钢厂
无抑制剂取向硅钢概述
概述了无抑制剂法生产取向电工钢的特性及其用途;总结无抑制剂生产取向电工钢的原理及工艺方案.重点讨论了成分方案,即元素对磁性能的影响和最终高温退火方案对二次再结晶的影响.研究结果表明,无抑制剂取向硅钢化学成分范围没有普通取向硅钢和高磁感取向硅钢严格,提高了成材率;最终高温退火决定了二次再结晶的好坏,从而最终决定成品磁性能,最佳的高温退火温度在850~950℃之间. This article provides an overview on the characteristics and uses of inhibitorless process producing grain-oriented electrical steels.The mechanism of inhibitorless process and technology programs were discussed.The results show that the chemical composition and final annealing were determined according to magnetic properties.The inhibitor-free grain oriented silicon steel has loose range of chemical composition;Secondary recrystallization occurs mainly in the final annealing and the best anneal...
无取向硅钢表面环保涂层的发展
简述了无取向硅钢环保涂层发展背景,分析了硅钢环保涂层的特点及国内、外研究进展,提出了硅钢保涂层下一步的发展方向。 The back ground of environmental protection coating of non-oriented silicon steel was described in this paper.The characteristics and study progress in domestic and foreign of environmental protection coating of non-oriented silicon steel were analysised.The next development direction of environmental protection coating of non-oriented silicon steel was put forward.
基于不同B-H曲线的取向硅钢叠片中损耗和磁通的分析与验证
基于TEAM(Testing Electromagnetic Analysis Methods)Problem 21基准模型和不同类型的磁化曲线Bm-Hm及Bm-Hb数据,分别在50 Hz至200 Hz的频率范围内计算了基准模型的硅钢叠片内的损耗及磁通,并考虑集肤效应和材料的电-磁各向异性的影响。数值计算结果与实验测量结果具有很好的一致性。提出的有限元建模方法和基于模拟结果的分析、结论有助于提高大型电力变压器的电磁设计的有效性。 Based on TEAM(Testing Electromagnetic Analysis Methods) Problem 21 standard model and the different B-H(such as Bm-Hm and Bm-Hb) curves,the iron loss and magnetic flux inside the grain-oriented(GO) silicon steel lamination are modeled under different frequency(from 50 Hz to 200 Hz) in this paper,And the influences of skin effect and electric-magnetic anisotropy on the numerical simulation results have been examined.The calculated and measured results with respect to the model are in good agreeme...
Cr对含Nb高强无取向硅钢组织、织构及性能的影响
高强无取向硅钢主要应用于高速电机,要求其具备高强度和优异磁性能,但目前无取向硅钢的磁性能和强度难以兼顾。因此,设计并制备了添加微量Cr的含Nb高强无取向硅钢,通过光学显微镜、EBSD、万能拉伸试验机、四探针测试仪和磁性能测量仪等研究了Cr对含Nb高强无取向硅钢微观组织、织构、力学性能及磁性能的影响。结果表明,添加质量分数为0.5%的Cr抑制了热轧组织的回复,使常化和退火组织再结晶减弱,常化和退火后有利织构面积分数增加,不利织构面积分数减小。添加质量分数为0.5%的Cr使含Nb无取向硅钢的屈服强度显著增大,磁感略升高,但对铁损几乎没有影响。Cr对屈服强度的影响一方面是由于Cr的固溶强化作用,另一方面Cr促进了Nb的析出而使Nb的析出强化效果增强;而Cr提高含Nb高强无取向硅钢的磁感主要是由于促进有利织构形成的同时抑制了不利织构的形成,使得织构因子增大;添加Cr使无取向硅钢的电阻率增加从而使铁损降低,同时Cr促进了Nb的析出,而这种富Nb析出相不仅抑制晶粒长大且会阻碍磁畴移动而使铁损增高,在两方面因素的综合作用下,添加质量分数为0.5%的Cr对含Nb高强无取向硅钢的铁损几乎没有影响。因此,... High strength non-oriented silicon steel is mainly used in high-speed motors, which requires good mechanical and magnetic properties. However, it is difficult for non-oriented silicon steel to obtain high strength and good magnetic properties at the same time. In this paper, the Cr-microalloyed Nb-containing high strength non-oriented silicon steel was designed and prepared. The effect of Cr on the microstructure, texture, mechanical properties and magnetic properties of Nb-containing high stren...
