无取向硅钢的磁性能主要取决于铁素体的晶粒尺寸、晶体织构和钢中的夹杂物。通过合适的化学成分设计以及采用适宜的夹杂物控制技术,可以获得最佳的夹杂物控制效果,使其纯净度大幅度提高或者无害,最终获得磁性能优良的高级别无取向硅钢。同时,为满足节能、环保、高效需求,无取向硅钢正朝着节能降耗、环境友好以及多功能、高效率、易加工等方向发展。 The magnetic properties of non-oriented silicon steel mainly depend on the grain size of ferrite,the crystallographic texture,and the inclusions in the steel.The optimum inclusion control effects can be obtained through a suitable chemical composition design and an appropriate inclusion control technique,and then the liquid steel will get be clean or the inclusion will get be harmless,finally the excellent magnetic property of the non-oriented silicon steel can be obtained.Meanwhile,in order to ... 
2013-03-28 161 5.8

介绍了国内无底层取向电工钢生产技术水平、产量和用途,简述了无底层取向电工钢作为取向电工钢超/极薄带母料及应用于制作大型发电机组铁心、风电等电机铁心和变压器铁心等的情况。 The production technology level,output and application of domestic glassless grainoriented electrical steel were introduced,and the application of glassless grain-oriented electrical steel as parent material of ultra-thin strip of grain-oriented electrical steel and in making large-scale electric generator cores,wind power motor cores and transformer cores were briefly described. 
2022-02-28 182 5.8

选取了三种50W 800无取向电工钢,分析了化学成分、晶粒尺寸、织构、以及200℃时效处理48 h前后的磁性能和第二相粒子析出状态的变化。结果表明,钢板中第二相粒子的分布密度对钢板铁损有最重要的影响。降低钢中C、N元素含量,或改进钢板热加工参数以降低成品钢板中第二相粒子形成元素的过饱和度均有利于明显降低钢板磁时效过程中的铁损增幅。钢板中对磁性能有利的织构也有利于降低钢板铁损的时效幅度。 The evolution of chemical composition,grain size,texture,as well as magnetic property after aging treatment at 200 ℃ for 48 h and distribution of second phase particles precipitation in three selected 50W800 non-oriented electrical steels were analyzed.The results show that the distribution density of second phase particles has great influence on core loss.Reducing C and N content,or improving hot-working parameters to reduce the supersaturation of elements forming second phase particles in prod... 
2011-08-28 177 5.8

变压器D21硅钢铁芯片采用冲压工艺生产。首先对其工艺进行了分析,确定了冲压方案。对产品进行了排样设计,计算了冲压力,确定了压力中心。然后,设计了单工序落料模具,完成了模具装配图。 D21 silicon steel chips for transformer are produced by stamping.First,its stamping process was analyzed and the scheme of the stamping process was determined.The product layout was designed,the punching pressure was calculated,the pressure center was determined.Then,the blanking die with single procedure was designed,the die assembly drawing was completed. 
2013-07-28 104 5.8

【摘要】 <正>为了确保电工钢的产品质量,在生产线...
2014-03-28 103 5.8

选用Q235和Q345钢,在纯锌浴和含钛量分别为0.05%、0.10%、0.15%、0.20%(质量分数)的合金浴中浸镀0.5、1、3、5、8 min。利用扫描电子显微镜和能谱仪研究了钛对热浸镀锌组织和生长动力学的影响,并提出钛对含硅钢铁锌反应抑制作用的机理。结果表明:钛的加入缩短了Γ的孕育期,促进了合金层中δ的生长和ζ的消失,δ的生长依然受扩散控制,呈抛物线生长规律;Zn-0.05%Ti锌浴可以很好的抑制高硅钢的硅反应性;含硅钢热浸镀锌钛合金浴时,在锌浴中会形成锌铁钛三元T相,该相能吸收ζ晶界处富集的硅,从而抑制了铁锌反应。 Both Q235 and Q345 steels were immersed for 0.5 to 8 min in Zn bath with different amount of Ti,ranging from 0 to 0.20 mass%,for galvanization.The effect of Ti in Zn bath on microstructure and growth kinetics of hot-dip galvanizing coatings on the two steels were investigated by means of SEM and EDS analysis.Base on the experiment,the mechanism of Ti additions in controlling Fe-Zn reaction was proposed.The results show that addition of Ti in the zinc bath decreases the incubation time of Γ phase... 
2013-09-28 154 5.8

