钢厂
CN202110004215.0一种拉矫机矫直低牌号无取向硅钢的方法
本发明公开了一种拉矫机矫直低牌号无取向硅钢的方法,当焊缝达到拉矫机前面时,生产线的整体速度降低至28‑32m/min、拉矫机的辊系辊缝全部打开同时辊系不接触钢带、拉矫机的延伸率降到0.08%‑0.12%、拉矫机前后张力辊的压辊全部压下,焊缝通过拉矫机后,均恢复到正常水平。本发明的目的是提供一种拉矫机矫直低牌号无取向硅钢的方法,解决焊缝经过拉矫机时焊缝在拉矫机的拉伸矫直作用下发生断带的事故的问题。
微量Sn对0.4%Si无取向硅钢组织和磁性能的影响
结合实际生产0.4%Si无取向硅钢,统计了不含Sn和0.025%Sn无取向硅钢的磁性能变化,利用金相显微镜、X射线衍射仪观察分析不同成分下试样的显微组织和微观织构。试验结果表明:Sn元素可以显著降低无取向硅钢的晶粒尺寸,0.025%Sn试样的平均晶粒尺寸比不含Sn减小28.4%;加入Sn元素后抑制了无取向硅钢中不利于磁性能的{111}面织构组分强度,提高了对磁性能有利的{100}面织构组分强度,0.025%Sn与不含Sn相比磁感均值从1.756 T提升至1.768 T,铁损均值从5.476 W/kg降低至5.204 W/kg,明显改善了无取向硅钢磁性能。 In this paper combined with the actual production of 0.4% Si non oriented silicon steel, the magnetic properties of non oriented silicon steel without Sn and 0.025% Sn were counted. The microstructure and microtexture of samples with different compositions were observed and analyzed by metallographic microscope and X-ray diffraction. The results show that: Sn can significantly reduce the grain size of non oriented silicon steel, and the average grain size of 0.025% Sn sample is 28.4% smaller tha...
CN202120886491.X一种环保硅钢绝缘涂生产加工用灌装装置
本实用新型涉及硅钢绝缘涂料生产技术领域,尤其为一种环保硅钢绝缘涂生产加工用灌装装置,包括底座,所述底座的顶端右侧固定连接有支架,所述支架的顶端内侧固定连接有加料管,所述加料管的底端外侧连通有电磁阀,所述支架的右端固定连接有控制器和报警灯,本实用新型中,通过设置的报警灯、加料管、储存桶、限位轴、弹簧、限位环和载物板,通过弹簧对载物板以及储存桶进行支撑,在储存桶内侧没有原料时加料管的一端处于储存桶的内侧,由于加料管的出料口在储存桶的内侧,同时加料管的出料口离储存桶的底部距离近,物料从加料管出来时不会出现迸溅的现象,随着储存桶内侧物料之间的增加,载物板以及储存桶也会一起往下移动,直到触碰限位开关。
CN202110155748.9一种用于硅钢片横剪线的冲孔和剪切的数控自动化车床
本发明涉及硅钢片横剪线技术领域,具体为一种用于硅钢片横剪线的冲孔和剪切的数控自动化车床,包括底座,底座的左侧上方与基座的底部上方设置有基座,基座的前侧中部设置有钢片辊,基座的右侧设置有凹槽,凹槽设置在底座内部,凹槽的左右两侧端部设置有齿轮,齿轮的外侧设置有皮带,凹槽的右侧上方设置有挡板,有益效果是:挡板的开口结构,使硅钢片自左向右经过挡板后,会处于底座上方正中间,方便调整硅钢片的水平位置,并使其可以准确进入夹板内部。通过弹簧的弹力作用,控制拉绳的位置,以此来实现拉绳带动夹块的关闭,使绕片筒在转动过程中,夹块可以将硅钢片的端部牢牢固定住。
CN202110192619.7用于控制硅钢毛刺状厚度波动的工艺及硅钢片产品
本发明涉及一种用于控制硅钢毛刺状厚度波动的工艺,包括如下步骤;将连铸坯送入加热炉中进行加热,连铸坯入炉温度为400‑680℃,连铸坯在炉时间为185‑220min;将加热后的连铸坯进行热轧,轧辊偏心量为0‑0.025mm,将热轧后的带钢进行卷取;将卷取后的带钢酸洗后进行冷轧,冷轧操作模式由多次阶段升降速模式调整为一次性升降速模式,且在一次性升降速阶段将MN‑AGC增益系数增大;将冷轧后的带钢进行卷取,退火后得到硅钢片成品。本发明所公开的用于控制硅钢毛刺状厚度波动的工艺,该工艺对加热、热轧、卷取及冷轧各工序进行优化协调,能够有效解决硅钢毛刺状厚度波动的问题,实现无取向硅钢全长厚度控制精度的提升,而且无需进行设备和系统改造,容易实现,易于推广。
