稀土元素在许多钢中发挥着独特而且不可替代的重要作用。半个世纪以来,它的作用已经在各种低合金和特殊合金钢中的研究及应用中得到充分的证明;然而,作为具有稀土资源优势的中国,在属于重要功能材料的无取向电工钢中稀土的应用却落后于国外,本文就中国稀土在无取向电工钢中的应用研究作简要的评述,希望能够进一步推进此领域的研究,并且促进中国稀土在无取向电工钢中应用技术的发展,缩短与国外差距,并提出了在此应用领域今后需深入开展的研究方向。 Rare earth elements play a unique and irreplaceable role in a lot of steels,it has given the full proof by the practice of various low alloy steels and special alloy steels since half century.However,as our country has the advantage of rare earth resources,RE application technology in non-oriented electrical steels has lagged behind abroad.The application researches of rare earth in non-oriented electrical steel in our country are briefly reviewed in this paper,which hope to promote the research... 
2014-05-28 161 5.8

采用EBSD检测技术,分析了50W800无取向电工钢在重要生产工序间织构的演变以及织构沿带钢宽度方向上的差异性。结果表明:热轧板织构沿带钢宽度方向上的差异性主要体现在表层织构。带钢边部表层织构主要由旋转立方织构、α纤维织构以及少量的γ纤维织构组成,带钢宽度1/4处的表层织构主要存在高斯织构,带钢宽度1/2处的表层织构主要为(110)面织构以及少量的铜型织构。各处的带钢宽度1/4处和1/2处的织构类型基本一致,都以α纤维织构和旋转立方织构为主。冷轧后,各处的表层织构类型差异较小,均为γ纤维织构和α纤维织构。由板宽边部至中心处织构强度值逐渐降低。退火后,各处织构的组分基本一致,为较强的γ纤维织构和较弱的(100)面织构。各处织构强度值差异较小,变化趋势与冷轧板一致。 The texture of non-oriented electrical steel 50W800 was detected by EBSD technique.The evolution of the texture between important processes and the difference of texture along the width direction of strip were analyzed.The result shows that the difference along the width direction of strip of texture at the surface of hot rolled plate is most obvious.The texture at the surface of strip edge is primarily made of rotating cube texture,αfiber texture and weakγfiber texture.Goss texture is mainly co... 
2014-09-28 160 5.8

研究了CSP工艺生产≤0.005%C-1.1%Si的2.2mm无取向电工钢热轧板在800~1000℃常化对0.5mm冷轧板840℃退火后组织和磁性能的影响。结果表明,热轧板常化温度升高,冷轧板退火后的再结晶晶粒增大,铁损降低,磁感增加;热轧板常化温度超过900℃,因第二相固溶而后弥散析出,退火后冷轧晶粒细化,铁损增加,因此该无取向电工钢热轧板最佳常化温度为900℃。 The effect of normalizing at 800-1000℃ of CSP produced plate(≤0.005%C-1.1%Si) on the microstructure and magnetic properties of downstream cold-rolled non-oriented electrical steel annealed at 840℃ was studied.Results show that with increasing normalizing temperature of hot-rolled material the recrystallized grain size of annealed sheet increases,iron loss reduced and magnetic induction increases.As normalizing temperature excesses 900℃,grain is refined and iron loss increases after annealing due... 
2012-03-28 148 5.8

