晶界位向对硅钢立方/旋转立方取向双晶轧制取向变化的影响
晶界和{100}柱状晶在硅钢生产过程中对织构的遗传和演变有关键作用,因此本文利用晶体塑性有限元方法进行立方和旋转立方取向双晶在晶界不同位向时晶体取向演变的全场模拟。模拟显示,三种晶界位向下,晶界都具有诱发晶内产生S形状形变不均匀和缓解局部形变不均匀区取向转动的特点,立方和旋转立方取向双晶在带有剪切作用的轧制条件下都显示明显的取向稳定性。GB⊥RD(表示晶界垂直于轧向)晶界位向时,旋转立方取向晶粒优先在晶界中心位置发生取向转动,而立方取向则优先在远离晶界的端部发生取向转动。GB⊥TD(表示晶界垂直于横向)的晶界位向下,其晶界阻碍作用最小,双晶内产生的取向漫散度大,织构强度较低;除绕TD转动外,也具有复杂的绕RD、ND的取向转动。GB⊥ND(表示晶界垂直于法向)的晶界位向下,取向转动与GB⊥RD时相近,但有少量取向绕ND转动。 Grain boundaries and initial{100}columnar grains play a key role in the inheritance and evolution of texture in the production of electrical steels.In this paper,the crystal plasticity finite element method was used to simulate the grain orientation evolution of cube and rotated-cube oriented bicrystals when grain boundary was set to different orientations.It was shown that the grain boundary in three grain boundary orientations demonstrated the characteristics of inducing Sshape deformation inh...
薄板坯连铸连轧生产中低牌号无取向硅钢的实践
本文中简要介绍了武汉钢铁有限公司采用薄板坯连铸连轧CSP(compact strip production, CSP)工艺生产中低牌号无取向硅钢的实践情况.CSP工艺生产的硅钢具有成品磁性均匀、板形好的优势,但是在利用该技术生产中低牌号无取向硅钢时,常存在成品板表面瓦楞状缺陷严重、连铸生产效率低等问题.通过优化炼钢成分、热轧等相关工艺,可消除热轧板厚度方向中心的粗大形变组织,从源头上避免了粗大{100}<011>纤维组织的出现,消除了瓦楞状缺陷;通过提升冶炼效率和控制钢中夹杂物总量,可优化隧道炉的加热温度与在炉时间,大幅度提升了连铸生产效率,实现了中低牌号无取向硅钢的批量稳定制造,使CSP产线成为中低牌号无取向硅钢热轧板原料的主要供给生产线.如何进一步提升钢水纯洁度、提高连铸生产效率、降低生产成本,以及挖掘该产线生产薄带钢的技术优点,是未来工作的重点. This paper briefly introduces the practice of producing medium and low grade non oriented silicon steel(NGO) with CSP(compact strip production, CSP)technology in Wuhan Iron and Steel Co., Ltd.. This technology has the inherent advantages of uniform magnetic properties and good shape for silicon steel finished strip. However, in the actual production process, there are serious corrugated defects on the surface of silicon steel finished strip, and production efficiency of continuous casting is low...
树脂含量对半无机型无铬无取向硅钢涂层性能的影响
本文研究了丙烯酸树脂含量对以Al(H2PO4)3为基料的无铬无取向硅钢绝缘涂层各项性能的影响.用盐雾实验、动电位极化及交流阻抗等试验手段研究了不同树脂含量对硅钢绝缘涂层的耐盐雾性能和电化学行为的影响,同时采用SEM对涂层的表面形貌和附着性进行研究.结果表明,树脂含量为19.9~29.4%时,涂层的耐蚀性和附着性最好;树脂含量过多时,涂层的耐蚀性和附着性均较差. This paper studies the influence of acrylic resin on the performance of insulating coating of aluminum dihydrogen phosphate on chromium-free non-oriented silicon steel.Salt spray experiment,potentiodynamic polarization and electrochemical impedance spectroscopy were used to study the influence of acrylic resin content on the salt spray resistance and electrochemical behavior of the insulation coating of nonoriented silicon steel.The surface morphologys and adhesion of coating were tested by SEM....
