钢厂
基于GTN损伤模型对含边部缺陷硅钢薄板冷轧时边裂的预测
采用拉伸试验和显微组织观测的方法确定了GTN损伤模型中的9个损伤参数,运用GTN损伤模型对冷轧硅钢薄板边部缺陷的扩展及边裂的产生进行了有限元模拟,并与预置缺口的钢板轧制试验进行对比。结果表明:轧制过程中边部缺陷是造成钢板边部裂纹萌生和扩展的一个重要原因,GTN损伤模型可用来预测含边部缺陷硅钢薄板在冷轧过程中边裂的产生;预测结果与试验结果基本一致。 The crack initiation and propagation of silicon steel strip with edge defect during cold rolling process was studied by using GTN damage model in this paper.Nine damage parameters in GTN model were identified by tensile testing and microstructure observing,and then the FE simulation of edge defect evolution of silicon steel strip during rolling process was conducted on the base of GTN damage model,and then the results were compared with rolling experimental results.The results show that the edge...
轧制力优化对20辊冷轧硅钢厚度精度的影响
轧制力是影响冷轧带钢厚度精度的关键因素。为实现高精度的冷轧带钢厚度控制,通过优化变形抗力模型参数和摩擦系数模型参数提高冷轧轧制力模型计算精度,并使用指数平滑法的自学习算法保证轧制力精度的稳定性。在首钢股份公司迁安钢铁公司20辊森基米尔轧机生产线进行S12硅钢钢种轧制力优化试验,将优化的模型参数应用于L2并投入现场生产,结果表明该优化方法不仅提高了轧制力设定精度,而且减小了冷轧硅钢的厚度超差长度,提高了成材率。 The rolling force is the key factor which influences the accuracy of cold-rolling strip thickness. To implement high precision control of cold-rolling strip thickness,we optimize the deformation resistance model parameters and friction coefficient model parameters to improve the calculation precision of cold-rolling force model,and use exponential smoothing self-learn algorithm to ensure the stability of rolling force accuracy. In Shougang Qiangang 20-high Sendzimir mill single stand production ...
高温硅钢加热炉双蓄热燃烧技术的探讨
介绍了双蓄热燃烧技术的特点和高温硅钢加热炉的特点,探讨了双蓄热燃烧技术在高温硅钢加热炉中使用的技术难点,分析了双蓄热燃烧技术在高温硅钢加热炉上使用的可能性。 Introduced characteristics of double regenerative combustion technology and high temperature silicon steel reheating furnace,discussed technical difficulties for using double regenerative combustion technology,analyzed the possibility of double regenerative combustion technology applied to high temperature silicon steel reheating furnace.
火花源原子发射光谱法在线测定电工钢中的超低碳
采用火花源原子发射光谱分析测定电工钢中超低C,研究试样制备方法、Ar纯度和压力等条件对分析结果的影响,并对工作曲线进行了优化,实现了一次分析同时测定电工钢的多种元素,满足炉前和精炼在线分析的要求。 Ultra-low carbon in electrical steel is determined with spark-source atom emission spectrum.It is researched the influence of sample making method,purity of Ar,and pressure on analysis result.The work curve is optimized.The determination of many elements in electrical steel only in one analysis is realized.It meets demands of on-line analysis for blast furnace and refining.
热轧无取向低硅钢SGG的研制开发及生产
针对川威950的工艺现状,结合无取向低硅钢SGG生产的工艺特点,主要从控制其钢坯加热和轧制以及终轧温度和卷曲温度几方面入手,进行无取向低硅钢生产的工艺控制研究。同时根据近6000吨的生产实践表明,该工艺措施能很好的满足该钢种的需要。 950 process Chuanwei status quo,with non-oriented silicon steel production process features low,mainly from the control of billet heating and rolling and finish rolling temperature and coiling temperature of several aspects,for non-oriented silicon steel production process of low control at the same time According to nearly 6,000 tons of production practice shows that the process measures could well meet the needs of the steel.
退火工艺对3.15%Si冷轧无取向硅钢组织和织构的影响
试验研究了退火温度(850~950℃)和时间(5~18 min)对2.3 mm热轧硅钢板(/%:0.036C,3.15Si,0.21Mn,0.005P,0.007S,0.032A1)6道次轧制的0.35 mm冷轧板组织和织构的影响。结果表明,退火温度越高,晶粒平均尺寸越大,900℃5 min退火时平均晶粒尺寸41.39μm,试样织构主要集中在γ取向线上的{111}<112>织构组分和{111}<110>织构组分;900℃18 min退火时平均晶粒尺寸为48.08μm,试样的{111}面织构和{112}面织构密度都明显减弱,{001}面织构增强,磁性能较优。 The effect of annealing temperature(850 ~950 ℃) and holding time(5 ~ 18 min) on structure and texture of 0.35 mm sheet by 6 passes cold-rolling from 2.3 mm hot-rolled plate of silicon steel(/%:0.036 C,3.15 Si,0.21 Mn,0.005 P,0.007 S,0.032A1) has been tested and studied.Results show that the higher the annealing temperature the coarser the average grain size;As annealing at 900 ℃ for 5 min the average grain size of steel sheet is 41.39 μm,and the texture in sample is mainly concentrated in y orie...
