钢厂
电工钢铸锭内析出相粒子特征及回溶行为
利用场发射电镜及能谱仪研究了取向电工钢薄、厚板坯铸锭中不同区域的析出相差异,确定了MnS、AlN及Fe3C的析出顺序和形貌特征。结果表明AlN以先析出的MnS为形核核心,形成粗大微米级的复合析出相。针状Fe3C既可以在复合析出相表面形成也可以在基体中单独出现,主要受冷却速度的影响。在1250℃保温1~2 h,AlN、Fe3C均可完全回溶,但部分MnS仍不回溶。MnS尺寸随着保温时间延长而增大。导致热轧板中沿轧向分布的粗大MnS,减弱了粒子钉扎力。 Precipitates in thin and thick slabs of electrical silicon steel were investigated by means of field emission SEM and EDS analysis.The precipitation sequence and the morphology of MnS,AlN and Fe3C particles were identified.AlN particles are observed to be nucleated on surface of MnS forming micron-meter-sized complex particles.Acicular Fe3C can precipitate on surface of the complex MnS/AlN particles or directly from matrix depending on cooling rate of the slabs.After holding at 1250 ℃ for 1-2 h,...
CN202122099636.4一种防溢出的无取向硅钢绝缘涂液存储装置
本实用新型公开了一种防溢出的无取向硅钢绝缘涂液存储装置,涉及无取向硅钢绝缘涂液技术领域,为解决现有无取向硅钢绝缘涂液存储设备在存储过程中存在涂液过满,导致液体溢出产生浪费现象的问题。所述绝缘涂液存储机构本体上方的一侧设置有液位监测器,所述液位监测器的下端设置有监测杆,所述液位监测器的输出端设置有单片机,且液位监测器的输出端与单片机电性连接,所述绝缘涂液存储机构本体的内壁设置有压力传感器,且压力传感器设置有若干个,所述压力传感器的输出端与单片机的输入端电性连接,所述绝缘涂液存储机构本体的内部设置有泵体,且泵体设置有两个,所述泵体的一端设置有溢流输送管。
退火工艺对无取向硅钢磁性能的影响
分析总结退火工艺各参数对冷轧无取向硅钢磁性能的影响,结合设计和生产实践经验介绍退火工艺中各参数的实际生产取值,并针对现生产工艺过程中出现的典型问题提出解决办法。 It is analyzed and summarized the great influences on magnetism of cold rolled non-oriented silicon steel affected by various annealing process data in this article.The relevant settled ways is raised.According to the actual value presetting ways for various annealing process data based on design and production,as well as typical problems occurred during production.
CN202110332150.2一种宽频率低铁损变频电机用无取向电工钢及制造方法
本发明公开了一种宽频率低铁损变频电机用无取向电工钢及制造方法,属于无取向电工钢领域。针对现有无取向钢在较宽频率范围内电磁性较差的问题,本发明提供一种宽频率低铁损变频电机用无取向电工钢,包括如下重量百分比的各组分:Si:2.80%~3.50%;Als:0.20%~0.60%;Mn:0.20%~0.60%;P:0.01%~0.20%;C:≤0.005%;S:≤0.02%;N:≤0.02%;Ti:≤0.005%;其余为铁和不可避免的杂质;其中C、S、N和Ti的重量百分比满足下式:C%+S%+N%+Ti%≤0.009%。通过控制合金元素的含量达到电工钢电阻率增加、磁滞伸缩减小,涡流和磁滞损耗均降低的目的。通过本发明提供的制造方法在正火过程中选用低温工艺,改善随着合金元素量的增加金属强度增加、塑性降低、冷加工性能降低的问题,使其最终在较宽频率范围内电磁性能优异。
CN202121910597.5硅钢冲压片质量筛查分拣装置
本实用新型涉及一种硅钢冲压片质量筛查分拣装置,包括:第一组传送带机构,第一摄像头,设置于第一组传送带机构的上方,用于对硅钢冲压片的第一表面的残损进行检测;第一机械手机构,设置于第一组传送带机构的上方且位于所述第一摄像头的后方;翻转装置,设置第一组传送带机构的后方,用于对第一组传送带机构传输的初检良品进行翻面并将翻面后的初检良品传输给第二组传送带机构;第二组传送带机构,设置于翻转装置的后方;第二摄像头,设置于第二组传送带机构的上方,用于对硅钢冲压片的第二表面的残损进行检测;第二机械手机构,设置于第二组传送带机构的上方且位于第二摄像头的后方。本实用新型可高效的检测每一个产品的外观质量。
热处理工艺对含Mn高硅钢热轧带的组织及硬度的影响
研究了热处理工艺(退火温度、保温时间、冷却方式)对含Mn的Fe-6.5wt%Si高硅钢热轧带的显微组织及硬度的影响。结果表明,退火温度对Fe-6.5wt%Si合金的组织和显微硬度均有较大影响,随退火温度升高,平均晶粒尺寸和显微硬度均明显增大。小于1 h退火时,晶粒长大缓慢,而长时间(>1 h)退火时,一些次表层晶粒将发生异常长大。水冷组织比空冷组织略细小,但水冷显著降低了显微硬度。Mn含量提高能抑制850℃退火时晶粒的长大,并且促进退火后高硅钢的软化。 The influences of heat treatment process(annealing temperature,heating time,cooling methods) on the microstructure and microhardness of Fe-6.5wt%Si high silicon steel containing manganese for hot rolled strip were studied.The results show that the annealing temperature has a great effect on the microstructure and microhardness of Fe-6.5wt%Si alloy,and as the annealing temperature increases,the average grain sizes and microhardness will significantly increase.When annealing time for less than 1 h...
