钢厂
含核壳异质结构6.5% Si高硅钢铁芯的制备与磁性能
以构建高磁感、低铁损、免轧制高硅电工钢铁芯为出发点,提出采用单辊甩带制备非晶铁硅合金薄带、微氧化法在铁硅合金粉末表面包覆高电阻率铁硅氧化物薄膜制备核壳异质结构高硅电工钢纳米粉末、放电等离子烧结快速成形制备颗粒间绝缘的高硅电工钢铁芯。研究了不同氧化包覆时间对SPS烧结试样密度、物相组成、微观结构和静磁性能的影响。研究表明,在氧化包覆5h烧结温度800℃工艺条件下,制备的6.5%Si高硅电工钢铁芯的静磁性能最佳,饱和磁化强度为128.84A.m2/kg、矫顽力为2.25kA/m、剩磁为3.47A.m2/kg。其饱和磁化强度与粉末压延法制备的高硅钢相当,但矫顽力降低了1/3。 The paper takes preparation 6.5%Si steel with high induction,low core loss and removing rolling as the starting point,amorphous Fe-Si ribbons was synthesized by melt spinning method,6.5%Si steel nanopowders with high resietivity core shell structure was prepared by the slight oxidation process and 6.5% Si steel iron core with evaluating internal was sintered by spark plasma sintering process(SPS).The essay focuses studies the effects of different oxidation cladding time on sample density,phase c...
锡或锑在无取向电工钢中的研究进展
近年来,在节能减排背景之下,国内外众多研究者对无取向电工钢磁性能的提升做了大量研究。为了探索无取向电工钢磁性能提升的方法,对锡或锑对无取向电工钢磁性能的作用机制(晶粒尺寸和晶体织构的控制)进行分析。基于该作用机制,介绍锡或锑的添加对无取向电工钢磁性能的影响。经研究发现,适量的锡或锑在晶界偏聚,不会阻碍晶界的移动并且致使晶粒尺寸降低;与此同时,锡或锑在晶界偏聚不仅抑制{111}织构在原始晶界处形核及生长,还降低(100)晶粒表面能,促进(100)晶粒生长。因此,适量添加锡或锑,可使无取向电工钢铁损下降、磁感提升。最后结合生产工艺,建议无取向电工钢的研究方向应为稀土含量对高牌号无取向硅钢夹杂物尺寸和数量分布的影响,锡或锑的添加量和常化工艺参数(常化时间、常化温度)对常化晶粒尺寸的影响。 In recent years, due to the background of energy saving and emission reduction, numerous researchers all around the world have done a lot of investigations on the improvement of magnetic properties for non-oriented electrical steel. In order to explore the method of improving the magnetic properties of non-oriented electrical steel, the mechanism of tin or antimony on the magnetic properties(the control of grain size and crystallographic texture) of non-oriented electrical steel is illuminated. ...
CN202122455295.X一种硅钢炉底辊套管生产用高效粉磨机
本实用新型公开了一种硅钢炉底辊套管生产用高效粉磨机,包括机壳,所述机壳顶部中央安装有第一轴承,且第一轴承内安装有驱动转轴,所述驱动转轴顶端连接驱动电机输出端,所述驱动转轴底端连接安装有第一粉磨辊,所述驱动转轴位于机壳内腔部分安装有安装架,且安装架上均匀安装有四组辊轮架,并且辊轮架上安装有第二粉磨辊。有益效果:本实用新型设置的第一粉磨辊和第二粉磨辊可对物料进行二次粉磨,粉磨效果更好,大大提高一种硅钢炉底辊套管生产用高效粉磨机的工作效率,且无需增设额外的驱动电机,而设置的顶针则极大的方便了工人对堵塞的下料孔进行疏通,保障了一种硅钢炉底辊套管生产用高效粉磨机的下料工作效率。
国产化高牌号无取向硅钢退火、涂层炉新技术
从影响高牌号无取向硅钢退火工艺的主要参数入手,介绍高牌号无取向硅钢退火炉在加热、气氛控制、冷却、涂层烘烤方面的新技术,并展望无取向硅钢退火炉的发展方向。 Based on the technology parameters of high-grade non-oriented silicon steel annealing,the new technology of the annealing line,which includes heating,atmosphere control,cooling,coating baking,is introduced,and the development direction of non-oriented silicon steel annealing furnace is pointed out.
夹杂物尺寸及数量对无取向硅钢磁性能影响的主成分回归分析
采用扫描电镜、场发射扫描电镜、能谱仪等对50SW1300冷轧无取向硅钢中的夹杂物分不同尺寸区间进行数量统计,利用主成分回归分析法,即数据的标准化处理—主成分分析—回归分析—标准化的变量还原成原始变量—确定显著影响因素,综合分析夹杂物总量及各尺寸区间的夹杂物数量对无取向硅钢磁性能的影响。结果表明:主成分回归分析能够从夹杂物尺寸区间及数量的多个影响因素中提取主要的因素,定量研究其对磁性能的影响。分析表明,显著影响无取向硅钢铁损的夹杂物为100~500nm的AlN、AlN+MnS、MnS、Al2O3、AlN+Al2O3,而劣化磁感最明显的夹杂物尺寸区间为100~200nm。 Different size intervals of inclusions in cold rolled non-oriented silicon steel 50SW1300 were counted by scanning electron microscope(SEM),field emission scanning electron microscope(FESEM)and energy disperse spectroscopy(EDS).With principal component regression method:standardization for experimental data,principal component analysis,regression analysis,transform standardized variables into original variables,determination of significant factor,effects of the total number of inclusions and the...