研究了冷轧95%变形量无取向硅钢不同退火温度(710~1 050℃)下再结晶织构特征.再结晶刚完成时(710℃退火),呈现强γ({111<112>~<134>)与弱{114}<481>织构特征;随退火温度升高至900℃,γ明显减弱,{114}<481>组分持续增强,形成典型的{h,1,1}<1/h,1,2>织构;进一步升温至1 050℃,再结晶织构不再发生明显变化.基于EBSD分析,{114}<481>组分的持续强化可归因于其明显的尺寸优势以及较高频率的高能晶界(取向差角为20°~45°). A non-oriented silicon steel was heavily rolled to 95% reduction and subsequently annealed at 710~1 050 ℃ to investigate recrystallization texture evolution.When annealed at 710 ℃ with complete recrystallization,the texture is characterized by a strong partial γ fiber spreading from {111}<112> to {111}<134> and a weak {114}<481> component.As annealing at 900 ℃,γ fiber is decreased significantly while {114}<481> is increased consistently,producing a typical {h,1,1}<1/h,... 
2013-05-28 177 5.8

【作者】 宋波; 朱一知; ...
2011-10-28 107 5.8

以水氯镁石为原料,采用氨法沉镁-煅烧-添加剂的方法制备硅钢级氧化镁。考察了反应温度、反应pH值、陈化时间对中间体氢氧化镁纯度及转化率的影响;研究了煅烧温度和煅烧时间对氧化镁水化率的影响及添加剂的量对氧化镁悬浮性能的影响。控制实验条件为:反应温度55℃,pH值为9.5,陈化时间2h,煅烧温度1050℃,煅烧时间2h,添加剂量为0.8%,制得氧化镁的纯度为98.99%、水化率为2.92%、悬浮性能为3mm/h,达到硅钢级氧化镁的要求。 Using bischofite as raw material,the preparation of magnesium oxide with silico-steel grade was studied.The effects of reaction temperature,reaction pH value and aging time on the intermediate magnesium hydroxide purity and conversion rate were studied.Calcinations temperature,calcinations time relationship to the hydration rate of MgO and amount of additive to the suspension performance of MgO were investigated.The results indicated that the optimum technological conditions were as follows:reac... 
2023-05-09 190 5.8

文章以国内某公司硅钢厂连续退火机组1号辐射管加热段为研究对象,分析炉内传热机理,建立并开发了辐射管加热段的传热模型。采用生产实际数据对模型进行了验证,以总燃料消耗量最小为目标,得出该炉段长度方向上燃料的最佳分配机制。所得结论为该公司连续退火机组节能控制提供理论依据。 Taking the radiant tube heating section of No.1 continuous annealing unit in a silicon steel plant of a domestic company as the research object, the heat transfer mechanism in the furnace is analyzed, and the heat transfer model of the radiant tube heating section is established and developed. The model is verified by the actual production data. Aiming at the minimum total fuel consumption, the optimal fuel distribution mechanism in the length direction of the furnace section is obtained. The co... 
2022-01-28 137 5.8

利用本钢技术中心试验厂技术手段,并与北京钢铁研究院合作,试制了用作家电用电机、微电机、小电机或部分中型电机铁芯的冷轧无取向电工钢。试制钢硅含量小于0.5%,钢板表面平滑,公称厚度0.5mm,且厚度均匀偏差小,性能测定结果表明,产品的磁性能、力学性能满足其使用要求。 BX STEELTechnology Center pilot plant using technical means,and with Beijing Iron and Steel Research Institute,trial cold rolled non-oriented electrical steel that has been used as appliance motor core,micro motor core,small motor core,or part of the medium-sized motor core。Trial steel of silicon content is less than 0.5%,steel plate surface is smooth,the nominal thickness of 0.5mm,and the thickness deviation is small,performance measurement results show that the magnetic properties,mechanical p... 
2011-01-28 186 5.8