钢厂
配分温度对碳-锰-硅钢显微组织与力学性能的影响
对碳-锰-硅钢进行不同配分温度的Q&P(Quenching and Partitioning)处理,测试了热处理后不同钢的力学性能和残余奥氏体含量,并用扫描电子显微镜和透射电镜观察其显微组织,分析了配分温度对显微组织和力学性能的影响。结果表明:试验钢显微组织基本由低碳板条状马氏体、块状铁素体和条状残余奥氏体组成;随配分温度的升高,试验钢的抗拉强度呈下降趋势,伸长率与奥氏体含量的变化趋势相同,但变化规律不确定;提高锰含量能稳定残余奥氏体,从而提高试验钢的伸长率,并使伸长率对配分温度不敏感。 The C-Mn-Si steel was quenched and partitioned at different partitioning temperatures,the mechanical properties and residual austenite contents were investigated,the microstructure was observed by SEM and TEM,and the effect of partitioning temperature on microstructure and mechanical properties was analyzed.The results show that the microstructure of the tested steel consisted of lath martensite with low carbon,nubby ferrite and banded residual austenite.The tensile strength of the tested steel ...
CN202110555870.5一种电化学评价取向硅钢氧化层的装置及方法
本发明公开了一种电化学评价取向硅钢氧化层的装置及方法,包括电解池、设于电解池一侧的磁铁组、设于电解池上的饱和甘汞电极和铂电极以及与电解池连接的电化学工作站;磁铁组包括固定在电解池上的固定磁铁和与固定磁铁磁性连接的移动磁铁,移动磁铁设于电解池侧面的出口上;参比电极设于磁铁组与辅助电极之间;参比电极和辅助电极与电化学工作站连接。本发明的评价方法通过电化学测量取向硅钢试样的电位‑时间曲线,计算出取向硅钢氧化层各分层的溶解电量,实现了对取向硅钢氧化层各分层的快速、准确测定,可以区分出Mg2SiO4玻璃膜底层、SiN层、SiO2层、FeO及铁橄榄石层等分层性能,为取向硅钢生产工艺参数的控制提供指导。
稀土处理无取向硅钢中夹杂物的控制
结合工业化生产的高效硅钢,进行了RH精炼稀土处理试验研究。针对不同的稀土处理条件,观察了夹杂物的形貌和尺寸分布,探讨了稀土处理后钢中的夹杂物形成、变化规律。结果表明:试验条件下,最佳的稀土合金添加数量为0.6~0.9 kg/t。经过合适的稀土处理后,可以有效抑制尺寸相对较小的、不规则的AlN、MnS复合夹杂生成,促进钢中微细夹杂物的聚合、上浮,钢质纯净度得到明显提高。此时,钢中全氧含量最低,脱硫效果最佳,钢中的夹杂物主要是尺寸相对较大的、近似球形或者椭球形的稀土类夹杂。 Based on the industrial production of non-oriented silicon steel,the experiment on RE treatment during the RH refining process was studied.The morphology and the size distribution were observed for the steel specimens treated with different RE treatment conditions.Further more,the formation and change of inclusions of final steel sheets after RE treatment were discussed.The results show that the suitable RE added amount was 0.6~0.9 kg/t.After the suitable RE treatment,the formation of AlN and Mn...
CN202110778749.9硅钢产品生产方案的智能设计评估方法
本发明公开了一种硅钢产品生产方案的智能设计评估方法,包括以下步骤:1、采集数据,并集成用户数据、实验室研发数据和大生产数据;2、构建用户数据主题、实验室研发数据主题和大生产数据主题;3、输入硅钢产品的种类、规格和性能需求的需求信息,并根据需求信息生成若干个硅钢产品的生产方案,生产方案包括优化产品的生产方案和新产品的生产方案;4、多维度综合评估步骤3中生成的每个硅钢产品的生产方案,得到硅钢产品生产方案的绿色设计指数,并根据绿色设计指数推荐生产方案。本发明基于产品设计需求,融合实验研发数据和大生产数据,生成并评估产品设计方案模型,缩短研发周期,提高研发效率。
无取向硅钢冶炼过程中的夹杂物遗传变化
研究表明,硅钢中的夹杂物对成品带钢的磁性能有显著影响。为研究冶炼过程硅钢中的夹杂物遗传变化,进而提出更有效的控制措施加以去除,本文结合典型的无取向硅钢生产炉次,采用非水溶液电解提取+扫描电镜观察方法分析冶炼过程中上述炉次典型试样的夹杂物。结果表明:转炉冶炼结束、RH精炼开始时,钢的氧化物夹杂总量最大,约为0.23%;RH精炼过程中,氧化物夹杂总量不断降低,并在脱碳结束时达到最低,约为0.02%;连铸过程中,氧化物夹杂总量仍有不断降低趋势,但夹杂物的平均尺寸变化不大。本试验条件下,中间包试样的夹杂物数量约为1.59×104个/mm3。 As we all know, the non-metallic inclusion effects magnetic properties of silicon steel sheets obviously. The article aims to study the heredity of non-metallic inclusion in non-oriented silicon steels during the steel making process, and then provides a more effective controlling measure to remove the inclusions. Based on the typical non-oriented silicon steel charges, the non-aqueous solution extraction and SEM observation were adopted to analyze the non-metallic inclusions. Results show that,...
