取向电工钢加工过程中第二相粒子的析出行为
利用场发射扫描电镜观察了以MnS为主要抑制剂的普通取向电工钢加工过程中第二相粒子的分布状态,统计了粒子面密度、平均尺寸以及相应的尺寸分布.结果显示,热轧加工造成了大量第二相粒子弥散、细小地析出,同时基体仍保持过饱和状态.冷轧变形会造成第二相粒子的回溶行为,而基体的过饱和状态会减弱回溶现象.中间退火与脱碳退火过程中会同时存在新粒子的形核及已析出粒子的粗化两个过程,而在最终二次再结晶升温阶段则以第二相粒子明显粗化为主. The distribution of second phase particles in conventional grain-oriented electrical steels during manufacturing processes with MnS as inhibitors was observed by field emission scanning electron microscopy,while the areal particle density,the average particle size and the corresponding size distribution were statistically determined.It is indicated that hot rolling leads to dispersive precipitation of a large amount of fine second phase particles and the matrix keeps a supersaturated state furth...
电工钢热连轧宽度自适应模型优化及应用
某厂对电工钢的轧制策略进行了优化,粗轧道次由“1+5”改为“1+3”。在优化后的生产过程中,每次变换钢种,烫辊材就会出现窄尺现象,而紧随其后的电工钢板则出现超宽现象。文中针对该问题,介绍了宽度设定模型和宽度自适应模型的原理,阐述了该问题出现的原因及解决方案,并通过对宽度自适应模型的应用研究及优化攻关,有效地解决了问题,大幅提升了实物质量,降低了宽度封锁率。 The rolling strategy of electrical steel was optimized in a factory,and the rough rolling pass was changed from “1+5”to“1+3”.Subsequently,the following problems were occurred in the production process:when the steel grade changed,the roasting roller steel before the electrical steel appeared the narrow width phenomenon,and then the electrical steel appeared the ultra-wide phenomenon.This paper introduced the principle of width setting model and width adaptive model,and expounded the causes and s...
冷轧无取向硅钢横向厚差控制
冷轧中中低牌号的无取向硅钢多采用万能凸度轧机(Universal crown mill,UCM)生产,其板形好坏受制于UCM轧机板形调节手段的协调使用。为掌握UCM轧机的板形控制特点,建立基于二维变厚度有限元的辊系弹性变形和基于三维差分的轧件塑性变形的六辊轧机耦合模型,对UCM轧机的板形调控性能进行详尽的分析,包括工作辊和中间辊弯辊、中间辊窜辊的调控功效、辊间接触压力分布等。在此基础上,提出可用指导生产的板形控制策略,指出UCM轧机在横向厚差控制方面的不足。针对工业生产中UCM轧机轧制无取向硅钢横向厚差大的问题,在大量仿真计算的基础上,开发具有高次曲线函数的边部变凸度(Edge variable crown,EVC)的工作辊。采用该工作辊后,各种品种的无取向硅钢的横向厚差不大于10μm的百分比由24%提高到99%,横向厚差的均值小于6μm,远小于之前的13μm。 Medium-low grade non-oriented silicon steel is rolled often by universal crown mill(UCM) during cold rolling.Its shape quality is dependent on the coordinated control of several shape adjustment devices of UCM.In order to understand the shape control characteristics of UCM,coupling model of six-high rolling mill,based on two-dimensional varying thickness finite element rolls elastic deformation model and three-dimensional finite difference strip plastic deformation model,is setup for the detaile...
硅钢DR510生产工艺优化
本文对某厂硅钢DR510温度、成分及过程控制水平和成品的组织、力学性能进行了研究,并在此基础上提出了工艺优化方案,有一定的借鉴和推广价值。 In this paper,the critical process and the products quality,including temperature,composition and process controlling level,the organization and mechanical properties of the finished product,were studied.On the basis of that the optimized technical plan provided,and this control technology is worth using and spreading.
