钢厂
钙合金处理硅钢中的夹杂物及晶粒成长变化
采用RH精炼添加钙合金方式对硅钢进行钙处理,结果表明,钙合金添加量为0.67、1.00和1.67 kg/t钢时,钢中Ca含量分别为0、2×10-6和4×10-(6质量分数);随着钙合金添加量的增加,钢中夹杂物粒度逐渐由0~2μm向2~4μm、4~6μm偏移;不同钙处理条件下,钢中均存在粒径小于1μm和粒径为1~5μm的MnS、CuxS夹杂物,后者或单独存在,或与AlN、CaS夹杂复合;钢中粒径为5~10μm的夹杂物基本以Ca的氧化物和硫化物为主。与未经钙处理的炉次相比,钙合金添加量为0.67、1.00和1.67 kg/t钢时,粒径小于1.0μm的夹杂物减少幅度分别为68.06%、87.50%和94.94%。钙合金添加量为1.67 kg/t钢时,可以去除钢中绝大部分的微细夹杂物。 In order to improve the properties of final silicon steels,the calcium treatment was adopted by adding Ca alloys into the liquid steel during the RH refining process.Results show that when the addition of Ca alloys is 0.67 kg/t,1.00 kg/t and 1.67 kg/t,the corresponding Ca content in silicon steels is 0,2 × 10-6 and 4 × 10-6 respectively.With the increase of Ca alloy addition,the particle sizes of inclusions in steels become 2~4 μm and 4~6 μm,from 0~2 μm.Under different calcium treatments,there e...
低温高磁感取向硅钢连铸与均热过程AlN与MnS析出的热力学
针对薄板坯连铸连轧流程结合\"获得抑制剂法\"所制备的低温高磁感取向硅钢,通过热力学计算研究了AlN与MnS在连铸与均热过程中的析出规律与行为。计算结果表明,连铸过程中AlN在凝固后的高温α相中便可能析出,而MnS仅可能在凝固后的α+γ两相区内析出。钢中AlN与MnS在均热过程中均处于部分固溶与部分析出的状态。后续高温渗氮处理后初次晶粒的异常长大并不明显,表明渗氮处理前钢中固有抑制剂的数量相对充足。 The precipitation behavior of MnS and AlN in low-temperature high magnetic induction grain-oriented silicon steel produced by thin slab casting and rolling process with\"acquired inhibitor method\"during continuous casting and soaking was studied by thermodynamic calculation.The calculated results show that AlN is likely to precipitate in ferrite after solidification.However,MnS can precipitate only in the two phase region of ferrite and austenite.Meanwhile,MnS and AlN in the steel can not be comp...
热处理工艺对含Mn高硅钢热轧带的组织及硬度的影响
研究了热处理工艺(退火温度、保温时间、冷却方式)对含Mn的Fe-6.5wt%Si高硅钢热轧带的显微组织及硬度的影响。结果表明,退火温度对Fe-6.5wt%Si合金的组织和显微硬度均有较大影响,随退火温度升高,平均晶粒尺寸和显微硬度均明显增大。小于1 h退火时,晶粒长大缓慢,而长时间(>1 h)退火时,一些次表层晶粒将发生异常长大。水冷组织比空冷组织略细小,但水冷显著降低了显微硬度。Mn含量提高能抑制850℃退火时晶粒的长大,并且促进退火后高硅钢的软化。 The influences of heat treatment process(annealing temperature,heating time,cooling methods) on the microstructure and microhardness of Fe-6.5wt%Si high silicon steel containing manganese for hot rolled strip were studied.The results show that the annealing temperature has a great effect on the microstructure and microhardness of Fe-6.5wt%Si alloy,and as the annealing temperature increases,the average grain sizes and microhardness will significantly increase.When annealing time for less than 1 h...
