钢厂
冷轧电工钢森吉米尔轧机研究进展
森吉米尔二十辊轧机是冷轧电工钢的主要机型,具有整体刚度大,辊径小,轧制道次压下量大,产品精度高等特点,简要介绍了近年来冷轧电工钢森吉米尔二十辊轧机领域进展,在轧机结构、厚度自动控制、板形自动控制等方面的技术及研究。 20-h Sendzmir reversible mill is the main type of cold rolled electrical steel which has the characteristic of high integral stiffness,small roller diameter,high pass reduction and high product quality.In this paper,the recent progress of frame structure,automatic gauge control,automatic flatness control of Sendzmir mill is introduced.
修正GTN模型及其在预测硅钢冷轧边裂中的应用
考虑剪应变对微孔洞损伤演化的影响,对GTN损伤模型的损伤演化机制进行修正,建立了适用于不同应力三轴度水平的损伤模型。结合隐式应力更新算法和显式有限元计算,采用VUMAT子程序实现了修正GTN模型在有限元软件ABAQUS中的数值计算。通过模拟纯剪切和剪切-拉伸两组试样的损伤演化和断裂行为,验证了修正GTN模型在不同应力三轴度承载条件下的有效性。运用修正GTN损伤模型模拟含边部缺口的带钢在轧制过程中裂纹的萌生和扩展行为,模拟结果与实验相一致,表明该模型可有效地用于带钢缺陷在轧制过程中扩展行为的分析和预测。模拟和实验结果表明,带钢边部缺口在轧制过程中,缺口前沿和后沿均会萌生裂纹,且后沿裂纹扩展更为明显。 Considering the effect of shear strain of micro-void on damage evolution, a modified GTN model applicable to various stress triaxiality conditions is proposed by modifying the damage evolution mechanism of the GTN damage model. The modified model is implemented in commercial finite element software ABAQUS by combining the implicit stress update method with an explicit finite element solving algorithm and through the user-defined material subroutine VUMAT. The damage evolution and the failure pro...
电工钢铸锭内析出相粒子特征及回溶行为
利用场发射电镜及能谱仪研究了取向电工钢薄、厚板坯铸锭中不同区域的析出相差异,确定了MnS、AlN及Fe3C的析出顺序和形貌特征。结果表明AlN以先析出的MnS为形核核心,形成粗大微米级的复合析出相。针状Fe3C既可以在复合析出相表面形成也可以在基体中单独出现,主要受冷却速度的影响。在1250℃保温1~2 h,AlN、Fe3C均可完全回溶,但部分MnS仍不回溶。MnS尺寸随着保温时间延长而增大。导致热轧板中沿轧向分布的粗大MnS,减弱了粒子钉扎力。 Precipitates in thin and thick slabs of electrical silicon steel were investigated by means of field emission SEM and EDS analysis.The precipitation sequence and the morphology of MnS,AlN and Fe3C particles were identified.AlN particles are observed to be nucleated on surface of MnS forming micron-meter-sized complex particles.Acicular Fe3C can precipitate on surface of the complex MnS/AlN particles or directly from matrix depending on cooling rate of the slabs.After holding at 1250 ℃ for 1-2 h,...
冷轧压下量对取向硅钢极薄带显微组织的影响
观察了取向硅钢极薄带经冷轧至不同厚度,并经过不同工艺热处理后的显微组织及亚结构。结果表明:冷轧压下量越大,显微组织中位错密度越高,冷变形组织越多,等轴晶粒越少;增加冷轧压下量可以使试样的再结晶温度降低,当钢带厚度为0.08 mm时,在650℃退火时就能发生明显的再结晶。 Microstructure and substructure of the grain oriented ultra-thin silicon steel sheets is analyzed,which are rolled down to different thickness and treated with different heat treatment process.The result shows that there are higher dislocation density,more cold deformation structure and less equiaxed crystal grain in microstructure of the steel sheets with more cold rolled reduction.Increase of cold rolled reduction will decrease recrystallization temperature,and when thickness of the steel shee...
锡或锑在无取向电工钢中的研究进展
近年来,在节能减排背景之下,国内外众多研究者对无取向电工钢磁性能的提升做了大量研究。为了探索无取向电工钢磁性能提升的方法,对锡或锑对无取向电工钢磁性能的作用机制(晶粒尺寸和晶体织构的控制)进行分析。基于该作用机制,介绍锡或锑的添加对无取向电工钢磁性能的影响。经研究发现,适量的锡或锑在晶界偏聚,不会阻碍晶界的移动并且致使晶粒尺寸降低;与此同时,锡或锑在晶界偏聚不仅抑制{111}织构在原始晶界处形核及生长,还降低(100)晶粒表面能,促进(100)晶粒生长。因此,适量添加锡或锑,可使无取向电工钢铁损下降、磁感提升。最后结合生产工艺,建议无取向电工钢的研究方向应为稀土含量对高牌号无取向硅钢夹杂物尺寸和数量分布的影响,锡或锑的添加量和常化工艺参数(常化时间、常化温度)对常化晶粒尺寸的影响。 In recent years, due to the background of energy saving and emission reduction, numerous researchers all around the world have done a lot of investigations on the improvement of magnetic properties for non-oriented electrical steel. In order to explore the method of improving the magnetic properties of non-oriented electrical steel, the mechanism of tin or antimony on the magnetic properties(the control of grain size and crystallographic texture) of non-oriented electrical steel is illuminated. ...