CN202123037575.5一种便于拼装硅钢片的变压器铁芯
本实用新型涉及一种便于拼装硅钢片的变压器铁芯,包括铁芯,设置在固定座的上方;硅钢片,固定安装在铁芯的侧壁上;连接座,固定在铁芯的底部,并安装在固定座上;有益效果是:本实用新型通过加入固定座和连接座的结构,方便将铁芯固定安装在固定座上,防止在对铁芯和硅钢片的拼装时,铁芯位置变化,造成铁芯和硅钢片碰撞磨损,通过转动环的转动结构,以及牵引绳的从动结构,有效控制卡柱的收缩,方便将连接座安装在固定座上,防止卡柱与连接座底部碰撞造成其损伤,硅钢片的两端均设置有规格相同的卡块,防止硅钢片出现反向安装的情况出现。
高强无取向硅钢组织演变与强化机制
针对新能源汽车的发展,制备了含Ni固溶强化、含Cu析出强化以及含Ni+Cu复合强化3%Si无取向硅钢,研究了强化方式对无取向硅钢组织、织构和性能的影响。结果表明:固溶强化型无取向硅钢热轧板中形成了粗大{221}<221>晶粒,冷轧过程中剪切变形明显并在退火后形成良好再结晶织构。析出强化型无取向硅钢热轧板中心层形成γ取向粗大晶粒,在后续的加工中γ织构逐渐增强并最终得到相对细小的再结晶晶粒。复合强化型无取向硅钢热轧板中保留了强λ取向带状组织,退火后形成了有益的Goss织构和λ织构。固溶强化型与复合强化型无取向硅钢磁感应强度B50分别达到1.742、1.688 T,高于析出强化型无取向硅钢的1.645 T。同时,复合强化型无取向硅钢高频铁损最低,其P1.0/400和P1.0/1 000分别低至20.97、82.69 W/kg,这与其较小的晶粒尺寸和织构改善有关。强度计算结果表明:Ni元素固溶强化对强度的提高有限,屈服强度为468 MPa,纳米Cu析出可显著提高屈服强度(强度增量约200 MPa),且主要来自于模量强... For the development of new energy vehicles, 3%Si non-oriented silicon steel were processed by solid solution strengthening with Ni, precipitation strengthening with Cu, and composite strengthening with Ni and Cu. The effects of different strengthening methods on the microstructure, texture and properties of high-strength non oriented silicon steel were studied.The results show that coarse {221}<221> grains are formed in the hot rolled sheet of solution strengthened non-oriented silicon ste...
冷轧无取向硅钢产品标准浅析
聚焦无取向硅钢产品标准,从电磁性能、表面性能、机械性能以及尺寸公差与边部质量等维度对国际标准IEC、EN、JIS、ASTM以及国标GB进行了分析研究。分析得出,各类标准在电磁性能方面要求基本一致;ASTM标准的机械性能要求有别于其他几个标准。 In this paper,non-oriented silicon steel standards of EN,JIS,GB and ASTM were compared and analyzed. It is showed that,all types of standards in electromagnetic performance requirements are basically the same. Surface properties in ASTM standard are expressed in the most detailed. The mechanical properties requirements of the standards,except for ASTM,are basically the same.