冷轧大压下量下新型无取向电工钢的退火组织演变
研究了冷轧大压下量,950℃退火时间对一种新型含铜无取向电工钢晶粒度和织构的影响。结果表明,大压下量冷轧,随压下量的增加,退火晶粒向γ线聚集,形成强{111}<112>织构。提高冷轧压下率,退火织构{111}<100>,{110}<001>强度减弱,增加退火时间,退火织构{111}<110>,{100}<001>,{110}<001>强度变弱。采用87.5%冷轧压下率和950℃退火60 s,有利织构{100},{110}占有率最大。 The effect of annealing(950 ℃) time with high cold rolling reduction on grain size and texture of a new non-oriented electrical steel containing copper was investigated.The results show that for high cold rolling reduction,most annealed grains are oriented along γ-fibre with increasing cold rolling reduction ratio and strong texture {111}<112> is formed.With increasing the cold rolling reduction ratio,the intensity of annealed texture {111}<110>,{011}<100> decreases.With increa...
RH精炼添加钙合金去除硅钢夹杂物研究
采用RH精炼添加钙合金方式对硅钢进行钙处理。结果表明,钙合金添加量为0.67、1.00、1.67kg/t钢时,钢中钙含量分别为0、2×10-6、4×10-6;随着钙合金添加量增大,钢中夹杂物粒度逐渐由0~2μm向2~4、4~6μm偏移;不同钙处理条件下,钢中均存在粒径小于1μm和粒径为1~5μm的MnS、CuxS夹杂物,后者或单独存在,或同AlN、CaS夹杂复合;粒径为5~10μm区间,钢中的夹杂物基本以钙的氧、硫化物为主。与钙处理前相比,钙合金添加量为0.67、1.00、1.67kg/t钢时,粒径小于1.0μm的微细夹杂物减少幅度分别为68.06%、87.50%、94.94%。钙合金添加量为1.67kg/t钢时,可以去除钢中绝大部分的微细夹杂物。 Ca alloy was added into the liquid steel during RH refining,and the results show that Ca concentration in final Si steel sheets is insignificant,about 0,2×10-6 and 4×10-6 when the added amount of Ca is 0.67,1.00 and 1.67 kg/t steel,respectively.With the increase in the added Ca alloy amount,the inclusions in the steel gradually change from those of 0~2 μm to those of 2~4 and 4~6 μm.Under different Ca treatments,there exist MnS and CuxS inclusions whose size is below 1 μm as well as MnS and CuxS ...
硅钢连退机组辐射管加热段数值模拟
文章以国内某公司硅钢厂连续退火机组1号辐射管加热段为研究对象,分析炉内传热机理,建立并开发了辐射管加热段的传热模型。采用生产实际数据对模型进行了验证,以总燃料消耗量最小为目标,得出该炉段长度方向上燃料的最佳分配机制。所得结论为该公司连续退火机组节能控制提供理论依据。 Taking the radiant tube heating section of No.1 continuous annealing unit in a silicon steel plant of a domestic company as the research object, the heat transfer mechanism in the furnace is analyzed, and the heat transfer model of the radiant tube heating section is established and developed. The model is verified by the actual production data. Aiming at the minimum total fuel consumption, the optimal fuel distribution mechanism in the length direction of the furnace section is obtained. The co...
高温退火气氛对硅钢表面硅酸镁底层形貌的影响
对取向硅钢在不同气氛下的高温退火工艺进行实验室模拟,利用X射线衍射仪(XRD)分析了硅钢退火至900℃和1170℃时的样品表面氧化层和底层的物相组成,采用场发射扫描电镜(SEM)观察了样品表面氧化层和底层在截面方向上的微观形貌特征,并计算了高温退火一次升温阶段氧化反应的吉布斯自由能以及900℃时退火气氛的氧分压。结果表明:当退火气氛的露点温度保持一定时,较高的氢气含量有利于生成完整连续的底层;当退火气氛的水氢分压比保持一定时,在露点温度与氢气含量两者较低的条件下,底层附着性不佳易脱落,较高条件下,底层中夹杂着较多的铁单质;当氧化层中无FeO时,底层完整连续但易脱落,当FeO层较薄时,底层下方存在部分未反应的SiO2,当FeO层较厚时,底层不完整连续且有分层。 The high temperature annealing process of grain-oriented silicon steel in different atmospheres was simulated in the laboratory. X-ray diffractometer(XRD) was used to analyze the phase compositions of the surface oxide layer and forsterite film of the silicon steel annealed to 900 ℃ and 1170 ℃. Field-emission scanning electron microscopy(SEM) was used to observe the micro morphology characteristics of the surface oxide layer and forsterite film of the samples in the cross section direction. The ...
