阐述了电工钢在\"双碳\"中的作用,强调了电工钢的生产工艺技术及在减少碳排放、降低能耗中的作用,对下游能效升级带来明显的节能及降碳成果。同时,分析了2021年电工钢的生产运行情况,介绍了电工钢的未来发展,并针对如何减少碳排放以及生产更多的更低铁损、更高磁感的电工钢谈了几点启示。 The effects of electrical steels on carbon peak and carbon neutralization were expounded,especially on the achievements of obvious energy saving and carbon reduction to the downstream energy efficiency upgrading bringing from the production technology of electrical steels and their effects to reducing carbon emission and energy consumption.Meanwhile the production situation of electrical steels in 2021 was analyzed,and the future development of electrical steels was introduced,and some advices w... 
2022-01-28 181 5.8

电工钢试样加工产生的剪切应力会恶化钢板的磁性,对不同牌号硅钢片的横向、纵向试样退火前后磁性能的变化进行研究,结果表明:无取向硅钢片在剪切过程中横向、纵向的磁性受到剪切应力影响是不一样的。 The electrical steel sample processing magnetic of electrical steel will worsen due to the shear stress of sample. In this paper,the magnetic change of transverse,longitudinal specimens of different type of silicon steel sheet before and after annealing are studied. The results show that the magnetic of non- oriented silicon steel sheet affected in the process of shear is not the same in horizontal and vertical direction. 
2013-05-28 174 5.8

取向硅钢常化工序主要采用现场实测带钢温度的方式测定冷却速率,并通过稳定冷却水温、调整冷却水量及喷梁运行数量等方式保证合理的冷却速率,给常化工艺设计和生产带来诸多不便。通过对常化工艺水冷过程带钢的传热分析求解,在建立带钢水冷温度模型的基础上,研究了不同冷却工艺参数对带钢温度及冷却速率的影响规律以及冷却工艺的交互作用结果。结果表明:模型计算结果能够较好地反映取向硅钢在常化水冷过程中的温度及冷却速率的变化,其计算误差为0.80%~4.11%;在特定取向硅钢厚度规格和常化工艺下,随着常化冷却水量及有效冷却长度的增加,带钢水冷温度及冷却速率与呈非线性变化;常化水冷工艺主要通过调控带钢与冷却水之间热交换量和交换时间实现对带钢温度的控制,实际生产中需综合考虑机组速度、冷却水量及有效冷却长度之间的交互作用,选定喷梁投入数量和冷却水量以获得稳定的冷却速率。 The cooling rate of normalization process mainly determined by measuring the grain oriented silicon steel strip temperature on site, and ensures the cooling rate by stabilizing the cooling water temperature, adjusting the cooling water volume and the operation quantity of spray beam, which brings inconvenience to the normalization process design and production. Based on the heat transfer of strip in the water cooling section of normalization process, the water cooling temperature model for the n... 
2022-01-28 190 5.8

对无取向硅钢炼钢全流程钢液增钛的原因进行了分析,认为铁水钛含量、转炉出钢温度、转炉下渣量、精炼渣TiO2含量、钢水罐及RH浸入管混钢种生产是影响钢液增钛的主要原因。通过采取低钛铁水冶炼,减少转炉下渣量,提高出钢温度,添加白灰改质精炼渣等措施,均能够降低钢液中的钛含量。 After analyzing the causes leading to increased content of titanium in molten nonoriented silicon steel during whole steelmaking process, it was concluded that such factors as content of titanium in hot metal, tapping temperature from converter, quantity of roughing slag entered into the ladle from converter, content of TiO2 in refining slag, molten steel ladle car,carrying out the steelmaking of different steel grades by the same ladle and same RH immersion tube were the main causes ... 
2022-01-28 173 5.8

无氧化炉具有加热效率高、投资与运营成本低、作业率高、表面质量及板型良好、NOx排放相对低等优势,在硅钢热处理领域应用前景广泛。本文阐述了确定无氧化炉(NOF)加热能力详细过程,涵盖炉温、炉断面尺寸、炉长、热平衡结算、加热能力计算等,为今后无氧化炉(NOF)在硅钢热处理应用时的设计提供了借鉴,同时也为今后明火直接加热的工业炉设计提供了参考。 Non-oxidation furnace has the advantage s of high heating efficiency, low investment and operation cost, high operation rate, good surface quality and plate shape, and relatively low NOxemission,and it still has wide application prospect in the field of silicon steel heat treatment. The detailed process of determining the heating capacity of a non-oxidizing furnace(NOF) is described, covering furnace temperature, furnace section size, furnace length, heat balance settlement, heating capacity cal... 
2022-01-28 182 5.8