钇元素对6.5%Si无取向硅钢组织、高温拉伸及断裂机制的影响
通过微观组织表征、高温拉伸和断口形貌分析,研究了钇(Y)元素对6.5%Si无取向硅钢组织、高温拉伸及断裂机制的影响。研究结果表明,添加Y元素可以在钢液中形成YS和YP的复合析出。YS和YP可以充当异质形核基底,提高形核率,细化凝固组织。热轧组织不均匀,由表层至芯部分别形成等轴晶、等轴晶/拉长晶和拉长晶的混合组织。退火后,热轧变形组织转变为等轴晶,含Y实验钢的退火组织得到明显细化。500℃时效处理后,含Y实验钢具备较低的有序度,300℃的拉伸断口呈现韧性断裂特征,断后伸长率达到20.2%。相反,无Y实验钢发生脆性断裂,断后伸长率仅为2.1%。研究结果证实,Y元素可以通过组织细化和降低有序度提高6.5%Si无取向硅钢的中温塑性。 The effects of yttrium(Y)on microstructure,elevated-temperature tensile properties and fracture mechanism of 6.5% Si non-oriented electrical steel were investigated by means of microstructure characterization,high-temperature tensile test and fracture analysis.The results showed that the doping of Y introduced composite Y-rich precipitates(YS/YP)in the melt.YS and YP precipitates were qualified for heterogeneous nucleation agents,which thus raised the nucleation rate and refined the solidificati...
压下率对6.5%Si电工钢温轧板织构的影响规律
6.5%Si电工钢是一种优异的软磁材料,织构对其磁性能影响很大。利用温轧工艺对6.5%Si电工钢热轧板进行不同压下率轧制,研究了温轧板织构随压下率的变化规律。实验结果显示,随着压下率的增大,{100}〈110〉、{110}〈100〉和γ纤维织构在薄板表层中的强度先增强后减弱,当压下率达到75%时,沿板厚方向形成3个组织区域:表层细晶粒区({110}〈100〉取向为主)、过渡层({111}〈110〉和{111}〈112〉变形晶粒区)和中心层(以拉长的γ纤维织构和{100}〈110〉取向晶粒为主),这种组织和织构不均性对后期织构的发展有重大影响。 6.5wt% Si electric steel has excellent soft magnetic properties,on which texture play important role.In this experiment,warm rolling technique was employed to investigate the effect of rolling reduction on texture.It was found that the density of {100}〈110〉,{110}〈100〉 and γ-fiber textures first increased and then decreased with increasing of the rolling reduction.At 75% reduction,the microstructure along the thickness of the sheet formed three zones,containing surface layer with {110}〈100〉 orien...
热变形温度对3%SiCGO硅钢组织和织构的影响
通过对3%Si CGO硅钢进行恒变形速率、不同变形温度下的单道次压缩实验,结合Thermal-Calc软件,金相分析,SEM及EBSD技术,研究了取向硅钢热变形过程中组织和微观织构的变化规律。结果表明:实验钢是在双相区变形,变形后组织主要是铁素体和少量的珠光体。随变形温度的升高,晶粒由长条状变为等轴状,尺寸逐渐变大;CGO硅钢在热变形过程中立方{100}<001>取向是较为稳定存在的。随着变形温度的提高,{111}<110>等取向逐渐转向{110}<1 10>取向,且{110}<1 10>取向逐渐变得锋锐。 3% Si CGO silicon steel was studied at constant strain rate and different deformation temperatures by single-pass compression deformation experiments to reveal the evolution of microstructure and texture during thermal deformation in oriented silicon steel,and the Thermal-Calc software,metallurgical,SEM and EBSD technique was used in the experiment. The results show that experimental steel is deformed at the temperatures of two-phase zone. The microstructure of the deformed steel consists of fer...
冷轧无取向电工钢的试制
利用本钢技术中心试验厂技术手段,并与北京钢铁研究院合作,试制了用作家电用电机、微电机、小电机或部分中型电机铁芯的冷轧无取向电工钢。试制钢硅含量小于0.5%,钢板表面平滑,公称厚度0.5mm,且厚度均匀偏差小,性能测定结果表明,产品的磁性能、力学性能满足其使用要求。 BX STEELTechnology Center pilot plant using technical means,and with Beijing Iron and Steel Research Institute,trial cold rolled non-oriented electrical steel that has been used as appliance motor core,micro motor core,small motor core,or part of the medium-sized motor core。Trial steel of silicon content is less than 0.5%,steel plate surface is smooth,the nominal thickness of 0.5mm,and the thickness deviation is small,performance measurement results show that the magnetic properties,mechanical p...
