冷轧无取向硅钢是高技术含量、高附加值产品,工艺复杂,生产周期长,过程控制难度大,被誉为钢铁产品中的\"工艺品\"。热轧生产工艺又是无取向硅钢生产的重中之重,直接决定了硅钢的铁损和电磁性等多项指标。 Cold rolled non-oriented silicon steel is high technology content 、high added value product. Its process is complex, its production cycle is of length, and its process control is difficult, which is known as the iron and steel products \" Arts and crafts\". Hot rolling production process is the top priority of non-oriented silicon steel, which directly determines iron loss of the silicon steel and electromagnetic property,as well as other many index. 
2014-02-28 194 5.8

针对薄板坯连铸连轧流程结合\"获得抑制剂法\"所制备的低温高磁感取向硅钢,通过热力学计算研究了AlN与MnS在连铸与均热过程中的析出规律与行为。计算结果表明,连铸过程中AlN在凝固后的高温α相中便可能析出,而MnS仅可能在凝固后的α+γ两相区内析出。钢中AlN与MnS在均热过程中均处于部分固溶与部分析出的状态。后续高温渗氮处理后初次晶粒的异常长大并不明显,表明渗氮处理前钢中固有抑制剂的数量相对充足。 The precipitation behavior of MnS and AlN in low-temperature high magnetic induction grain-oriented silicon steel produced by thin slab casting and rolling process with\"acquired inhibitor method\"during continuous casting and soaking was studied by thermodynamic calculation.The calculated results show that AlN is likely to precipitate in ferrite after solidification.However,MnS can precipitate only in the two phase region of ferrite and austenite.Meanwhile,MnS and AlN in the steel can not be comp... 
2014-10-28 172 5.8

采用RH精炼添加钙合金方式对硅钢进行钙处理。结果表明,钙合金添加量为0.67、1.00、1.67kg/t钢时,钢中钙含量分别为0、2×10-6、4×10-6;随着钙合金添加量增大,钢中夹杂物粒度逐渐由0~2μm向2~4、4~6μm偏移;不同钙处理条件下,钢中均存在粒径小于1μm和粒径为1~5μm的MnS、CuxS夹杂物,后者或单独存在,或同AlN、CaS夹杂复合;粒径为5~10μm区间,钢中的夹杂物基本以钙的氧、硫化物为主。与钙处理前相比,钙合金添加量为0.67、1.00、1.67kg/t钢时,粒径小于1.0μm的微细夹杂物减少幅度分别为68.06%、87.50%、94.94%。钙合金添加量为1.67kg/t钢时,可以去除钢中绝大部分的微细夹杂物。 Ca alloy was added into the liquid steel during RH refining,and the results show that Ca concentration in final Si steel sheets is insignificant,about 0,2×10-6 and 4×10-6 when the added amount of Ca is 0.67,1.00 and 1.67 kg/t steel,respectively.With the increase in the added Ca alloy amount,the inclusions in the steel gradually change from those of 0~2 μm to those of 2~4 and 4~6 μm.Under different Ca treatments,there exist MnS and CuxS inclusions whose size is below 1 μm as well as MnS and CuxS ... 
2013-02-28 172 5.8

以青海盐湖水氯镁石为初级原料,采用喷雾热解法制备原料氧化镁,原料氧化镁通过水化制备硅钢级氧化镁前驱体氢氧化镁。原料氧化镁水化实验中对水化剂、水化温度、水化时间、液固比、搅拌速度及陈化时间对水化率、过滤速度和纯度的影响进行系统研究。采用均匀实验设计和DPS数据处理,(依次)通过建模分析、二次多项式模型回归建立数学模型,再通过各因素方差分析和总方差分析,确定了理论最优实验条件,再用理论最优条件作重复实验进行验证,最终确定了原料氧化镁的最佳水化条件。在水化温度60℃,水化时间105 min,液固比4,陈化时间4 h,水化剂1含量4.0%,水化剂2含量3.15%,洗水量4倍,搅拌速度120 r/min时,原料氧化镁的水化率达99.50%以上,得到的硅钢级氧化镁前驱体氢氧化镁纯度高、过滤性能良好。 By spray pyrolysis method,bischofite in Qinghai salt Lake,as primary raw material,was used to prepare precursor raw material MgO for silicon-steel MgO.The precursor raw material MgO was used for preparing Mg(OH)2 which was the precursor of silicon-steel MgO,by hydration method.In the hydration experiment of precursor raw material MgO,some experiment parameters were investigated systematically.such as the hydrated agent,the temperature and time of hydration,liquid/solid ratio that affected the hy... 
2012-04-28 158 5.8

