钢厂
制备{100}织构无取向电工钢方法综述
{100}织构因具有两个易磁化方向能够明显的提高磁性能,因此如何在表面获得具有{100}织构一直是无取向电工钢研究焦点。本文主要介绍了获得{100}织构的主要工艺方法及其基本原理,并结合实际生产过程对各工艺方法的优缺点进行了分析;一方面,优化无取向电工钢的成分,降低碳、锰元素含量以避免脱碳退火和真空退火,简化生产工艺;另一方面,调节升温速度、降温速度和退火气氛,使{100}晶面的表面能或弹性应变能最低,制备具有{100}织构柱状晶组织的无取向电工钢是今后的发展方向。 Because { 100} texture has two easy magnetization directions,which can significantly improve magnetization properfies,how to develop { 100} texture is a focus for researchers and manufactures. In the paper,main manufacturing processes and basic principle are introdued,and their advantages and disadvantages in practical production are analyzed. On the one hand,the production process can be simplified by optimizing chemical compositions,such as reducing the content of C and Mn,which can avoid deca...
晶界位向对硅钢立方/旋转立方取向双晶轧制取向变化的影响
晶界和{100}柱状晶在硅钢生产过程中对织构的遗传和演变有关键作用,因此本文利用晶体塑性有限元方法进行立方和旋转立方取向双晶在晶界不同位向时晶体取向演变的全场模拟。模拟显示,三种晶界位向下,晶界都具有诱发晶内产生S形状形变不均匀和缓解局部形变不均匀区取向转动的特点,立方和旋转立方取向双晶在带有剪切作用的轧制条件下都显示明显的取向稳定性。GB⊥RD(表示晶界垂直于轧向)晶界位向时,旋转立方取向晶粒优先在晶界中心位置发生取向转动,而立方取向则优先在远离晶界的端部发生取向转动。GB⊥TD(表示晶界垂直于横向)的晶界位向下,其晶界阻碍作用最小,双晶内产生的取向漫散度大,织构强度较低;除绕TD转动外,也具有复杂的绕RD、ND的取向转动。GB⊥ND(表示晶界垂直于法向)的晶界位向下,取向转动与GB⊥RD时相近,但有少量取向绕ND转动。 Grain boundaries and initial{100}columnar grains play a key role in the inheritance and evolution of texture in the production of electrical steels.In this paper,the crystal plasticity finite element method was used to simulate the grain orientation evolution of cube and rotated-cube oriented bicrystals when grain boundary was set to different orientations.It was shown that the grain boundary in three grain boundary orientations demonstrated the characteristics of inducing Sshape deformation inh...
初次再结晶退火工艺对3%Si取向硅钢组织和织构的影响
试验研究了0.3 mm取向硅钢冷轧板(/%:0.046C,3.07Si,0.09Mn,0.029P,0.004S,0.005A1)的退火温度(760~880℃7 min)和退火时间(820℃3~9 min)对该钢的晶粒尺寸,再结晶和织构的影响。结果表明,最佳初次再结晶退火工艺为820℃5 min,该钢的平均晶粒尺寸为14.20μm,完全再结晶率为92%,不利{111}<110>结构含量为3.16%,有利织构{111}<112>,{012}<001>和高斯织构含量分别0.40%,4.73%和2.46%。 The effect of annealing temperature(at 760 ~ 880 X.for 7 min) and time(at 820℃ for 3~9 min) on grain size,recrystallization rate and texture of 0.3 mm cold-rolled sheet of oriented silicon steel(/%:0.046C,3.07Si,0.09Mn,0.029P,0.004S,0.005Al) has been tested and studied.Results show that with optimum recrystallized annealing at 820℃ for 5 min,the silicon steel average grain size is 14.20 fun,the complete recrystaUization rate is 92%,the unfavourable-texture {111}< 110 > content in steel is ...
CSP流程试制50W270高牌号无取向硅钢织构的演变
研究了CSP流程试制50W270高牌号无取向硅钢热轧→常化→冷轧→退火过程中织构的演变.利用电子背散射衍射技术对全流程织构进行测量和分析.发现热轧板织构在厚度方向上存在较大差异,表层主要为铜型、黄铜和高斯织构,1/4层存在微弱的高斯织构和旋转立方织构,中心层以γ纤维织构和旋转立方织构为主,还含有较弱的α纤维织构.与热轧板相比,常化板表层和1/4层织构变化不大,中心层旋转立方织构和α纤维织构增强.冷轧板各层均具有α纤维织构和γ纤维织构.与冷轧板相比,成品板各层中α纤维织构基本消失,还出现了立方织构和高斯织构. This article focuses on texture evolution in 50W270 high-brand non-oriented silicon steel produced by CSP in hot rolling,normalizing,cold rolling,and annealing processes.The texture in the whole process was measured and analyzed by electron back-scatter diffraction.It is found that the texture along the thickness direction in hot-rolled strips changes obviously;there are mainly copper,brass,and Goss textures in the surface layer;the 1/4 layer has weak Goss texture and rotating cube texture;γ-fib...
