钢厂
硅钢铸坯感应加热炉参数优化设计
采用经验设计法初步确定了取向硅钢铸坯感应加热线圈设计参数,应用Ansoft仿真软件分别对36组不同线圈高度、线圈内径的感应加热炉在不同频率下的三维整体磁场和铸坯的温度场进行了数值仿真。通过对比仿真结果,确定电磁场分布最佳的一组感应加热炉设计参数为线圈高度h=1.50 m、线圈内径D1=0.575 m、电流频率f=110 Hz。在该参数下应用Ansoft仿真软件对取向硅钢铸坯感应加热炉的温度场进行了仿真,结果发现温度场分布均匀,可满足取向硅钢铸坯加热要求。 The induction heating coil design parameters for the oriented silicon steel casting blank were determined preliminary by experience design method,and 36 groups three-dimensional electromagnetic field with different height and inside diameter of coil under different frequencies of the induction heating furnace and the temperature field of the casting blank were investigated by numerical simulation using Ansoft simulation software. By comparing the simulation results of electromagnetic field distr...
新能源车驱动电机用电工钢用量解析计算及预测方法
对新能源汽车以及驱动电机的现有市场和未来市场规模进行梳理分析,通过自建计算公式推导出我国2021年1-11月份驱动电机用电工钢的总量,进而预测未来10年中国新能源汽车驱动电机用电工钢情况,为无取向电工钢的生产和在电机中的应用提供有价值的参考。 The current market and future market size of new energy vehicles and traction motors were analyzed,and the total amount of electrical steels used in traction motors in China from January to November 2021 was derived by using self-built calculation formulas,and then the situation in the next ten years of electrical steel used in traction motors of new energy vehicles in China was predicted.It will provide a valuable reference for the production of non-grain oriented electrical steel and its appli...
新日铁高强度无取向电工钢的研究进展
针对新日铁公开的相关专利,总结日本高强度无取向电工钢的研究进展,分析了各专利化学成分、生产工艺及产品性能的特点,指出固溶强化、细晶强化、析出强化、位错强化都有可能被用来提高无取向电工钢的强度。在高强度无取向电工钢的研发过程中,需要根据其具体用途确定目标性能,再采用合适的强化手段,从而实现力学性能、磁性能和生产性能之间的平衡。 Authors summarize the research progress of high strength non-oriented electrical steel in Japan by learning related patents brought into the public by Nippon Steel. Authors also analyze the characteristics of the chemical composition, production technology and properties of products in the patents and point out that any ones of solution strengthening method, fine-grain strengthening method, precipitation strengthening method or dislocations strengthening method may be used to improve the strengt...
高效电机用无取向硅钢退火板组织和析出物研究
研究了组织和析出物对高效电机用无取向硅钢退火板磁性能的影响。结果表明:随着退火温度升高,退火板平均晶粒尺寸增加,P15/50明显降低,B50略有升高。退火温度在1 000℃时,退火板的综合性能较好。析出物主要是AlN、(MnS+AlN)和(MnS+Al2O3)复合析出物,尺寸较粗大,主要集中在1.0~2.5μm,还发现少量百纳米以下的细小AlN和TiN。实验室模拟TSCR流程试制的高效电机用无取向硅钢,铁损平均值小于4.00 W/kg,磁感应强度大于1.75 T,适合作中小型高效电机铁芯材料。 Effects of microstructure and precipitation on magnetic property of non-oriented silicon steel sheets after annealing for high-efficiency motor are studied in the paper by experiments.The annealed sheet exhibits a larger average grain size,obviously decreasing iron loss and slightly raising magnetic induction with increasing temperature.The annealed sheet has better comprehensive properties at a annealing temperature of 1 000 ℃.The main precipitates are compounds of AlN、(MnS+AlN)and(MnS+Al2O3) w...
薄板坯连铸连轧流程生产高磁感取向硅钢的研究现状与技术分析
概述了高磁感取向硅钢生产工艺的研究现状及发展趋势。介绍了国内外薄板坯连铸连轧流程生产高磁感取向硅钢的研究现状。从流程工序特点、热履历、组织与抑制剂控制方面进行对比,分析了薄板坯连铸连轧流程相对传统板坯流程生产高磁感取向硅钢的技术优势,在此基础上提出了利用该流程生产高磁感取向硅钢需要解决的主要技术难点。 The current status and development trend of production process for high magnetic induction grain-oriented silicon steel are summarized.The research status of producing high magnetic induction grain-oriented silicon steel by thin slab casting and rolling process at home and abroad is introduced.The potential technical advantages of producing high magnetic induction grain-oriented silicon steel by thin slab casting and rolling process are obtained by analyzing in terms of process characteristics,t...
无取向硅钢成品钢卷头、尾磁性能差异探讨
结合工业化生产过程中出现的同卷带钢头、尾磁性能差异现象,对50SW1300牌号无取向硅钢同卷带钢头、尾试样的夹杂物、晶体织构和显微组织进行了分析研究。结果表明,夹杂物、晶体织构是影响成品钢卷磁性能的重要因素。夹杂物是造成同卷带钢头、尾铁损差异的主要原因。夹杂物数量越多,尤其是小尺寸的夹杂物数量越多,对成品带钢的磁性能影响越大,对于本试验而言,AlN和MnS是影响成品带钢磁性能的主要夹杂物。晶体织构是造成同卷带钢头、尾磁感应强度差异的主要原因。有益的{100}和Goss织构含量越大,有害的{111}<110>和{111}<112>织构含量越小,即有益织构与有害织构含量比越大,成品带钢的磁感应强度越大。 Based on the industrial manufacture of non-oriented silicon steel sheets 50SW1300, the magnetic property variation of head and tail of the same finished steel sheets was discussed by analyzing non-metallic inclusion, crystal texture, and microstructure. Results show that, both of the non-metallic inclusion and the crystal texture will affect the magnetic properties significantly. The non-metallic inclusion is the key factor of the core loss variation of head and tail of the same finished steel s...