初次再结晶退火工艺对3%Si取向硅钢组织和织构的影响
试验研究了0.3 mm取向硅钢冷轧板(/%:0.046C,3.07Si,0.09Mn,0.029P,0.004S,0.005A1)的退火温度(760~880℃7 min)和退火时间(820℃3~9 min)对该钢的晶粒尺寸,再结晶和织构的影响。结果表明,最佳初次再结晶退火工艺为820℃5 min,该钢的平均晶粒尺寸为14.20μm,完全再结晶率为92%,不利{111}<110>结构含量为3.16%,有利织构{111}<112>,{012}<001>和高斯织构含量分别0.40%,4.73%和2.46%。 The effect of annealing temperature(at 760 ~ 880 X.for 7 min) and time(at 820℃ for 3~9 min) on grain size,recrystallization rate and texture of 0.3 mm cold-rolled sheet of oriented silicon steel(/%:0.046C,3.07Si,0.09Mn,0.029P,0.004S,0.005Al) has been tested and studied.Results show that with optimum recrystallized annealing at 820℃ for 5 min,the silicon steel average grain size is 14.20 fun,the complete recrystaUization rate is 92%,the unfavourable-texture {111}< 110 > content in steel is ...
大数据技术在硅钢产品质量管控中的应用实践
磁性能指标是硅钢产品最关键的质量指标之一,但是目前磁性能判定100%依赖于样品的离线实验室检测结果,生产线配置的在线检测仪的测量结果由于精度问题,不宜直接用于成品牌号判级。本文在现有硅钢产品质量管控体系基础上,利用大数据技术对生产数据进行分析与建模,构建不同磁性能指标在线检测模型,并在现有信息系统上完成模型库的集成部署,实现硅钢产品全长、多指标磁性能结果的拟合数据输出,支撑取样优化、精准分切、辅助综合判定等功能应用,进一步优化硅钢产品质量管控体系。 The magnetic performance index of silicon steel products is one of the most critical quality indexes.However,at present,100%determination of magnetic performance depends on the offline laboratory test results of samples,and the measurement results of the online detector configured in the production line cannot be applied in practice due to the accuracy problem.Based on the existing quality control system of silicon steel products,big data technology was used to analyze and model the production d...
低牌号无取向电工钢磁时效行为分析
选取了三种50W 800无取向电工钢,分析了化学成分、晶粒尺寸、织构、以及200℃时效处理48 h前后的磁性能和第二相粒子析出状态的变化。结果表明,钢板中第二相粒子的分布密度对钢板铁损有最重要的影响。降低钢中C、N元素含量,或改进钢板热加工参数以降低成品钢板中第二相粒子形成元素的过饱和度均有利于明显降低钢板磁时效过程中的铁损增幅。钢板中对磁性能有利的织构也有利于降低钢板铁损的时效幅度。 The evolution of chemical composition,grain size,texture,as well as magnetic property after aging treatment at 200 ℃ for 48 h and distribution of second phase particles precipitation in three selected 50W800 non-oriented electrical steels were analyzed.The results show that the distribution density of second phase particles has great influence on core loss.Reducing C and N content,or improving hot-working parameters to reduce the supersaturation of elements forming second phase particles in prod...
无取向硅钢夹杂物分析
采用非水溶液电解方法来提取无取向硅钢中夹杂物。通过扫描电镜(SEM)观察结果表明:无取向硅钢中主要夹杂物为六棱柱的AlN、不规则硅酸盐及球状的铁的硫化物和氧化物,其中AlN夹杂尺寸在1~5μm,数量较多,还有部分AlN的复合夹杂。进一步研究了AlN复合夹杂形成机理,采用了Thermo-Calc热力学计算软件计算出该钢样中AlN、MnS析出温度分别为1 240℃、1 200℃,而Al2O3析出温度大于1 800℃,从而为AlN复合夹杂形成机理提供了一个理论依据。 Extracting inclusions from non-oriented silicon steel in non-aqueous electrolysis is a nondestructive method to gain inclusions.Scanning electron microscopy shows that the main inclusions in non-oriented silicon steel were hexagonal AlN,which was of large quantity,irregular silicate,spherical iron sulfide and oxide.The size of AlN inclusions ranged from 1to 5μm,and there were some duplex inclusions of AlN.To further study the formation mechanism of AlN duplex inclusions,Thermo-Calc thermodynamic...
