钢厂
CN202023343140.9硅钢绝缘涂层液循环罐
本实用新型涉及具有搅拌器的装置领域。尤其涉及硅钢绝缘涂层液循环罐,包括罐体,罐体的顶部设有进液口,罐体的侧壁上设有出液口,罐体上端设有盖板,罐体的盖板上设有涡轮室,罐体与涡轮室上贯穿有竖直的中空轴,涡轮室的顶部设有热水口,涡轮室内设有涡轮叶片,涡轮叶片固定在中空轴上,涡轮叶片与罐体上端之间的中空轴上贯穿有流水口,中空轴上设有若干侧管,侧管位于罐体内,所述侧管的两端与中空轴连通,中空轴的内侧封堵有隔板,侧管的两端分别位于隔板的上侧与下侧,中空轴与罐本体以及中空轴与上空腔的结合部均设有密封圈。从而本实用新型可实现对硅钢绝缘涂层液进行均匀加热。
电工钢冶炼过程中硫含量控制
介绍了攀钢冶炼电工钢过程硫含量变化以及过程回硫、增硫情况,采取针对性措施,如:提高铁水装入量、转炉采用石英砂代替复合造渣剂造渣、RH脱硫等,降低钢中硫含量。结果表明:采取相应措施后,电工钢炼成率大幅提高,成品w[S]≤0.008%的比例由改进前的62%提高到92.4%,取得了明显的冶金效果。 The resulfurization and the change of sulphur content in production of electrical steel is analyzed.The targeted measures have been taken,such as increase the loaded quantity of liquid iron,quartz sand replaces the composite slagging agent in the converter and RH desulfurization to decrease the sulphur content of the steel.The result shows,after the measures have been taken,the finished product ratio of electrical steel increase a lot.The ratio of sulfur content of finished product no more than ...
双辊连铸无取向硅钢铸带特征及常化作用研究
双辊连铸技术是冶金及材料领域内的一项前沿技术,对于生产高品质硅钢具有独特优势.本实验研究了一种双辊铸轧w[Si]=4.5%的无取向硅钢,考察其铸态和常化处理后样品的组织、织构及析出相尺寸特征.结果表明:铸带组织以与铸带法向成5~20(°)倾角的柱状晶为主,晶内存在少量0.3~0.4μm的AlN析出相,铸带织构以λ(<001>//ND)织构为主,表层织构漫散.950℃/10 min常化处理后,析出相尺寸增大,表层λ织构增强. As an advanced technique of metallurgy and material science,twin- roll strip casting has unique advantages for producing high quality silicon steel. The present study was aimed at a 4. 5% Si non- oriented electrical steel for analyzing the structure,texture and the size of precipitates at the initial and normalized state. The results revealed that the initial structure mainly consisted of columnar grains with 5 ~ 20( °) angle to the normal of cast strip,and some AlN precipitates of 0. 3 ~ 0. 4 μ...
CN202111237550.1硅钢片组扣件自动压平装置
本发明公开了一种硅钢片组扣件自动压平装置,包括:定位单元,定位单元包括转盘、校位板和第一驱动组件,第一驱动组件连接并驱动校位板沿竖直方向运动,校位板滑动连接有第一校位柱,第一校位柱相对转盘偏心布置;第一推送单元,位于转盘的一侧,第一推送单元包括第一推送气缸和第一推块,第一推送气缸连接并驱动第一推块沿水平方向运动;冲压单元,位于转盘背离第一推送气缸的一侧,冲压单元包括第二驱动组件和冲压柱,第二驱动组件连接并驱动冲压柱沿竖直方向运动。转盘、校位柱和第一驱动组件配合,周向定位硅钢片组,再通过冲压柱将凸出于硅钢片组的扣件压平,完成硅钢片组的整形,整体更为美观,方便后续的装配使用。
CN202110569430.5一种提高取向硅钢冷轧加工性的生产方法
本发明涉及一种提高取向硅钢冷轧加工性的生产方法,工艺流程为:冶炼、连铸、热轧、常化、酸洗、冷轧、脱碳渗氮、涂MgO、高温退火、涂绝缘层及热拉伸平整;粗轧中坯厚度35‑45mm,两段常化后进行带钢横向分段式冷却水分布。本发明通过对热轧中坯厚度、终轧温度及卷取温度,常化冷却水量及控制方式的调控,使轧前表层晶粒尺寸降低5‑10μm、珠光体体积分数降低6%,轧材冷轧加工性明显改善、成材率可提高8%以上。通过后续冷轧、脱碳退火和高温退火等工序处理,可保证完善的二次再结晶组织及良好磁性能。
双辊薄带连铸3.98%Si-0.71%Al无取向硅钢的组织、织构和磁性能
采用双辊薄带连铸工艺制备了厚度为2.4mm的3.98%Si-0.71%Al无取向硅钢带,经常化、冷轧、不同温度退火后,对其显微组织、析出物、织构和磁性能进行了检测分析。结果表明:随着退火温度的提高,退火板晶粒尺寸增大,组织均匀性提高;退火板析出物主要是AlN和MnS与AlN复合析出物,尺寸较粗大,达0.5~2.5μm;退火板织构沿厚度方向变化明显,表层和1/2层存在较强的{100}织构,1/2层还存在较强的{111}织构,1/4层主要是{112}织构;随退火温度的升高相应的铁损和磁感应强度均降低。 Using twin roll thin strip continuous casting technique,the 3.98%Si-0.71%Al no-oriented silicon steel strip in thickness of 2.4mm was produced.The microstructure,precipitates,texture,and magnetic properties of the sheet after normalizing,cold rolling and annealing at different temperatures were studied.The results show that with annealing temperature increase,the grain size and uniformity of annealed sheet increased.The main precipitates in coarse size of 0.5-2.5μm in annealed sheet were AlN and...
