对CSP流程生产的高磁感无取向电工钢50W1300在偏离轧制方向不同角度处的磁性能进行了测试和分析。结果表明:在偏离轧向不同角度处,磁性能差异显著,尤其在α=60°时磁感最低;偏离轧制方向不同角度处的磁性能大小取决于织构类型、强度及分布状态;增强{100}<0vw>和α、η取向的有利织构组分,降低不利的γ取向织构组分,且使有利织构组分分布越漫散,磁各向异性越小。 Magnetic properties of high magnetic induction non-oriented electrical steel 50W1300 produced by CSP processes were investigated with different direction in relation to the rolling direction.The result shows that magnetic properties are significantly different in relation to the rolling direction,in particular,the minimum magnetic induction occurs at 60° in relation to the rolling direction.Magnetic properties of different directions in relation to rolling direction depend on type and distributi... 
2011-04-28 193 5.8

【作者】 王磊; ...
2014-06-28 161 5.8

【作者】 卢鹏; ...
2014-03-28 146 5.8

对高牌号无取向电工钢国内生产情况、工艺技术、产品性能及应用领域等进行了阐述,并探讨了高牌号无取向电工钢产品的发展趋势。 This paper introduces basic facts on the production status,process technology and products’ properties and their applications of non-oriented electrical steel with high grade at home,and then discusses the development trend on technology for producing the non-oriented electrical steel with high grade. 
2011-02-28 183 5.8

介绍了CSP工艺生产无取向电工钢各工序的设备特点、采用的工艺控制手段和电工钢产品质量情况,结合生产实践证明了马钢CSP工艺开发的无取向电工钢产品丰富了薄板坯连铸连轧的品种结构,发挥了薄板坯连铸连轧生产无取向电工钢性能均一、稳定的特点。 The equipment characteristic,the process control method and the quality of non-orientated silicon steel by CSP process were introduced.Combined with the production situation,it is proved that production of non-orientated silicon steel developed on Masteel CSP line would enrich product structure of thin slab continuous casting and rolling,and it exerts stable performance of non-orientated silicon steel. 
2013-06-28 199 5.8

对冷轧无取向硅钢在冶炼过程中各个工序的顶渣进行了检测,分析了顶渣变化原因,并得出结论:硅钢生产宜采用复吹转炉,以降低吹炼终点渣中TFe含量,进而减轻对精炼的压力;使用低S、低Al2O3含量中间包覆盖剂;RH脱氧及合金化顺序采用先加硅铁后加铝;首罐宜经LF提温并降低渣中TFe。 The top-surface slag used for the various production processes in smelting coldrolled non-oriented electrical steel is tested and based on tested results the cause of the top surface slag change is analyzed.So it is concluded that the combined blown converter is more suitable to be used for smelting electrical steel in order to reduce the content of TFe in slag at blow end point and then much better results can be achieved during the period of refining.Secondly the tundish flux contenting low co... 
2013-03-28 183 5.8

本发明提供一种改善表面麻点缺陷的薄规格中低牌号无取向硅钢及其生产方法,成分C≤0.0025%,1.2≤Si≤1.65%,0.25%≤Mn≤0.35%,0.06%≤P≤0.11%,0.1%≤Als≤0.2%,S≤0.0025%、N≤0.0025%,Ti≤0.0025%,其余为Fe及不可避免的杂质。与现有技术相比,本发明采用较低氢气浓度,防止炉内氧化铁皮还原,减轻碳套辊的腐蚀程度,减少碳套辊结瘤率,改善带钢表面质量;采用合理合金成分设计,提高带钢的力学强度,降低碳套辊结瘤对带钢表面的影响程度,改善带钢表面质量。产品厚度为0.35mm,板面麻点发生率降低,无手感,且辊身周长周期范围内麻点个数≤5个。
2021-10-14 188 6.8