研究了应用电感耦合等离子体质谱(ICP-MS)同时测定硅钢中痕量铝、钼、钒、钛、铌元素的分析方法。通过条件试验对测量参数进行了优化,确定RF功率1 400 W,泵速30rpm,采样深度140,雾化压力0.90。样品采用硝酸分解,以Be、Y混合内标校正了测量过程中高基体引起的信号漂移。根据测量时存在的质谱干扰情况,选择同位素27 Al、98 Mo、51 V、47 Ti和93 Nb作为测定同位素,同时通过调节仪器参数使得双电荷离子和氧化物离子的产率最低,以减少其带来的干扰。采用基体匹配法配制校准溶液,以标准加入法建立工作曲线,并扣除试剂空白。该方法各元素的测定下限均可达到1μg/g。用于硅钢标准样品的测定,所得结果与参考值完全吻合,各元素的RSD小于5.2%。 A method for the determination of trace aluminum,molybdenum,vanadium,titanium and niobium in silicon steel by inductively coupled plasma mass spectrometry(ICP-MS) was described.A series of single parameter condition experiment was conducted.The optimized operation parameters with RF power 1 400 W,turbo pump rate 30 rpm,sampling depth 140 and nebulizer pressure 0.90 were obtained.The samples were dissolved by HNO3,and the Be and Y mixing internal standard were used to eliminate the signal drift c... 
2013-01-28 180 5.8

在现普通冷轧无取向硅钢的基础上,降低Si含量,复合添加少量辅助元素,组合热轧板处理和成品退火加热技术,研制出了免常化处理的高磁感、低铁损并具有良好耐酸腐蚀性能的新系列无取向电工钢。 Based on existing common cold rolled non-oriented silicon steel,a new series of non-orientedelectrical steel with high induction,low core loss and excellent anti-corrosion property has been developed by reducing Si element,adding complexly a small amount of supplementary elements,and employing combined treatment of hot rolled sheet and finished product annealed heated technology. 
2013-02-28 146 5.8

磁性能指标是硅钢产品最关键的质量指标之一,但是目前磁性能判定100%依赖于样品的离线实验室检测结果,生产线配置的在线检测仪的测量结果由于精度问题,不宜直接用于成品牌号判级。本文在现有硅钢产品质量管控体系基础上,利用大数据技术对生产数据进行分析与建模,构建不同磁性能指标在线检测模型,并在现有信息系统上完成模型库的集成部署,实现硅钢产品全长、多指标磁性能结果的拟合数据输出,支撑取样优化、精准分切、辅助综合判定等功能应用,进一步优化硅钢产品质量管控体系。 The magnetic performance index of silicon steel products is one of the most critical quality indexes.However,at present,100%determination of magnetic performance depends on the offline laboratory test results of samples,and the measurement results of the online detector configured in the production line cannot be applied in practice due to the accuracy problem.Based on the existing quality control system of silicon steel products,big data technology was used to analyze and model the production d... 
2022-02-28 233 5.8

为提高无取向硅钢导磁性能,研究了不同剪切方式对无取向硅钢剪切处磁畴结构的影响。利用纳米磁流体观测无取向硅钢剪切后边部磁畴结构。结果表明,硅钢无论在机械剪切还是线切割后的边部磁畴都会发生不同程度的改变:线切割对边部磁畴结构改变较小,边部磁畴分布均匀且连续,在距边缘0~20μm范围内出现磁畴宽度变小现象;机械剪切对磁畴的改变较为严重,剪切处磁畴零乱且不连续,在距边缘20μm处仍难以观察到完整的磁畴结构。 The effects of different shearing modes on magnetic domain structure of cold rolled non-oriented silicon steel are studied in this paper.The magnetic domain of cold rolled non-oriented silicon steel is observed by nanometer magnetic fluid pattern method.The results show that the edge magnetic domain structure will be changed by mechanical shear and wire-electrode cutting,the variation of edge magnetic domain structure wire-electrode cutting edge is very small,the magnetic domain structure is wel... 
2012-04-28 157 5.8

