真空感应炉熔炼高硅电工钢脱氧工艺的研究
在50Kg氧化镁坩埚真空感应炉上进行高硅电工钢的脱氧试验。结果表明,通过控制原料的成分、高真空下的碳氧反应和炉衬分解向钢液中的供氧,可使钢液的总氧含量≤15×10-6;在维持高温高真空条件下,当钢液中的反应达到一定程度后,延长精炼时间并不能降低钢液的总氧含量;完成精炼后加入硅钙合金沉淀脱氧可进一步降低钢液的总含氧量,但脱氧效果有限。 The test of high-silicon electric steel deoxidation has been carried out in 50Kg vacuum induction furnace with magnesium oxide crucible.Results show that the total oxygen could be ≤15×10-6in molten steel by controlling material components,carbon-oxygen reaction in high vacuum and oxygen contamination from crucible materials on molten steel;And when the reaction was carried through to a certain extent,total oxygen in molten steel could not be reduced by the extension of refining period in high va...
球刻痕法对高磁感取向硅钢磁性的影响
试验研究了球刻痕法对高磁感取向硅钢的铁损、矫顽力、相对磁导率、巴克豪森噪声等磁学性能的影响.研究结果表明:经过球刻痕处理后,高磁感取向硅钢的铁损明显降低,矫顽力下降,8 mm球刻痕过后铁损值与矫顽力分别下降16.2%和14.7%,且铁损和矫顽力均随刻痕间距降低而减少.刻痕后的高磁感取向硅钢磁导率在高磁感应强度下明显上升,刻痕后巴克豪森噪声值明显降低,经过对比分析确定8 mm为球刻痕的最佳刻痕间距.从磁畴观察、细化磁畴的原理等方面解释了细化磁畴对高磁感取向硅钢性能的影响原因. The effects of the ball scribing on magnetic properties of high permeability grain-oriented silicon steels,including the iron loss,coercive force,relative permeability,and Barkhausen noise were investigated. The results showed that the iron loss and coercive force of the high permeability grain-oriented silicon steels apparently decreased 16. 2% and 14. 7% respectively after 8 mm ball scribing and they both decreased with the decrease of the scribing spacing at the same magnetic flux density. At...
400mm硅钢自动轧制试验轧机
西安重型机械研究所为武钢开发了目前国内第一台自动化水平较高的先进可靠的硅钢热轧试验轧机。本文介绍了该轧机的工艺参数、设备组成,技术特点及轧制流程,该轧机在规定的终轧温度范围内,实现了2.5 m/s的快速轧制速度,保证了控制系统准确及时的采集到轧件进出轧辊时的信号,缩短道次间隙时间,实现了自动控制,保证了产品板形及精度的高水平要求,对于硅钢尤其是对其取向硅钢新产品、新工艺的开发具有深远意义。 An experimental prototype of 400 mm silicon steel hot rolling mill was developed by Xi’an Heavy Machinery Research Institue for Wu Gang.The technological parameters,configuration and characteristic of advanced control system in the experimental prototype are introduced in detail.The experimental prototype was realized the fast rolling of 2.5 m/s in the range of specified rolling temperature.Its automatic rolling control system can acquisite the signals that a rolled piece enters in and exits fro...
CSP流程试制50W270高牌号无取向硅钢织构的演变
研究了CSP流程试制50W270高牌号无取向硅钢热轧→常化→冷轧→退火过程中织构的演变.利用电子背散射衍射技术对全流程织构进行测量和分析.发现热轧板织构在厚度方向上存在较大差异,表层主要为铜型、黄铜和高斯织构,1/4层存在微弱的高斯织构和旋转立方织构,中心层以γ纤维织构和旋转立方织构为主,还含有较弱的α纤维织构.与热轧板相比,常化板表层和1/4层织构变化不大,中心层旋转立方织构和α纤维织构增强.冷轧板各层均具有α纤维织构和γ纤维织构.与冷轧板相比,成品板各层中α纤维织构基本消失,还出现了立方织构和高斯织构. This article focuses on texture evolution in 50W270 high-brand non-oriented silicon steel produced by CSP in hot rolling,normalizing,cold rolling,and annealing processes.The texture in the whole process was measured and analyzed by electron back-scatter diffraction.It is found that the texture along the thickness direction in hot-rolled strips changes obviously;there are mainly copper,brass,and Goss textures in the surface layer;the 1/4 layer has weak Goss texture and rotating cube texture;γ-fib...