CN202023343140.9硅钢绝缘涂层液循环罐
本实用新型涉及具有搅拌器的装置领域。尤其涉及硅钢绝缘涂层液循环罐,包括罐体,罐体的顶部设有进液口,罐体的侧壁上设有出液口,罐体上端设有盖板,罐体的盖板上设有涡轮室,罐体与涡轮室上贯穿有竖直的中空轴,涡轮室的顶部设有热水口,涡轮室内设有涡轮叶片,涡轮叶片固定在中空轴上,涡轮叶片与罐体上端之间的中空轴上贯穿有流水口,中空轴上设有若干侧管,侧管位于罐体内,所述侧管的两端与中空轴连通,中空轴的内侧封堵有隔板,侧管的两端分别位于隔板的上侧与下侧,中空轴与罐本体以及中空轴与上空腔的结合部均设有密封圈。从而本实用新型可实现对硅钢绝缘涂层液进行均匀加热。
CN202120568349.0一种取向硅钢毛刷辊损耗检测装置及钢带刷洗机构
本实用新型公开了一种取向硅钢毛刷辊损耗检测装置及钢带刷洗机构。该取向硅钢毛刷辊损耗检测装置包括:固定基座,设置于刷辊的辊面侧方;压力测试元件,用于与刷辊的刷毛相顶压并测试刷毛对测力件的压力;接近机构,连接压力测试元件与固定基座,驱动测力件朝向或者背向刷辊运动。该取向硅钢毛刷辊损耗检测装置中的接近机构带动压力测试元件向刷辊一侧运动,直至刷毛与压力测试元件相顶压,当压力值至预定范围后,获得接近机构带动压力测试元件朝向刷辊的运动量,进而获得刷毛的损耗量;保证钢带刷洗清洁效果的同时,降低刷辊维护成本。
电工钢边缘降控制研究
以马鞍山钢铁集团公司电工钢板形优化控制研究项目为背景,系统地研究了热轧、冷连轧和单机架轧机在电工钢生产过程中的边缘降控制问题。通过现场数据采集、工况数值模拟计算和工业化大生产试验,设计出适用、合理的电工钢板形控制的辊型优化曲线,满足了不同工序、不同机型的板形控制策略要求,解决了电工钢板形质量问题,取得了显著的经济效益。 Based on the project of electric steel strip shape optimization control,problem of edge drop control was systematically studied in production of electric steel of hot-rolling mill,cold-rolling mill and single stand mill.Roll optimization contour was designed out in point and reasonable by collection of work condition data,numerical simulation and test of industrial production.The shape control system can meet with the different working steps and difference mills,and quality problem of electric s...
剪切方式对冷轧无取向硅钢边部磁畴的影响
为提高无取向硅钢导磁性能,研究了不同剪切方式对无取向硅钢剪切处磁畴结构的影响。利用纳米磁流体观测无取向硅钢剪切后边部磁畴结构。结果表明,硅钢无论在机械剪切还是线切割后的边部磁畴都会发生不同程度的改变:线切割对边部磁畴结构改变较小,边部磁畴分布均匀且连续,在距边缘0~20μm范围内出现磁畴宽度变小现象;机械剪切对磁畴的改变较为严重,剪切处磁畴零乱且不连续,在距边缘20μm处仍难以观察到完整的磁畴结构。 The effects of different shearing modes on magnetic domain structure of cold rolled non-oriented silicon steel are studied in this paper.The magnetic domain of cold rolled non-oriented silicon steel is observed by nanometer magnetic fluid pattern method.The results show that the edge magnetic domain structure will be changed by mechanical shear and wire-electrode cutting,the variation of edge magnetic domain structure wire-electrode cutting edge is very small,the magnetic domain structure is wel...