提高硅钢卷材下料利用率的几种方法
阐述了影响硅钢卷材下料利用率的因素,并结合具体事例利用计算机排样系统进行了详细分析,对提高硅钢卷材的利用率具有一定的指导作用。 It describes the factors influenceing the the utilization ratio of the roll of Silicon steel,and analyzes it in detail combined with concrete examples by a computer arrangement system,which can give a guide for increasing the utilization ratio of the roll of Silicon steel.
硅钢DR510生产工艺优化
本文对某厂硅钢DR510温度、成分及过程控制水平和成品的组织、力学性能进行了研究,并在此基础上提出了工艺优化方案,有一定的借鉴和推广价值。 In this paper,the critical process and the products quality,including temperature,composition and process controlling level,the organization and mechanical properties of the finished product,were studied.On the basis of that the optimized technical plan provided,and this control technology is worth using and spreading.
试样剪切应力对冷轧无取向电工钢磁性能的影响
电工钢试样加工产生的剪切应力会恶化钢板的磁性,对不同牌号硅钢片的横向、纵向试样退火前后磁性能的变化进行研究,结果表明:无取向硅钢片在剪切过程中横向、纵向的磁性受到剪切应力影响是不一样的。 The electrical steel sample processing magnetic of electrical steel will worsen due to the shear stress of sample. In this paper,the magnetic change of transverse,longitudinal specimens of different type of silicon steel sheet before and after annealing are studied. The results show that the magnetic of non- oriented silicon steel sheet affected in the process of shear is not the same in horizontal and vertical direction.
陶瓷辊除瘤方法在瑞致电工钢的应用
针对陶瓷辊表面结瘤清除时间长、清除效果差等缺陷,研究正反转陶瓷辊除瘤法,以缩短除瘤时间,增强除瘤效果。 The general removal of ceramic roller surface tumor costs a long time and the effect is poor.This paper probed into the ceramic roller tumor removal in order to shorten time and enhance the effect of eliminating.
冷轧无取向硅钢横向厚差控制
冷轧中中低牌号的无取向硅钢多采用万能凸度轧机(Universal crown mill,UCM)生产,其板形好坏受制于UCM轧机板形调节手段的协调使用。为掌握UCM轧机的板形控制特点,建立基于二维变厚度有限元的辊系弹性变形和基于三维差分的轧件塑性变形的六辊轧机耦合模型,对UCM轧机的板形调控性能进行详尽的分析,包括工作辊和中间辊弯辊、中间辊窜辊的调控功效、辊间接触压力分布等。在此基础上,提出可用指导生产的板形控制策略,指出UCM轧机在横向厚差控制方面的不足。针对工业生产中UCM轧机轧制无取向硅钢横向厚差大的问题,在大量仿真计算的基础上,开发具有高次曲线函数的边部变凸度(Edge variable crown,EVC)的工作辊。采用该工作辊后,各种品种的无取向硅钢的横向厚差不大于10μm的百分比由24%提高到99%,横向厚差的均值小于6μm,远小于之前的13μm。 Medium-low grade non-oriented silicon steel is rolled often by universal crown mill(UCM) during cold rolling.Its shape quality is dependent on the coordinated control of several shape adjustment devices of UCM.In order to understand the shape control characteristics of UCM,coupling model of six-high rolling mill,based on two-dimensional varying thickness finite element rolls elastic deformation model and three-dimensional finite difference strip plastic deformation model,is setup for the detaile...
退火工艺对3.15%Si冷轧无取向硅钢组织和织构的影响
试验研究了退火温度(850~950℃)和时间(5~18 min)对2.3 mm热轧硅钢板(/%:0.036C,3.15Si,0.21Mn,0.005P,0.007S,0.032A1)6道次轧制的0.35 mm冷轧板组织和织构的影响。结果表明,退火温度越高,晶粒平均尺寸越大,900℃5 min退火时平均晶粒尺寸41.39μm,试样织构主要集中在γ取向线上的{111}<112>织构组分和{111}<110>织构组分;900℃18 min退火时平均晶粒尺寸为48.08μm,试样的{111}面织构和{112}面织构密度都明显减弱,{001}面织构增强,磁性能较优。 The effect of annealing temperature(850 ~950 ℃) and holding time(5 ~ 18 min) on structure and texture of 0.35 mm sheet by 6 passes cold-rolling from 2.3 mm hot-rolled plate of silicon steel(/%:0.036 C,3.15 Si,0.21 Mn,0.005 P,0.007 S,0.032A1) has been tested and studied.Results show that the higher the annealing temperature the coarser the average grain size;As annealing at 900 ℃ for 5 min the average grain size of steel sheet is 41.39 μm,and the texture in sample is mainly concentrated in y orie...
冷轧无取向电工钢的试制
利用本钢技术中心试验厂技术手段,并与北京钢铁研究院合作,试制了用作家电用电机、微电机、小电机或部分中型电机铁芯的冷轧无取向电工钢。试制钢硅含量小于0.5%,钢板表面平滑,公称厚度0.5mm,且厚度均匀偏差小,性能测定结果表明,产品的磁性能、力学性能满足其使用要求。 BX STEELTechnology Center pilot plant using technical means,and with Beijing Iron and Steel Research Institute,trial cold rolled non-oriented electrical steel that has been used as appliance motor core,micro motor core,small motor core,or part of the medium-sized motor core。Trial steel of silicon content is less than 0.5%,steel plate surface is smooth,the nominal thickness of 0.5mm,and the thickness deviation is small,performance measurement results show that the magnetic properties,mechanical p...
6.5%Si硅钢的制备技术和发展前景
6.5%Si硅钢具有优异的磁学性能和广泛的应用前景。本文综述了6.5%Si硅钢的物理、机械及磁学特性,讨论了传统轧制、温轧、薄带连铸、快速凝固、CVD、粉末轧制等不同制备工艺的关键技术及特点,概括了6.5%Si硅钢在高效节能电机、汽车马达及磁屏蔽等领域中的主要应用,介绍了硅钢的制备技术取得的研究进展,并指出了其广阔的发展前景。 6.5% Si silicon steel has good magnetic properties and wide applications.In this paper physical and mechanical magnetic properties were summarized,and key technology and characteristic of several preparation methods,such as traditional rolling,warm rolling,thin strip continuous casting,rapid solidification,CVD and powder rolling,were discussed.Main applications of 6.5% Si steel in the fields of high-efficiency electrical motors,automobile motors,transformer cores and magnetic shielding were gene...
硅钢连续退火炉无氧化加热段辐射换热研究
以能量平衡和辐射换热理论为基础,通过合理假定,建立了硅钢无氧化加热炉数学模型。采用数值计算的方法,通过自编程序,完成对带钢加热过程温度场的仿真。结果显示:数学模型能够反映带钢在无氧化炉内的加热过程,其升温曲线能够与工艺曲线相吻合;现行炉温分布并非最优,数学模型能够为炉温分布的优化、炉段的设计提供理论依据。 Mathematical model of NOF Section of Continuous Annealing Furnace is established based on energy balance and radiation heat exchange. The temperature field of steel is simulated by mathematical computation. The simulating results show that the mathematical model can reflect the heating process of silicon steel in NOF section, and the heat-up curve is coincide with the processing curve. From the results,it is known that the current furnace temperature gradient is not the best, and the mathematica...