选用国内外无取向硅钢标杆企业A、B、C的产品,采用非水溶液电解提取+SEM(EDS)方法,分析了其典型牌号对应成品试样中的夹杂物。结果表明,从磁性能控制角度而言,受钢的化学成分及生产工艺影响,A、B、C企业成品试样的夹杂物尺寸、种类、数量存在差异,这些差异对其磁性能产生显著影响;从夹杂物控制角度而言,A、B、C企业对应成品试样的夹杂物,以MnS、CuxS复合或者AlN、MnS、CuxS复合为主,其中1.0μm以下的夹杂物数量分别为2.34×107个/mm3、2.98×107个/mm3和11.98×107个/mm3,1.0μm以上夹杂物数量均很少,夹杂物的平均尺寸从大到小依次为A企业、B企业、C企业。 According to the production of three benchmarking manufacture enterprises A,B and C of non-oriented silicon steel at home and abroad,the inclusions in finished steel samples with typical grades were investigated by electrolytic extraction from non-aqueous solution and SEM(EDS).Results show that,from the viewpoint of improving the magnetic properties,affected by chemical composition and production technique,the size,type and amount of inclusions in finished steel samples are various,which will af... 
2013-01-28 278 5.8

研究表明,硅钢中的夹杂物对成品带钢的磁性能有显著影响。为研究冶炼过程硅钢中的夹杂物遗传变化,进而提出更有效的控制措施加以去除,本文结合典型的无取向硅钢生产炉次,采用非水溶液电解提取+扫描电镜观察方法分析冶炼过程中上述炉次典型试样的夹杂物。结果表明:转炉冶炼结束、RH精炼开始时,钢的氧化物夹杂总量最大,约为0.23%;RH精炼过程中,氧化物夹杂总量不断降低,并在脱碳结束时达到最低,约为0.02%;连铸过程中,氧化物夹杂总量仍有不断降低趋势,但夹杂物的平均尺寸变化不大。本试验条件下,中间包试样的夹杂物数量约为1.59×104个/mm3。 As we all know, the non-metallic inclusion effects magnetic properties of silicon steel sheets obviously. The article aims to study the heredity of non-metallic inclusion in non-oriented silicon steels during the steel making process, and then provides a more effective controlling measure to remove the inclusions. Based on the typical non-oriented silicon steel charges, the non-aqueous solution extraction and SEM observation were adopted to analyze the non-metallic inclusions. Results show that,... 
2014-05-28 306 5.8

结合工业化生产的无取向硅钢,进行了RH精炼添加稀土合金实验。结果表明,1.15%(质量分数)Si钢的脱硫反应,主要发生在添加稀土合金之后的前5min。最佳的稀土合金添加量为0.6~0.9kg/t钢。钢液经过稀土处理后,加入的稀土总量越多,稀土氧硫化物夹杂物的尺寸就越大,但热轧带钢再结晶效果会逐渐变差,成品带钢晶粒尺寸先是快速长大,而后逐渐减小。最佳的钢中存留稀土含量与钢的化学成分有关,应严格控制在2.0×10-3%~6.0×10-3%(质量分数)。在此范围内,钢的铁损先是快速降低,而后缓慢升高,钢的磁感应强度则单调降低。 Based on the industrial production of non-oriented electrical steel,rare earth(RE) alloy treatment during the RH refining process was studied.The results showed that the effects of desulfurization and total concentration of RE remained in steel mainly depended on the chemical compositions of different steel grades.For 1.15wt% Si steel grade,the desulfurization reaction mainly focused on the initial 5min after RE alloy added during the RH refining process.The suitable RE alloy addition was 0.6-0.... 
2013-07-28 291 5.8

针对宝钢硅钢常化退火过程中产生的退火炉辊印缺陷问题,通过实际生产的大数据与产品质量问题相结合,将数据挖掘、数据分析方法应用到实际,一定程度上解决了现场实际生产中的痛点,为现场生产提供决策支撑,避免了以前通过人工识别判定存在疏漏和无法定量判断的问题,形成了一套具有鲁棒性和可操作性的钢铁生产过程数据分析方法。通过智慧决策系统平台获取实际生产和表检仪数据,基于Pearson相关系数算法进行变量挑选和特征工程,并应用随机森林算法对数据建立分类预测模型,实现了质量问题的溯源和监控,通过数据量化预测了炉辊印缺陷是否可通过轧制消除的质量问题,识别准确率达到96.43%。 In views of the normalizing annealing furnace roll marks problem occurred in the process of normalizing annealing of silicon steel in Baosteel,by combining big data from actual production with product quality problems,data mining and data analysis methods were applied to actual production to solve the pain points and provide decision support,a robust and practical data analysis method for the steel production process has been developed,which avoided the previous problems of omission and non-quan... 
2022-01-28 257 5.8

