钢厂
硅钢级氧化镁反应行为的研究
利用DSC、XRD,结合热焓分析对硅钢级氧化镁和二氧化硅的固相反应行为进行了研究。比较了不同二氧化硅原料及混合方法对硅钢级氧化镁反应性的影响,找到了一种更为有效的硅钢级氧化镁反应性的评估方法,克服了传统柠檬酸活性法在比较不同厂家生产的氧化镁的反应性上的局限性。进一步研究了Na2B4O7添加剂、TiO2添加剂对氧化镁和二氧化硅反应行为的影响,结果表明,Na2B4O7添加剂含量的增加对反应有利,而TiO2添加剂对反应有阻碍作用。 The solid-state reaction behavior between silicon-steel grade MgO and SiO2 was investigated by DSC and XRD combined with enthalpimetric analysis.The influence of different kinds of SiO2 and different preparation methods were studied and a specifical measurement that is more reliable was proposed to evaluate reactivity of silicon steel grade MgO.It overcomes the limitation of the traditional citric acid activity(CAA) method,which can not be used to evaluate the reactivity of...
取向硅钢成品晶粒的位向测定方法
取向硅钢成品的晶粒尺寸非常大,其易磁化方向[001]晶向对于轧向的偏差角度对其磁性能影响极大。本文介绍了取向硅钢二次再结晶后成品晶粒位向的几种测定方法,包括侵蚀法、劳厄法、OIM法、极图法和非对称X射线衍射法等,并对这几种测量方法进行了比较。 The finished product of grain-oriented silicon steel has immense grain size ranging from millimeters to centimeters and the deviation angles of easy magnetization direction from rolling direction plays a remarkable role in magnetic properties of grain-oriented silicon steel.The methods in common use for determining the deviation angles of crystal direction are introduced,which include the etch-figure method,the Laue method,the OIM method,the pole figure method and the asymmetrical X-Ray diffract...
硅元素对Fe-(4.5~7.0)%Si高硅钢组织和性能的影响
通过Axio Imager金相显微镜考察4.5%~7.0%硅(质量分数)对高硅钢材料组织形貌的影响,并利用Fe-6.5%Si高硅钢薄板制备方法对其进行轧制,通过DDL50电子万能试验机对阶段产品进行力学性能测试。结果证明,硅含量为5.58%的高硅钢在实验硅含量区间内存在最大延伸率及最小铸态组织晶粒尺寸。 An investigation about the influence of 4.5%-7.0% Si on microstructure and mechanical properties of high-silicon steel was presented.SEM was adopted to take an observation towards microstructure during fabrication,and DDL50electronic universal testing machine was applied into the detection of tensile curves.The results show that silicon steel with 5.58% Si provides the maximum elongation and minimum grain size as cast.
Si在纯Fe及低硅钢中扩散行为
采用磁控溅射方法,分别在纯Fe以及低硅钢基片上沉积富Si膜,并对其进行真空扩散热处理.通过能谱分析及X射线衍射研究了Si在纯Fe与低硅钢基体中的扩散特征,运用DICTRA软件建立了扩散模型.研究发现Si在纯Fe基体中扩散时发生γ-Fe(Si)→α-Fe(Si)相转变,扩散速率受控于相界面的迁移.当沿截面Si含量梯度不足以驱动相界面正向迁移时,延长扩散时间会发生相界面回迁现象,最终趋于单一相内均匀化扩散过程.Si在低硅钢基体中的扩散符合Fick扩散第二定律. Si-rich films were deposited on pure iron and low-Si steel substrates by direct current magnetron sputtering,and then were subjected to vacuum annealing.The distribution characteristics of Si across Fe and low-Si steel substrates were studied by energy spectrum analysis(EDS) and X-ray diffraction(XRD).DICTRA software was used to simulate the diffusion models.It is found that the diffusion behavior of Si in the Fe substrate is from γ-Fe(Si) phase to α-Fe(Si) phase and the rate of diffusion is con...