【作者】 常波; ...
2022-03-28 191 5.8

采用节能、环保、经济型的生产技术与工艺来制造高磁感取向硅钢目前已成为世界各大取向硅钢生产厂的研发热点。总结了国内外各大钢铁企业与研究机构采用低温板坯加热技术生产高磁感取向硅钢的开发及应用情况,概括了传统流程实现低温板坯加热技术的方法。介绍了薄板坯连铸连轧与双辊薄带连铸等短流程工艺生产高磁感取向硅钢的研发现状。在此基础上,探讨了高磁感取向硅钢生产技术与工艺的发展趋势及方向。 Utilizing energy-efficient,environmentally friendly,economic production processes and technologies to manufacture high magnetic induction grain-oriented silicon steel has become the focus of current research work.Based on using low-temperature slab reheating techniques to produce high magnetic induction grain-oriented silicon steel at both iron and steel enterprises and research institutions all over the world,the current application and exploitation was thoroughly generalized;the implementation... 
2013-03-28 150 5.8

【作者】 朱传芳; 潘恒韬; ...
2023-05-11 282 5.8

针对目前大部分无取向电工钢处理液为含铬处理液、且需在较高温度下固化的情况,在分析成膜物质性质的基础上,试验研究了一种可低温快速固化的电工钢环保绝缘处理液,研究了其涂装工艺,并测定了涂层的附着性、绝缘性、耐热性、耐蚀性等性能。试验结果表明:该处理液可在150~250℃下快速烘干固化,涂层表面光滑且致密均匀,性能优良,可满足中小电机的使用要求。 At present,most of the insulating fluid for non-oriented electrical steel contains chromium,and should be cured at high temperature.On the basis of analyzing the characteristics of the film-forming substance,a kind of eco-friendly insulating fluid with lower curing temperature for non-oriented electrical steel sheet was developed in the experiments.Then its coating process was studied,and the adhesiveness,insulativity,heat resistance,corrosion resistance and other properties of the coating was m... 
2013-04-28 156 5.8

采用EBSD技术研究了有、无拉应力作用下无取向硅钢在晶粒长大过程中织构转变及晶界变化的规律。结果表明:在晶粒生长期间,无应力作用下的硅钢中,{111}〈112〉,{111}〈110〉织构组分强化,而{100}〈001〉织构组分弱化;与无拉应力作用下的情况相比,施加5MPa的拉应力时,{111}〈112〉,{111}〈110〉织构组分强化的速率下降,{100}〈001〉织构组分变化不明显。对于在晶粒生长期间持续变化的{111}〈112〉,{111}〈110〉和{100}〈001〉织构组分而言,虽然有、无拉应力作用下硅钢的{111}〈112〉和{111}〈110〉织构组分的高取向差角度晶界频率均下降,而{100}〈001〉织构组分的高取向差角度晶界频率则上升,但当有拉应力作用后,{111}〈112〉和{111}〈110〉织构组分的高取向差角度晶界频率下降的速率变小,{100}〈001〉织构组分的高取向差角度晶界频率上升的速率稍有变小。通过对无取向硅钢在晶粒长大过程中织构转变及晶界变化规律的研究,分析了合金原子在晶界的偏聚行为。 The rules of texture and grain boundary transformation in the nonoriented silicon steel under applied stress or without applied stress during grain growth were investigated by EBSD.The results show that the {111}〈112〉 and {111}〈110〉 components in the nonoriented silicon steel without stress are strengthened during grain growth whereas {100}〈001〉 component is weakened,but the growth rate of {111}〈112〉 and {111}〈110〉 component decreases,while the area fraction of {100}〈001〉 component doesn’t chang... 
2012-09-28 167 5.8

