对冷轧无取向硅钢在冶炼过程中各个工序的顶渣进行了检测,分析了顶渣变化原因,并得出结论:硅钢生产宜采用复吹转炉,以降低吹炼终点渣中TFe含量,进而减轻对精炼的压力;使用低S、低Al2O3含量中间包覆盖剂;RH脱氧及合金化顺序采用先加硅铁后加铝;首罐宜经LF提温并降低渣中TFe。 The top-surface slag used for the various production processes in smelting coldrolled non-oriented electrical steel is tested and based on tested results the cause of the top surface slag change is analyzed.So it is concluded that the combined blown converter is more suitable to be used for smelting electrical steel in order to reduce the content of TFe in slag at blow end point and then much better results can be achieved during the period of refining.Secondly the tundish flux contenting low co... 
2013-03-28 205 5.8

【作者】 吴玉美; 陆晔; ...
2023-05-09 270 5.8

【作者】 常波; ...
2022-03-28 495 5.8

通过观察冲剪边缘组织,测量冲剪边缘的显微硬度、残余应力的分布情况和磁性能的变化研究了冲剪加工对无取向硅钢50WW800边缘组织和磁性能的影响。对冲剪后硅钢片进行750℃退火,分析退火对组织和磁性能的影响。结果表明,硅钢片剪切边缘会存在0.4 mm的形变硬化层,边缘应力大,铁损增加。退火后变形减小,形变硬化层变小,残余应力大幅度减少,铁损减少。 The influence of punching process on cutting edge microstructure and magnetic properties of non-oriented silicon steel 50WW800was studied by observing microstructure and measuring microhardness near cutting edge.The residual stress distribution in the silicon steel tooth and magnetic properties were measured.Effect of annealing at 750 ℃ on microstructure and magnetic properties of the silicon steel was analyzed.The results show that a cut-edge hardening layer up to 0.4 mm is observed,residual st... 
2023-04-28 278 5.8

在实验室试制了TSCR流程的低碳低硅无取向硅钢,研究了在850~1050℃不同温度常化对冷轧量0.5mm厚钢板再经950℃×7min退火后的组织、织构和磁性能的影响。结果表明:随常化温度的升高,使热轧板晶粒尺寸增大,晶界更清晰,组织均匀性更好;由于第二相AlN和MnS析出物尺寸比较大,使冷轧退火后钢板晶粒也随常化温度升高呈单调增大趋势;γ有利织构和{111}、{112}不利织构与常化温度升高同时增强,但前者增强更多;冷轧板退火后铁损随常化温度升高呈单调下降,磁感呈单调上升趋势。 The low-carbon and low-silicon non-oriented silicon steel was prepared by thin slab casting and rolling(TSCR) in lab.The effect of normalizing at different temperatures in 850-1 050℃on microstructure, texture and magnetic properties of 0.5 mm cold-rolled sheets after annealing at 950℃for 7 min was researched. The results show that with increasing the normalizing temperature,the grain size of hot-rolled sheets increased,the grain boundaries were more clear and the rnicrostructure uniformity was b... 
2011-03-28 383 5.8

【作者】 潘恒韬; 欧阳帆; ...
2023-05-09 284 5.8

针对攀钢高硫铁水冶炼现状,结合不同生产工艺路线,论述了攀钢近年来为实现低硫电工钢的生产,在铁水预处理、转炉冶炼、钢水精炼过程中硫控制技术的开发与应用,形成了低硫洁净钢生产工艺技术,实现了低硫电工钢的生产。低硫电工钢RH脱硫率可达到20%左右,成品[S]控制在0.006%左右。 According to the smelting situations of hot metal with high sulphur content at Panzhihua Steel,combined with different produce processes,technologies for controlling the sulfur content during hot metal pretreatment,converter smelting,and second refining are developed. Technologies in low-sulfur clean steelmaking are formed. Low-sulfur electric steel are produced. As for the desulfurization rate of lowsulfur electric steel can reach about 20%,and the content of [S] in products is controlled to ab... 
2013-03-28 409 5.8

