低温高磁感取向硅钢常化工艺中间冷却制度的研究
借助电子背散射(EBSD)技术对AlN为主抑制剂的Hi-B取向硅钢常化工艺的中间冷却制度进行了研究。结果表明:常化后试样均发生了完全再结晶,在60℃/s冷速下组织最均匀;在合适的冷却制度下常化板表层保留了强的Goss织构,它深入到1/4厚度处,并且形成对Goss织构有利的强{554}<225>织构。 The intermediate cooling system of Hi-B oriented silicon steel with AlN main inhibitor in normalizing process was studied by means of electron back diffraction(EBSD) technique. The results show that:the specimens after normalizing are fully recrystallization, and the microstructure is most uniform under the intermediate cooling rate of 60℃/s; under suitable cooling system, normalized plate surface retains strong Goss texture, it penetrates into the 1/4 thickness of the plate and forming strong {...
高硅钢薄板退火过程中的织构演变
采用传统的轧制和退火工艺制备了0.30mm厚的6.5%(质量分数)Si高硅电工钢薄板,采用X射线衍射技术对退火过程中的再结晶织构进行了研究。冷轧高硅钢薄板700℃退火形成以{111}〈112〉为峰值的γ织构(〈111〉∥ND)和以{001}〈210〉为峰值的{001}织构;而900℃以上温度退火则形成强{001}〈210〉织构。进一步的研究表明是在晶粒长大过程中{001}〈210〉发展成为主要再结晶织构组分。 High silicon steel thin sheets with thickness of 0.3mm were successfully produced by conventional rolling and annealing methods.Recrystallization texture was investigated by means of X-ray diffraction.It is found that recrystallization texture is mainly composed of γ fiber(〈111〉∥ND)with peak at {111}〈112〉 and {001} fiber with peak at {001}〈210〉 after annealing at 700℃,while strong {001}〈210〉 component dominates recrystallization texture after annealing above 900℃.It is during grain growth that {...
高温卷取的热轧态原料与常化态原料生产高牌号无取向硅钢的比较
研究了采用高温卷取热轧态原料和常化态原料生产高牌号冷轧无取向电工钢组织、织构和磁性能。研究发现钢卷采用750℃高温卷取,下线后立即采用\"保温罩\"对钢卷进行保温,时间96h,然后空冷至100℃时上线生产的工艺可取代常化工艺生产高牌号冷轧无取向电工钢。冷轧上线前,热轧态原料的表层为大量的再结晶组织,这部分组织包括了热轧轧制时保留下来的动态再结晶组织,钢卷本身高温回复后产生再结晶晶粒,以及在保温罩内保温时形成的再结晶组织。高温卷取的热轧态和常化态的热轧卷作为原料时,试样织构类型相似,取向分布密度接近,再结晶后织构类型仍然相似,取向分布密度仍然接近。Goss织构对磁性能增加有促进作用。实验钢中较好的磁性能对应的织构[{100}+Goss]/{111}的比值较高,体现了织构的遗传性。 Microstructure,texture and magnetic properties of high grade cold rolled nonoriented electrical steel which made of hot rolled material with high temperature coiling and with normalization were studied.Steels coiled in high temperature(at 750 ℃),stacked with insulation cover for 96hand air cooled to 100 ℃ were using to manufacture high grade nonoriented electrical steel.The process can replace the normalization process.There are a lot of recrystallized grains in the surface layer of the coil wit...
热轧组织对无取向硅钢织构的影响
采用X射线衍射仪分析无取向硅钢冷轧织构和再结晶退火织构的演化,研究了热轧组织对无取向硅钢织构以及磁性能的影响。结果表明,具有均匀、粗大晶粒组织的热轧板,冷轧形成更多的剪切带,导致成品板形成高的高斯织构组分,并提高了{100}织构强度,降低了γ纤维织构,最终导致成品磁感应强度升高,铁损下降。 The texture evolution of non-oriented silicon steel during cold-rolling and recrystallization annealing was investigated by X-ray diffractometer.The effects of hot band microstructure on the texture and magnetic properties of non-oriented silicon steel were analyzed.The results show that more shear bands appear during cold rolling due to homogeneous coarse grain in hot band.So strong{110}<001> texture after recrystallization annealing forms.At the same time,the {100} texture components inc...
冷轧无取向硅钢的边缘降控制优化研究
某冷连轧机生产无取向硅钢板材时,其边缘降的长度合格率频繁超标。为满足用户的叠片厚度精度要求,这类产品必须以增大切边量的方式来保证交货质量,而这种方式又直接降低了金属收得率,提高了生产成本。基于此,以该产线现有设备特性为基础,详细分析其软、硬件功能模式,分别对辊形与反馈控制进行全面分析与优化改进。通过现场试验论证,充分明确依托辊形优化与反馈控制程序的改进能显著提高边缘降的控制水平,该技术的使用为生产现场的边缘降控制提供了合理的技术支撑。 A cold rolling mill production of non-oriented silicon steel sheet,the thickness difference of the edge( edge-drop) is usually exceed the preset standard value,In order to meet the accuracy requirements of the user flatness,these production must be trimed wider length to meet the delivery quality of the user need, which directly reduce the metal yield and increase the manufacturing cost. Therefor,the software and hardware of the production line has been analyzed, and the work roll shape and feed...
