所有分类
  • 所有分类
  • 未分类

常化快冷是生产高牌号无取向硅钢和高磁感取向硅钢不可缺少的一个工艺环节,气-雾冷却则是实现常化快冷的关键方式之一。介绍了国内自主设计建设的常化酸洗机组气雾冷却系统的技术特性,并对其特点进行了系统分析,最后给出该系统在设计、运行参数的选择上若干注意事项,对气-雾冷却系统设计和使用具有一定的指导作用。 The normalizing rapid cooling is a indispensable process to high grade non-oriented silicon steel and high magnetic induction oriented silicon steel’ s production. The fog cooling is a key ways of coming true the normalizing rapid cooling. This paper introduces the technical features of the fog cooling system in normalizing pickling line which is the domestic independent design and construction. Meanwhile,the fog cooling system’s characteristic is analyzed systematacially. In the end,this paper ... 
2014-03-28 164 5.8

2.9 mm热轧3%Si高牌号无取向硅钢板(/%:0.004 6C、3.04Si、0.32Mn、0.49Als、0.004S、0.013P、0.0042N)由CSP(Compact Strip Production紧凑式带材生产线)流程:120 t BOF-70 mm CC-热轧工艺生产。热轧终轧温度872℃,卷取温度683℃。铸坯及热轧板的组织和夹杂物的分析结果表明,铸坯组织为典型的贯穿柱状晶组织;热轧板边部为再结晶组织,中部为纤维组织带有少量再结晶晶粒;高牌号无取向硅钢的主要夹杂物为铸坯-Al2O3,AlN和Cu2S+MnS;热轧板-Al2O3,AlN,AIN+MnS和Cu2S+MnS。 The 2.9 mm hot rolled 3%Si high grade non-oriented silicon steel plate(/%:0.004 6C,3.04Si, 0.32Mn,0.49Als,0.004S,0.013P,0.004 2N) is produced by CSP(Compact Strip Production) flow sheet i.e.120 t BOF-70 mm CC-hot rolling process with end rolling at 872℃and coiling at 683℃.The analysis results on structure and inclusions in casting slab and hot rolled plate show that the structure of slab is typical trans-columnar crystal,the structure of hot rolled plate at edge is recrystallized grain and in ce... 
2013-04-28 162 5.8

研究了CSP流程试制50W270高牌号无取向硅钢热轧→常化→冷轧→退火过程中织构的演变.利用电子背散射衍射技术对全流程织构进行测量和分析.发现热轧板织构在厚度方向上存在较大差异,表层主要为铜型、黄铜和高斯织构,1/4层存在微弱的高斯织构和旋转立方织构,中心层以γ纤维织构和旋转立方织构为主,还含有较弱的α纤维织构.与热轧板相比,常化板表层和1/4层织构变化不大,中心层旋转立方织构和α纤维织构增强.冷轧板各层均具有α纤维织构和γ纤维织构.与冷轧板相比,成品板各层中α纤维织构基本消失,还出现了立方织构和高斯织构. This article focuses on texture evolution in 50W270 high-brand non-oriented silicon steel produced by CSP in hot rolling,normalizing,cold rolling,and annealing processes.The texture in the whole process was measured and analyzed by electron back-scatter diffraction.It is found that the texture along the thickness direction in hot-rolled strips changes obviously;there are mainly copper,brass,and Goss textures in the surface layer;the 1/4 layer has weak Goss texture and rotating cube texture;γ-fib... 
2014-09-28 183 5.8

硅钢工业退火炉温度控制具有强耦合、纯滞后、多扰动等特点,它的控制方法代表着一类非线性系统控制的解决方法。以硅钢工业退火炉温度为控制对象,在双交叉限幅控制的基础上引入了智能学习系统,形成了基于智能学习系统的双交叉限幅控制方法来解决此类非线性系统的控制问题,并通过模块化的编程来实现其功能。结果表明:与传统的PID控制相比,该控制方法的控制精度、抗扰性等控制指标有明显提高,是解决此类非线性控制的一种有效方法。 The temperature control of silicon steel industrial annealing furnace has the features of strong coupling,pure lag,multidisturbance. The control method represents the solution of a class of nonlinear control systems. The control object is the temperature control of silicon steel industrial an-nealing furnace, the intelligent learning system based on Double Across Limit Control is introducedand used to solve control problem of this kind of nonlinear system, and the module programming isused to re... 
2014-05-28 163 5.8

采用Nb对Fe-6.5%Si(质量分数)高硅钢进行微合金化处理,结果表明:Nb在高硅钢薄板制备过程中细晶效果明显.铸态、锻态和热轧态组织的晶粒分别细化了17.50%,24.51%和30.13%.铸态样品压缩强度由1365 MPa提高至1520 MPa,延伸率提高77.78%;温轧板试样室温拉伸强度由573 MPa提高至621 MPa,延伸率提高44.44%.利用XRD对厚度为0.30—1.68 mm的温轧板的板面织构演变过程进行跟踪测量,结果发现:初始织构以(011)〈100〉Goss织构为主,单道次变形量为26.2%的情况下,Goss织构完全转化为(100)〈011〉旋转立方织构,随后,在单道次变形为22.6%的情况下,旋转立方织构完全转化为{111}面织构,即纤维织构,并稳定保持至0.30 mm. Fe-6.5%Si(mass fraction) alloy possess perfect magnetic properties,though intermetallics of Fe14Si2 phase brought 6.5%Si leads to room temperature brittleness and hinder this significant materials industrialization.Nb was adopted into micro-alloying of Fe-6.5%Si high silicon steel. OM,thermal simulated test machine and XRD were employed to study the influence of Nb on high silicon steel in processing stages.Textures of warm-rolled high silicon steel strips were determined b... 
2013-11-28 168 5.8

