冷轧无取向硅钢是高技术含量、高附加值产品,工艺复杂,生产周期长,过程控制难度大,被誉为钢铁产品中的\"工艺品\"。热轧生产工艺又是无取向硅钢生产的重中之重,直接决定了硅钢的铁损和电磁性等多项指标。 Cold rolled non-oriented silicon steel is high technology content 、high added value product. Its process is complex, its production cycle is of length, and its process control is difficult, which is known as the iron and steel products \" Arts and crafts\". Hot rolling production process is the top priority of non-oriented silicon steel, which directly determines iron loss of the silicon steel and electromagnetic property,as well as other many index. 
2014-02-28 519 5.8

取向硅钢利用析出物作为抑制剂,抑制初次再结晶晶粒的长大,抑制剂是取向硅钢发生二次再结晶的基本条件之一。文中通过低温板坯加热技术制备取向硅钢,采用透射电镜(TEM)观察并研究了高温退火阶段抑制剂的演化过程。结果表明,渗氮后形成的非晶态Si3N4析出物不稳定,在700~750℃退火升温阶段转化为(Al,Si)N;(Al,Si)N颗粒在800℃发生团聚,随后长大并粗化;(Al,Si)N是低温取向硅钢主要抑制剂,随退火温度的升高,(Al,Si)N抑制力大幅下降。 Precipitates as inhibitor are used to inhibit the grain growth of primary recrystallization in grain-oriented silicon steel,and inhibitor is one of the basic conditions for occurring of secondary recrystallization.The grain-oriented silicon steel was produced by low temperature slab heating and nitriding technique.The evolution of inhibitor was observed by transmission electron microscopy.The results show that Si3N4 particles are precipitated after nitriding,and Si3N4 particles are amorphous and... 
2011-11-28 590 5.8

综述了退火温度、时间对无取向电工钢磁性的影响。退火温度主要影响无取向电工钢不同织构的占有率,退火时间主要影响晶粒尺寸的大小,晶粒尺寸的变化对织构的形成也有一定的影响。磁感最高点出现在纤维组织完全消失,(111)面织构组分较弱的组织状态。铁损的降低主要依赖于磁滞损耗的降低,织构的影响不大。 The effects of annealing temperature and time on the non-oriented electrical steel magnetic properties were reviewed.Annealing temperature and time mainly affects the different textures share and the grain sizes of non-oriented electrical steel respectively.Changes of the grain sizes also have a certain effect on textures formation.The highest point of the magnetic induction value in the fibrous tissue completely disappears and{111} plane texture has a lower state of the component content.Iron l... 
2013-10-28 204 5.8

采用火花源原子发射光谱分析测定电工钢中超低C,研究试样制备方法、Ar纯度和压力等条件对分析结果的影响,并对工作曲线进行了优化,实现了一次分析同时测定电工钢的多种元素,满足炉前和精炼在线分析的要求。 Ultra-low carbon in electrical steel is determined with spark-source atom emission spectrum.It is researched the influence of sample making method,purity of Ar,and pressure on analysis result.The work curve is optimized.The determination of many elements in electrical steel only in one analysis is realized.It meets demands of on-line analysis for blast furnace and refining. 
2011-09-28 363 5.8

为了解决目前冷轧产线硅钢现有切边技术存在的微裂纹、应力、毛刺和边浪等问题,采用光纤激光器进行了高速切割实验,对激光功率、切割速度、激光模式等影响因素进行了分析,同时对高速切割时的切割前沿形状进行了研究。结果表明,切割最高速度随着功率的增加而增加;随着离焦量的增加,切割质量下降,挂渣增多,切缝宽度增加,切割深度变浅;基模激光器能量密度更高,所以薄板切割时的切割速度高于多模激光器;切割前沿随着切割速度的增加会变得平缓,速度足够大时,切割前沿甚至接近与切割方向平行,此时切缝下部存在挂渣现象。 In order to solve the problems such as micro crack,stress,burr,edge waves and so on,existing in cold rolling production line of silicon steel side cutting,experimentsof high speed laser cutting using fiber laser were carried out.Laser power,cutting speed,laser mode and other factors were analyzed,at the same time,cutting front geometries were studied.The results show that the maximum speed increases with power.And the increases of defocus result in poor quality,wider kerf and shallowerkerf.Energ... 
2013-04-28 332 5.8

