对w(Si)=3%无取向硅钢进行表面机械研磨处理(SMAT)和异步轧制(CSR),获得表面纳米结构,再进行550~650℃、4 h固体粉末渗硅处理,用透射电镜(TEM)、扫描电镜(SEM)和X射线衍射仪(XRD)研究表层组织演变。结果表明:经过SMAT后,w(Si)=3%无取向硅钢表面形成了等轴状、取向呈随机分布的、晶粒尺寸为10 nm的纳米晶组织;异步轧制后,表面纳米晶组织保持不变;550~650℃、4 h渗硅处理后,SMAT+CSR样品表面形成化合物层,其厚度随着温度的升高由17μm增加到52μm;化合物层由Fe3Si和FeSi相组成. Nanostructured surface layer was fabricated on a 3%(mass fraction) non-grain oriented silicon steel by means of surface mechanical attrition treatment(SMAT) and cross-shear rolling(CSR),and then a solid powder siliconizing treatment was carried out for the SMAT+CSR sample at 550~650 ℃ for 4 h.The microstructural evolution was examined by using transmission electron microscopy(TEM),scanning electron microscopy(SEM) and X-ray diffraction(XRD).Experimental results show that: equiaxed nanocrystallin... 
2011-03-28 166 5.8

本实用新型公开了一种高磁感低铁损取向硅钢生产用切割装置,包括激光切割台,所述激光切割台上端滑动连接有一个滑动导轨,所述滑动导轨上滑动连接有一个切割主机,所述激光切割台上端且与切割主机相对应位置均匀固定连接有一组锯齿板,所述激光切割台上端且与锯齿板相对应位置活动连接有一个升降板,所述升降板上且与锯齿板相对应位置均开设有一个穿孔,所述升降板上端均匀转动连接有一组滚珠,本实用新型的有益效果是:通过螺纹杆的转动,可以使螺纹套和滑动块滑动,从而利用连接转杆的传动,可以将升降板顶起,使待切割的板材可以在滚珠上滑动,方便对板材位置的调节,并且将升降板下降后,不会影响板材的正常切割。
2021-12-23 215 6.8

一种低温高磁感取向硅钢的热轧方法:经转炉冶炼并浇注成坯;对铸坯加热后进行粗轧:首先确定粗轧减宽量;根据所确定的粗轧减宽量进行粗轧;进行精轧;常规进行下工序。本发明采用低温板坯加热技术,降低了板坯烧损和修炉负担,且边裂发生率比现有技术的不低于18%的基础上能降低5%以上,由此节约资源及降低能耗。
2021-12-31 315 6.8

本实用新型公开了一种变压器铁芯硅钢片的堆叠装置,包括底座、摆动机构、摆动板和垫高倾板,所述底座上设置有摆动机构,所述摆动板的一端铰接设置在底座上,且所述摆动板间距于摆动轴线的板体与摆动机构对应设置,所述摆动机构驱动摆动板在竖向面内进行往复摆动,所述垫高倾板间距于摆动板设置在底座上,且所述垫高倾板与摆动板之间构成用于叠放硅钢片的叠放区,所述叠放区的底部呈高低倾斜设置,且所述叠放区的低端侧朝向于摆动板,能够使得硅钢片的收集简单,且十分整齐。
2021-12-30 317 6.8

提出以“云边一体化架构”构建硅钢智慧决策系统,来解决原硅钢制造L1~L5系统架构模式下的数字信息孤岛、业务功能割裂等问题。在此基础上,开发了云边协同的自学习型控制模型及业务决策模型,构建起硅钢“智慧大脑”,形成了以研发、制造、服务等核心业务数字化融合的智能化决策支持新模式,探索出一条钢铁制造业数字化、智能化转型之路。 SIDS(Silicon-steel Intelligent Decision-making System)based on \"cloud-edge integration architecture\" was proposed to solve the problems of data silos and business function fragmentation in the original L1~L5 system architecture.On this basis,the self-learning control model and decision-making model of cloud-edge collaboration were developed,the \"smart brain\" of silicon steel department was constructed,and a new intelligent decision-making support model of digital integration of core businesses s... 
2022-02-28 213 5.8

无取向硅钢中夹杂物的存在会抑止晶粒生长,使基体的均匀连续性中断,其在钢中的形态、含量及分布情况都不同程度影响着硅钢的性能,尤其是对磁性能起关键的作用。因此,全尺度分布考察夹杂物对无取向硅钢夹杂物的研究极为重要。本实验确定了适用于不同牌号无取向硅钢夹杂物全尺度分布的分析方法:样品制备—小样电解—过滤喷金—根据不同牌号的要求选择合适的放大倍率扫描观测—夹杂物颗粒的分类统计。通过统计的结果,结合电解的失重量可以得到不同尺度的体积分布数据。实验分析了不同牌号和工艺无取向硅钢夹杂物的种类、形貌、大小和尺度分布,并初步考查了夹杂物与磁性能的关系,对无取向硅钢的工艺研究具有一定参考价值。 Inclusions in non-oriented silica steel could inhibit the growth of grain and cause discontinuity of micro-structure.The configuration,content and size distribution of inclusion have different effects on the performance of silica steel,especially significant on the magnetic property.Therefore,it is very useful to completely characterize inclusions with full size distribution in silica steel.In our research,full size analysis method for inclusion in silica steel had been established as follows: s... 
2012-10-28 178 5.8

