本实用新型公开了一种硅钢片焊接模具,包括底座,底座上均匀排布有多条滑槽,每条滑槽内连接有一根垂直设置的定位杆,定位杆底部穿过底座连接一气缸,气缸连接在底座底部。本实用新型结构设计合理巧妙,移动不同位置的定位杆,将定位杆与硅钢片贴合,不同滑槽内的定位杆之间相互错位,并利用气缸将硅钢片定位,这种结构不可以适用于各种形状的硅钢片,使用方便快捷。
2020-12-28 178 6.8

分析了影响脱碳效果和结晶行为的各种要素及其相互制约关系,提出了Hi-B连续退火工艺曲线,总结得出快速加热及合理稳态气氛是实现工艺制度的关键。结合实际工程,介绍了在连续退火炉设计中快速加热和气氛设计的考虑方法,并指出随着Hi-B产品的发展,如何改进这些方法将是连退工程研发的方向之一。 The factors which affect decarbonization and crystallization and the mutual restriction between them were analyzed.A complete continuous annealing process for Hi-B was put forward.As a result,the rapid heating and the proper steady atmosphere were two important factors.According to an actual project,the consider methods for designing rapid heating and proper steady atmosphere were introduced,and it is pointed that with the development of Hi-B technique,how to improve these techniques would be on... 
2011-02-28 178 5.8

本实用新型公开了一种变压器铁芯硅钢片纵剪滚切装置,包括纵剪机本体、弹性压覆机构和涂油机构,所述纵剪机本体的进料端设置有弹性压覆机构,料带通过弹性压覆机构压覆在纵剪机本体的支撑平台上,所述支撑平台上凹设有安装凹槽,所述安装凹槽内设置有涂油机构,所述涂油机构朝向于料带的底面涂油,通过涂油机构对板材的切割面进行涂油,能够对料带起到润滑和冷却的作用,提升料带切割质量。
2021-12-13 177 6.8

研究了冷轧95%变形量无取向硅钢不同退火温度(710~1 050℃)下再结晶织构特征.再结晶刚完成时(710℃退火),呈现强γ({111<112>~<134>)与弱{114}<481>织构特征;随退火温度升高至900℃,γ明显减弱,{114}<481>组分持续增强,形成典型的{h,1,1}<1/h,1,2>织构;进一步升温至1 050℃,再结晶织构不再发生明显变化.基于EBSD分析,{114}<481>组分的持续强化可归因于其明显的尺寸优势以及较高频率的高能晶界(取向差角为20°~45°). A non-oriented silicon steel was heavily rolled to 95% reduction and subsequently annealed at 710~1 050 ℃ to investigate recrystallization texture evolution.When annealed at 710 ℃ with complete recrystallization,the texture is characterized by a strong partial γ fiber spreading from {111}<112> to {111}<134> and a weak {114}<481> component.As annealing at 900 ℃,γ fiber is decreased significantly while {114}<481> is increased consistently,producing a typical {h,1,1}<1/h,... 
2013-05-28 177 5.8

选取了三种50W 800无取向电工钢,分析了化学成分、晶粒尺寸、织构、以及200℃时效处理48 h前后的磁性能和第二相粒子析出状态的变化。结果表明,钢板中第二相粒子的分布密度对钢板铁损有最重要的影响。降低钢中C、N元素含量,或改进钢板热加工参数以降低成品钢板中第二相粒子形成元素的过饱和度均有利于明显降低钢板磁时效过程中的铁损增幅。钢板中对磁性能有利的织构也有利于降低钢板铁损的时效幅度。 The evolution of chemical composition,grain size,texture,as well as magnetic property after aging treatment at 200 ℃ for 48 h and distribution of second phase particles precipitation in three selected 50W800 non-oriented electrical steels were analyzed.The results show that the distribution density of second phase particles has great influence on core loss.Reducing C and N content,or improving hot-working parameters to reduce the supersaturation of elements forming second phase particles in prod... 
2011-08-28 177 5.8

利用EBSD技术研究了电工钢中长轴平行于轧向的柱状晶样品在热轧和退火过程中组织和取向的演变规律,并与长轴平行于板法向的样品的已有研究结果进行对比。结果表明,无论柱状晶按何种方向排列,只要表面存在剪切力,热轧后都可形成剪切织构,同时中心形成轧制织构,主要包括旋转立方织构和{112}<1-10>。柱状晶造成的影响主要体现在板中心层,长轴平行于轧向排列的样品热轧时形成的粗大旋转立方晶粒要到脱碳退火后才能完全消除,但破坏了正常的不同取向晶粒间的取向差分布及尺寸均匀性,导致二次再结晶不完全及磁性能降低。 The evolution of microstructure and grain orientation in an electrical steel containing columnar grains with its long axis being parallel to the rolling direction of sheet was studied during hot rolling and annealing by EBSD technique.The results are compared with those of samples containing columnar grains being parallel to normal direction of sheet reported in the reference [3].It was shown that,whether the long axis of columnar grains was arranged in RD or ND,shear textures can be formed in t... 
2011-02-28 177 5.8

本发明属于硅钢制造技术领域,具体涉及一种改善硅钢热轧板边部质量的加工方法,包括:连铸、铸坯预变形处理、铸坯加热处理和热轧处理;其中,所述铸坯预变形处理包括:在所述铸坯的温度为500~900℃下,对所述铸坯的沿长度方向的两侧壁通过立辊施加压力,直至形变量h为10~50mm;所述铸坯加热处理的加热温度为1100~1200℃,保温时间为4~6h。本发明提供的改善硅钢热轧板边部质量的加工方法,采用铸坯两侧壁的侧压工艺,有效解决了热轧板边部裂纹的缺陷,提高了边部塑性,提高了成材率并降低了生产成本。
2020-12-15 177 6.8

