结合工业化生产的无取向硅钢,进行了RH精炼喂CaSi线去除钢中的非金属夹杂物试验研究。针对不同的钙处理条件,分析了CaS夹杂生成热力学,观察了夹杂物的形貌和尺寸分布,确定了夹杂物的类型、数量,探讨了钙处理后钢中夹杂物的变化规律。结果表明,本试验条件下,钙处理可以有效抑制MnS、AlN夹杂物的生成,有效促进钢中微细夹杂物的聚合、上浮、去除,钢质纯净度明显提高。经过合适的钙处理后,钢中的夹杂物以独立存在的CaO为主,同时有少量含CaO、SiO2、MgO的复合夹杂,没有发现CaS夹杂存在。这部分夹杂物的尺寸集中分布在2~20μm,数量约为1.8×105个/mm3。 Experimental study on removal of non-metallic inclusions in non-oriented silicon steel obtained from industrial production by CaSi wire feeding during RH refining process was carried out.The thermodynamics of CaS inclusion formation was analyzed,the morphology and the size distribution of inclusions were observed,and the numbers and types of inclusions were also determined for the steel specimens treated under different calcium treatment conditions.Furthermore,the variation of inclusion characte... 
2013-01-28 509 5.8

采用电解法和扫描电镜研究了300 t转炉-RH精炼钙处理对无取向硅钢板(%:≤0.005C、1.2~2.2Si、0.2~0.6Mn、≤0.20P、≤0.005S、0.2~0.6Al、0~0.01Ca)中夹杂物的影响。结果表明,钢中Al含量为0.25%和0.35%时,钢中溶解氧均小于1×10-4%,钙处理后都会产生CaS夹杂物,尤其是含0.35%Al的钢水;钙处理可以有效减少钢中的夹杂物数量,尤其是0.5μm以下的微细夹杂物数量;钙处理后夹杂物的种类以AlN、CaS为主,同时还含有少量的氧化物夹杂物以及AlN-CaS复合夹杂物,尺寸主要为1.5~5.0μm。 The effect of 300 t converter-RH refining calcium treatment on inclusions in non-oriented silicon steel sheet (%:≤0.005C,1.2~2.2Si,0.2~0.6Mn,≤0.20P,≤0.005S,0.2~0.6A1,0~0.01Ca) has been studied by electrolysis and scanning electron microscope.Results show that with 0.25%and 0.35%Al content in steel,all the dissolved oxygen in liquid is less than 1×10-4%,and the CaS inclusions are produced after calcium treatment,especial for the liquid containing 0.35%Al;the amount of inclusions in ste... 
2011-01-28 424 5.8

为了弄清楚高硫硅钢中的硫化物析出行为及其对钢的微观组织和电磁性能的影响,以便为工业化生产制定更为合理的硫含量控制标准和采取更为有效措施减轻炼钢生产的硫含量控制压力,结合0.25% Si 无取向硅钢 ,采用非水溶液电解提取 + 扫描电镜/透射电镜观察相结合的方法 ,研究了0.006 8%、0.010 2%、0.025 5% 和 0.035 3% 硫含量条件下,钢中的硫化物夹杂物组成和存在形式及其形貌、种类、尺寸、数量变化,以及相应的热轧、成品试样的微观组织和电磁性能变化。结果表明,随着钢中硫含量的增加,钢中的硫化物逐渐由 MnS→MnS+Cu2S→Cu2S转变,数量逐渐增多,尺寸向高低两个方向发展。相应地,导致热轧再结晶组织劣化和抑制了成品晶粒尺寸长大。随着钢中硫含量的增加,钢的磁感、铁损劣化程度逐渐增大。钢中的硫含量平均每增加 0.01%,涡流损耗、磁滞损耗分别劣化0.24 W/kg 和 0.41 W/kg,而磁感会劣化 0.009 T。但是 ,在硫含量为 0.010 2% 时 ,铁损可以低于 6.0W/kg,而在硫含量为 0.025 5% ... In order to find out the precipitation behavior of sulfide inclusions and the corresponding changes of microstructure and electromagnetic properties of high sulfur silicon steel sheets, so that to design more suitable sulfur concentration controlling limit for industrial manufacture and to release the steel-making difficulty effectively, Based on the change of given sulfur concentration 0.006 8%, 0.010 2%0.025 3% and 0.035 3%, the type and composition, the size and number, and the size distribut... 
2022-02-28 238 5.8

