所有分类
  • 所有分类
  • 未分类

根据新日铁、JFE及浦项等国外钢铁公司2008年以来在日本专利局、欧洲专利局(EP)及世界知识产权组织(WIPO)申请公开的有关生产Hi-B取向电工钢典型专利技术,概述了近年来国外大型钢铁企业采用低温板坯加热(坯加热温度<1 280℃)技术生产Hi-B取向电工钢主要技术重点,即将调节关键化学成分Al、N、Sn及Sb等与工艺改进相结合。最后介绍了国外大型钢铁企业采用低温板坯加热技术生产Hi-B取向电工钢实例。 The latest developments on technology for manufacturing Hi-B grain oriented electrical steel sheets developed by Nippon Steel Corp.,JFE Steel and POSCO were described according to the patents published by World Intellectual Property Organization,Japan Patent Office and European Patent Office over the recent years.The low temperature slab heating process(particularly slab-heating temperature<1 280 ℃) together with suitably adjusting key chemical elements such as Al,N,Sn and Sb elements was the... 
2013-03-28 138 5.8

以试验室模拟CSP工艺生产的Fe-3Si热轧钢带为研究对象,采用正交试验及方差分析的方法,研究了取向硅钢初次再结晶退火工艺对高温退火后获得锋锐的高斯织构的影响。结果表明:取向硅钢两段式初次再结晶脱碳退火工艺参数加热段保温时间及加热温度是高温退火后获得锋锐高斯织构的主要影响因素,其可信度分别在90%和85%以上;在本试验条件下,通过正交试验获得的最佳退火工艺为:冷硬板经600℃保温3 min和850℃保温6 min。 Fe-3Si hot rolled strip was produced by simulating CSP technology in the laboratory.Orthogonal experiment and analysis of variance were carried out to investigate the influence of primary recrystallization on the sharp Goss texture of the oriented silicon steel.The results show that holding time of the heating section and the heating temperature for a sharp Goss texture of the samples annealed has important implications in this experiment conditions,the two-step decarburization annealing process... 
2013-02-28 160 5.8

在现普通冷轧无取向硅钢的基础上,降低Si含量,复合添加少量辅助元素,组合热轧板处理和成品退火加热技术,研制出了免常化处理的高磁感、低铁损并具有良好耐酸腐蚀性能的新系列无取向电工钢。 Based on existing common cold rolled non-oriented silicon steel,a new series of non-orientedelectrical steel with high induction,low core loss and excellent anti-corrosion property has been developed by reducing Si element,adding complexly a small amount of supplementary elements,and employing combined treatment of hot rolled sheet and finished product annealed heated technology. 
2013-02-28 138 5.8

对RH法(真空循环脱气法)生产的冷轧硅钢的脱硫原理及影响因素进行了分析研究。研究表明:降低顶渣中FeO、MnO的含量,提高钢液温度,增加脱硫剂的加入量并延长其循环时间有利于提高脱硫效率。 The principles of desulfurization and its influence factors of cold rolling silicon steel during RH process have been studied in this paper.The result indicated that reducing contents of FeO and MnO,rising temperature of the liquid steel,increasing quantity of desulfurizer,lengthening cycle time of desulfurzer are benefit for desulfurization. 
2011-06-28 137 5.8

介绍了CSP工艺生产无取向电工钢各工序的设备特点、采用的工艺控制手段和电工钢产品质量情况,结合生产实践证明了马钢CSP工艺开发的无取向电工钢产品丰富了薄板坯连铸连轧的品种结构,发挥了薄板坯连铸连轧生产无取向电工钢性能均一、稳定的特点。 The equipment characteristic,the process control method and the quality of non-orientated silicon steel by CSP process were introduced.Combined with the production situation,it is proved that production of non-orientated silicon steel developed on Masteel CSP line would enrich product structure of thin slab continuous casting and rolling,and it exerts stable performance of non-orientated silicon steel. 
2013-06-28 176 5.8

【作者】 侯桂芹; 张颖; ...
2023-05-09 203 5.8

阐述了电工钢在\"双碳\"中的作用,强调了电工钢的生产工艺技术及在减少碳排放、降低能耗中的作用,对下游能效升级带来明显的节能及降碳成果。同时,分析了2021年电工钢的生产运行情况,介绍了电工钢的未来发展,并针对如何减少碳排放以及生产更多的更低铁损、更高磁感的电工钢谈了几点启示。 The effects of electrical steels on carbon peak and carbon neutralization were expounded,especially on the achievements of obvious energy saving and carbon reduction to the downstream energy efficiency upgrading bringing from the production technology of electrical steels and their effects to reducing carbon emission and energy consumption.Meanwhile the production situation of electrical steels in 2021 was analyzed,and the future development of electrical steels was introduced,and some advices w... 
2022-01-28 184 5.8

