以试验室模拟CSP工艺生产的Fe-3Si热轧钢带为研究对象,采用正交试验及方差分析的方法,研究了取向硅钢初次再结晶退火工艺对高温退火后获得锋锐的高斯织构的影响。结果表明:取向硅钢两段式初次再结晶脱碳退火工艺参数加热段保温时间及加热温度是高温退火后获得锋锐高斯织构的主要影响因素,其可信度分别在90%和85%以上;在本试验条件下,通过正交试验获得的最佳退火工艺为:冷硬板经600℃保温3 min和850℃保温6 min。 Fe-3Si hot rolled strip was produced by simulating CSP technology in the laboratory.Orthogonal experiment and analysis of variance were carried out to investigate the influence of primary recrystallization on the sharp Goss texture of the oriented silicon steel.The results show that holding time of the heating section and the heating temperature for a sharp Goss texture of the samples annealed has important implications in this experiment conditions,the two-step decarburization annealing process... 
2013-02-28 233 5.8

【摘要】 <正>近日,从重钢集团获悉,日前重钢炼钢厂...
2013-01-28 418 5.8

采用双辊薄带连铸工艺制备了厚度为2.4mm的3.98%Si-0.71%Al无取向硅钢带,经常化、冷轧、不同温度退火后,对其显微组织、析出物、织构和磁性能进行了检测分析。结果表明:随着退火温度的提高,退火板晶粒尺寸增大,组织均匀性提高;退火板析出物主要是AlN和MnS与AlN复合析出物,尺寸较粗大,达0.5~2.5μm;退火板织构沿厚度方向变化明显,表层和1/2层存在较强的{100}织构,1/2层还存在较强的{111}织构,1/4层主要是{112}织构;随退火温度的升高相应的铁损和磁感应强度均降低。 Using twin roll thin strip continuous casting technique,the 3.98%Si-0.71%Al no-oriented silicon steel strip in thickness of 2.4mm was produced.The microstructure,precipitates,texture,and magnetic properties of the sheet after normalizing,cold rolling and annealing at different temperatures were studied.The results show that with annealing temperature increase,the grain size and uniformity of annealed sheet increased.The main precipitates in coarse size of 0.5-2.5μm in annealed sheet were AlN and... 
2014-01-28 318 5.8

主要研究了0.7%Si无取向电工钢退火试样的组织、晶粒尺寸和织构对其磁性能的影响。结果表明,随着退火温度的升高,晶粒尺寸逐渐增大,组织的均匀性得到改善;ɑ取向线上的纤维织构多集中于{114}<110>和{223}<110>附近,再结晶结束后,织构含量变化不大。{111}<110>织构取向密度值随温度升高而下降,{112}<111>织构与{111}<110>织构变化相反。晶粒尺寸增大对磁感强度的影响较小,而对铁损的影响较大。 Influences of microstructure,grain size and texture on the magnetic properties of 0.7% Si non-oriented electrical steels annealed samples were studied.The results show that with annealing temperature increasing the average grain size is increased gradually.Uniformity of the microstructure is improved;the textures of ɑ-fiber gathered in the vicinity of the { 114} < 110 > and { 223 } < 110 > texture.After recrystallization,the volume fraction of texture changes small.{ 111} < 110 &g... 
2013-07-28 218 5.8

【作者】 卢鹏; ...
2014-03-28 177 5.8

采用双辊薄带连铸工艺试制了2.6 mm厚5.28%Si-1.11%Al高硅钢薄带,对比了1050℃×5 min正火及不正火铸带280℃冷轧至0.5 mm后,再经900~1100℃退火的磁性能。结果表明,高硅钢铸带显微组织为等轴晶组织,正火后铸带边部晶粒长大,中心层晶粒变化较小。成品中析出物主要为较粗大的AlN和AlN+MnS复合析出物,尺寸为0.5~2.5μm。与不正火试样相比,正火试样成品铁损大幅降低,磁感小幅下降;随退火温度的升高,两种工艺下铁损和磁感都是先降低后升高,在1050℃出现最低值。 2.6 mm thickness 5.28% Si-1.11% Al non-oriented high silicon steel was produced by twin roll thin strip casting.Magnetic property of the strip un-normalized and normalized at 1050 ℃×5 min was contrasted after cold rolled to 0.5 mm at 280 ℃ and 900-1100 ℃ final annealing.The results show that microstructure of the strip is equiaxed crystal.The surface grain is coarsened and the center layer grain has little change of the normalized strip.The main precipitates are AlN and MnS+AlN with 0.5-2.5 μm s... 
2013-06-28 289 5.8