双辊连铸无取向硅钢铸带特征及常化作用研究
双辊连铸技术是冶金及材料领域内的一项前沿技术,对于生产高品质硅钢具有独特优势.本实验研究了一种双辊铸轧w[Si]=4.5%的无取向硅钢,考察其铸态和常化处理后样品的组织、织构及析出相尺寸特征.结果表明:铸带组织以与铸带法向成5~20(°)倾角的柱状晶为主,晶内存在少量0.3~0.4μm的AlN析出相,铸带织构以λ(<001>//ND)织构为主,表层织构漫散.950℃/10 min常化处理后,析出相尺寸增大,表层λ织构增强. As an advanced technique of metallurgy and material science,twin- roll strip casting has unique advantages for producing high quality silicon steel. The present study was aimed at a 4. 5% Si non- oriented electrical steel for analyzing the structure,texture and the size of precipitates at the initial and normalized state. The results revealed that the initial structure mainly consisted of columnar grains with 5 ~ 20( °) angle to the normal of cast strip,and some AlN precipitates of 0. 3 ~ 0. 4 μ...
火花源原子发射光谱法测定取向硅钢中碳硅锰磷硫
通过试验确定氩气分析流量为3.5L/min,静态流量为0.75L/min,冲洗时间为3s,预燃时间为12s,积分时间为5s的激发条件,采用火花源原子发射光谱法测定取向硅钢中碳、硅、锰、磷、硫。分别采用铣床铣样、砂轮磨样两种制样方式进行了精密度考察,发现制样方式对结果影响不大;讨论了取向硅钢样品中碳、硅、锰、磷、硫测定时可能存在的共存元素干扰,发现硅对锰元素的干扰不可忽略,采用干扰系数法进行了校正,据此拟合得到各元素校准曲线的相关系数均在0.999 0以上。精密度考察结果表明,碳、硅、锰、磷、硫的相对标准偏差(n=10)在0.71%~9.4%之间。对两块取向硅钢生产样品进行分析,并与钢铁研究总院进行比对分析,结果一致,且偏差均在允许范围内。 Carbon,silicon,manganese,phosphorus and sulfur in oriented silicon steel were determined by spark source atomic emission spectrometry.The selected excitation conditions were as follows:the analytical flow rate of argon was 3.5L/min,the static flow rate was 0.75L/min,the flush time was3s,the precombustion time was 12sand the integration time was 5s.Two sample preparation methods,including milling machine and grinding wheel,were investigated.The precision test results showed that,the determination...
低温高磁感取向硅钢连铸与均热过程AlN与MnS析出的热力学
针对薄板坯连铸连轧流程结合\"获得抑制剂法\"所制备的低温高磁感取向硅钢,通过热力学计算研究了AlN与MnS在连铸与均热过程中的析出规律与行为。计算结果表明,连铸过程中AlN在凝固后的高温α相中便可能析出,而MnS仅可能在凝固后的α+γ两相区内析出。钢中AlN与MnS在均热过程中均处于部分固溶与部分析出的状态。后续高温渗氮处理后初次晶粒的异常长大并不明显,表明渗氮处理前钢中固有抑制剂的数量相对充足。 The precipitation behavior of MnS and AlN in low-temperature high magnetic induction grain-oriented silicon steel produced by thin slab casting and rolling process with\"acquired inhibitor method\"during continuous casting and soaking was studied by thermodynamic calculation.The calculated results show that AlN is likely to precipitate in ferrite after solidification.However,MnS can precipitate only in the two phase region of ferrite and austenite.Meanwhile,MnS and AlN in the steel can not be comp...
锌浴中钛对含硅钢Fe-Zn反应的抑制作用
选用Q235和Q345钢,在纯锌浴和含钛量分别为0.05%、0.10%、0.15%、0.20%(质量分数)的合金浴中浸镀0.5、1、3、5、8 min。利用扫描电子显微镜和能谱仪研究了钛对热浸镀锌组织和生长动力学的影响,并提出钛对含硅钢铁锌反应抑制作用的机理。结果表明:钛的加入缩短了Γ的孕育期,促进了合金层中δ的生长和ζ的消失,δ的生长依然受扩散控制,呈抛物线生长规律;Zn-0.05%Ti锌浴可以很好的抑制高硅钢的硅反应性;含硅钢热浸镀锌钛合金浴时,在锌浴中会形成锌铁钛三元T相,该相能吸收ζ晶界处富集的硅,从而抑制了铁锌反应。 Both Q235 and Q345 steels were immersed for 0.5 to 8 min in Zn bath with different amount of Ti,ranging from 0 to 0.20 mass%,for galvanization.The effect of Ti in Zn bath on microstructure and growth kinetics of hot-dip galvanizing coatings on the two steels were investigated by means of SEM and EDS analysis.Base on the experiment,the mechanism of Ti additions in controlling Fe-Zn reaction was proposed.The results show that addition of Ti in the zinc bath decreases the incubation time of Γ phase...