钙合金处理硅钢中的夹杂物及晶粒成长变化
采用RH精炼添加钙合金方式对硅钢进行钙处理,结果表明,钙合金添加量为0.67、1.00和1.67 kg/t钢时,钢中Ca含量分别为0、2×10-6和4×10-(6质量分数);随着钙合金添加量的增加,钢中夹杂物粒度逐渐由0~2μm向2~4μm、4~6μm偏移;不同钙处理条件下,钢中均存在粒径小于1μm和粒径为1~5μm的MnS、CuxS夹杂物,后者或单独存在,或与AlN、CaS夹杂复合;钢中粒径为5~10μm的夹杂物基本以Ca的氧化物和硫化物为主。与未经钙处理的炉次相比,钙合金添加量为0.67、1.00和1.67 kg/t钢时,粒径小于1.0μm的夹杂物减少幅度分别为68.06%、87.50%和94.94%。钙合金添加量为1.67 kg/t钢时,可以去除钢中绝大部分的微细夹杂物。 In order to improve the properties of final silicon steels,the calcium treatment was adopted by adding Ca alloys into the liquid steel during the RH refining process.Results show that when the addition of Ca alloys is 0.67 kg/t,1.00 kg/t and 1.67 kg/t,the corresponding Ca content in silicon steels is 0,2 × 10-6 and 4 × 10-6 respectively.With the increase of Ca alloy addition,the particle sizes of inclusions in steels become 2~4 μm and 4~6 μm,from 0~2 μm.Under different calcium treatments,there e...
国内外中低牌号无取向硅钢夹杂物控制效果解析
选用国内外无取向硅钢标杆企业A、B、C的产品,采用非水溶液电解提取+SEM(EDS)方法,分析了其典型牌号对应成品试样中的夹杂物。结果表明,从磁性能控制角度而言,受钢的化学成分及生产工艺影响,A、B、C企业成品试样的夹杂物尺寸、种类、数量存在差异,这些差异对其磁性能产生显著影响;从夹杂物控制角度而言,A、B、C企业对应成品试样的夹杂物,以MnS、CuxS复合或者AlN、MnS、CuxS复合为主,其中1.0μm以下的夹杂物数量分别为2.34×107个/mm3、2.98×107个/mm3和11.98×107个/mm3,1.0μm以上夹杂物数量均很少,夹杂物的平均尺寸从大到小依次为A企业、B企业、C企业。 According to the production of three benchmarking manufacture enterprises A,B and C of non-oriented silicon steel at home and abroad,the inclusions in finished steel samples with typical grades were investigated by electrolytic extraction from non-aqueous solution and SEM(EDS).Results show that,from the viewpoint of improving the magnetic properties,affected by chemical composition and production technique,the size,type and amount of inclusions in finished steel samples are various,which will af...
