电工钢检测方法及标准综述
综述了电工钢从生产到成品过程中涉及到的检测项目、检测方法及仪器,并通过对电工钢标准的发展改进,详细阐述了我国现有的电工钢技术标准体系,同时对代表企业的电工钢重点指标进行了摘录对比,为综合应用电工钢检测方法并促进电工钢的发展提供了一定的参考。 This article summarizes the testing items,methods,and instruments involved in the process from manufacturing to finished products of electric steel. The current electric steel technical standards system in our country is also elaborated in detail,along with the development and improvement of electric steel standards. Meanwhile,by comparison of electric steel KPI in representitive companies,this article provides references for comprehensive application of electric steels testing methods and promo...
脱碳温度和脱碳时间对CGO取向硅钢碳含量控制的试验研究
通过测试取向硅钢不同工艺条件下的碳含量,探讨了CGO取向硅钢碳含量控制的最优处理条件,研究了脱碳温度和脱碳时间对相同初始碳含量取向硅钢的脱碳效果的影响。结果表明,在气氛为(15%~20%)H2+(75%~80%)N2,炉压差为10~20 Pa的条件下,CGO取向硅钢合适的脱碳温度为1 073 K~1 123 K,脱碳时间为10~20 min。在该处理条件下,能取得较好的脱碳效果。 By means of testing carbon content of oriented silicon steel below the distinct technical conditions,inquires the excellent handle terms of carbon content controlling for CGO oriented silicon steel,studies effects of decarburization annealing temperature and decarburization annealing time to the oriented silicon steel decarburization efficiency in same initial carbon content.The results show that,under the condition of atmosphere(15% ~ 20%) H2+(75% ~ 80%)N2 and furnace pressure difference 10 ~ 2...
退火工艺对3.15%Si冷轧无取向硅钢组织和织构的影响
试验研究了退火温度(850~950℃)和时间(5~18 min)对2.3 mm热轧硅钢板(/%:0.036C,3.15Si,0.21Mn,0.005P,0.007S,0.032A1)6道次轧制的0.35 mm冷轧板组织和织构的影响。结果表明,退火温度越高,晶粒平均尺寸越大,900℃5 min退火时平均晶粒尺寸41.39μm,试样织构主要集中在γ取向线上的{111}<112>织构组分和{111}<110>织构组分;900℃18 min退火时平均晶粒尺寸为48.08μm,试样的{111}面织构和{112}面织构密度都明显减弱,{001}面织构增强,磁性能较优。 The effect of annealing temperature(850 ~950 ℃) and holding time(5 ~ 18 min) on structure and texture of 0.35 mm sheet by 6 passes cold-rolling from 2.3 mm hot-rolled plate of silicon steel(/%:0.036 C,3.15 Si,0.21 Mn,0.005 P,0.007 S,0.032A1) has been tested and studied.Results show that the higher the annealing temperature the coarser the average grain size;As annealing at 900 ℃ for 5 min the average grain size of steel sheet is 41.39 μm,and the texture in sample is mainly concentrated in y orie...
锰含量对无取向电工钢组织性能的影响
研究了锰含量对w(Si)=1.8%Si无取向电工钢组织和性能的影响。结果表明,钢中锰含量从0.3%增加到1.2%时,由于α_γ相变的产生,铸坯低倍组织、热轧板金相组织及成品织构等均发生了不同程度的变化,对成品表面质量及磁性能产生了明显的影响。 The effects of manganese content on structure and properties of w(Si)=1.8% non-oriented electrical steels have been studied.Results show that with increasing manganese content to 1.2% from 0.3%,macrostructure of continuous casting slab,hot rolled band metallurgical structure and finished product texture vary in some extent because of the occurrence of α-γ phase transformation,the surface quality and magnetic properties of finished product are affected greatly.
