所有分类
  • 所有分类
  • 未分类

利用光学显微镜、TEM和EBSD研究了退火温度对双辊连铸无取向硅钢再结晶组织的影响。结果表明,900℃退火后组织分布不均匀,有大量带状组织,平均晶粒尺寸29.5μm。提高退火温度,晶粒尺寸增大,组织均匀化程度增加,1050℃退火时,带状组织基本消失,平均晶粒尺寸42.2μm。 Effect of annealing temperature on recrystallization microstructure of non-oriented electrical steel produced by twin-roll casting process was investigated using OM,TEM and EBSD.The results show that the recrystallization microstructure is uneven because of many banded grains existing,average grain size is 29.5 μm.With annealing temperature increasing,the recrystallization grain size increases,microstructure becomes more homogeneous.When 1050 ℃ annealing,the banded structure almost disappear and... 
2013-03-28 225 5.8

本发明提供了一种无取向硅钢RH顶枪喷粉脱硫工艺,RH脱碳结束测温定氧,立即加入铝粒脱氧合金化、之后立即依次连续加入合金进行成分调整,合金加完后立即开始顶枪喷粉;加入铝粒的量=铝粒理论加入量+0.2‑0.4kg/t钢;喷粉时,控制喷粉速度与钢液循环流量相匹配;本发明从真空条件下脱硫热力学和动力学角度出发对具有顶枪喷粉功能的RH脱硫工艺进行改进,提高脱硫率。
2021-11-30 213 6.8

本文介绍了无取向硅钢C6涂液的性能,研究了配水量、固化程度和涂层厚度等因素对无取向硅钢C6涂层性能的影响。结果表明,随着配水量的增加,完全固化所需的时间增加,涂液固体含量降低,涂层厚度减小;随着固化程度的提高,涂层硬度先增大然后趋于恒定,而柔韧性逐渐变差,在过固化后急剧恶化;涂层厚度对涂层的表面外观、附着性和绝缘层间电阻均有显著影响。 Based on the introduction about the performance of C6 varnish for non-oriented silicon steel sheets,effects of water amount,curing degree and coating thickness are discussed. Results show that with the increase of water amount,the time required to cure completely extends,and both the solid content of C6 varnish and the coating thickness decrease. As the curing degree increases,the hardness of the coating increases first and then tends to be constant,however the flexibility degenerates,especially... 
2014-02-28 362 5.8

采用X-射线衍射分析技术测定了取向硅钢热轧板在不同压下率下不同厚度处的织构。结果表明,在压下率低于80%的情况下,几乎所有试样的不同厚度处的织构均为旋转立方织构类型{100}<011>,但不同压下率、不同厚度处的织构强度存在很大差异;在压下率大于80%的情况下,不同试样的不同厚度处的织构类型发生了变化,其织构类型为旋转立方织构或高斯织构{011}<100>,且当织构类型为旋转立方织构时,织构强度存在很大差异,而当织构类型为高斯织构时,织构强度差异相对较小。 The texture of the grain oriented silicon steel hot rolled plate at different compressibility has been measured.The experimental results have shown that the texture of all samples at different thickness is {100}<011> when the compressibility is below 80%,and its intensity at different compressibility and thickness is difference.The texture of all samples at different thickness is variable when the compressibility is above 80%,it is {100}<011> or {011}<100>,and the intensity of ... 
2011-04-28 393 5.8

一种高硅钢材料的制备方法,步骤包括靶材、金属基材表面清理;排除密闭容器内空气、通保护气;双辉光等离子预轰击靶材和基材,净化表面;等离子溅射、加热、保温;缓慢冷却取出。预轰击靶材、基材,去除表面吸附层、活化基材,交替升高基材电压、靶材电压,使靶材中的合金元素被离子轰击而溅射出来、扩散进入基材内部形成表面高硅钢层。“双辉光等离子表面冶金技术”制备高硅钢的工艺简单易行、可控性高、成本低、无污染且基体和表面的结合力高,适合大规模产业化生产;更重要的是该方法采用交替离子轰击、扩渗速度快,结合强度高,得到硅含量均匀分布或呈梯度分布的高硅钢材料,为制备更高品质的无噪音、低铁损的高硅钢产业化奠定基础。
2021-12-30 339 6.8

阐述了电工钢在\"双碳\"中的作用,强调了电工钢的生产工艺技术及在减少碳排放、降低能耗中的作用,对下游能效升级带来明显的节能及降碳成果。同时,分析了2021年电工钢的生产运行情况,介绍了电工钢的未来发展,并针对如何减少碳排放以及生产更多的更低铁损、更高磁感的电工钢谈了几点启示。 The effects of electrical steels on carbon peak and carbon neutralization were expounded,especially on the achievements of obvious energy saving and carbon reduction to the downstream energy efficiency upgrading bringing from the production technology of electrical steels and their effects to reducing carbon emission and energy consumption.Meanwhile the production situation of electrical steels in 2021 was analyzed,and the future development of electrical steels was introduced,and some advices w... 
2022-01-28 241 5.8

