成品第二次退火工艺对高牌号无取向电工钢35W300组织和性能的影响
对高牌号无取向电工钢35W300的成品进行了第二次退火,对第二次退火后的成品性能、纵横向磁性能差异和组织变化进行了分析。结果表明,随着第二次退火温度的升高,晶粒长大,磁性能优化。铁损平均值下降0.087 5W/kg,磁感平均值升高0.008T。第二次退火温度为820℃的产品的磁性能能够满足用户使用要求。 The product of high grade non-oriented electrical steel 35W300 was annealed at the second time.Microstructure,the difference of magnetic properties in the vertical and horizontal and were studied.The results show that the grain grew up and magnetic properties optimized with the increase of annealing temperature for the second time.Iron loss average declines in 0.0875 W/kg,magnetic induction average increases 0.008 T.The magnetic properties can meet the requirements of users at the second anneali...
辉光放电发射光谱法测定电工钢中8种元素
通过对辉光放电发射光谱法分析电工钢样品光谱行为的研究,分析其工作参数如:电压、电流、预溅射时间和积分时间对光谱强度和稳定性的影响,并以铁为内标元素,优化了工作参数。确定了直流辉光放电光谱法测定电工钢中碳、硅、锰、磷、硫、铬、镍、铜共8种元素的定量分析方法,并对该方法分析的精密度和准确度进行验证,结果表明,各元素的测定结果与认定值和其他方法测定值一致,测量元素结果RSD值小于2%。 Based on research on analyzing the spectrum behavior of the sample taken from the electrical steel by glow discharge optical emission spectrometry,the effect of its operational parameters such as current,voltage,pre-sputtering time and integrating time on the spectral intensity and spectral stability is analyzed.Taking the Fe as an element applied by internal standard method,these operational parameters are optimized,and therefore the quantitative analysis method for testing eight kinds of eleme...
典型半工艺电工钢产品M660-50K5生产及应用技术解析
对欧盟市场汽车压缩机专用产品进行技术解析,对比分析了其电磁性能、退火和发蓝处理、物理性能、化学成分、应用特点等参数。探讨国内外电工钢产品应用方式的不同特点,并结合鞍钢自身工艺装备和炼钢、热轧、冷轧工艺参数介绍了其生产可行性。提供了冶金工艺流程下,后工序电工钢专业生产线及传统冷轧系统生产线两种生产方式,均能满足用户最终使用要求。 The technology of automotive compressor accommodation manufacture of European Economic and Monetary Union market was described.The magnetic properties,annealing bluing,physical properties,chemical composition,application parameters were analysed.The different characteristics of the application of electrical steel products,the feasibility of manufacture on the existing technology and equipment,steelmaking,hot rolled,cold rolled technical parameters were discussed.The professional product line of ...
热轧工艺对TSCR流程生产取向硅钢组织和性能的影响
取向硅钢热轧板中组织、织构梯度对发展完善的二次再结晶十分关键,通过对2种不同热轧工艺生产取向硅钢的组织、织构进行研究,结果表明:采用后道次大压下热轧工艺时热轧板表层再结区晶粒平均尺寸增加,再结晶区厚度增加,高温退火后二次晶粒尺寸减小;采用后道次大压下热轧工艺热轧时,热轧板中平均等效应变高,热轧板厚度心部{100}〈011〉和{100}〈001〉位向取向强度降低,({111}~{113})〈110〉位向取向强度提高,高温退火后{110}〈001〉位向偏离角降低,磁性能提高。 The texture and microstructure gradient in hot rolled grain oriented silicon steel strip was one of the essential factors to achieve a perfect secondary recrystallization.The texture and microstructure of grain oriented silicon steel strip as-rolled with two different hot rolling parameters was investigated.The results show that with big reduction at the end rolling process,the intensity of {100}〈011〉 and {100}〈001〉 orientation reduces with({111}-{113})〈110〉 orientation intensity enhanced in hot...