CN202111200887.5一种改善表面麻点缺陷的薄规格中低牌号无取向硅钢及其生产方法
本发明提供一种改善表面麻点缺陷的薄规格中低牌号无取向硅钢及其生产方法,成分C≤0.0025%,1.2≤Si≤1.65%,0.25%≤Mn≤0.35%,0.06%≤P≤0.11%,0.1%≤Als≤0.2%,S≤0.0025%、N≤0.0025%,Ti≤0.0025%,其余为Fe及不可避免的杂质。与现有技术相比,本发明采用较低氢气浓度,防止炉内氧化铁皮还原,减轻碳套辊的腐蚀程度,减少碳套辊结瘤率,改善带钢表面质量;采用合理合金成分设计,提高带钢的力学强度,降低碳套辊结瘤对带钢表面的影响程度,改善带钢表面质量。产品厚度为0.35mm,板面麻点发生率降低,无手感,且辊身周长周期范围内麻点个数≤5个。
CN202023204913.5硅钢片冲压模具
本实用新型公开了一种硅钢片冲压模具,包括上模和下模,上模和下模之间通过导向杆连接,下模上设有出料槽,出料槽的底部设有一磨盘,磨盘通过齿轮连接电机。本实用新型结构设计合理巧妙,当硅钢片冲压下落时,磨盘通过电机带动转动,对硅钢片的周围进行打磨,使硅钢片边缘平整,叠铆时上下不易错位。
CN202121280824.0一种硅钢片叠装上料用转运装置
本实用新型涉及一种硅钢片叠装上料用转运装置,包括一输送单元,输送单元包括输送支架、输送辊,在各个输送支架均配备有一用于接收裁切好的硅钢片并堆放形成硅钢片料堆的放置板;一供料单元,包括供料板、供料支架、供料辊、支撑组件;一转运单元,包括转运支架、转运底座、转运辊、推料板、推动机构、电磁铁、转运齿条、转运齿轮、转运导轨、转运导座、导向轮、行走滚轮。本实用新型的优点在于:通过输送单元、供料单元及转运单元之间的相互配合,从而能够将满料的放置板自动输送并呈日字形自动排布好,无需再由人工搬运放置,大大减少了人工劳动,降低了人工劳动强度。
高性能取向硅钢生产过程中的节能降耗
从取向硅钢生产路线的选择、工艺技术的改进和生产设备的改造三方面进行了生产取向硅钢的节能降耗技术改造.通过完善多元抑制剂配方生产低温取向硅钢,通过加抛丸的酸洗、带面超声波清洗、改进连续退火炉以及余热循环利用等技术改造,使2012年取向硅钢的产量与未进行技术改造前的2009年相比提高了2.5倍,产品磁性上升了一个半牌号,能耗下降了8.9%,成材率提高了6.4%,生产成本下降了22%,综合效益显著. Energy saving technological transformation was carried out in the production of grain oriented silicon steel from three aspects of the oriented silicon steel production process route selection,technology improvement and equipment renovation.Through the improvement of multiple inhibitor formulations for producing low-temperature grain-oriented silicon steel,and by adding the blasting pickling,the belt surface ultrasonic cleaning,improvement of continuous annealing furnace,waste heat recycling tec...
CN202023317762.4一种硅钢片加工装置
本实用新型公开了一种硅钢片加工装置,涉及到硅钢片加工装置技术领域,包括安装板,所述安装板的上表面两端均固定连接有固定板,所述安装板的上表面一侧固定连接有涂覆装置,所述安装板的上表面中部固定连接有压平装置,所述安装板的上表面另一侧固定连接有烘干装置,所述固定板的一侧底端通过轴承活动连接有传动辊。本实用新型通过在安装板的上表面一侧设置涂覆装置,涂覆装置对硅钢片的两面进行绝缘层涂覆,在安装板的上表面中部设置压平装置,压平装置包括两个压辊,压辊的一侧设置的限位块中部开设有螺纹孔,转动双向螺杆使得限位块运动,从而使得两个压辊之间的间距被调节,可以根据生产需求调节绝缘涂料的压平厚度。
CN202122506341.4一种用于取向硅钢激光刻痕设备的烟尘收集装置
本实用新型涉及烟气收集净化技术领域,尤其是一种用于取向硅钢激光刻痕设备的烟尘收集装置。其包括集尘罩,所述集尘罩左右两侧对称设置第一集尘仓和第二集尘仓,第一集尘仓和第二集尘仓沿着集尘罩长度方向分布设置;所述第一集尘仓内侧和集尘罩内腔连通,第一集尘仓外侧分别设置多个进气口,所述第二集尘仓内侧和集尘罩内腔连通,第二集尘仓外侧分别设置多个出气口;所述集尘罩左右两侧分别设置第一分流器和第二分流器,第一分流器一侧并排设置多个第一分流器出气口。本实用新型通过设置在第一分流器进风口的鼓风机主动送风,与吸风口吸尘设备配合,在密闭集尘罩内形成顺畅且稳定的、方向固定的风流,将烟尘带走。