为了确定普通冷轧取向硅钢最优的中间完全脱碳退火工艺,在其一次冷轧后进行5种不同工艺的脱碳退火处理,借助扫描电镜及电子背散射衍射技术研究了不同工艺脱碳退火后的组织、织构和脱碳效果。结果表明:经5种工艺脱碳退火处理后,初次再结晶的平均晶粒尺寸均约为19μm,且不随退火温度和时间的变化而变化;经840℃×10min工艺退火后的晶粒最均匀,高斯织构位向更准确,高斯织构面积分数最多,为3.1%,可将碳脱至0.003 5%。 In order to determine the optimal intermediate complete decarburizing annealing processes for common grain-oriented(CGO)silicon steel,five kinds of intermediate decarburizing annealing processes were conducted,the microstructure,texture and decarbonization after different decarburizing annealing processes were studied by scanning electron microscopy and electro back-scattered diffraction(EBSD)technology.The results show that the average grains sizes of primary recrystallization were about 19μm a... 
2013-11-28 221 5.8

研究了铝和铬元素在无取向电工钢晶粒长大过程中对织构及晶界变化的影响规律。试验结果表明:电工钢在晶粒长大过程中的主要织构组分均为{111}<112>。在晶粒生长期间,不加铝的1号试样中,{111}<112>、{111}<110>织构组分强化,而{100}<001>织构组分弱化;与1号试样相比,在加入0.2%的铝(质量分数,下同)的2号试样中,{111}<112>、{111}<110>织构组分强化(增加)的速率下降,{100}<001>织构组分变化不明显,甚至稍有增加。在含铝的试样中再加入0.3 5%的铬之后(3号试样),{111}<112>{、111}<110>和{100}<001>织构组分的变化规律与1号试样相似,但当电工钢中加入0.72%的铬之后(4号试样),上述3种织构组分的变化规律与2号试样相似。对于在晶粒生长期间持续变化的3种织构组分而言,1号试样的{1 1 1}<112>和{111}<110>织构组分的高(低)取向差角度晶界频率下降(... The effect rule of Aluminm and Chromium on texture and grain boundary transformation in the nonoriented electrical steel during grain growth was investigated.The experimental result shows that the main texture component is {111}<112> in the electrical steel.The {111}<112> and {111}<110> components in specimen 1 without Alumium were strengthened during grain growth whereas {100}<001> component was weakened.But the growth rate of {111}<112> and {111}<110> compon... 
2011-06-28 461 5.8

承钢采用铁水预处理(脱硫)→转炉提钒→转炉冶炼→RH精炼→连铸→轧制工艺,成功研发了无取向电工钢CGW800。试制的CGW800钢碳含量≤0.006 0%、氮含量<0.004 0%,热轧后的金相组织为铁素体和少量渗碳体,晶粒度5.5级,获得了较粗大、均匀的晶粒,钢板的成分和力学性能达到了标准要求。 In Cheng Steel,the CGW800 non- oriented electrical steel is successfully developed with process of hot metal pre- treating,vanadium extracting with converter,smelting with converter,RH refining,continuous casting and rolling. In the steel,the carbon content is not higher than 0. 006 0%,nitrogen less than0. 004 0%,the metallographic structure after hot rolling is ferrite and a little amount of cementite,grain size is 5. 5 degree,relative large and even grain got. The composition and mechanical pr... 
2014-08-28 334 5.8

【摘要】 <正>目前,日本进口硅钢猛增,6月份4181吨,...
2011-05-28 716 5.8

为了优化激光刻痕降低取向硅钢铁损的工艺,寻找刻痕速度、脉冲能量、扫描间距等重要刻痕参数的最佳匹配关系,提出了一种基于人工神经网络与遗传算法的优化模型,并利用这种模型对30Q130取向硅钢材料的刻痕工艺进行了优化实验,结果表明,这种模型稳定可靠,可以作为取向硅钢刻痕工艺优化的一种有效的措施。 A laser is often considered to scribe the grain-oriented silicon steel surfaces after cold-rolling and annealing to reduce the core loss.It is necessary to select the best scribing parameters to maximize the reduction in this process.This paper proposes an optimization method of genetic algorithm during laser scribing of 30Q130 steel,by developing an artificial neural network prediction model using a database form a designed orthogonal experiment.The objective is to determine the best combinatio... 
2011-08-28 346 5.8

提出以“云边一体化架构”构建硅钢智慧决策系统,来解决原硅钢制造L1~L5系统架构模式下的数字信息孤岛、业务功能割裂等问题。在此基础上,开发了云边协同的自学习型控制模型及业务决策模型,构建起硅钢“智慧大脑”,形成了以研发、制造、服务等核心业务数字化融合的智能化决策支持新模式,探索出一条钢铁制造业数字化、智能化转型之路。 SIDS(Silicon-steel Intelligent Decision-making System)based on \"cloud-edge integration architecture\" was proposed to solve the problems of data silos and business function fragmentation in the original L1~L5 system architecture.On this basis,the self-learning control model and decision-making model of cloud-edge collaboration were developed,the \"smart brain\" of silicon steel department was constructed,and a new intelligent decision-making support model of digital integration of core businesses s... 
2022-02-28 243 5.8