介绍了双蓄热燃烧技术的特点和高温硅钢加热炉的特点,探讨了双蓄热燃烧技术在高温硅钢加热炉中使用的技术难点,分析了双蓄热燃烧技术在高温硅钢加热炉上使用的可能性。 Introduced characteristics of double regenerative combustion technology and high temperature silicon steel reheating furnace,discussed technical difficulties for using double regenerative combustion technology,analyzed the possibility of double regenerative combustion technology applied to high temperature silicon steel reheating furnace. 
2013-03-28 292 5.8

借助于EBSD对比研究了常化退火对高牌号无取向电工钢热轧组织和织构演变的影响,分析了常化退火对热轧板各厚度层织构的演变规律。结果表明,常化退火改善了热轧组织的均匀性,并弱化了热轧变形的γ纤维织构。升高常化退火温度,可增大热轧板的晶粒尺寸,提高{100}和{110}织构组分占有率,有利于提高无取向电工钢成品板的磁性能。 Effects of normalizing annealing on microstructure and texture of high-grade non-oriented electrical steel hot-rolled sheet were investigated by EBSD. Emphasis was put on the effects of normalizing annealing on texture evolution in the sheet thickness. The results show that the hot-rolled microstructure homogeneity is improved and the γ-fiber texture is weakened by normalizing annealing treatment. The grain size of hot-rolled sheet and intensity of the {100} and {110} favorable texture can be in... 
2014-02-28 194 5.8

【机构】 商务部进出口公平贸易局; ...
2013-02-28 531 5.8

从取向硅钢生产路线的选择、工艺技术的改进和生产设备的改造三方面进行了生产取向硅钢的节能降耗技术改造.通过完善多元抑制剂配方生产低温取向硅钢,通过加抛丸的酸洗、带面超声波清洗、改进连续退火炉以及余热循环利用等技术改造,使2012年取向硅钢的产量与未进行技术改造前的2009年相比提高了2.5倍,产品磁性上升了一个半牌号,能耗下降了8.9%,成材率提高了6.4%,生产成本下降了22%,综合效益显著. Energy saving technological transformation was carried out in the production of grain oriented silicon steel from three aspects of the oriented silicon steel production process route selection,technology improvement and equipment renovation.Through the improvement of multiple inhibitor formulations for producing low-temperature grain-oriented silicon steel,and by adding the blasting pickling,the belt surface ultrasonic cleaning,improvement of continuous annealing furnace,waste heat recycling tec... 
2013-02-28 263 5.8

采用RH精炼添加钙合金方式对硅钢进行钙处理。结果表明,钙合金添加量为0.67、1.00、1.67kg/t钢时,钢中钙含量分别为0、2×10-6、4×10-6;随着钙合金添加量增大,钢中夹杂物粒度逐渐由0~2μm向2~4、4~6μm偏移;不同钙处理条件下,钢中均存在粒径小于1μm和粒径为1~5μm的MnS、CuxS夹杂物,后者或单独存在,或同AlN、CaS夹杂复合;粒径为5~10μm区间,钢中的夹杂物基本以钙的氧、硫化物为主。与钙处理前相比,钙合金添加量为0.67、1.00、1.67kg/t钢时,粒径小于1.0μm的微细夹杂物减少幅度分别为68.06%、87.50%、94.94%。钙合金添加量为1.67kg/t钢时,可以去除钢中绝大部分的微细夹杂物。 Ca alloy was added into the liquid steel during RH refining,and the results show that Ca concentration in final Si steel sheets is insignificant,about 0,2×10-6 and 4×10-6 when the added amount of Ca is 0.67,1.00 and 1.67 kg/t steel,respectively.With the increase in the added Ca alloy amount,the inclusions in the steel gradually change from those of 0~2 μm to those of 2~4 and 4~6 μm.Under different Ca treatments,there exist MnS and CuxS inclusions whose size is below 1 μm as well as MnS and CuxS ... 