电解清洗装置在电工钢生产线上的应用
介绍了电工钢生产线连退机组的表面处理工艺,特别是电解清洗系统的工作机理、设备构造、生产工艺及各种影响因素。 This paper introduces the technology of surface treatment of continuous annealing unit in electrical steel production line,in particular the working mechanism,structure of equipment,production techniques and various influence factors of the electrolytic cleaning system.
轧制力优化对20辊冷轧硅钢厚度精度的影响
轧制力是影响冷轧带钢厚度精度的关键因素。为实现高精度的冷轧带钢厚度控制,通过优化变形抗力模型参数和摩擦系数模型参数提高冷轧轧制力模型计算精度,并使用指数平滑法的自学习算法保证轧制力精度的稳定性。在首钢股份公司迁安钢铁公司20辊森基米尔轧机生产线进行S12硅钢钢种轧制力优化试验,将优化的模型参数应用于L2并投入现场生产,结果表明该优化方法不仅提高了轧制力设定精度,而且减小了冷轧硅钢的厚度超差长度,提高了成材率。 The rolling force is the key factor which influences the accuracy of cold-rolling strip thickness. To implement high precision control of cold-rolling strip thickness,we optimize the deformation resistance model parameters and friction coefficient model parameters to improve the calculation precision of cold-rolling force model,and use exponential smoothing self-learn algorithm to ensure the stability of rolling force accuracy. In Shougang Qiangang 20-high Sendzimir mill single stand production ...
我国冷轧无取向硅钢涂层专利技术分析
对1990~2010年在我国申请的冷轧无取向硅钢涂层的专利数量、专利技术领域分布进行了统计,对典型涂层专利技术进行了分析,探讨了无取向硅钢涂层的发展趋势。统计分析结果表明,目前无取向硅钢涂层典型的专利技术主要有自粘结涂层、无铬含稀土元素涂层、含钼酸盐环保涂层及采用有机-无机纳米杂化材料为主成膜物形成的涂层等。无取向硅钢涂层发展的趋势主要是无铬环保的半无机、半有机型涂层。 The patent quantity of cold-rolled non-oriented silicon steel coating and distribution of technology fields applied in China in 1990-2010 were summarized.The analysis results indicate that typical patent technologies include self-adhesion coating,chromium-free and with rare earth element coating,environment-friendly and with molybdate coating,coatings with organic-inorganic hybrid materials as main forming agent and so on.The main development trends of coatings on silicon steel are among semi-in...
新型无取向电工钢在退火过程中组织和织构取向的演变
通过金相分析和电子背散射衍射技术研究了一种新型含铜无取向电工钢在950℃退火不同时间(3~180s)空冷后的组织和织构取向的演变。结果表明:该钢在退火3s时的主要织构为α和γ线织构,{100}<110>织构最强;退火20s时织构以<111><112>、{111}<110>、{112}<110>、高斯织构和立方织构为主,随着退火时间的延长,高斯织构和立方织构强度呈减弱趋势;合理控制保温时间有利于提高{100}、{110}面织构的占有率。 Evolution of microstructure and texture oriented of a new non-oriented electrical steel during annealing at 950℃for different times(3-180) s and air cooling was studied by metallography and electron back-scattering diffraction analysis.The results show that after annealing for 3 s most of the texture oriented alongα-fibre andγ-fibre,the intensity of {100}〈110〉was the strongest.{111}〈112〉,{111}〈110〉,{112}〈110〉,Gauss texture and cube texture were the main texture after annealing for 20 s,with the ...
罩式炉常化工艺对热轧硅钢50W350组织和性能的影响
研究了罩式炉常化工艺对50W350硅钢热轧板组织、夹杂物和性能的影响。研究结果显示,罩式炉常化工艺在温度一定的情况下,随着保温时间延长,硅钢晶粒逐步再结晶并长大,同时析出物也在聚集长大。通过制定合理的罩式炉常化工艺,可以实现硅钢晶粒的再结晶和长大,从而达到连续退火炉常化工艺产品技术要求。 The influence of normalization process with a bell furnace on the structure,inclusions and properties of 50W350electrical steel hot-rolled sheet was studied.The research results showed that:when the steel was normalized at a certain temperature in the bell furnace,the silicon steel grains gradually recrystallized and grew up with the extension of the annealing holding time,and at the same time,the precipitates also gathered and grew up.The recrystallization and growth of the silicon steel grains...
基于人工神经网络-遗传算法的取向硅钢刻痕工艺优化
为了优化激光刻痕降低取向硅钢铁损的工艺,寻找刻痕速度、脉冲能量、扫描间距等重要刻痕参数的最佳匹配关系,提出了一种基于人工神经网络与遗传算法的优化模型,并利用这种模型对30Q130取向硅钢材料的刻痕工艺进行了优化实验,结果表明,这种模型稳定可靠,可以作为取向硅钢刻痕工艺优化的一种有效的措施。 A laser is often considered to scribe the grain-oriented silicon steel surfaces after cold-rolling and annealing to reduce the core loss.It is necessary to select the best scribing parameters to maximize the reduction in this process.This paper proposes an optimization method of genetic algorithm during laser scribing of 30Q130 steel,by developing an artificial neural network prediction model using a database form a designed orthogonal experiment.The objective is to determine the best combinatio...
浅谈无底层取向电工钢的多种应用
介绍了国内无底层取向电工钢生产技术水平、产量和用途,简述了无底层取向电工钢作为取向电工钢超/极薄带母料及应用于制作大型发电机组铁心、风电等电机铁心和变压器铁心等的情况。 The production technology level,output and application of domestic glassless grainoriented electrical steel were introduced,and the application of glassless grain-oriented electrical steel as parent material of ultra-thin strip of grain-oriented electrical steel and in making large-scale electric generator cores,wind power motor cores and transformer cores were briefly described.