提高热轧硅钢凸度精度的工艺措施
以太钢热连轧厂的硅钢为研究对象,利用凸度仪测量热轧带钢出口凸度值,采用矩阵和失效模式的分析方法了解影响带钢凸度变化的主次因素。研究结果表明:通过有效控制轧制过程中的加热温度、时间及采用合理的辊型,硅钢凸度精度提高了4.34%左右。 In this paper,we take the hot-rolled silicon steelsheet of Taigang as the research symbol,exit profile was measured by convex instrument,the primary and secondary factors that affect the strip profile were measured by using matrix and failure mode analysis methed.The results indicate that convexity accuracy has significantly improved by nearly 4.34% through the effective control of the heating temperature,heating time and the use of correct roller type in the process of hot rolling.
压下率对6.5%Si电工钢温轧板织构的影响规律
6.5%Si电工钢是一种优异的软磁材料,织构对其磁性能影响很大。利用温轧工艺对6.5%Si电工钢热轧板进行不同压下率轧制,研究了温轧板织构随压下率的变化规律。实验结果显示,随着压下率的增大,{100}〈110〉、{110}〈100〉和γ纤维织构在薄板表层中的强度先增强后减弱,当压下率达到75%时,沿板厚方向形成3个组织区域:表层细晶粒区({110}〈100〉取向为主)、过渡层({111}〈110〉和{111}〈112〉变形晶粒区)和中心层(以拉长的γ纤维织构和{100}〈110〉取向晶粒为主),这种组织和织构不均性对后期织构的发展有重大影响。 6.5wt% Si electric steel has excellent soft magnetic properties,on which texture play important role.In this experiment,warm rolling technique was employed to investigate the effect of rolling reduction on texture.It was found that the density of {100}〈110〉,{110}〈100〉 and γ-fiber textures first increased and then decreased with increasing of the rolling reduction.At 75% reduction,the microstructure along the thickness of the sheet formed three zones,containing surface layer with {110}〈100〉 orien...
CN202111247576.4一种冷轧硅钢厚度缺陷识别方法、装置及系统
本发明涉及一种冷轧硅钢厚度缺陷识别方法、装置及系统,本发明的方法包括如下步骤:采集带钢设定厚度及其实际测量厚度并保存;将带钢实际测量厚度与带钢设定厚度相减得到实时厚度差;根据实时厚度差计算厚度缺陷评分;根据评分结果,确定带钢在厚度这一指标的缺陷等级。本发明评估过程考虑了厚度波动情况,并进行量化,能成功识别冷轧硅钢的厚度缺陷,设别准确性较高,提高了冷轧硅钢生产水平,为冷轧硅钢质量控制提供依据。
基于Matlab的硅钢连续退火线纠偏系统分析及仿真
硅钢连续退火线是无取向硅钢生产的成品线。由于受机组布置的影响,带钢经转向辊进出口活套后,当套量达到60%后就出现偏离生产线的情况,从而影响最终产品的质量及成材率,甚至损坏设备。针对某冷轧厂硅钢连续退火机组出口活套入口处带钢跑偏开展纠偏研究,利用Matlab对该纠偏系统进行动态仿真研究,分析系统的稳定性。 Silicon steel continuous annealing line is non oriented silicon steel production of finished product line.Due to the influence of unit layout,strip by roll Import & Export loop,when the set volume reached 60% after the emergence of deviation from the production line,thus affecting the quality of the final product and the rate of finished products,and even damage the equipment.For the export of continuous annealing line in cold rolling silicon steel strip deviation rectification loop at the e...
CN202120000229.0一种镀铝锌硅钢钣冲压装置
本实用新型公开了一种镀铝锌硅钢钣冲压装置,包括安装板,所述安装板的上表面延伸至下表面开设有上下管贯通的板件交换槽,所述安装板的上表面且位于板件交换槽的正上方通过固定螺栓固定连接有模座板。本实用新型,通过设置二次镀膜箱,对冲压后的硅钢钣进行二次铝锌镀膜,避免了冲裁面的暴露导致硅钢钣慢性腐蚀,提升了镀铝锌硅钢板的质量和使用寿命,通过设置夹取机构,对硅钢钣自动取放操作,减少了人力操作,提高了效率的同时,提高了设备安全性,通过设置废料回收槽,对冲压产生的边角料进行集中回收在利用,提升了生产过程中的环保性,通过优化结构设计,提高了镀锌硅钢钣的生产效率,降低生产成本。
CN202123227418.0一种铁芯硅钢片卷材的自动放卷上料装置
本实用新型公开了一种铁芯硅钢片卷材的自动放卷上料装置,包括放卷机、导向平台和防折组件,所述导向平台间距设置在放卷机的下方,所述导向平台与放卷机之间构成供料带缓冲的缓冲空间,所述料带在缓冲空间内呈U型状走向,所述导向平台的上方间距设置有防折组件,所述防折组件与导向平台之间构成供所述料带通过的导向通道,所述防折组件设置在料带的内弯侧。通过防折组件对料带的内弯侧进行支撑,能够有效的防止料带被过度弯折,能够对料带进行缓冲和缓冲保护,保证料带放卷上料的稳定性。