钢厂
取向硅钢成品晶粒的位向测定方法
取向硅钢成品的晶粒尺寸非常大,其易磁化方向[001]晶向对于轧向的偏差角度对其磁性能影响极大。本文介绍了取向硅钢二次再结晶后成品晶粒位向的几种测定方法,包括侵蚀法、劳厄法、OIM法、极图法和非对称X射线衍射法等,并对这几种测量方法进行了比较。 The finished product of grain-oriented silicon steel has immense grain size ranging from millimeters to centimeters and the deviation angles of easy magnetization direction from rolling direction plays a remarkable role in magnetic properties of grain-oriented silicon steel.The methods in common use for determining the deviation angles of crystal direction are introduced,which include the etch-figure method,the Laue method,the OIM method,the pole figure method and the asymmetrical X-Ray diffract...
Nb微合金化Fe14Si2高硅钢温轧板织构演变规律
采用Nb对Fe-6.5%Si(质量分数)高硅钢进行微合金化处理,结果表明:Nb在高硅钢薄板制备过程中细晶效果明显.铸态、锻态和热轧态组织的晶粒分别细化了17.50%,24.51%和30.13%.铸态样品压缩强度由1365 MPa提高至1520 MPa,延伸率提高77.78%;温轧板试样室温拉伸强度由573 MPa提高至621 MPa,延伸率提高44.44%.利用XRD对厚度为0.30—1.68 mm的温轧板的板面织构演变过程进行跟踪测量,结果发现:初始织构以(011)〈100〉Goss织构为主,单道次变形量为26.2%的情况下,Goss织构完全转化为(100)〈011〉旋转立方织构,随后,在单道次变形为22.6%的情况下,旋转立方织构完全转化为{111}面织构,即纤维织构,并稳定保持至0.30 mm. Fe-6.5%Si(mass fraction) alloy possess perfect magnetic properties,though intermetallics of Fe14Si2 phase brought 6.5%Si leads to room temperature brittleness and hinder this significant materials industrialization.Nb was adopted into micro-alloying of Fe-6.5%Si high silicon steel. OM,thermal simulated test machine and XRD were employed to study the influence of Nb on high silicon steel in processing stages.Textures of warm-rolled high silicon steel strips were determined b...
薄板坯连铸连轧流程生产高磁感取向硅钢的研究现状与技术分析
概述了高磁感取向硅钢生产工艺的研究现状及发展趋势。介绍了国内外薄板坯连铸连轧流程生产高磁感取向硅钢的研究现状。从流程工序特点、热履历、组织与抑制剂控制方面进行对比,分析了薄板坯连铸连轧流程相对传统板坯流程生产高磁感取向硅钢的技术优势,在此基础上提出了利用该流程生产高磁感取向硅钢需要解决的主要技术难点。 The current status and development trend of production process for high magnetic induction grain-oriented silicon steel are summarized.The research status of producing high magnetic induction grain-oriented silicon steel by thin slab casting and rolling process at home and abroad is introduced.The potential technical advantages of producing high magnetic induction grain-oriented silicon steel by thin slab casting and rolling process are obtained by analyzing in terms of process characteristics,t...
普通取向硅钢轧制过程中组织和织构的演变
借助电子背散射衍射(EBSD)及ZEISS-200MAT金相显微镜对某钢厂普通取向硅钢(CGO)进行研究,研究结果表明:热轧板组织、织构沿板厚方向存在明显的不均匀性,在热轧板表层及次表层发生再结晶,同时存在强度较高的Goss织构,中心层存在较强的{001}<110>变形织构。冷轧组织均呈纤维状条带组织,一次冷轧后,热轧板中的Goss织构消失,织构主要为α、γ织构,经中间脱碳退火后,α、γ织构强度减弱,并出现一定强度的Goss织构和利于Goss织构发展的{554}<225>、{332}<113>等织构,经二次冷轧后,二次冷轧织构类型与一次冷轧织构一致,但织构强度不同。 The grain-oriented silicon steel produced by a steel factory was investigated by EBSD and ZEISS-200 MAT metallographic microscope.The results show that the textures and microstructures along thickness of hot rolled slab are inhomogeneous.The surface layer and the layer near that are recrystallized structure which has a high Goss texture,but there is deformation texture{001}<110>in the central layer.The structure after cold rolling is a structure like fiber strip.After the first cold rollin...
硅钢高温氧化铁皮的显微结构表征
利用电子探针面分析、状态分析及电子背散射衍射相分析技术研究硅钢高温氧化铁皮的显微结构。电子探针面分析可以直观的看出元素的分布状态,初步判断氧化铁皮的结构,而状态分析可以准确表征常规氧化铁皮中铁元素的状态,对于合金元素富集区域则通过电子背散射衍射相分析技术来标定。结果表明,高温氧化铁皮的结构主要有4层,即最外层为厚度约为10μm的Fe2O3相,次外层为Fe3O4相,中间层为FeO相上分布有颗粒状的Fe3O4相,最内层为FeO相和Si元素富集的Fe2SiO4相。其中Fe2SiO4层的分布特征与加热温度密切相关:1 100℃时,Fe2SiO4相呈颗粒状,弥散分布在FeO层;1 200℃时,Fe2SiO4相呈液态,侵入基体和疏松的FeO层,且沿着FeO晶界呈网状分布。 The microstructure of high temperature oxide scale on silicon steel was characterized by electron probe microanalyzer(EPMA)mapping analysis,state analysis and electron backscatter diffraction(EBSD)phase analysis.The element distribution and the initial structure of the oxide scale could be detected by EPMA mapping analysis apparently.And the state of iron in the conventional oxide scales could be determined by state analysis.Meanwhile,the alloy-rich region could be identified by EBSD phase analy...
