本实用新型涉及一种硅钢片自动分拨装置,包括U型座,U型座内倒扣有同为U型结构的盖磁板,U型座和盖磁板之间构成封闭的容纳空间,容纳空间内放置有磁铁,紧贴着盖磁板外顶面安装有压板;U型座开口处的两臂之间安装有手杆,U型座外底面间隔平行设置有外凸的肋筋;将分拨装置设置有肋筋的底面靠近堆叠的硅钢片端面,容纳空间中的磁铁将硅钢片磁化,磁化后的硅钢片由于同性相斥的原理,堆叠上部的相邻硅钢片之间自动分拨开,从而便于工人的手工作业,降低了作业难度,极大地减轻了人员工作负担,提高了叠装效率,并且体积小巧携带方便,安全性能好。
2021-01-27 122 6.8

介绍了CSP工艺生产无取向电工钢各工序的设备特点、采用的工艺控制手段和电工钢产品质量情况,结合生产实践证明了马钢CSP工艺开发的无取向电工钢产品丰富了薄板坯连铸连轧的品种结构,发挥了薄板坯连铸连轧生产无取向电工钢性能均一、稳定的特点。 The equipment characteristic,the process control method and the quality of non-orientated silicon steel by CSP process were introduced.Combined with the production situation,it is proved that production of non-orientated silicon steel developed on Masteel CSP line would enrich product structure of thin slab continuous casting and rolling,and it exerts stable performance of non-orientated silicon steel. 
2013-06-28 165 5.8

本发明涉及一种取向硅钢热轧钢带的板形控制方法,所述取向硅钢热轧钢带的工艺流程包括铸坯加热过程、轧制过程及层流冷却过程;其中轧制过程中采取取向硅钢与普钢交叉轧制的方式;粗轧过程采取R1轧制1道次、R2轧制5道次的1+5轧制工艺,并控制轧制工艺参数;精轧过程中控制F1~F7轧制工艺参数。本发明通过设定合理的交叉轧制工艺及取向硅钢热轧工艺,使取向硅钢的轧制稳定性大幅提高,取向硅钢带形控制良好,凸度控制在30~50μm之内,楔形控制在30μm之内,板形平坦度控制在25iu之内;从而为冷轧工序提供了优质原料。
2021-03-18 140 6.8

本发明提出了一种控制磁畴结构来降低铁损的取向性电磁钢板的制造方法中,即使在实施了去应力退火的情况下,也能够保持铁损降低效果,并且在磁畴控制处理后磁通密度不会降低的方法。本发明的制造方法中,在取向性电磁钢板的表面,沿与钢板的轧制方向交叉的方向线状地照射周边比中心低的环状的强度分布的激光。
2021-08-26 172 6.8

本实用新型公开了一种取向硅钢绝缘涂层液生产用分散机,包括固定底座,固定底座顶端的一侧固定安装有套筒,套筒的内部滑动设有活塞杆,套筒的内部设有电动液压升降柱,电动液压升降柱的底端固定安装在固定底座顶端的中部,电动液压升降柱的顶端与活塞杆的底端固定连接,活塞杆的顶端固定连接有箱体,箱体底端的一侧固定安装有伺服电机,本实用新型的有益效果是:通过滑块、橡胶块、空心转轴和伺服电机的配合使涂层液搅拌分散的更加均匀,通过固定装置可以将盛有涂层液的桶固定住,防止涂层液桶转动,这样可以使涂层液进行充分搅拌,不需要时刻对其调整固定,这样也可以提升工作效率,提高生产速率,而且操作方便。
2020-12-26 143 6.8

本实用新型公开了一种风电机组取向电工钢用罩式炉的砂封振动装置,包括:基座,设置有行走机构,行走机构带动基座沿环形砂封槽槽壁行走;振动齿座,与基座连接,定位座和基座之间夹设有弹性缓振件;振动件,与定位座固定连接;振动齿,与振动齿座固定连接,设置于基座的行走轨迹内侧。该风电机组取向电工钢用罩式炉的砂封振动装置利用砂封槽的槽壁作为行走机构的轨道,振动齿不仅可以平整砂封槽中的密封砂,振动状态下还能使密封砂填充得更趋密实,避免局部密封不良的问题,优化密封效果。
2021-08-28 152 6.8

