钢厂
TSCR试制高强度无取向电工钢
采用固溶强化、细晶强化和位错强化方法,模拟TSCR流程试开发高强度无取向电工钢,试开发钢的主要合金成分为3%Si、0.83%Al和2.99%Mn。分析热轧、常化、退火后的钢板组织,并针对不同的成品板组织,详尽地分析了相应的力学性能和磁性能。试验电工钢平均晶粒直径为12.37μm时,R p0.2为530 MPa,R m为618 MPa;当退火制度为700℃×4 min,成品组织完全为未再结晶的回复组织时,R p0.2为853.5 MPa,R m为895.5 MPa。该成分的电工钢P15/50或P10/400最小时,对应的平均晶粒直径都大于59.67μm;P10/800或P10/1000最小时,对应的平均晶粒直径都处于12.37~59.67μm尺寸区间。 TSCR was simulated to develop high-strength non-oriented electrical steel with 3% of Si,0.83% of Al and 2.99% of Mn by solution strengthening,grain refinement strengthening and dislocation strengthening.The microstructures of hot rolled plates,normalized plates and annealed plates were analyzed.Furthermore,the mechanical properties and magnetic properties of products with different microstructures were detailedly studied.As the average grain diameter of the steel was 12.37 μm,the yield strength ...
基于CSP工艺取向硅钢初次再结晶晶界特征对宏观织构的影响
利用背散射衍射技术(EBSD)和XRD,研究了两段式脱碳退火工艺对取向硅钢纵截面初次再结晶的微区取向、取向差分布、特殊晶界(CSL)及高温退火试样高斯织构。分析了初次再结晶晶界特征对取向硅钢高温退火后宏观织构的影响。结果表明:初次再结晶的纵截面基体中Σ3和Σ5晶界使得高斯晶粒有着较高的迁移率,在高温退火时借助20o~45°的大角度晶界的界面能吞并周围{111}<112>晶粒迅速长大,形成密度水平较高的高斯织构。 Micro area orientation of primary recrystallization,the misorientation distribution,special boundaries under different two-stage decarburization annealing and the Goss texture under high temperature annealing the longitudinal section of grain-oriented silicon steel were detected by electron back scattering diffraction(EBSD) and X-ray diffraction(XRD).The effect of primary recrystallization grain boundary on macrotexture after high temperature annealing was analyzed.The results show that the Σ3 a...
高硫硅钢的硫化物析出行为及其微观组织和电磁性能变化
为了弄清楚高硫硅钢中的硫化物析出行为及其对钢的微观组织和电磁性能的影响,以便为工业化生产制定更为合理的硫含量控制标准和采取更为有效措施减轻炼钢生产的硫含量控制压力,结合0.25% Si 无取向硅钢 ,采用非水溶液电解提取 + 扫描电镜/透射电镜观察相结合的方法 ,研究了0.006 8%、0.010 2%、0.025 5% 和 0.035 3% 硫含量条件下,钢中的硫化物夹杂物组成和存在形式及其形貌、种类、尺寸、数量变化,以及相应的热轧、成品试样的微观组织和电磁性能变化。结果表明,随着钢中硫含量的增加,钢中的硫化物逐渐由 MnS→MnS+Cu2S→Cu2S转变,数量逐渐增多,尺寸向高低两个方向发展。相应地,导致热轧再结晶组织劣化和抑制了成品晶粒尺寸长大。随着钢中硫含量的增加,钢的磁感、铁损劣化程度逐渐增大。钢中的硫含量平均每增加 0.01%,涡流损耗、磁滞损耗分别劣化0.24 W/kg 和 0.41 W/kg,而磁感会劣化 0.009 T。但是 ,在硫含量为 0.010 2% 时 ,铁损可以低于 6.0W/kg,而在硫含量为 0.025 5% ... In order to find out the precipitation behavior of sulfide inclusions and the corresponding changes of microstructure and electromagnetic properties of high sulfur silicon steel sheets, so that to design more suitable sulfur concentration controlling limit for industrial manufacture and to release the steel-making difficulty effectively, Based on the change of given sulfur concentration 0.006 8%, 0.010 2%0.025 3% and 0.035 3%, the type and composition, the size and number, and the size distribut...