本发明公开了一种硅钢产品生产方案的智能设计评估方法,包括以下步骤:1、采集数据,并集成用户数据、实验室研发数据和大生产数据;2、构建用户数据主题、实验室研发数据主题和大生产数据主题;3、输入硅钢产品的种类、规格和性能需求的需求信息,并根据需求信息生成若干个硅钢产品的生产方案,生产方案包括优化产品的生产方案和新产品的生产方案;4、多维度综合评估步骤3中生成的每个硅钢产品的生产方案,得到硅钢产品生产方案的绿色设计指数,并根据绿色设计指数推荐生产方案。本发明基于产品设计需求,融合实验研发数据和大生产数据,生成并评估产品设计方案模型,缩短研发周期,提高研发效率。
2021-07-09 231 6.8

本发明公开了一种免常化中间退火的无取向电工钢板,其各化学元素质量百分含量为:0<C≤0.004%、Si:1.0~2.6%、Mn:0.2~1.0%、Al:0.2~1.6%、Ca:0.0003%~0.0035%,余量为Fe和其他不可避免的杂质。此外本发明还公开了上述无取向电工钢板的制造方法,其包括步骤:(1)冶炼和连铸,其中在该步骤不采用电磁搅拌;(2)热轧,其包括:粗轧、精轧、卷取和保温;其中控制粗轧之后、精轧之前的中间坯温度≥950℃;(3)上述热轧步骤后不进行常化中间退火或罩式炉中间退火而直接进行冷轧;(4)连续退火。本发明所述的无取向电工钢板通过采用合理的化学成分和工艺设计,可以在保证较低生产成本的同时,获得高磁感和低铁损的特性。
2021-04-09 397 6.8

结合工业化生产的无取向硅钢,探讨了氧硫交互作用对钢中夹杂物生成的影响。借助非水溶液电解+扫描电镜法,研究了不同O、S含量下钢中夹杂物的变化规律。结果表明,本实验条件下,提高O含量、降低S含量,会劣化热轧组织再结晶效果。在劣化效果上,O的作用大于S;低Si、无Al硅钢中,应尽可能降低O含量、适当提高S含量,以粗化钢中微细夹杂物,减少尺寸小于1.0μm的夹杂物的数量;O、S含量与钢中夹杂物数量不具有关联性。生产过程中,不仅要严格控制O、S含量,还要严格控制生产工艺,以免生成较多的有害夹杂物。 Based on the industrial production of non-oriented silicon steel,the effects of interaction between oxygen and sulfur on the formation of inclusions were discussed.The change of non-metallic inclusions in steel sheets was investigated by means of electrolysis with non-aqueous solution under different oxygen and sulfur content.Results show that the recrystallization microstructure of hot rolled sheets will be deteriorated with the increase of oxygen content and the decrease of sulfur content.The ... 
2012-04-28 207 5.8

本发明一种铝镇静含硅钢的脱氧方法,包括转炉冶炼、LF炉精炼工序,转炉工序:转炉出钢过程采用含硅脱氧剂进行脱氧,出钢完毕后,向钢液表面加入顶渣改质剂,数量为400±25kg/炉,所述顶渣改质剂的成分及其质量百分含量为:Al2O3:9%±1%,CaO:27.5%±1.5%,SiO2:3%±1%,Al:50%±2%,CaF2:7%±1%。精炼工序:采用铝脱氧剂进行脱氧、造渣。本发明通过两步脱氧工艺,大幅降低脱氧成本同时提高钢水质量,由于硅脱氧相对于铝脱氧在钢水中形成的夹杂物更容易上浮,所以也提高了钢水纯净度,提高钢水质量。
2021-04-07 237 6.8

