钢厂
硅钢轧制过程中乳化液流量数学模型研究及应用
目前高磁感冷轧硅钢生产过程中,采用经验方法确定的乳化液流量设定值往往会造成硅钢产品的磁感性能达不到预期目标,针对此情况,基于轧机轧制机理研究了的乳化液流量数学模型,确定了乳化液流量设定值。实践表明,使用该数学模型输出的乳化液流量设定值,可提高轧制过程中乳化液流量控制精度,从而提高高磁感冷轧硅钢的轧制性能。 In view of the current production process of high magnetically inductive cold-rolled silicon steel, the mathematical model of emulsified fluid flow based on mill rolling mechanism is studied in view of the situation in which the magnetic sensing performance of silicon steel products is often not up to the expected target by using empirical method to determine the emulsified liquid flow setting. Practice shows that the emulsified fluid flow setting value output from this mathematical model improv...
钒钛对取向硅钢组织、织构和析出物的影响
通过在实验室条件下模拟薄板坯连铸连轧流程,并在以Cu2S为主抑制剂制造普通取向硅钢(CGO)的基础上,加入适量钒钛,研究了钒钛对取向硅钢组织与磁性能的影响。结果表明,适量钒钛使热轧板和脱碳退火板组织更好,尤其使脱碳退火板的晶粒更加细小和均匀;加入适量钒钛不但使热轧板表面高斯织构强度更高,更使脱碳退火板中有利于高斯织构发展的γ织构强度更高;适量钒钛能形成Cu2S+(V,Ti)N等复合析出物,起到辅助抑制剂作用,加强抑制能力。细小均匀的晶粒、强度更高的有利织构和更强的抑制能力使CGO钢磁性能更佳。 Effect of V and Ti on microstructure and magnetic properties of conventional grain-oriented silicon steel(CGO) were investigated under simulated thin slab continuous casting and rolling process in laboratory with Cu2 S as the dominant inhibitor. The results show that appropriate amount V and Ti make the microstructures of the hot rolled sheet and the decarburizing annealed sheet better,especially make the grains of the decarburizing annealed sheet more tiny and uniform. Adding appropriate V and ...
冲剪加工对无取向硅钢边缘组织和磁性能的影响
通过观察冲剪边缘组织,测量冲剪边缘的显微硬度、残余应力的分布情况和磁性能的变化研究了冲剪加工对无取向硅钢50WW800边缘组织和磁性能的影响。对冲剪后硅钢片进行750℃退火,分析退火对组织和磁性能的影响。结果表明,硅钢片剪切边缘会存在0.4 mm的形变硬化层,边缘应力大,铁损增加。退火后变形减小,形变硬化层变小,残余应力大幅度减少,铁损减少。 The influence of punching process on cutting edge microstructure and magnetic properties of non-oriented silicon steel 50WW800was studied by observing microstructure and measuring microhardness near cutting edge.The residual stress distribution in the silicon steel tooth and magnetic properties were measured.Effect of annealing at 750 ℃ on microstructure and magnetic properties of the silicon steel was analyzed.The results show that a cut-edge hardening layer up to 0.4 mm is observed,residual st...
无取向硅钢冶炼过程中的夹杂物遗传变化
研究表明,硅钢中的夹杂物对成品带钢的磁性能有显著影响。为研究冶炼过程硅钢中的夹杂物遗传变化,进而提出更有效的控制措施加以去除,本文结合典型的无取向硅钢生产炉次,采用非水溶液电解提取+扫描电镜观察方法分析冶炼过程中上述炉次典型试样的夹杂物。结果表明:转炉冶炼结束、RH精炼开始时,钢的氧化物夹杂总量最大,约为0.23%;RH精炼过程中,氧化物夹杂总量不断降低,并在脱碳结束时达到最低,约为0.02%;连铸过程中,氧化物夹杂总量仍有不断降低趋势,但夹杂物的平均尺寸变化不大。本试验条件下,中间包试样的夹杂物数量约为1.59×104个/mm3。 As we all know, the non-metallic inclusion effects magnetic properties of silicon steel sheets obviously. The article aims to study the heredity of non-metallic inclusion in non-oriented silicon steels during the steel making process, and then provides a more effective controlling measure to remove the inclusions. Based on the typical non-oriented silicon steel charges, the non-aqueous solution extraction and SEM observation were adopted to analyze the non-metallic inclusions. Results show that,...