高Si电工钢铁芯的MA-SPS制备工艺和磁性能研究
以一种新的Fe-Si合金制备工艺为出发点,研究了不同放电等离子体快速烧结工艺(SPS)和Si含量变化对Fe-Si合金材料显微组织与磁性能的影响。结果表明,在烧结温度为1 000℃时制备的Fe-6.5%Si合金(质量分数,下同)的综合磁性能较好,其在50Hz下的铁损为0.549W/kg,最大磁感应强度为0.124 3T,矫顽力245.6 A/m,磁导率0.338mH/m。另外,材料的最大磁感应强度随Si含量的增加显著增长,1 000Hz下,Fe-10.0%Si的最大磁感应强度可达到Fe-6.5%Si合金的5倍左右。 The effects of Si content and SPS technology on microstructure and magnetic properties of Fe-Si alloy material were studied in the paper.It shows that the magnetic properties are the best when the content of Si is 6.5wt% and the sintering temperature is 1 000℃,the iron loss is 0.549W / kg in 50Hz,maximum magnetic induction is 0.124 3T,coercive force is 245.6A / m and permeability is 0.338mH / m。And,the maximum magnetic induction increases significantly with the increase of Si.The maximum magneti...
Al含量对2.2%Si无取向硅钢组织、织构和磁性能的影响
通过实验室25 kg真空感应炉冶炼和锻轧研究了0.26%~0.95%Al含量对0.5 mm 2.2%Si无取向硅钢冷轧板组织、织构和磁性能的影响。试验结果表明,0.26%~0.81%Al含量时,随钢中Al含量的增加,成品退火钢板的晶粒尺寸增加同时铁损减少;当Al含量大于0.81%时,随Al含量增加,钢板的晶粒尺寸减小,同时铁损增加。Al含量对硅钢板磁感的影响没有明显的规律。2.2%Si无取向硅钢的合适Al含量为0.48%~0.81%。 The effect of 0.26%~0.95%Al content on structure,texture and magnetic performance of 0.5 mm cold rolled sheet of 2.2%Si non-oriented silicon steel has been studied by a 25 kg vacuum induction furnace smelting,and forging -rolling in laboratory.Results show that as 0.26%~0.81%Al,with increasing Al content in steel the grain size of annealed finished sheet increases while iron loss of sheet decreases,and as Al content in steel is more than 0.81%,the grain size of sheet decreases while iron loss in...
冲剪加工对无取向硅钢边缘组织和磁性能的影响
通过观察冲剪边缘组织,测量冲剪边缘的显微硬度、残余应力的分布情况和磁性能的变化研究了冲剪加工对无取向硅钢50WW800边缘组织和磁性能的影响。对冲剪后硅钢片进行750℃退火,分析退火对组织和磁性能的影响。结果表明,硅钢片剪切边缘会存在0.4 mm的形变硬化层,边缘应力大,铁损增加。退火后变形减小,形变硬化层变小,残余应力大幅度减少,铁损减少。 The influence of punching process on cutting edge microstructure and magnetic properties of non-oriented silicon steel 50WW800was studied by observing microstructure and measuring microhardness near cutting edge.The residual stress distribution in the silicon steel tooth and magnetic properties were measured.Effect of annealing at 750 ℃ on microstructure and magnetic properties of the silicon steel was analyzed.The results show that a cut-edge hardening layer up to 0.4 mm is observed,residual st...
冷轧无取向硅钢产品标准浅析
聚焦无取向硅钢产品标准,从电磁性能、表面性能、机械性能以及尺寸公差与边部质量等维度对国际标准IEC、EN、JIS、ASTM以及国标GB进行了分析研究。分析得出,各类标准在电磁性能方面要求基本一致;ASTM标准的机械性能要求有别于其他几个标准。 In this paper,non-oriented silicon steel standards of EN,JIS,GB and ASTM were compared and analyzed. It is showed that,all types of standards in electromagnetic performance requirements are basically the same. Surface properties in ASTM standard are expressed in the most detailed. The mechanical properties requirements of the standards,except for ASTM,are basically the same.