取向硅钢中含铜抑制剂的固溶析出行为
含铜抑制剂作为取向硅钢的主抑制剂或辅助抑制剂不仅可以抑制初次晶粒的长大,促进二次再结晶,还可以降低铸坯的加热温度。取向硅钢中主要抑制剂为10~50 nm Cu2S,在钢的铸坯、热轧、冷轧、脱碳等工艺过程均可析出;(Cu,Mn)1.8S、Cu1.8S、ε-Cu等主要作为辅助抑制剂,尺寸一般为30~50 nm(或大于50 nm),主要在热轧阶段析出。总结了国内外有关取向硅钢中含铜抑制剂析出行为的研究进展,当前主要研究不同生产流程和工序中含铜抑制剂的析出行为和作用机理。 As main inhibitor or auxiliary inhibitor for grain-oriented silicon steel,the particles of inhibitor bearing copper not only inhibit the primary crystal growing and promote the secondary recrystallization,but also decrease the heat temperature of casting slab.The main inhibitor for grain-oriented silicon steel is 10~50 nm Cu2S,which precipitate in process and procedure including steel casting slab,hot rolling,cold rolling and decarburizing process,while the 30~50 nm or more than 50 nm...
电脉冲对取向硅钢凝固组织的影响
对熔融态钢液进行处理,研究了电脉冲对于取向硅钢凝固组织的影响作用,利用正交试验法研究了脉冲电容、频率、处理时间和电压等脉冲参数的作用效果。结果表明:电脉冲对钢锭晶粒组织具有明显的细化作用,凝固组织的等轴晶比例大幅上升,影响等轴晶比例的最显著性因素为脉冲频率,最优正交试验参数为电容1 200μF,脉冲频率1 Hz,处理时间5 s,脉冲电压800 V。随着输入能量的增大等轴晶率先增大后减小,脉冲输入能量为某值时,等轴晶率最大,利用经典形核理论和热力学对这一现象进行了解释。 The influence of electric pulse on the solidification structure of oriented silicon steel was investigated by applying electric pulse in molten steel.The affection due to different electric pulse parameters such as electric capacity,frequency,applied time and voltage was studied by orthogonal design test.The result showed that solidification structure of oriented silicon steel could be improved by the electric pulse,and the equiaxed crystal ratio increased obviously.The most influential paramete...
微合金元素Sn、Nb、Re对无取向硅钢性能的影响
介绍了微合金元素锡、铌、稀土对无取向硅钢性能的影响,并扼要分析了这些元素对硅钢性能的影响机理:晶界偏聚元素Sn可细化晶粒提高硅钢磁性能;微合金元素Nb细化铁素体晶粒,提高硅钢的强度、韧性和塑性及磁性能;稀土元素(RE)在硅钢中的主要作用包括净化钢液、变质夹杂物、改善铸态组织和性能及微合金化,减少晶界上出现偏析的几率。 The influence of micro-alloy elements on properties of non-oriented silicon steel and the mechanism for effect of the micro-alloy elements including Sn、Nb and RE on the properties of steel are presented and analyzed in this paper.Grain boundary segregation elements Sn in steel can grain refinement and improve the magnetic properties;Micro-alloy elements Nb can refine the ferrite grain,increase the silicon steel strength,toughness and plastic;The main role of the RE in the silicon steel including...
冷轧无取向硅钢横向厚差控制
冷轧中中低牌号的无取向硅钢多采用万能凸度轧机(Universal crown mill,UCM)生产,其板形好坏受制于UCM轧机板形调节手段的协调使用。为掌握UCM轧机的板形控制特点,建立基于二维变厚度有限元的辊系弹性变形和基于三维差分的轧件塑性变形的六辊轧机耦合模型,对UCM轧机的板形调控性能进行详尽的分析,包括工作辊和中间辊弯辊、中间辊窜辊的调控功效、辊间接触压力分布等。在此基础上,提出可用指导生产的板形控制策略,指出UCM轧机在横向厚差控制方面的不足。针对工业生产中UCM轧机轧制无取向硅钢横向厚差大的问题,在大量仿真计算的基础上,开发具有高次曲线函数的边部变凸度(Edge variable crown,EVC)的工作辊。采用该工作辊后,各种品种的无取向硅钢的横向厚差不大于10μm的百分比由24%提高到99%,横向厚差的均值小于6μm,远小于之前的13μm。 Medium-low grade non-oriented silicon steel is rolled often by universal crown mill(UCM) during cold rolling.Its shape quality is dependent on the coordinated control of several shape adjustment devices of UCM.In order to understand the shape control characteristics of UCM,coupling model of six-high rolling mill,based on two-dimensional varying thickness finite element rolls elastic deformation model and three-dimensional finite difference strip plastic deformation model,is setup for the detaile...