酸溶铝对铸态取向硅钢中第二相粒子组成和形貌的影响
试验的铸态取向硅钢(/%:0.0440.056C,3.123.32Si,0.080.11Mn,0.0020.008S,0.002 90.029 1Als,0.006 20.010 9N)由30 kg高频真空感应炉熔炼。通过场发射扫描电子显微镜/能谱仪(FE-SEM/EDS)研究结果表明,0.002 9%Als钢中氧化物主要为SiO2,存在片状、棒状及近似球状的独立MnS,未发现含铝的氧化物或氮化物;0.0090%Als钢中出现以Al2O3为主的复合氧化夹杂物,存在MnS与AlN的复合析出物。钢中Als增加,复合析出物多呈簇状发展。氧化物容易成为MnS-AlN复合析出的核心,钢中Als含量越低,夹杂物中的MnS含量越高;作为核心的氧化物夹杂的尺寸越小,形成的复合夹杂物的形状越规则,尺寸也越小。热力学计算结果表明,钢中Als含量主要影响了钢中氧化物夹杂的组成和AlN的析出温度及析出量。 Test as-cast grain-oriented silicon steel(/%:0.044 0.056C,3.12 3.32Si,0.08 0.11Mn,0.0020.008S,0.002 90.029 1 Als,0.006 20.010 9N) is melted by a 30 kg high frequency vacuum induction furnace.The research results by using field emission-scanning electron microscope/energy dispersive spectrometer(FE-SEM/EDS) show that in 0.002 9%Als steel the main oxide is SiO2,and there is independent laminable,rod-like and approximate ...
电感耦合等离子体质谱法测定硅钢中痕量铝钼钒钛铌
研究了应用电感耦合等离子体质谱(ICP-MS)同时测定硅钢中痕量铝、钼、钒、钛、铌元素的分析方法。通过条件试验对测量参数进行了优化,确定RF功率1 400 W,泵速30rpm,采样深度140,雾化压力0.90。样品采用硝酸分解,以Be、Y混合内标校正了测量过程中高基体引起的信号漂移。根据测量时存在的质谱干扰情况,选择同位素27 Al、98 Mo、51 V、47 Ti和93 Nb作为测定同位素,同时通过调节仪器参数使得双电荷离子和氧化物离子的产率最低,以减少其带来的干扰。采用基体匹配法配制校准溶液,以标准加入法建立工作曲线,并扣除试剂空白。该方法各元素的测定下限均可达到1μg/g。用于硅钢标准样品的测定,所得结果与参考值完全吻合,各元素的RSD小于5.2%。 A method for the determination of trace aluminum,molybdenum,vanadium,titanium and niobium in silicon steel by inductively coupled plasma mass spectrometry(ICP-MS) was described.A series of single parameter condition experiment was conducted.The optimized operation parameters with RF power 1 400 W,turbo pump rate 30 rpm,sampling depth 140 and nebulizer pressure 0.90 were obtained.The samples were dissolved by HNO3,and the Be and Y mixing internal standard were used to eliminate the signal drift c...
取向硅钢用特种氧化镁的应用研究
采用XRD、SEM和激光粒度仪等手段,观察并研究了不同特性氧化镁在硅钢表面形成硅酸镁底层形貌特点,并结合热力学和差热-失重分析了MgO-SiO2的反应机理。研究结果表明:粒度小,活性值高的特种氧化镁在高温退火过程中与基体表面氧化物生成的硅酸镁底层,界面中硅酸镁底层嵌入基体较多,表面致密,颗粒细小,有利于形成附着性能优良的硅酸镁底层。 Surface microstructure of Mg2SiO4 coatings formed on the surface of oriented silicon steel coated with different kinds of MgO was investigated by XRD and SEM.The reaction mechanism between MgO and SiO2 was analyzed by TG-DSC and thermodynamic calculation.Results revealed that when the MgO with finer microstructure size and higher activity is employed,a dense Mg2SiO4 layer with finer microstructure and good binding to the steel substrate can be obtained.The results are very helpful for the prepar...
高牌号无取向电工钢热轧板常化退火组织的EBSD分析
借助于EBSD对比研究了常化退火对高牌号无取向电工钢热轧组织和织构演变的影响,分析了常化退火对热轧板各厚度层织构的演变规律。结果表明,常化退火改善了热轧组织的均匀性,并弱化了热轧变形的γ纤维织构。升高常化退火温度,可增大热轧板的晶粒尺寸,提高{100}和{110}织构组分占有率,有利于提高无取向电工钢成品板的磁性能。 Effects of normalizing annealing on microstructure and texture of high-grade non-oriented electrical steel hot-rolled sheet were investigated by EBSD. Emphasis was put on the effects of normalizing annealing on texture evolution in the sheet thickness. The results show that the hot-rolled microstructure homogeneity is improved and the γ-fiber texture is weakened by normalizing annealing treatment. The grain size of hot-rolled sheet and intensity of the {100} and {110} favorable texture can be in...
