钢厂
CN202123201562.7一种取向硅钢氧化镁涂层线用冷涂辊
本实用新型涉及一种取向硅钢氧化镁线涂层装置,尤其涉及一种取向硅钢氧化镁涂层线用冷涂辊,具有涂层辊本体及包覆在涂层辊本体外层的橡胶涂层;涂层辊本体内部为空腔结构,空腔结构内通有循环冷冻液。本实用新型涂层辊内部设计成空腔结构,并通过循环冷冻液对涂层辊进行冷却降温,既可以达到通过涂层辊对氧化镁进行降温的目的,从而满足工艺要求,防止质量缺陷的产生,还可延缓涂层辊因反复摩擦生热造成橡胶层老化,从而延缓涂层辊使用寿命。
CN202111200887.5一种改善表面麻点缺陷的薄规格中低牌号无取向硅钢及其生产方法
本发明提供一种改善表面麻点缺陷的薄规格中低牌号无取向硅钢及其生产方法,成分C≤0.0025%,1.2≤Si≤1.65%,0.25%≤Mn≤0.35%,0.06%≤P≤0.11%,0.1%≤Als≤0.2%,S≤0.0025%、N≤0.0025%,Ti≤0.0025%,其余为Fe及不可避免的杂质。与现有技术相比,本发明采用较低氢气浓度,防止炉内氧化铁皮还原,减轻碳套辊的腐蚀程度,减少碳套辊结瘤率,改善带钢表面质量;采用合理合金成分设计,提高带钢的力学强度,降低碳套辊结瘤对带钢表面的影响程度,改善带钢表面质量。产品厚度为0.35mm,板面麻点发生率降低,无手感,且辊身周长周期范围内麻点个数≤5个。
铸坯热装温度对无取向硅钢中AlN和MnS析出行为的影响
通过固溶度积公式计算及热模拟实验,对不同热装和加热温度条件下的无取向硅钢铸坯中析出相进行了研究.在低于950℃热装时,铸坯中AlN的析出量和尺寸不再变化,但MnS和AlN-MnS的数量及平均尺寸随着热装温度降低而进一步增加,并在温度低于600℃时达到最大值后保持不变.与1200℃相比,1100℃加热的铸坯中AlN、MnS的总固溶量相对更少.相比850℃热装,600℃热装再加热到1100℃的铸坯中AlN和MnS的总固溶量更少,且AlN和MnS尺寸更大.合适的热装温度和加热温度分别为600℃和1100℃. Based on solubility product calculation and thermal simulation experiments,precipitated phases in continuous casting slabs of non-oriented silicon steel were systematically studied at different hot charging and heating temperatures.When the hot charging temperature is below 950 ℃,the content and size of AlN remain unchanged,but the quantity and size of MnS and AlN-MnS increase when the hot charging temperature decreases,reach maximum and remain unchanged when the hot charging temperature is belo...
CN202111240507.0一种切口耐蚀性良好的无取向硅钢及其生产方法
本发明公开了一种切口耐蚀性良好的无取向硅钢及其生产方法,属于电工钢生产技术领域。本发明的无取向硅钢包括以下质量百分比的元素:Si:0.2~2.7%,Mn:0.15~1.0%、Als:0.5~1.0%,Cr:0.1~0.3%;Ni:0.2~0.5%,P:≤0.01%,其余为Fe及不可避免的杂质。其生产工艺为:铁水预处理、转炉炼钢、真空处理、连铸、加热、热轧、酸洗、冷轧、退火处理和涂覆绝缘层。本发明通过合理的成分配比以及相匹配的生产工艺进行生产,最终得到了切口耐蚀性优良的低铁损、高磁感的无取向硅钢,从而能够有效满足电工钢的使用需求。
CN202111012116.3无取向电工钢以及制造方法
本发明提供了一种无取向电工钢,包括:C0.001~0.010%,Si0.5~4.0%,Mn0.05~0.8%,Al0.2~1.5%,P≤0.002%,S≤0.0015%,O≤0.002%,N≤0.0015%,各成分均为质量百分比;还提供一种无取向电工钢制造方法,包括:冶炼钢水、薄带连铸、常化酸洗、冷轧以及退火涂层。本发明中,在冶炼钢水时,控制钢水中C、Si、Mn、Al、P、S、O以及N几种成分的含量,且通过常化工艺,可以有效控制无取向电工钢成品的产品质量,具有较低的铁损以及较高的电磁性能,另外整体制造流程比较短,能够达到节能环保的目的,而通过冷连扎,有利于提高产品的质量、成材率和生产效率。
加热温度对W470高硅钢连铸坯氧化铁皮的影响
采用SEM、EDS和XRD对不同加热温度下W470连铸坯氧化铁皮的微观形貌及相结构进行研究。结果表明,W470氧化铁皮难以除去的原因是氧化铁皮熔化,液相包裹着FeO,凝固时发生共晶反应,生成FeO/Fe2SiO4共晶混合物,并深嵌入基体。降低加热炉的加热温度,使连铸坯全程在FeO/Fe2SiO4共晶混合物熔点(1177℃)以下加热,可降低氧化铁皮与基体的结合力,能够有效解决W470除鳞困难问题。 The microstructure and phase structure of iron scale of W470 continuous casting billet at different heating temperatures were investigated by SEM,EDS,and XRD.The results show that the reason why the iron scale of W470 removes hardly is that iron scale is melted and the FeO is surrounded by the liquid phase,which forms FeO / Fe2SiO4eutectic mixture and is embedded into the matrix after solidification.Lowering the heating temperature and keeping the continuous casting billet heating under the melt...
