轧制力是影响冷轧带钢厚度精度的关键因素。为实现高精度的冷轧带钢厚度控制,通过优化变形抗力模型参数和摩擦系数模型参数提高冷轧轧制力模型计算精度,并使用指数平滑法的自学习算法保证轧制力精度的稳定性。在首钢股份公司迁安钢铁公司20辊森基米尔轧机生产线进行S12硅钢钢种轧制力优化试验,将优化的模型参数应用于L2并投入现场生产,结果表明该优化方法不仅提高了轧制力设定精度,而且减小了冷轧硅钢的厚度超差长度,提高了成材率。 The rolling force is the key factor which influences the accuracy of cold-rolling strip thickness. To implement high precision control of cold-rolling strip thickness,we optimize the deformation resistance model parameters and friction coefficient model parameters to improve the calculation precision of cold-rolling force model,and use exponential smoothing self-learn algorithm to ensure the stability of rolling force accuracy. In Shougang Qiangang 20-high Sendzimir mill single stand production ... 
2014-05-28 26 5.8

采用扫描电镜、场发射扫描电镜、能谱仪等对50SW1300冷轧无取向硅钢中的夹杂物分不同尺寸区间进行数量统计,利用主成分回归分析法,即数据的标准化处理—主成分分析—回归分析—标准化的变量还原成原始变量—确定显著影响因素,综合分析夹杂物总量及各尺寸区间的夹杂物数量对无取向硅钢磁性能的影响。结果表明:主成分回归分析能够从夹杂物尺寸区间及数量的多个影响因素中提取主要的因素,定量研究其对磁性能的影响。分析表明,显著影响无取向硅钢铁损的夹杂物为100~500nm的AlN、AlN+MnS、MnS、Al2O3、AlN+Al2O3,而劣化磁感最明显的夹杂物尺寸区间为100~200nm。 Different size intervals of inclusions in cold rolled non-oriented silicon steel 50SW1300 were counted by scanning electron microscope(SEM),field emission scanning electron microscope(FESEM)and energy disperse spectroscopy(EDS).With principal component regression method:standardization for experimental data,principal component analysis,regression analysis,transform standardized variables into original variables,determination of significant factor,effects of the total number of inclusions and the... 
2014-10-28 48 5.8

采用电子背散射衍射技术测定50SW1300冷轧无取向硅钢中不同尺寸范围晶粒的含量,利用主成分回归分析法,综合研究不同尺寸范围晶粒的含量对无取向硅钢磁性能的影响。结果表明:通过主成分回归分析法能够从不同尺寸范围晶粒的含量的多个影响因素中获取主要的因素,定量研究它们对无取向硅钢磁性能的影响规律。分析表明,无取向硅钢的铁损与不同尺寸范围晶粒的含量之间存在着可靠的多元线性关系,在一定范围内,较大尺寸晶粒的含量越多,其对铁损优化的作用越明显;而无取向硅钢的磁感与不同尺寸范围晶粒的含量之间并无线性关系。 Distribution of grain size in cold rolled non-oriented silicon steel 50SW1300 was measured by EBSD.The effects of the distribution of grain size on magnetic properties of the non-oriented silicon steel were comprehensively researched by means of principal component regression method.The results indicate that the main factors influencing the magnetic properties in the distribution of grain sizes,which can be used to guantitative study the magnetlic properies of the steel,are obtained by principal... 
2014-11-28 48 5.8

通过试验确定氩气分析流量为3.5L/min,静态流量为0.75L/min,冲洗时间为3s,预燃时间为12s,积分时间为5s的激发条件,采用火花源原子发射光谱法测定取向硅钢中碳、硅、锰、磷、硫。分别采用铣床铣样、砂轮磨样两种制样方式进行了精密度考察,发现制样方式对结果影响不大;讨论了取向硅钢样品中碳、硅、锰、磷、硫测定时可能存在的共存元素干扰,发现硅对锰元素的干扰不可忽略,采用干扰系数法进行了校正,据此拟合得到各元素校准曲线的相关系数均在0.999 0以上。精密度考察结果表明,碳、硅、锰、磷、硫的相对标准偏差(n=10)在0.71%~9.4%之间。对两块取向硅钢生产样品进行分析,并与钢铁研究总院进行比对分析,结果一致,且偏差均在允许范围内。 Carbon,silicon,manganese,phosphorus and sulfur in oriented silicon steel were determined by spark source atomic emission spectrometry.The selected excitation conditions were as follows:the analytical flow rate of argon was 3.5L/min,the static flow rate was 0.75L/min,the flush time was3s,the precombustion time was 12sand the integration time was 5s.Two sample preparation methods,including milling machine and grinding wheel,were investigated.The precision test results showed that,the determination... 
2013-10-28 30 5.8

