选取了三种50W 800无取向电工钢,分析了化学成分、晶粒尺寸、织构、以及200℃时效处理48 h前后的磁性能和第二相粒子析出状态的变化。结果表明,钢板中第二相粒子的分布密度对钢板铁损有最重要的影响。降低钢中C、N元素含量,或改进钢板热加工参数以降低成品钢板中第二相粒子形成元素的过饱和度均有利于明显降低钢板磁时效过程中的铁损增幅。钢板中对磁性能有利的织构也有利于降低钢板铁损的时效幅度。 The evolution of chemical composition,grain size,texture,as well as magnetic property after aging treatment at 200 ℃ for 48 h and distribution of second phase particles precipitation in three selected 50W800 non-oriented electrical steels were analyzed.The results show that the distribution density of second phase particles has great influence on core loss.Reducing C and N content,or improving hot-working parameters to reduce the supersaturation of elements forming second phase particles in prod... 
2011-08-28 182 5.8

阐述了国内外高磁感取向硅钢的生产研究水平与发展趋势,包括通过提高高斯晶粒取向度、细化磁畴、涂覆张力涂层、减薄钢片厚度进一步降低铁损以及低温加热技术和短流程技术新工艺。分析高磁感取向硅钢在我国大型电力变压器上的应用情况,结果表明,发展更薄规格高磁感、低铁损、低磁致伸缩取向硅钢可为大型变压器的安全性、节能性及环保性提供有效保障。 The research progress and development trend of high magnetic induction grain-oriented silicon steel at home and abroad are summarized,including the technology of improving the Goss alignment,refining domain wall,adding stress coating,decreasing thickness of sheet,and the new technique of reducing heating temperature of casting slab and shortening operational.Moreover,the application of high magnetic induction grain-oriented silicon in power transformer is presented.Developing grain-oriented sili... 
2014-11-28 182 5.8

本实用新型涉及一种硅钢片叠压精准定位设备,包括压台、压板和仿形燕尾键,所述压台上开有与仿形燕尾键下端相对的限位槽,所述压板设置与压台上方,所述压板上开有与仿形燕尾键上端相对的限位孔。本技术方案当硅钢片叠放压合之后,仿形燕尾键可以去除,并能够在硅钢片组成的铁芯上形成燕尾槽,用于后期燕尾键的组装,且能够保证燕尾槽内的结构规则,便于后期燕尾键组装。
2021-11-22 182 6.8

取向硅钢因其高磁导率、低矫顽力和大电阻系数等特性,被广泛应用于大中型变压器和大型电动机铁芯的制造。因取向硅钢性能和成分控制严格,生产工艺复杂,故其产品代表了钢铁企业特殊钢生产的最高水平。本文介绍了新钢公司卷板厂1580热连轧线生产取向硅钢过程中出现的窄尺问题,研究了取向硅钢产品的特点,分析了热轧过程中的组织转变,并结合生产实际提出了改进措施。通过对加热炉钢坯加热模式、粗轧轧制策略、精轧轧制工艺、二级模型等方面的优化和改进,取向硅钢窄尺情况明显好转,提高了产品的成材率和市场口碑。 The oriented silicon steel is widely used in the iron core manufacture of large and mediumsized transformers and large motors because of its high permeability, low coercivity and large resistance coefficient. Due to the performance and composition control of oriented silicon steel is strict, the production process is complex,therefore, its products represent the highest level of special steel production in iron and steel enterprises. This paper introduces the problem of narrow gauge in the produ... 
2022-06-28 182 5.8

以取向电工钢成分为基础,制备了含C或Mn和S的4种实验钢。观察了接近平衡析出状态实验钢经60%冷轧后在600~1000℃范围再结晶退火过程中微观组织演变,统计分析了再结晶体积分数随退火时间的变化规律,进而计算了各实验钢静态再结晶的激活能。观察了高含C实验钢退火初期再结晶晶粒优先出现的部位。结果表明900~1000℃范围内各实验钢铁素体的化学成分相似,因而其再结晶激活能基本一致。在600~800℃范围内铁素体内会有阻碍再结晶进程的三次渗碳体析出,从而使再结晶激活能明显提高。高C含量实验钢中还会有从奥氏体转变而来的粗大珠光体或渗碳体,轧制过程中其附近形成的变形区会促进600~800℃加热时该区域附近率先发生再结晶形核、降低再结晶激活能。固溶的Mn、S元素可微弱提高再结晶激活能,但高Mn、S含量会改变粗渗碳体从奥氏体析出时的形态。 Four experimental steels based on grain oriented electrical steel containing C,or Mn and S were prepared.Microstructure evolution of the steels close to a state of equilibrium precipitation were observed during annealing processes at 600-1000 ℃after 60% cold rolling,the changes of recrystallization volume fraction were analyzed statistically as the annealing was prolonged,and the activation energy for static recrystallization of the steels were calculated.The locations,where the recrystallizatio... 
2011-12-28 181 5.8

针对某厂DMS森吉米尔轧机生产无取向硅钢表面麻面缺陷的问题,根据生产实际,对其形成原因从乳化液及工作辊两方面因素进行了分析。结果表明:乳化液对麻面缺陷的产生有一定影响,但不是主要因素,主要原因是由于二十辊森吉米尔轧机工作辊辊径较小,轧制相同长度带钢轧辊运转周期较大,容易产生疲劳失效而导致。为此,提出通过调整冷轧工序成品轧制道次的压下率以减小轧制力,从而减小工作辊的磨损疲劳;通过对轧制乳化液浓度、温度的合理控制,以改善润滑效果、提高轧制速度,而进一步缓解轧辊疲劳的改进措施,使该钢厂无取向硅钢麻面缺陷发生率由原来的18%降至0.8%,带钢表面质量明显改善。 For the problem of surface pockmarks of non-oriented silicon steel strip produced by a DMS Sendzimir mill, based on the production practice, the formation causes were analyzed from two aspects of emulsion and working roll. The results show that the emulsion has a certain effect on the formation of surface pockmarks defects, but it is not the main factor. The main reason is that the working roll diameter of the 20-high Sendzimir mill is small, and the running period of the roll rolling the same l... 
2022-01-28 181 5.8

