所有分类
  • 所有分类
  • 未分类

本发明涉及一种硅钢片纵剪边料收卷装置,包括:用于将收卷装置固定于地面的机架底座,机架底座一端设置固定支架,固定支架上安装电动定尺收料盘;在机架底座上设置电动可移动支架,电动可移动支架在机架底座的长方向上相对固定支架移动,电动可移动支架上安装电动可调收料盘;电动可移动支架、电动定尺收料盘、电动可调收料盘与PLC控制系统连接,PLC控制系统用于控制电动可移动支架的移动距离、以及控制电动定尺收料盘和电动可调收料盘的收料速度。本发明还涉及一种硅钢片纵剪边料收卷方法。将本发明的收卷装置安装在硅钢片滚剪线切刀后面的输送平台下部,卧式布局,不占用外部空间,和滚剪线无缝集成在一起,自动完成硅钢片纵剪边料收卷工作。
2021-01-11 153 6.8

变压器D21硅钢铁芯片采用冲压工艺生产。首先对其工艺进行了分析,确定了冲压方案。对产品进行了排样设计,计算了冲压力,确定了压力中心。然后,设计了单工序落料模具,完成了模具装配图。 D21 silicon steel chips for transformer are produced by stamping.First,its stamping process was analyzed and the scheme of the stamping process was determined.The product layout was designed,the punching pressure was calculated,the pressure center was determined.Then,the blanking die with single procedure was designed,the die assembly drawing was completed. 
2013-07-28 118 5.8

本发明公开了一种生产高表面质量镀铝硅钢带的方法,属于连续热浸镀铝硅技术领域。本发明的生产高表面质量镀铝硅钢带的方法,包括酸洗、冷轧、清洗、连续退火、热浸镀铝硅和冷却处理,所述冷却包括预冷段和强冷段,其中预冷段是通过预冷风机将带钢温度冷却至620~630℃,强冷段包括三段强冷,三段强冷采用水雾冷却,且控制强冷段冷却速率≥30℃/s。本发明通过控制钢带表面粗糙度、清洗质量、退火炉气氛、气刀参数以及镀层结晶控制器参数,可以有效控制铝硅产品表面结晶尺寸、减少漏镀等典型缺陷,生产出高表面镀铝硅钢带。
2021-08-18 139 6.8

本实用新型涉及一种用于叠装变压器铁芯硅钢片的装置,包括托板,托板的上表面固定设置有固定板,固定板的内部开设有沉槽;双向螺纹杆,双向螺纹杆设置在固定板的内部,双向螺纹杆的一端贯穿固定板的侧壁并连接有把手;支撑柱,支撑柱的表面开设有连接槽,连接槽的内部铰接有连接杆;有益效果为:本实用新型提出的一种用于叠装变压器铁芯硅钢片的装置在托板的左右两侧设置有两组对称分布的固定板,通过对双向螺纹杆的旋转,螺接在双向螺纹杆表面的两组滑块将会相对移动,铰接在滑块上表面的两组支撑柱将会形成三角形对铁芯进行防护。
2021-12-06 165 6.8

研究了CSP工艺流程生产的硅含量为1.5%的无取向电工钢在不同常化温度下对磁性能的变化。研究结果表明:随着常化温度的提高,热轧板的晶粒尺寸增大,且组织均匀性提高;此外成品的有利织构组分{100}<0vw>、α、η增强,不利织构组分减弱;铁损P1.5/50呈下降趋势,磁感B50上升平缓。在常化工艺为970℃×2.5min下,对应的铁损P1.5/50<3.4W/kg,磁感B50>1.74T。 The effect of normalizing temperature on the magnetic properties of non-oriented electrical steel containing 1.5%silicon produced by CSP process was studied.The results show that with increasing normalizing temperature,the average grain size of hot-rolled plate increases and the microstructure uniformity is improved.Furthermore,the texture components of finished products are improved through enhancing of{100}<0vw>,αandηtextures and weakening of{111}<112>texture;the core loss P1.5/50 ... 
2014-03-28 161 5.8

结合扫描电镜和大样电解研究了CSP流程W800牌号无取向电工钢表面线状缺陷中夹杂物成分及来源,采用SPSS软件回归分析了生产过程各因素对表面线状缺陷的影响。研究表明:稳态浇铸过程铸坯中大型夹杂物含量为5.39 mg/10 kg。引起无取向电工钢表面线状缺陷的大型夹杂物主要为脱氧产物、镁铝尖晶石和钢包顶渣,主要类型为Al2O3、MgO-Al2O3、CaO-Al2O3-MgO和CaO-Al2O3-SiO2。非稳态浇铸过程钢水洁净度明显降低,热轧板表面线状缺陷比例上升。影响表面线状缺陷的主要因素为RH出站时顶渣的w(CaO)/w(Al2O3)、RH脱氧结束氧位及中间包最低吨位。 Combining scanning electron microscopy and large sample electrolysis, the composition and source of inclusions in the surface linear defects of W800 grade non-oriented electrical steel in the CSP process were studied. SPSS software was used to regress and analyze the main factors which affected the surface linear defects in the steelmaking process. Research shows that the content of large inclusions in the steady state casting process is 5.39 mg/10 kg. The large inclusions which cause linear def... 
2022-02-28 215 5.8

