钢厂
修正GTN模型及其在预测硅钢冷轧边裂中的应用
考虑剪应变对微孔洞损伤演化的影响,对GTN损伤模型的损伤演化机制进行修正,建立了适用于不同应力三轴度水平的损伤模型。结合隐式应力更新算法和显式有限元计算,采用VUMAT子程序实现了修正GTN模型在有限元软件ABAQUS中的数值计算。通过模拟纯剪切和剪切-拉伸两组试样的损伤演化和断裂行为,验证了修正GTN模型在不同应力三轴度承载条件下的有效性。运用修正GTN损伤模型模拟含边部缺口的带钢在轧制过程中裂纹的萌生和扩展行为,模拟结果与实验相一致,表明该模型可有效地用于带钢缺陷在轧制过程中扩展行为的分析和预测。模拟和实验结果表明,带钢边部缺口在轧制过程中,缺口前沿和后沿均会萌生裂纹,且后沿裂纹扩展更为明显。 Considering the effect of shear strain of micro-void on damage evolution, a modified GTN model applicable to various stress triaxiality conditions is proposed by modifying the damage evolution mechanism of the GTN damage model. The modified model is implemented in commercial finite element software ABAQUS by combining the implicit stress update method with an explicit finite element solving algorithm and through the user-defined material subroutine VUMAT. The damage evolution and the failure pro...
CN202023147451.8一种带缓冲保护装置的硅钢片纵剪线
本实用新型公开了一种带缓冲保护装置的硅钢片纵剪线,包括工作台,工作台的顶部外壁设置有放料辊,工作台靠近放料辊的一侧设置有牵引辊,工作台靠近牵引辊的一侧设置有整平机构,工作台的内部设置有第一缓冲坑,第一缓冲坑的顶部设置有导料辊,第一缓冲坑的内部设置有第三转轴,第三转轴的外壁传动连接有皮带,皮带的内壁传动连接有第二转轴,皮带的外壁传动连接有第一转轴,第三转轴的外壁固定安装有转筒,转筒的外壁设置有伸缩杆,伸缩杆的外壁套接有弹簧,伸缩杆的底部设置有滚珠,通过设置的第一缓冲坑与第二缓冲坑结构,可防止硅钢片在进入第一缓冲坑与第二缓冲坑时弯曲程度过大导致的断裂,且双重的缓冲装置更有利于对硅钢片的保护。
CN202110964795.8一种电机定子硅钢片叠片工装平台
本发明涉及电机生产技术领域,特别涉及一种电机定子硅钢片叠片工装平台,包括底板、放置板、整齐装置和清理装置,所述的底板上端通过支撑柱安装有放置板,放置板上端安装有整齐装置,放置板上设置有清理装置;本发明可以解决现有的工装平台在针对多个硅钢片进行叠片时,只能对一种尺寸的硅钢片进行叠片,不能根据硅钢片的直径和硅钢片上间隔孔的宽度进行相应的调节,因此不能实现对不同尺寸的硅钢片进行整齐的功能,降低了工装平台使用的灵活性问题。本发明所采用的整齐装置在一定范围内可以根据硅钢片的直径进行相应的调节,从而实现对不同尺寸的硅钢片进行整齐的功能,提高了工装平台使用的灵活性。
CN202121481825.1变压器铁芯硅钢片打磨设备
本实用新型涉及板材加工设备领域,具体为变压器铁芯硅钢片打磨设备,包括本体,本体内部开设有工作腔,本体内部设置有用于运输硅钢片的运输机构,本体内部设置有用于打磨硅钢片的打磨机构,本体内部设置有用检测硅钢片边缘整洁程度的检测机构,本实用新型通过运输机构和打磨机构进行配合从而对硅钢片进行去除毛刺和毛边,从而保证铁芯中每组硅钢片均不直接接触;通过检测机构对加工完成的硅钢片进行毛刺和毛边的检测,进一步保证了每组硅钢片的整体质量以及尺寸的精准。
CN202110288598.9一种取向硅钢热轧钢带的板形控制方法
本发明涉及一种取向硅钢热轧钢带的板形控制方法,所述取向硅钢热轧钢带的工艺流程包括铸坯加热过程、轧制过程及层流冷却过程;其中轧制过程中采取取向硅钢与普钢交叉轧制的方式;粗轧过程采取R1轧制1道次、R2轧制5道次的1+5轧制工艺,并控制轧制工艺参数;精轧过程中控制F1~F7轧制工艺参数。本发明通过设定合理的交叉轧制工艺及取向硅钢热轧工艺,使取向硅钢的轧制稳定性大幅提高,取向硅钢带形控制良好,凸度控制在30~50μm之内,楔形控制在30μm之内,板形平坦度控制在25iu之内;从而为冷轧工序提供了优质原料。
CN202023271356.9一种硅钢片卷料悬吊上料装置
本实用新型公开一种硅钢片卷料悬吊上料装置,包括装配架,装配架之间装配有若干个左右间隔设置的硅钢片卷料限位装置,所述硅钢片卷料限位装置用于装载硅钢片卷料、装配架包括前后对称设置的架板,所述架板上具有矩形凸出端、前、后部位之间所述矩形凸出端之间装配有若干个左右间隔设置的长螺杆、长螺杆贯穿所述硅钢片卷料限位装置,所述长螺杆的端部螺纹连接有螺母、架板的底部固定连接有两个左右间隔设置的轮架杆,所述轮架杆的左右两端均转动连接有滚轮、轮架杆之间固定连接有C形架杆,所述C形架杆上固定连接有悬吊环体,实现将大量生产加工使用的硅钢片卷料进行上料。采用上述方式不仅实现将大量生产加工需要的硅钢片卷料进行输送。
无取向硅钢磁性能提升技术进步及其发展动向
无取向硅钢的磁性能主要取决于铁素体的晶粒尺寸、晶体织构和钢中的夹杂物。通过合适的化学成分设计以及采用适宜的夹杂物控制技术,可以获得最佳的夹杂物控制效果,使其纯净度大幅度提高或者无害,最终获得磁性能优良的高级别无取向硅钢。同时,为满足节能、环保、高效需求,无取向硅钢正朝着节能降耗、环境友好以及多功能、高效率、易加工等方向发展。 The magnetic properties of non-oriented silicon steel mainly depend on the grain size of ferrite,the crystallographic texture,and the inclusions in the steel.The optimum inclusion control effects can be obtained through a suitable chemical composition design and an appropriate inclusion control technique,and then the liquid steel will get be clean or the inclusion will get be harmless,finally the excellent magnetic property of the non-oriented silicon steel can be obtained.Meanwhile,in order to ...