晶粒尺寸对无取向硅钢磁性能影响的主成分回归分析
采用电子背散射衍射技术测定50SW1300冷轧无取向硅钢中不同尺寸范围晶粒的含量,利用主成分回归分析法,综合研究不同尺寸范围晶粒的含量对无取向硅钢磁性能的影响。结果表明:通过主成分回归分析法能够从不同尺寸范围晶粒的含量的多个影响因素中获取主要的因素,定量研究它们对无取向硅钢磁性能的影响规律。分析表明,无取向硅钢的铁损与不同尺寸范围晶粒的含量之间存在着可靠的多元线性关系,在一定范围内,较大尺寸晶粒的含量越多,其对铁损优化的作用越明显;而无取向硅钢的磁感与不同尺寸范围晶粒的含量之间并无线性关系。 Distribution of grain size in cold rolled non-oriented silicon steel 50SW1300 was measured by EBSD.The effects of the distribution of grain size on magnetic properties of the non-oriented silicon steel were comprehensively researched by means of principal component regression method.The results indicate that the main factors influencing the magnetic properties in the distribution of grain sizes,which can be used to guantitative study the magnetlic properies of the steel,are obtained by principal...
取向硅钢生产工艺技术分析和发展趋势
介绍了普通取向硅钢(CGO)和高磁感取向硅钢(Hi-B)铸坯高温加热两次冷轧、一次冷轧和铸坯低温加热两次冷轧、一次冷轧法4种成熟生产工艺的主要技术参数,取向硅钢理论研究(Goss晶核和抑制剂)和生产技术现状。取向钢的发展趋势为:提高(110)[001]晶粒取向度,降低取向硅钢铁损,发展铸坯低温加热(≤1 300℃)和薄板坯连铸连轧流程生产取向硅钢工艺。 Main technology parameters of four developed process:cast bloom higher temperature heating-double cold rolling or single cold rolling,lower temperature heating-double cold rolling or single rolling process for production of common grain oriented silicon steel(CGO) and high magnetic induction grain oriented silicon steel(Hi-B),theory research on grain oriented steel(Goss nucleus and inhibitor) and present situation of process are summarized in this paper.The development trend of grain oriented si...
国产化高牌号无取向硅钢退火、涂层炉新技术
从影响高牌号无取向硅钢退火工艺的主要参数入手,介绍高牌号无取向硅钢退火炉在加热、气氛控制、冷却、涂层烘烤方面的新技术,并展望无取向硅钢退火炉的发展方向。 Based on the technology parameters of high-grade non-oriented silicon steel annealing,the new technology of the annealing line,which includes heating,atmosphere control,cooling,coating baking,is introduced,and the development direction of non-oriented silicon steel annealing furnace is pointed out.
热轧卷取时间对新型冷轧无取向电工钢组织和性能的影响
研究了热轧卷取时间对无取向电工钢晶粒组织、织构演变、铁损和磁感的影响。结果表明,成品晶粒尺寸在120~140μm之间,随卷取时间的增加,成品晶粒尺寸增大。成品织构主要由γ纤维、а纤维和高斯织构等构成。随着保温时间的增加,{111}<110>和{112}<110>织构强度降低。随卷取时间的增加,成品P1.5降低。热轧板最佳的卷取工艺为550℃保温2~3 h,电工钢的综合磁性能优良。 The effects of hot-rolling coiling time on microstructure,texture,core loss and magnetic induction of a new cold-rolled non-oriented electrical steel containing copper were investigated.The test results showed that for final product the grain sizes are 120-140um,with the increase of coiling time,the grain size increase.For final product there are mainly γ-fibre,а-fibre,and {110}<001> texture,Coiling at 550℃ for hot rolled plate,the {111}<110>,{112}<110> texture was weaked with ...
微合金元素Sn、Nb、Re对无取向硅钢性能的影响
介绍了微合金元素锡、铌、稀土对无取向硅钢性能的影响,并扼要分析了这些元素对硅钢性能的影响机理:晶界偏聚元素Sn可细化晶粒提高硅钢磁性能;微合金元素Nb细化铁素体晶粒,提高硅钢的强度、韧性和塑性及磁性能;稀土元素(RE)在硅钢中的主要作用包括净化钢液、变质夹杂物、改善铸态组织和性能及微合金化,减少晶界上出现偏析的几率。 The influence of micro-alloy elements on properties of non-oriented silicon steel and the mechanism for effect of the micro-alloy elements including Sn、Nb and RE on the properties of steel are presented and analyzed in this paper.Grain boundary segregation elements Sn in steel can grain refinement and improve the magnetic properties;Micro-alloy elements Nb can refine the ferrite grain,increase the silicon steel strength,toughness and plastic;The main role of the RE in the silicon steel including...
取向硅钢连续退火的工艺与设计
分析了影响脱碳效果和结晶行为的各种要素及其相互制约关系,提出了Hi-B连续退火工艺曲线,总结得出快速加热及合理稳态气氛是实现工艺制度的关键。结合实际工程,介绍了在连续退火炉设计中快速加热和气氛设计的考虑方法,并指出随着Hi-B产品的发展,如何改进这些方法将是连退工程研发的方向之一。 The factors which affect decarbonization and crystallization and the mutual restriction between them were analyzed.A complete continuous annealing process for Hi-B was put forward.As a result,the rapid heating and the proper steady atmosphere were two important factors.According to an actual project,the consider methods for designing rapid heating and proper steady atmosphere were introduced,and it is pointed that with the development of Hi-B technique,how to improve these techniques would be on...