奥氏体化温度对高碳含硅钢等温转变的影响
采用XRD物相分析、金相组织观察及TEM精细组织分析研究了奥氏体组织结构状态对Fe-0.88C-1.35Si-1.03Cr-0.43Mn钢中温等温相变鼻温和孕育期的影响,以及不同温度奥氏体化后240℃等温20 min试样的组织结构特征。试验发现,随着奥氏体化温度的升高,中温等温开始转变的鼻温移向更低温度并且相变孕育期缩短;不同温度奥氏体化后同为240℃等温20 min处理,虽然均形成由贝氏体铁素体亚条平行排列构成的束状贝氏体组织,但贝氏体组织的精细结构状态不同,突出的差别在于对应低温奥氏体化贝氏体亚条端部边界具有凸起结构,而对应高温奥氏体化贝氏体亚条端部边界较为平齐且呈现楔形结构。不能简单地以马氏体切变机制认识试验钢中贝氏体组织的形成。 The influence of austenitization temperature on the incubation period and the bainitic phase transformation behaviour in high-carbon silicon steel has been investigated using X-ray diffraction(XRD), optical microscopy and transmission electron microscopy(TEM). The microstructure characteristics of the isothermal transformation(240 ℃, 20 min)products were also studied. It was found that the nose temperature of bainite transformation and incubation period decreased with the increasing austenitizin...
CSP流程生产高磁感无取向电工钢磁各向异性研究
对CSP流程生产的高磁感无取向电工钢50W1300在偏离轧制方向不同角度处的磁性能进行了测试和分析。结果表明:在偏离轧向不同角度处,磁性能差异显著,尤其在α=60°时磁感最低;偏离轧制方向不同角度处的磁性能大小取决于织构类型、强度及分布状态;增强{100}<0vw>和α、η取向的有利织构组分,降低不利的γ取向织构组分,且使有利织构组分分布越漫散,磁各向异性越小。 Magnetic properties of high magnetic induction non-oriented electrical steel 50W1300 produced by CSP processes were investigated with different direction in relation to the rolling direction.The result shows that magnetic properties are significantly different in relation to the rolling direction,in particular,the minimum magnetic induction occurs at 60° in relation to the rolling direction.Magnetic properties of different directions in relation to rolling direction depend on type and distributi...
典型半工艺电工钢产品M660-50K5生产及应用技术解析
对欧盟市场汽车压缩机专用产品进行技术解析,对比分析了其电磁性能、退火和发蓝处理、物理性能、化学成分、应用特点等参数。探讨国内外电工钢产品应用方式的不同特点,并结合鞍钢自身工艺装备和炼钢、热轧、冷轧工艺参数介绍了其生产可行性。提供了冶金工艺流程下,后工序电工钢专业生产线及传统冷轧系统生产线两种生产方式,均能满足用户最终使用要求。 The technology of automotive compressor accommodation manufacture of European Economic and Monetary Union market was described.The magnetic properties,annealing bluing,physical properties,chemical composition,application parameters were analysed.The different characteristics of the application of electrical steel products,the feasibility of manufacture on the existing technology and equipment,steelmaking,hot rolled,cold rolled technical parameters were discussed.The professional product line of ...
无取向电工钢XG800WR连铸电磁搅拌试验研究
采用铸坯低倍组织检验和化学分析的方法,研究板坯连铸机二冷区电磁搅拌器电流和频率参数对无取向电工钢XG800WR板坯中心偏析和等轴晶率的影响,结果表明:铸坯等轴晶率随着搅拌器电流强度和电流频率的增大而增加。采用二冷区电磁搅拌可减小中心易偏析元素S的偏析,试验得出:减小铸坯S偏析效果最好的电磁搅拌参数为电流380~400A,频率6Hz。 The effect of electromagnetic stirring current and frequency parameter at secondary cooling area on the central segregation and equiaxed crystal ratio of XG800WR non - oriented electrical steels slab was investigated through the methods of chemical and macrostructure analysis.The results shows that the rate of equiaxed crystal zone is going up with increasing of current intensity and current frequency.Electromagnetic stirring in the secondary cooling area can be easily reduced segregation caused...
Al含量对2.2%Si无取向硅钢组织、织构和磁性能的影响
通过实验室25 kg真空感应炉冶炼和锻轧研究了0.26%~0.95%Al含量对0.5 mm 2.2%Si无取向硅钢冷轧板组织、织构和磁性能的影响。试验结果表明,0.26%~0.81%Al含量时,随钢中Al含量的增加,成品退火钢板的晶粒尺寸增加同时铁损减少;当Al含量大于0.81%时,随Al含量增加,钢板的晶粒尺寸减小,同时铁损增加。Al含量对硅钢板磁感的影响没有明显的规律。2.2%Si无取向硅钢的合适Al含量为0.48%~0.81%。 The effect of 0.26%~0.95%Al content on structure,texture and magnetic performance of 0.5 mm cold rolled sheet of 2.2%Si non-oriented silicon steel has been studied by a 25 kg vacuum induction furnace smelting,and forging -rolling in laboratory.Results show that as 0.26%~0.81%Al,with increasing Al content in steel the grain size of annealed finished sheet increases while iron loss of sheet decreases,and as Al content in steel is more than 0.81%,the grain size of sheet decreases while iron loss in...