主要对硅钢退火炉耐材施工进行阐述,对一期工程与二期工程施工经验进行总结,包括设计、施工、耐材生产、人员素质等方面,指出了工程项目所所存在的不足,为同类型炉窑的施工提供借鉴。 This paper describes the construction of silicon steel annealing furnace refractories;and it was summarized the construction experience of phase-Ⅰ and phase-Ⅱ projects,including design,construction,refractory production,the quality of personnel etc,and pointed out the shortcomings of the project,which provided a reference for the construction of the same type of furnaces. 
2023-05-11 1.37k 5.8

某厂对电工钢的轧制策略进行了优化,粗轧道次由“1+5”改为“1+3”。在优化后的生产过程中,每次变换钢种,烫辊材就会出现窄尺现象,而紧随其后的电工钢板则出现超宽现象。文中针对该问题,介绍了宽度设定模型和宽度自适应模型的原理,阐述了该问题出现的原因及解决方案,并通过对宽度自适应模型的应用研究及优化攻关,有效地解决了问题,大幅提升了实物质量,降低了宽度封锁率。 The rolling strategy of electrical steel was optimized in a factory,and the rough rolling pass was changed from “1+5”to“1+3”.Subsequently,the following problems were occurred in the production process:when the steel grade changed,the roasting roller steel before the electrical steel appeared the narrow width phenomenon,and then the electrical steel appeared the ultra-wide phenomenon.This paper introduced the principle of width setting model and width adaptive model,and expounded the causes and s... 
2022-02-28 172 5.8

轧制力是影响冷轧带钢厚度精度的关键因素。为实现高精度的冷轧带钢厚度控制,通过优化变形抗力模型参数和摩擦系数模型参数提高冷轧轧制力模型计算精度,并使用指数平滑法的自学习算法保证轧制力精度的稳定性。在首钢股份公司迁安钢铁公司20辊森基米尔轧机生产线进行S12硅钢钢种轧制力优化试验,将优化的模型参数应用于L2并投入现场生产,结果表明该优化方法不仅提高了轧制力设定精度,而且减小了冷轧硅钢的厚度超差长度,提高了成材率。 The rolling force is the key factor which influences the accuracy of cold-rolling strip thickness. To implement high precision control of cold-rolling strip thickness,we optimize the deformation resistance model parameters and friction coefficient model parameters to improve the calculation precision of cold-rolling force model,and use exponential smoothing self-learn algorithm to ensure the stability of rolling force accuracy. In Shougang Qiangang 20-high Sendzimir mill single stand production ... 
2014-05-28 168 5.8

采用\"热轧复合+冷轧减薄+退火\"方法成功制备了0.20mm厚的硅浓度梯度高硅钢薄带,并采用SEM和X射线衍射技术对制备过程中组织和织构演变进行了研究。热轧复合板微观组织呈明显层状分布,复合界面为紧密冶金结合且经过83%的大冷轧变形未开裂。热轧和冷轧复合板带中均形成强α和γ织构,再结晶退火后形成强γ织构。冷轧和退火织构沿板厚呈显著的梯度分布特征,其主要来自于复合界面两侧硅浓度和初始热轧织构的差异性以及冷变形的不均匀性。 Gradient high silicon steel thin sheets with thickness of 0.20 mm were successfully produced by the rolling and annealing method,including hot rolling bonding,cold rolling,and annealing.Microstructure and texture evolution was investigated by means of SEM and X-ray diffraction.Microstructure of hot-rolling-bonding shows obviously layered distribution,the composite interface was closely metallurgical bonding and no cracking appears even after 83%cold rolling.Strongαandγfibers develop in the hot a... 
2023-05-09 220 5.8