轧制力优化对20辊冷轧硅钢厚度精度的影响
轧制力是影响冷轧带钢厚度精度的关键因素。为实现高精度的冷轧带钢厚度控制,通过优化变形抗力模型参数和摩擦系数模型参数提高冷轧轧制力模型计算精度,并使用指数平滑法的自学习算法保证轧制力精度的稳定性。在首钢股份公司迁安钢铁公司20辊森基米尔轧机生产线进行S12硅钢钢种轧制力优化试验,将优化的模型参数应用于L2并投入现场生产,结果表明该优化方法不仅提高了轧制力设定精度,而且减小了冷轧硅钢的厚度超差长度,提高了成材率。 The rolling force is the key factor which influences the accuracy of cold-rolling strip thickness. To implement high precision control of cold-rolling strip thickness,we optimize the deformation resistance model parameters and friction coefficient model parameters to improve the calculation precision of cold-rolling force model,and use exponential smoothing self-learn algorithm to ensure the stability of rolling force accuracy. In Shougang Qiangang 20-high Sendzimir mill single stand production ...
CN202121016000.2一种冷轧取向硅钢带整平装置
本实用新型公开了一种冷轧取向硅钢带整平装置,包括两个上下对称分布的保护罩,所述保护罩的内部均转动连接有展平辊,且展平辊的一端均延伸至保护罩的外部,所述保护罩的外壁设置有传动罩,且传动罩的外壁设置有动力箱,所述动力箱与展平辊传动连接,上下两个所述展平辊之间设置有其,特征在于,所述保护罩的两侧外壁均固定连接有支撑架,且支撑架的一侧外壁均设置有延展机构,两个所述延展机构之间设置有连接架,且连接架的一侧外壁设置有吸水布,所述吸水布的内部设置有胶板。本实用新型吸水布与硅钢带本体的外壁滑动接触,以此将展平时涂抹在硅钢带本体表面的水溶性润滑剂刮抹掉,减少硅钢带本体表面上的水分。
湿H_2气氛下CGO硅钢初次再结晶织构演变行为
通过对湿H2气氛下,相同退火温度、不同退火时间的CGO硅钢初次再结晶样品进行金相组织观察,并进行了EBSD微观织构分析,研究了CGO硅钢初次再结晶过程中的组织及再结晶织构演变行为。结果表明,在湿H2气氛下,820℃保温,CGO硅钢初次再结晶过程约在120 s时完成。随着退火时间的延长,γ面上{111}<112>织构含量逐渐减少,{111}<110>织构先减少后增多,随着再结晶的完成,部分{111}<112>取向晶粒向高斯{110}<001>取向转化的同时,也向{111}<110>取向转化,高斯{110}<001>织构含量逐渐增多。高斯取向晶粒较多是由{111}<112>取向晶粒转化而来,同时也证明了CGO硅钢高斯取向晶粒的二次再结晶异常长大生长机制为择优形核。 Microstructure development and texture evolution of conventional grain oriented silicon steel,which were annealed at same annealing temperature and different annealing time under wet H2 atmosphere,were investigated through metallographic observation and electron backscattered diffraction analyzing.The results show that the primary recrystallization finishes in 120 s at 820 ℃ under wet H2 atmosphere.With the extending of annealing time,{111}<112> texture decreases,{111}<110> texture d...
CN202120063732.0硅钢片纵剪边料收卷装置
本实用新型涉及一种硅钢片纵剪边料收卷装置,包括:用于将收卷装置固定于地面的机架底座,机架底座一端设置固定支架,固定支架上安装电动定尺收料盘;在机架底座上设置电动可移动支架,电动可移动支架在机架底座的长方向上相对固定支架移动,电动可移动支架上安装电动可调收料盘;电动可移动支架、电动定尺收料盘、电动可调收料盘与PLC控制系统连接,PLC控制系统用于控制电动可移动支架的移动距离、以及控制电动定尺收料盘和电动可调收料盘的收料速度。将本实用新型的硅钢片纵剪边料收卷装置安装在硅钢片滚剪线切刀后面的输送平台的下部,卧式布局,不占用外部空间,和滚剪线无缝集成在一起,自动完成硅钢片纵剪边料的收卷工作。