钢厂
双辊连铸无取向硅钢铸带特征及常化作用研究
双辊连铸技术是冶金及材料领域内的一项前沿技术,对于生产高品质硅钢具有独特优势.本实验研究了一种双辊铸轧w[Si]=4.5%的无取向硅钢,考察其铸态和常化处理后样品的组织、织构及析出相尺寸特征.结果表明:铸带组织以与铸带法向成5~20(°)倾角的柱状晶为主,晶内存在少量0.3~0.4μm的AlN析出相,铸带织构以λ(<001>//ND)织构为主,表层织构漫散.950℃/10 min常化处理后,析出相尺寸增大,表层λ织构增强. As an advanced technique of metallurgy and material science,twin- roll strip casting has unique advantages for producing high quality silicon steel. The present study was aimed at a 4. 5% Si non- oriented electrical steel for analyzing the structure,texture and the size of precipitates at the initial and normalized state. The results revealed that the initial structure mainly consisted of columnar grains with 5 ~ 20( °) angle to the normal of cast strip,and some AlN precipitates of 0. 3 ~ 0. 4 μ...
硅钢50A1300的流变应力和临界动态再结晶行为
用Gleeble1500D模拟试验机在变形温度为950~1 200℃、应变速率为0.01~8s-1、最大变形程度为60%的条件下,对硅钢50A1300做单道次压缩试验,首先分析了不同参数对流变应力的影响,然后用回归法确定了应力模型中的变形激活能及材料常数,得到硅钢50A1300在峰值应力条件和稳态应力条件下的变形激活能分别为270.360和91.557kJ/mol,同时得到了流变峰值应力模型,模型的相关系数为0.997。最后通过作lnθ-ε图的方法找到了硅钢50A1300发生动态再结晶的临界应变量,并回归得到峰值应变量、临界应变量与参数Z/C的关系式。 To analyze the effects of different parameters on the flow stress and critical strain of the dynamic recrystallization,single-pass compression experiments were carried out with silicon steel 50A1300 specimens using a Gleeble1500D thermal simulator at a temperature range of 950-1 200 ℃ and strain rate range of 0.01-8 s-1 under the condition of maximum deformation of 60%.The average deformation activation energy is respectively 270.360 and 91.557 kJ/mol under the peak stress and steady-state stres...
D21硅钢芯片冲压工艺分析及模具设计
变压器D21硅钢铁芯片采用冲压工艺生产。首先对其工艺进行了分析,确定了冲压方案。对产品进行了排样设计,计算了冲压力,确定了压力中心。然后,设计了单工序落料模具,完成了模具装配图。 D21 silicon steel chips for transformer are produced by stamping.First,its stamping process was analyzed and the scheme of the stamping process was determined.The product layout was designed,the punching pressure was calculated,the pressure center was determined.Then,the blanking die with single procedure was designed,the die assembly drawing was completed.
CN202111348422.4一种厚度≤0.15mm无取向硅钢带及生产方法
一种厚度≤0.15mm无取向硅钢带,其组分及wt%为:Si:2.0~6.5%,Mn:0.13~0.40%,S≤0.020%,P≤0.020%,Als:0.15~0.9%,C≤0.010%;工艺:经冶炼、浇注成坯后热轧至中间坯厚度;冷轧;常温脱脂;光亮罩式退火;经碱洗后涂覆;分条。本发明在保证铁损P1.0/400£13W/kg,磁感B2000³1.5T下,还使钢带厚度公差不超过±0.005mm,最小叠装系数³0.92完全满足连续冲制要求。
氢氧化镁煅烧制备硅钢级氧化镁的研究
以青海盐湖氯化镁为初级原料,采用喷雾热解法制备原料氧化镁。原料氧化镁通过水化制备氢氧化镁。将氢氧化镁过滤、洗涤、烘干、粉碎、煅烧,制备硅钢级氧化镁。本文重点考察煅烧温度、煅烧时间、料层厚度等因素对氧化镁水化率的影响,采用均匀实验设计和DPS数据处理,确定最优煅烧实验条件为:煅烧温度1250℃,煅烧保温时间4小时,料层厚度0.5cm。在此条件下得到的硅钢级氧化镁完全满足硅钢及氧化镁的行业标准。 The magnesium oxide is prepared by Spray pyrolysis process,which magnesium chloride from Qinghai Salt Lake is used as primary raw material,and hydrated to magnesium hydroxide,then obtained silicon steel magnesia through filtering,washing,drying,crushing and calcinations.In this paper,influences of some factors on magnesia hydration rate are studied,such as calcination temperature,calcination time and material thickness.After average experimental design and DPS data processing,optimal calcination...