本发明特别涉及一种控制边部质量的低牌号无取向硅钢的热轧生产方法,属于无取向硅钢热轧生产技术领域,方法包括:将低牌号无取向硅钢的板坯进行第一次粗轧,将第一次粗轧后的板坯进行第二次粗轧,其中,在第二次粗轧机前的立辊上设置立辊润滑装置,所述立辊润滑装置向所述立辊供给的润滑油的油量为100mL/min‑400mL/min;将第二次粗轧后的板坯进行精除鳞、精轧和卷取,获得边部质量合格的热轧卷;保证良好的立辊辊面状态,可有效解决边部粗糙,有效解决了低牌号无取向硅钢边部粗糙状态,极大的提高了冷轧后工序毛边轧制率,提高了硅钢全工序成材率。
2021-07-28 162 6.8

采用光学显微镜和X射线衍射仪研究了常化退火处理对无取向硅钢热轧板和成品退火板显微组织和织构的影响。结果表明:常化退火处理消除了热轧板中的变形组织,促使变形晶粒完成再结晶;常化退火处理使高斯织构和立方织构易通过再结晶在变形带内形核和长大,可显著降低成品退火板的{111}和{112}不利织构组分的占有率,提高{100}和{110}有利织构组分的占有率,从而有利于提高无取向硅钢成品板的磁性能。 The effect of normalizing annealing treatment on microstructure and texture of non-oriented silicon steel hot rolled plates and final products were investigated by means of optical microscope and X-ray diffractometer analysis.The results show that the deformed microstructure of the hot rolled plates transformed into recrystallized grain after normalizing annealing treatment.The grains of Goss texture and cubic texture crystallographic orientation were formed and grown by recrystallization in the... 
2013-02-28 202 5.8

本发明涉及一种硅钢片铁芯用自动叠装系统,托板、上料单元、精定位单元、叠装单元、抓取单元,所述上料单元有一个,位于中部位置,所述精定位单元一共有两个,分别位于上料单元的两侧,所述叠装单元一共有两个,分别位于两个精定位单元的两侧,从而使得整个自动叠装系统由中间向两侧方向均依次为上料单元、精定位单元、叠装单元。本发明的优点在于:通过对上料单元、精定位单元、叠装单元的数量及排布位置进行重新设计,采用由中间向两侧供料的方式,使得两侧的上料顺序均独立运行,不存在相互干涉的风险,确保单侧的上料顺序的顺利进行,相对应的也就降低了程序设计的复杂程度,减轻了设计人员的工作强度。
2021-06-30 168 6.8

介绍了CSP工艺生产无取向电工钢各工序的设备特点、采用的工艺控制手段和电工钢产品质量情况,结合生产实践证明了马钢CSP工艺开发的无取向电工钢产品丰富了薄板坯连铸连轧的品种结构,发挥了薄板坯连铸连轧生产无取向电工钢性能均一、稳定的特点。 The equipment characteristic,the process control method and the quality of non-orientated silicon steel by CSP process were introduced.Combined with the production situation,it is proved that production of non-orientated silicon steel developed on Masteel CSP line would enrich product structure of thin slab continuous casting and rolling,and it exerts stable performance of non-orientated silicon steel. 
2013-06-28 191 5.8

本实用新型涉及一种硅钢切边重卷机组,包括依次衔接布置的开卷机、入口穿带装置、入口转向夹送辊、入口剪、切边单元、出口转向夹送辊和卷取单元,所述切边单元包括沿带钢运行方向依次衔接布置的切边夹送辊、入口稳定辊、切边剪和出口稳定辊,所述切边剪的废料出口侧衔接布置有碎边剪,所述碎边剪的废料出口侧配置有切边废料输出装置。本实用新型提供的硅钢切边重卷机组,采用切边剪+碎边剪的组合对带钢进行切边操作,避免了传统的废边卷取方式,能较好地适用于硅钢切边操作。采用切边夹送辊与入口稳定辊和出口稳定辊配合,能显著地提高切边操作时带钢运行稳定性以及保证带钢切边质量,可相应地提高生产效率。
2021-02-22 157 6.8

采用电子背散射衍射技术测定50SW1300冷轧无取向硅钢中不同尺寸范围晶粒的含量,利用主成分回归分析法,综合研究不同尺寸范围晶粒的含量对无取向硅钢磁性能的影响。结果表明:通过主成分回归分析法能够从不同尺寸范围晶粒的含量的多个影响因素中获取主要的因素,定量研究它们对无取向硅钢磁性能的影响规律。分析表明,无取向硅钢的铁损与不同尺寸范围晶粒的含量之间存在着可靠的多元线性关系,在一定范围内,较大尺寸晶粒的含量越多,其对铁损优化的作用越明显;而无取向硅钢的磁感与不同尺寸范围晶粒的含量之间并无线性关系。 Distribution of grain size in cold rolled non-oriented silicon steel 50SW1300 was measured by EBSD.The effects of the distribution of grain size on magnetic properties of the non-oriented silicon steel were comprehensively researched by means of principal component regression method.The results indicate that the main factors influencing the magnetic properties in the distribution of grain sizes,which can be used to guantitative study the magnetlic properies of the steel,are obtained by principal... 
2014-11-28 198 5.8