冷轧无取向硅钢横向厚差控制
冷轧中中低牌号的无取向硅钢多采用万能凸度轧机(Universal crown mill,UCM)生产,其板形好坏受制于UCM轧机板形调节手段的协调使用。为掌握UCM轧机的板形控制特点,建立基于二维变厚度有限元的辊系弹性变形和基于三维差分的轧件塑性变形的六辊轧机耦合模型,对UCM轧机的板形调控性能进行详尽的分析,包括工作辊和中间辊弯辊、中间辊窜辊的调控功效、辊间接触压力分布等。在此基础上,提出可用指导生产的板形控制策略,指出UCM轧机在横向厚差控制方面的不足。针对工业生产中UCM轧机轧制无取向硅钢横向厚差大的问题,在大量仿真计算的基础上,开发具有高次曲线函数的边部变凸度(Edge variable crown,EVC)的工作辊。采用该工作辊后,各种品种的无取向硅钢的横向厚差不大于10μm的百分比由24%提高到99%,横向厚差的均值小于6μm,远小于之前的13μm。 Medium-low grade non-oriented silicon steel is rolled often by universal crown mill(UCM) during cold rolling.Its shape quality is dependent on the coordinated control of several shape adjustment devices of UCM.In order to understand the shape control characteristics of UCM,coupling model of six-high rolling mill,based on two-dimensional varying thickness finite element rolls elastic deformation model and three-dimensional finite difference strip plastic deformation model,is setup for the detaile...
Fe-6.5%Si高硅钢铁芯与Epstein Square标准单片铁损检测结果对比及数据差异分析
作为一种具有优异高频铁磁性能的合金,Fe-6.5%Si(质量分数)高硅钢在高频工况条件下降损效果明显,对电气行业应用器件高频化、小型化、节能等具有十分重要的意义。通过与取向硅钢测量B-P数据对比,验证了高硅钢高频超低损特性,且轧制高硅钢与日本CVD法生产高硅钢存在基本相同的铁损值。采用国标Epstein Square法对0.30mm高硅钢薄板进行单片测试,并对由0.30mm高硅钢薄板首次装配成的电感器进行铁损测试,对比测试结果表明,元件测试与单片测试数据基本吻合,高磁感应强度条件下,元件测试结果略低于单片测试,分析原因为:线圈引起励磁压降;元件叠片间出现短路,电流增大,损耗增加;气隙板厚度过大。 As one core material with excellent high-frequency ferromagnetism,Fe-6.5%Si performs obviously reduction on core loss in high field frequency which means much to high frequency,minimization,energy conservation in electric industry.Super low loss was verified by drawing B-P curves based on detected experimental data,and which went equal to Fe-6.5%Si thin strip fabricated by CVD in Japan.Fe-6.5%Si was firstly fabricated as inductor in this research,and its core loss was determined for comparison w...
高Si电工钢铁芯的MA-SPS制备工艺和磁性能研究
以一种新的Fe-Si合金制备工艺为出发点,研究了不同放电等离子体快速烧结工艺(SPS)和Si含量变化对Fe-Si合金材料显微组织与磁性能的影响。结果表明,在烧结温度为1 000℃时制备的Fe-6.5%Si合金(质量分数,下同)的综合磁性能较好,其在50Hz下的铁损为0.549W/kg,最大磁感应强度为0.124 3T,矫顽力245.6 A/m,磁导率0.338mH/m。另外,材料的最大磁感应强度随Si含量的增加显著增长,1 000Hz下,Fe-10.0%Si的最大磁感应强度可达到Fe-6.5%Si合金的5倍左右。 The effects of Si content and SPS technology on microstructure and magnetic properties of Fe-Si alloy material were studied in the paper.It shows that the magnetic properties are the best when the content of Si is 6.5wt% and the sintering temperature is 1 000℃,the iron loss is 0.549W / kg in 50Hz,maximum magnetic induction is 0.124 3T,coercive force is 245.6A / m and permeability is 0.338mH / m。And,the maximum magnetic induction increases significantly with the increase of Si.The maximum magneti...