本发明涉及无取向硅钢技术领域,尤其涉及一种改善高牌号无取向硅钢冷轧断带的控制方法。按重量百分比计:[Si+Al]≥4.0%;Mn、S含量满足:S≤0.0015,[Mn]/[S]:200~400;1)热轧过程中使用保温罩,热轧轧制时投入边部加热,头尾100米内卷曲温度提高15~30℃;2)常化机组圆盘剪进行边部剪边前增加加热装置,剪切后增加毛刺打磨装置,采用煤气明火加热,保证钢板温度在韧脆转变温度以上;3)圆盘剪间隙满足关系式:ds=(0.15~0.45)d0ds:圆盘剪间隙,μm;d0:常化板板厚,mm;4)常化采用快速加热,控制钢带的预热段升温速度320~380℃/min,机组速度20~30m/min;5)常化工艺后,控制边部小于20μm的晶粒占比在5%以内。有效的减少了冷轧断带的发生,提高成材率1.30%以上,降低了生产成本。
2021-09-13 147 6.8

对两种硅钢水溶性极厚绝缘涂层进行了不同温度的热老化实验。通过TG-DTA,GDS,FT-IR,SEM和光泽度仪等测试方法对老化的涂层进行分析表征,提出了评估硅钢水溶性极厚绝缘涂层热老化性能的合理温度区间,探讨了涂层热老化行为,并分析了两种涂层热老化性能的差异。结果表明,涂层附着性随着老化时间的延长逐渐下降。FT-IR表征结果显示,热老化过程中,涂料交联形成的化学键未发生断裂,交联剂氨基树脂的三嗪环被破坏是聚合物三维网络结构坍塌的主要原因。 Thermal aging expriments at different temperature were carried out on two types of water-soluble and extra-thick insulation coatings for non-oriented silicon steel,and a series of test methods such as glossmeters,TG-DTA,FT-IR,GDS,SEM were applied in analysis.For evaluating the thermal aging effect of this kind of insulation coating,the proper temperature range was proposed.The difference of aging performance between two coatings was been investigated and the related behaviors were been discussed... 
2011-04-28 143 5.8

阐述了国内外高磁感取向硅钢的生产研究水平与发展趋势,包括通过提高高斯晶粒取向度、细化磁畴、涂覆张力涂层、减薄钢片厚度进一步降低铁损以及低温加热技术和短流程技术新工艺。分析高磁感取向硅钢在我国大型电力变压器上的应用情况,结果表明,发展更薄规格高磁感、低铁损、低磁致伸缩取向硅钢可为大型变压器的安全性、节能性及环保性提供有效保障。 The research progress and development trend of high magnetic induction grain-oriented silicon steel at home and abroad are summarized,including the technology of improving the Goss alignment,refining domain wall,adding stress coating,decreasing thickness of sheet,and the new technique of reducing heating temperature of casting slab and shortening operational.Moreover,the application of high magnetic induction grain-oriented silicon in power transformer is presented.Developing grain-oriented sili... 
2014-11-28 173 5.8

目前高磁感冷轧硅钢生产过程中,采用经验方法确定的乳化液流量设定值往往会造成硅钢产品的磁感性能达不到预期目标,针对此情况,基于轧机轧制机理研究了的乳化液流量数学模型,确定了乳化液流量设定值。实践表明,使用该数学模型输出的乳化液流量设定值,可提高轧制过程中乳化液流量控制精度,从而提高高磁感冷轧硅钢的轧制性能。 In view of the current production process of high magnetically inductive cold-rolled silicon steel, the mathematical model of emulsified fluid flow based on mill rolling mechanism is studied in view of the situation in which the magnetic sensing performance of silicon steel products is often not up to the expected target by using empirical method to determine the emulsified liquid flow setting. Practice shows that the emulsified fluid flow setting value output from this mathematical model improv... 
2022-01-28 154 5.8

本发明公开了一种用于测量电工钢片的二维磁性能的系统及方法,所述系统通过将承载待测样品的托盘与旋转机构连接,在测量各个角度的二维磁性能时只需控制旋转机构驱动待测样品转动,旋转机构的负载很小,旋转机构的制作较为简单。而且,励磁测量线圈是绕制在托盘的外围,而不是在磁轭上,这样使得待测样品相当于处于一个均匀的螺线管中,磁场更加均匀,保证了磁场测量的准确性,并且励磁源不需要像RSST一样要保证两路励磁机构的相位差的准确度,从而使得励磁源的制作更加简单,降低了制作的成本和门槛。同时,不需要对待测样品打孔来绕制线圈,待测样品无破坏,可以保证待测样品的完整性以及数据的重复性和可对比性,测量结果更可靠。