硅钢连退机组无氧化炉加热能力计算
无氧化炉具有加热效率高、投资与运营成本低、作业率高、表面质量及板型良好、NOx排放相对低等优势,在硅钢热处理领域应用前景广泛。本文阐述了确定无氧化炉(NOF)加热能力详细过程,涵盖炉温、炉断面尺寸、炉长、热平衡结算、加热能力计算等,为今后无氧化炉(NOF)在硅钢热处理应用时的设计提供了借鉴,同时也为今后明火直接加热的工业炉设计提供了参考。 Non-oxidation furnace has the advantage s of high heating efficiency, low investment and operation cost, high operation rate, good surface quality and plate shape, and relatively low NOxemission,and it still has wide application prospect in the field of silicon steel heat treatment. The detailed process of determining the heating capacity of a non-oxidizing furnace(NOF) is described, covering furnace temperature, furnace section size, furnace length, heat balance settlement, heating capacity cal...
凝固速率对定向凝固50W600无取向硅钢固液界面稳定性和枝晶间距的影响
采用ZMLMC超高梯度定向凝固装置,研究了5种凝固速率(10、35、80、150和450μm/s)对定向凝固50W600无取向硅钢的固液界面稳定性转变规律和一次、二次枝晶间距的影响。研究结果表明,在特定的温度梯度下,随着凝固速率的增加,定向凝固的固液界面由胞状晶转变为胞状枝晶,再转变为细小的树枝晶。随着凝固速率的增加,定向凝固组织的枝晶形貌逐渐细化,一次和二次枝晶间距逐渐减小,且与冷却速率之间都符合指数关系:λ1=151.73×(G L·R)-0.31,λ2=22.07×(G L·R)-0.44。当冷却速率达到4.275℃/s时,一次、二次枝晶间距分别为112μm、14.1μm。 Under the conditions of certain temperature gradient and different solidification rate,the directional solidification experiment of non-oriented electrical steel 50W600 was carried out.The microstructure of 50W600 steel was also analyzed in different solidification rate.The result shows that the solid/liquid interface of the steel undergoes an evolution from cellular,cellular dendrite and finally to fine dendrite morphologies.The dendrite refines gradually and the distance between dendrites decr...
碳化法制备硅钢氧化镁过程中杂质脱除研究
以轻烧氧化镁粉为原料,经消化、碳化制得重镁水,在热解反应前采用络合剂对重镁水中的杂质钙、铁进行络合掩蔽,再经热解得到碱式碳酸镁,碱式碳酸镁经煅烧可制得钙、铁杂质含量较低的氧化镁。在重镁水络合除杂过程中,考察了络合剂三乙醇胺、柠檬酸、草酸单独和复合使用的除铁、除钙效果。以三乙醇胺为络合剂时,在200 mL重镁水中加10 mL三乙醇胺(1∶1),氧化镁产品中w(氧化镁)=99.3%、w(氧化钙)=0.31%、w(氧化铁)=0.042%;使用草酸和柠檬酸作为复合络合剂时,在200 mL重镁水中加入1.0 g柠檬酸和2.0 g草酸,氧化镁产品中w(氧化镁)=98.2%、w(氧化钙)=0.24%、w(氧化铁)=0.030%。 Light-burned magnesia as a raw material was hydrated and carbonated to obtain magnesium bicarbonate liquor.Before the pyrolyzing of magnesium bicarbonate liquor,complexants were used to cover Fe and Ca impurities.Then the treated liquid was pyrolyzed to obtain basic magnesium carbonate which was calcined to magnesium oxide with low calcium and iron content.During the complexing purification of magnesium bicarbonate liquor,the Fe and Ca removing effects of single or compound complexing agents,suc...
卷取工艺对新型冷轧无取向电工钢组织性能的影响
研究了卷取工艺对一种新型含铜无取向电工钢晶粒尺寸、织构演变、铁损和磁感应强度的影响。结果表明,试样织构组分主要为{111}、{112}、{100}和高斯织构,在550℃卷取、保温2~3h,{100}织构有增强趋势,磁感应强度较高,铁损较低。 The effects of coiling process on grain size,texture,core loss and magnetic induction of a new cold rolled non-oriented electrical steel with copper were investigated.The results show that there are mainly {111},{112},{100} and {110}<001> texture.Coiling at 550℃and keeping for 2~3 hours,the {100} texture is enhanced,magnetic induction is higher and core loss is lower.
