低硅钢冶炼过程硅质量分数控制

【作者】
周贺贺;
曹余良;
王攀峰;
孟令东;

【Author】
ZHOU He-he,CAO Yu-liang,WANG Pan-feng,MENG Ling-dong(Nisco Wide Plate/Coil Plant;Nanjing Iron and Steel Co.,Ltd.,Nanjing 210035,Jiangsu,China)

【机构】
南京钢铁股份有限公司中厚板卷厂;

【摘要】 抑制回硅是低硅品种钢冶炼的重点和难点,南钢中厚板卷厂通过转炉出钢弱脱氧操作,精炼炉弱脱氧升温,脱氧、脱硫造渣,连铸严格的保护浇注及吹氩塞棒、吹氩浸入式上水口的应用等一系列工艺优化和操作的改进,使整个冶炼过程钢水回硅量稳定控制在200×10-6以内,钢水终点成分完全满足低硅钢要求。 

【Abstract】 Control of increasing silicon is the emphasis and difficulty in low silicon varieties steel smelting.The Nisco Wide Plate/Coil Plant can control the silicon content in molten steel keeping within 200×10-6 through whole steelmaking process by using oxygen residual operation in converter tapping,oxygen residual and increasing temperature,deoxidation,desulfurization,slag refining,protection cast,blowing argon by plugged nozzle,blowing argon by submerged entry nozzle in continuous casting,and other … 

【关键词】 低硅钢;
回硅;
弱脱氧;
脱硫;

【Key words】 low silicon steel;
increasing silicon;
remaining oxygen;
desulfurization;

原文发表于《中国冶金》2013年第05期

论文PDF全文下载

此内容查看价格为5.8立即购买(VIP免费)
不用注册会员、不用登陆账号,直接支付购买查看,客服QQ:1093451816,此外成为本站VIP可免费查看本内容。
原文链接:http://1guigang.com/down/thesis/44046.html,转载请注明出处~~~
0
广告位招租

站点公告

网站试运行,请大家关注本站公众号,多提宝贵意见!

显示验证码
没有账号?注册  忘记密码?