二次冷轧法对薄带连铸无取向高硅钢组织和磁性能的影响
采用双辊薄带连铸技术试制了3.98%Si-0.71%Al无取向硅钢铸带,研究了二次冷轧法对硅钢组织和磁性能的影响。结果表明:硅钢铸带显微组织为等轴晶组织,铸带再结晶较完全,常化对铸带显微组织影响较小。二次冷轧工艺和一次冷轧工艺下,最终退火后成品显微组织为等轴晶组织,二次冷轧法最终退火后的晶粒尺寸小于一次冷轧法。二次冷轧法能够提高成品磁性能. Effect of double cold rolling on magnetic properties and microstructure of 3.98%Si-0.71%Al non-oriented silicon Steel Sheets cast by twin-roll thin strip casting process were investigated.The results show that the structure of the thin strip is equiaxed crystal,the recrystallization is complete and normalizing has lesser effect on microstructure.Using both cold rolled and double cold rolled process,the microstructure is equiaxed grain after final annealing.The average grain size of annealed shee...
210 t BOF-RH-CC炼钢过程无取向硅钢XG800WR洁净度的试验研究
两炉次无取向硅钢XG800WR(/%:0.003~0.004C、0.71~0.75Si、0.32~0.33Mn、0.004~0.007S、0.016P)的炼钢流程为铁水预处理(KR)-210 t顶底复吹转炉-钢包吹氩-RH脱碳精炼-230mm×1220 mm板坯连铸。53 t中间包钢水过热度为25~30℃,钢包到中间包采用长水口全程吹氩保护浇铸,中间包至结晶器采用浸入式水口浇铸。结果表明,在RH、中间包、结晶器过程中钢中总氧以及夹杂物数量和尺寸均明显降低;但在钢包到中间包过程T[O]、[N]和钢中夹杂物数量增加,说明长水口浇铸过程存在二次氧化。连铸坯中T[O]、[N]平均他分别为11×10-6和30×10-6,显微夹杂物数量平均为4个/mm2。铸坯中的显微夹杂物主要为3~5μm的AlN,同时存在少量的MnS、Al2O3·AlN和Al2O3·MgO·MnS。 The steelmaking flow sheet for two heats non-oriented silicon steel XG800WR(/%:0.003~0.004C. 0.71~0.75Si,0.32~0.33Mn,0.004~0.007S,0.016P) is hot metal pretreatment(KR)-210 t top and bottom combined blown converter-ladle argon blowing-RH decarburization refining-230 mm×1 220 mm slab casting.The superheating extent of liquid in 53 t tundish is 25~30℃,whole casting is shielded by blowing argon with long nozzle from ladle to tundish and the submerged nozzle is adopted in casting from tundish to mold...
ICP-AES法测定硅钢中铌的不确定度评定
分析了电感耦合等离子体发射光谱法(ICP-AES)测定硅钢中铌的检测过程,讨论了该检测过程中不确定度的主要来源,建立了该方法的定量的数学模型,并根据这一模型计算出了检测结果的合成标准不确定度和扩展不确定度。 The measurement of niobium content in silicon steel by inductively coupled plasma atomic emission spectrometry(ICP-AES) was analyzed,by which the main factors affecting the uncertainty of the measurement were ascertained and the calculation formula was given.Finally,according to the formula the combined uncertainty and expanded uncertainty were obtained.
锰含量对无取向电工钢组织性能的影响
研究了锰含量对w(Si)=1.8%Si无取向电工钢组织和性能的影响。结果表明,钢中锰含量从0.3%增加到1.2%时,由于α_γ相变的产生,铸坯低倍组织、热轧板金相组织及成品织构等均发生了不同程度的变化,对成品表面质量及磁性能产生了明显的影响。 The effects of manganese content on structure and properties of w(Si)=1.8% non-oriented electrical steels have been studied.Results show that with increasing manganese content to 1.2% from 0.3%,macrostructure of continuous casting slab,hot rolled band metallurgical structure and finished product texture vary in some extent because of the occurrence of α-γ phase transformation,the surface quality and magnetic properties of finished product are affected greatly.
无取向硅钢磷酸盐型杂化涂层性能测试
以质量分数为25%的丙烯酸乳液MC-102、15%Al(H2PO4)3溶液、0.01%H3BO3、0.01%Zn(Ac)2·2H2O和2%二乙二醇丁醚组分,在不同固化工艺下制备涂层。极化曲线和电导率测试发现300℃处理60 s得到的涂层具有良好的耐腐蚀性和绝缘性;水煮实验证明该涂层具有良好的耐水性;断口线扫描发现涂层具有良好的附着性。 A formula comprising MC-102 acrylic emulsion 25%,aluminium dihydrogen phosphate15%,boric acid 0. 01%,zinc acetate dihydrate 0. 01% and diethylene glycol monobutyl ether 2% was used to prepare coatings via different treatment process. The conductivity test and polarization curves revealed that a coating cured at 300 ℃ for 60 s showed good insulative and anticorrosive properties. The water boiling test indicated that the said coating had good water resistance. A cross section of the coating was in...