【机构】 商务部进出口公平贸易局; ...
2013-02-28 491 5.8

【作者】 朱传芳; 潘恒韬; ...
2023-05-12 349 5.8

采用节能、环保、经济型的生产技术与工艺来制造高磁感取向硅钢目前已成为世界各大取向硅钢生产厂的研发热点。总结了国内外各大钢铁企业与研究机构采用低温板坯加热技术生产高磁感取向硅钢的开发及应用情况,概括了传统流程实现低温板坯加热技术的方法。介绍了薄板坯连铸连轧与双辊薄带连铸等短流程工艺生产高磁感取向硅钢的研发现状。在此基础上,探讨了高磁感取向硅钢生产技术与工艺的发展趋势及方向。 Utilizing energy-efficient,environmentally friendly,economic production processes and technologies to manufacture high magnetic induction grain-oriented silicon steel has become the focus of current research work.Based on using low-temperature slab reheating techniques to produce high magnetic induction grain-oriented silicon steel at both iron and steel enterprises and research institutions all over the world,the current application and exploitation was thoroughly generalized;the implementation... 
2013-03-28 310 5.8

研究了热处理工艺(退火温度、保温时间、冷却方式)对含Mn的Fe-6.5wt%Si高硅钢热轧带的显微组织及硬度的影响。结果表明,退火温度对Fe-6.5wt%Si合金的组织和显微硬度均有较大影响,随退火温度升高,平均晶粒尺寸和显微硬度均明显增大。小于1 h退火时,晶粒长大缓慢,而长时间(>1 h)退火时,一些次表层晶粒将发生异常长大。水冷组织比空冷组织略细小,但水冷显著降低了显微硬度。Mn含量提高能抑制850℃退火时晶粒的长大,并且促进退火后高硅钢的软化。 The influences of heat treatment process(annealing temperature,heating time,cooling methods) on the microstructure and microhardness of Fe-6.5wt%Si high silicon steel containing manganese for hot rolled strip were studied.The results show that the annealing temperature has a great effect on the microstructure and microhardness of Fe-6.5wt%Si alloy,and as the annealing temperature increases,the average grain sizes and microhardness will significantly increase.When annealing time for less than 1 h... 
2023-05-12 1.49k 5.8

【摘要】 <正>近日,从重钢集团获悉,日前重钢炼钢厂...
2013-01-28 410 5.8

借助OM、激光共聚焦显微镜、质谱仪和电解萃取等设备和方法,研究了添加微量稀土La(质量分数0.001 1%)的取向硅钢在轧制前采用不同加热保温时间对抑制剂固溶行为的影响。结果表明:当稀土取向硅钢在1 250℃分别保温10、20、30 min后,试验钢晶粒尺寸随保温时间延长有先快后慢的长大趋势;三种抑制剂元素Mn、Cu和Al均发生固溶,保温时间对Mn和Cu两种元素的固溶影响明显,固溶量分别由69.8%和43.7%增加至84.2%和85.2%;随着保温时间的延长,稀土取向硅钢中抑制剂的小尺寸未溶物逐渐减少直至消失,较大尺寸未溶物(300~600 nm)逐渐转变为小尺寸未溶物逐步溶入基体中,数量减少且未溶物的类型由复杂逐渐转变为单一。 In this paper the solid solution behavior of the inhibitor under various holding time in 0.001 1 %La oriented silicon steel during reheating had been investigated by using OM, LM, methods of electrolytic extraction and mass spectrometer. The results showed that grain size of the test steel increased significantly with the holding time prolonging when the rare earth oriented silicon steel was heated to1 250 ℃ and held for 10, 20 min and 30 min respectively, and the growth trend slowed down after ... 
2022-02-28 527 5.8

【作者】 张煜; 朱国辉; ...
2013-03-28 254 5.8