以取向电工钢成分为基础,制备了含C或Mn和S的4种实验钢。观察了接近平衡析出状态实验钢经60%冷轧后在600~1000℃范围再结晶退火过程中微观组织演变,统计分析了再结晶体积分数随退火时间的变化规律,进而计算了各实验钢静态再结晶的激活能。观察了高含C实验钢退火初期再结晶晶粒优先出现的部位。结果表明900~1000℃范围内各实验钢铁素体的化学成分相似,因而其再结晶激活能基本一致。在600~800℃范围内铁素体内会有阻碍再结晶进程的三次渗碳体析出,从而使再结晶激活能明显提高。高C含量实验钢中还会有从奥氏体转变而来的粗大珠光体或渗碳体,轧制过程中其附近形成的变形区会促进600~800℃加热时该区域附近率先发生再结晶形核、降低再结晶激活能。固溶的Mn、S元素可微弱提高再结晶激活能,但高Mn、S含量会改变粗渗碳体从奥氏体析出时的形态。 Four experimental steels based on grain oriented electrical steel containing C,or Mn and S were prepared.Microstructure evolution of the steels close to a state of equilibrium precipitation were observed during annealing processes at 600-1000 ℃after 60% cold rolling,the changes of recrystallization volume fraction were analyzed statistically as the annealing was prolonged,and the activation energy for static recrystallization of the steels were calculated.The locations,where the recrystallizatio... 
2011-12-28 177 5.8

阐述了电工钢在\"双碳\"中的作用,强调了电工钢的生产工艺技术及在减少碳排放、降低能耗中的作用,对下游能效升级带来明显的节能及降碳成果。同时,分析了2021年电工钢的生产运行情况,介绍了电工钢的未来发展,并针对如何减少碳排放以及生产更多的更低铁损、更高磁感的电工钢谈了几点启示。 The effects of electrical steels on carbon peak and carbon neutralization were expounded,especially on the achievements of obvious energy saving and carbon reduction to the downstream energy efficiency upgrading bringing from the production technology of electrical steels and their effects to reducing carbon emission and energy consumption.Meanwhile the production situation of electrical steels in 2021 was analyzed,and the future development of electrical steels was introduced,and some advices w... 
2022-01-28 177 5.8

针对宝钢集团、日本新日铁住金和JFE公司公开的相关专利等资料,总结了国内外高强度无取向电工钢的研究进展,分析了不同电工钢的化学成分、生产工艺及产品性能,指出固溶强化、细晶强化、析出强化、位错强化都有可能被用来提高无取向电工钢的强度,并阐述了四种强化方式的优缺点;指出在高强度无取向电工钢的研发过程中,需根据其具体用途确定目标性能,再采用合适的强化手段,最终实现力学性能、磁性能和生产性能之间的平衡。 The research progress of high strength non-oriented electrical steels at home and abroad is summarized according to related patents brought into the public by Baosteel,Nippon Steel & Sumitomo Metal corporation and JFE corporation.The characteristics of chemical composition,production technology and properties of products in the patents are analyzed.Each of solution strengthening method,fine-grain strengthening method, precipitation strengthening method or dislocations strengthening method ma... 
2014-04-28 177 5.8

针对宝钢硅钢常化退火过程中产生的退火炉辊印缺陷问题,通过实际生产的大数据与产品质量问题相结合,将数据挖掘、数据分析方法应用到实际,一定程度上解决了现场实际生产中的痛点,为现场生产提供决策支撑,避免了以前通过人工识别判定存在疏漏和无法定量判断的问题,形成了一套具有鲁棒性和可操作性的钢铁生产过程数据分析方法。通过智慧决策系统平台获取实际生产和表检仪数据,基于Pearson相关系数算法进行变量挑选和特征工程,并应用随机森林算法对数据建立分类预测模型,实现了质量问题的溯源和监控,通过数据量化预测了炉辊印缺陷是否可通过轧制消除的质量问题,识别准确率达到96.43%。 In views of the normalizing annealing furnace roll marks problem occurred in the process of normalizing annealing of silicon steel in Baosteel,by combining big data from actual production with product quality problems,data mining and data analysis methods were applied to actual production to solve the pain points and provide decision support,a robust and practical data analysis method for the steel production process has been developed,which avoided the previous problems of omission and non-quan... 
2022-01-28 177 5.8

研究了退火温度对3.1%Si无取向硅钢组织和磁性能的影响规律。结果表明:退火温度从940℃提高至1 000℃,平均晶粒尺寸由98μm增加到145μm,铁损P1.5/50从2.576 W/kg降低至2.408W/kg。随着退火温度的升高,γ不利织构组分强度逐渐降低,{111}〈112〉织构组分强度降低约16%,磁感B50逐渐升高,磁性能水平提高。 The effects of annealing temperature on microstructure and texture and magnetic properties of 3.1%Si non-oriented silicon steel were investigated in this paper.The results showed that,when the annealing temperature increased from 940℃ to 1 000℃,the average grain size of metallographic structure increased from 98μm to 145μm,the iron loss value P1.5/50 decreased from2.576 W/kg to 2.408 W/kg.And as the annealing temperature increased,the strength of the unfavorable texture componentγgrad... 