针对硅钢连续退火机组的主要能源介质消耗现状,对现有生产工艺和设备研究采取机组循环用水、增加清洗段漂洗级数等措施可节约大概27 m3/h的过滤水量,并可减少78%的弱碱处理量;将炉子烟气换热系统增加一级余热回收,每年回收的余热相当于583 t标煤消耗,可节约蒸汽5 368 t。 The present situation of energy consumption for silicon steel annealing line is analyzed in this paper.In existing process and equipment conditions,increasing the number of cleaning series will lead to a saving of about 27 m3/h of filter water and reduce 78 % of weak base processing volume.For the flue gas heat-exchange system,adding a waste heat recovery device will recover waste heat equivalent to 583 tons of standard coal per year,corresponding to a saving of steam 5 368 t per year. 
2011-05-28 158 5.8

广泛应用于电子电力行业的取向硅钢材料的磁性能与其晶体取向密切关联,对取向硅钢晶体衍射花样的研究非常重要.采用理论计算的方式研究了取向硅钢的晶体衍射花样特征,并绘制了取向硅钢的高斯织构理论极图、理论单晶透射电子衍射斑点花样和理论电子背散射衍射(Electron backscatter diffraction, EBSD)菊池花样.取向硅钢理论单晶衍射花样不仅可以为以后标定样品实测晶体衍射花样提供一种简单快捷的方法,也可以为样品检测提供一种标准.这种研究方法不仅限于取向硅钢,也被期待应用于其他材料晶体衍射花样研究. The magnetic properties of oriented silicon steels which are widely used in electronic and power industries are closely related to their crystal orientations, so it is very important to study the crystal diffraction patterns of oriented silicon steels. The characteristics of crystal diffraction patterns of oriented silicon steels are studied by means of theoretical calculation. The theoretical pole figures, theoretical single crystal transmitted electron diffraction patterns and theoretical elec... 
2022-03-28 180 5.8

介绍了双蓄热燃烧技术的特点和高温硅钢加热炉的特点,探讨了双蓄热燃烧技术在高温硅钢加热炉中使用的技术难点,分析了双蓄热燃烧技术在高温硅钢加热炉上使用的可能性。 Introduced characteristics of double regenerative combustion technology and high temperature silicon steel reheating furnace,discussed technical difficulties for using double regenerative combustion technology,analyzed the possibility of double regenerative combustion technology applied to high temperature silicon steel reheating furnace. 
2013-03-28 122 5.8

采用RH精炼添加钙合金方式对硅钢进行钙处理,结果表明,钙合金添加量为0.67、1.00和1.67 kg/t钢时,钢中Ca含量分别为0、2×10-6和4×10-(6质量分数);随着钙合金添加量的增加,钢中夹杂物粒度逐渐由0~2μm向2~4μm、4~6μm偏移;不同钙处理条件下,钢中均存在粒径小于1μm和粒径为1~5μm的MnS、CuxS夹杂物,后者或单独存在,或与AlN、CaS夹杂复合;钢中粒径为5~10μm的夹杂物基本以Ca的氧化物和硫化物为主。与未经钙处理的炉次相比,钙合金添加量为0.67、1.00和1.67 kg/t钢时,粒径小于1.0μm的夹杂物减少幅度分别为68.06%、87.50%和94.94%。钙合金添加量为1.67 kg/t钢时,可以去除钢中绝大部分的微细夹杂物。 In order to improve the properties of final silicon steels,the calcium treatment was adopted by adding Ca alloys into the liquid steel during the RH refining process.Results show that when the addition of Ca alloys is 0.67 kg/t,1.00 kg/t and 1.67 kg/t,the corresponding Ca content in silicon steels is 0,2 × 10-6 and 4 × 10-6 respectively.With the increase of Ca alloy addition,the particle sizes of inclusions in steels become 2~4 μm and 4~6 μm,from 0~2 μm.Under different calcium treatments,there e... 
2013-02-28 184 5.8

森吉米尔二十辊轧机是冷轧电工钢的主要机型,具有整体刚度大,辊径小,轧制道次压下量大,产品精度高等特点,简要介绍了近年来冷轧电工钢森吉米尔二十辊轧机领域进展,在轧机结构、厚度自动控制、板形自动控制等方面的技术及研究。 20-h Sendzmir reversible mill is the main type of cold rolled electrical steel which has the characteristic of high integral stiffness,small roller diameter,high pass reduction and high product quality.In this paper,the recent progress of frame structure,automatic gauge control,automatic flatness control of Sendzmir mill is introduced. 
2023-05-06 220 5.8

【作者】 姚昌国; ...
2011-05-28 151 5.8

介绍了普通取向硅钢(CGO)和高磁感取向硅钢(Hi-B)铸坯高温加热两次冷轧、一次冷轧和铸坯低温加热两次冷轧、一次冷轧法4种成熟生产工艺的主要技术参数,取向硅钢理论研究(Goss晶核和抑制剂)和生产技术现状。取向钢的发展趋势为:提高(110)[001]晶粒取向度,降低取向硅钢铁损,发展铸坯低温加热(≤1 300℃)和薄板坯连铸连轧流程生产取向硅钢工艺。 Main technology parameters of four developed process:cast bloom higher temperature heating-double cold rolling or single cold rolling,lower temperature heating-double cold rolling or single rolling process for production of common grain oriented silicon steel(CGO) and high magnetic induction grain oriented silicon steel(Hi-B),theory research on grain oriented steel(Goss nucleus and inhibitor) and present situation of process are summarized in this paper.The development trend of grain oriented si... 
2013-05-28 166 5.8

