介绍了CSP工艺生产无取向电工钢各工序的设备特点、采用的工艺控制手段和电工钢产品质量情况,结合生产实践证明了马钢CSP工艺开发的无取向电工钢产品丰富了薄板坯连铸连轧的品种结构,发挥了薄板坯连铸连轧生产无取向电工钢性能均一、稳定的特点。 The equipment characteristic,the process control method and the quality of non-orientated silicon steel by CSP process were introduced.Combined with the production situation,it is proved that production of non-orientated silicon steel developed on Masteel CSP line would enrich product structure of thin slab continuous casting and rolling,and it exerts stable performance of non-orientated silicon steel. 
2013-06-28 164 5.8

针对新能源汽车的发展,制备了含Ni固溶强化、含Cu析出强化以及含Ni+Cu复合强化3%Si无取向硅钢,研究了强化方式对无取向硅钢组织、织构和性能的影响。结果表明:固溶强化型无取向硅钢热轧板中形成了粗大{221}<221>晶粒,冷轧过程中剪切变形明显并在退火后形成良好再结晶织构。析出强化型无取向硅钢热轧板中心层形成γ取向粗大晶粒,在后续的加工中γ织构逐渐增强并最终得到相对细小的再结晶晶粒。复合强化型无取向硅钢热轧板中保留了强λ取向带状组织,退火后形成了有益的Goss织构和λ织构。固溶强化型与复合强化型无取向硅钢磁感应强度B50分别达到1.742、1.688 T,高于析出强化型无取向硅钢的1.645 T。同时,复合强化型无取向硅钢高频铁损最低,其P1.0/400和P1.0/1 000分别低至20.97、82.69 W/kg,这与其较小的晶粒尺寸和织构改善有关。强度计算结果表明:Ni元素固溶强化对强度的提高有限,屈服强度为468 MPa,纳米Cu析出可显著提高屈服强度(强度增量约200 MPa),且主要来自于模量强... For the development of new energy vehicles, 3%Si non-oriented silicon steel were processed by solid solution strengthening with Ni, precipitation strengthening with Cu, and composite strengthening with Ni and Cu. The effects of different strengthening methods on the microstructure, texture and properties of high-strength non oriented silicon steel were studied.The results show that coarse {221}<221> grains are formed in the hot rolled sheet of solution strengthened non-oriented silicon ste... 
2022-06-28 196 5.8

研究了CSP工艺流程生产的硅含量为1.5%的无取向电工钢在不同常化温度下对磁性能的变化。研究结果表明:随着常化温度的提高,热轧板的晶粒尺寸增大,且组织均匀性提高;此外成品的有利织构组分{100}<0vw>、α、η增强,不利织构组分减弱;铁损P1.5/50呈下降趋势,磁感B50上升平缓。在常化工艺为970℃×2.5min下,对应的铁损P1.5/50<3.4W/kg,磁感B50>1.74T。 The effect of normalizing temperature on the magnetic properties of non-oriented electrical steel containing 1.5%silicon produced by CSP process was studied.The results show that with increasing normalizing temperature,the average grain size of hot-rolled plate increases and the microstructure uniformity is improved.Furthermore,the texture components of finished products are improved through enhancing of{100}<0vw>,αandηtextures and weakening of{111}<112>texture;the core loss P1.5/50 ... 
2014-03-28 139 5.8

采用Nb对Fe-6.5%Si(质量分数)高硅钢进行微合金化处理,结果表明:Nb在高硅钢薄板制备过程中细晶效果明显.铸态、锻态和热轧态组织的晶粒分别细化了17.50%,24.51%和30.13%.铸态样品压缩强度由1365 MPa提高至1520 MPa,延伸率提高77.78%;温轧板试样室温拉伸强度由573 MPa提高至621 MPa,延伸率提高44.44%.利用XRD对厚度为0.30—1.68 mm的温轧板的板面织构演变过程进行跟踪测量,结果发现:初始织构以(011)〈100〉Goss织构为主,单道次变形量为26.2%的情况下,Goss织构完全转化为(100)〈011〉旋转立方织构,随后,在单道次变形为22.6%的情况下,旋转立方织构完全转化为{111}面织构,即纤维织构,并稳定保持至0.30 mm. Fe-6.5%Si(mass fraction) alloy possess perfect magnetic properties,though intermetallics of Fe14Si2 phase brought 6.5%Si leads to room temperature brittleness and hinder this significant materials industrialization.Nb was adopted into micro-alloying of Fe-6.5%Si high silicon steel. OM,thermal simulated test machine and XRD were employed to study the influence of Nb on high silicon steel in processing stages.Textures of warm-rolled high silicon steel strips were determined b... 
2013-11-28 148 5.8

为满足用户对无取向电工钢中硫含量的要求,采用CaO-CaF2复合渣系为脱硫剂,利用RH投入法对无取向电工钢进行深脱硫试验。试验结果表明,RH精炼渣成分控制在w CaO43%~51%、w Al2O325%~31%、w MgO4%~6%、w SiO29%~12%、w(FeO+MnO)3%~6%,在脱硫剂加入量为6~8 kg/t时,钢中平均硫含量从32×10-6降低到18×10-6,RH平均脱硫率为43.3%,最高达47.1%。利用KTH模型计算精炼终渣平均硫容量为0.003 1,RH精炼结束时渣-钢间实际平均硫分配比从14增加到52。 In order to satisfy the requirements of consumers on sulfur content in non-oriented electrical steel,taking( CaO-CaF 2) based flux as desulfurizer,industrial experiments on deep desulphurization of non-oriented electrical steel were carried out during RH process. The results show that as the compositions of refining slag are appropriately controlled with w CaO of 43% ~ 51%,w Al2O3 of 25% ~ 31%,w MgO of 4% ~ 6%,w SiO2 of 9% ~ 12%,and w( FeO + MnO) of 3% ~ 6%,and the desulfurizer added are at 6 ~ ... 
2013-06-28 133 5.8