CN202110837023.8一种基于大数据分析技术的电工钢用户选材询单推荐方法
一种基于大数据分析技术的电工钢用户选材询单推荐方法,于终端计算机内、以可与终端计算机各数据库进行信息交互的形式、设置一计算模块;经此计算模块完成依次的基于各数据库的有效信息的采集、用户询单选材推荐方案模型的设置、基于有效信息及推荐方案模型完成推荐牌号的生成,根据设定的评估模型对生成的推荐牌号及信息评估运算的运行,据此建立对用户的选材询单推荐。本发明的一种基于大数据分析技术的电工钢用户选材询单推荐方法,基于L4计算机系统开发出的计算模块及相应的可与计算模块进行信息交互的用户界面完成,形成可根据不同用户需求对应的不同评价体系,完成与不同用户需求适配的方案推荐。
CN202110933882.7一种取向硅钢产品的在线性能判级与精确分切装置和方法
本发明公开了一种取向硅钢产品的在线性能判级与精确分切装置和方法,使得同一个分卷上的性能分布均匀,避免分卷出现性能废品或多个性能等级的情况,提高分卷性能稳定性。提供的一种取向硅钢产品的在线性能判级与精准分切方法包括生产数据采集、铁损曲线自学习、数据存储、性能在线判级、缺陷数据采集、缺陷判级、智能分切等模块,依据修正后的磁性能全长数据,得到产品的性能判级结果,结合表面缺陷判级结果,综合确定分切位置,制定最佳分切方案。本发明可以实现取向硅钢生产过程中的性能在线判级和精准分切,得到性能均匀、表面质量好的分卷,减少分卷性能不稳定带来的损失。
CN202111121077.0一种耐热刻痕型取向硅钢涂层用涂液、取向硅钢板及其制造方法
本发明公开了一种耐热刻痕型取向硅钢涂层用涂液,其溶剂为水,其含有:磷酸盐、胶态二氧化硅、铬酐和乙醇。本发明还公开了一种耐热刻痕型取向硅钢板,其包括基板,所述基板表面具有采用上述的耐热刻痕型取向硅钢涂层用涂液涂覆在基板上而形成的涂层。相应地,本发明还公开了上述取向硅钢板的制造方法,其包括步骤:在基板表面涂覆所述涂液,基板的刻痕沟槽涂液填充率>95%;进行烧结处理,其中烧结处理中的板温为780‑900℃。本发明的耐热刻痕型取向硅钢涂层用涂液具有良好的流动性,其可以涂覆于耐热刻痕取向硅钢基板的表面中,涂覆后,能有效填充基板的刻痕沟槽,且可以在其表面形成涂层,保证耐热刻痕取向硅钢在具有低铁损的同时具备更高的安全性。
硅钢水溶性极厚绝缘涂层的热老化行为研究
对两种硅钢水溶性极厚绝缘涂层进行了不同温度的热老化实验。通过TG-DTA,GDS,FT-IR,SEM和光泽度仪等测试方法对老化的涂层进行分析表征,提出了评估硅钢水溶性极厚绝缘涂层热老化性能的合理温度区间,探讨了涂层热老化行为,并分析了两种涂层热老化性能的差异。结果表明,涂层附着性随着老化时间的延长逐渐下降。FT-IR表征结果显示,热老化过程中,涂料交联形成的化学键未发生断裂,交联剂氨基树脂的三嗪环被破坏是聚合物三维网络结构坍塌的主要原因。 Thermal aging expriments at different temperature were carried out on two types of water-soluble and extra-thick insulation coatings for non-oriented silicon steel,and a series of test methods such as glossmeters,TG-DTA,FT-IR,GDS,SEM were applied in analysis.For evaluating the thermal aging effect of this kind of insulation coating,the proper temperature range was proposed.The difference of aging performance between two coatings was been investigated and the related behaviors were been discussed...
CN202111215913.1一种高磁感取向硅钢及其制造方法
本发明公开了一种高磁感取向硅钢,其含有Fe及不可避免的杂质元素,其还含有质量百分含量如下的下述各化学元素:C:0.02~0.08%,Si:2.0~4.5%,Mn:0.02~0.30%,S≤0.0050%,Als:0.01~0.04%,N:0.002~0.01%,Nb:0.0050~0.0600%;以及P:0.01~0.1%,Sn:0.01~0.30%,Cu:0.01~0.50%的至少其中一种。此外,本发明还公开了上述高磁感取向硅钢的制造方法,其包括步骤:(1)制得板坯;(2)板坯加热;(3)热轧,其包括:粗轧、在热卷箱内卷取保温,以及精轧;其中粗轧结束温度高于970℃;卷取温度为800~1050℃,卷取时间为30~200s;精轧开始温度低于1050℃;(4)冷轧;(5)脱碳退火;(6)渗氮;(7)涂覆退火隔离剂;(8)高温退火;(9)涂覆绝缘涂层和激光刻痕。