钙处理对无取向硅钢中非金属夹杂物的影响
采用电解法和扫描电镜研究了300 t转炉-RH精炼钙处理对无取向硅钢板(%:≤0.005C、1.2~2.2Si、0.2~0.6Mn、≤0.20P、≤0.005S、0.2~0.6Al、0~0.01Ca)中夹杂物的影响。结果表明,钢中Al含量为0.25%和0.35%时,钢中溶解氧均小于1×10-4%,钙处理后都会产生CaS夹杂物,尤其是含0.35%Al的钢水;钙处理可以有效减少钢中的夹杂物数量,尤其是0.5μm以下的微细夹杂物数量;钙处理后夹杂物的种类以AlN、CaS为主,同时还含有少量的氧化物夹杂物以及AlN-CaS复合夹杂物,尺寸主要为1.5~5.0μm。 The effect of 300 t converter-RH refining calcium treatment on inclusions in non-oriented silicon steel sheet (%:≤0.005C,1.2~2.2Si,0.2~0.6Mn,≤0.20P,≤0.005S,0.2~0.6A1,0~0.01Ca) has been studied by electrolysis and scanning electron microscope.Results show that with 0.25%and 0.35%Al content in steel,all the dissolved oxygen in liquid is less than 1×10-4%,and the CaS inclusions are produced after calcium treatment,especial for the liquid containing 0.35%Al;the amount of inclusions in ste...
晶粒尺寸对无取向硅钢磁性能影响的主成分回归分析
采用电子背散射衍射技术测定50SW1300冷轧无取向硅钢中不同尺寸范围晶粒的含量,利用主成分回归分析法,综合研究不同尺寸范围晶粒的含量对无取向硅钢磁性能的影响。结果表明:通过主成分回归分析法能够从不同尺寸范围晶粒的含量的多个影响因素中获取主要的因素,定量研究它们对无取向硅钢磁性能的影响规律。分析表明,无取向硅钢的铁损与不同尺寸范围晶粒的含量之间存在着可靠的多元线性关系,在一定范围内,较大尺寸晶粒的含量越多,其对铁损优化的作用越明显;而无取向硅钢的磁感与不同尺寸范围晶粒的含量之间并无线性关系。 Distribution of grain size in cold rolled non-oriented silicon steel 50SW1300 was measured by EBSD.The effects of the distribution of grain size on magnetic properties of the non-oriented silicon steel were comprehensively researched by means of principal component regression method.The results indicate that the main factors influencing the magnetic properties in the distribution of grain sizes,which can be used to guantitative study the magnetlic properies of the steel,are obtained by principal...
冷轧产线硅钢激光高速切边实验研究
为了解决目前冷轧产线硅钢现有切边技术存在的微裂纹、应力、毛刺和边浪等问题,采用光纤激光器进行了高速切割实验,对激光功率、切割速度、激光模式等影响因素进行了分析,同时对高速切割时的切割前沿形状进行了研究。结果表明,切割最高速度随着功率的增加而增加;随着离焦量的增加,切割质量下降,挂渣增多,切缝宽度增加,切割深度变浅;基模激光器能量密度更高,所以薄板切割时的切割速度高于多模激光器;切割前沿随着切割速度的增加会变得平缓,速度足够大时,切割前沿甚至接近与切割方向平行,此时切缝下部存在挂渣现象。 In order to solve the problems such as micro crack,stress,burr,edge waves and so on,existing in cold rolling production line of silicon steel side cutting,experimentsof high speed laser cutting using fiber laser were carried out.Laser power,cutting speed,laser mode and other factors were analyzed,at the same time,cutting front geometries were studied.The results show that the maximum speed increases with power.And the increases of defocus result in poor quality,wider kerf and shallowerkerf.Energ...
