钢厂
电解清洗装置在电工钢生产线上的应用
介绍了电工钢生产线连退机组的表面处理工艺,特别是电解清洗系统的工作机理、设备构造、生产工艺及各种影响因素。 This paper introduces the technology of surface treatment of continuous annealing unit in electrical steel production line,in particular the working mechanism,structure of equipment,production techniques and various influence factors of the electrolytic cleaning system.
EBSD技术在硅钢织构研究中的应用
运用电子背散射衍射(EBSD)和X射线衍射(XRD)技术对硅钢热轧板的织构在板厚方向的分布进行了研究,并分析了两种织构测量方法的特点。EBSD技术能直观给出板厚方向的微观织构,XRD能得到钢板的宏观统计织构信息,结合两种技术的分析,能更直观更精确的研究不同织构在板厚方向的分布。 The texture distribution along the thickness of the silicon steel has been investigated by electron backscatter diffraction(EBSD) and X-ray diffraction(XRD) technique.The characteristics of two technique of texture analysis have been investigated.Combined the two techniques,the texture distribution along the thickness of the silicon steel could be realized distinctly and accurately.
无取向硅钢冶炼过程中的夹杂物遗传变化
研究表明,硅钢中的夹杂物对成品带钢的磁性能有显著影响。为研究冶炼过程硅钢中的夹杂物遗传变化,进而提出更有效的控制措施加以去除,本文结合典型的无取向硅钢生产炉次,采用非水溶液电解提取+扫描电镜观察方法分析冶炼过程中上述炉次典型试样的夹杂物。结果表明:转炉冶炼结束、RH精炼开始时,钢的氧化物夹杂总量最大,约为0.23%;RH精炼过程中,氧化物夹杂总量不断降低,并在脱碳结束时达到最低,约为0.02%;连铸过程中,氧化物夹杂总量仍有不断降低趋势,但夹杂物的平均尺寸变化不大。本试验条件下,中间包试样的夹杂物数量约为1.59×104个/mm3。 As we all know, the non-metallic inclusion effects magnetic properties of silicon steel sheets obviously. The article aims to study the heredity of non-metallic inclusion in non-oriented silicon steels during the steel making process, and then provides a more effective controlling measure to remove the inclusions. Based on the typical non-oriented silicon steel charges, the non-aqueous solution extraction and SEM observation were adopted to analyze the non-metallic inclusions. Results show that,...
无取向电工钢RH脱硫渣系的研究
在15 kg真空感应炉上,用CaO-Al2O3-SiO2-MgO渣系进行脱硫试验,探讨了脱硫渣系碱度、MI、Al2O3、CaF2对脱硫效果的影响。研究结果表明,随脱硫渣系碱度、MI、Al2O3和CaF2含量的增加,脱硫率都呈现先增加后减少的趋势。初始硫含量为0.009 33%~0.010 73%,加入脱硫渣系4 min时间内表观脱硫速率为(0.000 96~0.001 49)%/min,平均脱硫率为81.2%,最高达86.8%。当脱硫渣中w(CaO)=58.15%、w(SiO2)=4.85%、w(Al2O3)=25%、w(MgO)=6%、w(CaF2)=6%,脱硫效果最好,此时钢液中硫为0.001 33%。 Experiments on desulfurization of molten steel using CaO-Al2O3-SiO2-MgO based desulfurization slag was carried out in a 15 kg vacuum induction furnace. The effects of desulfurization slag basicity,MI, Al2O3and CaF2on desulfurization of molten steel were studied. The results show that with the increase of basicity,MI,Al2O3or CaF2in desulfurization slag,the desulfurization rate rises initially and then decreases. In addition,as the initial sulfur content is 0. 009 33% ~ 0. 010 73%,the apparent des...
电脉冲对取向硅钢凝固组织的影响
对熔融态钢液进行处理,研究了电脉冲对于取向硅钢凝固组织的影响作用,利用正交试验法研究了脉冲电容、频率、处理时间和电压等脉冲参数的作用效果。结果表明:电脉冲对钢锭晶粒组织具有明显的细化作用,凝固组织的等轴晶比例大幅上升,影响等轴晶比例的最显著性因素为脉冲频率,最优正交试验参数为电容1 200μF,脉冲频率1 Hz,处理时间5 s,脉冲电压800 V。随着输入能量的增大等轴晶率先增大后减小,脉冲输入能量为某值时,等轴晶率最大,利用经典形核理论和热力学对这一现象进行了解释。 The influence of electric pulse on the solidification structure of oriented silicon steel was investigated by applying electric pulse in molten steel.The affection due to different electric pulse parameters such as electric capacity,frequency,applied time and voltage was studied by orthogonal design test.The result showed that solidification structure of oriented silicon steel could be improved by the electric pulse,and the equiaxed crystal ratio increased obviously.The most influential paramete...
