所有分类
  • 所有分类
  • 未分类

【作者】 杨得草; ...
2014-04-28 178 5.8

利用OM、EBSD等手段研究了热轧板两段式正火时在700℃保温不同时间(0、10、30、60 min)对含Sb冷轧无取向电工钢磁性能的影响。结果表明,700℃保温10 min处理的样品铁损最小,磁感最高。对成品板的组织分析结果表明,试样的晶粒尺寸随700℃保温时间的延长先增大后减小,保温10 min时晶粒尺寸达到最大;分析成品试样织构发现,有利织构组分随700℃保温时间的延长先增加后减少,保温10 min时有利织构组分所占百分比最高。因此,含Sb冷轧无取向电工钢两段式正火时在700℃保温10 min时磁性能最好。 Effect of two-stage normalization on magnetic property of non-oriented electrical steel containing antimony was investigated by using optical microscope(OM) and electron back-scattered diffraction technology(EBSD).The experimental results show that the iron loss and magnetic permeability of the specimen insulated at 700 ℃ for 10 min are lowest and highest respectively.The grain size of the finish specimens increases first and then decreases with the increase of holding time.Similarly,the advanta... 
2013-11-28 243 5.8

为了消除硅钢在连续退火机组产生的浪形缺陷,对浪形缺陷产生的主要原因进行了分析。制定了相应控制措施,对炉内带钢张力、冷却段输出、碳套辊与带钢的同步性、无氧化炉燃烧状态等参数进行了调整;在生产组织上安排高低牌号宽窄规格穿插生产、定期更换碳套辊等,实施后效果明显。 The main cause leading to waviness defects of silicon steel is analyzed in order to eliminate the waviness defects of silicon steel in continuous annealing line.And thus corresponding measures for controlling these defects are made by means of adjusting these parameters such as the tension of silicon steel coils in continuous annealing furnace,the output in cooling section and the combusting condition of the non-oxidation furnace as well as keeping the synchronization between carbon sleeved roll... 
2013-03-28 198 5.8

变压器D21硅钢铁芯片采用冲压工艺生产。首先对其工艺进行了分析,确定了冲压方案。对产品进行了排样设计,计算了冲压力,确定了压力中心。然后,设计了单工序落料模具,完成了模具装配图。 D21 silicon steel chips for transformer are produced by stamping.First,its stamping process was analyzed and the scheme of the stamping process was determined.The product layout was designed,the punching pressure was calculated,the pressure center was determined.Then,the blanking die with single procedure was designed,the die assembly drawing was completed. 
2013-07-28 469 5.8

采用Nb对Fe-6.5%Si(质量分数)高硅钢进行微合金化处理,结果表明:Nb在高硅钢薄板制备过程中细晶效果明显.铸态、锻态和热轧态组织的晶粒分别细化了17.50%,24.51%和30.13%.铸态样品压缩强度由1365 MPa提高至1520 MPa,延伸率提高77.78%;温轧板试样室温拉伸强度由573 MPa提高至621 MPa,延伸率提高44.44%.利用XRD对厚度为0.30—1.68 mm的温轧板的板面织构演变过程进行跟踪测量,结果发现:初始织构以(011)〈100〉Goss织构为主,单道次变形量为26.2%的情况下,Goss织构完全转化为(100)〈011〉旋转立方织构,随后,在单道次变形为22.6%的情况下,旋转立方织构完全转化为{111}面织构,即纤维织构,并稳定保持至0.30 mm. Fe-6.5%Si(mass fraction) alloy possess perfect magnetic properties,though intermetallics of Fe14Si2 phase brought 6.5%Si leads to room temperature brittleness and hinder this significant materials industrialization.Nb was adopted into micro-alloying of Fe-6.5%Si high silicon steel. OM,thermal simulated test machine and XRD were employed to study the influence of Nb on high silicon steel in processing stages.Textures of warm-rolled high silicon steel strips were determined b... 
2013-11-28 438 5.8

【摘要】 <正>目前,日本进口硅钢猛增,6月份4181吨,...
2011-05-28 738 5.8

以青海盐湖氯化镁为初级原料,采用喷雾热解法制备原料氧化镁。原料氧化镁通过水化制备氢氧化镁。将氢氧化镁过滤、洗涤、烘干、粉碎、煅烧,制备硅钢级氧化镁。本文重点考察煅烧温度、煅烧时间、料层厚度等因素对氧化镁水化率的影响,采用均匀实验设计和DPS数据处理,确定最优煅烧实验条件为:煅烧温度1250℃,煅烧保温时间4小时,料层厚度0.5cm。在此条件下得到的硅钢级氧化镁完全满足硅钢及氧化镁的行业标准。 The magnesium oxide is prepared by Spray pyrolysis process,which magnesium chloride from Qinghai Salt Lake is used as primary raw material,and hydrated to magnesium hydroxide,then obtained silicon steel magnesia through filtering,washing,drying,crushing and calcinations.In this paper,influences of some factors on magnesia hydration rate are studied,such as calcination temperature,calcination time and material thickness.After average experimental design and DPS data processing,optimal calcination... 
2013-05-28 199 5.8