正火对双辊薄带连铸5.28%Si-1.11%Al无取向高硅钢磁性能的影响
采用双辊薄带连铸工艺试制了2.6 mm厚5.28%Si-1.11%Al高硅钢薄带,对比了1050℃×5 min正火及不正火铸带280℃冷轧至0.5 mm后,再经900~1100℃退火的磁性能。结果表明,高硅钢铸带显微组织为等轴晶组织,正火后铸带边部晶粒长大,中心层晶粒变化较小。成品中析出物主要为较粗大的AlN和AlN+MnS复合析出物,尺寸为0.5~2.5μm。与不正火试样相比,正火试样成品铁损大幅降低,磁感小幅下降;随退火温度的升高,两种工艺下铁损和磁感都是先降低后升高,在1050℃出现最低值。 2.6 mm thickness 5.28% Si-1.11% Al non-oriented high silicon steel was produced by twin roll thin strip casting.Magnetic property of the strip un-normalized and normalized at 1050 ℃×5 min was contrasted after cold rolled to 0.5 mm at 280 ℃ and 900-1100 ℃ final annealing.The results show that microstructure of the strip is equiaxed crystal.The surface grain is coarsened and the center layer grain has little change of the normalized strip.The main precipitates are AlN and MnS+AlN with 0.5-2.5 μm s...
纳米TiO_2轧制液对硅钢冷轧性能的影响
分别采用传统冷轧轧制液和纳米TiO2的冷轧轧制液,对无取向硅钢板进行了四辊冷轧实验.重点研究两种冷轧轧制液的轧制润滑性能和对轧后硅钢薄带表面质量和耐蚀性能的影响.通过场发射电子显微镜和能谱仪对使用两种轧制液轧后得到的硅钢薄带表面形貌和成分进行了分析.给出了轧制液中TiO2纳米粒子在轧制过程中的抗磨减摩机理.在轧制载荷较高时,纳米TiO2轧制液具有优良的轧制润滑性能并能显著改善轧后硅钢薄带的表面质量.同时在高载荷作用下,TiO2纳米粒子被压入硅钢薄带基体,形成一个滑动系来支撑载荷,从而使润滑膜的耐磨性提高. Non-oriented silicon steel strips were rolled on a four-high cold rolling mill lubricated by a traditional cold rolling liquid and a nano-TiO2 cold rolling liquid,with emphasis on studying the rolling lubrication performance of both the liquids and their effect on the surface quality and corrosion resisting property of the silicon steel strips.The surface micrograph and composition of the silicon steel strips after being rolled with both the liquids were characterized by field emissio...
TSCR试制高强度无取向电工钢
采用固溶强化、细晶强化和位错强化方法,模拟TSCR流程试开发高强度无取向电工钢,试开发钢的主要合金成分为3%Si、0.83%Al和2.99%Mn。分析热轧、常化、退火后的钢板组织,并针对不同的成品板组织,详尽地分析了相应的力学性能和磁性能。试验电工钢平均晶粒直径为12.37μm时,R p0.2为530 MPa,R m为618 MPa;当退火制度为700℃×4 min,成品组织完全为未再结晶的回复组织时,R p0.2为853.5 MPa,R m为895.5 MPa。该成分的电工钢P15/50或P10/400最小时,对应的平均晶粒直径都大于59.67μm;P10/800或P10/1000最小时,对应的平均晶粒直径都处于12.37~59.67μm尺寸区间。 TSCR was simulated to develop high-strength non-oriented electrical steel with 3% of Si,0.83% of Al and 2.99% of Mn by solution strengthening,grain refinement strengthening and dislocation strengthening.The microstructures of hot rolled plates,normalized plates and annealed plates were analyzed.Furthermore,the mechanical properties and magnetic properties of products with different microstructures were detailedly studied.As the average grain diameter of the steel was 12.37 μm,the yield strength ...
硅钢脱硫影响因素分析研究
对RH法(真空循环脱气法)生产的冷轧硅钢的脱硫原理及影响因素进行了分析研究。研究表明:降低顶渣中FeO、MnO的含量,提高钢液温度,增加脱硫剂的加入量并延长其循环时间有利于提高脱硫效率。 The principles of desulfurization and its influence factors of cold rolling silicon steel during RH process have been studied in this paper.The result indicated that reducing contents of FeO and MnO,rising temperature of the liquid steel,increasing quantity of desulfurizer,lengthening cycle time of desulfurzer are benefit for desulfurization.