无取向硅钢成品钢卷头、尾磁性能差异探讨
结合工业化生产过程中出现的同卷带钢头、尾磁性能差异现象,对50SW1300牌号无取向硅钢同卷带钢头、尾试样的夹杂物、晶体织构和显微组织进行了分析研究。结果表明,夹杂物、晶体织构是影响成品钢卷磁性能的重要因素。夹杂物是造成同卷带钢头、尾铁损差异的主要原因。夹杂物数量越多,尤其是小尺寸的夹杂物数量越多,对成品带钢的磁性能影响越大,对于本试验而言,AlN和MnS是影响成品带钢磁性能的主要夹杂物。晶体织构是造成同卷带钢头、尾磁感应强度差异的主要原因。有益的{100}和Goss织构含量越大,有害的{111}<110>和{111}<112>织构含量越小,即有益织构与有害织构含量比越大,成品带钢的磁感应强度越大。 Based on the industrial manufacture of non-oriented silicon steel sheets 50SW1300, the magnetic property variation of head and tail of the same finished steel sheets was discussed by analyzing non-metallic inclusion, crystal texture, and microstructure. Results show that, both of the non-metallic inclusion and the crystal texture will affect the magnetic properties significantly. The non-metallic inclusion is the key factor of the core loss variation of head and tail of the same finished steel s...
常化工艺对Si的质量分数为1.6%的无取向电工钢磁性能的影响
研究了常化温度、常化时间及常化后冷却速度对Si的质量分数为1.6%的无取向电工钢成品磁性能的影响。结果表明:在850~1 050℃范围内,随着常化温度的升高,成品铁损先减小后增大,成品磁感应强度先增大后减小;当常化温度为1 000℃时,成品平均铁损最低,平均磁感应强度最高;常化时间从3min延长到7min时,成品铁损先减小后增大,成品磁感应强度则呈单调下降趋势;随着常化冷却速度的降低,成品铁损先减小后增大,成品磁感应强度则呈单调增大趋势;对于Si的质量分数为1.6%的无取向电工钢,最佳的常化制度为:在1 000℃进行常化,时间5min,常化后空冷。对热轧板进行常化后,热轧板发生了不同程度的再结晶和晶粒长大。提高常化温度、延长常化时间、降低冷却速度,都能使常化板晶粒粗化,进而粗化成品板晶粒,改善磁性能。通过扫描电镜观察发现,成品板中析出物主要为AlN和MnS的复合析出物,以及少量的单独析出的AlN和MnS,而常化工艺主要是通过粗化析出相,减少细小析出相数量,从而减少对晶界钉扎作用来改善成品磁性能。 The effects of normalizing temperature,normalizing time and cooling rate after normalizing on magnetic properties of non-oriented electrical steel with mass fraction of Si of 1.6% were investigated.The results show that core loss of product decreases first and then increases,while magnetic induction increases first and then decreases with the increase of normalizing temperature from 850 to 1 050℃.Average core loss of product is the lowest and average magnetic induction is the highest when normal...
硼酸对无铬无取向硅钢涂层性能的影响
研究了硼酸对以Al(H2PO4)3为基料的无铬无取向硅钢绝缘涂层各项性能的影响。用盐雾实验、动电位极化及交流阻抗等试验手段研究了不同硼酸含量对硅钢绝缘涂层的耐蚀性和电化学行为的影响,同时采用SEM对涂层的表面形貌进行了研究。结果表明,硼酸含量为9.7%时,涂层的耐盐雾性及电化学性能最好;硼酸含量过少或过多时,涂层的耐蚀性和电化学性能都较差。 Influence of boric acid on the performance of chromium-free non-oriented silicon steel insulating coating based on aluminum dihydrogen phosphate was investigated.Salt spray experiment,potentiodynamic polarization and electrochemical impedance spectroscopy were used to study the influence of boric acid content on the corrosion resistance and electrochemical behavior of the insulation coating of silicon steel.Surface morphologies of the coatings were tested by SEM.Result shows that when the boric ...
高强无取向硅钢组织演变与强化机制
针对新能源汽车的发展,制备了含Ni固溶强化、含Cu析出强化以及含Ni+Cu复合强化3%Si无取向硅钢,研究了强化方式对无取向硅钢组织、织构和性能的影响。结果表明:固溶强化型无取向硅钢热轧板中形成了粗大{221}<221>晶粒,冷轧过程中剪切变形明显并在退火后形成良好再结晶织构。析出强化型无取向硅钢热轧板中心层形成γ取向粗大晶粒,在后续的加工中γ织构逐渐增强并最终得到相对细小的再结晶晶粒。复合强化型无取向硅钢热轧板中保留了强λ取向带状组织,退火后形成了有益的Goss织构和λ织构。固溶强化型与复合强化型无取向硅钢磁感应强度B50分别达到1.742、1.688 T,高于析出强化型无取向硅钢的1.645 T。同时,复合强化型无取向硅钢高频铁损最低,其P1.0/400和P1.0/1 000分别低至20.97、82.69 W/kg,这与其较小的晶粒尺寸和织构改善有关。强度计算结果表明:Ni元素固溶强化对强度的提高有限,屈服强度为468 MPa,纳米Cu析出可显著提高屈服强度(强度增量约200 MPa),且主要来自于模量强... For the development of new energy vehicles, 3%Si non-oriented silicon steel were processed by solid solution strengthening with Ni, precipitation strengthening with Cu, and composite strengthening with Ni and Cu. The effects of different strengthening methods on the microstructure, texture and properties of high-strength non oriented silicon steel were studied.The results show that coarse {221}<221> grains are formed in the hot rolled sheet of solution strengthened non-oriented silicon ste...