研究了常化对CSP流程生产的wSi=1.6%的无取向电工钢组织、织构和成品磁性能的影响。结果表明,经CSP流程生产,且在相同的冷轧及退火制度下,经1 000℃×2min常化处理的wSi=1.6%的无取向电工钢热轧板,其最终退火成品的铁损P15/50比不常化试样下降了10.5%,磁感B50比不常化试样提高了2.5%;常化使wSi=1.6%的无取向电工钢成品的平均晶粒尺寸增大,成品铁损P15/50相应减小;同时,常化使wSi=1.6%的无取向电工钢成品中高斯织构的强度增加,γ纤维织构的强度减弱,这有利于成品磁感B50的提高。 The effect of normalizing on microstructure,texture and magnetic properties of non-oriented electrical steel with wSi=1.6% produced by CSP process was investigated.The results show that,under the same cold rolling and annealing system,the iron loss(P15/50) of annealed samples whose hot bands has been normalized by 1 000 ℃×2 min process decreases by 10.5% and magnetic induction(B50) increases by 2.5% compared with the samples whose hot bands was not normalized.The average grain size of non-orient... 
2012-11-28 227 5.8

针对川威950的工艺现状,结合无取向低硅钢SGG生产的工艺特点,主要从控制其钢坯加热和轧制以及终轧温度和卷曲温度几方面入手,进行无取向低硅钢生产的工艺控制研究。同时根据近6000吨的生产实践表明,该工艺措施能很好的满足该钢种的需要。 950 process Chuanwei status quo,with non-oriented silicon steel production process features low,mainly from the control of billet heating and rolling and finish rolling temperature and coiling temperature of several aspects,for non-oriented silicon steel production process of low control at the same time According to nearly 6,000 tons of production practice shows that the process measures could well meet the needs of the steel. 
2011-01-28 393 5.8

取向硅钢常化工序主要采用现场实测带钢温度的方式测定冷却速率,并通过稳定冷却水温、调整冷却水量及喷梁运行数量等方式保证合理的冷却速率,给常化工艺设计和生产带来诸多不便。通过对常化工艺水冷过程带钢的传热分析求解,在建立带钢水冷温度模型的基础上,研究了不同冷却工艺参数对带钢温度及冷却速率的影响规律以及冷却工艺的交互作用结果。结果表明:模型计算结果能够较好地反映取向硅钢在常化水冷过程中的温度及冷却速率的变化,其计算误差为0.80%~4.11%;在特定取向硅钢厚度规格和常化工艺下,随着常化冷却水量及有效冷却长度的增加,带钢水冷温度及冷却速率与呈非线性变化;常化水冷工艺主要通过调控带钢与冷却水之间热交换量和交换时间实现对带钢温度的控制,实际生产中需综合考虑机组速度、冷却水量及有效冷却长度之间的交互作用,选定喷梁投入数量和冷却水量以获得稳定的冷却速率。 The cooling rate of normalization process mainly determined by measuring the grain oriented silicon steel strip temperature on site, and ensures the cooling rate by stabilizing the cooling water temperature, adjusting the cooling water volume and the operation quantity of spray beam, which brings inconvenience to the normalization process design and production. Based on the heat transfer of strip in the water cooling section of normalization process, the water cooling temperature model for the n... 
2022-01-28 258 5.8

试验研究了0.3 mm取向硅钢冷轧板(/%:0.046C,3.07Si,0.09Mn,0.029P,0.004S,0.005A1)的退火温度(760~880℃7 min)和退火时间(820℃3~9 min)对该钢的晶粒尺寸,再结晶和织构的影响。结果表明,最佳初次再结晶退火工艺为820℃5 min,该钢的平均晶粒尺寸为14.20μm,完全再结晶率为92%,不利{111}<110>结构含量为3.16%,有利织构{111}<112>,{012}<001>和高斯织构含量分别0.40%,4.73%和2.46%。 The effect of annealing temperature(at 760 ~ 880 X.for 7 min) and time(at 820℃ for 3~9 min) on grain size,recrystallization rate and texture of 0.3 mm cold-rolled sheet of oriented silicon steel(/%:0.046C,3.07Si,0.09Mn,0.029P,0.004S,0.005Al) has been tested and studied.Results show that with optimum recrystallized annealing at 820℃ for 5 min,the silicon steel average grain size is 14.20 fun,the complete recrystaUization rate is 92%,the unfavourable-texture {111}< 110 > content in steel is ... 
2014-03-28 488 5.8

针对新日铁公开的相关专利,总结日本高强度无取向电工钢的研究进展,分析了各专利化学成分、生产工艺及产品性能的特点,指出固溶强化、细晶强化、析出强化、位错强化都有可能被用来提高无取向电工钢的强度。在高强度无取向电工钢的研发过程中,需要根据其具体用途确定目标性能,再采用合适的强化手段,从而实现力学性能、磁性能和生产性能之间的平衡。 Authors summarize the research progress of high strength non-oriented electrical steel in Japan by learning related patents brought into the public by Nippon Steel. Authors also analyze the characteristics of the chemical composition, production technology and properties of products in the patents and point out that any ones of solution strengthening method, fine-grain strengthening method, precipitation strengthening method or dislocations strengthening method may be used to improve the strengt... 
2013-11-28 218 5.8

站点公告

网站试运行,请大家关注本站公众号,多提宝贵意见!

显示验证码
没有账号?注册  忘记密码?