稀土元素Ce含量对50W470无取向硅钢显微组织及性能的影响
利用光学显微镜(OM)和扫描电镜(SEM)研究了不同稀土Ce含量的50W470无取向硅钢的铸坯、热轧板和冷轧退火板的宏观和微观组织,并采用磁性能测试仪测定其磁性能。结果表明:当稀土Ce的加入量从0增加到66×10-6(质量分数)时,铸坯的柱状晶平均宽度从3.82 mm减小到3.24 mm,等轴晶率从43.1%增加到51.3%;热轧板的平均晶粒尺寸逐渐增加,从26.2μm增加到33.3μm,再结晶百分数从24%增加到37%;退火板的平均晶粒尺寸从36.2μm增加到39.3μm;磁性能测试表明,微观组织的变化有利于50W470无取向硅钢铁损降低和磁感提高。 Macro-structure and microstructure of as-cast plate, hot rolled plate and cold rolled annealed plate of 50 W470 non-oriented silicon steel with different rare earth Ce content was studied by optical microscope(OM) and scanning electron microscopy(SEM), and their magnetic properties were measured by magnetic property tester. The results show that when the addition amount of rare earth Ce increases from 0 to 66×10-6(mass fraction), the average width of columnar crystal of the as-cast pl...
无取向硅钢中的夹杂物析出在线观察
借助高温激光共聚焦显微镜,在线观察了不同Mn含量的无取向硅钢中夹杂物的尺寸、类型、数量变化。结果表明,Mn含量(质量分数)为0.77%、0.32%时,试样中的夹杂物数量分别约为1000万个/mm3、1600万个/mm3。Mn含量较高的钢种,会优先析出球形、椭球形MnS夹杂物,其析出数量较少,尺寸相对较大,可以有效抑制AlN、CuxS夹杂物析出;Mn含量较低的钢种,会在试样再加热后冷却过程中,先析出相当数量MnS夹杂物,并作为AlN夹杂物析出核心,形成MnS+AlN复合夹杂物。这种复合夹杂物数量较多,尺寸也较大。 Based on the high temperature confocal microscope, the chage of size, type, and quantity of inclusions in non-oriented silicon steels with different Mn content were observed by in-situ SEM. Results show that the inclusion quantities are 10 million per mm3 and 16 million per mm3,while the mass fractions of Mn are 0.77% and 0.32%, respectively. In the silicon steel with higher Mn content, the spherical and ellipsoidal MnS inclusion will precipitate first, which can retard the precipitation of AlN ...
离散粒子群优化算法在硅钢涂层近红外光谱厚度检测中的应用研究
提出一种基于粒子群优化算法实现的硅钢涂层厚度近红外光谱检测新方法。首先,采用近红外光谱仪采集获得了硅钢表面绝缘涂层的近红外光谱,然后,采用离散粒子群算法筛选出近红外光谱数据的最佳波长变量并组成新的光谱数据,最后,建立涂层厚度的核偏最小二乘定量分析模型。实验显示,所建定量分析模型对检验样本分析的绝对误差范围为-0.12~0.19μm,最大相对误差为14.31%,完全符合现场检验需要。研究表明,离散粒子群算法可以有效地筛选出携带更多有用信息的波长变量,提高定量分析模型的分析准确度和速度,是一种有效的近红外光谱波长筛选方法,同时,近红外光谱法也是一种有效的硅钢绝缘涂层厚度检测方法。 A novel thickness measurement NIR spectrometry for surface insulation coating of silicon steel based on discrete binary particle swarm optimization(DBPSO) algorithm is presented.First,we used NIR spectrometer to collect the NIR spectra of insulation coating of silicon steel,and then,DBPSO algorithm was used to select the optimal wavelength variates and composed a new spectra set.Last,the authors created the thickness quantitative analysis model using kernel partial least square algorithm.The exp...