研究了冷轧大压下量,950℃退火时间对一种新型含铜无取向电工钢晶粒度和织构的影响。结果表明,大压下量冷轧,随压下量的增加,退火晶粒向γ线聚集,形成强{111}<112>织构。提高冷轧压下率,退火织构{111}<100>,{110}<001>强度减弱,增加退火时间,退火织构{111}<110>,{100}<001>,{110}<001>强度变弱。采用87.5%冷轧压下率和950℃退火60 s,有利织构{100},{110}占有率最大。 The effect of annealing(950 ℃) time with high cold rolling reduction on grain size and texture of a new non-oriented electrical steel containing copper was investigated.The results show that for high cold rolling reduction,most annealed grains are oriented along γ-fibre with increasing cold rolling reduction ratio and strong texture {111}<112> is formed.With increasing the cold rolling reduction ratio,the intensity of annealed texture {111}<110>,{011}<100> decreases.With increa... 
2011-01-28 157 5.8

为探究铬、锰元素及退火温度对高强无取向硅钢性能的影响规律,借助OM、SEM、EBSD与万能拉伸试验机等分析不同制造工艺下3组不同含量铬、锰元素的无取向硅钢热轧、常化及退火处理后组织与性能。结果表明,试验钢热轧后组织不均匀,心部为沿轧向分布纤维状组织,边部为少量再结晶晶粒,常化处理能显著改善热轧板组织均匀性,消除热轧板中心部位的纤维状组织。经冷轧及退火后得到多边形铁素体晶粒,其中960℃退火,晶粒尺寸偏大,有利织构{100}组分体积分数减少,不利织构{111}组分体积分数增加,成分为0.2Mn-1Cr的1号试验钢960℃退火后铁损最大,磁感强度偏小;成分为0.5Mn-1Cr的2号试验钢930℃退火后,磁性能与强度等综合性能最佳,工频铁损P1.5/50为2.41W/kg,高频铁损P1.0/400为17.36W/kg,磁感应强度B5 000为1.638T,抗拉强度为685MPa。 In order to study the effect of Cr,Mn and annealing temperature on the properties of high-strength non-oriented silicon steel,the microstructure and properties of three groups of non-oriented silicon steel with different Cr,Mn content under different manufacturing processes were analyzed by means of OM,SEM,EBSD and universal tensile tester.The results show that the structure of experimental steel is not uniform after hot rolling,and the core is distributed in fibrous structure along the rolling ... 
2020-05-28 166 5.8

采用铸坯低倍组织检验和化学分析的方法,研究板坯连铸机二冷区电磁搅拌器电流和频率参数对无取向电工钢XG800WR板坯中心偏析和等轴晶率的影响,结果表明:铸坯等轴晶率随着搅拌器电流强度和电流频率的增大而增加。采用二冷区电磁搅拌可减小中心易偏析元素S的偏析,试验得出:减小铸坯S偏析效果最好的电磁搅拌参数为电流380~400A,频率6Hz。 The effect of electromagnetic stirring current and frequency parameter at secondary cooling area on the central segregation and equiaxed crystal ratio of XG800WR non - oriented electrical steels slab was investigated through the methods of chemical and macrostructure analysis.The results shows that the rate of equiaxed crystal zone is going up with increasing of current intensity and current frequency.Electromagnetic stirring in the secondary cooling area can be easily reduced segregation caused... 
2011-01-28 166 5.8

采用Nb对Fe-6.5%Si(质量分数)高硅钢进行微合金化处理,结果表明:Nb在高硅钢薄板制备过程中细晶效果明显.铸态、锻态和热轧态组织的晶粒分别细化了17.50%,24.51%和30.13%.铸态样品压缩强度由1365 MPa提高至1520 MPa,延伸率提高77.78%;温轧板试样室温拉伸强度由573 MPa提高至621 MPa,延伸率提高44.44%.利用XRD对厚度为0.30—1.68 mm的温轧板的板面织构演变过程进行跟踪测量,结果发现:初始织构以(011)〈100〉Goss织构为主,单道次变形量为26.2%的情况下,Goss织构完全转化为(100)〈011〉旋转立方织构,随后,在单道次变形为22.6%的情况下,旋转立方织构完全转化为{111}面织构,即纤维织构,并稳定保持至0.30 mm. Fe-6.5%Si(mass fraction) alloy possess perfect magnetic properties,though intermetallics of Fe14Si2 phase brought 6.5%Si leads to room temperature brittleness and hinder this significant materials industrialization.Nb was adopted into micro-alloying of Fe-6.5%Si high silicon steel. OM,thermal simulated test machine and XRD were employed to study the influence of Nb on high silicon steel in processing stages.Textures of warm-rolled high silicon steel strips were determined b... 
2013-11-28 144 5.8