借助高温激光共聚焦显微镜,在线观察了不同Mn含量的无取向硅钢中夹杂物的尺寸、类型、数量变化。结果表明,Mn含量(质量分数)为0.77%、0.32%时,试样中的夹杂物数量分别约为1000万个/mm3、1600万个/mm3。Mn含量较高的钢种,会优先析出球形、椭球形MnS夹杂物,其析出数量较少,尺寸相对较大,可以有效抑制AlN、CuxS夹杂物析出;Mn含量较低的钢种,会在试样再加热后冷却过程中,先析出相当数量MnS夹杂物,并作为AlN夹杂物析出核心,形成MnS+AlN复合夹杂物。这种复合夹杂物数量较多,尺寸也较大。 Based on the high temperature confocal microscope, the chage of size, type, and quantity of inclusions in non-oriented silicon steels with different Mn content were observed by in-situ SEM. Results show that the inclusion quantities are 10 million per mm3 and 16 million per mm3,while the mass fractions of Mn are 0.77% and 0.32%, respectively. In the silicon steel with higher Mn content, the spherical and ellipsoidal MnS inclusion will precipitate first, which can retard the precipitation of AlN ... 
2014-05-28 204 5.8

对碳-锰-硅钢进行不同配分温度的Q&P(Quenching and Partitioning)处理,测试了热处理后不同钢的力学性能和残余奥氏体含量,并用扫描电子显微镜和透射电镜观察其显微组织,分析了配分温度对显微组织和力学性能的影响。结果表明:试验钢显微组织基本由低碳板条状马氏体、块状铁素体和条状残余奥氏体组成;随配分温度的升高,试验钢的抗拉强度呈下降趋势,伸长率与奥氏体含量的变化趋势相同,但变化规律不确定;提高锰含量能稳定残余奥氏体,从而提高试验钢的伸长率,并使伸长率对配分温度不敏感。 The C-Mn-Si steel was quenched and partitioned at different partitioning temperatures,the mechanical properties and residual austenite contents were investigated,the microstructure was observed by SEM and TEM,and the effect of partitioning temperature on microstructure and mechanical properties was analyzed.The results show that the microstructure of the tested steel consisted of lath martensite with low carbon,nubby ferrite and banded residual austenite.The tensile strength of the tested steel ... 
2011-09-28 350 5.8

一种基于大数据分析技术的电工钢用户选材询单推荐方法,于终端计算机内、以可与终端计算机各数据库进行信息交互的形式、设置一计算模块;经此计算模块完成依次的基于各数据库的有效信息的采集、用户询单选材推荐方案模型的设置、基于有效信息及推荐方案模型完成推荐牌号的生成,根据设定的评估模型对生成的推荐牌号及信息评估运算的运行,据此建立对用户的选材询单推荐。本发明的一种基于大数据分析技术的电工钢用户选材询单推荐方法,基于L4计算机系统开发出的计算模块及相应的可与计算模块进行信息交互的用户界面完成,形成可根据不同用户需求对应的不同评价体系,完成与不同用户需求适配的方案推荐。
2021-07-23 247 6.8

本发明涉及一种高压电机用无取向硅钢50SBW600的制备方法,包括,S1,将装有精炼钢水的钢包运至回转台,回转台转到浇铸位置后,将钢水注入中间包;S2,中间包通过水口将所述钢水分配至若干个结晶器中,所述结晶器中设置有浸入式水口,S3,钢水在结晶器内生成晶核,结晶器将带有晶核的钢水下放至通道;S4,通道上设有第二电磁搅拌器,第二电磁搅拌器对通道内钢水进行电磁搅拌,所述钢水在通道中逐步转换为钢坯;S5,拉矫辊将的所述钢坯拉出通道并对钢坯进行形态矫正;S6,切断装置所述钢坯进行切割。本发明通过在无取向硅钢50SBW600制备过程中设置双电磁搅拌装置,充分保证连铸过程中钢坯中的等轴晶数量,保障了产品表面缺陷质量。
2021-04-13 284 6.8