无取向电工钢XG800WR连铸电磁搅拌试验研究
采用铸坯低倍组织检验和化学分析的方法,研究板坯连铸机二冷区电磁搅拌器电流和频率参数对无取向电工钢XG800WR板坯中心偏析和等轴晶率的影响,结果表明:铸坯等轴晶率随着搅拌器电流强度和电流频率的增大而增加。采用二冷区电磁搅拌可减小中心易偏析元素S的偏析,试验得出:减小铸坯S偏析效果最好的电磁搅拌参数为电流380~400A,频率6Hz。 The effect of electromagnetic stirring current and frequency parameter at secondary cooling area on the central segregation and equiaxed crystal ratio of XG800WR non - oriented electrical steels slab was investigated through the methods of chemical and macrostructure analysis.The results shows that the rate of equiaxed crystal zone is going up with increasing of current intensity and current frequency.Electromagnetic stirring in the secondary cooling area can be easily reduced segregation caused...
无取向电工钢表面线状缺陷的影响因素分析
结合扫描电镜和大样电解研究了CSP流程W800牌号无取向电工钢表面线状缺陷中夹杂物成分及来源,采用SPSS软件回归分析了生产过程各因素对表面线状缺陷的影响。研究表明:稳态浇铸过程铸坯中大型夹杂物含量为5.39 mg/10 kg。引起无取向电工钢表面线状缺陷的大型夹杂物主要为脱氧产物、镁铝尖晶石和钢包顶渣,主要类型为Al2O3、MgO-Al2O3、CaO-Al2O3-MgO和CaO-Al2O3-SiO2。非稳态浇铸过程钢水洁净度明显降低,热轧板表面线状缺陷比例上升。影响表面线状缺陷的主要因素为RH出站时顶渣的w(CaO)/w(Al2O3)、RH脱氧结束氧位及中间包最低吨位。 Combining scanning electron microscopy and large sample electrolysis, the composition and source of inclusions in the surface linear defects of W800 grade non-oriented electrical steel in the CSP process were studied. SPSS software was used to regress and analyze the main factors which affected the surface linear defects in the steelmaking process. Research shows that the content of large inclusions in the steady state casting process is 5.39 mg/10 kg. The large inclusions which cause linear def...
新能源车驱动电机用电工钢用量解析计算及预测方法
对新能源汽车以及驱动电机的现有市场和未来市场规模进行梳理分析,通过自建计算公式推导出我国2021年1-11月份驱动电机用电工钢的总量,进而预测未来10年中国新能源汽车驱动电机用电工钢情况,为无取向电工钢的生产和在电机中的应用提供有价值的参考。 The current market and future market size of new energy vehicles and traction motors were analyzed,and the total amount of electrical steels used in traction motors in China from January to November 2021 was derived by using self-built calculation formulas,and then the situation in the next ten years of electrical steel used in traction motors of new energy vehicles in China was predicted.It will provide a valuable reference for the production of non-grain oriented electrical steel and its appli...
硅钢常化退火炉辊印缺陷预测分类预警方法研究
针对宝钢硅钢常化退火过程中产生的退火炉辊印缺陷问题,通过实际生产的大数据与产品质量问题相结合,将数据挖掘、数据分析方法应用到实际,一定程度上解决了现场实际生产中的痛点,为现场生产提供决策支撑,避免了以前通过人工识别判定存在疏漏和无法定量判断的问题,形成了一套具有鲁棒性和可操作性的钢铁生产过程数据分析方法。通过智慧决策系统平台获取实际生产和表检仪数据,基于Pearson相关系数算法进行变量挑选和特征工程,并应用随机森林算法对数据建立分类预测模型,实现了质量问题的溯源和监控,通过数据量化预测了炉辊印缺陷是否可通过轧制消除的质量问题,识别准确率达到96.43%。 In views of the normalizing annealing furnace roll marks problem occurred in the process of normalizing annealing of silicon steel in Baosteel,by combining big data from actual production with product quality problems,data mining and data analysis methods were applied to actual production to solve the pain points and provide decision support,a robust and practical data analysis method for the steel production process has been developed,which avoided the previous problems of omission and non-quan...
