钢厂
低铁损高磁通密度无取向硅钢的应用与生产技术进展
分析了高转矩和高转速条件下高效驱动马达铁芯材料对无取向硅钢磁性能要求,讨论了无取向硅钢的高磁通密度和低铁损对电机转矩和效率的影响,介绍了国内外高磁感无取向硅钢发展情况。在生产工艺上,提高钢质纯净度,弱化夹杂物和第二相粒子对畴壁移动和再结晶晶粒长大的钉扎作用,添加微量晶界和带钢表面的偏析元素促使有利织构发展等技术可提高无取向硅钢的磁通密度。 The requirements of high efficient drive motor core materials under the conditions of high torque and high speed were analyzed.The effects of high magnetic flux density of non-oriented silicon steel on the torque and efficiency of the motor were discussed.The development of non-oriented silicon steel with high magnetic was introduced.The magnetic flux density of non-oriented silicon steel sheet can be obviously improved by some production technologies,such as purification steel,weakening the pin...
TSCR热轧工艺对3.2%Si无取向硅钢组织性能的影响
研究了薄板坯连铸连轧流程(TSCR)条件下热轧工艺对3.2%Si-0.7%Al无取向硅钢组织、织构演变及磁性能的影响规律。结果表明,提高均热温度和热轧温度有助于获得粗大的变形组织和强烈的{001}〈110〉织构,进而对后续的组织、织构演变进程及磁性能产生有利的遗传影响。与低温均热和低温热轧相比,高温均热和高温热轧得到的最终成品板的再结晶晶粒较粗大,λ纤维再结晶织构较强而γ纤维再结晶织构较弱,磁感应强度较高。 It was investigated that the effects of thin slab cast rolling(TSCR) hot rolling processes on microstructural,textural evolution and magnetic properties of 3.2%Si-0.7%Al non-oriented silicon steel.The results show that much larger hot rolling deformed microstructure and much stronger {001}〈110〉 texture could be obtained by increasing the soaking and hot rolling temperatures,which had good heritable effects on subsequent microstructural,textural evolution and magnetic properties.The final sheets ...
钇元素对6.5%Si无取向硅钢组织、高温拉伸及断裂机制的影响
通过微观组织表征、高温拉伸和断口形貌分析,研究了钇(Y)元素对6.5%Si无取向硅钢组织、高温拉伸及断裂机制的影响。研究结果表明,添加Y元素可以在钢液中形成YS和YP的复合析出。YS和YP可以充当异质形核基底,提高形核率,细化凝固组织。热轧组织不均匀,由表层至芯部分别形成等轴晶、等轴晶/拉长晶和拉长晶的混合组织。退火后,热轧变形组织转变为等轴晶,含Y实验钢的退火组织得到明显细化。500℃时效处理后,含Y实验钢具备较低的有序度,300℃的拉伸断口呈现韧性断裂特征,断后伸长率达到20.2%。相反,无Y实验钢发生脆性断裂,断后伸长率仅为2.1%。研究结果证实,Y元素可以通过组织细化和降低有序度提高6.5%Si无取向硅钢的中温塑性。 The effects of yttrium(Y)on microstructure,elevated-temperature tensile properties and fracture mechanism of 6.5% Si non-oriented electrical steel were investigated by means of microstructure characterization,high-temperature tensile test and fracture analysis.The results showed that the doping of Y introduced composite Y-rich precipitates(YS/YP)in the melt.YS and YP precipitates were qualified for heterogeneous nucleation agents,which thus raised the nucleation rate and refined the solidificati...
电解清洗装置在电工钢生产线上的应用
介绍了电工钢生产线连退机组的表面处理工艺,特别是电解清洗系统的工作机理、设备构造、生产工艺及各种影响因素。 This paper introduces the technology of surface treatment of continuous annealing unit in electrical steel production line,in particular the working mechanism,structure of equipment,production techniques and various influence factors of the electrolytic cleaning system.
