利用DSC、XRD,结合热焓分析对硅钢级氧化镁和二氧化硅的固相反应行为进行了研究。比较了不同二氧化硅原料及混合方法对硅钢级氧化镁反应性的影响,找到了一种更为有效的硅钢级氧化镁反应性的评估方法,克服了传统柠檬酸活性法在比较不同厂家生产的氧化镁的反应性上的局限性。进一步研究了Na2B4O7添加剂、TiO2添加剂对氧化镁和二氧化硅反应行为的影响,结果表明,Na2B4O7添加剂含量的增加对反应有利,而TiO2添加剂对反应有阻碍作用。 The solid-state reaction behavior between silicon-steel grade MgO and SiO2 was investigated by DSC and XRD combined with enthalpimetric analysis.The influence of different kinds of SiO2 and different preparation methods were studied and a specifical measurement that is more reliable was proposed to evaluate reactivity of silicon steel grade MgO.It overcomes the limitation of the traditional citric acid activity(CAA) method,which can not be used to evaluate the reactivity of... 
2014-03-28 206 5.8

采用RH精炼添加钙合金方式对硅钢进行钙处理。结果表明,钙合金添加量为0.67、1.00、1.67kg/t钢时,钢中钙含量分别为0、2×10-6、4×10-6;随着钙合金添加量增大,钢中夹杂物粒度逐渐由0~2μm向2~4、4~6μm偏移;不同钙处理条件下,钢中均存在粒径小于1μm和粒径为1~5μm的MnS、CuxS夹杂物,后者或单独存在,或同AlN、CaS夹杂复合;粒径为5~10μm区间,钢中的夹杂物基本以钙的氧、硫化物为主。与钙处理前相比,钙合金添加量为0.67、1.00、1.67kg/t钢时,粒径小于1.0μm的微细夹杂物减少幅度分别为68.06%、87.50%、94.94%。钙合金添加量为1.67kg/t钢时,可以去除钢中绝大部分的微细夹杂物。 Ca alloy was added into the liquid steel during RH refining,and the results show that Ca concentration in final Si steel sheets is insignificant,about 0,2×10-6 and 4×10-6 when the added amount of Ca is 0.67,1.00 and 1.67 kg/t steel,respectively.With the increase in the added Ca alloy amount,the inclusions in the steel gradually change from those of 0~2 μm to those of 2~4 and 4~6 μm.Under different Ca treatments,there exist MnS and CuxS inclusions whose size is below 1 μm as well as MnS and CuxS ... 
2013-02-28 344 5.8

本发明公开了一种基于硅钢服役特性的立体卷铁心单框损耗测量方法及系统,根据硅钢片在立体卷铁心中的服役特性,获得测量铁心单框所需的非正弦励磁电压波形,通过所述立体卷铁心的心柱绕组电压和单框绕组电压之间的关系,确定所述被测立体卷铁心单框所需的电压有效值,再通过计算机、数据采集卡D/A转换器、功率放大器、隔离变压器和示波器,直接在所述立体卷铁心单框上加载励磁电压,利用功率表测量立体卷铁心单框损耗。本发明利用硅钢的服役特性,获得测量立体卷铁心单框所需的非正弦励磁电压波形和电压有效值,再将励磁电压直接加载到被测立体卷铁心单框,测量立体卷单框铁心损耗。
2021-08-31 236 6.8

采用电解法和扫描电镜研究了300 t转炉-RH精炼钙处理对无取向硅钢板(%:≤0.005C、1.2~2.2Si、0.2~0.6Mn、≤0.20P、≤0.005S、0.2~0.6Al、0~0.01Ca)中夹杂物的影响。结果表明,钢中Al含量为0.25%和0.35%时,钢中溶解氧均小于1×10-4%,钙处理后都会产生CaS夹杂物,尤其是含0.35%Al的钢水;钙处理可以有效减少钢中的夹杂物数量,尤其是0.5μm以下的微细夹杂物数量;钙处理后夹杂物的种类以AlN、CaS为主,同时还含有少量的氧化物夹杂物以及AlN-CaS复合夹杂物,尺寸主要为1.5~5.0μm。 The effect of 300 t converter-RH refining calcium treatment on inclusions in non-oriented silicon steel sheet (%:≤0.005C,1.2~2.2Si,0.2~0.6Mn,≤0.20P,≤0.005S,0.2~0.6A1,0~0.01Ca) has been studied by electrolysis and scanning electron microscope.Results show that with 0.25%and 0.35%Al content in steel,all the dissolved oxygen in liquid is less than 1×10-4%,and the CaS inclusions are produced after calcium treatment,especial for the liquid containing 0.35%Al;the amount of inclusions in ste... 
2011-01-28 425 5.8