冷轧无取向硅钢横向厚差控制
冷轧中中低牌号的无取向硅钢多采用万能凸度轧机(Universal crown mill,UCM)生产,其板形好坏受制于UCM轧机板形调节手段的协调使用。为掌握UCM轧机的板形控制特点,建立基于二维变厚度有限元的辊系弹性变形和基于三维差分的轧件塑性变形的六辊轧机耦合模型,对UCM轧机的板形调控性能进行详尽的分析,包括工作辊和中间辊弯辊、中间辊窜辊的调控功效、辊间接触压力分布等。在此基础上,提出可用指导生产的板形控制策略,指出UCM轧机在横向厚差控制方面的不足。针对工业生产中UCM轧机轧制无取向硅钢横向厚差大的问题,在大量仿真计算的基础上,开发具有高次曲线函数的边部变凸度(Edge variable crown,EVC)的工作辊。采用该工作辊后,各种品种的无取向硅钢的横向厚差不大于10μm的百分比由24%提高到99%,横向厚差的均值小于6μm,远小于之前的13μm。 Medium-low grade non-oriented silicon steel is rolled often by universal crown mill(UCM) during cold rolling.Its shape quality is dependent on the coordinated control of several shape adjustment devices of UCM.In order to understand the shape control characteristics of UCM,coupling model of six-high rolling mill,based on two-dimensional varying thickness finite element rolls elastic deformation model and three-dimensional finite difference strip plastic deformation model,is setup for the detaile...
稀土在无取向电工钢中应用的研究进展
稀土元素在许多钢中发挥着独特而且不可替代的重要作用。半个世纪以来,它的作用已经在各种低合金和特殊合金钢中的研究及应用中得到充分的证明;然而,作为具有稀土资源优势的中国,在属于重要功能材料的无取向电工钢中稀土的应用却落后于国外,本文就中国稀土在无取向电工钢中的应用研究作简要的评述,希望能够进一步推进此领域的研究,并且促进中国稀土在无取向电工钢中应用技术的发展,缩短与国外差距,并提出了在此应用领域今后需深入开展的研究方向。 Rare earth elements play a unique and irreplaceable role in a lot of steels,it has given the full proof by the practice of various low alloy steels and special alloy steels since half century.However,as our country has the advantage of rare earth resources,RE application technology in non-oriented electrical steels has lagged behind abroad.The application researches of rare earth in non-oriented electrical steel in our country are briefly reviewed in this paper,which hope to promote the research...
冷轧大压下量下新型无取向电工钢的退火组织演变
研究了冷轧大压下量,950℃退火时间对一种新型含铜无取向电工钢晶粒度和织构的影响。结果表明,大压下量冷轧,随压下量的增加,退火晶粒向γ线聚集,形成强{111}<112>织构。提高冷轧压下率,退火织构{111}<100>,{110}<001>强度减弱,增加退火时间,退火织构{111}<110>,{100}<001>,{110}<001>强度变弱。采用87.5%冷轧压下率和950℃退火60 s,有利织构{100},{110}占有率最大。 The effect of annealing(950 ℃) time with high cold rolling reduction on grain size and texture of a new non-oriented electrical steel containing copper was investigated.The results show that for high cold rolling reduction,most annealed grains are oriented along γ-fibre with increasing cold rolling reduction ratio and strong texture {111}<112> is formed.With increasing the cold rolling reduction ratio,the intensity of annealed texture {111}<110>,{011}<100> decreases.With increa...
硅钢脱硫影响因素分析研究
对RH法(真空循环脱气法)生产的冷轧硅钢的脱硫原理及影响因素进行了分析研究。研究表明:降低顶渣中FeO、MnO的含量,提高钢液温度,增加脱硫剂的加入量并延长其循环时间有利于提高脱硫效率。 The principles of desulfurization and its influence factors of cold rolling silicon steel during RH process have been studied in this paper.The result indicated that reducing contents of FeO and MnO,rising temperature of the liquid steel,increasing quantity of desulfurizer,lengthening cycle time of desulfurzer are benefit for desulfurization.