离散粒子群优化算法在硅钢涂层近红外光谱厚度检测中的应用研究
提出一种基于粒子群优化算法实现的硅钢涂层厚度近红外光谱检测新方法。首先,采用近红外光谱仪采集获得了硅钢表面绝缘涂层的近红外光谱,然后,采用离散粒子群算法筛选出近红外光谱数据的最佳波长变量并组成新的光谱数据,最后,建立涂层厚度的核偏最小二乘定量分析模型。实验显示,所建定量分析模型对检验样本分析的绝对误差范围为-0.12~0.19μm,最大相对误差为14.31%,完全符合现场检验需要。研究表明,离散粒子群算法可以有效地筛选出携带更多有用信息的波长变量,提高定量分析模型的分析准确度和速度,是一种有效的近红外光谱波长筛选方法,同时,近红外光谱法也是一种有效的硅钢绝缘涂层厚度检测方法。 A novel thickness measurement NIR spectrometry for surface insulation coating of silicon steel based on discrete binary particle swarm optimization(DBPSO) algorithm is presented.First,we used NIR spectrometer to collect the NIR spectra of insulation coating of silicon steel,and then,DBPSO algorithm was used to select the optimal wavelength variates and composed a new spectra set.Last,the authors created the thickness quantitative analysis model using kernel partial least square algorithm.The exp...
取向硅钢连续退火的工艺与设计
分析了影响脱碳效果和结晶行为的各种要素及其相互制约关系,提出了Hi-B连续退火工艺曲线,总结得出快速加热及合理稳态气氛是实现工艺制度的关键。结合实际工程,介绍了在连续退火炉设计中快速加热和气氛设计的考虑方法,并指出随着Hi-B产品的发展,如何改进这些方法将是连退工程研发的方向之一。 The factors which affect decarbonization and crystallization and the mutual restriction between them were analyzed.A complete continuous annealing process for Hi-B was put forward.As a result,the rapid heating and the proper steady atmosphere were two important factors.According to an actual project,the consider methods for designing rapid heating and proper steady atmosphere were introduced,and it is pointed that with the development of Hi-B technique,how to improve these techniques would be on...
CN202111247576.4一种冷轧硅钢厚度缺陷识别方法、装置及系统
本发明涉及一种冷轧硅钢厚度缺陷识别方法、装置及系统,本发明的方法包括如下步骤:采集带钢设定厚度及其实际测量厚度并保存;将带钢实际测量厚度与带钢设定厚度相减得到实时厚度差;根据实时厚度差计算厚度缺陷评分;根据评分结果,确定带钢在厚度这一指标的缺陷等级。本发明评估过程考虑了厚度波动情况,并进行量化,能成功识别冷轧硅钢的厚度缺陷,设别准确性较高,提高了冷轧硅钢生产水平,为冷轧硅钢质量控制提供依据。
CN202110269190.7一种含Bi高磁感取向硅钢热轧带钢边部质量控制方法
一种含Bi高磁感取向硅钢热轧带钢边部质量控制方法:炼钢;连铸;铸坯加热;粗轧,粗轧道次不低于4道次,各道次压下率控制在20~33%;规精轧及进行后工序。本发明通过对热轧工序的控制,能使热轧带钢边部开裂的尺寸降低至不超过5mm,且边部开裂≤2mm比率能达到95%以上,后工序切边量很少甚至无需切边即可进行冷轧,使产品成材率能比现有技术提高2~4%;且由于铸坯加热温度的降低使能耗也随之降低。
CN202110784113.5一种硅钢连退炉辊除瘤方法及装置
本发明涉及硅钢技术领域,尤其涉及一种硅钢连退炉辊除瘤方法及装置。包括连杆、手柄、磨削片、密封盖、端盖与套筒;磨削片垂直固接在连杆一端的外壁上,手柄固接在连杆的另一端,手柄与磨削片处于同一平面上;连杆套接在套筒内,连杆能沿套筒轴向移动,套筒固接在端盖上;硅钢连退炉辊下方的炉墙设有与连杆及磨削片相应的磨辊孔,端盖或密封盖固接在磨辊孔处。1)确定结瘤炉辊;2)确定结瘤在碳套辊上的位置;3)插入除瘤装置;4)磨削;5)抽出。本发明降低废品量,提高成材率;减少停炉处理结瘤时间,降低能耗,提高生产率;提高难磨瘤辊的修复率,降低炉辊成本。
CN202110494444.5一种物理喷砂方式制备取向硅钢薄带无底层原料的方法
本发明公开了一种物理喷砂方式制备取向硅钢薄带无底层原料的方法,步骤包括:S1、坯料预处理;S2、涂覆隔离剂,后进行高温退火;S3、拉伸热平整;S4、表面喷砂处理,去除底层;S5、去应力退火;本发明优点在于,采用喷砂的物理办法制备取向硅钢薄带无底层原料,代替了传统的用酸去除取向硅钢涂层或硅酸镁底层,结合退火去应力,显著改善了加工质量,使整个加工过程更加环保,也有利于控制成本。