无取向电工钢表面线状缺陷的影响因素分析
结合扫描电镜和大样电解研究了CSP流程W800牌号无取向电工钢表面线状缺陷中夹杂物成分及来源,采用SPSS软件回归分析了生产过程各因素对表面线状缺陷的影响。研究表明:稳态浇铸过程铸坯中大型夹杂物含量为5.39 mg/10 kg。引起无取向电工钢表面线状缺陷的大型夹杂物主要为脱氧产物、镁铝尖晶石和钢包顶渣,主要类型为Al2O3、MgO-Al2O3、CaO-Al2O3-MgO和CaO-Al2O3-SiO2。非稳态浇铸过程钢水洁净度明显降低,热轧板表面线状缺陷比例上升。影响表面线状缺陷的主要因素为RH出站时顶渣的w(CaO)/w(Al2O3)、RH脱氧结束氧位及中间包最低吨位。 Combining scanning electron microscopy and large sample electrolysis, the composition and source of inclusions in the surface linear defects of W800 grade non-oriented electrical steel in the CSP process were studied. SPSS software was used to regress and analyze the main factors which affected the surface linear defects in the steelmaking process. Research shows that the content of large inclusions in the steady state casting process is 5.39 mg/10 kg. The large inclusions which cause linear def...
日本取向电工钢生产工艺最新研发进展
根据相关的取向电工钢典型专利技术,概述了日本高磁感低铁损取向电工钢低温板坯加热、抑制剂合理调节、关键成分Mn、C、Sn和Sb调节与利用、新型退火剂和绝缘溶液的制备及细化磁畴等生产工艺最新动态和进展情况,并提出了国内企业申请取向电工钢专利时应当借鉴之处。 According to related typical patent technology for grain-oriented electrical steel sheets,the recent trends and progress situation for production process of grain-oriented electrical steel sheets with high magnetic flux density and low core loss in Japan are summarized including low temperature slab heating,suitably regulating inhibitors,adjusting and utilizing key element Mn,C,Sn and Sb,manufacturing for new annealing agent and insulating solutions,and fining magnetic domain,and some suggestion...
高硅钢薄板退火过程中的织构演变
采用传统的轧制和退火工艺制备了0.30mm厚的6.5%(质量分数)Si高硅电工钢薄板,采用X射线衍射技术对退火过程中的再结晶织构进行了研究。冷轧高硅钢薄板700℃退火形成以{111}〈112〉为峰值的γ织构(〈111〉∥ND)和以{001}〈210〉为峰值的{001}织构;而900℃以上温度退火则形成强{001}〈210〉织构。进一步的研究表明是在晶粒长大过程中{001}〈210〉发展成为主要再结晶织构组分。 High silicon steel thin sheets with thickness of 0.3mm were successfully produced by conventional rolling and annealing methods.Recrystallization texture was investigated by means of X-ray diffraction.It is found that recrystallization texture is mainly composed of γ fiber(〈111〉∥ND)with peak at {111}〈112〉 and {001} fiber with peak at {001}〈210〉 after annealing at 700℃,while strong {001}〈210〉 component dominates recrystallization texture after annealing above 900℃.It is during grain growth that {...
硅钢轧制过程中乳化液流量数学模型研究及应用
目前高磁感冷轧硅钢生产过程中,采用经验方法确定的乳化液流量设定值往往会造成硅钢产品的磁感性能达不到预期目标,针对此情况,基于轧机轧制机理研究了的乳化液流量数学模型,确定了乳化液流量设定值。实践表明,使用该数学模型输出的乳化液流量设定值,可提高轧制过程中乳化液流量控制精度,从而提高高磁感冷轧硅钢的轧制性能。 In view of the current production process of high magnetically inductive cold-rolled silicon steel, the mathematical model of emulsified fluid flow based on mill rolling mechanism is studied in view of the situation in which the magnetic sensing performance of silicon steel products is often not up to the expected target by using empirical method to determine the emulsified liquid flow setting. Practice shows that the emulsified fluid flow setting value output from this mathematical model improv...
电工钢显微结构和疲劳性能的研究
研究了电工钢SXRC的显微结构和疲劳性能,并与DP钢进行了比较。结果表明,退火温度低温化能够有效的抑制电工钢的再结晶。该钢在固溶铌的作用下,能够在保证电机磁性的同时具有一定的强度。与DP钢相比,SXRC钢的抗疲劳性能更好。 The microstructures and fatigue properties of the electrical steel SXRC we re investigated, and the properties were also compared with the steel DP. The results show that the recrystallization of the electrical steel can be suppressed at lower annealing temperature. The steel presents favorable motor magnetic and also a compatible strength with the help of solid-solution Nb. Compared with the steel DP, the fatigue resistance of the steel SXRC is preferable.
热轧组织对无取向硅钢织构的影响
采用X射线衍射仪分析无取向硅钢冷轧织构和再结晶退火织构的演化,研究了热轧组织对无取向硅钢织构以及磁性能的影响。结果表明,具有均匀、粗大晶粒组织的热轧板,冷轧形成更多的剪切带,导致成品板形成高的高斯织构组分,并提高了{100}织构强度,降低了γ纤维织构,最终导致成品磁感应强度升高,铁损下降。 The texture evolution of non-oriented silicon steel during cold-rolling and recrystallization annealing was investigated by X-ray diffractometer.The effects of hot band microstructure on the texture and magnetic properties of non-oriented silicon steel were analyzed.The results show that more shear bands appear during cold rolling due to homogeneous coarse grain in hot band.So strong{110}<001> texture after recrystallization annealing forms.At the same time,the {100} texture components inc...