钢厂
CN202022991890.0一种新型的去角硅钢片
本实用新型提供了一种新型的去角硅钢片,包括硅钢片本体,所述硅钢片本体包括叠放区和防护区,所述硅钢片本体设有防护结构,所述防护结构包括叠放区上设有的多个均匀分布的降噪凹槽,所述防护区上下两端分别设有多个防护条,且两两防护条之间设为连接槽,每个所述防护条皆包括与硅钢片本体连接的防护层和减震层,所述防护区底部两侧分别设有减震柱,所述防护区中间设有贯穿孔,所述贯穿孔内设有绝缘螺栓。本实用新型能降低噪音和减少震动影响,从而避免使得变压器寿命及功能性降低。
双辊连铸法制备硅钢薄带的组织和性能
采用双辊连铸工艺制备了硅的质量分数分别为0.5%,1.0%,3.0%,4.5%的硅钢薄带,用光学显微镜观察其组织,并研究了后处理工艺对薄带组织和性能的影响。结果表明:硅含量为0.5%和1.0%的薄带适合采用一次冷轧+850~950℃退火的后处理工艺,而硅含量在3.0%以上的薄带适合采用二次冷轧+950℃退火的后处理工艺;硅含量为3.0%和4.5%的薄带在冷轧并950℃退火后,其磁性能最佳,铁芯损耗约为4.30 W·kg-1,磁感应强度约为1.68T。 Silicon steel thin strips with silicon content of 0.5wt%,1.0wt%,3.0wt%and 4.5wt%were prepared by twin-roll continuous casting process,and the microstructure of the strips were observed by means of optical microscopy,and on the basis,the effect of post-treatment process on microstructure and properties of the strips was studied.The results show that the post-treatment process of one-time cold rolling and annealing between 850—950℃was suitable for the strips with silicon content of 0.5wt%and 1.0wt...
CN202110111527.1硅钢卷取机卷筒结构
本发明涉及卷取领域,具体涉及硅钢卷取机卷筒结构,包括机架、收卷辊和按压捆绑机构,按压捆绑机构位于收卷辊一侧,按压捆绑机构包括按压单元和捆绑单元,捆绑单元包括捆绑辊、转动辊、成卷的胶带和两个滑块,两个滑块均滑动设置于机架上,滑块的下端固定有能与机架相抵的下卡块,捆绑辊固定设置于两个滑块之间,捆绑辊上设有凹槽;按压单元包括两个按压部,每个按压部包括按压管和弹簧,按压管通过弹簧与凹槽的侧壁连接,转动辊设置于按压管内,成卷的胶带套设于转动辊上,凹槽的侧壁设有供胶带通过的通槽。采用本技术方案时,有利于避免成卷的硅钢卷松动且能对硅钢卷进行捆绑。
退火工艺对普通取向硅钢初次再结晶组织的影响
为研究退火工艺对普通取向硅钢初次再结晶组织的影响,对经不同温度、保温时间和升温速率退火后的材料组织进行了分析。结果表明:在等温退火条件下,加热至600℃时开始发生初次再结晶,800℃以上初次再结晶组织发展完善;而在最终冷轧板直接进行最终高温退火的情况下,加热温度在500~700℃时,将升温速率提高到80℃/h,初次再结晶组织更易于发展完善。 To investigate the influence of annealing process on the recrystallization of common grain oriented silicon steel,microstructures of sheets annealed at different temperature,soaking time and heating rate are observed.Results show that under the condition of isothermal annealing,recrystallization begins at 600℃ and fully develops above 800℃,while in the case that the final cold rolled sheets are directly thrown to final high temperature annealing,recrystallization is likely to develop with the he...
硅钢高温氧化铁皮的显微结构表征
利用电子探针面分析、状态分析及电子背散射衍射相分析技术研究硅钢高温氧化铁皮的显微结构。电子探针面分析可以直观的看出元素的分布状态,初步判断氧化铁皮的结构,而状态分析可以准确表征常规氧化铁皮中铁元素的状态,对于合金元素富集区域则通过电子背散射衍射相分析技术来标定。结果表明,高温氧化铁皮的结构主要有4层,即最外层为厚度约为10μm的Fe2O3相,次外层为Fe3O4相,中间层为FeO相上分布有颗粒状的Fe3O4相,最内层为FeO相和Si元素富集的Fe2SiO4相。其中Fe2SiO4层的分布特征与加热温度密切相关:1 100℃时,Fe2SiO4相呈颗粒状,弥散分布在FeO层;1 200℃时,Fe2SiO4相呈液态,侵入基体和疏松的FeO层,且沿着FeO晶界呈网状分布。 The microstructure of high temperature oxide scale on silicon steel was characterized by electron probe microanalyzer(EPMA)mapping analysis,state analysis and electron backscatter diffraction(EBSD)phase analysis.The element distribution and the initial structure of the oxide scale could be detected by EPMA mapping analysis apparently.And the state of iron in the conventional oxide scales could be determined by state analysis.Meanwhile,the alloy-rich region could be identified by EBSD phase analy...
