钢厂
硅钢车间ST机组粉尘调质与除尘系统改造
针对某硅钢车间ST机组的除尘系统除尘效率较低、排放浓度不达标、二次污染较严重的问题,通过现场调研,对除尘系统、含尘气体组分与物性参数等进行测试和分析,运用管道伴热技术改善粉尘黏性后,再选取合适的除尘器对粉尘进行除尘处理,大大地提高了系统的除尘效率。 To solve the problems of low dust removal efficiency, substandard emission concentration and severe secondary pollution, some investigations are conducted to test and analyze the dust removal system,dust-gas composition and relevant physical parameters.Moreover, dust removal efficiency is greatly improved by the use of pipe heat tracing technology and by choosing appropriate dust remover.
基于爱泼斯坦方圈组合和损耗加权处理技术的取向电工钢磁性能扩展模拟
提出了一种基于爱泼斯坦方圈族(包括标准25cm爱泼斯坦方圈、缩比的17.5cm和20cm爱泼斯坦方圈)和二级加权处理方法对爱泼斯坦测试数据,包括有效磁路长度、比损耗、励磁功率,进行处理的晶粒取向电工钢磁性能扩展模拟方法。详细地考察了励磁频率、试样剪切角度和环境温度对爱泼斯坦方圈测量结果的影响。研究结果表明,利用本文提出的爱泼斯坦方圈组合以及二级加权处理技术,可以有效地建立取向电工钢损耗模拟模型,从而更加准确地确定了取向电工钢的损耗,改善并提高了爱泼斯坦磁性能测试数据的应用价值。 The extended modeling of the magnetic properties of GO(grain oriented) electrical steel is presented in this paper which is based on a set of standard and scaled-down Epstein frames and a proposed two-level weighted processing of Epstein data, including the mean magnetic path length, specific magnetization loss and exciting power. The effects of excitation frequency, strip angle and ambient temperature on the results obtained from the Epstein frames are investigated. It is shown that using the p...
退火工艺对3.15%Si冷轧无取向硅钢组织和织构的影响
试验研究了退火温度(850~950℃)和时间(5~18 min)对2.3 mm热轧硅钢板(/%:0.036C,3.15Si,0.21Mn,0.005P,0.007S,0.032A1)6道次轧制的0.35 mm冷轧板组织和织构的影响。结果表明,退火温度越高,晶粒平均尺寸越大,900℃5 min退火时平均晶粒尺寸41.39μm,试样织构主要集中在γ取向线上的{111}<112>织构组分和{111}<110>织构组分;900℃18 min退火时平均晶粒尺寸为48.08μm,试样的{111}面织构和{112}面织构密度都明显减弱,{001}面织构增强,磁性能较优。 The effect of annealing temperature(850 ~950 ℃) and holding time(5 ~ 18 min) on structure and texture of 0.35 mm sheet by 6 passes cold-rolling from 2.3 mm hot-rolled plate of silicon steel(/%:0.036 C,3.15 Si,0.21 Mn,0.005 P,0.007 S,0.032A1) has been tested and studied.Results show that the higher the annealing temperature the coarser the average grain size;As annealing at 900 ℃ for 5 min the average grain size of steel sheet is 41.39 μm,and the texture in sample is mainly concentrated in y orie...
制备硅钢级氧化镁前驱体的原料水化研究
以青海盐湖水氯镁石为初级原料,采用喷雾热解法制备原料氧化镁,原料氧化镁通过水化制备硅钢级氧化镁前驱体氢氧化镁。原料氧化镁水化实验中对水化剂、水化温度、水化时间、液固比、搅拌速度及陈化时间对水化率、过滤速度和纯度的影响进行系统研究。采用均匀实验设计和DPS数据处理,(依次)通过建模分析、二次多项式模型回归建立数学模型,再通过各因素方差分析和总方差分析,确定了理论最优实验条件,再用理论最优条件作重复实验进行验证,最终确定了原料氧化镁的最佳水化条件。在水化温度60℃,水化时间105 min,液固比4,陈化时间4 h,水化剂1含量4.0%,水化剂2含量3.15%,洗水量4倍,搅拌速度120 r/min时,原料氧化镁的水化率达99.50%以上,得到的硅钢级氧化镁前驱体氢氧化镁纯度高、过滤性能良好。 By spray pyrolysis method,bischofite in Qinghai salt Lake,as primary raw material,was used to prepare precursor raw material MgO for silicon-steel MgO.The precursor raw material MgO was used for preparing Mg(OH)2 which was the precursor of silicon-steel MgO,by hydration method.In the hydration experiment of precursor raw material MgO,some experiment parameters were investigated systematically.such as the hydrated agent,the temperature and time of hydration,liquid/solid ratio that affected the hy...
获得抑制剂法生产低温高磁感取向硅钢的抑制剂控制研究进展
综述了国内外大钢铁企业与研究机构采用获得抑制剂法生产低温高磁感取向硅钢的开发及应用情况,分析了以该法生产高磁感取向硅钢过程中抑制剂的控制技术,包括固有抑制剂组成方案、气态渗氮方式与工艺及高温退火工艺的制定.研究表明,固有抑制剂组成方案的设计思路大体一致,化合物抑制剂以AlN为主、硫化物为辅,同时添加少量Sn,Sb等单元素抑制剂,但组成元素含量存在一定差别;在脱碳退火后用NH3进行非平衡渗氮处理已成为气态渗氮的主要方式,但最佳方式仍未明确,具体选择需依据实际生产条件,相应脱碳及渗氮工艺的控制条件差别较大;高温退火工艺中升温制度差别不大,升温阶段退火气氛中N2含量的选择存在差别.此外,分析了抑制剂控制技术目前存在的关键问题,并指出了进一步的研究方向. The current application and exploitation on production of low-temperature high magnetic induction grain-oriented silicon steel with acquired inhibitor method at both iron and steel enterprises and research institutions in the world are reviewed. The control techniques of inhibitors, which include the composition design for inherent inhibitors, nitriding method and process, and secondary recrystallization annealing, are thoroughly analyzed and proposed. It is indicated that the design ideas for i...