【作者】 陈迪安; 李春生; ...
2023-05-09 53 5.8

【作者】 吴玉美; 陆晔; ...
2023-05-09 53 5.8

对无取向电工钢中的夹杂进行了系统的分析。利用小样电解,采取不同电解液,不同的分离方法对无取向电工钢中稳定和不稳定夹杂物进行了提取、分离和收集。利用扫描电镜(SEM)、X-射线衍射、ICP等对电解分离收集的夹杂物进行了定性和定量分析。 The inclusion analysis of the non-oriented electrical steel has been investigated.By using small sample electrolytic analysis,with different electrolytes and different separation ways,the stable inclusions and unstable inclusions was drew,separated,and collected.With utilizing the methods of SEM,X-ray and ICP,the qualitative and quantitative analysis of inclusions in the non-oriented electrical steel was obtained. 
2023-05-09 65 5.8

根据现场实际的生产控制情况,指出了热轧原料断面轮廓缺陷以一定的比列遗传给了冷轧带钢,分析了不同热轧原料断面轮廓对冷轧电工钢尺寸精度的具体影响,提出了相应的规律。并阐明了严格控制热轧原料断面轮廓形貌,对保证冷轧电工钢尺寸精度具有重大意义,对于中国现行的冷轧电工钢生产具有指导意义。 Based on the actual situation of production control,it was pointed out that the section profile defects of hot-rolled raw materials were geneticed to the cold-rolled strip.The specific impact analysis for the profile of different hot-rolled raw materials to the dimensional accuracy of cold-rolled silicon steel was analyzed.As a result, the corresponding orderliness are given;And the strict control to section profile of the hot-rolled material is of great significance to ensure the dimensional ac... 
2014-01-28 11 5.8

无取向硅钢的磁性能主要取决于铁素体的晶粒尺寸、晶体织构和钢中的夹杂物。通过合适的化学成分设计以及采用适宜的夹杂物控制技术,可以获得最佳的夹杂物控制效果,使其纯净度大幅度提高或者无害,最终获得磁性能优良的高级别无取向硅钢。同时,为满足节能、环保、高效需求,无取向硅钢正朝着节能降耗、环境友好以及多功能、高效率、易加工等方向发展。 The magnetic properties of non-oriented silicon steel mainly depend on the grain size of ferrite,the crystallographic texture,and the inclusions in the steel.The optimum inclusion control effects can be obtained through a suitable chemical composition design and an appropriate inclusion control technique,and then the liquid steel will get be clean or the inclusion will get be harmless,finally the excellent magnetic property of the non-oriented silicon steel can be obtained.Meanwhile,in order to ... 
2013-03-28 34 5.8

【作者】 罗海文; 向睿; ...
2014-10-28 24 5.8

绝缘涂层可以有效提高硅钢片的耐蚀、耐腐、磁、绝缘等性能,因此取向硅钢涂装绝缘涂层是取向硅钢生产过程中重要的一环。本文对取向硅钢含铬无机绝缘涂层以及氮化铬涂层的性能优缺点进行了介绍,并对国内无机含铬取向硅钢绝缘涂层及氮化铬涂层的研究现状进行了综述。最后对未来含铬无机绝缘涂层的研发方向进行了展望。 Insulation coating can effectively improve the corrosion resistance of silicon steel sheet, such as corrosion, magnetic, insulation performance, thus oriented silicon steel insulation coating is the important part of oriented silicon steel production process. In this paper, the inorganic insulation coating oriented silicon steel containing chromium and chromium nitride coating performance advantages and disadvantages are introduced.In addition, the research status of insulation coating and chrom... 
2022-02-28 39 5.8

就冷轧硅钢废水处理生产中面临的主要问题进行分析,从技术角度及运行管理角度提出工艺优化升级改进措施及应对策略;同时从后续深度处理,逐步实现零排放目标的角度进行探讨,为冷轧硅钢废水减量化、出路乃至废水零排放提供一些思路。 The main problems in the wastewater treatment process of cold-rolled silicon steel lines are analyzed and process upgrading measures and optimization strategy are put forward from both technical and management views.At the same time,downstream deep treatment to gradually achieve the target of zero discharge is discussed,to provide some ideas for reduction or even zero discharge of wastewater from cold-rolled silicon steel lines. 