对高牌号无取向电工钢国内生产情况、工艺技术、产品性能及应用领域等进行了阐述,并探讨了高牌号无取向电工钢产品的发展趋势。 This paper introduces basic facts on the production status,process technology and products’ properties and their applications of non-oriented electrical steel with high grade at home,and then discusses the development trend on technology for producing the non-oriented electrical steel with high grade. 
2011-02-28 166 5.8

6.5%Si硅钢具有优异的磁学性能和广泛的应用前景。本文综述了6.5%Si硅钢的物理、机械及磁学特性,讨论了传统轧制、温轧、薄带连铸、快速凝固、CVD、粉末轧制等不同制备工艺的关键技术及特点,概括了6.5%Si硅钢在高效节能电机、汽车马达及磁屏蔽等领域中的主要应用,介绍了硅钢的制备技术取得的研究进展,并指出了其广阔的发展前景。 6.5% Si silicon steel has good magnetic properties and wide applications.In this paper physical and mechanical magnetic properties were summarized,and key technology and characteristic of several preparation methods,such as traditional rolling,warm rolling,thin strip continuous casting,rapid solidification,CVD and powder rolling,were discussed.Main applications of 6.5% Si steel in the fields of high-efficiency electrical motors,automobile motors,transformer cores and magnetic shielding were gene... 
2012-06-28 155 5.8

简要介绍了宝钢无取向电工钢的发展历程、产品大纲、电磁性能控制情况,以及高附加值新产品的开发、应用情况。概述了近年来宝钢无取向电工钢生产技术进步,主要包括夹杂物控制技术、连轧机高牌号硅钢制造技术、同板差控制技术、环保涂层开发技术等。 This paper briefly summarizes the development history, product catalogue, and magnetic properties of non-oriented electrical steel sheets at Baosteel, as well as the development and application of high-value-added steel grades. Recent advances in manufacturing electrical steel sheets are also introduced, including technologies for controlling inclusion, producing high-grade steel strips by a tandem rolling mill, and controlling the transverse thickness difference of steel sheets, as well as the ... 
2014-05-28 172 5.8

冷轧无取向硅钢(/%:0.003C,2.35Si,0.22Mn,0.011P,0.002S,0.36A1,0.003 0N)经890℃或940℃3 min常化的2.3 mm热轧板冷轧成0.35 mm薄板。研究了常化温度和800920℃3 min退火对该钢高频(400Hz)磁性能和抗拉强度的影响。结果表明,830920℃退火时高频铁损P10/400值最低,随退火温度增加,晶粒尺寸增大,钢的抗拉强度降低;该钢的最佳热处理工艺为常化温度940℃,退火温度830℃,其抗拉强度Rm、高频铁损P10/400和磁感应强度J50分别为565 MPa,21.5 W/kg和1.69 T。 The cold-rolled non-oriented silicon steel(/%:0.003C,2.35Si,0.22Mn,0.011P,0.002S,0.36A1,0.003 0N) is cold-rolled to 0.35 mm sheet from 2.3 mm hot-rolled plate normalized at 890 ℃ or 940℃ for 3 min.The effect of normalizing temperature and annealing process at 800 920 °C for 3 min on high frequency(400 Hz) magnetic properties and tensile strength of the steel has been tested and studied.Results show that with annealing at 830 920 ℃the high frequency iron loss value P10... 
2014-03-28 159 5.8

采用CVD法制备6.5%Si高硅钢,介绍了具体的制备工艺过程,研究了温度对渗硅速率和试样质量减轻的影响,同时分析了扩散时间对高硅钢中硅分布的影响。结果表明:在CVD反应过程中,反应温度高于1050℃将大大提高渗硅速率,但当温度大于1200℃后,渗硅速率趋于稳定;渗硅后,试样会减轻、减薄,随着温度升高,试样质量减轻的速率逐渐增大,在1200℃左右趋于稳定;扩散时间越长,硅分布越均匀,结合制备效率进行考虑,满足Δw表-中/b≤5的时间为适宜的扩散时间。 6.5%Si high silicon steel was manufactured by using CVD method and the process was introduced,the influence of temperature on the siliconizing rate and quality reducing rate,diffusion time on silicon distribution were investigated.Results as follows: the siliconizing rate will increase quickly when the temperature is higher than 1050 ℃,but the siliconizing rate will become steadily as the temperature up to 1200 ℃;The quality reducing rate will increase with the elevating of temperature and the r... 
2013-01-28 159 5.8

站点公告

网站试运行,请大家关注本站公众号,多提宝贵意见!

显示验证码