修正GTN模型及其在预测硅钢冷轧边裂中的应用
考虑剪应变对微孔洞损伤演化的影响,对GTN损伤模型的损伤演化机制进行修正,建立了适用于不同应力三轴度水平的损伤模型。结合隐式应力更新算法和显式有限元计算,采用VUMAT子程序实现了修正GTN模型在有限元软件ABAQUS中的数值计算。通过模拟纯剪切和剪切-拉伸两组试样的损伤演化和断裂行为,验证了修正GTN模型在不同应力三轴度承载条件下的有效性。运用修正GTN损伤模型模拟含边部缺口的带钢在轧制过程中裂纹的萌生和扩展行为,模拟结果与实验相一致,表明该模型可有效地用于带钢缺陷在轧制过程中扩展行为的分析和预测。模拟和实验结果表明,带钢边部缺口在轧制过程中,缺口前沿和后沿均会萌生裂纹,且后沿裂纹扩展更为明显。 Considering the effect of shear strain of micro-void on damage evolution, a modified GTN model applicable to various stress triaxiality conditions is proposed by modifying the damage evolution mechanism of the GTN damage model. The modified model is implemented in commercial finite element software ABAQUS by combining the implicit stress update method with an explicit finite element solving algorithm and through the user-defined material subroutine VUMAT. The damage evolution and the failure pro...
热轧原料断面轮廓对冷轧硅钢尺寸精度的影响分析
根据现场实际的生产控制情况,指出了热轧原料断面轮廓缺陷以一定的比列遗传给了冷轧带钢,分析了不同热轧原料断面轮廓对冷轧电工钢尺寸精度的具体影响,提出了相应的规律。并阐明了严格控制热轧原料断面轮廓形貌,对保证冷轧电工钢尺寸精度具有重大意义,对于中国现行的冷轧电工钢生产具有指导意义。 Based on the actual situation of production control,it was pointed out that the section profile defects of hot-rolled raw materials were geneticed to the cold-rolled strip.The specific impact analysis for the profile of different hot-rolled raw materials to the dimensional accuracy of cold-rolled silicon steel was analyzed.As a result, the corresponding orderliness are given;And the strict control to section profile of the hot-rolled material is of great significance to ensure the dimensional ac...
电感耦合等离子体质谱法测定硅钢中痕量铜和镍
研究了应用电感耦合等离子体质谱法(ICP-MS)测定硅钢中痕量铜和镍的分析方法。采用硝酸分解样品,通过内标校正和基体匹配消除了基体干扰的影响,同时根据测量时存在的质谱干扰情况,选择同位素65Cu和60Ni作为测定元素和通过调节仪器参数使双电荷离子的产率最低,以减少带来的干扰。该方法用于硅钢中痕量铜和镍的测定,所得的结果与ICP-AES法测定结果完全吻合,各元素测定结果的RSD值小于5%,加标回收率为97.3%~100.3%。 A method for the determination trace copper and nickel in silicon steel by inductively coupled plasma mass spectrometry(ICP-MS) was studied.The samples were dissolved in HNO3.The effect of matrix interference was eliminated by internal standard correction and matrix matching.Meanwhile,according to the mass spectral interferences in determination,the isotopes including 65Cu and 60Ni were used as measuring elements.The yield of double-charge ions were minimized by adjusting instrumental parameters...
冷轧取向硅钢工程混凝土结构裂缝控制施工技术
冷轧取向硅钢工程中有很多的超长、大体积以及薄壁的混凝土结构,裂缝控制是土建施工的关键。在工程中,按照\"抗放兼施、先放后抗、以抗为主\"的原则,采用\"无缝分块跳仓法\",防止超长混凝土结构收缩产生裂缝;在隧道和池体的底板与墙板施工中,采用\"整体浇筑\"法,避免了墙板因约束应力而产生的裂缝。 In the Cold-rolled grain-oriented silicon steel project,there are many overlength,bulk mass,thin-walled concretes structures,how to control the crack is the key of civil engineering construction.In these projects,according to the principle of\"release with resist,resist before release,resist is dominant \",the crack of the over-long structure and shrinkage can be prevented by the method of\"seamless block skip bin \".In the construction of the bottom plate and wall of the tunnel and the pool,the cra...