【作者】 张煜; 朱国辉; ...
2013-03-28 142 5.8

试验研究了0.3 mm取向硅钢冷轧板(/%:0.046C,3.07Si,0.09Mn,0.029P,0.004S,0.005A1)的退火温度(760~880℃7 min)和退火时间(820℃3~9 min)对该钢的晶粒尺寸,再结晶和织构的影响。结果表明,最佳初次再结晶退火工艺为820℃5 min,该钢的平均晶粒尺寸为14.20μm,完全再结晶率为92%,不利{111}<110>结构含量为3.16%,有利织构{111}<112>,{012}<001>和高斯织构含量分别0.40%,4.73%和2.46%。 The effect of annealing temperature(at 760 ~ 880 X.for 7 min) and time(at 820℃ for 3~9 min) on grain size,recrystallization rate and texture of 0.3 mm cold-rolled sheet of oriented silicon steel(/%:0.046C,3.07Si,0.09Mn,0.029P,0.004S,0.005Al) has been tested and studied.Results show that with optimum recrystallized annealing at 820℃ for 5 min,the silicon steel average grain size is 14.20 fun,the complete recrystaUization rate is 92%,the unfavourable-texture {111}< 110 > content in steel is ... 
2014-03-28 142 5.8

冷轧中中低牌号的无取向硅钢多采用万能凸度轧机(Universal crown mill,UCM)生产,其板形好坏受制于UCM轧机板形调节手段的协调使用。为掌握UCM轧机的板形控制特点,建立基于二维变厚度有限元的辊系弹性变形和基于三维差分的轧件塑性变形的六辊轧机耦合模型,对UCM轧机的板形调控性能进行详尽的分析,包括工作辊和中间辊弯辊、中间辊窜辊的调控功效、辊间接触压力分布等。在此基础上,提出可用指导生产的板形控制策略,指出UCM轧机在横向厚差控制方面的不足。针对工业生产中UCM轧机轧制无取向硅钢横向厚差大的问题,在大量仿真计算的基础上,开发具有高次曲线函数的边部变凸度(Edge variable crown,EVC)的工作辊。采用该工作辊后,各种品种的无取向硅钢的横向厚差不大于10μm的百分比由24%提高到99%,横向厚差的均值小于6μm,远小于之前的13μm。 Medium-low grade non-oriented silicon steel is rolled often by universal crown mill(UCM) during cold rolling.Its shape quality is dependent on the coordinated control of several shape adjustment devices of UCM.In order to understand the shape control characteristics of UCM,coupling model of six-high rolling mill,based on two-dimensional varying thickness finite element rolls elastic deformation model and three-dimensional finite difference strip plastic deformation model,is setup for the detaile... 
2011-10-28 157 5.8

6.5%Si电工钢是一种优异的软磁材料,织构对其磁性能影响很大。利用温轧工艺对6.5%Si电工钢热轧板进行不同压下率轧制,研究了温轧板织构随压下率的变化规律。实验结果显示,随着压下率的增大,{100}〈110〉、{110}〈100〉和γ纤维织构在薄板表层中的强度先增强后减弱,当压下率达到75%时,沿板厚方向形成3个组织区域:表层细晶粒区({110}〈100〉取向为主)、过渡层({111}〈110〉和{111}〈112〉变形晶粒区)和中心层(以拉长的γ纤维织构和{100}〈110〉取向晶粒为主),这种组织和织构不均性对后期织构的发展有重大影响。 6.5wt% Si electric steel has excellent soft magnetic properties,on which texture play important role.In this experiment,warm rolling technique was employed to investigate the effect of rolling reduction on texture.It was found that the density of {100}〈110〉,{110}〈100〉 and γ-fiber textures first increased and then decreased with increasing of the rolling reduction.At 75% reduction,the microstructure along the thickness of the sheet formed three zones,containing surface layer with {110}〈100〉 orien... 
2023-05-09 218 5.8

冷轧无取向硅钢(/%:0.003C,2.35Si,0.22Mn,0.011P,0.002S,0.36A1,0.003 0N)经890℃或940℃3 min常化的2.3 mm热轧板冷轧成0.35 mm薄板。研究了常化温度和800920℃3 min退火对该钢高频(400Hz)磁性能和抗拉强度的影响。结果表明,830920℃退火时高频铁损P10/400值最低,随退火温度增加,晶粒尺寸增大,钢的抗拉强度降低;该钢的最佳热处理工艺为常化温度940℃,退火温度830℃,其抗拉强度Rm、高频铁损P10/400和磁感应强度J50分别为565 MPa,21.5 W/kg和1.69 T。 The cold-rolled non-oriented silicon steel(/%:0.003C,2.35Si,0.22Mn,0.011P,0.002S,0.36A1,0.003 0N) is cold-rolled to 0.35 mm sheet from 2.3 mm hot-rolled plate normalized at 890 ℃ or 940℃ for 3 min.The effect of normalizing temperature and annealing process at 800 920 °C for 3 min on high frequency(400 Hz) magnetic properties and tensile strength of the steel has been tested and studied.Results show that with annealing at 830 920 ℃the high frequency iron loss value P10... 
2014-03-28 156 5.8