  • 未分类

本实用新型公开了一种将硅钢片堆栈模块化的电机转子,包括:堆栈模块、转子端板和电机轴;堆栈模块卡接在电机轴的外侧,且堆栈模块的两端通过转子端板连接固定;堆栈模块包括多个相互连接的硅钢片,每个硅钢片上均设有连接件,硅钢片通过连接件相互连接。本实用新型通过在硅钢片上增设连接件将多个硅钢片叠加成堆栈模块,降低了固定难度和管理难度,而且可以使用机器人自动化产线的大规模生产,生产效率高。
2021-03-18 171 6.8

针对宝钢集团、日本新日铁住金和JFE公司公开的相关专利等资料,总结了国内外高强度无取向电工钢的研究进展,分析了不同电工钢的化学成分、生产工艺及产品性能,指出固溶强化、细晶强化、析出强化、位错强化都有可能被用来提高无取向电工钢的强度,并阐述了四种强化方式的优缺点;指出在高强度无取向电工钢的研发过程中,需根据其具体用途确定目标性能,再采用合适的强化手段,最终实现力学性能、磁性能和生产性能之间的平衡。 The research progress of high strength non-oriented electrical steels at home and abroad is summarized according to related patents brought into the public by Baosteel,Nippon Steel & Sumitomo Metal corporation and JFE corporation.The characteristics of chemical composition,production technology and properties of products in the patents are analyzed.Each of solution strengthening method,fine-grain strengthening method, precipitation strengthening method or dislocations strengthening method ma... 
2014-04-28 179 5.8

本发明特别涉及一种控制边部翘皮的热轧电工钢的生产方法和生产系统,属于钢表面质量检测技术领域,方法包括:建立热轧电工钢边部翘皮的数据库,数据库包括翘皮类型及各翘皮类型的翘皮发生原因和翘皮发生的区域;对待质检的热轧电工钢表面进行识别,并对比数据库,获得待质检的热轧电工钢表面翘皮的翘皮类型;根据待质检的热轧电工钢表面翘皮的俏皮类型获得该类型翘皮的翘皮发生原因和翘皮发生的区域;根据翘皮发生原因和翘皮发生的区域,调整生产操作,用以减少热轧电工钢的边部翘皮;通过对边部翘皮进行准确分类及识别,能够准确的分辨出边部翘皮的产生原因,采取有针对性的措施防止缺陷扩大,最大程度的降低缺陷发生量,提高质量控制水平。
2021-07-28 174 6.8

本实用新型公开了一种风电机组取向电工钢用罩式炉的砂封振动装置,包括:基座,设置有行走机构,行走机构带动基座沿环形砂封槽槽壁行走;振动齿座,与基座连接,定位座和基座之间夹设有弹性缓振件;振动件,与定位座固定连接;振动齿,与振动齿座固定连接,设置于基座的行走轨迹内侧。该风电机组取向电工钢用罩式炉的砂封振动装置利用砂封槽的槽壁作为行走机构的轨道,振动齿不仅可以平整砂封槽中的密封砂,振动状态下还能使密封砂填充得更趋密实,避免局部密封不良的问题,优化密封效果。
2021-08-28 167 6.8

阐述了国内外高磁感取向硅钢的生产研究水平与发展趋势,包括通过提高高斯晶粒取向度、细化磁畴、涂覆张力涂层、减薄钢片厚度进一步降低铁损以及低温加热技术和短流程技术新工艺。分析高磁感取向硅钢在我国大型电力变压器上的应用情况,结果表明,发展更薄规格高磁感、低铁损、低磁致伸缩取向硅钢可为大型变压器的安全性、节能性及环保性提供有效保障。 The research progress and development trend of high magnetic induction grain-oriented silicon steel at home and abroad are summarized,including the technology of improving the Goss alignment,refining domain wall,adding stress coating,decreasing thickness of sheet,and the new technique of reducing heating temperature of casting slab and shortening operational.Moreover,the application of high magnetic induction grain-oriented silicon in power transformer is presented.Developing grain-oriented sili... 
2014-11-28 181 5.8

分析了高转矩和高转速条件下高效驱动马达铁芯材料对无取向硅钢磁性能要求,讨论了无取向硅钢的高磁通密度和低铁损对电机转矩和效率的影响,介绍了国内外高磁感无取向硅钢发展情况。在生产工艺上,提高钢质纯净度,弱化夹杂物和第二相粒子对畴壁移动和再结晶晶粒长大的钉扎作用,添加微量晶界和带钢表面的偏析元素促使有利织构发展等技术可提高无取向硅钢的磁通密度。 The requirements of high efficient drive motor core materials under the conditions of high torque and high speed were analyzed.The effects of high magnetic flux density of non-oriented silicon steel on the torque and efficiency of the motor were discussed.The development of non-oriented silicon steel with high magnetic was introduced.The magnetic flux density of non-oriented silicon steel sheet can be obviously improved by some production technologies,such as purification steel,weakening the pin... 
2023-05-11 1.37k 5.8

