本钢热轧厂无取向硅钢生产工艺
冷轧无取向硅钢是高技术含量、高附加值产品,工艺复杂,生产周期长,过程控制难度大,被誉为钢铁产品中的\"工艺品\"。热轧生产工艺又是无取向硅钢生产的重中之重,直接决定了硅钢的铁损和电磁性等多项指标。 Cold rolled non-oriented silicon steel is high technology content、high addedvalue product. Its process is complex, Its production cycle is of Length, and Its Process control is difficult. Which is known as the iron and steel products \" Arts and crafts\". Hot rolling production process is the top priority of non-oriented silicon steel, Which Directly determines iron loss of the silicon steel and electromagnetic property, etc many index.
冷轧压下量对取向硅钢极薄带显微组织的影响
观察了取向硅钢极薄带经冷轧至不同厚度,并经过不同工艺热处理后的显微组织及亚结构。结果表明:冷轧压下量越大,显微组织中位错密度越高,冷变形组织越多,等轴晶粒越少;增加冷轧压下量可以使试样的再结晶温度降低,当钢带厚度为0.08 mm时,在650℃退火时就能发生明显的再结晶。 Microstructure and substructure of the grain oriented ultra-thin silicon steel sheets is analyzed,which are rolled down to different thickness and treated with different heat treatment process.The result shows that there are higher dislocation density,more cold deformation structure and less equiaxed crystal grain in microstructure of the steel sheets with more cold rolled reduction.Increase of cold rolled reduction will decrease recrystallization temperature,and when thickness of the steel shee...
修正GTN模型及其在预测硅钢冷轧边裂中的应用
考虑剪应变对微孔洞损伤演化的影响,对GTN损伤模型的损伤演化机制进行修正,建立了适用于不同应力三轴度水平的损伤模型。结合隐式应力更新算法和显式有限元计算,采用VUMAT子程序实现了修正GTN模型在有限元软件ABAQUS中的数值计算。通过模拟纯剪切和剪切-拉伸两组试样的损伤演化和断裂行为,验证了修正GTN模型在不同应力三轴度承载条件下的有效性。运用修正GTN损伤模型模拟含边部缺口的带钢在轧制过程中裂纹的萌生和扩展行为,模拟结果与实验相一致,表明该模型可有效地用于带钢缺陷在轧制过程中扩展行为的分析和预测。模拟和实验结果表明,带钢边部缺口在轧制过程中,缺口前沿和后沿均会萌生裂纹,且后沿裂纹扩展更为明显。 Considering the effect of shear strain of micro-void on damage evolution, a modified GTN model applicable to various stress triaxiality conditions is proposed by modifying the damage evolution mechanism of the GTN damage model. The modified model is implemented in commercial finite element software ABAQUS by combining the implicit stress update method with an explicit finite element solving algorithm and through the user-defined material subroutine VUMAT. The damage evolution and the failure pro...
TSCR试制高强度无取向电工钢
采用固溶强化、细晶强化和位错强化方法,模拟TSCR流程试开发高强度无取向电工钢,试开发钢的主要合金成分为3%Si、0.83%Al和2.99%Mn。分析热轧、常化、退火后的钢板组织,并针对不同的成品板组织,详尽地分析了相应的力学性能和磁性能。试验电工钢平均晶粒直径为12.37μm时,R p0.2为530 MPa,R m为618 MPa;当退火制度为700℃×4 min,成品组织完全为未再结晶的回复组织时,R p0.2为853.5 MPa,R m为895.5 MPa。该成分的电工钢P15/50或P10/400最小时,对应的平均晶粒直径都大于59.67μm;P10/800或P10/1000最小时,对应的平均晶粒直径都处于12.37~59.67μm尺寸区间。 TSCR was simulated to develop high-strength non-oriented electrical steel with 3% of Si,0.83% of Al and 2.99% of Mn by solution strengthening,grain refinement strengthening and dislocation strengthening.The microstructures of hot rolled plates,normalized plates and annealed plates were analyzed.Furthermore,the mechanical properties and magnetic properties of products with different microstructures were detailedly studied.As the average grain diameter of the steel was 12.37 μm,the yield strength ...
大压下率冷轧无取向硅钢织构演变及性能
组织和织构是影响无取向硅钢性能的重要因素。为改善产品性能,研究了冷轧压下率(71.7%~87.0%)对高牌号无取向硅钢组织、织构、磁性能和力学性能的影响。结果表明,随冷轧压下率的增加,退火晶粒平均尺寸先减小后增大;高斯和立方织构强度减弱,γ纤维织构增强,α纤维织构转变为较强的α*({h, 1, 1}〈1/h, 1, 2〉)织构,并随冷轧压下率的增加而增强,同时其峰值逐渐向{111}面移动;工频铁损P1.5/50、高频铁损P1.0/400和磁极化强度J5000同时降低,屈服强度变化不大,表面硬度逐渐增加。当冷轧压下率由84.7%增至87.0%、厚度减至0.30 mm时,高频铁损降幅是工频铁损的11倍,表面硬度增幅变大。以上研究成果对硅钢减薄后织构及组织的优化提供了很好的指导。 Microstructure and texture are critical factors on non-oriented silicon steel properties. In order to improve product properties, this paper studied the effect of cold rolling reduction rate(71.7%-87.0%) on microstructure, texture, magnetic properties and mechanical properties of high-grade non-oriented silicon steel. The results show that with the increase of cold rolling reduction rate, the average size of annealing grain decreases first and then increases. The intensity of Goss and λ fiber te...
