试样剪切应力对冷轧无取向电工钢磁性能的影响
电工钢试样加工产生的剪切应力会恶化钢板的磁性,对不同牌号硅钢片的横向、纵向试样退火前后磁性能的变化进行研究,结果表明:无取向硅钢片在剪切过程中横向、纵向的磁性受到剪切应力影响是不一样的。 The electrical steel sample processing magnetic of electrical steel will worsen due to the shear stress of sample. In this paper,the magnetic change of transverse,longitudinal specimens of different type of silicon steel sheet before and after annealing are studied. The results show that the magnetic of non- oriented silicon steel sheet affected in the process of shear is not the same in horizontal and vertical direction.
冷轧工艺对取向硅钢初次再结晶织构的影响
研究了取向硅钢制备过程中常见的两种冷轧工艺,主要研究了一阶段冷轧与两阶段冷轧+中间退火工艺对初次再结晶组织及织构的影响.结果表明:采用两阶段冷轧+中间退火工艺制备以Cu2S为主抑制剂的取向硅钢,其初次再结晶平均晶粒尺寸为18.1μm,高斯晶粒的体积分数为0.6%,迁移性强的重位点阵晶界(Σ5+Σ9)和高能晶界(20°~45°取向偏差角)所占比例分别为1.8%和50.4%.与一阶段冷轧工艺相比,其初次再结晶晶粒较细,且高斯晶核与特征晶界所占的比例较高,有利于高斯晶粒发生二次再结晶. Two common cold-rolling processes of grain oriented silicon steel and the effects of the single stage cold rolling and tw o-stage cold rolling w ith intermediate annealing processes on the primary recrystallization microstructure and texture w ere investigated. The results revealed that for the grain oriented silicon steel prepared under the tw o-stage cold rolling process w ith intermediate annealing w ith Cu 2 S as the main inhibitor,the average grain size of the primary recrystallization micr...
无取向电工钢织构的演变及其沿带钢宽度方向上的差异
采用EBSD检测技术,分析了50W800无取向电工钢在重要生产工序间织构的演变以及织构沿带钢宽度方向上的差异性。结果表明:热轧板织构沿带钢宽度方向上的差异性主要体现在表层织构。带钢边部表层织构主要由旋转立方织构、α纤维织构以及少量的γ纤维织构组成,带钢宽度1/4处的表层织构主要存在高斯织构,带钢宽度1/2处的表层织构主要为(110)面织构以及少量的铜型织构。各处的带钢宽度1/4处和1/2处的织构类型基本一致,都以α纤维织构和旋转立方织构为主。冷轧后,各处的表层织构类型差异较小,均为γ纤维织构和α纤维织构。由板宽边部至中心处织构强度值逐渐降低。退火后,各处织构的组分基本一致,为较强的γ纤维织构和较弱的(100)面织构。各处织构强度值差异较小,变化趋势与冷轧板一致。 The texture of non-oriented electrical steel 50W800 was detected by EBSD technique.The evolution of the texture between important processes and the difference of texture along the width direction of strip were analyzed.The result shows that the difference along the width direction of strip of texture at the surface of hot rolled plate is most obvious.The texture at the surface of strip edge is primarily made of rotating cube texture,αfiber texture and weakγfiber texture.Goss texture is mainly co...
二次冷轧中间退火对基于CSP工艺的取向硅钢组织及织构的影响
在实验室模拟CSP工艺条件下制备了取向硅钢,研究了二次冷轧中间退火工艺对组织和织构的影响。结果表明,中间退火温度对取向硅钢脱碳,高温退火组织及织构均产生明显影响。经940℃中间退火后,取向硅钢脱碳再结晶晶粒较850℃中间退火的多,且再经高温退火处理后,晶粒粗化,最大晶粒尺寸达4.8 mm;高斯织构组分密度达27.00,较850℃中间退火试样高。 Grain-oriented silicon steel was prepared by simulated CSP technology in laboratory. Effects of secondary cold-rolled intermediate annealing on microstructure and texture were studied. The results show that intermediate annealing has obvious effects on the microstructure and texture of the steels after decarburization annealing and high temperature annealing. After intermediate annealing at 940 ℃,recrystallized grain of decarburization annealed steel is more than that of intermediate annealed at...
辉光放电发射光谱法测定硅钢薄板中微量硼元素
通过对辉光放电发射光谱参数的优化,以铁元素为内标来消除基体效应,建立了测定硅钢薄板中微量硼元素的方法。优化的实验参数为:放电电压1200 V,放电电流50 mA,预溅射时间40 s,积分时间10 s。校准曲线硼元素含量范围0.0001%~0.022%,相关系数大于0.999,测量结果与认定值一致,相对标准偏差小于10%。完全能够满足日常分析测试的要求。 A glow discharge optical emission spectrometry(GD-OES) method for determining trace boron element in silicon steel sheets were established through optimization of instrumental parameters and using Fe element as an internal standard to eliminate the matrix effect.The optimized instrumental parameters included discharge voltage,discharge current,pre-sputtering time and integration time,which are 1200 V,50 mA,40 s,and 10 s,respectively.The content of boron element that can be determined from the ca...