ICP-AES法测定硅钢中铌的不确定度评定
分析了电感耦合等离子体发射光谱法(ICP-AES)测定硅钢中铌的检测过程,讨论了该检测过程中不确定度的主要来源,建立了该方法的定量的数学模型,并根据这一模型计算出了检测结果的合成标准不确定度和扩展不确定度。 The measurement of niobium content in silicon steel by inductively coupled plasma atomic emission spectrometry(ICP-AES) was analyzed,by which the main factors affecting the uncertainty of the measurement were ascertained and the calculation formula was given.Finally,according to the formula the combined uncertainty and expanded uncertainty were obtained.
CN202111244946.9一种减少低温高磁感取向硅钢点状露金缺陷的方法
本发明公开了一种减少低温高磁感取向硅钢点状露金缺陷的方法。本发明通过控制低温高磁感取向硅钢的脱碳和渗氮工艺,特别是通过控制脱碳露点、渗氮露点、脱碳氧化度、脱碳时间来调节钢板经脱碳渗氮后表面形成的内氧化层中FeO/SiO2的比例,结合氧化镁退火隔离剂的含水率控制,获得了一种可避免点状露金缺陷的低温高磁感取向硅钢生产方法。
CN202110396796.7一种高压电机用无取向硅钢50SBW600的制备方法
本发明涉及一种高压电机用无取向硅钢50SBW600的制备方法,包括,S1,将装有精炼钢水的钢包运至回转台,回转台转到浇铸位置后,将钢水注入中间包;S2,中间包通过水口将所述钢水分配至若干个结晶器中,所述结晶器中设置有浸入式水口,S3,钢水在结晶器内生成晶核,结晶器将带有晶核的钢水下放至通道;S4,通道上设有第二电磁搅拌器,第二电磁搅拌器对通道内钢水进行电磁搅拌,所述钢水在通道中逐步转换为钢坯;S5,拉矫辊将的所述钢坯拉出通道并对钢坯进行形态矫正;S6,切断装置所述钢坯进行切割。本发明通过在无取向硅钢50SBW600制备过程中设置双电磁搅拌装置,充分保证连铸过程中钢坯中的等轴晶数量,保障了产品表面缺陷质量。
CN202120638252.2无取向硅钢蠕变性能测试装置
本实用新型涉及一种无取向硅钢蠕变性能测试装置,包括基座,基座的顶部和侧面设有开口;试样夹持装置,试样夹持装置安装在基座的顶部,用于夹持硅钢蠕变试样;转换力杆,转换力杆安装在基座的侧面,与试样夹持装置连接;可调节式砝码盘,可调节式砝码盘安装在转换力杆上,可调节式砝码盘上能够放置不同重量的砝码,转换力杆将砝码的重力转换成水平力,以实现对硅钢蠕变试样不同应力水平的加载;可调节式灯座,设置在试验腔内并与基座的侧面插接;加热装置,放置到可调节式灯座上,用于给硅钢蠕变试样加热。本实用新型具有解决无法实现不同应力和温度下硅钢材料的蠕变研究的问题的效果。
CN202023271514.0一种镀铝锌硅钢板平整装置
本实用新型公开了一种镀铝锌硅钢板平整装置,包括辊轮整形装置与曲面压平装置,所述辊轮整形装置包括第二底板,所述第二底板的上表面固定连接有两个驱动电机,所述驱动电机的输出端固定连接有第二推杆,所述第二推杆的输出端固定连接有滑动块,所述滑动块的左侧壁转动连接有转杆,所述转杆的中部固定连接有辊轮;所述曲面压平装置包括第一底板、顶板,所述第一底板与顶板之间固定连接有四根导柱,所述导柱的中部滑动连接有上模座,所述上模座的下表面可拆卸连接有上模具,所述第一底板的上表面固定连接有下模座,所述下模座的上表面可拆卸连接有下模具。本实用新型中,辊轮整形机与曲面压平机结合能够有效地提高钢板的压平后的平整度。
CN202123075500.6一种硅钢前处理高液回流装置
本实用新型属于硅钢技术领域,具体的说是一种硅钢前处理高液回流装置,包括机体;所述机体的侧端固接有一号导管;所述一号导管上安装有二号导管;所述机体的顶端固接有连接管;所述连接管上安装有入泡管;所述二号导管的内侧壁固接有电机;所述电机的输出端固接有扇叶;所述二号导管的顶端内侧壁固接有定位板;所述定位板的侧端转动连接有旋转叶轮;所述二号导管的底端固接有排泡管;通过一号导管和二号导管的配合可以把溢出的泡沫进行导向,通过扇叶和旋转叶轮的配合可以使泡沫快速流动,再通过排泡管排出进入机体的内部,可以使泡沫循环使用,避免泡沫的溢流造成环境的污染及碱液的浪费。
硅钢脱硫影响因素分析研究
对RH法(真空循环脱气法)生产的冷轧硅钢的脱硫原理及影响因素进行了分析研究。研究表明:降低顶渣中FeO、MnO的含量,提高钢液温度,增加脱硫剂的加入量并延长其循环时间有利于提高脱硫效率。 The principles of desulfurization and its influence factors of cold rolling silicon steel during RH process have been studied in this paper.The result indicated that reducing contents of FeO and MnO,rising temperature of the liquid steel,increasing quantity of desulfurizer,lengthening cycle time of desulfurzer are benefit for desulfurization.