采用RH精炼添加钙合金方式对硅钢进行钙处理。结果表明,钙合金添加量为0.67、1.00、1.67kg/t钢时,钢中钙含量分别为0、2×10-6、4×10-6;随着钙合金添加量增大,钢中夹杂物粒度逐渐由0~2μm向2~4、4~6μm偏移;不同钙处理条件下,钢中均存在粒径小于1μm和粒径为1~5μm的MnS、CuxS夹杂物,后者或单独存在,或同AlN、CaS夹杂复合;粒径为5~10μm区间,钢中的夹杂物基本以钙的氧、硫化物为主。与钙处理前相比,钙合金添加量为0.67、1.00、1.67kg/t钢时,粒径小于1.0μm的微细夹杂物减少幅度分别为68.06%、87.50%、94.94%。钙合金添加量为1.67kg/t钢时,可以去除钢中绝大部分的微细夹杂物。 Ca alloy was added into the liquid steel during RH refining,and the results show that Ca concentration in final Si steel sheets is insignificant,about 0,2×10-6 and 4×10-6 when the added amount of Ca is 0.67,1.00 and 1.67 kg/t steel,respectively.With the increase in the added Ca alloy amount,the inclusions in the steel gradually change from those of 0~2 μm to those of 2~4 and 4~6 μm.Under different Ca treatments,there exist MnS and CuxS inclusions whose size is below 1 μm as well as MnS and CuxS ... 
2013-02-28 344 5.8

试验的铸态取向硅钢(/%:0.0440.056C,3.123.32Si,0.080.11Mn,0.0020.008S,0.002 90.029 1Als,0.006 20.010 9N)由30 kg高频真空感应炉熔炼。通过场发射扫描电子显微镜/能谱仪(FE-SEM/EDS)研究结果表明,0.002 9%Als钢中氧化物主要为SiO2,存在片状、棒状及近似球状的独立MnS,未发现含铝的氧化物或氮化物;0.0090%Als钢中出现以Al2O3为主的复合氧化夹杂物,存在MnS与AlN的复合析出物。钢中Als增加,复合析出物多呈簇状发展。氧化物容易成为MnS-AlN复合析出的核心,钢中Als含量越低,夹杂物中的MnS含量越高;作为核心的氧化物夹杂的尺寸越小,形成的复合夹杂物的形状越规则,尺寸也越小。热力学计算结果表明,钢中Als含量主要影响了钢中氧化物夹杂的组成和AlN的析出温度及析出量。 Test as-cast grain-oriented silicon steel(/%:0.044 0.056C,3.12 3.32Si,0.08 0.11Mn,0.0020.008S,0.002 90.029 1 Als,0.006 20.010 9N) is melted by a 30 kg high frequency vacuum induction furnace.The research results by using field emission-scanning electron microscope/energy dispersive spectrometer(FE-SEM/EDS) show that in 0.002 9%Als steel the main oxide is SiO2,and there is independent laminable,rod-like and approximate ... 
2014-02-28 342 5.8

一种生产取向硅钢的氧化镁涂层烘烤质量控制方法,通过对带钢的实时温度测量建立对烘烤输出功率的实时反馈调节,据此形成基于烘烤输出功率的烘烤质量的实时控制。本发明的一种生产取向硅钢的氧化镁涂层烘烤质量控制方法,通过在烘烤炉出口的带钢上方增加一套可在带钢横向方向移动的在线板温计,基于在线板温检测值对烘烤炉状态进行监控,并建立烘烤输出功率控制系统实时调整,使得氧化镁涂层烘烤质量均匀,提高取向硅钢产品质量稳定性,节省能源消耗。
2021-07-27 218 6.8

本发明公开了一种用于无取向硅钢清洗液的洁净度检测分析方法,包括以下步骤:步骤1:从清洗液循环槽中取含有污物的清洗液样品,并进行脱水、烘干、研磨,得到污物粉末样品;步骤2:根据含有污物的清洗液样品和污物粉末样品计算清洗液循环槽中清洗液的洁净度;步骤3:根据含有污物的清洗液样品的洁净度建立清洗液洁净度评定标准;步骤4:根据清洗液洁净度评定标准控制含有污物的清洗液的排放和换液。本发明能简便且直观的了解当前清洗段循环槽内清洗液的状态,并可以根据清洗液的洁净度评级对清洗液的使用和排放做出及时的在线调整。