针对宝钢集团、日本新日铁住金和JFE公司公开的相关专利等资料,总结了国内外高强度无取向电工钢的研究进展,分析了不同电工钢的化学成分、生产工艺及产品性能,指出固溶强化、细晶强化、析出强化、位错强化都有可能被用来提高无取向电工钢的强度,并阐述了四种强化方式的优缺点;指出在高强度无取向电工钢的研发过程中,需根据其具体用途确定目标性能,再采用合适的强化手段,最终实现力学性能、磁性能和生产性能之间的平衡。 The research progress of high strength non-oriented electrical steels at home and abroad is summarized according to related patents brought into the public by Baosteel,Nippon Steel & Sumitomo Metal corporation and JFE corporation.The characteristics of chemical composition,production technology and properties of products in the patents are analyzed.Each of solution strengthening method,fine-grain strengthening method, precipitation strengthening method or dislocations strengthening method ma... 
2014-04-28 181 5.8

本发明涉及一种冷轧硅钢厚度缺陷识别方法、装置及系统,本发明的方法包括如下步骤:采集带钢设定厚度及其实际测量厚度并保存;将带钢实际测量厚度与带钢设定厚度相减得到实时厚度差;根据实时厚度差计算厚度缺陷评分;根据评分结果,确定带钢在厚度这一指标的缺陷等级。本发明评估过程考虑了厚度波动情况,并进行量化,能成功识别冷轧硅钢的厚度缺陷,设别准确性较高,提高了冷轧硅钢生产水平,为冷轧硅钢质量控制提供依据。
2021-10-26 181 6.8

本发明揭示了一种无取向硅钢及其生产方法。所述生产方法包括:按照Si0.8~1.1%、Mn0.2~0.4%、不添加Sn和Sb进行炼钢,并制坯;将铸坯加热到1060~1120℃并保温150min以上,而后轧成厚度40~45mm的中间坯,再经精轧、卷取得到厚度为3.00±0.25mm的热轧卷板,精轧开轧温度≤872℃+1000*(11*[Si]‑14*[Mn]+21*[Al]);精轧终轧温度≤820℃,卷取温度≤560℃;常化、酸连轧,得到厚度为0.500±0.005mm的冷硬卷,常化温度850~900℃;成品退火温度820~880℃,退火后经冷却、涂层和精整,得到无取向硅钢。
2021-06-17 181 6.8

本实用新型公开了一种变压器铁芯硅钢片纵剪滚切装置,包括纵剪机本体、弹性压覆机构和涂油机构,所述纵剪机本体的进料端设置有弹性压覆机构,料带通过弹性压覆机构压覆在纵剪机本体的支撑平台上,所述支撑平台上凹设有安装凹槽,所述安装凹槽内设置有涂油机构,所述涂油机构朝向于料带的底面涂油,通过涂油机构对板材的切割面进行涂油,能够对料带起到润滑和冷却的作用,提升料带切割质量。
2021-12-13 181 6.8

采用电子背散射衍射技术测定50SW1300冷轧无取向硅钢中不同尺寸范围晶粒的含量,利用主成分回归分析法,综合研究不同尺寸范围晶粒的含量对无取向硅钢磁性能的影响。结果表明:通过主成分回归分析法能够从不同尺寸范围晶粒的含量的多个影响因素中获取主要的因素,定量研究它们对无取向硅钢磁性能的影响规律。分析表明,无取向硅钢的铁损与不同尺寸范围晶粒的含量之间存在着可靠的多元线性关系,在一定范围内,较大尺寸晶粒的含量越多,其对铁损优化的作用越明显;而无取向硅钢的磁感与不同尺寸范围晶粒的含量之间并无线性关系。 Distribution of grain size in cold rolled non-oriented silicon steel 50SW1300 was measured by EBSD.The effects of the distribution of grain size on magnetic properties of the non-oriented silicon steel were comprehensively researched by means of principal component regression method.The results indicate that the main factors influencing the magnetic properties in the distribution of grain sizes,which can be used to guantitative study the magnetlic properies of the steel,are obtained by principal... 
2014-11-28 181 5.8

本发明涉及取向硅钢技术领域,且公开了包括以下步骤:步骤一:冶炼,冶炼经转炉和RH精炼后得到钢水,在进行冶炼的过程中通入空气并设置总进气量100‑300Nl/min,且通入的空气中氧含量为20‑21%之间。该磁性优良的高磁感取向硅钢的气氛控制工艺,通过在不同的流程中,加入一定配比的氧气和氮气的含量,有效的提升每个阶段的气氛控制精度,从而得到最终的高磁感取向硅钢达到优良,避免了因气压、流量等因素影响最终高磁感取向硅钢磁力效果,炉渣中FeO含量减少,提高钢回收率和炉衬寿命,进而也起到降低生产成本的效果,且进行精确的气氛控制,使得在进行高磁感取向硅钢的冶炼中,使得冶炼的效果更好,使得冶炼出来的高磁感取向硅钢的磁性更加的优良。
2020-12-14 181 6.8