对1990~2010年在我国申请的冷轧无取向硅钢涂层的专利数量、专利技术领域分布进行了统计,对典型涂层专利技术进行了分析,探讨了无取向硅钢涂层的发展趋势。统计分析结果表明,目前无取向硅钢涂层典型的专利技术主要有自粘结涂层、无铬含稀土元素涂层、含钼酸盐环保涂层及采用有机-无机纳米杂化材料为主成膜物形成的涂层等。无取向硅钢涂层发展的趋势主要是无铬环保的半无机、半有机型涂层。 The patent quantity of cold-rolled non-oriented silicon steel coating and distribution of technology fields applied in China in 1990-2010 were summarized.The analysis results indicate that typical patent technologies include self-adhesion coating,chromium-free and with rare earth element coating,environment-friendly and with molybdate coating,coatings with organic-inorganic hybrid materials as main forming agent and so on.The main development trends of coatings on silicon steel are among semi-in... 
2011-02-28 179 5.8

阐述了电工钢在\"双碳\"中的作用,强调了电工钢的生产工艺技术及在减少碳排放、降低能耗中的作用,对下游能效升级带来明显的节能及降碳成果。同时,分析了2021年电工钢的生产运行情况,介绍了电工钢的未来发展,并针对如何减少碳排放以及生产更多的更低铁损、更高磁感的电工钢谈了几点启示。 The effects of electrical steels on carbon peak and carbon neutralization were expounded,especially on the achievements of obvious energy saving and carbon reduction to the downstream energy efficiency upgrading bringing from the production technology of electrical steels and their effects to reducing carbon emission and energy consumption.Meanwhile the production situation of electrical steels in 2021 was analyzed,and the future development of electrical steels was introduced,and some advices w... 
2022-01-28 198 5.8

【作者】 宋波; 朱一知; ...
2011-10-28 118 5.8

某冷连轧机生产无取向硅钢板材时,其边缘降的长度合格率频繁超标。为满足用户的叠片厚度精度要求,这类产品必须以增大切边量的方式来保证交货质量,而这种方式又直接降低了金属收得率,提高了生产成本。基于此,以该产线现有设备特性为基础,详细分析其软、硬件功能模式,分别对辊形与反馈控制进行全面分析与优化改进。通过现场试验论证,充分明确依托辊形优化与反馈控制程序的改进能显著提高边缘降的控制水平,该技术的使用为生产现场的边缘降控制提供了合理的技术支撑。 A cold rolling mill production of non-oriented silicon steel sheet,the thickness difference of the edge( edge-drop) is usually exceed the preset standard value,In order to meet the accuracy requirements of the user flatness,these production must be trimed wider length to meet the delivery quality of the user need, which directly reduce the metal yield and increase the manufacturing cost. Therefor,the software and hardware of the production line has been analyzed, and the work roll shape and feed... 
2014-02-28 172 5.8

连续酸洗退火机组(CPAL)对于当前生产高磁感取向硅钢和高牌号无取向硅钢是必不可少的一个环节。常化炉是常化酸洗机组关键的组成部分。本文对国内自主建造的两条退火酸洗机组的工艺流程,特别是常化炉段进行了对比分析。总结出了常化炉的工艺及组成特点,对生产过程中暴露的问题进行了仔细的分析并提出了改进的意见,对于以后新建常化炉具有一定的提示作用。 The continous pickling annealing line(CPAL) is an essential step in producing high magnetic induction grain-oriented silicon steel and high grade non-oriented silicon steel.The normalizing furnace is a very important part of the CAPL.In this paper,the process flows of two CAPL with independent manufacture in our country have been compared,especially the part of normalizing furnaces.The characteristics of process and component are summarized and problems of the normalizing furnace during the prod... 
2013-03-28 150 5.8

研究了铝和铬元素在无取向电工钢晶粒长大过程中对织构及晶界变化的影响规律。试验结果表明:电工钢在晶粒长大过程中的主要织构组分均为{111}<112>。在晶粒生长期间,不加铝的1号试样中,{111}<112>、{111}<110>织构组分强化,而{100}<001>织构组分弱化;与1号试样相比,在加入0.2%的铝(质量分数,下同)的2号试样中,{111}<112>、{111}<110>织构组分强化(增加)的速率下降,{100}<001>织构组分变化不明显,甚至稍有增加。在含铝的试样中再加入0.3 5%的铬之后(3号试样),{111}<112>{、111}<110>和{100}<001>织构组分的变化规律与1号试样相似,但当电工钢中加入0.72%的铬之后(4号试样),上述3种织构组分的变化规律与2号试样相似。对于在晶粒生长期间持续变化的3种织构组分而言,1号试样的{1 1 1}<112>和{111}<110>织构组分的高(低)取向差角度晶界频率下降(... The effect rule of Aluminm and Chromium on texture and grain boundary transformation in the nonoriented electrical steel during grain growth was investigated.The experimental result shows that the main texture component is {111}<112> in the electrical steel.The {111}<112> and {111}<110> components in specimen 1 without Alumium were strengthened during grain growth whereas {100}<001> component was weakened.But the growth rate of {111}<112> and {111}<110> compon... 
2011-06-28 175 5.8

【摘要】 <正>编号:2012016获奖等级:特等完成单位:...
2012-11-28 168 5.8

站点公告

网站试运行,请大家关注本站公众号,多提宝贵意见!