6.5%Si硅钢具有优异的磁学性能和广泛的应用前景。本文综述了6.5%Si硅钢的物理、机械及磁学特性,讨论了传统轧制、温轧、薄带连铸、快速凝固、CVD、粉末轧制等不同制备工艺的关键技术及特点,概括了6.5%Si硅钢在高效节能电机、汽车马达及磁屏蔽等领域中的主要应用,介绍了硅钢的制备技术取得的研究进展,并指出了其广阔的发展前景。 6.5% Si silicon steel has good magnetic properties and wide applications.In this paper physical and mechanical magnetic properties were summarized,and key technology and characteristic of several preparation methods,such as traditional rolling,warm rolling,thin strip continuous casting,rapid solidification,CVD and powder rolling,were discussed.Main applications of 6.5% Si steel in the fields of high-efficiency electrical motors,automobile motors,transformer cores and magnetic shielding were gene... 
2012-06-28 140 5.8

森吉米尔二十辊轧机是冷轧电工钢的主要机型,具有整体刚度大,辊径小,轧制道次压下量大,产品精度高等特点,简要介绍了近年来冷轧电工钢森吉米尔二十辊轧机领域进展,在轧机结构、厚度自动控制、板形自动控制等方面的技术及研究。 20-h Sendzmir reversible mill is the main type of cold rolled electrical steel which has the characteristic of high integral stiffness,small roller diameter,high pass reduction and high product quality.In this paper,the recent progress of frame structure,automatic gauge control,automatic flatness control of Sendzmir mill is introduced. 
2023-05-06 206 5.8

研究了CSP工艺生产≤0.005%C-1.1%Si的2.2mm无取向电工钢热轧板在800~1000℃常化对0.5mm冷轧板840℃退火后组织和磁性能的影响。结果表明,热轧板常化温度升高,冷轧板退火后的再结晶晶粒增大,铁损降低,磁感增加;热轧板常化温度超过900℃,因第二相固溶而后弥散析出,退火后冷轧晶粒细化,铁损增加,因此该无取向电工钢热轧板最佳常化温度为900℃。 The effect of normalizing at 800-1000℃ of CSP produced plate(≤0.005%C-1.1%Si) on the microstructure and magnetic properties of downstream cold-rolled non-oriented electrical steel annealed at 840℃ was studied.Results show that with increasing normalizing temperature of hot-rolled material the recrystallized grain size of annealed sheet increases,iron loss reduced and magnetic induction increases.As normalizing temperature excesses 900℃,grain is refined and iron loss increases after annealing due... 
2012-03-28 128 5.8

无取向硅钢的磁性能主要取决于铁素体的晶粒尺寸、晶体织构和钢中的夹杂物。通过合适的化学成分设计以及采用适宜的夹杂物控制技术,可以获得最佳的夹杂物控制效果,使其纯净度大幅度提高或者无害,最终获得磁性能优良的高级别无取向硅钢。同时,为满足节能、环保、高效需求,无取向硅钢正朝着节能降耗、环境友好以及多功能、高效率、易加工等方向发展。 The magnetic properties of non-oriented silicon steel mainly depend on the grain size of ferrite,the crystallographic texture,and the inclusions in the steel.The optimum inclusion control effects can be obtained through a suitable chemical composition design and an appropriate inclusion control technique,and then the liquid steel will get be clean or the inclusion will get be harmless,finally the excellent magnetic property of the non-oriented silicon steel can be obtained.Meanwhile,in order to ... 
2013-03-28 155 5.8

电动汽车电机在高速旋转时承受离心力和电磁力的作用,在进行电机转子设计时,既要考虑电磁性能,还要考虑机械性能。对电机转子受力情况进行了综述,分析了转子用电工钢疲劳性能参数的重要性,详细阐述了试样抛光、表面处理、试样的对中和安装对测试结果的影响。 The motor of electric vehicle bears big force for high speed rotors,mainly including centrifugal and electromagnetic forces.The magnetic and mechanical aspects of the electrical steel are crucial to machine design.In this paper,the forces applied on the motor were summarized and importance of fatigue properties was analyzed.The influence of specimen polish,surface treatment,alignment and installation on fatigue testing result were represented in detail. 
2014-10-28 147 5.8

利用DSC、XRD,结合热焓分析对硅钢级氧化镁和二氧化硅的固相反应行为进行了研究。比较了不同二氧化硅原料及混合方法对硅钢级氧化镁反应性的影响,找到了一种更为有效的硅钢级氧化镁反应性的评估方法,克服了传统柠檬酸活性法在比较不同厂家生产的氧化镁的反应性上的局限性。进一步研究了Na2B4O7添加剂、TiO2添加剂对氧化镁和二氧化硅反应行为的影响,结果表明,Na2B4O7添加剂含量的增加对反应有利,而TiO2添加剂对反应有阻碍作用。 The solid-state reaction behavior between silicon-steel grade MgO and SiO2 was investigated by DSC and XRD combined with enthalpimetric analysis.The influence of different kinds of SiO2 and different preparation methods were studied and a specifical measurement that is more reliable was proposed to evaluate reactivity of silicon steel grade MgO.It overcomes the limitation of the traditional citric acid activity(CAA) method,which can not be used to evaluate the reactivity of... 
2014-03-28 135 5.8

【摘要】 <正>含6.5%Si的电工钢是软磁特性最佳的电...
2014-04-28 110 5.8