对碳-锰-硅钢进行不同配分温度的Q&P(Quenching and Partitioning)处理,测试了热处理后不同钢的力学性能和残余奥氏体含量,并用扫描电子显微镜和透射电镜观察其显微组织,分析了配分温度对显微组织和力学性能的影响。结果表明:试验钢显微组织基本由低碳板条状马氏体、块状铁素体和条状残余奥氏体组成;随配分温度的升高,试验钢的抗拉强度呈下降趋势,伸长率与奥氏体含量的变化趋势相同,但变化规律不确定;提高锰含量能稳定残余奥氏体,从而提高试验钢的伸长率,并使伸长率对配分温度不敏感。 The C-Mn-Si steel was quenched and partitioned at different partitioning temperatures,the mechanical properties and residual austenite contents were investigated,the microstructure was observed by SEM and TEM,and the effect of partitioning temperature on microstructure and mechanical properties was analyzed.The results show that the microstructure of the tested steel consisted of lath martensite with low carbon,nubby ferrite and banded residual austenite.The tensile strength of the tested steel ... 
2011-09-28 351 5.8

选用国内外无取向硅钢标杆企业A、B、C的产品,采用非水溶液电解提取+SEM(EDS)方法,分析了其典型牌号对应成品试样中的夹杂物。结果表明,从磁性能控制角度而言,受钢的化学成分及生产工艺影响,A、B、C企业成品试样的夹杂物尺寸、种类、数量存在差异,这些差异对其磁性能产生显著影响;从夹杂物控制角度而言,A、B、C企业对应成品试样的夹杂物,以MnS、CuxS复合或者AlN、MnS、CuxS复合为主,其中1.0μm以下的夹杂物数量分别为2.34×107个/mm3、2.98×107个/mm3和11.98×107个/mm3,1.0μm以上夹杂物数量均很少,夹杂物的平均尺寸从大到小依次为A企业、B企业、C企业。 According to the production of three benchmarking manufacture enterprises A,B and C of non-oriented silicon steel at home and abroad,the inclusions in finished steel samples with typical grades were investigated by electrolytic extraction from non-aqueous solution and SEM(EDS).Results show that,from the viewpoint of improving the magnetic properties,affected by chemical composition and production technique,the size,type and amount of inclusions in finished steel samples are various,which will af... 
2013-01-28 278 5.8

结合工业化生产的50A1300牌号无取向硅钢,分析了化学成分、RH精炼脱氧方式、板坯装炉温度以及热轧平整工艺等对磁性能的影响,探讨成品钢磁性能的改善。结果表明,采取改善后,50A1300牌号无取向硅钢的磁性能得到明显改善。2012年,该钢种平均铁损、磁感应强度分别达到5.26 W/kg、1.762 T,能够较好地满足用户市场需求及同行对标需要。 Based on the industrial manufacture of 50A1300 grade non-oriented silicon steel sheets,effects of chemical composition,deoxidization method in RH vacuum refining,charging temperature of steel slabs,hot rolling and flattening progress on magnetic properties are analyzed.The optimization methods of magnetic properties of steels are discussed. Results show that the magnetic properties are obviously improved by the adopted measures above. In 2012,the average core loss and the magnetic induction of 5... 
2014-02-28 262 5.8