取向硅钢的晶体衍射花样特征研究
广泛应用于电子电力行业的取向硅钢材料的磁性能与其晶体取向密切关联,对取向硅钢晶体衍射花样的研究非常重要.采用理论计算的方式研究了取向硅钢的晶体衍射花样特征,并绘制了取向硅钢的高斯织构理论极图、理论单晶透射电子衍射斑点花样和理论电子背散射衍射(Electron backscatter diffraction, EBSD)菊池花样.取向硅钢理论单晶衍射花样不仅可以为以后标定样品实测晶体衍射花样提供一种简单快捷的方法,也可以为样品检测提供一种标准.这种研究方法不仅限于取向硅钢,也被期待应用于其他材料晶体衍射花样研究. The magnetic properties of oriented silicon steels which are widely used in electronic and power industries are closely related to their crystal orientations, so it is very important to study the crystal diffraction patterns of oriented silicon steels. The characteristics of crystal diffraction patterns of oriented silicon steels are studied by means of theoretical calculation. The theoretical pole figures, theoretical single crystal transmitted electron diffraction patterns and theoretical elec...
晶粒尺寸对无取向硅钢磁性能影响的主成分回归分析
采用电子背散射衍射技术测定50SW1300冷轧无取向硅钢中不同尺寸范围晶粒的含量,利用主成分回归分析法,综合研究不同尺寸范围晶粒的含量对无取向硅钢磁性能的影响。结果表明:通过主成分回归分析法能够从不同尺寸范围晶粒的含量的多个影响因素中获取主要的因素,定量研究它们对无取向硅钢磁性能的影响规律。分析表明,无取向硅钢的铁损与不同尺寸范围晶粒的含量之间存在着可靠的多元线性关系,在一定范围内,较大尺寸晶粒的含量越多,其对铁损优化的作用越明显;而无取向硅钢的磁感与不同尺寸范围晶粒的含量之间并无线性关系。 Distribution of grain size in cold rolled non-oriented silicon steel 50SW1300 was measured by EBSD.The effects of the distribution of grain size on magnetic properties of the non-oriented silicon steel were comprehensively researched by means of principal component regression method.The results indicate that the main factors influencing the magnetic properties in the distribution of grain sizes,which can be used to guantitative study the magnetlic properies of the steel,are obtained by principal...
余热利用系统在硅钢连续退火机组中的应用
介绍了烟气余热利用系统的工艺流程及控制思想,结合该系统在钢厂硅钢连续退火机组中的应用实践,估算出烟气余热利用系统每年可节约蒸汽5 040 t,经济效益良好,同时分析了该系统存在的问题及对策。 Introduced a method about the process and control of the application of waste heat system, which had been used into a silicon steel continuous annealing line and profiting a good economic benefit by saving a large number of steam every year, which has been estimated about 5 040 tons, and analyzed the problems and solutions existed in this system.
高硅钢薄板退火过程中的织构演变
采用传统的轧制和退火工艺制备了0.30mm厚的6.5%(质量分数)Si高硅电工钢薄板,采用X射线衍射技术对退火过程中的再结晶织构进行了研究。冷轧高硅钢薄板700℃退火形成以{111}〈112〉为峰值的γ织构(〈111〉∥ND)和以{001}〈210〉为峰值的{001}织构;而900℃以上温度退火则形成强{001}〈210〉织构。进一步的研究表明是在晶粒长大过程中{001}〈210〉发展成为主要再结晶织构组分。 High silicon steel thin sheets with thickness of 0.3mm were successfully produced by conventional rolling and annealing methods.Recrystallization texture was investigated by means of X-ray diffraction.It is found that recrystallization texture is mainly composed of γ fiber(〈111〉∥ND)with peak at {111}〈112〉 and {001} fiber with peak at {001}〈210〉 after annealing at 700℃,while strong {001}〈210〉 component dominates recrystallization texture after annealing above 900℃.It is during grain growth that {...