电感耦合等离子体质谱法测定硅钢中痕量铜和镍
研究了应用电感耦合等离子体质谱法(ICP-MS)测定硅钢中痕量铜和镍的分析方法。采用硝酸分解样品,通过内标校正和基体匹配消除了基体干扰的影响,同时根据测量时存在的质谱干扰情况,选择同位素65Cu和60Ni作为测定元素和通过调节仪器参数使双电荷离子的产率最低,以减少带来的干扰。该方法用于硅钢中痕量铜和镍的测定,所得的结果与ICP-AES法测定结果完全吻合,各元素测定结果的RSD值小于5%,加标回收率为97.3%~100.3%。 A method for the determination trace copper and nickel in silicon steel by inductively coupled plasma mass spectrometry(ICP-MS) was studied.The samples were dissolved in HNO3.The effect of matrix interference was eliminated by internal standard correction and matrix matching.Meanwhile,according to the mass spectral interferences in determination,the isotopes including 65Cu and 60Ni were used as measuring elements.The yield of double-charge ions were minimized by adjusting instrumental parameters...
硅钢常化退火炉气-雾冷却技术及其特点分析
常化快冷是生产高牌号无取向硅钢和高磁感取向硅钢不可缺少的一个工艺环节,气-雾冷却则是实现常化快冷的关键方式之一。介绍了国内自主设计建设的常化酸洗机组气雾冷却系统的技术特性,并对其特点进行了系统分析,最后给出该系统在设计、运行参数的选择上若干注意事项,对气-雾冷却系统设计和使用具有一定的指导作用。 The normalizing rapid cooling is a indispensable process to high grade non-oriented silicon steel and high magnetic induction oriented silicon steel’ s production. The fog cooling is a key ways of coming true the normalizing rapid cooling. This paper introduces the technical features of the fog cooling system in normalizing pickling line which is the domestic independent design and construction. Meanwhile,the fog cooling system’s characteristic is analyzed systematacially. In the end,this paper ...
进入硅钢叠片内的漏磁通和附加损耗的模拟实验与仿真
基于简化的取向硅钢片模型,系统地对不同的交流激励下的硅钢叠片内铁损、交链磁通和空气中指定位置的法向漏磁的分布进行了\"单片级\"的测量,并建立了相应的硅钢叠片级问题的三维有限元分析模型,进行了大规模的数值计算分析。模型实验和数值分析的结果表明垂直进入硅钢片的漏磁通和损耗呈现浅透入的特点,在硅钢片内引起的涡流损耗在总铁损中占据了\"举足轻重\"的份额。用电磁场有限元分析软件MagNet瞬态场时步法计算结果与测量结果相吻合,说明本文方法研究复杂的硅钢叠片问题的有效性。 The measurement and 3D finite element analysis of the iron loss,interlinkage flux inside the laminated silicon steel sheets and the magnetic flux densities at the specified positions are carried out based on a verifying silicon steel sheet model.The modeling results show that the leakage flux vertically through the silicon steel sheets has the peculiarity of shin effect,and the eddy current loss caused by the AC leakage flux is a significant component of the total iron loss.The calculated result...
电感耦合等离子体质谱法测定硅钢中痕量铝钼钒钛铌
研究了应用电感耦合等离子体质谱(ICP-MS)同时测定硅钢中痕量铝、钼、钒、钛、铌元素的分析方法。通过条件试验对测量参数进行了优化,确定RF功率1 400 W,泵速30rpm,采样深度140,雾化压力0.90。样品采用硝酸分解,以Be、Y混合内标校正了测量过程中高基体引起的信号漂移。根据测量时存在的质谱干扰情况,选择同位素27 Al、98 Mo、51 V、47 Ti和93 Nb作为测定同位素,同时通过调节仪器参数使得双电荷离子和氧化物离子的产率最低,以减少其带来的干扰。采用基体匹配法配制校准溶液,以标准加入法建立工作曲线,并扣除试剂空白。该方法各元素的测定下限均可达到1μg/g。用于硅钢标准样品的测定,所得结果与参考值完全吻合,各元素的RSD小于5.2%。 A method for the determination of trace aluminum,molybdenum,vanadium,titanium and niobium in silicon steel by inductively coupled plasma mass spectrometry(ICP-MS) was described.A series of single parameter condition experiment was conducted.The optimized operation parameters with RF power 1 400 W,turbo pump rate 30 rpm,sampling depth 140 and nebulizer pressure 0.90 were obtained.The samples were dissolved by HNO3,and the Be and Y mixing internal standard were used to eliminate the signal drift c...