CN202111176370.7高磁感低铁损硅钢极薄带的生产方法
本发明提供一种高磁感低铁损硅钢极薄带的生产方法,包括:对硅钢极薄带进行清洗,并对清洗后的所述硅钢极薄带进行烘干;对烘干后的硅钢极薄带进行涂覆隔离层;将涂覆有所述隔离层的硅钢极薄带进行高温退火处理,其中,高温退火过程包括:快速升温至300~600℃,慢速升温至800~1300℃,并在预设温度时进行保温,保温至预设时间后进行冷却,冷却至50~300℃;对退火处理后的硅钢极薄带进行表面清洗、干燥以及涂覆绝缘层;将涂敷绝缘涂层的硅钢极薄带进行烘干烧结处理,并卷取成品。利用本发明,解决目前硅钢极薄带在连续退火涂层工艺存中存在张力不易控制,而导致硅钢带材的板形变差且极易发生断带等问题。
CN202122693326.5一种电工钢切片用清洁设备
本实用新型涉及电工钢加工技术领域,尤其涉及一种电工钢切片用清洁设备,其包括箱体、第一盒体、烘干装置、清洁组件、进水管和出水管;箱体后侧内壁上转动设置导向辊;第一盒体前侧面上设置第二盒体;烘干装置设置在箱体内壁上;第一转动轴转动设置在第一盒体前后内壁上;刷辊设置在第一转动轴上,刷辊上的刷毛与电工钢钢带表面接触;清洁组件设置两组;第二盒体内设置有带动第一转动轴转动且沿第一转动轴轴线方向来回运动的动力组件;两组进水管出水口位于第一盒体上方且朝向电工钢钢带表面;出水管竖直设置在箱体底部。本实用新型中,刷辊转动的同时沿第一转动轴轴线方向来回做往复运动,不存在清洁间隙,提高了清洁效果。
CN202120300684.2一种用于硅钢片叠装的工装
本实用新型公开了一种用于硅钢片叠装的工装,包括安装底座,所述安装底座上设置有限位装置,所述限位装置包括多个水平限位柱和多个竖直限位柱;各个水平限位柱之间的缝隙的尺寸等于其对应放置的硅钢片的宽度,各个竖直限位柱与安装底座的底边之间的距离等于其对应放置的硅钢片的总长度;所述各个竖直限位柱设置在各个水平限位柱之间的缝隙所正对的位置;采用多个水平限位柱和多个竖直限位柱进行水平和竖直方向上均对硅钢片进行定位;使用此工装叠装出来的成品,长短一致,侧面相当整齐;本实用新型,结构简单,操作方便。
CN202110667000.7一种用于风力发电机定子铁芯扇形硅钢片的保护工装
本发明公开了一种用于风力发电机定子铁芯扇形硅钢片的保护工装,包括第一防护罩和第二防护罩,第一防护罩、第二防护罩均为扇形罩体,其由弧形底板和两个扇形侧板构成,第一防护罩的两端连接有能够折叠收纳的柔性罩;第一防护罩滑动套设在扇形硅钢的外侧,第二防护罩滑动套设在第一防护罩的外侧。本发明提供的保护工装主要有两个功能,当扇形硅钢片处于运输过程中时,利用第一防护罩、第二防护罩、柔性罩协同配合为其防刮伤防护;当扇形硅钢片装配后,利用第一防护罩内部的冷却散热系统提供散热防护,防止出现高温过热现象;通过这种方式,本发明保护工装满足大规格定子铁芯扇形硅钢片的防护需求。
CN202023178253.8一种电工钢自粘涂层液生产用搅拌釜
本实用新型公开了一种电工钢自粘涂层液生产用搅拌釜,包括釜体,釜体的内部通过两个第一隔板分隔成第一安装腔、第二安装腔和搅拌腔,釜体的内部设有传动组件,传动组件包括伺服电机、主动轴和两个从动轴,伺服电机固定安装在釜体顶端的中部,伺服电机的输出轴与主动轴的顶端固定连接,本实用新型的有益效果是:通过设有八个与十二个搅拌叶片相交错的挡板,避免搅拌轴在搅拌过程中产生离心力造成漩涡,使自粘内外侧的涂层液得到充分搅拌,通过设有循环泵机、第二隔板和流通槽使搅拌釜内的自粘涂层液处于流通的状态,使底部不易被搅拌的涂层液能够得到充分搅拌,在提高搅拌釜的灵活性的同时,保留其原有的稳定性。