钢厂
晶界位向对硅钢立方/旋转立方取向双晶轧制取向变化的影响
晶界和{100}柱状晶在硅钢生产过程中对织构的遗传和演变有关键作用,因此本文利用晶体塑性有限元方法进行立方和旋转立方取向双晶在晶界不同位向时晶体取向演变的全场模拟。模拟显示,三种晶界位向下,晶界都具有诱发晶内产生S形状形变不均匀和缓解局部形变不均匀区取向转动的特点,立方和旋转立方取向双晶在带有剪切作用的轧制条件下都显示明显的取向稳定性。GB⊥RD(表示晶界垂直于轧向)晶界位向时,旋转立方取向晶粒优先在晶界中心位置发生取向转动,而立方取向则优先在远离晶界的端部发生取向转动。GB⊥TD(表示晶界垂直于横向)的晶界位向下,其晶界阻碍作用最小,双晶内产生的取向漫散度大,织构强度较低;除绕TD转动外,也具有复杂的绕RD、ND的取向转动。GB⊥ND(表示晶界垂直于法向)的晶界位向下,取向转动与GB⊥RD时相近,但有少量取向绕ND转动。 Grain boundaries and initial{100}columnar grains play a key role in the inheritance and evolution of texture in the production of electrical steels.In this paper,the crystal plasticity finite element method was used to simulate the grain orientation evolution of cube and rotated-cube oriented bicrystals when grain boundary was set to different orientations.It was shown that the grain boundary in three grain boundary orientations demonstrated the characteristics of inducing Sshape deformation inh...
电力系统绝缘子防污闪纳米硅钢涂层应用研究
为了更好的解决电力系统防污闪涂料RTV-Ⅰ长期应用暴露出来的问题以及目前RTV-Ⅱ防污闪涂料存在的一些不足,结合具体实际需求,在电力系统外绝缘领域,应用新型防污闪硬质涂层——防污闪纳米硅钢涂层,并对分别喷涂了防污闪纳米硅钢涂层以及RTV涂料的绝缘子进行对比运行情况研究分析。研究结果表明,防污闪纳米硅钢涂层是一种同时具有优异憎水性迁移性能和自洁性能的新型涂层,具有良好的应用前景。 In order to solve the problem exposed of anti-pollution flashover coating RTV-Ⅰwhich has been used long-term in power system,as well as to better solve some shortcomings of the current anti-pollution flashover coating RTV-Ⅱ,in this paper,a new anti-pollution flashover hard coating — anti-pollution flashover nanometer silicon hard coating(NSHC) is applied in the field of power system insulation for the specific practical needs.At the same time insulators which are separately sprayed by the NSHC a...
水氯镁石制备硅钢级氧化镁
以水氯镁石为原料,采用氨法沉镁-煅烧-添加剂的方法制备硅钢级氧化镁。考察了反应温度、反应pH值、陈化时间对中间体氢氧化镁纯度及转化率的影响;研究了煅烧温度和煅烧时间对氧化镁水化率的影响及添加剂的量对氧化镁悬浮性能的影响。控制实验条件为:反应温度55℃,pH值为9.5,陈化时间2h,煅烧温度1050℃,煅烧时间2h,添加剂量为0.8%,制得氧化镁的纯度为98.99%、水化率为2.92%、悬浮性能为3mm/h,达到硅钢级氧化镁的要求。 Using bischofite as raw material,the preparation of magnesium oxide with silico-steel grade was studied.The effects of reaction temperature,reaction pH value and aging time on the intermediate magnesium hydroxide purity and conversion rate were studied.Calcinations temperature,calcinations time relationship to the hydration rate of MgO and amount of additive to the suspension performance of MgO were investigated.The results indicated that the optimum technological conditions were as follows:reac...