CN202123227418.0一种铁芯硅钢片卷材的自动放卷上料装置
本实用新型公开了一种铁芯硅钢片卷材的自动放卷上料装置,包括放卷机、导向平台和防折组件,所述导向平台间距设置在放卷机的下方,所述导向平台与放卷机之间构成供料带缓冲的缓冲空间,所述料带在缓冲空间内呈U型状走向,所述导向平台的上方间距设置有防折组件,所述防折组件与导向平台之间构成供所述料带通过的导向通道,所述防折组件设置在料带的内弯侧。通过防折组件对料带的内弯侧进行支撑,能够有效的防止料带被过度弯折,能够对料带进行缓冲和缓冲保护,保证料带放卷上料的稳定性。
CN202110627061.0电工钢及其制备方法
本申请提供一种电工钢及其制备方法,制备方法包括:将电工钢的板坯进行热轧获得钢卷;将热轧后的钢卷进行酸洗冷轧;将酸洗冷轧后的钢卷进行第一次罩式退火;将第一次罩式退火后的钢卷进行平整;将平整后的钢卷进行第二次罩式退火;将第二次罩式退火后的钢卷进行重卷,以获得电工钢。本申请提供的电工钢的制备方法采用两次罩式退火,退火的主要目的是消除酸洗冷轧工序产生的加工硬化,使钢板充分再结晶,获得理想的铁损及磁感应强度。而采用两次罩式退火,相对于一次罩式退火工序来说,能够进一步降低铁损,提高电工钢的磁性能。
CN202023339783.6一种利于常化的硅钢缝合结构
本实用新型属于硅钢片加工技术领域,具体涉及一种利于常化的硅钢缝合结构,包括上层硅钢片、下层硅钢片和连接带,下层硅钢片的一端位于上层硅钢片的下方并与上层硅钢片叠合,上层硅钢片和下层硅钢片的叠合处开有多个排成直线的桥型孔,连接带依次穿过各个桥型孔并同时卡合在上层硅钢片和下层硅钢片上。本方案中,在上层硅钢片和下层硅钢片的叠合处开设桥型孔,利用连接带穿过上层硅钢片和下层硅钢片叠合处的桥型孔,相当于利用连接带将上层硅钢片和下层硅钢片缝合在一起,这样设置能够较好将上层硅钢片和下层硅钢片连接成一体。
CN202122410654.X一种便于清洗的冷轧硅钢生产用轧机
本实用新型提供了一种便于清洗的冷轧硅钢生产用轧机,两个所述支架安装在底座上,所述支架上设有安装盖,支架之间设有上支撑辊,上支撑辊下设有上工作辊,上工作辊安装在支架之间,上工作辊下设有下工作辊,这种便于清洗的冷轧硅钢生产用轧机,在使用的时候,可以对于冷轧硅钢进行生产处理,生产之后可以进行清洗设备,安装的上工作辊与下工作辊可以对于硅钢进行冷轧处理,在工作时,两侧安装的承重块可以对于机械进行一个固定,起到稳固作用,两侧安装的转动辊可以放置硅钢,安装的清洗头可以对于机械进行清洗,吹风器可以对于机械进行干燥处理,防止机械生锈,底座上安装的沥水板可以隔断灰尘和铁屑,防止堵塞。
CN202080097262.8电工钢板粘接涂料组合物、电工钢板层叠体及其制造方法
根据本发明的一个实施例的粘接涂料组合物,其包含聚乙烯丙烯酸酯,所述聚乙烯丙烯酸酯包含由以下化学式1表示的重复单元和由以下化学式2表示的重复单元,所述聚乙烯丙烯酸酯包含65至90重量%的由以下化学式1表示的重复单元、10至35重量%的由以下化学式2表示的重复单元。
CN202180018973.6电磁钢板的加工方法、马达以及马达铁芯的制造方法
本发明相对于板厚较薄的电磁钢板提供不会导致磁特性劣化的基于激光的加工方法。在对电磁钢板进行使用激光的熔断并将该电磁钢板加工成规定的形状的电磁钢板的加工方法中,使上述激光的扫描速度成为10000mm/min以上来进行上述熔断。