钢厂
余热利用系统在硅钢连续退火机组中的应用
介绍了烟气余热利用系统的工艺流程及控制思想,结合该系统在钢厂硅钢连续退火机组中的应用实践,估算出烟气余热利用系统每年可节约蒸汽5 040 t,经济效益良好,同时分析了该系统存在的问题及对策。 Introduced a method about the process and control of the application of waste heat system, which had been used into a silicon steel continuous annealing line and profiting a good economic benefit by saving a large number of steam every year, which has been estimated about 5 040 tons, and analyzed the problems and solutions existed in this system.
CSP工艺生产无取向电工钢
介绍了CSP工艺生产无取向电工钢各工序的设备特点、采用的工艺控制手段和电工钢产品质量情况,结合生产实践证明了马钢CSP工艺开发的无取向电工钢产品丰富了薄板坯连铸连轧的品种结构,发挥了薄板坯连铸连轧生产无取向电工钢性能均一、稳定的特点。 The equipment characteristic,the process control method and the quality of non-orientated silicon steel by CSP process were introduced.Combined with the production situation,it is proved that production of non-orientated silicon steel developed on Masteel CSP line would enrich product structure of thin slab continuous casting and rolling,and it exerts stable performance of non-orientated silicon steel.
硅钢连续退火机组的节能措施
针对硅钢连续退火机组的主要能源介质消耗现状,对现有生产工艺和设备研究采取机组循环用水、增加清洗段漂洗级数等措施可节约大概27 m3/h的过滤水量,并可减少78%的弱碱处理量;将炉子烟气换热系统增加一级余热回收,每年回收的余热相当于583 t标煤消耗,可节约蒸汽5 368 t。 The present situation of energy consumption for silicon steel annealing line is analyzed in this paper.In existing process and equipment conditions,increasing the number of cleaning series will lead to a saving of about 27 m3/h of filter water and reduce 78 % of weak base processing volume.For the flue gas heat-exchange system,adding a waste heat recovery device will recover waste heat equivalent to 583 tons of standard coal per year,corresponding to a saving of steam 5 368 t per year.
无取向硅钢热轧卷结疤缺陷产生的原因及控制
针对不同牌号的无取向硅钢产生结疤缺陷的难易程度和表面结疤缺陷的外形特征及分布规律,分析了该缺陷产生的原因。通过调整剪前导板的对中度,设置精轧侧导板开度余量及短行程数值,及时修补与更换侧导板,减少带坯与侧导板挤撞程度,有效地降低了结疤缺陷发生率。 This article analyses the cause of the scab defects according to the defects appearance characters and distribution law,degree of difficulty to form scar of non-oriented silicon steel. It can effectively decrease the scabs by different methods,such as adjusting the center line of guide plate,setting the opening margin and short stroke value of the side guide on finishing mill,timely repairing and replacing of side guide,decreasing the collision between the strip and side guide.
6.5%Si硅钢的制备技术和发展前景
6.5%Si硅钢具有优异的磁学性能和广泛的应用前景。本文综述了6.5%Si硅钢的物理、机械及磁学特性,讨论了传统轧制、温轧、薄带连铸、快速凝固、CVD、粉末轧制等不同制备工艺的关键技术及特点,概括了6.5%Si硅钢在高效节能电机、汽车马达及磁屏蔽等领域中的主要应用,介绍了硅钢的制备技术取得的研究进展,并指出了其广阔的发展前景。 6.5% Si silicon steel has good magnetic properties and wide applications.In this paper physical and mechanical magnetic properties were summarized,and key technology and characteristic of several preparation methods,such as traditional rolling,warm rolling,thin strip continuous casting,rapid solidification,CVD and powder rolling,were discussed.Main applications of 6.5% Si steel in the fields of high-efficiency electrical motors,automobile motors,transformer cores and magnetic shielding were gene...
冷轧无取向硅钢的边缘降控制优化研究
某冷连轧机生产无取向硅钢板材时,其边缘降的长度合格率频繁超标。为满足用户的叠片厚度精度要求,这类产品必须以增大切边量的方式来保证交货质量,而这种方式又直接降低了金属收得率,提高了生产成本。基于此,以该产线现有设备特性为基础,详细分析其软、硬件功能模式,分别对辊形与反馈控制进行全面分析与优化改进。通过现场试验论证,充分明确依托辊形优化与反馈控制程序的改进能显著提高边缘降的控制水平,该技术的使用为生产现场的边缘降控制提供了合理的技术支撑。 A cold rolling mill production of non-oriented silicon steel sheet,the thickness difference of the edge( edge-drop) is usually exceed the preset standard value,In order to meet the accuracy requirements of the user flatness,these production must be trimed wider length to meet the delivery quality of the user need, which directly reduce the metal yield and increase the manufacturing cost. Therefor,the software and hardware of the production line has been analyzed, and the work roll shape and feed...
新钢1580取向硅钢宽度窄尺原因分析
取向硅钢因其高磁导率、低矫顽力和大电阻系数等特性,被广泛应用于大中型变压器和大型电动机铁芯的制造。因取向硅钢性能和成分控制严格,生产工艺复杂,故其产品代表了钢铁企业特殊钢生产的最高水平。本文介绍了新钢公司卷板厂1580热连轧线生产取向硅钢过程中出现的窄尺问题,研究了取向硅钢产品的特点,分析了热轧过程中的组织转变,并结合生产实际提出了改进措施。通过对加热炉钢坯加热模式、粗轧轧制策略、精轧轧制工艺、二级模型等方面的优化和改进,取向硅钢窄尺情况明显好转,提高了产品的成材率和市场口碑。 The oriented silicon steel is widely used in the iron core manufacture of large and mediumsized transformers and large motors because of its high permeability, low coercivity and large resistance coefficient. Due to the performance and composition control of oriented silicon steel is strict, the production process is complex,therefore, its products represent the highest level of special steel production in iron and steel enterprises. This paper introduces the problem of narrow gauge in the produ...
硅钢DR510生产工艺优化
本文对某厂硅钢DR510温度、成分及过程控制水平和成品的组织、力学性能进行了研究,并在此基础上提出了工艺优化方案,有一定的借鉴和推广价值。 In this paper,the critical process and the products quality,including temperature,composition and process controlling level,the organization and mechanical properties of the finished product,were studied.On the basis of that the optimized technical plan provided,and this control technology is worth using and spreading.