聚焦无取向硅钢产品标准,从电磁性能、表面性能、机械性能以及尺寸公差与边部质量等维度对国际标准IEC、EN、JIS、ASTM以及国标GB进行了分析研究。分析得出,各类标准在电磁性能方面要求基本一致;ASTM标准的机械性能要求有别于其他几个标准。 In this paper,non-oriented silicon steel standards of EN,JIS,GB and ASTM were compared and analyzed. It is showed that,all types of standards in electromagnetic performance requirements are basically the same. Surface properties in ASTM standard are expressed in the most detailed. The mechanical properties requirements of the standards,except for ASTM,are basically the same. 
2014-02-28 220 5.8

无取向硅钢中夹杂物的存在会抑止晶粒生长,使基体的均匀连续性中断,其在钢中的形态、含量及分布情况都不同程度影响着硅钢的性能,尤其是对磁性能起关键的作用。因此,全尺度分布考察夹杂物对无取向硅钢夹杂物的研究极为重要。本实验确定了适用于不同牌号无取向硅钢夹杂物全尺度分布的分析方法:样品制备—小样电解—过滤喷金—根据不同牌号的要求选择合适的放大倍率扫描观测—夹杂物颗粒的分类统计。通过统计的结果,结合电解的失重量可以得到不同尺度的体积分布数据。实验分析了不同牌号和工艺无取向硅钢夹杂物的种类、形貌、大小和尺度分布,并初步考查了夹杂物与磁性能的关系,对无取向硅钢的工艺研究具有一定参考价值。 Inclusions in non-oriented silica steel could inhibit the growth of grain and cause discontinuity of micro-structure.The configuration,content and size distribution of inclusion have different effects on the performance of silica steel,especially significant on the magnetic property.Therefore,it is very useful to completely characterize inclusions with full size distribution in silica steel.In our research,full size analysis method for inclusion in silica steel had been established as follows: s... 
2012-10-28 220 5.8

本发明公开了一种利用取向硅钢氧化镁废弃物生产镁质球团的方法,采用取向硅钢生产过程中的废氧化镁污泥、废氧化镁粉等氧化镁废弃物,以及粗粒铁矿粉、镜像赤铁矿、磁铁精矿、膨润土和石灰石粉为原料,依次经预处理、配料、造球后,再在链箅机‑回转窑‑环冷机上进行干燥预热、焙烧和冷却,得到镁质球团。本发明利用氧化镁废弃物制备镁质球团,既有利于减少氧化镁废弃物带来的环保压力及其外运时产生的处置费用,也能显著降低镁质球团的制造成本,综合利用了钢铁厂的现有资源,生产出环境友好、低成本的镁质球团,为高炉提供优质原料,最终降低炼铁过程的污染物排放,减少环境污染。
2021-01-15 172 6.8

本发明公开了一种耐热刻痕型取向硅钢涂层用涂液,其溶剂为水,其含有:磷酸盐、胶态二氧化硅、铬酐和乙醇。本发明还公开了一种耐热刻痕型取向硅钢板,其包括基板,所述基板表面具有采用上述的耐热刻痕型取向硅钢涂层用涂液涂覆在基板上而形成的涂层。相应地,本发明还公开了上述取向硅钢板的制造方法,其包括步骤:在基板表面涂覆所述涂液,基板的刻痕沟槽涂液填充率>95%;进行烧结处理,其中烧结处理中的板温为780‑900℃。本发明的耐热刻痕型取向硅钢涂层用涂液具有良好的流动性,其可以涂覆于耐热刻痕取向硅钢基板的表面中,涂覆后,能有效填充基板的刻痕沟槽,且可以在其表面形成涂层,保证耐热刻痕取向硅钢在具有低铁损的同时具备更高的安全性。
2021-09-24 241 6.8