采用磁控溅射方法,分别在纯Fe以及低硅钢基片上沉积富Si膜,并对其进行真空扩散热处理.通过能谱分析及X射线衍射研究了Si在纯Fe与低硅钢基体中的扩散特征,运用DICTRA软件建立了扩散模型.研究发现Si在纯Fe基体中扩散时发生γ-Fe(Si)→α-Fe(Si)相转变,扩散速率受控于相界面的迁移.当沿截面Si含量梯度不足以驱动相界面正向迁移时,延长扩散时间会发生相界面回迁现象,最终趋于单一相内均匀化扩散过程.Si在低硅钢基体中的扩散符合Fick扩散第二定律. Si-rich films were deposited on pure iron and low-Si steel substrates by direct current magnetron sputtering,and then were subjected to vacuum annealing.The distribution characteristics of Si across Fe and low-Si steel substrates were studied by energy spectrum analysis(EDS) and X-ray diffraction(XRD).DICTRA software was used to simulate the diffusion models.It is found that the diffusion behavior of Si in the Fe substrate is from γ-Fe(Si) phase to α-Fe(Si) phase and the rate of diffusion is con... 
2012-10-28 145 5.8

硅钢工业退火炉温度控制具有强耦合、纯滞后、多扰动等特点,它的控制方法代表着一类非线性系统控制的解决方法。以硅钢工业退火炉温度为控制对象,在双交叉限幅控制的基础上引入了智能学习系统,形成了基于智能学习系统的双交叉限幅控制方法来解决此类非线性系统的控制问题,并通过模块化的编程来实现其功能。结果表明:与传统的PID控制相比,该控制方法的控制精度、抗扰性等控制指标有明显提高,是解决此类非线性控制的一种有效方法。 The temperature control of silicon steel industrial annealing furnace has the features of strong coupling,pure lag,multidisturbance. The control method represents the solution of a class of nonlinear control systems. The control object is the temperature control of silicon steel industrial an-nealing furnace, the intelligent learning system based on Double Across Limit Control is introducedand used to solve control problem of this kind of nonlinear system, and the module programming isused to re... 
2014-05-28 167 5.8

研究了采用高温卷取热轧态原料和常化态原料生产高牌号冷轧无取向电工钢组织、织构和磁性能。研究发现钢卷采用750℃高温卷取,下线后立即采用\"保温罩\"对钢卷进行保温,时间96h,然后空冷至100℃时上线生产的工艺可取代常化工艺生产高牌号冷轧无取向电工钢。冷轧上线前,热轧态原料的表层为大量的再结晶组织,这部分组织包括了热轧轧制时保留下来的动态再结晶组织,钢卷本身高温回复后产生再结晶晶粒,以及在保温罩内保温时形成的再结晶组织。高温卷取的热轧态和常化态的热轧卷作为原料时,试样织构类型相似,取向分布密度接近,再结晶后织构类型仍然相似,取向分布密度仍然接近。Goss织构对磁性能增加有促进作用。实验钢中较好的磁性能对应的织构[{100}+Goss]/{111}的比值较高,体现了织构的遗传性。 Microstructure,texture and magnetic properties of high grade cold rolled nonoriented electrical steel which made of hot rolled material with high temperature coiling and with normalization were studied.Steels coiled in high temperature(at 750 ℃),stacked with insulation cover for 96hand air cooled to 100 ℃ were using to manufacture high grade nonoriented electrical steel.The process can replace the normalization process.There are a lot of recrystallized grains in the surface layer of the coil wit... 
2014-03-28 171 5.8