一种硅钢生产线上的牵引装置,包含有底座(1)、支架(2)、平移机构(3)、上压板(4)、下托板(5)、气缸(6)、转向辊(7)和对中摄像头(8);所述的平移机构(3)包含有长条齿轮(14)、齿轮(15)、电机(16)和滚轮轴承(17);其特征在于:所述的齿轮(15)固定在电机(16)的输出轴上,并且与长条齿轮(14)啮合;使得平移机构(3)可以由电机(16)驱动在导轨(10)上左右滑动。本实用新型通过气缸(6)驱动上压板(4)和下托板(5)夹紧钢带(9),由平移机构(3)带动钢带(9)进行左右平移,避免了原先夹送辊刮伤钢带(9)表面涂层,减少了带头的浪费。
2021-12-01 400 6.8

本实用新型涉及一种改进的点火器线圈硅钢片结构,包括E型件和I型件,所述E型件和I型件组合成日字形,它们可相互转动;所述E型件包括竖边和设置在竖边三个横边,三个横边分别为上横边,中横边和下横边,它们分别与竖边垂直连接;其中所述竖边的转角位置圆角处理,竖边外侧为弧形边;所述上横边的端面设置插缝;所述中横边的端头设置凹部;所述下横边的端头设置凸部;所述I型件上端两侧对称设置凹台;所述凹台具有弧形凹边;所述I型件通过凹台设置在插缝可以旋转。本实用新型设计新颖,改进巧妙,由于E型件具有弧形边可以有利于拾取,方便工作操作,E型件和I型件采用插合的方式,整体结构稳定,便于安装,增加了组合体的稳定性。
2021-08-20 450 6.8

本发明提供了一种高硅钢及其制备方法,所述高硅钢由如下质量分数的化学成分组成:Si:5.0‑7.0%,Ni:0.001‑0.05%,Ce:0.0001‑0.0002%,其余为Fe和不可避免的杂质。本发明提供的高硅钢的延伸率为15‑22%,抗拉强度为739‑824MPa,磁感应强度B8为1.26‑1.29T,铁损P2/10k=68‑80W/kg,矫顽力为10.6‑13.4/m,最大磁导率为19000‑25000,具有良好的磁性能和延伸性能,易加工且可大规模生产应用。
2021-01-22 339 6.8

采用铸坯低倍组织检验和化学分析的方法,研究板坯连铸机二冷区电磁搅拌器电流和频率参数对无取向电工钢XG800WR板坯中心偏析和等轴晶率的影响,结果表明:铸坯等轴晶率随着搅拌器电流强度和电流频率的增大而增加。采用二冷区电磁搅拌可减小中心易偏析元素S的偏析,试验得出:减小铸坯S偏析效果最好的电磁搅拌参数为电流380~400A,频率6Hz。 The effect of electromagnetic stirring current and frequency parameter at secondary cooling area on the central segregation and equiaxed crystal ratio of XG800WR non - oriented electrical steels slab was investigated through the methods of chemical and macrostructure analysis.The results shows that the rate of equiaxed crystal zone is going up with increasing of current intensity and current frequency.Electromagnetic stirring in the secondary cooling area can be easily reduced segregation caused... 
2011-01-28 227 5.8

本实用新型公开了一种用于硅钢板带的表面清理装置,包括机体,所述机体的内部设置有转动机构,所述转动机构的内部安装有固定机构,所述机体的外表面一侧固定连接有驱动电机,所述驱动电机的输出端固定连接有螺杆,所述螺杆的外部设置有螺纹套,且螺纹套在螺杆上螺纹转动连接,所述螺纹套的底部固定连接有电动推杆,所述电动推杆的输出端固定连接有连接板。本实用新型,利用转动机构可很好的进行翻转,便于对两面进行清理,从而提高了一定的工作效率,相比人工翻转清理时效果更好,具有一定的实用性,利用固定机构可很好对于成硅钢板带进行固定,可方便进行清理,提高清理时的工作效率,实用性较强。
2021-08-25 185 6.8

本实用新型公开了一种无取向硅钢喷涂用即时干燥装置,包括干燥箱,所述干燥箱内滑动连接有加热台,所述干燥箱顶部设置有加热箱,所述加热箱左右两侧分别设置有进风管和出风管,所述进风管和出风管均与干燥箱连通,所述加热箱内部从左到有依次固定连接有风机和加热网,所述干燥箱内设有带式传送机,通过带式传送机使喷涂过后的硅钢在干燥箱中移动,首先经过加热台加热,使涂层表面干燥硬化,不会变形,然后再经过加热箱吹出的风对硅钢表面的涂层进行进一步的烘干,从而保证干燥过程中涂层不会起褶皱。
2021-12-02 253 6.8

站点公告

网站试运行,请大家关注本站公众号,多提宝贵意见!

显示验证码
没有账号?注册  忘记密码?