余热利用系统在硅钢连续退火机组中的应用
介绍了烟气余热利用系统的工艺流程及控制思想,结合该系统在钢厂硅钢连续退火机组中的应用实践,估算出烟气余热利用系统每年可节约蒸汽5 040 t,经济效益良好,同时分析了该系统存在的问题及对策。 Introduced a method about the process and control of the application of waste heat system, which had been used into a silicon steel continuous annealing line and profiting a good economic benefit by saving a large number of steam every year, which has been estimated about 5 040 tons, and analyzed the problems and solutions existed in this system.
无取向硅钢铬酸镁绝缘涂层结构与耐蚀性能研究
采用扫描电镜、原子力显微镜研究了铬酸镁半无机绝缘涂层的微观结构。结果表明,涂层厚度为数微米,涂层中的有机树脂乳液颗粒均匀分布在无机涂层的表面,从而保证了涂层具有良好的冲片性能。采用极化曲线研究了涂层的耐蚀性能,发现铬酸镁与铬酸锌绝缘涂层的耐蚀性能相当。 In this paper,the microstructure and anti-corrosion property of magnesium chromate coating on non-oriented silicon steel were studied.The microstructure was observed by SEM and AFM.The anti-corrosion properties were evaluated by polarization curves.The results show that the thickness of coating is several microns and the polymer particles were scattered on the surface of inorganic coating,which is the guarantee for lamination property.The corrosion resistance of the magnesium chromate film was e...
硅钢连续退火生产线设备改造
针对硅钢连续生产线设备存在的故障、隐患以及精度等影响产品质量的问题进行分析及改造,实现保证生产线设备稳定运行、提高设备精度及硅钢产品质量的目的。 This paper analyzes and transforms the electrical equipment failures, risks existed in slicon continuous production line, and the effect of accuracy to product quality, in order to ensure stable operation of equipment in production line and improve the accuracy of device, quality of silicon.
低铁损高磁通密度无取向硅钢的应用与生产技术进展
分析了高转矩和高转速条件下高效驱动马达铁芯材料对无取向硅钢磁性能要求,讨论了无取向硅钢的高磁通密度和低铁损对电机转矩和效率的影响,介绍了国内外高磁感无取向硅钢发展情况。在生产工艺上,提高钢质纯净度,弱化夹杂物和第二相粒子对畴壁移动和再结晶晶粒长大的钉扎作用,添加微量晶界和带钢表面的偏析元素促使有利织构发展等技术可提高无取向硅钢的磁通密度。 The requirements of high efficient drive motor core materials under the conditions of high torque and high speed were analyzed.The effects of high magnetic flux density of non-oriented silicon steel on the torque and efficiency of the motor were discussed.The development of non-oriented silicon steel with high magnetic was introduced.The magnetic flux density of non-oriented silicon steel sheet can be obviously improved by some production technologies,such as purification steel,weakening the pin...
取向硅钢含铬无机绝缘涂层的研究进展
绝缘涂层可以有效提高硅钢片的耐蚀、耐腐、磁、绝缘等性能,因此取向硅钢涂装绝缘涂层是取向硅钢生产过程中重要的一环。本文对取向硅钢含铬无机绝缘涂层以及氮化铬涂层的性能优缺点进行了介绍,并对国内无机含铬取向硅钢绝缘涂层及氮化铬涂层的研究现状进行了综述。最后对未来含铬无机绝缘涂层的研发方向进行了展望。 Insulation coating can effectively improve the corrosion resistance of silicon steel sheet, such as corrosion, magnetic, insulation performance, thus oriented silicon steel insulation coating is the important part of oriented silicon steel production process. In this paper, the inorganic insulation coating oriented silicon steel containing chromium and chromium nitride coating performance advantages and disadvantages are introduced.In addition, the research status of insulation coating and chrom...