薄板坯连铸连轧生产中低牌号无取向硅钢的实践
本文中简要介绍了武汉钢铁有限公司采用薄板坯连铸连轧CSP(compact strip production, CSP)工艺生产中低牌号无取向硅钢的实践情况.CSP工艺生产的硅钢具有成品磁性均匀、板形好的优势,但是在利用该技术生产中低牌号无取向硅钢时,常存在成品板表面瓦楞状缺陷严重、连铸生产效率低等问题.通过优化炼钢成分、热轧等相关工艺,可消除热轧板厚度方向中心的粗大形变组织,从源头上避免了粗大{100}<011>纤维组织的出现,消除了瓦楞状缺陷;通过提升冶炼效率和控制钢中夹杂物总量,可优化隧道炉的加热温度与在炉时间,大幅度提升了连铸生产效率,实现了中低牌号无取向硅钢的批量稳定制造,使CSP产线成为中低牌号无取向硅钢热轧板原料的主要供给生产线.如何进一步提升钢水纯洁度、提高连铸生产效率、降低生产成本,以及挖掘该产线生产薄带钢的技术优点,是未来工作的重点. This paper briefly introduces the practice of producing medium and low grade non oriented silicon steel(NGO) with CSP(compact strip production, CSP)technology in Wuhan Iron and Steel Co., Ltd.. This technology has the inherent advantages of uniform magnetic properties and good shape for silicon steel finished strip. However, in the actual production process, there are serious corrugated defects on the surface of silicon steel finished strip, and production efficiency of continuous casting is low...
脱碳温度和脱碳时间对CGO取向硅钢碳含量控制的试验研究
通过测试取向硅钢不同工艺条件下的碳含量,探讨了CGO取向硅钢碳含量控制的最优处理条件,研究了脱碳温度和脱碳时间对相同初始碳含量取向硅钢的脱碳效果的影响。结果表明,在气氛为(15%~20%)H2+(75%~80%)N2,炉压差为10~20 Pa的条件下,CGO取向硅钢合适的脱碳温度为1 073 K~1 123 K,脱碳时间为10~20 min。在该处理条件下,能取得较好的脱碳效果。 By means of testing carbon content of oriented silicon steel below the distinct technical conditions,inquires the excellent handle terms of carbon content controlling for CGO oriented silicon steel,studies effects of decarburization annealing temperature and decarburization annealing time to the oriented silicon steel decarburization efficiency in same initial carbon content.The results show that,under the condition of atmosphere(15% ~ 20%) H2+(75% ~ 80%)N2 and furnace pressure difference 10 ~ 2...
高磁感取向硅钢生产技术与工艺的研发进展及趋势
采用节能、环保、经济型的生产技术与工艺来制造高磁感取向硅钢目前已成为世界各大取向硅钢生产厂的研发热点。总结了国内外各大钢铁企业与研究机构采用低温板坯加热技术生产高磁感取向硅钢的开发及应用情况,概括了传统流程实现低温板坯加热技术的方法。介绍了薄板坯连铸连轧与双辊薄带连铸等短流程工艺生产高磁感取向硅钢的研发现状。在此基础上,探讨了高磁感取向硅钢生产技术与工艺的发展趋势及方向。 Utilizing energy-efficient,environmentally friendly,economic production processes and technologies to manufacture high magnetic induction grain-oriented silicon steel has become the focus of current research work.Based on using low-temperature slab reheating techniques to produce high magnetic induction grain-oriented silicon steel at both iron and steel enterprises and research institutions all over the world,the current application and exploitation was thoroughly generalized;the implementation...
电解清洗装置在电工钢生产线上的应用
介绍了电工钢生产线连退机组的表面处理工艺,特别是电解清洗系统的工作机理、设备构造、生产工艺及各种影响因素。 This paper introduces the technology of surface treatment of continuous annealing unit in electrical steel production line,in particular the working mechanism,structure of equipment,production techniques and various influence factors of the electrolytic cleaning system.
低铁损高磁通密度无取向硅钢的应用与生产技术进展
分析了高转矩和高转速条件下高效驱动马达铁芯材料对无取向硅钢磁性能要求,讨论了无取向硅钢的高磁通密度和低铁损对电机转矩和效率的影响,介绍了国内外高磁感无取向硅钢发展情况。在生产工艺上,提高钢质纯净度,弱化夹杂物和第二相粒子对畴壁移动和再结晶晶粒长大的钉扎作用,添加微量晶界和带钢表面的偏析元素促使有利织构发展等技术可提高无取向硅钢的磁通密度。 The requirements of high efficient drive motor core materials under the conditions of high torque and high speed were analyzed.The effects of high magnetic flux density of non-oriented silicon steel on the torque and efficiency of the motor were discussed.The development of non-oriented silicon steel with high magnetic was introduced.The magnetic flux density of non-oriented silicon steel sheet can be obviously improved by some production technologies,such as purification steel,weakening the pin...