轧制力优化对20辊冷轧硅钢厚度精度的影响
轧制力是影响冷轧带钢厚度精度的关键因素。为实现高精度的冷轧带钢厚度控制,通过优化变形抗力模型参数和摩擦系数模型参数提高冷轧轧制力模型计算精度,并使用指数平滑法的自学习算法保证轧制力精度的稳定性。在首钢股份公司迁安钢铁公司20辊森基米尔轧机生产线进行S12硅钢钢种轧制力优化试验,将优化的模型参数应用于L2并投入现场生产,结果表明该优化方法不仅提高了轧制力设定精度,而且减小了冷轧硅钢的厚度超差长度,提高了成材率。 The rolling force is the key factor which influences the accuracy of cold-rolling strip thickness. To implement high precision control of cold-rolling strip thickness,we optimize the deformation resistance model parameters and friction coefficient model parameters to improve the calculation precision of cold-rolling force model,and use exponential smoothing self-learn algorithm to ensure the stability of rolling force accuracy. In Shougang Qiangang 20-high Sendzimir mill single stand production ...
冷轧硅钢废水处理现状、问题及对策浅析
就冷轧硅钢废水处理生产中面临的主要问题进行分析,从技术角度及运行管理角度提出工艺优化升级改进措施及应对策略;同时从后续深度处理,逐步实现零排放目标的角度进行探讨,为冷轧硅钢废水减量化、出路乃至废水零排放提供一些思路。 The main problems in the wastewater treatment process of cold-rolled silicon steel lines are analyzed and process upgrading measures and optimization strategy are put forward from both technical and management views.At the same time,downstream deep treatment to gradually achieve the target of zero discharge is discussed,to provide some ideas for reduction or even zero discharge of wastewater from cold-rolled silicon steel lines.
EB5325涂层液在冷轧无取向电工钢中的应用
介绍了EB5325涂层液的主要性能和中冶新材生产冷轧无取向电工钢所用的涂层设备,通过多次试验摸索出使用EB5325涂层液的工艺,对涂层出现的缺陷进行分析研究,并提出解决方法,使中冶新材生产的冷轧无取向电工钢的涂层质量满足了用户的要求。 This article introduces the main properties of EB5325 and the coating equipments for cold-rolled non-oriented electrical steel. A process using EB5325 coating liquid is made through many time experiments and exploration. The appeared defects in the coating are studied and analyzed,and the solutions are proposed. The coating quality meets clients’ requirements of cold rolled non-oriented electrical steel.
本钢薄板坯连铸机生产无取向电工钢的工艺优化
针对本钢薄板坯铸机在生产无取向电工硅钢的过程中存在的铸坯拉断、中包增碳、增氮等问题,进行了连铸工艺优化。通过采用新型无碳中间包覆盖剂、环保中间包干式料及专用结晶器保护渣后,降低了铸坯增碳量;通过控制钢包到中间包的增氮环节,降低钢水增氮;适当增大二冷水量,控制钢水过热度,防止铸坯拉断等生产事故的发生。改进工艺后,精炼后到成品铸坯的平均增碳量能控制在10×10-6以内,平均增氮量能控制在4×10-6以内。 The technology optimization has been adopted for preventing nitrogen increasing and carbon increasing in Benxi thin slab producing non-oriented silicon steel.Measures accordingly were adopted and satisfactory results were achieved.
电工钢中柱状晶尺寸及退火工艺对{100}织构的影响
利用EBSD技术研究了电工钢中不同的柱状晶尺寸及退火工艺下{100}织构的演变规律。结果表明,初始晶粒尺寸的影响最显著。细小柱状晶热轧后经过常化处理,组织已均匀,但中心层有强{100}织构。粗大柱状晶中{100}织构的遗传性强,常化及中间退火后,中心层仍有粗大的以{100}取向为主的晶粒;脱碳退火后才能完成组织均匀化和织构梯度的弱化。常化时的升温速度也对织构演变存在影响,低的升温速度有利于{100}织构的保留,但升温速度的影响没有初始晶粒尺寸及退火次数的影响显著。细小柱状晶样品经过热轧及三次退火工艺适合制备取向电工钢。 Evolution of {100} texture of different columnar grains and annealing process was investigated in electrical steels with the help of EBSD technique.The results show that the effect of initial grain size is the strongest.The initial fine-grained specimen shows uniform microstructure after the normalizing process,while {100} grains appear preferentially in the central layer of sheets.The heredity of {100} texture in the initial coarse-grained specimen is more significant.{100} mainly-oriented coar...