试验研究了0.3 mm取向硅钢冷轧板(/%:0.046C,3.07Si,0.09Mn,0.029P,0.004S,0.005A1)的退火温度(760~880℃7 min)和退火时间(820℃3~9 min)对该钢的晶粒尺寸,再结晶和织构的影响。结果表明,最佳初次再结晶退火工艺为820℃5 min,该钢的平均晶粒尺寸为14.20μm,完全再结晶率为92%,不利{111}<110>结构含量为3.16%,有利织构{111}<112>,{012}<001>和高斯织构含量分别0.40%,4.73%和2.46%。 The effect of annealing temperature(at 760 ~ 880 X.for 7 min) and time(at 820℃ for 3~9 min) on grain size,recrystallization rate and texture of 0.3 mm cold-rolled sheet of oriented silicon steel(/%:0.046C,3.07Si,0.09Mn,0.029P,0.004S,0.005Al) has been tested and studied.Results show that with optimum recrystallized annealing at 820℃ for 5 min,the silicon steel average grain size is 14.20 fun,the complete recrystaUization rate is 92%,the unfavourable-texture {111}< 110 > content in steel is ... 
2014-03-28 459 5.8

【摘要】 <正>3月15日,随着第5754卷HiB钢下线,武钢...
2011-02-28 340 5.8

研究了薄板坯连铸连轧流程(TSCR)条件下热轧工艺对3.2%Si-0.7%Al无取向硅钢组织、织构演变及磁性能的影响规律。结果表明,提高均热温度和热轧温度有助于获得粗大的变形组织和强烈的{001}〈110〉织构,进而对后续的组织、织构演变进程及磁性能产生有利的遗传影响。与低温均热和低温热轧相比,高温均热和高温热轧得到的最终成品板的再结晶晶粒较粗大,λ纤维再结晶织构较强而γ纤维再结晶织构较弱,磁感应强度较高。 It was investigated that the effects of thin slab cast rolling(TSCR) hot rolling processes on microstructural,textural evolution and magnetic properties of 3.2%Si-0.7%Al non-oriented silicon steel.The results show that much larger hot rolling deformed microstructure and much stronger {001}〈110〉 texture could be obtained by increasing the soaking and hot rolling temperatures,which had good heritable effects on subsequent microstructural,textural evolution and magnetic properties.The final sheets ... 
2023-05-09 326 5.8

【机构】 武钢研究院; ...
2013-06-28 183 5.8

【作者】 凌健; ...
2011-03-28 330 5.8

综述了电工钢从生产到成品过程中涉及到的检测项目、检测方法及仪器,并通过对电工钢标准的发展改进,详细阐述了我国现有的电工钢技术标准体系,同时对代表企业的电工钢重点指标进行了摘录对比,为综合应用电工钢检测方法并促进电工钢的发展提供了一定的参考。 This article summarizes the testing items,methods,and instruments involved in the process from manufacturing to finished products of electric steel. The current electric steel technical standards system in our country is also elaborated in detail,along with the development and improvement of electric steel standards. Meanwhile,by comparison of electric steel KPI in representitive companies,this article provides references for comprehensive application of electric steels testing methods and promo... 
2014-05-28 300 5.8

【摘要】 <正>10月9日至11日,武钢一硅钢技术改造工...
2011-06-28 378 5.8

针对节能电机对无取向电工钢在磁性能方面的特殊要求,采用普通W600牌号的热轧板为原料,通过大量的现场工艺试验,研究总结出了\"超低张力\"的运行工艺、\"先快后慢\"的加热工艺、\"先湿后干\"的退火脱碳工艺、\"先缓后急\"的冷却工艺,生产出P1.5/50≤4.0 W/kg、B50≥1.70 T的冷轧电工钢产品,满足了节能电机的要求。 Based on the special requirements of no-oriented electrical steel for saving energy motor in magnetic aspects,using common W600 brand of hot rolled plate as raw material,through a large number of real tests,an ultra-low tension process,heating process which was quick at first and then slow,annealing decarburization process which was dry after the first wet,and a cooling technology of \"slow after the first urgent\" were concluded.Electrical steel product with P1.5/50≤4.0W/kg,B50≥1.70T was produced... 
2014-08-28 193 5.8

【作者】 朱传芳; 潘恒韬; ...
2023-05-11 368 5.8

分析了影响脱碳效果和结晶行为的各种要素及其相互制约关系,提出了Hi-B连续退火工艺曲线,总结得出快速加热及合理稳态气氛是实现工艺制度的关键。结合实际工程,介绍了在连续退火炉设计中快速加热和气氛设计的考虑方法,并指出随着Hi-B产品的发展,如何改进这些方法将是连退工程研发的方向之一。 The factors which affect decarbonization and crystallization and the mutual restriction between them were analyzed.A complete continuous annealing process for Hi-B was put forward.As a result,the rapid heating and the proper steady atmosphere were two important factors.According to an actual project,the consider methods for designing rapid heating and proper steady atmosphere were introduced,and it is pointed that with the development of Hi-B technique,how to improve these techniques would be on... 
2011-02-28 375 5.8

采用扫描电镜、原子力显微镜研究了铬酸镁半无机绝缘涂层的微观结构。结果表明,涂层厚度为数微米,涂层中的有机树脂乳液颗粒均匀分布在无机涂层的表面,从而保证了涂层具有良好的冲片性能。采用极化曲线研究了涂层的耐蚀性能,发现铬酸镁与铬酸锌绝缘涂层的耐蚀性能相当。 In this paper,the microstructure and anti-corrosion property of magnesium chromate coating on non-oriented silicon steel were studied.The microstructure was observed by SEM and AFM.The anti-corrosion properties were evaluated by polarization curves.The results show that the thickness of coating is several microns and the polymer particles were scattered on the surface of inorganic coating,which is the guarantee for lamination property.The corrosion resistance of the magnesium chromate film was e... 
2011-03-28 329 5.8

针对川威950的工艺现状,结合无取向低硅钢SGG生产的工艺特点,主要从控制其钢坯加热和轧制以及终轧温度和卷曲温度几方面入手,进行无取向低硅钢生产的工艺控制研究。同时根据近6000吨的生产实践表明,该工艺措施能很好的满足该钢种的需要。 950 process Chuanwei status quo,with non-oriented silicon steel production process features low,mainly from the control of billet heating and rolling and finish rolling temperature and coiling temperature of several aspects,for non-oriented silicon steel production process of low control at the same time According to nearly 6,000 tons of production practice shows that the process measures could well meet the needs of the steel. 
2011-01-28 377 5.8