辉光放电发射光谱法测定电工钢中8种元素
通过对辉光放电发射光谱法分析电工钢样品光谱行为的研究,分析其工作参数如:电压、电流、预溅射时间和积分时间对光谱强度和稳定性的影响,并以铁为内标元素,优化了工作参数。确定了直流辉光放电光谱法测定电工钢中碳、硅、锰、磷、硫、铬、镍、铜共8种元素的定量分析方法,并对该方法分析的精密度和准确度进行验证,结果表明,各元素的测定结果与认定值和其他方法测定值一致,测量元素结果RSD值小于2%。 Based on research on analyzing the spectrum behavior of the sample taken from the electrical steel by glow discharge optical emission spectrometry,the effect of its operational parameters such as current,voltage,pre-sputtering time and integrating time on the spectral intensity and spectral stability is analyzed.Taking the Fe as an element applied by internal standard method,these operational parameters are optimized,and therefore the quantitative analysis method for testing eight kinds of eleme...
预退火温度对高磁感取向硅钢初次再结晶织构的影响
对高磁感取向硅钢冷轧板分别进行800、950、1050和1120℃不脱碳的预退火处理,在800℃预退火,成品的磁性能较好。织构分析的结果表明,随着预退火温度升高,初次再结晶后有利织构组分{111}<112>与不利织构组分(118)[110]的比值f(111)/f(118)逐渐降低,初次再结晶织构的变化是成品磁性的影响因素之一。 Preliminary annealing process at different temperatures for cold-rolled strips of a high permeability grain-oriented silicon steel was investigated to study the effect of the annealing temperature on microstructure and magnetic performance of the steel.Results show that the magnetic performances of the products annealed at 800 ℃ are best.Analysis of primary recrystallization texture indicates that with rising temperature,f(111)/f(118) which is the ratio of the favorable component {111}<112>...
轧制裂纹及热处理工艺对高硅电工钢复合板磁性能的影响
对3层高硅电工钢复合板铸坯进行热轧及温轧变形加工后,采用正火、退火两种热处理方式处理,并观察轧制过程中产生的裂纹,研究不同状态下复合板的磁性能。对不同状态下的试样进行扩散退火处理,研究复合板中裂纹变化及其对磁性能的影响。结果表明:不同热处理工艺下合金内部的裂纹尺寸差异明显,裂纹尺寸对复合板的磁性能影响显著,相对于深裂纹,其他因素的影响较小;温轧变形加工后,复合板内层出现有序组织,但该有序组织在合金存在深裂纹的前提下并不能从本质上提高合金的磁性能;扩散退火工艺可以消除复合板内部的浅裂纹及微裂纹,但不能消除尺寸较大的裂纹,故而不能显著提高存在深裂纹的复合板的磁性能。 After hot rolling and warm rolling deformation processing of casting billet for three-layer high silicon electrical steel composite plate, it was normalized and annealed for heat treatment. Then, the cracks produced during the rolling process were observed, and the magnetic properties of composite plate in different states were also investigated. Furthermore, the samples in different states were subjected to diffusion annealing treatment, and the changes of crack in composite plate and their eff...
无取向电工钢深脱硫试验
为满足用户对无取向电工钢中硫含量的要求,采用CaO-CaF2复合渣系为脱硫剂,利用RH投入法对无取向电工钢进行深脱硫试验。试验结果表明,RH精炼渣成分控制在w CaO43%~51%、w Al2O325%~31%、w MgO4%~6%、w SiO29%~12%、w(FeO+MnO)3%~6%,在脱硫剂加入量为6~8 kg/t时,钢中平均硫含量从32×10-6降低到18×10-6,RH平均脱硫率为43.3%,最高达47.1%。利用KTH模型计算精炼终渣平均硫容量为0.003 1,RH精炼结束时渣-钢间实际平均硫分配比从14增加到52。 In order to satisfy the requirements of consumers on sulfur content in non-oriented electrical steel,taking( CaO-CaF 2) based flux as desulfurizer,industrial experiments on deep desulphurization of non-oriented electrical steel were carried out during RH process. The results show that as the compositions of refining slag are appropriately controlled with w CaO of 43% ~ 51%,w Al2O3 of 25% ~ 31%,w MgO of 4% ~ 6%,w SiO2 of 9% ~ 12%,and w( FeO + MnO) of 3% ~ 6%,and the desulfurizer added are at 6 ~ ...
