel,the source of sulphur and the effect of metallugic parameters like slag properties,temperature of molten steel and bottom stirring on desulphurizing ability were investigated.The results show that the main source of sulphur is molten metal,scrap,the remaining slag volume in hot metal and lime.The degree of desulphurization for smelting silicon steel can be increased through adopting the following measures,such as the basicity of finishing ... 
2011-02-28 182 5.8

分析了冲裁硅钢芯片时出现的质量问题,针对影响硅钢芯片冲裁质量的4大因素——人、原材料状态、工艺和工装进行了工艺试验和分析,根据原材料状态的差异,采用不同工艺方案,特别是如何合理选择冲裁模具间隙,解决了硅钢芯片冲裁时产生的主要质量问题,使冲裁的硅钢芯片达到最佳质量状态,并满足硅钢芯片的使用性能。 The problems occurred during silicon steel chip punching and the factors that affect the quality of silicon steel chip punching were analyzed,the factors include 4aspects,that is,people,raw material status,process and frock,at the same time,process tests and analysis aimed at the factors that affect punching quality were did,according to the difference of raw material status,corresponding process schedules wee taken,especially in how to reasonably select punching dies clearance,which solved the ... 
2013-10-28 118 5.8

无取向硅钢的磁性能主要取决于铁素体的晶粒尺寸、晶体织构和钢中的夹杂物。通过合适的化学成分设计以及采用适宜的夹杂物控制技术,可以获得最佳的夹杂物控制效果,使其纯净度大幅度提高或者无害,最终获得磁性能优良的高级别无取向硅钢。同时,为满足节能、环保、高效需求,无取向硅钢正朝着节能降耗、环境友好以及多功能、高效率、易加工等方向发展。 The magnetic properties of non-oriented silicon steel mainly depend on the grain size of ferrite,the crystallographic texture,and the inclusions in the steel.The optimum inclusion control effects can be obtained through a suitable chemical composition design and an appropriate inclusion control technique,and then the liquid steel will get be clean or the inclusion will get be harmless,finally the excellent magnetic property of the non-oriented silicon steel can be obtained.Meanwhile,in order to ... 
2013-03-28 181 5.8

通过Axio Imager金相显微镜考察4.5%~7.0%硅(质量分数)对高硅钢材料组织形貌的影响,并利用Fe-6.5%Si高硅钢薄板制备方法对其进行轧制,通过DDL50电子万能试验机对阶段产品进行力学性能测试。结果证明,硅含量为5.58%的高硅钢在实验硅含量区间内存在最大延伸率及最小铸态组织晶粒尺寸。 An investigation about the influence of 4.5%-7.0% Si on microstructure and mechanical properties of high-silicon steel was presented.SEM was adopted to take an observation towards microstructure during fabrication,and DDL50electronic universal testing machine was applied into the detection of tensile curves.The results show that silicon steel with 5.58% Si provides the maximum elongation and minimum grain size as cast. 
2023-05-09 209 5.8

本实用新型公开了一种高精度硅钢片加工用多向定位组件,包括底板、安装板、橡胶轮组一和橡胶轮组二,所述底板上端两侧对称设置有U型的所述安装板,所述安装板内底端中部安装有安装架二,所述安装架二上安装有所述橡胶轮组二。有益效果在于:本实用新型通过螺杆、调节套、安装架一、安装架二、橡胶轮组一、橡胶轮组二、弹簧以及连接柱的设计,能够实现高精度硅钢片在加工时的有效夹紧定位,避免了高精度硅钢片在加工时的晃动滑移,提高了高精度硅钢片的加工质量,通过电推杆、滑块以及滑槽的设计,能够根据高精度硅钢片的尺寸来调节安装板之间的间距,以满足也不同尺寸高精度硅钢片的加工需求,提高了定位组件使用的灵活性。
2021-07-02 224 6.8

介绍了电工钢生产线连退机组的表面处理工艺,特别是电解清洗系统的工作机理、设备构造、生产工艺及各种影响因素。 This paper introduces the technology of surface treatment of continuous annealing unit in electrical steel production line,in particular the working mechanism,structure of equipment,production techniques and various influence factors of the electrolytic cleaning system. 
2023-05-11 1.37k 5.8

本实用新型涉及电机技术领域,具体涉及一种具有低应力隔磁桥的硅钢片和电机转子。包括硅钢片、开设在硅钢片上的若干个磁钢槽组和永磁体,若干个磁钢槽组沿所述硅钢片周向分布,每个磁钢槽组均至少包括一对沿径向对称分布的磁钢槽,永磁体嵌设于磁钢槽内,磁钢槽朝向硅钢片内侧的一端设有空腔,一对磁钢槽的空腔之间通过隔磁桥隔离,隔磁桥的空腔上壁面与空腔侧壁面之间通过第一椭圆弧过渡连接,隔磁桥的空腔下壁面与空腔侧壁面之间通过第二椭圆弧过渡连接。有效降低该处隔磁桥在拐角处所受应力,进而提高该隔磁桥的强度,避免磁钢和铁芯产生形变而断裂。
2021-04-15 179 6.8

研究了CSP工艺生产≤0.005%C-1.1%Si的2.2mm无取向电工钢热轧板在800~1000℃常化对0.5mm冷轧板840℃退火后组织和磁性能的影响。结果表明,热轧板常化温度升高,冷轧板退火后的再结晶晶粒增大,铁损降低,磁感增加;热轧板常化温度超过900℃,因第二相固溶而后弥散析出,退火后冷轧晶粒细化,铁损增加,因此该无取向电工钢热轧板最佳常化温度为900℃。 The effect of normalizing at 800-1000℃ of CSP produced plate(≤0.005%C-1.1%Si) on the microstructure and magnetic properties of downstream cold-rolled non-oriented electrical steel annealed at 840℃ was studied.Results show that with increasing normalizing temperature of hot-rolled material the recrystallized grain size of annealed sheet increases,iron loss reduced and magnetic induction increases.As normalizing temperature excesses 900℃,grain is refined and iron loss increases after annealing due... 