为进行磷酸盐系无铬无取向硅钢涂层烧结固化工艺研究,首先对磷酸盐系无铬无取向硅钢涂层进行热重-差示扫描量热(TG-DSC)分析;然后在不同烧结固化温度条件下,测定涂层板温随时间变化曲线;最终获得涂层烧结固化温度与时间(T-t)工艺曲线。通过中性盐雾试验、动电位极化、交流阻抗、涂层附着力以及扫描电子显微镜(SEM)和能谱(EDS)分析验证。结果表明,根据涂层烧结固化温度与时间(T-t)工艺曲线制备的涂层结构致密、性能优异,证明该工艺曲线具有合理性与正确性。 In order to study the curing process of chromium-free non-oriented silicon steel coatings,phosphatic chromium-free non-oriented silicon steel insulating coating was prepared and TG-DSC analysis of the coating was conducted,then the change of the actual temperature of the coated non-oriented silicon steel sheet with time at different curing temperatures was studied. Based on the experiments,the processing curves of curing temperature vs. curing time( T-t) for the chromium-free non-oriented silico... 
2013-12-28 137 5.8

抑制回硅是低硅品种钢冶炼的重点和难点,南钢中厚板卷厂通过转炉出钢弱脱氧操作,精炼炉弱脱氧升温,脱氧、脱硫造渣,连铸严格的保护浇注及吹氩塞棒、吹氩浸入式上水口的应用等一系列工艺优化和操作的改进,使整个冶炼过程钢水回硅量稳定控制在200×10-6以内,钢水终点成分完全满足低硅钢要求。 Control of increasing silicon is the emphasis and difficulty in low silicon varieties steel smelting.The Nisco Wide Plate/Coil Plant can control the silicon content in molten steel keeping within 200×10-6 through whole steelmaking process by using oxygen residual operation in converter tapping,oxygen residual and increasing temperature,deoxidation,desulfurization,slag refining,protection cast,blowing argon by plugged nozzle,blowing argon by submerged entry nozzle in continuous casting,and other ... 
2013-05-28 123 5.8

利用X-射线衍射织构分析和线形分析技术测定了交叉轧制双取向硅钢在制备工艺各阶段的织构及微结构,进而探讨了立方织构({100}<001>)的形成过程。通过对实验结果的分析可知,二次冷轧和交叉轧制工艺为立方织构提供了内能优势和有利的形变织构,而低温预退火工艺既强化了立方织构的内能优势,又为立方织构的异常长大提供了有利的组织保证,最终在抑制剂(AlN和MnS)的协同作用下,硅钢在二次再结晶退火后形成了强烈的立方织构。 The texture and substructure of the double oriented electrical steels produced by the cross rolling technology during the difference process has been measured by means of the X-ray texture and diffraction peak profile analysis technology,and research the formation mechanism of cube texture,{100}<001>.The results show that the dominances of inner energy and deformation texture were supplied by secondary cold rolling and the cross rolling technology and strengthened by pre-annealing at a low... 
2011-02-28 157 5.8