为了消除硅钢在连续退火机组产生的浪形缺陷,对浪形缺陷产生的主要原因进行了分析。制定了相应控制措施,对炉内带钢张力、冷却段输出、碳套辊与带钢的同步性、无氧化炉燃烧状态等参数进行了调整;在生产组织上安排高低牌号宽窄规格穿插生产、定期更换碳套辊等,实施后效果明显。 The main cause leading to waviness defects of silicon steel is analyzed in order to eliminate the waviness defects of silicon steel in continuous annealing line.And thus corresponding measures for controlling these defects are made by means of adjusting these parameters such as the tension of silicon steel coils in continuous annealing furnace,the output in cooling section and the combusting condition of the non-oxidation furnace as well as keeping the synchronization between carbon sleeved roll... 
2013-03-28 171 5.8

取向硅钢热轧板中组织、织构梯度对发展完善的二次再结晶十分关键,通过对2种不同热轧工艺生产取向硅钢的组织、织构进行研究,结果表明:采用后道次大压下热轧工艺时热轧板表层再结区晶粒平均尺寸增加,再结晶区厚度增加,高温退火后二次晶粒尺寸减小;采用后道次大压下热轧工艺热轧时,热轧板中平均等效应变高,热轧板厚度心部{100}〈011〉和{100}〈001〉位向取向强度降低,({111}~{113})〈110〉位向取向强度提高,高温退火后{110}〈001〉位向偏离角降低,磁性能提高。 The texture and microstructure gradient in hot rolled grain oriented silicon steel strip was one of the essential factors to achieve a perfect secondary recrystallization.The texture and microstructure of grain oriented silicon steel strip as-rolled with two different hot rolling parameters was investigated.The results show that with big reduction at the end rolling process,the intensity of {100}〈011〉 and {100}〈001〉 orientation reduces with({111}-{113})〈110〉 orientation intensity enhanced in hot... 
2012-12-28 183 5.8

针对马钢无取向电工钢孔洞缺陷的分布规律及形貌特征,对缺陷样进行了显微分析,并利用生产实绩数据分析了该缺陷产生的原因。结合热轧生产过程,主要通过避免带钢撞击导卫以及降低导卫结瘤的产生等措施,可有效抑制热卷异物压入产生,从而降低冷轧工序孔洞的产生。 In viewing of the distribution and morphology characteristics of the hole defect of non-oriented electrical steel in Maanshan Iron and Steel Co.,Ltd.,the causes of the defect were analyzed by micro analysis of the defect sample and the production data.Combined with the production process of hot rolling,by avoiding the impact of strip steel on the guide and reducing the nodule formation on the guide,the pressing of foreign bodies in hot coiling could be effectively suppressed,thus reducing the fo... 
2022-01-28 192 5.8

本发明涉及一种含磷高磁感无取向硅钢的生产方法,工艺路线:铁水脱硫-转炉冶炼-RH精炼-连铸-热轧-酸洗-冷轧-连续炉退火-涂层-性能检验-包装,具体步骤包括:1)将钢水冶炼至目标成分后采用连铸方式将钢水铸成坯;2)热轧板坯加热炉均热段板坯温度950~1050℃,终轧温度控制在780~830℃,卷取温度600~680℃;3)酸洗后冷轧,控制冷轧整体压下率80%以上,至成品厚度,增加剪切带组织;4)连续退火炉快速加热段温度设定1000~1150℃,增加有利织构组织形核;均热段温度设定750~830℃,全氮气干气氛保护,退火工艺速度110~150m/min,满足晶粒度8~4级。本发明在减少硅、铝、锰合金添加量的情况下,改善铁损提高磁感性能,提高机械性能。
2021-08-19 190 6.8

本发明涉及一种常化后免酸洗生产取向硅钢的方法,取向硅钢的生产工艺路线为:冶炼→连铸→热轧→常化退火→拉伸矫直→抛丸→冷轧→脱碳退火→渗氮→涂MgO→高温退火→热拉伸平整及涂绝缘膜;本发明在常化退火后通过物理方法去除带钢表面的氧化铁皮,且效率高、效果好、操作简单、易于控制;与常规工艺相比,省去了酸洗及后续废酸处理工作,排除了酸雾对环境的污染,消除了取向硅钢带因酸洗而产生的潜在缺陷,产品质量更加稳定可靠。
2021-02-09 172 6.8