一种高磁感低铁损取向硅钢生产用表面涂层涂覆装置,包括:加工台,加工台上端固定连接支撑架,支撑架下端一侧固定连接伺服电机,伺服电机输出端固定连接第一齿轮,第一齿轮下端啮合连接第二齿轮,第二齿轮中部固定连接螺纹杆,螺纹杆上螺纹连接移动环,螺纹杆远离第二齿轮一侧转动连接支撑板,支撑板上端固定连接支撑架,移动环下端固定连接伸缩杆,支撑架下端前后部均固定连接连接框,本实用新型的有益效果是:通过设置的伺服电机、第一齿轮、第二齿轮、螺纹杆和移动环等结构,能够实现伸缩板带动硅钢板移动,从而能够完成自动化推料,减少工人劳力支出的同时,也能够避免工作人员手臂靠近涂层辊,从而避免安全事故的发生。
2021-12-22 188 6.8

本实用新型公开了硅钢片生产用上料装置,属于硅钢片生产领域,包括本体,所述本体包括侧板和U型板,所述侧板固定连接在U型板的一侧,所述本体的顶部横向设置有平移机构,所述平移机构上安装有气缸,所述气缸的底部安装有吸盘,所述U型板内腔的底部竖向固定连接有弹簧,所述弹簧远离U型板的一端水平固定连接有升降板,所述平移机构包括电机、螺纹杆、限位板和移动块,所述电机安装在侧板的顶部,所述电机的输出轴与螺纹杆的一端固定连接,通过设置弹簧,在第一个物料从上料装置移出后弹簧的弹力推动剩余物料,使得剩余物料进行上升,避免吸盘触碰不到物料的问题,简化吸盘移动轨迹,加快上料速度。
2021-12-14 167 6.8

本发明提供了一种无取向硅钢RH顶枪喷粉脱硫工艺,RH脱碳结束测温定氧,立即加入铝粒脱氧合金化、之后立即依次连续加入合金进行成分调整,合金加完后立即开始顶枪喷粉;加入铝粒的量=铝粒理论加入量+0.2‑0.4kg/t钢;喷粉时,控制喷粉速度与钢液循环流量相匹配;本发明从真空条件下脱硫热力学和动力学角度出发对具有顶枪喷粉功能的RH脱硫工艺进行改进,提高脱硫率。
2021-11-30 157 6.8

一种变压器硅钢片转运吊车,属变压器生产技术领域,包括车架、驱动部和承载部,驱动部连接车架和承载部,承载部上承载硅钢片。车架包括底板、支撑单耳、后耳片,底板前端两侧向前上方各延伸一个支撑单耳,支撑单耳连接驱动部,底板的中后部两侧各具有一个后耳片,后耳片也连接驱动部。驱动部包括连杆、底双耳、支撑双耳、轴座、转轴和液压缸,连杆具有一对,连杆下端具有底双耳,连杆的中下部具有支撑双耳,连杆的顶部具有轴座,底双耳铰接在支撑单耳上,转轴安装在两个连杆顶部的轴座上,液压缸的两端分别连接在后耳片和支撑双耳上。承载部包括托盘、侧部耳片、拉杆、下双耳和上挂耳,托盘两侧各具有一对侧部耳片,拉杆呈倒Y字形结构。
2021-11-15 121 6.8

本发明公开了一种低损耗宽料取向硅钢的生产方法。本发明所述生产方法是通过在罩式炉的内罩中增加带有通气孔的聚气罩及与聚气罩配合的炉底板,配合工艺优化,控制原料化学成分,使气体和钢卷之间的浓度更均匀,反应更充分,气流流动方向更易控制,所制备的取向硅钢性能稳定,磁性能优良,且铁损达到1.12W/KG以下的比例提高至98.77%,平均铁损达到1.06W/KG以内,使取向硅钢卷的铁损大幅度降低,电磁性能更好。
2021-10-26 173 6.8

本发明涉及无取向硅钢技术领域,具体提供了一种无取向硅钢的制备方法,对再结晶率为70‑90%、平均晶粒尺寸为10‑15μm、硬度HV为140‑170的硅钢半成品在温度为T=(772~777)+2900×W(Si)的条件下进行去应力退火,制得无取向硅钢,晶粒在去应力退火过程中均匀长大,平均晶粒尺寸80μm以上,有效降低铁损,使磁性能大幅度提高,铁损P1.5/50≤3.5W/kg,磁感B5000≥1.72T,电磁性能优异,满足客户使用要求,此外,本发明采用的硬度HV为140‑170的硅钢半成品在冲压过程中不易变形,机械加工性能优良。
2021-10-08 204 6.8

本申请提供了一种取向硅钢铸坯的制备方法及铸坯系统,该制备方法用于对精炼后的钢水进行连铸处理,所述连铸处理包括以下步骤:进行凝固处理,以使所述精炼后的部分钢水凝固形成坯壳;凝固处理时,进行电磁搅拌,以使所述精炼后的剩余钢水最终形成铸坯,其中,所述电磁搅拌的位置和结晶器出口的间距为0.3~1.5m,所述电磁搅拌的电流范围为0A~900A。上述制备方法通过调节电磁搅拌的位置和电流大小来调节电磁搅拌的强度,进而通过电磁搅拌的强度来调节等轴晶的生成量,扩大等轴晶率的范围。
2021-09-14 179 6.8