结合工业化生产的高效硅钢,进行了RH精炼稀土处理试验研究。针对不同的稀土处理条件,观察了夹杂物的形貌和尺寸分布,探讨了稀土处理后钢中的夹杂物形成、变化规律。结果表明:试验条件下,最佳的稀土合金添加数量为0.6~0.9 kg/t。经过合适的稀土处理后,可以有效抑制尺寸相对较小的、不规则的AlN、MnS复合夹杂生成,促进钢中微细夹杂物的聚合、上浮,钢质纯净度得到明显提高。此时,钢中全氧含量最低,脱硫效果最佳,钢中的夹杂物主要是尺寸相对较大的、近似球形或者椭球形的稀土类夹杂。 Based on the industrial production of non-oriented silicon steel,the experiment on RE treatment during the RH refining process was studied.The morphology and the size distribution were observed for the steel specimens treated with different RE treatment conditions.Further more,the formation and change of inclusions of final steel sheets after RE treatment were discussed.The results show that the suitable RE added amount was 0.6~0.9 kg/t.After the suitable RE treatment,the formation of AlN and Mn... 
2011-03-28 240 5.8

借助高温激光共聚焦显微镜,在线观察了不同Mn含量的无取向硅钢中夹杂物的尺寸、类型、数量变化。结果表明,Mn含量(质量分数)为0.77%、0.32%时,试样中的夹杂物数量分别约为1000万个/mm3、1600万个/mm3。Mn含量较高的钢种,会优先析出球形、椭球形MnS夹杂物,其析出数量较少,尺寸相对较大,可以有效抑制AlN、CuxS夹杂物析出;Mn含量较低的钢种,会在试样再加热后冷却过程中,先析出相当数量MnS夹杂物,并作为AlN夹杂物析出核心,形成MnS+AlN复合夹杂物。这种复合夹杂物数量较多,尺寸也较大。 Based on the high temperature confocal microscope, the chage of size, type, and quantity of inclusions in non-oriented silicon steels with different Mn content were observed by in-situ SEM. Results show that the inclusion quantities are 10 million per mm3 and 16 million per mm3,while the mass fractions of Mn are 0.77% and 0.32%, respectively. In the silicon steel with higher Mn content, the spherical and ellipsoidal MnS inclusion will precipitate first, which can retard the precipitation of AlN ... 
2014-05-28 204 5.8

本发明一种铝镇静含硅钢的脱氧方法,包括转炉冶炼、LF炉精炼工序,转炉工序:转炉出钢过程采用含硅脱氧剂进行脱氧,出钢完毕后,向钢液表面加入顶渣改质剂,数量为400±25kg/炉,所述顶渣改质剂的成分及其质量百分含量为:Al2O3:9%±1%,CaO:27.5%±1.5%,SiO2:3%±1%,Al:50%±2%,CaF2:7%±1%。精炼工序:采用铝脱氧剂进行脱氧、造渣。本发明通过两步脱氧工艺,大幅降低脱氧成本同时提高钢水质量,由于硅脱氧相对于铝脱氧在钢水中形成的夹杂物更容易上浮,所以也提高了钢水纯净度,提高钢水质量。
2021-04-07 238 6.8

本发明公开了一种免常化中间退火的无取向电工钢板,其各化学元素质量百分含量为:0<C≤0.004%、Si:1.0~2.6%、Mn:0.2~1.0%、Al:0.2~1.6%、Ca:0.0003%~0.0035%,余量为Fe和其他不可避免的杂质。此外本发明还公开了上述无取向电工钢板的制造方法,其包括步骤:(1)冶炼和连铸,其中在该步骤不采用电磁搅拌;(2)热轧,其包括:粗轧、精轧、卷取和保温;其中控制粗轧之后、精轧之前的中间坯温度≥950℃;(3)上述热轧步骤后不进行常化中间退火或罩式炉中间退火而直接进行冷轧;(4)连续退火。本发明所述的无取向电工钢板通过采用合理的化学成分和工艺设计,可以在保证较低生产成本的同时,获得高磁感和低铁损的特性。
2021-04-09 398 6.8

聚焦无取向硅钢产品标准,从电磁性能、表面性能、机械性能以及尺寸公差与边部质量等维度对国际标准IEC、EN、JIS、ASTM以及国标GB进行了分析研究。分析得出,各类标准在电磁性能方面要求基本一致;ASTM标准的机械性能要求有别于其他几个标准。 In this paper,non-oriented silicon steel standards of EN,JIS,GB and ASTM were compared and analyzed. It is showed that,all types of standards in electromagnetic performance requirements are basically the same. Surface properties in ASTM standard are expressed in the most detailed. The mechanical properties requirements of the standards,except for ASTM,are basically the same. 
2014-02-28 220 5.8