高牌号无取向硅钢CSP流程铸坯及热轧板的组织和夹杂物分析
2.9 mm热轧3%Si高牌号无取向硅钢板(/%:0.004 6C、3.04Si、0.32Mn、0.49Als、0.004S、0.013P、0.0042N)由CSP(Compact Strip Production紧凑式带材生产线)流程:120 t BOF-70 mm CC-热轧工艺生产。热轧终轧温度872℃,卷取温度683℃。铸坯及热轧板的组织和夹杂物的分析结果表明,铸坯组织为典型的贯穿柱状晶组织;热轧板边部为再结晶组织,中部为纤维组织带有少量再结晶晶粒;高牌号无取向硅钢的主要夹杂物为铸坯-Al2O3,AlN和Cu2S+MnS;热轧板-Al2O3,AlN,AIN+MnS和Cu2S+MnS。 The 2.9 mm hot rolled 3%Si high grade non-oriented silicon steel plate(/%:0.004 6C,3.04Si, 0.32Mn,0.49Als,0.004S,0.013P,0.004 2N) is produced by CSP(Compact Strip Production) flow sheet i.e.120 t BOF-70 mm CC-hot rolling process with end rolling at 872℃and coiling at 683℃.The analysis results on structure and inclusions in casting slab and hot rolled plate show that the structure of slab is typical trans-columnar crystal,the structure of hot rolled plate at edge is recrystallized grain and in ce...
无取向硅钢热轧卷结疤缺陷产生的原因及控制
针对不同牌号的无取向硅钢产生结疤缺陷的难易程度和表面结疤缺陷的外形特征及分布规律,分析了该缺陷产生的原因。通过调整剪前导板的对中度,设置精轧侧导板开度余量及短行程数值,及时修补与更换侧导板,减少带坯与侧导板挤撞程度,有效地降低了结疤缺陷发生率。 This article analyses the cause of the scab defects according to the defects appearance characters and distribution law,degree of difficulty to form scar of non-oriented silicon steel. It can effectively decrease the scabs by different methods,such as adjusting the center line of guide plate,setting the opening margin and short stroke value of the side guide on finishing mill,timely repairing and replacing of side guide,decreasing the collision between the strip and side guide.
硅钢常化炉段工艺特征及问题分析
连续酸洗退火机组(CPAL)对于当前生产高磁感取向硅钢和高牌号无取向硅钢是必不可少的一个环节。常化炉是常化酸洗机组关键的组成部分。本文对国内自主建造的两条退火酸洗机组的工艺流程,特别是常化炉段进行了对比分析。总结出了常化炉的工艺及组成特点,对生产过程中暴露的问题进行了仔细的分析并提出了改进的意见,对于以后新建常化炉具有一定的提示作用。 The continous pickling annealing line(CPAL) is an essential step in producing high magnetic induction grain-oriented silicon steel and high grade non-oriented silicon steel.The normalizing furnace is a very important part of the CAPL.In this paper,the process flows of two CAPL with independent manufacture in our country have been compared,especially the part of normalizing furnaces.The characteristics of process and component are summarized and problems of the normalizing furnace during the prod...
无取向硅钢钙处理前后夹杂物的行为研究
研究了无取向硅钢钙处理前后夹杂物的行为,重点考察了钙处理前后夹杂物的成分、类型、形貌和尺寸研究的变化情况,为实际生产中无取向硅钢的钙处理提供理论指导。试验发现:钙处理前夹杂物主要以Al2O3、Al2O3-MgO为主,且在夹杂物表面有AlN析出,钙处理后夹杂物以Al2O3-MgO-CaS-CaO系复合夹杂物为主,还含有少量的SiO2或AlN;钙处理前后,夹杂物形貌由多边形或不规则形逐渐向球形或近似球形转变,并且夹杂物尺寸不断增大;钙处理前后,含钙夹杂物的比例发生突变,由10%增大到74.5%,且随着钙处理时间的延长,含钙夹杂物比例下降,表明钙处理使夹杂物变性后易聚集长大并上浮去除。 Behavior of inclusions before and after calcium treatment in non-oriented silicon steel was researched by investigating changes of compositions,types,shapes and sizes of inclusions before and after calcium treatment,for the purpose of providing theoretical guidance for calcium treatment of non-oriented silicon steel in actual situation. Results indicated that Al2O3 and Al2O3-MgO were main types of inclusions before calcium treatment,sometimes AlN maybe precipitate in the outer of inclusions. Al2...