硅钢轧制过程中乳化液流量数学模型研究及应用
目前高磁感冷轧硅钢生产过程中,采用经验方法确定的乳化液流量设定值往往会造成硅钢产品的磁感性能达不到预期目标,针对此情况,基于轧机轧制机理研究了的乳化液流量数学模型,确定了乳化液流量设定值。实践表明,使用该数学模型输出的乳化液流量设定值,可提高轧制过程中乳化液流量控制精度,从而提高高磁感冷轧硅钢的轧制性能。 In view of the current production process of high magnetically inductive cold-rolled silicon steel, the mathematical model of emulsified fluid flow based on mill rolling mechanism is studied in view of the situation in which the magnetic sensing performance of silicon steel products is often not up to the expected target by using empirical method to determine the emulsified liquid flow setting. Practice shows that the emulsified fluid flow setting value output from this mathematical model improv...
硅钢脱硫影响因素分析研究
对RH法(真空循环脱气法)生产的冷轧硅钢的脱硫原理及影响因素进行了分析研究。研究表明:降低顶渣中FeO、MnO的含量,提高钢液温度,增加脱硫剂的加入量并延长其循环时间有利于提高脱硫效率。 The principles of desulfurization and its influence factors of cold rolling silicon steel during RH process have been studied in this paper.The result indicated that reducing contents of FeO and MnO,rising temperature of the liquid steel,increasing quantity of desulfurizer,lengthening cycle time of desulfurzer are benefit for desulfurization.
Al含量对2.2%Si无取向硅钢组织、织构和磁性能的影响
通过实验室25 kg真空感应炉冶炼和锻轧研究了0.26%~0.95%Al含量对0.5 mm 2.2%Si无取向硅钢冷轧板组织、织构和磁性能的影响。试验结果表明,0.26%~0.81%Al含量时,随钢中Al含量的增加,成品退火钢板的晶粒尺寸增加同时铁损减少;当Al含量大于0.81%时,随Al含量增加,钢板的晶粒尺寸减小,同时铁损增加。Al含量对硅钢板磁感的影响没有明显的规律。2.2%Si无取向硅钢的合适Al含量为0.48%~0.81%。 The effect of 0.26%~0.95%Al content on structure,texture and magnetic performance of 0.5 mm cold rolled sheet of 2.2%Si non-oriented silicon steel has been studied by a 25 kg vacuum induction furnace smelting,and forging -rolling in laboratory.Results show that as 0.26%~0.81%Al,with increasing Al content in steel the grain size of annealed finished sheet increases while iron loss of sheet decreases,and as Al content in steel is more than 0.81%,the grain size of sheet decreases while iron loss in...
热轧工艺对TSCR流程生产取向硅钢组织和性能的影响
取向硅钢热轧板中组织、织构梯度对发展完善的二次再结晶十分关键,通过对2种不同热轧工艺生产取向硅钢的组织、织构进行研究,结果表明:采用后道次大压下热轧工艺时热轧板表层再结区晶粒平均尺寸增加,再结晶区厚度增加,高温退火后二次晶粒尺寸减小;采用后道次大压下热轧工艺热轧时,热轧板中平均等效应变高,热轧板厚度心部{100}〈011〉和{100}〈001〉位向取向强度降低,({111}~{113})〈110〉位向取向强度提高,高温退火后{110}〈001〉位向偏离角降低,磁性能提高。 The texture and microstructure gradient in hot rolled grain oriented silicon steel strip was one of the essential factors to achieve a perfect secondary recrystallization.The texture and microstructure of grain oriented silicon steel strip as-rolled with two different hot rolling parameters was investigated.The results show that with big reduction at the end rolling process,the intensity of {100}〈011〉 and {100}〈001〉 orientation reduces with({111}-{113})〈110〉 orientation intensity enhanced in hot...
多元抑制剂对高磁感取向硅钢性能的影响
介绍在取向硅钢生产中抑制剂的作用以及多元抑制剂的机理和应用情况,分析多元抑制剂方案中各种元素对高磁感取向硅钢性能的影响,并根据生产实践提出了进一步研究的方向. The role of an inhibitor in the production of grain oriented silicon steel,and the mechanism of multiplex inhibitor in the production are described in the present article.In addition,the influence of various elements in the multiplex inhibitor on the performance of grain oriented silicon steel with high magnetic induction is elucidated.Further work needed in this research is also indicated.
取向硅钢常化水冷温度模型及控制方法研究
取向硅钢常化工序主要采用现场实测带钢温度的方式测定冷却速率,并通过稳定冷却水温、调整冷却水量及喷梁运行数量等方式保证合理的冷却速率,给常化工艺设计和生产带来诸多不便。通过对常化工艺水冷过程带钢的传热分析求解,在建立带钢水冷温度模型的基础上,研究了不同冷却工艺参数对带钢温度及冷却速率的影响规律以及冷却工艺的交互作用结果。结果表明:模型计算结果能够较好地反映取向硅钢在常化水冷过程中的温度及冷却速率的变化,其计算误差为0.80%~4.11%;在特定取向硅钢厚度规格和常化工艺下,随着常化冷却水量及有效冷却长度的增加,带钢水冷温度及冷却速率与呈非线性变化;常化水冷工艺主要通过调控带钢与冷却水之间热交换量和交换时间实现对带钢温度的控制,实际生产中需综合考虑机组速度、冷却水量及有效冷却长度之间的交互作用,选定喷梁投入数量和冷却水量以获得稳定的冷却速率。 The cooling rate of normalization process mainly determined by measuring the grain oriented silicon steel strip temperature on site, and ensures the cooling rate by stabilizing the cooling water temperature, adjusting the cooling water volume and the operation quantity of spray beam, which brings inconvenience to the normalization process design and production. Based on the heat transfer of strip in the water cooling section of normalization process, the water cooling temperature model for the n...