硅钢连续退火炉无氧化加热段辐射换热研究
以能量平衡和辐射换热理论为基础,通过合理假定,建立了硅钢无氧化加热炉数学模型。采用数值计算的方法,通过自编程序,完成对带钢加热过程温度场的仿真。结果显示:数学模型能够反映带钢在无氧化炉内的加热过程,其升温曲线能够与工艺曲线相吻合;现行炉温分布并非最优,数学模型能够为炉温分布的优化、炉段的设计提供理论依据。 Mathematical model of NOF Section of Continuous Annealing Furnace is established based on energy balance and radiation heat exchange. The temperature field of steel is simulated by mathematical computation. The simulating results show that the mathematical model can reflect the heating process of silicon steel in NOF section, and the heat-up curve is coincide with the processing curve. From the results,it is known that the current furnace temperature gradient is not the best, and the mathematica...
热轧加热时间对稀土取向硅钢抑制剂固溶行为的影响
借助OM、激光共聚焦显微镜、质谱仪和电解萃取等设备和方法,研究了添加微量稀土La(质量分数0.001 1%)的取向硅钢在轧制前采用不同加热保温时间对抑制剂固溶行为的影响。结果表明:当稀土取向硅钢在1 250℃分别保温10、20、30 min后,试验钢晶粒尺寸随保温时间延长有先快后慢的长大趋势;三种抑制剂元素Mn、Cu和Al均发生固溶,保温时间对Mn和Cu两种元素的固溶影响明显,固溶量分别由69.8%和43.7%增加至84.2%和85.2%;随着保温时间的延长,稀土取向硅钢中抑制剂的小尺寸未溶物逐渐减少直至消失,较大尺寸未溶物(300~600 nm)逐渐转变为小尺寸未溶物逐步溶入基体中,数量减少且未溶物的类型由复杂逐渐转变为单一。 In this paper the solid solution behavior of the inhibitor under various holding time in 0.001 1 %La oriented silicon steel during reheating had been investigated by using OM, LM, methods of electrolytic extraction and mass spectrometer. The results showed that grain size of the test steel increased significantly with the holding time prolonging when the rare earth oriented silicon steel was heated to1 250 ℃ and held for 10, 20 min and 30 min respectively, and the growth trend slowed down after ...
TSCR试制高强度无取向电工钢
采用固溶强化、细晶强化和位错强化方法,模拟TSCR流程试开发高强度无取向电工钢,试开发钢的主要合金成分为3%Si、0.83%Al和2.99%Mn。分析热轧、常化、退火后的钢板组织,并针对不同的成品板组织,详尽地分析了相应的力学性能和磁性能。试验电工钢平均晶粒直径为12.37μm时,R p0.2为530 MPa,R m为618 MPa;当退火制度为700℃×4 min,成品组织完全为未再结晶的回复组织时,R p0.2为853.5 MPa,R m为895.5 MPa。该成分的电工钢P15/50或P10/400最小时,对应的平均晶粒直径都大于59.67μm;P10/800或P10/1000最小时,对应的平均晶粒直径都处于12.37~59.67μm尺寸区间。 TSCR was simulated to develop high-strength non-oriented electrical steel with 3% of Si,0.83% of Al and 2.99% of Mn by solution strengthening,grain refinement strengthening and dislocation strengthening.The microstructures of hot rolled plates,normalized plates and annealed plates were analyzed.Furthermore,the mechanical properties and magnetic properties of products with different microstructures were detailedly studied.As the average grain diameter of the steel was 12.37 μm,the yield strength ...
