一种硅钢厂调功器故障报警自动复位的方法,包括:通过人机界面对炼钢炉温度进行设定,并在炼钢过程中实时获取炼钢炉温度;将炼钢炉实时温度与设定温度进行对比,当炼钢炉实时温度低于设定温度时,启动调节器;调节器输出功率使电阻带加热,使炼钢炉实时温度达到设定温度;当调节器发生故障时,调节器将故障信号发送给后台服务器,后台服务器根据故障指令,按预设规则控制与调节器连接的继电器,控制继电器按压复位按钮,使调节器自动复位。本发明解决了现有技术中通过电气人员来通过复位消除故障状态,耽误时间长,容易产生废品的问题。
2021-03-29 296 6.8

研究了退火温度和退火时间对电沉积硅钢试样中的断面层组织、硅在试样中的分布情况、织构分布和磁性能的影响。结果表明:退火温度为1000℃、退火时间为210 min时得到的试样晶粒分布均匀、硅在试样中分布均匀、硅平均浓度为6.3715%(接近6.5%)。试样的织构分析及磁性能检测的结果表明,在较高温度下延长退火时间可增加{100}和{110}面织构,降低铁损,所得试样的磁性能较为良好。 The effect of annealing temperature and time on the microstructure, distribution of silicon,texture and magnetism of the high silicon steel prepared by electrodeposition was investigated. The results showed that after annealing at 1000℃ for 210 min, the mean grain size of steel was about 190 μm with a uniform grain size distribution, and the silicon is also uniformly distributed on the entire cross section with an average Si concentration 6.3715%(close to 6.5%); With the increasing annealing tim... 
2014-07-28 215 5.8

从取向硅钢生产路线的选择、工艺技术的改进和生产设备的改造三方面进行了生产取向硅钢的节能降耗技术改造.通过完善多元抑制剂配方生产低温取向硅钢,通过加抛丸的酸洗、带面超声波清洗、改进连续退火炉以及余热循环利用等技术改造,使2012年取向硅钢的产量与未进行技术改造前的2009年相比提高了2.5倍,产品磁性上升了一个半牌号,能耗下降了8.9%,成材率提高了6.4%,生产成本下降了22%,综合效益显著. Energy saving technological transformation was carried out in the production of grain oriented silicon steel from three aspects of the oriented silicon steel production process route selection,technology improvement and equipment renovation.Through the improvement of multiple inhibitor formulations for producing low-temperature grain-oriented silicon steel,and by adding the blasting pickling,the belt surface ultrasonic cleaning,improvement of continuous annealing furnace,waste heat recycling tec... 
2013-02-28 249 5.8

介绍了国内无底层取向电工钢生产技术水平、产量和用途,简述了无底层取向电工钢作为取向电工钢超/极薄带母料及应用于制作大型发电机组铁心、风电等电机铁心和变压器铁心等的情况。 The production technology level,output and application of domestic glassless grainoriented electrical steel were introduced,and the application of glassless grain-oriented electrical steel as parent material of ultra-thin strip of grain-oriented electrical steel and in making large-scale electric generator cores,wind power motor cores and transformer cores were briefly described. 
2022-02-28 578 5.8

根据本发明的一个实施例的粘接涂料组合物,其包含聚乙烯丙烯酸酯100重量份和无机颗粒3至25重量份,所述聚乙烯丙烯酸酯包含由以下化学式1表示的重复单元和由以下化学式2表示的重复单元,所述聚乙烯丙烯酸酯包含75至95重量%的由以下化学式1表示的重复单元、5至25重量%的由以下化学式2表示的重复单元。
2020-12-17 231 6.8

采用双辊薄带连铸工艺制备了厚度为2.4mm的3.98%Si-0.71%Al无取向硅钢带,经常化、冷轧、不同温度退火后,对其显微组织、析出物、织构和磁性能进行了检测分析。结果表明:随着退火温度的提高,退火板晶粒尺寸增大,组织均匀性提高;退火板析出物主要是AlN和MnS与AlN复合析出物,尺寸较粗大,达0.5~2.5μm;退火板织构沿厚度方向变化明显,表层和1/2层存在较强的{100}织构,1/2层还存在较强的{111}织构,1/4层主要是{112}织构;随退火温度的升高相应的铁损和磁感应强度均降低。 Using twin roll thin strip continuous casting technique,the 3.98%Si-0.71%Al no-oriented silicon steel strip in thickness of 2.4mm was produced.The microstructure,precipitates,texture,and magnetic properties of the sheet after normalizing,cold rolling and annealing at different temperatures were studied.The results show that with annealing temperature increase,the grain size and uniformity of annealed sheet increased.The main precipitates in coarse size of 0.5-2.5μm in annealed sheet were AlN and... 
2014-01-28 308 5.8