高Cu无取向电工钢的制备
运用EBSD和光学显微镜,研究了0.25%~0.45%Cu对无取向电工钢热轧板显微组织,成品板显微组织、织构和磁性能的影响。实验结果表明:卷取过程中Cu元素在热轧板表层的偏聚作用显著阻碍了热轧板表层再结晶晶粒长大,导致热轧板表层晶粒尺寸随着Cu含量增加而逐渐较小,但热轧板中间晶粒尺寸变化不大。同时发现Cu元素能够明显改善织构类型,使有利织构组分增加,不利织构组分减少,同时减弱织构强度。从实验结果可知0.35%Cu能够显著改善电工钢的磁性能,铁损P15/50最低达到4.1 W/kg,磁感B50最高值达到1.8 T。 Effects of high content Cu on microstructure of hot rolled plates and microstructure,texture and magnetic properties of annealed finish product plates of non-oriented electrical steel were examined by means of EBSD technique and optical microscope. The results show that surface segregation of Cu significantly hindered recrystallized grain growth of surface layer in hot rolled plate during the coiling,as a result,the surface grain sizes of the hot-rohed plates decrease with the increase of Cu con...
冷轧工艺对取向硅钢初次再结晶织构的影响
研究了取向硅钢制备过程中常见的两种冷轧工艺,主要研究了一阶段冷轧与两阶段冷轧+中间退火工艺对初次再结晶组织及织构的影响.结果表明:采用两阶段冷轧+中间退火工艺制备以Cu2S为主抑制剂的取向硅钢,其初次再结晶平均晶粒尺寸为18.1μm,高斯晶粒的体积分数为0.6%,迁移性强的重位点阵晶界(Σ5+Σ9)和高能晶界(20°~45°取向偏差角)所占比例分别为1.8%和50.4%.与一阶段冷轧工艺相比,其初次再结晶晶粒较细,且高斯晶核与特征晶界所占的比例较高,有利于高斯晶粒发生二次再结晶. Two common cold-rolling processes of grain oriented silicon steel and the effects of the single stage cold rolling and tw o-stage cold rolling w ith intermediate annealing processes on the primary recrystallization microstructure and texture w ere investigated. The results revealed that for the grain oriented silicon steel prepared under the tw o-stage cold rolling process w ith intermediate annealing w ith Cu 2 S as the main inhibitor,the average grain size of the primary recrystallization micr...
微合金元素对冷轧取向电工钢再结晶行为的影响
以取向电工钢成分为基础,制备了含C或Mn和S的4种实验钢。观察了接近平衡析出状态实验钢经60%冷轧后在600~1000℃范围再结晶退火过程中微观组织演变,统计分析了再结晶体积分数随退火时间的变化规律,进而计算了各实验钢静态再结晶的激活能。观察了高含C实验钢退火初期再结晶晶粒优先出现的部位。结果表明900~1000℃范围内各实验钢铁素体的化学成分相似,因而其再结晶激活能基本一致。在600~800℃范围内铁素体内会有阻碍再结晶进程的三次渗碳体析出,从而使再结晶激活能明显提高。高C含量实验钢中还会有从奥氏体转变而来的粗大珠光体或渗碳体,轧制过程中其附近形成的变形区会促进600~800℃加热时该区域附近率先发生再结晶形核、降低再结晶激活能。固溶的Mn、S元素可微弱提高再结晶激活能,但高Mn、S含量会改变粗渗碳体从奥氏体析出时的形态。 Four experimental steels based on grain oriented electrical steel containing C,or Mn and S were prepared.Microstructure evolution of the steels close to a state of equilibrium precipitation were observed during annealing processes at 600-1000 ℃after 60% cold rolling,the changes of recrystallization volume fraction were analyzed statistically as the annealing was prolonged,and the activation energy for static recrystallization of the steels were calculated.The locations,where the recrystallizatio...