钢厂
修正GTN模型及其在预测硅钢冷轧边裂中的应用
考虑剪应变对微孔洞损伤演化的影响,对GTN损伤模型的损伤演化机制进行修正,建立了适用于不同应力三轴度水平的损伤模型。结合隐式应力更新算法和显式有限元计算,采用VUMAT子程序实现了修正GTN模型在有限元软件ABAQUS中的数值计算。通过模拟纯剪切和剪切-拉伸两组试样的损伤演化和断裂行为,验证了修正GTN模型在不同应力三轴度承载条件下的有效性。运用修正GTN损伤模型模拟含边部缺口的带钢在轧制过程中裂纹的萌生和扩展行为,模拟结果与实验相一致,表明该模型可有效地用于带钢缺陷在轧制过程中扩展行为的分析和预测。模拟和实验结果表明,带钢边部缺口在轧制过程中,缺口前沿和后沿均会萌生裂纹,且后沿裂纹扩展更为明显。 Considering the effect of shear strain of micro-void on damage evolution, a modified GTN model applicable to various stress triaxiality conditions is proposed by modifying the damage evolution mechanism of the GTN damage model. The modified model is implemented in commercial finite element software ABAQUS by combining the implicit stress update method with an explicit finite element solving algorithm and through the user-defined material subroutine VUMAT. The damage evolution and the failure pro...
低温取向硅钢高温退火抑制剂的演化
取向硅钢利用析出物作为抑制剂,抑制初次再结晶晶粒的长大,抑制剂是取向硅钢发生二次再结晶的基本条件之一。文中通过低温板坯加热技术制备取向硅钢,采用透射电镜(TEM)观察并研究了高温退火阶段抑制剂的演化过程。结果表明,渗氮后形成的非晶态Si3N4析出物不稳定,在700~750℃退火升温阶段转化为(Al,Si)N;(Al,Si)N颗粒在800℃发生团聚,随后长大并粗化;(Al,Si)N是低温取向硅钢主要抑制剂,随退火温度的升高,(Al,Si)N抑制力大幅下降。 Precipitates as inhibitor are used to inhibit the grain growth of primary recrystallization in grain-oriented silicon steel,and inhibitor is one of the basic conditions for occurring of secondary recrystallization.The grain-oriented silicon steel was produced by low temperature slab heating and nitriding technique.The evolution of inhibitor was observed by transmission electron microscopy.The results show that Si3N4 particles are precipitated after nitriding,and Si3N4 particles are amorphous and...
电工钢生产中硫的控制
针对攀钢高硫铁水冶炼现状,结合不同生产工艺路线,论述了攀钢近年来为实现低硫电工钢的生产,在铁水预处理、转炉冶炼、钢水精炼过程中硫控制技术的开发与应用,形成了低硫洁净钢生产工艺技术,实现了低硫电工钢的生产。低硫电工钢RH脱硫率可达到20%左右,成品[S]控制在0.006%左右。 According to the smelting situations of hot metal with high sulphur content at Panzhihua Steel,combined with different produce processes,technologies for controlling the sulfur content during hot metal pretreatment,converter smelting,and second refining are developed. Technologies in low-sulfur clean steelmaking are formed. Low-sulfur electric steel are produced. As for the desulfurization rate of lowsulfur electric steel can reach about 20%,and the content of [S] in products is controlled to ab...
TSCR热轧工艺对3.2%Si无取向硅钢组织性能的影响
研究了薄板坯连铸连轧流程(TSCR)条件下热轧工艺对3.2%Si-0.7%Al无取向硅钢组织、织构演变及磁性能的影响规律。结果表明,提高均热温度和热轧温度有助于获得粗大的变形组织和强烈的{001}〈110〉织构,进而对后续的组织、织构演变进程及磁性能产生有利的遗传影响。与低温均热和低温热轧相比,高温均热和高温热轧得到的最终成品板的再结晶晶粒较粗大,λ纤维再结晶织构较强而γ纤维再结晶织构较弱,磁感应强度较高。 It was investigated that the effects of thin slab cast rolling(TSCR) hot rolling processes on microstructural,textural evolution and magnetic properties of 3.2%Si-0.7%Al non-oriented silicon steel.The results show that much larger hot rolling deformed microstructure and much stronger {001}〈110〉 texture could be obtained by increasing the soaking and hot rolling temperatures,which had good heritable effects on subsequent microstructural,textural evolution and magnetic properties.The final sheets ...
RH精炼喂CaSi线去除无取向硅钢中的非金属夹杂物
结合工业化生产的无取向硅钢,进行了RH精炼喂CaSi线去除钢中的非金属夹杂物试验研究。针对不同的钙处理条件,分析了CaS夹杂生成热力学,观察了夹杂物的形貌和尺寸分布,确定了夹杂物的类型、数量,探讨了钙处理后钢中夹杂物的变化规律。结果表明,本试验条件下,钙处理可以有效抑制MnS、AlN夹杂物的生成,有效促进钢中微细夹杂物的聚合、上浮、去除,钢质纯净度明显提高。经过合适的钙处理后,钢中的夹杂物以独立存在的CaO为主,同时有少量含CaO、SiO2、MgO的复合夹杂,没有发现CaS夹杂存在。这部分夹杂物的尺寸集中分布在2~20μm,数量约为1.8×105个/mm3。 Experimental study on removal of non-metallic inclusions in non-oriented silicon steel obtained from industrial production by CaSi wire feeding during RH refining process was carried out.The thermodynamics of CaS inclusion formation was analyzed,the morphology and the size distribution of inclusions were observed,and the numbers and types of inclusions were also determined for the steel specimens treated under different calcium treatment conditions.Furthermore,the variation of inclusion characte...