基于BOF→RH→CSP生产工艺,研究了RH精炼过程钢中夹杂物类型演变及MgO·Al2O3夹杂物形成规律,同时对MgO·Al2O3夹杂物的形成条件进行了热力学计算,借助CFD数值模拟软件研究了RH精炼过程卷渣行为。研究发现,RH精炼过程20和30 min时,w([MgO])/w([Al2O3])为0.005~0.020,未发现MgO·Al2O3夹杂物;RH出站后夹杂物w([MgO])/w([Al2O3])为0.3~0.5,且RH精炼结束后MgO·Al2O3夹杂物占夹杂物总量的58.4%;另外,RH精炼过程钢液表面速度CFD模拟结果为0.57 m/s,大于临界卷渣速度0.45 m/s,且顶渣成分与夹杂物成分相近,存在卷渣现象。热力学计算表明,钢液与炉渣平衡时钢中w([Al])为0.31%~0.37%,w([Mg])为0.00024%~0.00028%,在MgO·Al2O3生成区域之内。减少RH处理过程卷渣,浇铸过程下渣及控制顶渣和包衬相中MgO质量分数可抑制MgO·Al2O3夹杂物形成。 Based on the practical production of non-oriented silicon steel, the evolution of inclusion type and the formation of MgO·Al2O3inclusion were analyzed in the process of BOF→RH→CSP. The thermodynamic conditions for forming MgO·Al2O3inclusion were discussed and the behavior of slag entrapment of molten steel was also simulated by CFD software during RH refining. The results showed that the value of w([MgO])/w([Al2O3]) was in the range of 0.005-0.020 and no MgO · Al2O3 inclusion was observed at 20 ... 
2014-09-28 158 5.8

采用取向分布函数分析了无取向电工钢不同再结晶退火温度下的织构变化及织构对磁感应强度和铁损的影响,并计算了无取向电工钢的磁晶各向异性能。结果表明,随着实验钢的再结晶退火温度升高,Goss织构和立方织构组分显著增强,而{111}面织构强度却减弱。较高的退火温度有利于减小织构因子,提高磁感应强度。磁晶各向异性能计算结果显示,随着再结晶退火温度升高,无取向电工钢板的磁晶各向异性能降低。 The recrystallization texture and the relationship of texture to magnetic induction intensity and core loss of a non-oriented electrical steel were investigated by orientation distribution function analysis. The magnetic anisotropy energy of the steel was calculated also. The results show that,the intensity of Goss texture and cubic texture increases,but the intensity of { 111} texture decreases with increasing recrystallization annealing temperatures of the steel. The higher annealing temperatu... 
2014-02-28 165 5.8

文章以国内某公司硅钢厂连续退火机组1号辐射管加热段为研究对象,分析炉内传热机理,建立并开发了辐射管加热段的传热模型。采用生产实际数据对模型进行了验证,以总燃料消耗量最小为目标,得出该炉段长度方向上燃料的最佳分配机制。所得结论为该公司连续退火机组节能控制提供理论依据。 Taking the radiant tube heating section of No.1 continuous annealing unit in a silicon steel plant of a domestic company as the research object, the heat transfer mechanism in the furnace is analyzed, and the heat transfer model of the radiant tube heating section is established and developed. The model is verified by the actual production data. Aiming at the minimum total fuel consumption, the optimal fuel distribution mechanism in the length direction of the furnace section is obtained. The co... 
2022-01-28 126 5.8

借助OM、激光共聚焦显微镜、质谱仪和电解萃取等设备和方法,研究了添加微量稀土La(质量分数0.001 1%)的取向硅钢在轧制前采用不同加热保温时间对抑制剂固溶行为的影响。结果表明:当稀土取向硅钢在1 250℃分别保温10、20、30 min后,试验钢晶粒尺寸随保温时间延长有先快后慢的长大趋势;三种抑制剂元素Mn、Cu和Al均发生固溶,保温时间对Mn和Cu两种元素的固溶影响明显,固溶量分别由69.8%和43.7%增加至84.2%和85.2%;随着保温时间的延长,稀土取向硅钢中抑制剂的小尺寸未溶物逐渐减少直至消失,较大尺寸未溶物(300~600 nm)逐渐转变为小尺寸未溶物逐步溶入基体中,数量减少且未溶物的类型由复杂逐渐转变为单一。 In this paper the solid solution behavior of the inhibitor under various holding time in 0.001 1 %La oriented silicon steel during reheating had been investigated by using OM, LM, methods of electrolytic extraction and mass spectrometer. The results showed that grain size of the test steel increased significantly with the holding time prolonging when the rare earth oriented silicon steel was heated to1 250 ℃ and held for 10, 20 min and 30 min respectively, and the growth trend slowed down after ... 
2022-02-28 154 5.8

【作者】 陈迪安; 李春生; ...
2023-05-09 178 5.8