所有分类
  • 所有分类
  • 未分类

本申请涉及激光焊接技术领域,特别涉及一种电机定子硅钢片自动焊接工装。该工装包括定位组件,压板组件和旋转组件。其中,定位组件用于承载定子硅钢片,所述定位组件具有用于在径向上对定子硅钢片进行限位的限位结构;所述压板组件位于定位组件的顶端,用于压住定子硅钢片;旋转组件承托于定位组件的底端,并带动定位组件转动。本申请实施例提供的一种电机定子硅钢片自动焊接工装,能够解决在旋转焊接时,无法保证定子硅钢片与工装夹具的同心度相同,致使焊缝质量不过关的问题,以及激光焊接中,硅钢片与工装夹具易粘连的问题。
2021-12-21 148 6.8

结合冶炼无取向硅钢的生产实际,对钢中硫的来源,以及炉渣性质、钢水温度、底吹强度对脱硫的影响进行了分析。研究表明,转炉钢中硫的主要来源为铁水、废钢、铁水渣及石灰带入;冶炼硅钢时,终渣碱度为3.0~3.5,w((FeO))≤20%,终点钢水温度大于等于1 680℃,加大底吹搅拌强度能提高转炉脱硫效果。硅钢平均出钢硫的质量分数为0.004 8%,能满足无取向硅钢对硫含量的要求。 With the actual production of non-oriented silicon steel,the source of sulphur and the effect of metallugic parameters like slag properties,temperature of molten steel and bottom stirring on desulphurizing ability were investigated.The results show that the main source of sulphur is molten metal,scrap,the remaining slag volume in hot metal and lime.The degree of desulphurization for smelting silicon steel can be increased through adopting the following measures,such as the basicity of finishing ... 
2011-02-28 127 5.8

本实用新型公开了一种变压器铁芯用硅钢片成型铁测量平台,包括游标测量尺及定位台;定位台包括基架、操作台及至少两根的定位销,操作台I及操作台II分别设置于基架的横向两端,且操作台I及操作台II之间留有宽度a的间距区,操作台II上设置有至少一组的沿横向均匀分布的定位孔组,且至少两根的定位销能够与该定位孔组的定位孔配合,游标测量尺设置于基架上间距区处。在操作台II上设置有至少一组的沿横向均匀分布的定位孔组,且至少两根的定位销能够与定位孔配合,以将该硅钢片成型铁定位区域限定在操作台II台面上,采用多个定位孔和定位销配合结构,同时能够沿横向调整硅钢片成型铁定位位置,以便测量各个区域尺寸。
2021-12-29 144 6.8

一种硅钢生产线退火炉前的换热装置,包含有抽风机(1)、立柱(2)、热交换器(3)、软管(4)和热风机(5);其特征在于:所述的热交换器(3)由若干组U形不锈钢管连接而成,一端固定在轴套(8)上,另一端通过链条(10)连接在立柱(2)顶端的链条盘(9)上,当链条盘(9)转动时,链条(10)拉动热交换器(3)绕着横轴(7)抬起或放下。本实用新型通过抽风机(1)将清洁空气抽到热交换器(3)内进行加热,然后再通过软管(4)将热空气输送到热风机(5)内来加热硅钢板(14),有效的利用了热能,避免了凝露导致的板面发蓝现象。
2020-12-25 114 6.8

试验了通过NaCl-KCl-NaF-SiO2熔盐在电流密度50 mA/cm2、电沉积脉冲电流正反向比9:1和750850℃60min电沉积下阴极(/mm)20×20×0.5的1.6Si无取向冷轧硅钢片断面层硅的分布,并通过计算得出Si的扩散系数。结果表明,电沉积温度由750℃提高至850℃时,试样中Si含量增加,扩散的深度由18μm提高到40μm;电沉积温度与Si在钢中的扩散系数近似符合Arrhenius指数关系。 The distribution of silicon at cross section of cathode(/mm) 20 × 20 × 0.5 sheet of 1.6Si non-oriented cold rolled silicon steel after electro-deposit treatment by NaCl-KCl-NaF-SiO2 molten salt with current intensity 50 mA/cm2,electro-deposit pulse current positive-negative ratio 9:1 at 750 850 ℃ for 60 min has been tested and the diffusion coefficient of Si is obtained by calculation.Results show that with increasing electro-deposit temperature from 750 ℃ to 85... 
2014-06-28 127 5.8

对西昌钢钒炼钢厂200 t BOF(顶底复吹)-RH-CC工艺生产50PRW800无取向硅钢RH精炼过程中主要成份进行了分析。找出了目前工艺中影响钢液质量的主要因素是钢水脱氧处理不彻底,造成加入的部分硅元素烧损。操作工艺改为铝的脱氧即合金化操作一步完成,保证了钢水中氧处于一个较低的范围,从而减少对硅元素的烧损,提高合金收得率。 The factors of BOF-RH-CC process affecting the compositions of liquid steel were systematically investigated and studied of Xichang Steel and Vanadium Company. The main factors affecting the steel cleanliness were picked out. All results showed that the loss of silicon elements resulting from the deoxidization of liquid steel was not completely. It was suggested that the addition of aluminum for deoxidizing and alloying of molten steel was executed as one step in order to lower the oxygen potent... 
2014-03-28 118 5.8