硅钢级氧化镁颗粒度检测工艺的研究
通过对激光粒度分析仪测量硅钢级氧化镁(MgO)的分析条件进行优化,如分散介质、分散方式、样品预处理、仪器暗淡度等,探讨了硅钢级MgO粒度范围测量重现性较好的试验方法,满足硅钢生产过程控制对MgO粒度的要求。 The analysis condition of the laser particle size analyzer on grain oriented silicon-steel grade magnesium oxide is optimized,including the dispersion medium,dispersion methods,sample preparation,and instrument obscuration,etc.Therefore,particle size measurement with good reproducibility for silicon-steel magnesium oxide is discussed,which may meet the requirement of MgO particle size for silicon-steel process control.
夹杂物尺寸及数量对无取向硅钢磁性能影响的主成分回归分析
采用扫描电镜、场发射扫描电镜、能谱仪等对50SW1300冷轧无取向硅钢中的夹杂物分不同尺寸区间进行数量统计,利用主成分回归分析法,即数据的标准化处理—主成分分析—回归分析—标准化的变量还原成原始变量—确定显著影响因素,综合分析夹杂物总量及各尺寸区间的夹杂物数量对无取向硅钢磁性能的影响。结果表明:主成分回归分析能够从夹杂物尺寸区间及数量的多个影响因素中提取主要的因素,定量研究其对磁性能的影响。分析表明,显著影响无取向硅钢铁损的夹杂物为100~500nm的AlN、AlN+MnS、MnS、Al2O3、AlN+Al2O3,而劣化磁感最明显的夹杂物尺寸区间为100~200nm。 Different size intervals of inclusions in cold rolled non-oriented silicon steel 50SW1300 were counted by scanning electron microscope(SEM),field emission scanning electron microscope(FESEM)and energy disperse spectroscopy(EDS).With principal component regression method:standardization for experimental data,principal component analysis,regression analysis,transform standardized variables into original variables,determination of significant factor,effects of the total number of inclusions and the...
高效电机用冷轧无取向电工钢退火板析出物的析出特征研究
通过热力学计算,分析了实验钢中主要析出物析出的可能性。结果表明:在液相和固液两相区中,AlN和MnS均不能析出;在奥氏体区,AlN和MnS具备热力学析出条件,平衡析出温度分别为1547、1582 K。成品退火板中的析出物主要为AlN和MnS。扫描电镜下观察到的AlN形貌多为长条状,MnS形貌多为棒状或近似球形。这两种析出物占了析出物总量的85%以上,尺寸集中分布在400~800nm;复合析出物主要是(Al2O3+MnS)和(AlN+MnS),形貌不规则,尺寸集中在0.7~1.5μm;透射电镜下观察到了少量100nm以下独立的AlN析出。 According to thermodynamic calculation, the precipitation probability of precipitates was analyzed, AlN and MnS can not precipitate in liquid phase area and solid-liquid two-phase area. In austenite area, both the AlN and MnS have precipitation condition in thermodynamics and precipitates at 1547 K and 1582 K, respectively. The precipitates in annealing plate are mainly AlN and MnS. The shape of AlN is mostly strip, and MnS is stick or near sphericity. They accounted for over 85% of the total qu...
冷轧无取向硅钢产品标准浅析
聚焦无取向硅钢产品标准,从电磁性能、表面性能、机械性能以及尺寸公差与边部质量等维度对国际标准IEC、EN、JIS、ASTM以及国标GB进行了分析研究。分析得出,各类标准在电磁性能方面要求基本一致;ASTM标准的机械性能要求有别于其他几个标准。 In this paper,non-oriented silicon steel standards of EN,JIS,GB and ASTM were compared and analyzed. It is showed that,all types of standards in electromagnetic performance requirements are basically the same. Surface properties in ASTM standard are expressed in the most detailed. The mechanical properties requirements of the standards,except for ASTM,are basically the same.
热轧辊冷却对冷轧无取向电工钢卷纵向磁性的影响及工艺优化
通过对35W300高牌号0.35 mm冷轧无取向电工钢卷(/%:0.002C、2.71Si、0.22Mn、0.015P、0.003S、0.0020N、0.55Als)头、中、尾组织、织构及对应的磁性能的试验研究,发现因热轧时12 MPa高压水连续冷却造成接触轧辊的钢卷头、中、尾在不同温度下轧制,卷取后钢卷头部处于卷心、温度略高而冷却速度略低于钢卷尾部,致使钢卷纵向组织、织构不同,成品卷头、尾各250 m内磁感逐渐增加,铁损逐渐降低,250 m外至钢卷中部磁性能稳定。通过将热轧辊的冷却方式改为周期冷却和卷取后的层流冷却改为钢卷70 m后开始冷却,至钢卷尾部70 m前停止冷却的方式使得钢卷纵向铁损差异明显减小,磁感差异略有改善。 According to the test research on structure and texture of head,meddle and end of 35W300 high grade 0.35 mm cold rolled non-oriented electrical steel strip coil(/%:0.002C,2.71Si,0.22Mn,0.015P,0.003S,0.002 0 N,0.55Als) and corresponding magnetic properties,It is found that due to 12 MPa high pressure water continuous cooling the roller in hot rolling process led to head,middle and tail of strip rolling at different temperature and after coiling the head of strip coil being in center of coil led t...
电工钢极薄带生产现状及市场应用
介绍了国内、外电工钢极薄带的生产现状及市场应用的情况,以及典型生产企业的生产规模、产品性能和应用领域,指出扩大高牌号无取向电工钢生产、提高产品质量是目前电工钢发展的迫切要求。 The production situation and market application of ultra thin electrical steel strip at home and abroad were described.The production capability,product property and application area of typical corporation were introduced.The results indicate that the urgency needed of electrical steel development is expanding high-grade non-oriented electrical steel production and improving products quality at present.