冷轧无取向硅钢表面麻面缺陷成因分析及其控制措施
针对某厂DMS森吉米尔轧机生产无取向硅钢表面麻面缺陷的问题,根据生产实际,对其形成原因从乳化液及工作辊两方面因素进行了分析。结果表明:乳化液对麻面缺陷的产生有一定影响,但不是主要因素,主要原因是由于二十辊森吉米尔轧机工作辊辊径较小,轧制相同长度带钢轧辊运转周期较大,容易产生疲劳失效而导致。为此,提出通过调整冷轧工序成品轧制道次的压下率以减小轧制力,从而减小工作辊的磨损疲劳;通过对轧制乳化液浓度、温度的合理控制,以改善润滑效果、提高轧制速度,而进一步缓解轧辊疲劳的改进措施,使该钢厂无取向硅钢麻面缺陷发生率由原来的18%降至0.8%,带钢表面质量明显改善。 For the problem of surface pockmarks of non-oriented silicon steel strip produced by a DMS Sendzimir mill, based on the production practice, the formation causes were analyzed from two aspects of emulsion and working roll. The results show that the emulsion has a certain effect on the formation of surface pockmarks defects, but it is not the main factor. The main reason is that the working roll diameter of the 20-high Sendzimir mill is small, and the running period of the roll rolling the same l...
EB5325涂层液在冷轧无取向电工钢中的应用
介绍了EB5325涂层液的主要性能和中冶新材生产冷轧无取向电工钢所用的涂层设备,通过多次试验摸索出使用EB5325涂层液的工艺,对涂层出现的缺陷进行分析研究,并提出解决方法,使中冶新材生产的冷轧无取向电工钢的涂层质量满足了用户的要求。 This article introduces the main properties of EB5325 and the coating equipments for cold-rolled non-oriented electrical steel. A process using EB5325 coating liquid is made through many time experiments and exploration. The appeared defects in the coating are studied and analyzed,and the solutions are proposed. The coating quality meets clients’ requirements of cold rolled non-oriented electrical steel.
稀土铈含量对1.2%Si无取向电工钢组织、织构及磁性能的影响
在实验室模拟CSP流程制备了不同含量稀土铈(质量分数0~0.018%)的1.2%Si无取向电工钢,并对其进行1 000℃×5min的再结晶退火处理,研究了铈质量分数对无取向电工钢夹杂物、显微组织、再结晶织构和磁性能的影响。结果表明:随着铈质量分数的增加,微细夹杂物数量、再结晶晶粒尺寸、{100}和{110}织构组分、磁感应强度先增后减,{111}织构组分、铁损先减后增;铈的质量分数为0.005 1%时,钢中的夹杂物数量最少,再结晶晶粒尺寸最大,有利织构最多,磁性能最优,铁损P15/50为3.253W·kg-1,磁感应强度B50为1.751T。 Non-oriented electrical steels containing different contents rare earth Ce element(0-0.018wt%) were prepared in the laboratory by simulated CSP(compact strip production)process,and then recrystallization annealing at 1 000 ℃ for 5 min were performed,the effects of Ce content on inclusion,microstructure, recrystallization texture and magnetic properties of non-oriented electrical steels were studied.The results show that with the increase of Ce content,the amounts of fine inclusion,the size of re...
无取向硅钢热轧卷结疤缺陷产生的原因及控制
针对不同牌号的无取向硅钢产生结疤缺陷的难易程度和表面结疤缺陷的外形特征及分布规律,分析了该缺陷产生的原因。通过调整剪前导板的对中度,设置精轧侧导板开度余量及短行程数值,及时修补与更换侧导板,减少带坯与侧导板挤撞程度,有效地降低了结疤缺陷发生率。 This article analyses the cause of the scab defects according to the defects appearance characters and distribution law,degree of difficulty to form scar of non-oriented silicon steel. It can effectively decrease the scabs by different methods,such as adjusting the center line of guide plate,setting the opening margin and short stroke value of the side guide on finishing mill,timely repairing and replacing of side guide,decreasing the collision between the strip and side guide.
冷轧工艺对取向硅钢初次再结晶织构的影响
研究了取向硅钢制备过程中常见的两种冷轧工艺,主要研究了一阶段冷轧与两阶段冷轧+中间退火工艺对初次再结晶组织及织构的影响.结果表明:采用两阶段冷轧+中间退火工艺制备以Cu2S为主抑制剂的取向硅钢,其初次再结晶平均晶粒尺寸为18.1μm,高斯晶粒的体积分数为0.6%,迁移性强的重位点阵晶界(Σ5+Σ9)和高能晶界(20°~45°取向偏差角)所占比例分别为1.8%和50.4%.与一阶段冷轧工艺相比,其初次再结晶晶粒较细,且高斯晶核与特征晶界所占的比例较高,有利于高斯晶粒发生二次再结晶. Two common cold-rolling processes of grain oriented silicon steel and the effects of the single stage cold rolling and tw o-stage cold rolling w ith intermediate annealing processes on the primary recrystallization microstructure and texture w ere investigated. The results revealed that for the grain oriented silicon steel prepared under the tw o-stage cold rolling process w ith intermediate annealing w ith Cu 2 S as the main inhibitor,the average grain size of the primary recrystallization micr...