试验研究了0.3 mm取向硅钢冷轧板(/%:0.046C,3.07Si,0.09Mn,0.029P,0.004S,0.005A1)的退火温度(760~880℃7 min)和退火时间(820℃3~9 min)对该钢的晶粒尺寸,再结晶和织构的影响。结果表明,最佳初次再结晶退火工艺为820℃5 min,该钢的平均晶粒尺寸为14.20μm,完全再结晶率为92%,不利{111}<110>结构含量为3.16%,有利织构{111}<112>,{012}<001>和高斯织构含量分别0.40%,4.73%和2.46%。 The effect of annealing temperature(at 760 ~ 880 X.for 7 min) and time(at 820℃ for 3~9 min) on grain size,recrystallization rate and texture of 0.3 mm cold-rolled sheet of oriented silicon steel(/%:0.046C,3.07Si,0.09Mn,0.029P,0.004S,0.005Al) has been tested and studied.Results show that with optimum recrystallized annealing at 820℃ for 5 min,the silicon steel average grain size is 14.20 fun,the complete recrystaUization rate is 92%,the unfavourable-texture {111}< 110 > content in steel is ... 
2014-03-28 141 5.8

【作者】 杨佳直; ...
2013-05-28 112 5.8

本发明公开了一种高强度碳化硅钢球,所述高强度碳化硅钢球包括以下重量份的原料:碳化硅20‑30份、铬1‑2份、氮化硼3‑5份、铁10‑20份、钼2‑3份、锰钢30‑40份、镍5‑8份、钛6‑8份、磷2‑3份、硫2‑3份;一种高强度碳化硅钢球制备方法,包括如下步骤S1、熔融;S2、模锻成球;S3、打磨;S4、二次加热;S5、高温淬火;S6、机油回火;S7、检测成品。本发明制备的高强度碳化硅钢球具有抗折强度高、洛氏硬度高及抗压强度高等优异的机械性能,并且使用寿命长,运转精确度高,并且其工艺简单,生产耗能低,无“三废”产生,环保性高。
2021-08-02 157 6.8

电工钢反复弯曲次数是电工钢性能检验的重要指标之一,直接影响到用户在使用电工钢过程的机加工性能。主要分析了试样宽度、试样张力、晶粒取向、反复弯曲设备等因素对电工钢反复弯曲试验的影响,并对各个因素的影响程度进行量化以及原因探讨,从而归纳形成各影响因素的基本规律,以便为电工钢实际生产、用户使用提供科学指导。结果表明:试样宽度增加,反复弯曲次数也会不断增加,晶粒位向对取向电工钢的反复弯曲次数影响较大,当支座顶部到拨杆底部的距离减小或拉紧力增加时,反复弯曲次数会不断减小,但当拉紧力达到60N以上时,对反复弯曲次数影响不大,试样经退火后,反复弯曲次数略有上升。 The reverse bend number is an important performance of electrical steels′capabilities,affecting the machining performance directly when the customers used.It investigated some factors,such as sample′s width,sample′s tension load,grain orientation and equipment,how to effect the reverse bend test for electrical steel,measured the influence degree,and discussed the reason,in order to form basic rules which could be guided the manufacturing and using for electrical steel.Results showed that the rev... 
2014-07-28 159 5.8

本实用新型公开了一种适用于自动线的硅钢叠装系数性能检测装置,涉及实验仪器自动化技术领域,为解决机器人自动上样至叠装系数测量仪经常发生碰撞的问题;本实用新型包括框架、上压板、下压板、压紧驱动机构、高度探规和加载力值传感器,其中压紧驱动机构设置于框架上端,下压板固定于框架内的下端,上压板安装于下压板上方且与压紧驱动机构的输出端传动连接,加载力值传感器安装于上压板与压紧驱动机构的输出端之间,高度探规安装在上压板上,且探头向下伸出上压板下端面,框架为“C”字形一体式刚性结构,其设有上下两个水平板,以及位于一侧的竖直板;本实用新型能够避免机器人自动上样时碰撞到框架,以及下压时高度探规压到试样。
2021-10-25 151 6.8

本发明涉及硅钢技术领域,尤其涉及一种硅钢连退炉辊除瘤方法及装置。包括连杆、手柄、磨削片、密封盖、端盖与套筒;磨削片垂直固接在连杆一端的外壁上,手柄固接在连杆的另一端,手柄与磨削片处于同一平面上;连杆套接在套筒内,连杆能沿套筒轴向移动,套筒固接在端盖上;硅钢连退炉辊下方的炉墙设有与连杆及磨削片相应的磨辊孔,端盖或密封盖固接在磨辊孔处。1)确定结瘤炉辊;2)确定结瘤在碳套辊上的位置;3)插入除瘤装置;4)磨削;5)抽出。本发明降低废品量,提高成材率;减少停炉处理结瘤时间,降低能耗,提高生产率;提高难磨瘤辊的修复率,降低炉辊成本。
2021-07-12 157 6.8