钢厂
试样剪切应力对冷轧无取向电工钢磁性能的影响
电工钢试样加工产生的剪切应力会恶化钢板的磁性,对不同牌号硅钢片的横向、纵向试样退火前后磁性能的变化进行研究,结果表明:无取向硅钢片在剪切过程中横向、纵向的磁性受到剪切应力影响是不一样的。 The electrical steel sample processing magnetic of electrical steel will worsen due to the shear stress of sample. In this paper,the magnetic change of transverse,longitudinal specimens of different type of silicon steel sheet before and after annealing are studied. The results show that the magnetic of non- oriented silicon steel sheet affected in the process of shear is not the same in horizontal and vertical direction.
硅钢轧制过程中乳化液流量数学模型研究及应用
目前高磁感冷轧硅钢生产过程中,采用经验方法确定的乳化液流量设定值往往会造成硅钢产品的磁感性能达不到预期目标,针对此情况,基于轧机轧制机理研究了的乳化液流量数学模型,确定了乳化液流量设定值。实践表明,使用该数学模型输出的乳化液流量设定值,可提高轧制过程中乳化液流量控制精度,从而提高高磁感冷轧硅钢的轧制性能。 In view of the current production process of high magnetically inductive cold-rolled silicon steel, the mathematical model of emulsified fluid flow based on mill rolling mechanism is studied in view of the situation in which the magnetic sensing performance of silicon steel products is often not up to the expected target by using empirical method to determine the emulsified liquid flow setting. Practice shows that the emulsified fluid flow setting value output from this mathematical model improv...
表面机械研磨/异步轧制无取向硅钢薄带的渗硅行为
对w(Si)=3%无取向硅钢进行表面机械研磨处理(SMAT)和异步轧制(CSR),获得表面纳米结构,再进行550~650℃、4 h固体粉末渗硅处理,用透射电镜(TEM)、扫描电镜(SEM)和X射线衍射仪(XRD)研究表层组织演变。结果表明:经过SMAT后,w(Si)=3%无取向硅钢表面形成了等轴状、取向呈随机分布的、晶粒尺寸为10 nm的纳米晶组织;异步轧制后,表面纳米晶组织保持不变;550~650℃、4 h渗硅处理后,SMAT+CSR样品表面形成化合物层,其厚度随着温度的升高由17μm增加到52μm;化合物层由Fe3Si和FeSi相组成. Nanostructured surface layer was fabricated on a 3%(mass fraction) non-grain oriented silicon steel by means of surface mechanical attrition treatment(SMAT) and cross-shear rolling(CSR),and then a solid powder siliconizing treatment was carried out for the SMAT+CSR sample at 550~650 ℃ for 4 h.The microstructural evolution was examined by using transmission electron microscopy(TEM),scanning electron microscopy(SEM) and X-ray diffraction(XRD).Experimental results show that: equiaxed nanocrystallin...
固溶处理对高牌号无取向硅钢磁性能的影响
对商用50W330型无取向硅钢成品在930℃下保温2 h固溶并以不同方式冷却处理,利用磁性检测仪检测分析了处理前后的磁感和铁损变化,应用光学显微镜、扫描电子显微镜、X射线衍射仪观测分析了显微组织结构的演变。考察了平均晶粒尺寸、织构组分比及第二相粒子状态对磁性能的影响规律,结果表明:固溶处理前后平均晶粒尺寸的变化对硅钢磁性能的影响非常显著;当平均晶粒尺寸相差不大时,织构组分比[Goss+{100}]/{111}越大,磁感会越高;固溶处理会将细小弥散的第二相粒子重新回溶到基体中,减小了其对磁畴壁的钉扎作用,铁损随之下降。 The commercial 50W330 non-oriented silicon steel samples were heat treated at 930℃ for 2 h and cooled in different ways,then the iron loss and the magnetic induction of the samples before and after solution treatment were measured with a magnetic detector.The evolution of microstructural texture was analyzed by optical microscopy,scanning electron microscopy and X-ray diffractometry.The effects of average grain size,texture composition ratio and the second phase particles on the magnetic propert...
高效电机用无取向硅钢退火板组织和析出物研究
研究了组织和析出物对高效电机用无取向硅钢退火板磁性能的影响。结果表明:随着退火温度升高,退火板平均晶粒尺寸增加,P15/50明显降低,B50略有升高。退火温度在1 000℃时,退火板的综合性能较好。析出物主要是AlN、(MnS+AlN)和(MnS+Al2O3)复合析出物,尺寸较粗大,主要集中在1.0~2.5μm,还发现少量百纳米以下的细小AlN和TiN。实验室模拟TSCR流程试制的高效电机用无取向硅钢,铁损平均值小于4.00 W/kg,磁感应强度大于1.75 T,适合作中小型高效电机铁芯材料。 Effects of microstructure and precipitation on magnetic property of non-oriented silicon steel sheets after annealing for high-efficiency motor are studied in the paper by experiments.The annealed sheet exhibits a larger average grain size,obviously decreasing iron loss and slightly raising magnetic induction with increasing temperature.The annealed sheet has better comprehensive properties at a annealing temperature of 1 000 ℃.The main precipitates are compounds of AlN、(MnS+AlN)and(MnS+Al2O3) w...