研究了常化温度、常化时间及常化后冷却速度对Si的质量分数为1.6%的无取向电工钢成品磁性能的影响。结果表明:在850~1 050℃范围内,随着常化温度的升高,成品铁损先减小后增大,成品磁感应强度先增大后减小;当常化温度为1 000℃时,成品平均铁损最低,平均磁感应强度最高;常化时间从3min延长到7min时,成品铁损先减小后增大,成品磁感应强度则呈单调下降趋势;随着常化冷却速度的降低,成品铁损先减小后增大,成品磁感应强度则呈单调增大趋势;对于Si的质量分数为1.6%的无取向电工钢,最佳的常化制度为:在1 000℃进行常化,时间5min,常化后空冷。对热轧板进行常化后,热轧板发生了不同程度的再结晶和晶粒长大。提高常化温度、延长常化时间、降低冷却速度,都能使常化板晶粒粗化,进而粗化成品板晶粒,改善磁性能。通过扫描电镜观察发现,成品板中析出物主要为AlN和MnS的复合析出物,以及少量的单独析出的AlN和MnS,而常化工艺主要是通过粗化析出相,减少细小析出相数量,从而减少对晶界钉扎作用来改善成品磁性能。 The effects of normalizing temperature,normalizing time and cooling rate after normalizing on magnetic properties of non-oriented electrical steel with mass fraction of Si of 1.6% were investigated.The results show that core loss of product decreases first and then increases,while magnetic induction increases first and then decreases with the increase of normalizing temperature from 850 to 1 050℃.Average core loss of product is the lowest and average magnetic induction is the highest when normal... 
2014-09-28 241 5.8

为了提升新能源车用驱动电机的功率密度,各大电机厂商都在不断地提升电机转速,随之而来的问题就是电机的铁耗也在不断增高,如何降低电机铁耗成为了电机厂商必须要解决的难题。本文讨论了电机铁耗的组成部分及影响因素,并对1台8极48槽的永磁同步电机分别使用3种不同厚度的材料进行仿真,对比其效率及铁耗分布,推导出驱动电机中硅钢厚度、铁耗及成本的关系,最后对驱动电机选材提出建议。 In order to increase the power density of traction motor for new energy vehicles,major motor manufacturers have been constantly increasing the motor speed.The following problem that manufacturers have to solve is how to reduce the increasing iron loss when the motor speed is increased.The components and influencing factors of motors’ iron loss were discussed in this paper,and an 8-pole 48-slot permanent magnet synchronous motor using three different thickness materials was simulated.To compare i... 
2022-01-28 337 5.8

对无取向硅钢炼钢全流程钢液增钛的原因进行了分析,认为铁水钛含量、转炉出钢温度、转炉下渣量、精炼渣TiO2含量、钢水罐及RH浸入管混钢种生产是影响钢液增钛的主要原因。通过采取低钛铁水冶炼,减少转炉下渣量,提高出钢温度,添加白灰改质精炼渣等措施,均能够降低钢液中的钛含量。 After analyzing the causes leading to increased content of titanium in molten nonoriented silicon steel during whole steelmaking process, it was concluded that such factors as content of titanium in hot metal, tapping temperature from converter, quantity of roughing slag entered into the ladle from converter, content of TiO2 in refining slag, molten steel ladle car,carrying out the steelmaking of different steel grades by the same ladle and same RH immersion tube were the main causes ... 
2022-01-28 229 5.8

介绍了国内、外电工钢极薄带的生产现状及市场应用的情况,以及典型生产企业的生产规模、产品性能和应用领域,指出扩大高牌号无取向电工钢生产、提高产品质量是目前电工钢发展的迫切要求。 The production situation and market application of ultra thin electrical steel strip at home and abroad were described.The production capability,product property and application area of typical corporation were introduced.The results indicate that the urgency needed of electrical steel development is expanding high-grade non-oriented electrical steel production and improving products quality at present. 
2011-04-28 258 5.8

试验2.3Si无取向硅钢(/%:0.003C,2.30Si,0.16Mn,≤0.020P,≤0.005S,0.54Al)冷轧板由常化和未常化的2.5 mm热轧板冷轧至0.6 mm(压下率76%),经750~950℃2.5 min中间退火后再冷轧至0.5 mm(压下率16.7%),成品板经890℃+960℃2.5 min退火。研究了中间退火温度对该钢晶粒尺寸、织构和磁性能的影响。结果表明,随中间退火温度的升高,二次冷轧前晶粒和成品晶粒增大,成品中不利织构组分{111}和{112}减弱,磁性能得到改善。热轧板经过常化时的磁性能明显好于未经常化时的磁性能,但中间退火温度较高时常化对磁性能的有利作用减弱。 The test cold sheet of 2.3Si non-oriented silicon steel(/%:0.003C,2.30Si,0.16Mn,≤0.020P,≤0.005S,0.54Al) is first cold-rolled from normalized and un-normalizing 2.5 mm hot-rolled plate to 0.6 mm sheet(reduction 76%),then intermediate annealed at 750~950℃ for 2.5 min and double cold-rolled to 0.5 mm sheet(reduction16.7%),the finished sheet annealed at 890℃+960℃ for 2.5 min.Effect of the intermediate annealing temperature on grain size,texture and magnetic performance of the steel has been studied.... 