钢厂
CN202023246515.X硅钢用氧化镁冷涂托盘结构
本实用新型涉及硅钢生产设备技术领域,具体公开了硅钢用氧化镁冷涂托盘结构,包括机架和托盘本体,托盘本体固定在机架上,托盘本体位于涂层机上,所述涂层机包括一对上下设置且转动连接在机架上的胶辊,所述托盘内设有气管,所述气管一端固定在机架上,另一端水平设置在托盘本体靠近底部的位置,机架上设有连通气管的供气件。本专利中,通过对气管提供气流,从气管鼓出的气体对托盘本体内的涂层液形成搅拌的作用,避免涂层液中的氧化镁颗粒沉底结晶,本方案结构简单,无需对托盘本体进行其它加工改造,适合在结构紧凑的涂层机中使用。
6.5%Si硅钢的制备技术和发展前景
6.5%Si硅钢具有优异的磁学性能和广泛的应用前景。本文综述了6.5%Si硅钢的物理、机械及磁学特性,讨论了传统轧制、温轧、薄带连铸、快速凝固、CVD、粉末轧制等不同制备工艺的关键技术及特点,概括了6.5%Si硅钢在高效节能电机、汽车马达及磁屏蔽等领域中的主要应用,介绍了硅钢的制备技术取得的研究进展,并指出了其广阔的发展前景。 6.5% Si silicon steel has good magnetic properties and wide applications.In this paper physical and mechanical magnetic properties were summarized,and key technology and characteristic of several preparation methods,such as traditional rolling,warm rolling,thin strip continuous casting,rapid solidification,CVD and powder rolling,were discussed.Main applications of 6.5% Si steel in the fields of high-efficiency electrical motors,automobile motors,transformer cores and magnetic shielding were gene...
CN202111463911.4含铜一般取向硅钢及其制备方法
本发明提供一种含铜一般取向硅钢及其制备方法,制备方法包括:对钢板进行脱碳退火,得到脱碳钢,其中,将所述脱碳钢的氧含量控制在如下公式计算的范围内:ψO=(0.0504×ωSi×H2±0.00005)×106,其中,ψO为脱碳钢的氧含量,单位为ppm;ωSi为钢板中Si的重量百分含量;H为钢板的厚度,单位为mm;将所述脱碳钢进行冷轧、涂布氧化镁涂层、卷曲和成卷退火,得到退火钢卷;对所述退火钢卷进行开卷,再涂敷张应力涂层和拉伸平整退火,制得含铜一般取向硅钢。本发明根据钢板中Si的实际含量及钢板厚度,调整脱碳钢的氧含量,以获得表面质量良好、磁性水平稳定的含铜一般取向硅钢产品。
CN202110014039.9一种免涂层高碳高强耐蚀电磁钢板及其生产方法
本发明涉及电磁钢板技术领域,尤其涉及一种免涂层高碳高强耐蚀电磁钢板及其生产方法。所述电磁钢板按重量百分比计,包括如下组分:C为0.010%~0.150%,Si为1.30%~2.50%,Mn为0.50%~1.50%,P为0.04%~0.15%,S≤0.015%,Cr为0.10%~1.50%,Cu为0.2%~0.6%,Al为0.10%~1.50%,Sn为0.02%~0.10%,Ni≤0.0050%,Nb≤0.0050%,Ti≤0.0050%,N≤0.0050%,V≤0.0050%,其余为Fe和不可控残余元素。所述钢板生产方法包括如下步骤:1)板坯浇铸;2)板坯连轧及卷曲;3)热轧卷酸洗及冷轧;4)罩式退火;5)钢卷矫直或拉矫。本发明所生产专用产品在电磁性能相近情况下,强度进一步提升、耐蚀性能提高、生产流程缩短、生产难度下降,减少了涂层工序,降低了生产成本,同时不同盐雾试验锈蚀减少85%以上。
CN202122912643.1一种硅钢片立式送料装置
本实用新型公开了一种硅钢片立式送料装置,包括装置主体,装置主体上方安装有固定板架和活动板架,固定板架和活动板架上方均安装有料架,固定板架通过螺栓固定在装置主体的上方,活动板架滑动安装在装置主体的上方;装置主体内部位于固定板架和活动板架的下方安装有推料板,本实用新型适用于硅钢片生产,该装置通过将其中一个料架安装安装在活动板架的上方,而装置主体的两侧上方开设有滑槽,滑槽沿装置主体的长度方向开设,活动板架采用倒“U”型结构,活动板架的两个竖直端滑动卡合在滑槽内,这样的结构设置使得活动板架能够在水平方向移动调整位置,从而使两个料架的间距可调,使该装置能够适用于不同大小型号的物料使用。
电工钢显微结构和疲劳性能的研究
研究了电工钢SXRC的显微结构和疲劳性能,并与DP钢进行了比较。结果表明,退火温度低温化能够有效的抑制电工钢的再结晶。该钢在固溶铌的作用下,能够在保证电机磁性的同时具有一定的强度。与DP钢相比,SXRC钢的抗疲劳性能更好。 The microstructures and fatigue properties of the electrical steel SXRC we re investigated, and the properties were also compared with the steel DP. The results show that the recrystallization of the electrical steel can be suppressed at lower annealing temperature. The steel presents favorable motor magnetic and also a compatible strength with the help of solid-solution Nb. Compared with the steel DP, the fatigue resistance of the steel SXRC is preferable.