试验2.3Si无取向硅钢(/%:0.003C,2.30Si,0.16Mn,≤0.020P,≤0.005S,0.54Al)冷轧板由常化和未常化的2.5 mm热轧板冷轧至0.6 mm(压下率76%),经750~950℃2.5 min中间退火后再冷轧至0.5 mm(压下率16.7%),成品板经890℃+960℃2.5 min退火。研究了中间退火温度对该钢晶粒尺寸、织构和磁性能的影响。结果表明,随中间退火温度的升高,二次冷轧前晶粒和成品晶粒增大,成品中不利织构组分{111}和{112}减弱,磁性能得到改善。热轧板经过常化时的磁性能明显好于未经常化时的磁性能,但中间退火温度较高时常化对磁性能的有利作用减弱。 The test cold sheet of 2.3Si non-oriented silicon steel(/%:0.003C,2.30Si,0.16Mn,≤0.020P,≤0.005S,0.54Al) is first cold-rolled from normalized and un-normalizing 2.5 mm hot-rolled plate to 0.6 mm sheet(reduction 76%),then intermediate annealed at 750~950℃ for 2.5 min and double cold-rolled to 0.5 mm sheet(reduction16.7%),the finished sheet annealed at 890℃+960℃ for 2.5 min.Effect of the intermediate annealing temperature on grain size,texture and magnetic performance of the steel has been studied.... 
2014-02-28 183 5.8

【作者】 严伟明; ...
2013-09-28 141 5.8

利用DSC、XRD,结合热焓分析对硅钢级氧化镁和二氧化硅的固相反应行为进行了研究。比较了不同二氧化硅原料及混合方法对硅钢级氧化镁反应性的影响,找到了一种更为有效的硅钢级氧化镁反应性的评估方法,克服了传统柠檬酸活性法在比较不同厂家生产的氧化镁的反应性上的局限性。进一步研究了Na2B4O7添加剂、TiO2添加剂对氧化镁和二氧化硅反应行为的影响,结果表明,Na2B4O7添加剂含量的增加对反应有利,而TiO2添加剂对反应有阻碍作用。 The solid-state reaction behavior between silicon-steel grade MgO and SiO2 was investigated by DSC and XRD combined with enthalpimetric analysis.The influence of different kinds of SiO2 and different preparation methods were studied and a specifical measurement that is more reliable was proposed to evaluate reactivity of silicon steel grade MgO.It overcomes the limitation of the traditional citric acid activity(CAA) method,which can not be used to evaluate the reactivity of... 
2014-03-28 157 5.8

采用扫描电镜、场发射扫描电镜、能谱仪等对50SW1300冷轧无取向硅钢中的夹杂物分不同尺寸区间进行数量统计,利用主成分回归分析法,即数据的标准化处理—主成分分析—回归分析—标准化的变量还原成原始变量—确定显著影响因素,综合分析夹杂物总量及各尺寸区间的夹杂物数量对无取向硅钢磁性能的影响。结果表明:主成分回归分析能够从夹杂物尺寸区间及数量的多个影响因素中提取主要的因素,定量研究其对磁性能的影响。分析表明,显著影响无取向硅钢铁损的夹杂物为100~500nm的AlN、AlN+MnS、MnS、Al2O3、AlN+Al2O3,而劣化磁感最明显的夹杂物尺寸区间为100~200nm。 Different size intervals of inclusions in cold rolled non-oriented silicon steel 50SW1300 were counted by scanning electron microscope(SEM),field emission scanning electron microscope(FESEM)and energy disperse spectroscopy(EDS).With principal component regression method:standardization for experimental data,principal component analysis,regression analysis,transform standardized variables into original variables,determination of significant factor,effects of the total number of inclusions and the... 
2014-10-28 204 5.8

为探究铬、锰元素及退火温度对高强无取向硅钢性能的影响规律,借助OM、SEM、EBSD与万能拉伸试验机等分析不同制造工艺下3组不同含量铬、锰元素的无取向硅钢热轧、常化及退火处理后组织与性能。结果表明,试验钢热轧后组织不均匀,心部为沿轧向分布纤维状组织,边部为少量再结晶晶粒,常化处理能显著改善热轧板组织均匀性,消除热轧板中心部位的纤维状组织。经冷轧及退火后得到多边形铁素体晶粒,其中960℃退火,晶粒尺寸偏大,有利织构{100}组分体积分数减少,不利织构{111}组分体积分数增加,成分为0.2Mn-1Cr的1号试验钢960℃退火后铁损最大,磁感强度偏小;成分为0.5Mn-1Cr的2号试验钢930℃退火后,磁性能与强度等综合性能最佳,工频铁损P1.5/50为2.41W/kg,高频铁损P1.0/400为17.36W/kg,磁感应强度B5 000为1.638T,抗拉强度为685MPa。 In order to study the effect of Cr,Mn and annealing temperature on the properties of high-strength non-oriented silicon steel,the microstructure and properties of three groups of non-oriented silicon steel with different Cr,Mn content under different manufacturing processes were analyzed by means of OM,SEM,EBSD and universal tensile tester.The results show that the structure of experimental steel is not uniform after hot rolling,and the core is distributed in fibrous structure along the rolling ... 
2020-05-28 201 5.8