常化对含硅1.6%的无取向电工钢组织和织构的影响
研究了常化对CSP流程生产的wSi=1.6%的无取向电工钢组织、织构和成品磁性能的影响。结果表明,经CSP流程生产,且在相同的冷轧及退火制度下,经1 000℃×2min常化处理的wSi=1.6%的无取向电工钢热轧板,其最终退火成品的铁损P15/50比不常化试样下降了10.5%,磁感B50比不常化试样提高了2.5%;常化使wSi=1.6%的无取向电工钢成品的平均晶粒尺寸增大,成品铁损P15/50相应减小;同时,常化使wSi=1.6%的无取向电工钢成品中高斯织构的强度增加,γ纤维织构的强度减弱,这有利于成品磁感B50的提高。 The effect of normalizing on microstructure,texture and magnetic properties of non-oriented electrical steel with wSi=1.6% produced by CSP process was investigated.The results show that,under the same cold rolling and annealing system,the iron loss(P15/50) of annealed samples whose hot bands has been normalized by 1 000 ℃×2 min process decreases by 10.5% and magnetic induction(B50) increases by 2.5% compared with the samples whose hot bands was not normalized.The average grain size of non-orient...
常化冷却工艺对低温取向硅钢组织及析出相的影响(英文)
利用OM、TEM与EDS技术,对Fe-3.2%Si低温取向硅钢热轧板进行不同常化冷却工艺处理后的显微组织、析出相及最终产品的磁性能进行分析,并与热轧板的组织和析出相进行对比。结果表明,常化板较热轧板的表层组织均匀,基体中再结晶比例增加,带状组织变窄;常化板中析出物的数量明显比热轧板的多,析出物主要有AlN、MnS及复合析出的(Cu,Mn)S等。在常化温度1120℃、保温3 min的条件下,采用二段式冷却较空冷、淬沸水、淬常温水的冷却工艺,常化板表层显微组织更均匀,沿板厚方向的显微组织的不均匀性显著,取向硅钢的磁性能最高;常化后采用二段式冷却工艺析出的细小析出物数量最多,且弥散分布在基体中,抑制剂的抑制效果最好,对成品获得高磁性最有利。 Microstructure, precipitate and magnetic characteristic of final products with different normalizing cooling processes for Fe-3.2%Si low-temperature hot-rolled grain-oriented silicon steel were analyzed and compared with the hot-rolled plate by optical microscopy(OM), transmission electron microscopy(TEM), and energy dispersive spectrometry(EDS). The results show that, the surface microstructure is uniform, the proportion of recrystallization in matrix increases, and the banding textures are nar...
双辊连铸法制备硅钢薄带的组织和性能
采用双辊连铸工艺制备了硅的质量分数分别为0.5%,1.0%,3.0%,4.5%的硅钢薄带,用光学显微镜观察其组织,并研究了后处理工艺对薄带组织和性能的影响。结果表明:硅含量为0.5%和1.0%的薄带适合采用一次冷轧+850~950℃退火的后处理工艺,而硅含量在3.0%以上的薄带适合采用二次冷轧+950℃退火的后处理工艺;硅含量为3.0%和4.5%的薄带在冷轧并950℃退火后,其磁性能最佳,铁芯损耗约为4.30 W·kg-1,磁感应强度约为1.68T。 Silicon steel thin strips with silicon content of 0.5wt%,1.0wt%,3.0wt%and 4.5wt%were prepared by twin-roll continuous casting process,and the microstructure of the strips were observed by means of optical microscopy,and on the basis,the effect of post-treatment process on microstructure and properties of the strips was studied.The results show that the post-treatment process of one-time cold rolling and annealing between 850—950℃was suitable for the strips with silicon content of 0.5wt%and 1.0wt...
微量Sn对0.4%Si无取向硅钢组织和磁性能的影响
结合实际生产0.4%Si无取向硅钢,统计了不含Sn和0.025%Sn无取向硅钢的磁性能变化,利用金相显微镜、X射线衍射仪观察分析不同成分下试样的显微组织和微观织构。试验结果表明:Sn元素可以显著降低无取向硅钢的晶粒尺寸,0.025%Sn试样的平均晶粒尺寸比不含Sn减小28.4%;加入Sn元素后抑制了无取向硅钢中不利于磁性能的{111}面织构组分强度,提高了对磁性能有利的{100}面织构组分强度,0.025%Sn与不含Sn相比磁感均值从1.756 T提升至1.768 T,铁损均值从5.476 W/kg降低至5.204 W/kg,明显改善了无取向硅钢磁性能。 In this paper combined with the actual production of 0.4% Si non oriented silicon steel, the magnetic properties of non oriented silicon steel without Sn and 0.025% Sn were counted. The microstructure and microtexture of samples with different compositions were observed and analyzed by metallographic microscope and X-ray diffraction. The results show that: Sn can significantly reduce the grain size of non oriented silicon steel, and the average grain size of 0.025% Sn sample is 28.4% smaller tha...
冷轧取向硅钢工程混凝土结构裂缝控制施工技术
冷轧取向硅钢工程中有很多的超长、大体积以及薄壁的混凝土结构,裂缝控制是土建施工的关键。在工程中,按照\"抗放兼施、先放后抗、以抗为主\"的原则,采用\"无缝分块跳仓法\",防止超长混凝土结构收缩产生裂缝;在隧道和池体的底板与墙板施工中,采用\"整体浇筑\"法,避免了墙板因约束应力而产生的裂缝。 In the Cold-rolled grain-oriented silicon steel project,there are many overlength,bulk mass,thin-walled concretes structures,how to control the crack is the key of civil engineering construction.In these projects,according to the principle of\"release with resist,resist before release,resist is dominant \",the crack of the over-long structure and shrinkage can be prevented by the method of\"seamless block skip bin \".In the construction of the bottom plate and wall of the tunnel and the pool,the cra...