双取向硅钢在制备过程各阶段的织构和微结构
利用X-射线衍射织构分析和线形分析技术测定了交叉轧制双取向硅钢在制备工艺各阶段的织构及微结构,进而探讨了立方织构({100}<001>)的形成过程。通过对实验结果的分析可知,二次冷轧和交叉轧制工艺为立方织构提供了内能优势和有利的形变织构,而低温预退火工艺既强化了立方织构的内能优势,又为立方织构的异常长大提供了有利的组织保证,最终在抑制剂(AlN和MnS)的协同作用下,硅钢在二次再结晶退火后形成了强烈的立方织构。 The texture and substructure of the double oriented electrical steels produced by the cross rolling technology during the difference process has been measured by means of the X-ray texture and diffraction peak profile analysis technology,and research the formation mechanism of cube texture,{100}<001>.The results show that the dominances of inner energy and deformation texture were supplied by secondary cold rolling and the cross rolling technology and strengthened by pre-annealing at a low...
CN202122014099.9一种用于硅钢板带的表面清理装置
本实用新型公开了一种用于硅钢板带的表面清理装置,包括机体,所述机体的内部设置有转动机构,所述转动机构的内部安装有固定机构,所述机体的外表面一侧固定连接有驱动电机,所述驱动电机的输出端固定连接有螺杆,所述螺杆的外部设置有螺纹套,且螺纹套在螺杆上螺纹转动连接,所述螺纹套的底部固定连接有电动推杆,所述电动推杆的输出端固定连接有连接板。本实用新型,利用转动机构可很好的进行翻转,便于对两面进行清理,从而提高了一定的工作效率,相比人工翻转清理时效果更好,具有一定的实用性,利用固定机构可很好对于成硅钢板带进行固定,可方便进行清理,提高清理时的工作效率,实用性较强。
CN202023350704.1一种叠片装置以及硅钢片收料设备
本实用新型公开了叠片装置,以及采用该叠片装置的硅钢片收料设备,包括分料装置和本实用新型第一方面实施例的叠片装置,分料装置包括有分料件、上分料传送带和下分料传送带,上分料传送带的一端和下分料传送带的一端与分料件连接,分料件用于将硅钢片分别输送至上分料传送带和下分料传送带,本实用新型第一方面实施例的叠片装置,叠片装置的数量为两个,两个叠片装置上下平行设置,并且分别与上分料传送带和下分料传送带的远离分料件的一端连接。根据本实用新型的叠片装置,以及采用该叠片装置的硅钢片收料设备,可实现硅钢片的自动叠片,提高生产效率。
铸坯热装温度对无取向硅钢中AlN和MnS析出行为的影响
通过固溶度积公式计算及热模拟实验,对不同热装和加热温度条件下的无取向硅钢铸坯中析出相进行了研究.在低于950℃热装时,铸坯中AlN的析出量和尺寸不再变化,但MnS和AlN-MnS的数量及平均尺寸随着热装温度降低而进一步增加,并在温度低于600℃时达到最大值后保持不变.与1200℃相比,1100℃加热的铸坯中AlN、MnS的总固溶量相对更少.相比850℃热装,600℃热装再加热到1100℃的铸坯中AlN和MnS的总固溶量更少,且AlN和MnS尺寸更大.合适的热装温度和加热温度分别为600℃和1100℃. Based on solubility product calculation and thermal simulation experiments,precipitated phases in continuous casting slabs of non-oriented silicon steel were systematically studied at different hot charging and heating temperatures.When the hot charging temperature is below 950 ℃,the content and size of AlN remain unchanged,but the quantity and size of MnS and AlN-MnS increase when the hot charging temperature decreases,reach maximum and remain unchanged when the hot charging temperature is belo...