50W600无取向硅钢钙处理的热力学分析及实验研究
通过热力学计算及实验室研究,对钙处理前后50W600无取向硅钢退火冷轧板中夹杂物的类型、数量及尺寸进行了系统分析。结果表明,50W600无取向硅钢经钙处理后(w(Ca)=0.002 6%),钙在1 600℃的钢液中主要以固态的CaO·2Al2O3、CaO·6Al2O3及溶解钙的形式存在。在钢液的凝固过程中,钢中的溶解钙和硫反应生成了CaS和CaS-MnS复合夹杂,有效抑制了MnS的弥散析出,减少了钢中微细夹杂物的数量。同时钙处理促进了钢中微细夹杂物的聚合长大,导致显微夹杂物的数量增加。 Based on thermodynamic calculation and laboratory experiment,the type,quantity and size of inclusions in annealed cold-rolled steel sheets of 50W600 non-oriented silicon steel before and after calcium treatment were systematically studied.Results showed that after calcium treatment(w(Ca) = 0.002 6%),calcium was mainly in the form of CaO·2Al2O3,CaO·6Al2O3 and dissolved calcium in steel at 1 600 ℃.Dissolved calcium could combine with sulfur to form CaS inclusions and compound CaS-MnS inclusions du...
电工钢生产中硫的控制
针对攀钢高硫铁水冶炼现状,结合不同生产工艺路线,论述了攀钢近年来为实现低硫电工钢的生产,在铁水预处理、转炉冶炼、钢水精炼过程中硫控制技术的开发与应用,形成了低硫洁净钢生产工艺技术,实现了低硫电工钢的生产。低硫电工钢RH脱硫率可达到20%左右,成品[S]控制在0.006%左右。 According to the smelting situations of hot metal with high sulphur content at Panzhihua Steel,combined with different produce processes,technologies for controlling the sulfur content during hot metal pretreatment,converter smelting,and second refining are developed. Technologies in low-sulfur clean steelmaking are formed. Low-sulfur electric steel are produced. As for the desulfurization rate of lowsulfur electric steel can reach about 20%,and the content of [S] in products is controlled to ab...
电子探针波谱仪定量测定硅钢中硅含量结果的不确定度评定
依据GB/T 15616—2008《金属及合金的电子探针定量分析方法》,采用电子探针波谱仪对某W600硅钢中的硅含量进行了定量测定,对影响其定量测定结果的不确定度分量进行了分析,并对不确定度的各个分量进行了计算和合成,最后给出了硅钢中硅含量测定结果的不确定度报告:该硅钢中的硅含量(质量分数)为1.50%,扩展不确定度U=0.20%,取包含因子k=2。 According to GB/T 15616-2008\"Quantitative Method for Electron Prohe Microanalysis of Metals and Alloys\",the quantitative results of Si content in some W600 silicon steel was measured hy EPMA-WDS.The uncertainty components which might affect the measurement results were considered,calculated and synthesized. Finally the uncertainty result for the quantitative value of Si content in the silicon steel was got.The mass content of Si was 1.50%,and expanded uncertainty U=0.20%under the condition of co...
本钢高硬度无取向电工钢50BW600的研发
目前随着电工钢用户冲压设备的升级,冲压速度逐步提高,对电工钢产品的硬度和强度指标提出了更高的要求。与普通硬度级别的无取向硅钢相比,高硬度50BW600的Hv硬度提高15~20,达到125以上,同时对电磁性能指标也有较高要求。本钢通过化学成份和热轧及冷轧连退生产工艺的设计,经过小批量生产试验,满足用户要求。通过对工艺的严格控制,在大批量生产过程中,保证了产品的力学性能和电磁性的检验合格率。 Currently with upgrading of stamping equipment of silicon steel user, gradually increasing of stamping speed, propose higher demand for hardness and strength of silicon steel. Compared with conventional 50BW600, high hardness 50BW600 have higher hardness, reach greater than 125Hv. Through design of chemical composition with hot mill and annealing, production test of small quantities, stamping performance meet user request.
修正GTN模型及其在预测硅钢冷轧边裂中的应用
考虑剪应变对微孔洞损伤演化的影响,对GTN损伤模型的损伤演化机制进行修正,建立了适用于不同应力三轴度水平的损伤模型。结合隐式应力更新算法和显式有限元计算,采用VUMAT子程序实现了修正GTN模型在有限元软件ABAQUS中的数值计算。通过模拟纯剪切和剪切-拉伸两组试样的损伤演化和断裂行为,验证了修正GTN模型在不同应力三轴度承载条件下的有效性。运用修正GTN损伤模型模拟含边部缺口的带钢在轧制过程中裂纹的萌生和扩展行为,模拟结果与实验相一致,表明该模型可有效地用于带钢缺陷在轧制过程中扩展行为的分析和预测。模拟和实验结果表明,带钢边部缺口在轧制过程中,缺口前沿和后沿均会萌生裂纹,且后沿裂纹扩展更为明显。 Considering the effect of shear strain of micro-void on damage evolution, a modified GTN model applicable to various stress triaxiality conditions is proposed by modifying the damage evolution mechanism of the GTN damage model. The modified model is implemented in commercial finite element software ABAQUS by combining the implicit stress update method with an explicit finite element solving algorithm and through the user-defined material subroutine VUMAT. The damage evolution and the failure pro...