CN202111444256.8无取向硅钢RH顶枪喷粉脱硫工艺
本发明提供了一种无取向硅钢RH顶枪喷粉脱硫工艺,RH脱碳结束测温定氧,立即加入铝粒脱氧合金化、之后立即依次连续加入合金进行成分调整,合金加完后立即开始顶枪喷粉;加入铝粒的量=铝粒理论加入量+0.2‑0.4kg/t钢;喷粉时,控制喷粉速度与钢液循环流量相匹配;本发明从真空条件下脱硫热力学和动力学角度出发对具有顶枪喷粉功能的RH脱硫工艺进行改进,提高脱硫率。
热轧辊冷却对冷轧无取向电工钢卷纵向磁性的影响及工艺优化
通过对35W300高牌号0.35 mm冷轧无取向电工钢卷(/%:0.002C、2.71Si、0.22Mn、0.015P、0.003S、0.0020N、0.55Als)头、中、尾组织、织构及对应的磁性能的试验研究,发现因热轧时12 MPa高压水连续冷却造成接触轧辊的钢卷头、中、尾在不同温度下轧制,卷取后钢卷头部处于卷心、温度略高而冷却速度略低于钢卷尾部,致使钢卷纵向组织、织构不同,成品卷头、尾各250 m内磁感逐渐增加,铁损逐渐降低,250 m外至钢卷中部磁性能稳定。通过将热轧辊的冷却方式改为周期冷却和卷取后的层流冷却改为钢卷70 m后开始冷却,至钢卷尾部70 m前停止冷却的方式使得钢卷纵向铁损差异明显减小,磁感差异略有改善。 According to the test research on structure and texture of head,meddle and end of 35W300 high grade 0.35 mm cold rolled non-oriented electrical steel strip coil(/%:0.002C,2.71Si,0.22Mn,0.015P,0.003S,0.002 0 N,0.55Als) and corresponding magnetic properties,It is found that due to 12 MPa high pressure water continuous cooling the roller in hot rolling process led to head,middle and tail of strip rolling at different temperature and after coiling the head of strip coil being in center of coil led t...
冷轧无取向硅钢横向厚差控制
冷轧中中低牌号的无取向硅钢多采用万能凸度轧机(Universal crown mill,UCM)生产,其板形好坏受制于UCM轧机板形调节手段的协调使用。为掌握UCM轧机的板形控制特点,建立基于二维变厚度有限元的辊系弹性变形和基于三维差分的轧件塑性变形的六辊轧机耦合模型,对UCM轧机的板形调控性能进行详尽的分析,包括工作辊和中间辊弯辊、中间辊窜辊的调控功效、辊间接触压力分布等。在此基础上,提出可用指导生产的板形控制策略,指出UCM轧机在横向厚差控制方面的不足。针对工业生产中UCM轧机轧制无取向硅钢横向厚差大的问题,在大量仿真计算的基础上,开发具有高次曲线函数的边部变凸度(Edge variable crown,EVC)的工作辊。采用该工作辊后,各种品种的无取向硅钢的横向厚差不大于10μm的百分比由24%提高到99%,横向厚差的均值小于6μm,远小于之前的13μm。 Medium-low grade non-oriented silicon steel is rolled often by universal crown mill(UCM) during cold rolling.Its shape quality is dependent on the coordinated control of several shape adjustment devices of UCM.In order to understand the shape control characteristics of UCM,coupling model of six-high rolling mill,based on two-dimensional varying thickness finite element rolls elastic deformation model and three-dimensional finite difference strip plastic deformation model,is setup for the detaile...
CN202122561833.3一种适用于自动线的硅钢叠装系数性能检测装置
本实用新型公开了一种适用于自动线的硅钢叠装系数性能检测装置,涉及实验仪器自动化技术领域,为解决机器人自动上样至叠装系数测量仪经常发生碰撞的问题;本实用新型包括框架、上压板、下压板、压紧驱动机构、高度探规和加载力值传感器,其中压紧驱动机构设置于框架上端,下压板固定于框架内的下端,上压板安装于下压板上方且与压紧驱动机构的输出端传动连接,加载力值传感器安装于上压板与压紧驱动机构的输出端之间,高度探规安装在上压板上,且探头向下伸出上压板下端面,框架为“C”字形一体式刚性结构,其设有上下两个水平板,以及位于一侧的竖直板;本实用新型能够避免机器人自动上样时碰撞到框架,以及下压时高度探规压到试样。
电工钢边缘降控制研究
以马鞍山钢铁集团公司电工钢板形优化控制研究项目为背景,系统地研究了热轧、冷连轧和单机架轧机在电工钢生产过程中的边缘降控制问题。通过现场数据采集、工况数值模拟计算和工业化大生产试验,设计出适用、合理的电工钢板形控制的辊型优化曲线,满足了不同工序、不同机型的板形控制策略要求,解决了电工钢板形质量问题,取得了显著的经济效益。 Based on the project of electric steel strip shape optimization control,problem of edge drop control was systematically studied in production of electric steel of hot-rolling mill,cold-rolling mill and single stand mill.Roll optimization contour was designed out in point and reasonable by collection of work condition data,numerical simulation and test of industrial production.The shape control system can meet with the different working steps and difference mills,and quality problem of electric s...