高硅钢温轧过程压下率及中间退火对组织、织构的影响
传统轧制法制备6.5wt.%高硅钢过程中温轧工艺具有显著不同于3 wt.%Si的电工钢的特点及组织织构特征,是开发新型基于织构优化的高硅钢的关键环节。采用EBSD技术对通过热轧、温轧、冷轧及退火工艺制备0.3mm厚的6.5wt.%Si电工钢板的组织和织构进行分析,重点研究温轧过程中的中间退火和大、小压下率组合以控制织构。结果表明,在热轧退火板是部分再结晶组织的情况下,一次性温轧或先小形变量、中间退火后再大形变量的工艺可得到更多的Goss晶粒;经过最终退火后Goss取向会发生偏转,形成部分黄铜取向,而{111}〈112〉取向的晶粒内形核生成近Goss取向的再结晶晶粒;大压下量轧制是最终组织中{111}取向晶粒较多的主要原因。 Warm rolling,a key process of developing new type high-Si electrical steel based on texture optimization,has significant different characteristics from 3wt% Si steel in conventional preparing process. 0. 3mm thickness 6. 5wt. % Si steel,obtained by a series of processes including hot and warm rolling,intermediate annealing and then cold rolling,was analyzed from microstructure and texture by EBSD,which are utilized mainly for investigating the intermediate annealing process and the combination o...
电工钢冶炼过程中硫含量控制
介绍了攀钢冶炼电工钢过程硫含量变化以及过程回硫、增硫情况,采取针对性措施,如:提高铁水装入量、转炉采用石英砂代替复合造渣剂造渣、RH脱硫等,降低钢中硫含量。结果表明:采取相应措施后,电工钢炼成率大幅提高,成品w[S]≤0.008%的比例由改进前的62%提高到92.4%,取得了明显的冶金效果。 The resulfurization and the change of sulphur content in production of electrical steel is analyzed.The targeted measures have been taken,such as increase the loaded quantity of liquid iron,quartz sand replaces the composite slagging agent in the converter and RH desulfurization to decrease the sulphur content of the steel.The result shows,after the measures have been taken,the finished product ratio of electrical steel increase a lot.The ratio of sulfur content of finished product no more than ...
无取向硅钢热轧卷结疤缺陷产生的原因及控制
针对不同牌号的无取向硅钢产生结疤缺陷的难易程度和表面结疤缺陷的外形特征及分布规律,分析了该缺陷产生的原因。通过调整剪前导板的对中度,设置精轧侧导板开度余量及短行程数值,及时修补与更换侧导板,减少带坯与侧导板挤撞程度,有效地降低了结疤缺陷发生率。 This article analyses the cause of the scab defects according to the defects appearance characters and distribution law,degree of difficulty to form scar of non-oriented silicon steel. It can effectively decrease the scabs by different methods,such as adjusting the center line of guide plate,setting the opening margin and short stroke value of the side guide on finishing mill,timely repairing and replacing of side guide,decreasing the collision between the strip and side guide.
常化冷却工艺对低温取向硅钢组织及析出相的影响(英文)
利用OM、TEM与EDS技术,对Fe-3.2%Si低温取向硅钢热轧板进行不同常化冷却工艺处理后的显微组织、析出相及最终产品的磁性能进行分析,并与热轧板的组织和析出相进行对比。结果表明,常化板较热轧板的表层组织均匀,基体中再结晶比例增加,带状组织变窄;常化板中析出物的数量明显比热轧板的多,析出物主要有AlN、MnS及复合析出的(Cu,Mn)S等。在常化温度1120℃、保温3 min的条件下,采用二段式冷却较空冷、淬沸水、淬常温水的冷却工艺,常化板表层显微组织更均匀,沿板厚方向的显微组织的不均匀性显著,取向硅钢的磁性能最高;常化后采用二段式冷却工艺析出的细小析出物数量最多,且弥散分布在基体中,抑制剂的抑制效果最好,对成品获得高磁性最有利。 Microstructure, precipitate and magnetic characteristic of final products with different normalizing cooling processes for Fe-3.2%Si low-temperature hot-rolled grain-oriented silicon steel were analyzed and compared with the hot-rolled plate by optical microscopy(OM), transmission electron microscopy(TEM), and energy dispersive spectrometry(EDS). The results show that, the surface microstructure is uniform, the proportion of recrystallization in matrix increases, and the banding textures are nar...