选用Q235和Q345钢,在纯锌浴和含钛量分别为0.05%、0.10%、0.15%、0.20%(质量分数)的合金浴中浸镀0.5、1、3、5、8 min。利用扫描电子显微镜和能谱仪研究了钛对热浸镀锌组织和生长动力学的影响,并提出钛对含硅钢铁锌反应抑制作用的机理。结果表明:钛的加入缩短了Γ的孕育期,促进了合金层中δ的生长和ζ的消失,δ的生长依然受扩散控制,呈抛物线生长规律;Zn-0.05%Ti锌浴可以很好的抑制高硅钢的硅反应性;含硅钢热浸镀锌钛合金浴时,在锌浴中会形成锌铁钛三元T相,该相能吸收ζ晶界处富集的硅,从而抑制了铁锌反应。 Both Q235 and Q345 steels were immersed for 0.5 to 8 min in Zn bath with different amount of Ti,ranging from 0 to 0.20 mass%,for galvanization.The effect of Ti in Zn bath on microstructure and growth kinetics of hot-dip galvanizing coatings on the two steels were investigated by means of SEM and EDS analysis.Base on the experiment,the mechanism of Ti additions in controlling Fe-Zn reaction was proposed.The results show that addition of Ti in the zinc bath decreases the incubation time of Γ phase... 
2013-09-28 112 5.8

本实用新型涉及一种硅钢冲压片质量筛查分拣装置,包括:第一组传送带机构,第一摄像头,设置于第一组传送带机构的上方,用于对硅钢冲压片的第一表面的残损进行检测;第一机械手机构,设置于第一组传送带机构的上方且位于所述第一摄像头的后方;翻转装置,设置第一组传送带机构的后方,用于对第一组传送带机构传输的初检良品进行翻面并将翻面后的初检良品传输给第二组传送带机构;第二组传送带机构,设置于翻转装置的后方;第二摄像头,设置于第二组传送带机构的上方,用于对硅钢冲压片的第二表面的残损进行检测;第二机械手机构,设置于第二组传送带机构的上方且位于第二摄像头的后方。本实用新型可高效的检测每一个产品的外观质量。
2021-08-16 84 6.8

本实用新型公开了一种硅钢卷上料装置,包括两支撑台和设置在两支撑台之间的输送组件,所述输送组件包括轨道和设置在轨道上的输送件,所述输送件包括滑板、支撑板、承重板和气缸,所述轨道平行于两支撑台设置在两支撑台之间,所述滑板可滑动设置在轨道上,所述支撑板通过气缸可升降设置在滑板上,所述承重板设置在支撑板上,所述承重板的截面呈U型,其上设置有第二缓冲条。其可实现硅钢卷的轻松上料,省时省力的同时,安全性大大提高。
2021-12-20 123 6.8

本发明涉及硅钢片切片领域,具体涉及一种硅钢片自动切片设备,包括下拉机构、推料机构、硅钢片输送机构、硅钢片推动机构、压片机构、导料壳、两个斜切机构、连接机构和三角切边机构,该硅钢片自动切片设备,通过移动连接机构,使得该设备能够进行两种硅钢片的切割加工,使得该设备能够满足多种硅钢片的加工,通过在移动三角切边机构和斜切机构的位置,使得该设备能够加工出各种硅钢片,且能够单一旋转加工那种硅钢片,并且一次加工出两张硅钢片,通过硅钢片输送机构带动推料机构进行同时运动,避免两个硅钢片之间叠起,当原料与推料机构的端部接触时,由于推料机构的拉动速度比硅钢片推动机构的速度快,避免原料上发生褶皱而影响切割的位置。
2021-10-31 130 6.8

本实用新型公开了一种硅钢片组扣件自动压平装置,包括:定位单元,定位单元包括转盘、校位板和第一驱动组件,第一驱动组件连接并驱动校位板沿竖直方向运动,校位板滑动连接有第一校位柱,第一校位柱相对转盘偏心布置;第一推送单元,位于转盘的一侧,第一推送单元包括第一推送气缸和第一推块,第一推送气缸连接并驱动第一推块沿水平方向运动;冲压单元,位于转盘背离第一推送气缸的一侧,冲压单元包括第二驱动组件和冲压柱,第二驱动组件连接并驱动冲压柱沿竖直方向运动。转盘、校位柱和第一驱动组件配合,周向定位硅钢片组,再通过冲压柱将凸出于硅钢片组的扣件压平,完成硅钢片组的整形,整体更为美观,方便后续的装配使用。
2021-10-22 109 6.8

本发明公开了一种硅钢高温加热炉用铬基高氮合金垫块及其制备方法,所述合金垫块含有Cr、Mo、N、La、Ce和Fe,不含有钨;所述合金垫块在高温抗氧化性能和高温抗蠕变性能上,优于现有技术的铬铁合金;本发明可以优化替代现有的硅钢高温加热炉用铬铁合金垫块,满足硅钢在加热炉中的加热需求,大规模工厂化生产,拥有极高的使用价值和广阔的应用市场。
2021-07-08 104 6.8