冷轧压下量对取向硅钢极薄带显微组织的影响
观察了取向硅钢极薄带经冷轧至不同厚度,并经过不同工艺热处理后的显微组织及亚结构。结果表明:冷轧压下量越大,显微组织中位错密度越高,冷变形组织越多,等轴晶粒越少;增加冷轧压下量可以使试样的再结晶温度降低,当钢带厚度为0.08 mm时,在650℃退火时就能发生明显的再结晶。 Microstructure and substructure of the grain oriented ultra-thin silicon steel sheets is analyzed,which are rolled down to different thickness and treated with different heat treatment process.The result shows that there are higher dislocation density,more cold deformation structure and less equiaxed crystal grain in microstructure of the steel sheets with more cold rolled reduction.Increase of cold rolled reduction will decrease recrystallization temperature,and when thickness of the steel shee...
二次冷轧的中间退火温度对2.3Si无取向硅钢组织和性能的影响
试验2.3Si无取向硅钢(/%:0.003C,2.30Si,0.16Mn,≤0.020P,≤0.005S,0.54Al)冷轧板由常化和未常化的2.5 mm热轧板冷轧至0.6 mm(压下率76%),经750~950℃2.5 min中间退火后再冷轧至0.5 mm(压下率16.7%),成品板经890℃+960℃2.5 min退火。研究了中间退火温度对该钢晶粒尺寸、织构和磁性能的影响。结果表明,随中间退火温度的升高,二次冷轧前晶粒和成品晶粒增大,成品中不利织构组分{111}和{112}减弱,磁性能得到改善。热轧板经过常化时的磁性能明显好于未经常化时的磁性能,但中间退火温度较高时常化对磁性能的有利作用减弱。 The test cold sheet of 2.3Si non-oriented silicon steel(/%:0.003C,2.30Si,0.16Mn,≤0.020P,≤0.005S,0.54Al) is first cold-rolled from normalized and un-normalizing 2.5 mm hot-rolled plate to 0.6 mm sheet(reduction 76%),then intermediate annealed at 750~950℃ for 2.5 min and double cold-rolled to 0.5 mm sheet(reduction16.7%),the finished sheet annealed at 890℃+960℃ for 2.5 min.Effect of the intermediate annealing temperature on grain size,texture and magnetic performance of the steel has been studied....
酸溶铝对铸态取向硅钢中第二相粒子组成和形貌的影响
试验的铸态取向硅钢(/%:0.0440.056C,3.123.32Si,0.080.11Mn,0.0020.008S,0.002 90.029 1Als,0.006 20.010 9N)由30 kg高频真空感应炉熔炼。通过场发射扫描电子显微镜/能谱仪(FE-SEM/EDS)研究结果表明,0.002 9%Als钢中氧化物主要为SiO2,存在片状、棒状及近似球状的独立MnS,未发现含铝的氧化物或氮化物;0.0090%Als钢中出现以Al2O3为主的复合氧化夹杂物,存在MnS与AlN的复合析出物。钢中Als增加,复合析出物多呈簇状发展。氧化物容易成为MnS-AlN复合析出的核心,钢中Als含量越低,夹杂物中的MnS含量越高;作为核心的氧化物夹杂的尺寸越小,形成的复合夹杂物的形状越规则,尺寸也越小。热力学计算结果表明,钢中Als含量主要影响了钢中氧化物夹杂的组成和AlN的析出温度及析出量。 Test as-cast grain-oriented silicon steel(/%:0.044 0.056C,3.12 3.32Si,0.08 0.11Mn,0.0020.008S,0.002 90.029 1 Als,0.006 20.010 9N) is melted by a 30 kg high frequency vacuum induction furnace.The research results by using field emission-scanning electron microscope/energy dispersive spectrometer(FE-SEM/EDS) show that in 0.002 9%Als steel the main oxide is SiO2,and there is independent laminable,rod-like and approximate ...