采用化学气相沉积(CVD)渗硅处理工艺连续制备6.5%Si高硅钢,具有优质的软磁性能,通过理论研究化学反应并且用简单的试验设备做进一步的探讨。根据试验的结果对连续制备6.5%Si高硅钢的CVD工艺构造提出全面、有效的建议,实现制备6.5%Si高硅钢系统。 CVD method for continuously manufacturing 6.5%Si Steel Sheet has excellent soft magnetic.Carried out a theoretical study of related chemical reaction and performing basic research with a simple test apparatus.Based on the results,finally proposed an overall process configuration to realize such a production-CVD method for continuously manufacturing 6.5%Si Steel Sheet. 
2011-12-28 529 5.8

含铜抑制剂作为取向硅钢的主抑制剂或辅助抑制剂不仅可以抑制初次晶粒的长大,促进二次再结晶,还可以降低铸坯的加热温度。取向硅钢中主要抑制剂为10~50 nm Cu2S,在钢的铸坯、热轧、冷轧、脱碳等工艺过程均可析出;(Cu,Mn)1.8S、Cu1.8S、ε-Cu等主要作为辅助抑制剂,尺寸一般为30~50 nm(或大于50 nm),主要在热轧阶段析出。总结了国内外有关取向硅钢中含铜抑制剂析出行为的研究进展,当前主要研究不同生产流程和工序中含铜抑制剂的析出行为和作用机理。 As main inhibitor or auxiliary inhibitor for grain-oriented silicon steel,the particles of inhibitor bearing copper not only inhibit the primary crystal growing and promote the secondary recrystallization,but also decrease the heat temperature of casting slab.The main inhibitor for grain-oriented silicon steel is 10~50 nm Cu2S,which precipitate in process and procedure including steel casting slab,hot rolling,cold rolling and decarburizing process,while the 30~50 nm or more than 50 nm... 
2013-03-28 333 5.8

研究了常化对CSP流程生产的wSi=1.6%的无取向电工钢组织、织构和成品磁性能的影响。结果表明,经CSP流程生产,且在相同的冷轧及退火制度下,经1 000℃×2min常化处理的wSi=1.6%的无取向电工钢热轧板,其最终退火成品的铁损P15/50比不常化试样下降了10.5%,磁感B50比不常化试样提高了2.5%;常化使wSi=1.6%的无取向电工钢成品的平均晶粒尺寸增大,成品铁损P15/50相应减小;同时,常化使wSi=1.6%的无取向电工钢成品中高斯织构的强度增加,γ纤维织构的强度减弱,这有利于成品磁感B50的提高。 The effect of normalizing on microstructure,texture and magnetic properties of non-oriented electrical steel with wSi=1.6% produced by CSP process was investigated.The results show that,under the same cold rolling and annealing system,the iron loss(P15/50) of annealed samples whose hot bands has been normalized by 1 000 ℃×2 min process decreases by 10.5% and magnetic induction(B50) increases by 2.5% compared with the samples whose hot bands was not normalized.The average grain size of non-orient... 
2012-11-28 225 5.8

运用电子背散射衍射(EBSD)技术,研究了50W600无取向硅钢在热轧→冷轧→退火工序间织构的演变。结果表明:由于热轧板沿板厚方向的应力场和温度场存在差异,导致热轧板不同层织构类型和强度存在差异;热轧板表层主要存在铜型、黄铜和高斯织构,1/4层织构主要为α纤维织构和较弱的高斯织构,中心层织构较单一,主要为α纤维织构;和热轧板相比,冷轧板各层织构差异较小,为典型的轧制织构(α纤维织构和γ纤维织构);退火板各层都表现为γ纤维织构增强、α纤维织构减弱,旋转立方织构基本消失。 The texture evolution of 50W600non-oriented silicon steel in hot rolling,cold rolling and annealing process was investigated by electron back-scatter diffraction(EBSD)technology.Results show that the hot rolled plate texture types and intensities along thickness direction were different because of the different stress fields and temperature fields.The major texture types in the surface of hot rolled plate were copper,brass and Gauss texture.The texture was composed ofαfibre texture and weaker Ga... 
2014-08-28 221 5.8

【作者】 李波; 杨晓江; ...
2014-03-28 157 5.8

目前随着电工钢用户冲压设备的升级,冲压速度逐步提高,对电工钢产品的硬度和强度指标提出了更高的要求。与普通硬度级别的无取向硅钢相比,高硬度50BW600的Hv硬度提高15~20,达到125以上,同时对电磁性能指标也有较高要求。本钢通过化学成份和热轧及冷轧连退生产工艺的设计,经过小批量生产试验,满足用户要求。通过对工艺的严格控制,在大批量生产过程中,保证了产品的力学性能和电磁性的检验合格率。 Currently with upgrading of stamping equipment of silicon steel user, gradually increasing of stamping speed, propose higher demand for hardness and strength of silicon steel. Compared with conventional 50BW600, high hardness 50BW600 have higher hardness, reach greater than 125Hv. Through design of chemical composition with hot mill and annealing, production test of small quantities, stamping performance meet user request. 