高牌号无取向电工钢RH深脱硫
以CaO-CaF2复合渣系为脱硫剂,在RH精炼过程采用真空投入法进行高牌号无取向电工钢深脱硫工业试验,采用KTH模型计算分析了RH炉渣成分对硫容量CS的影响。研究结果表明,炉渣成分控制在w((CaO))/w((SiO2))为5~7,w((CaO))/w((Al2O3))为1.5~1.8,w((Al2O3))为25%~30%,w((FeO+MnO))<5%,脱硫剂加入量为6~8kg/t时,钢中硫质量分数从平均0.003 1%降低到0.001 8%,最高脱硫率达到47.1%,平均脱硫率为41.7%。 The industrial trials on deep desulphurization of high grade non-oriented electrical steel were finished through using CaO-CaF2complex based fluxes in RH process.Using the KTH model,the effect of refining slag composition on the sulfide capacities was analyzed.The results show that the chemical composition of refining slag(mass fraction,%)is w((CaO/SiO2))between 5to 7,w((CaO))/w((Al2O3))beween 1.5to 1.8,w((Al2O3)) between 25%to 30%,w((FeO+MnO))less than 5%,and the desulphurizer addition level of...
无取向硅钢晶粒长大过程中应力对织构和晶界变化的影响
采用EBSD技术研究了有、无拉应力作用下无取向硅钢在晶粒长大过程中织构转变及晶界变化的规律。结果表明:在晶粒生长期间,无应力作用下的硅钢中,{111}〈112〉,{111}〈110〉织构组分强化,而{100}〈001〉织构组分弱化;与无拉应力作用下的情况相比,施加5MPa的拉应力时,{111}〈112〉,{111}〈110〉织构组分强化的速率下降,{100}〈001〉织构组分变化不明显。对于在晶粒生长期间持续变化的{111}〈112〉,{111}〈110〉和{100}〈001〉织构组分而言,虽然有、无拉应力作用下硅钢的{111}〈112〉和{111}〈110〉织构组分的高取向差角度晶界频率均下降,而{100}〈001〉织构组分的高取向差角度晶界频率则上升,但当有拉应力作用后,{111}〈112〉和{111}〈110〉织构组分的高取向差角度晶界频率下降的速率变小,{100}〈001〉织构组分的高取向差角度晶界频率上升的速率稍有变小。通过对无取向硅钢在晶粒长大过程中织构转变及晶界变化规律的研究,分析了合金原子在晶界的偏聚行为。 The rules of texture and grain boundary transformation in the nonoriented silicon steel under applied stress or without applied stress during grain growth were investigated by EBSD.The results show that the {111}〈112〉 and {111}〈110〉 components in the nonoriented silicon steel without stress are strengthened during grain growth whereas {100}〈001〉 component is weakened,but the growth rate of {111}〈112〉 and {111}〈110〉 component decreases,while the area fraction of {100}〈001〉 component doesn’t chang...
ZnO对硅钢绝缘涂层组织与性能的影响
通过制备磷酸二氢铝硅钢涂层,研究了氧化锌对无铬涂层耐盐雾性能、电化学性能和附着性的影响。结果表明,硅钢表面涂层含有4.0%的氧化锌时,涂层具有最高的耐腐蚀性能和电化学性能,而且其致密表面最为平整,没有裂纹出现。 The effects of ZnO on the salt spray resistance property, electrochemical performance and adhesiveness of silicon steel insulating coating were studied. The results show that the best corrosion resistance and electrochemical properties can be obtained when the coating contains 4.0% oxide zinc, and the dense surface is smooth without cracks.