本发明公开了一种宽频率低铁损变频电机用无取向电工钢及制造方法,属于无取向电工钢领域。针对现有无取向钢在较宽频率范围内电磁性较差的问题,本发明提供一种宽频率低铁损变频电机用无取向电工钢,包括如下重量百分比的各组分:Si:2.80%~3.50%;Als:0.20%~0.60%;Mn:0.20%~0.60%;P:0.01%~0.20%;C:≤0.005%;S:≤0.02%;N:≤0.02%;Ti:≤0.005%;其余为铁和不可避免的杂质;其中C、S、N和Ti的重量百分比满足下式:C%+S%+N%+Ti%≤0.009%。通过控制合金元素的含量达到电工钢电阻率增加、磁滞伸缩减小,涡流和磁滞损耗均降低的目的。通过本发明提供的制造方法在正火过程中选用低温工艺,改善随着合金元素量的增加金属强度增加、塑性降低、冷加工性能降低的问题,使其最终在较宽频率范围内电磁性能优异。
2021-03-29 202 6.8

本发明揭示了一种新能源驱动电机用无取向硅钢及其生产方法。所述硅钢通过依序进行的炼钢、连铸、热轧、常化、酸洗、无预热单机架冷轧、退火、冷却、涂层和精整制备而成,炼钢时不添加Cu、Cr、Ni、Nb、V、Ti,硅钢的化学成分:Si:2.95%~3.15%,Al:0.75%~0.95%,Si+2Al:4.6%~4.9%,Mn:0.5%~0.7%,Sn:0.03%~0.04%,C≤0.0025%,余量铁;Mn/S≥380,Al/N≥200。本发明在保证磁性能的同时,提高了强度,解决了现有技术所存在的磁性能和强度的兼顾问题,能够满足新能源汽车的驱动电机上的应用要求。
2021-10-26 523 6.8

针对本钢薄板坯铸机在生产无取向电工硅钢的过程中存在的铸坯拉断、中包增碳、增氮等问题,进行了连铸工艺优化。通过采用新型无碳中间包覆盖剂、环保中间包干式料及专用结晶器保护渣后,降低了铸坯增碳量;通过控制钢包到中间包的增氮环节,降低钢水增氮;适当增大二冷水量,控制钢水过热度,防止铸坯拉断等生产事故的发生。改进工艺后,精炼后到成品铸坯的平均增碳量能控制在10×10-6以内,平均增氮量能控制在4×10-6以内。 The technology optimization has been adopted for preventing nitrogen increasing and carbon increasing in Benxi thin slab producing non-oriented silicon steel.Measures accordingly were adopted and satisfactory results were achieved. 
2011-05-28 356 5.8

【作者】 安斌; ...
2014-09-28 311 5.8

一种提高有效氮和底层质量的高磁感取向硅钢制造方法:冶炼后连铸成坯;对铸坯加热;热轧、常化及酸洗后时效冷轧;在湿式气氛下脱碳退火;在湿式混合气氛下均热;在湿式混合气氛下渗氮退火;进行后工序。本发明与现有技术相比,通过合理控制渗氮过程,提高渗氮后钢板基体内氮含量与总氮量之间的比例达到80%以上,使无点状露晶产生,最终获得产品的底层质量优异。
2021-01-29 194 6.8

对新能源汽车以及驱动电机的现有市场和未来市场规模进行梳理分析,通过自建计算公式推导出我国2021年1-11月份驱动电机用电工钢的总量,进而预测未来10年中国新能源汽车驱动电机用电工钢情况,为无取向电工钢的生产和在电机中的应用提供有价值的参考。 The current market and future market size of new energy vehicles and traction motors were analyzed,and the total amount of electrical steels used in traction motors in China from January to November 2021 was derived by using self-built calculation formulas,and then the situation in the next ten years of electrical steel used in traction motors of new energy vehicles in China was predicted.It will provide a valuable reference for the production of non-grain oriented electrical steel and its appli... 