研究表明,硅钢中的夹杂物对成品带钢的磁性能有显著影响。为研究冶炼过程硅钢中的夹杂物遗传变化,进而提出更有效的控制措施加以去除,本文结合典型的无取向硅钢生产炉次,采用非水溶液电解提取+扫描电镜观察方法分析冶炼过程中上述炉次典型试样的夹杂物。结果表明:转炉冶炼结束、RH精炼开始时,钢的氧化物夹杂总量最大,约为0.23%;RH精炼过程中,氧化物夹杂总量不断降低,并在脱碳结束时达到最低,约为0.02%;连铸过程中,氧化物夹杂总量仍有不断降低趋势,但夹杂物的平均尺寸变化不大。本试验条件下,中间包试样的夹杂物数量约为1.59×104个/mm3。 As we all know, the non-metallic inclusion effects magnetic properties of silicon steel sheets obviously. The article aims to study the heredity of non-metallic inclusion in non-oriented silicon steels during the steel making process, and then provides a more effective controlling measure to remove the inclusions. Based on the typical non-oriented silicon steel charges, the non-aqueous solution extraction and SEM observation were adopted to analyze the non-metallic inclusions. Results show that,... 
2014-05-28 167 5.8

研究稀土Ce的添加对含Sn高磁感无取向电工钢磁性能及夹杂物的影响。对比分析了两种成分钢的磁性能以及各过程工艺条件下夹杂物种类和分布情况。结果表明,在含Sn高磁感无取向电工钢中加入稀土元素Ce可以粗化夹杂物,提高成品晶粒的均匀性,有效降低铁损;同时Ce的添加不影响Sn元素提高磁感的效果,磁感保持不变。 Effect of Ce on magnetic properties and inclusion of Sn-bearing high permeability non-oriented electrical steel was investigated. A comparative analysis of the magnetic properties and the types and distributions of inclusion in the two sheets with different composition shows that the addition of Ce to the Sn-bearing high permeability non-oriented electrical steel can coarse the inclusion,improve the homogeneity of the finished grain and effectively decrease the core loss. Also,the addition of Ce... 
2014-08-28 195 5.8

介绍了普通取向硅钢(CGO)和高磁感取向硅钢(Hi-B)铸坯高温加热两次冷轧、一次冷轧和铸坯低温加热两次冷轧、一次冷轧法4种成熟生产工艺的主要技术参数,取向硅钢理论研究(Goss晶核和抑制剂)和生产技术现状。取向钢的发展趋势为:提高(110)[001]晶粒取向度,降低取向硅钢铁损,发展铸坯低温加热(≤1 300℃)和薄板坯连铸连轧流程生产取向硅钢工艺。 Main technology parameters of four developed process:cast bloom higher temperature heating-double cold rolling or single cold rolling,lower temperature heating-double cold rolling or single rolling process for production of common grain oriented silicon steel(CGO) and high magnetic induction grain oriented silicon steel(Hi-B),theory research on grain oriented steel(Goss nucleus and inhibitor) and present situation of process are summarized in this paper.The development trend of grain oriented si... 
2013-05-28 178 5.8

研究了CSP流程试制50W270高牌号无取向硅钢热轧→常化→冷轧→退火过程中织构的演变.利用电子背散射衍射技术对全流程织构进行测量和分析.发现热轧板织构在厚度方向上存在较大差异,表层主要为铜型、黄铜和高斯织构,1/4层存在微弱的高斯织构和旋转立方织构,中心层以γ纤维织构和旋转立方织构为主,还含有较弱的α纤维织构.与热轧板相比,常化板表层和1/4层织构变化不大,中心层旋转立方织构和α纤维织构增强.冷轧板各层均具有α纤维织构和γ纤维织构.与冷轧板相比,成品板各层中α纤维织构基本消失,还出现了立方织构和高斯织构. This article focuses on texture evolution in 50W270 high-brand non-oriented silicon steel produced by CSP in hot rolling,normalizing,cold rolling,and annealing processes.The texture in the whole process was measured and analyzed by electron back-scatter diffraction.It is found that the texture along the thickness direction in hot-rolled strips changes obviously;there are mainly copper,brass,and Goss textures in the surface layer;the 1/4 layer has weak Goss texture and rotating cube texture;γ-fib... 
2014-09-28 178 5.8