某冷连轧机生产无取向硅钢板材时,其边缘降的长度合格率频繁超标。为满足用户的叠片厚度精度要求,这类产品必须以增大切边量的方式来保证交货质量,而这种方式又直接降低了金属收得率,提高了生产成本。基于此,以该产线现有设备特性为基础,详细分析其软、硬件功能模式,分别对辊形与反馈控制进行全面分析与优化改进。通过现场试验论证,充分明确依托辊形优化与反馈控制程序的改进能显著提高边缘降的控制水平,该技术的使用为生产现场的边缘降控制提供了合理的技术支撑。 A cold rolling mill production of non-oriented silicon steel sheet,the thickness difference of the edge( edge-drop) is usually exceed the preset standard value,In order to meet the accuracy requirements of the user flatness,these production must be trimed wider length to meet the delivery quality of the user need, which directly reduce the metal yield and increase the manufacturing cost. Therefor,the software and hardware of the production line has been analyzed, and the work roll shape and feed... 
2014-02-28 166 5.8

考虑剪应变对微孔洞损伤演化的影响,对GTN损伤模型的损伤演化机制进行修正,建立了适用于不同应力三轴度水平的损伤模型。结合隐式应力更新算法和显式有限元计算,采用VUMAT子程序实现了修正GTN模型在有限元软件ABAQUS中的数值计算。通过模拟纯剪切和剪切-拉伸两组试样的损伤演化和断裂行为,验证了修正GTN模型在不同应力三轴度承载条件下的有效性。运用修正GTN损伤模型模拟含边部缺口的带钢在轧制过程中裂纹的萌生和扩展行为,模拟结果与实验相一致,表明该模型可有效地用于带钢缺陷在轧制过程中扩展行为的分析和预测。模拟和实验结果表明,带钢边部缺口在轧制过程中,缺口前沿和后沿均会萌生裂纹,且后沿裂纹扩展更为明显。 Considering the effect of shear strain of micro-void on damage evolution, a modified GTN model applicable to various stress triaxiality conditions is proposed by modifying the damage evolution mechanism of the GTN damage model. The modified model is implemented in commercial finite element software ABAQUS by combining the implicit stress update method with an explicit finite element solving algorithm and through the user-defined material subroutine VUMAT. The damage evolution and the failure pro... 
2014-06-28 158 5.8

采用电解法和扫描电镜研究了300 t转炉-RH精炼钙处理对无取向硅钢板(%:≤0.005C、1.2~2.2Si、0.2~0.6Mn、≤0.20P、≤0.005S、0.2~0.6Al、0~0.01Ca)中夹杂物的影响。结果表明,钢中Al含量为0.25%和0.35%时,钢中溶解氧均小于1×10-4%,钙处理后都会产生CaS夹杂物,尤其是含0.35%Al的钢水;钙处理可以有效减少钢中的夹杂物数量,尤其是0.5μm以下的微细夹杂物数量;钙处理后夹杂物的种类以AlN、CaS为主,同时还含有少量的氧化物夹杂物以及AlN-CaS复合夹杂物,尺寸主要为1.5~5.0μm。 The effect of 300 t converter-RH refining calcium treatment on inclusions in non-oriented silicon steel sheet (%:≤0.005C,1.2~2.2Si,0.2~0.6Mn,≤0.20P,≤0.005S,0.2~0.6A1,0~0.01Ca) has been studied by electrolysis and scanning electron microscope.Results show that with 0.25%and 0.35%Al content in steel,all the dissolved oxygen in liquid is less than 1×10-4%,and the CaS inclusions are produced after calcium treatment,especial for the liquid containing 0.35%Al;the amount of inclusions in ste... 
2011-01-28 184 5.8