硅钢连续退火机组的节能措施
针对硅钢连续退火机组的主要能源介质消耗现状,对现有生产工艺和设备研究采取机组循环用水、增加清洗段漂洗级数等措施可节约大概27 m3/h的过滤水量,并可减少78%的弱碱处理量;将炉子烟气换热系统增加一级余热回收,每年回收的余热相当于583 t标煤消耗,可节约蒸汽5 368 t。 The present situation of energy consumption for silicon steel annealing line is analyzed in this paper.In existing process and equipment conditions,increasing the number of cleaning series will lead to a saving of about 27 m3/h of filter water and reduce 78 % of weak base processing volume.For the flue gas heat-exchange system,adding a waste heat recovery device will recover waste heat equivalent to 583 tons of standard coal per year,corresponding to a saving of steam 5 368 t per year.
CN202123109665.0一种高磁感取向硅钢加工用具有定位结构的热轧装置
本实用新型涉及热轧设备技术领域,公开了一种高磁感取向硅钢加工用具有定位结构的热轧装置,包括:机体,所述机体的下端固定有底座,所述机体的上端固定有顶板,所述机体的中部开设有安置腔,所述安置腔的两侧内壁开设有滑槽,所述顶板的上端嵌装有液压杆,且液压杆的伸缩端贯穿在安置腔的内部,所述液压杆的伸缩端固定有第一辊座,所述第一辊座的下方安置有第二辊座。该高磁感取向硅钢加工用具有定位结构的热轧装置设置有辊盘,辊盘用于通过螺栓固定内侧的轧辊,使得轧辊能够跟随辊盘的转动而转动,动力传输较为稳定,且轧辊可以从辊盘上进行拆卸,在轧辊损坏进行应急处理时操作更加便利,轧辊便于更换和维护。
CN202123127843.2硅钢片生产用上料装置
本实用新型公开了硅钢片生产用上料装置,属于硅钢片生产领域,包括本体,所述本体包括侧板和U型板,所述侧板固定连接在U型板的一侧,所述本体的顶部横向设置有平移机构,所述平移机构上安装有气缸,所述气缸的底部安装有吸盘,所述U型板内腔的底部竖向固定连接有弹簧,所述弹簧远离U型板的一端水平固定连接有升降板,所述平移机构包括电机、螺纹杆、限位板和移动块,所述电机安装在侧板的顶部,所述电机的输出轴与螺纹杆的一端固定连接,通过设置弹簧,在第一个物料从上料装置移出后弹簧的弹力推动剩余物料,使得剩余物料进行上升,避免吸盘触碰不到物料的问题,简化吸盘移动轨迹,加快上料速度。
CN202023339444.8防飞料的硅钢抛丸设备
本实用新型属于抛丸设备技术领域,具体涉及一种防飞料的硅钢抛丸设备,包括料仓和安装在料仓内的抛丸器,料仓的相对两侧上开有对称设置的通口,抛丸室内设有穿过两通口并向料仓室外延伸的输送辊道,输送辊道包括辊架和转动连接在辊架上的多个转辊;料仓的侧壁上滑动连接有用于封堵通口的挡料板,挡料板上设有用于固定挡料板的固定件;挡料板的下部内滑动连接有一端伸出挡料板的密封板,密封板与挡料板之间连接有弹性件。使用本方案,硅钢与通口之间的缝隙能被有效封堵,有效避免钢丸通过通口与硅钢之间的缝隙排出,提高抛丸设备的密封性,防止飞料。
CN202080097255.8无取向电工钢板及其制造方法
根据本发明的一个实施例的无取向电工钢板,以重量%计,所述钢板包含Si:2.1至3.8%、Mn:0.001至0.6%、Al:0.001至0.6%、Bi:0.0005至0.003%和Ge:0.0003至0.001%,余量包含Fe和不可避免的杂质。
CN202123193716.2硅钢专用消泡剂生产温度控制装置
本实用新型公开了硅钢专用消泡剂生产温度控制装置,包括底板及设置在底板上端的温控桶,所述温控桶的内部设置有温控腔,所述温控桶的上下两端分别安装有进料口及出料口,所述温控桶的内部设置有便于温度控制的温度控制机构,所述底板上设置有用于搅拌的搅拌机构;所述温度控制机构包括安装在温控桶上的进气管及出气管,所述进气管及出气管与温控腔的内部相通设置。本实用新型的硅钢专用消泡剂生产温度控制装置,整个温控处理操作简单、实施便捷,便于对消泡剂进行温度控制,且冷却介质或者加热介质可以直接对消泡剂进行加热或是降温,降低了输送过程中的能量消耗,提高了消泡剂温度控制的效率。