借助于EBSD对比研究了常化退火对高牌号无取向电工钢热轧组织和织构演变的影响,分析了常化退火对热轧板各厚度层织构的演变规律。结果表明,常化退火改善了热轧组织的均匀性,并弱化了热轧变形的γ纤维织构。升高常化退火温度,可增大热轧板的晶粒尺寸,提高{100}和{110}织构组分占有率,有利于提高无取向电工钢成品板的磁性能。 Effects of normalizing annealing on microstructure and texture of high-grade non-oriented electrical steel hot-rolled sheet were investigated by EBSD. Emphasis was put on the effects of normalizing annealing on texture evolution in the sheet thickness. The results show that the hot-rolled microstructure homogeneity is improved and the γ-fiber texture is weakened by normalizing annealing treatment. The grain size of hot-rolled sheet and intensity of the {100} and {110} favorable texture can be in... 
2014-02-28 160 5.8

【作者】 吴玉美; 陆晔; ...
2023-05-09 204 5.8

本申请实施例公开了一种硅钢片卷绕机调节装置,包括底部支撑座,所述底部支撑座一侧的内部活动套接有伸缩调节板,所述伸缩调节板的上部固定连接有上部定位套,所述上部定位套内部的上端活动套接有第一定位板,所述上部定位套的内部安装有第一螺纹定位杆。该硅钢片卷绕机调节装置,通过带动硅钢片夹持在上下两个夹持板之间,即可带动夹持板之间的挤压力,带动硅钢片两侧位置进行限定,避免硅钢片收卷时出现振动和偏移的问题,同时装置夹持板的内部活动套接有滚轮,即可在硅钢片移动过程中,可带动滚轮旋转,即可带动硅钢片与滚轮之间的摩擦阻力降低,至此可带动硅钢片移动时的灵活性,避免硅钢片移动时出现卡死的问题。
2021-12-15 186 6.8

一种使铋收得率不低于70%的含铋取向硅钢冶炼方法,其步骤:常规转炉冶炼并出钢至钢包中;RH精炼处理,其间:控制渣层厚度不低于45mm,且渣成分在:Al2O3:25~35wt%,CaO:40~50wt%,MgO:10~15wt%,且结束时钢水温度控制在1530~1590℃;真空精炼结束后进行镇静;后将铋颗粒与石灰石颗粒混装容器加入钢水中;保护浇注和后工序生产。本发明将铋颗粒与石灰石颗粒混合加入,石灰石在钢液中分解产生的气体不仅可以减缓铋颗粒下沉速度,使铋能够快速扩散均匀,更主要的是还可以强化铋颗粒在钢液中的扩散,最终可获得铋收得率高于70%即在71~75%的理想效果。
2020-12-22 186 6.8

本实用新型公开了一种防护性能好的硅钢板带加工用卷曲设备,包括底座,所述底座的上表面固定连接有L型安装架,所述L型安装架的一侧固定设有第一电机,所述第一电机的输出端固定连接有第一转轴,所述第一转轴的外表面沿周向等间距设有多组可调卷绕机构,所述第一转轴的一侧设有驱动调节机构。本实用新型通过设置可调卷绕机构及驱动调节机构,硅钢板带卷绕完成后,第二电机带动主动齿轮转动,主动齿轮带动从动齿轮及第二转轴转动,从而两个移动块相互远离带动连杆转动,两个连杆转动带动弧形板向靠近第二转轴的方向移动,从而使弧形板脱离钢带卷的内圈,便于将钢带卷取下,防止工人用力操作过程中划伤。
2021-08-11 172 6.8

本实用新型公开了一种新型取向硅钢薄板,所述硅钢薄板包括薄板主体,薄板主体呈方形,薄板主体的内部具有硅钢基板,所述薄板主体的上部具有耐磨层,耐磨层底部还具有抗压层,耐磨层具有若干均匀分布的耐磨条,耐磨层之间分别等距间隔布置,间隔的耐磨条之间形成透气槽,透气槽具有两个侧边,透气槽底部具有透气通孔,所述透气槽两侧具有导风侧凸条,导风侧凸条具有根部和端部,根部分布在透气槽的底部左侧和右侧位置,所述端部延向透气槽两侧边部上部,所述耐磨条为均匀排列的若干双V型结构,双V型结构纵向排列,耐磨条和抗压层之间具有硬质包覆层,在不影响耐磨作用的前提下能够起到透气通风的效果,不需要增加硅钢薄板的厚度。
2021-06-24 155 6.8

站点公告

网站试运行,请大家关注本站公众号,多提宝贵意见!

显示验证码
没有账号?注册  忘记密码?