为了确定普通冷轧取向硅钢最优的中间完全脱碳退火工艺,在其一次冷轧后进行5种不同工艺的脱碳退火处理,借助扫描电镜及电子背散射衍射技术研究了不同工艺脱碳退火后的组织、织构和脱碳效果。结果表明:经5种工艺脱碳退火处理后,初次再结晶的平均晶粒尺寸均约为19μm,且不随退火温度和时间的变化而变化;经840℃×10min工艺退火后的晶粒最均匀,高斯织构位向更准确,高斯织构面积分数最多,为3.1%,可将碳脱至0.003 5%。 In order to determine the optimal intermediate complete decarburizing annealing processes for common grain-oriented(CGO)silicon steel,five kinds of intermediate decarburizing annealing processes were conducted,the microstructure,texture and decarbonization after different decarburizing annealing processes were studied by scanning electron microscopy and electro back-scattered diffraction(EBSD)technology.The results show that the average grains sizes of primary recrystallization were about 19μm a... 
2013-11-28 159 5.8

【作者】 凌健; ...
2011-03-28 149 5.8

为了确保硅钢铬酸盐涂料的环保性,需要严格控制涂料的固化工艺,保证涂料固化过程中涂料中的六价铬充分转化为三价铬。对涂料及原料进行热重分析(TG)及差示扫描量热法分析(DSC)。结果表明,MgO与铬酐混合转化为MgCrO4,使六价铬稳定性增强,其中大部分Cr6+转变为Cr3+发生在620~700℃,在450~500℃高于铬酐发生大量失重,因此必须加入还原剂保证涂料中六价铬被充分还原;超过360℃后树脂会发生分解,因此实际板温不能超过360℃;加入了还原剂的整体涂料的失重温度区间主要在260~320℃,因此涂料固化时钢板的实际温度最佳区间为320~360℃。 Because of the silicon steel chromate coating’s environmental requirements,the paint curing process must be controlled strictly to ensure all Cr( Ⅵ) transforms to Cr( Ⅲ). The TG and DSC analyses of the paint are studied. The reaction of MgO and CrO3 would generate MgCrO4,enhancing the stability of Cr( Ⅵ). The most r( Ⅵ) in MgCrO4 changes to Cr( Ⅲ) at 620-700 ℃,while the CrO3 has a large weight loss at 450-500 ℃. The reductant must be added in the paint to make sure the Cr( Ⅵ) could transform suf... 
2014-09-28 162 5.8

研究了冷轧95%变形量无取向硅钢不同退火温度(710~1 050℃)下再结晶织构特征.再结晶刚完成时(710℃退火),呈现强γ({111<112>~<134>)与弱{114}<481>织构特征;随退火温度升高至900℃,γ明显减弱,{114}<481>组分持续增强,形成典型的{h,1,1}<1/h,1,2>织构;进一步升温至1 050℃,再结晶织构不再发生明显变化.基于EBSD分析,{114}<481>组分的持续强化可归因于其明显的尺寸优势以及较高频率的高能晶界(取向差角为20°~45°). A non-oriented silicon steel was heavily rolled to 95% reduction and subsequently annealed at 710~1 050 ℃ to investigate recrystallization texture evolution.When annealed at 710 ℃ with complete recrystallization,the texture is characterized by a strong partial γ fiber spreading from {111}<112> to {111}<134> and a weak {114}<481> component.As annealing at 900 ℃,γ fiber is decreased significantly while {114}<481> is increased consistently,producing a typical {h,1,1}<1/h,... 
2013-05-28 186 5.8

【摘要】 <正>2014年5月9日,从武钢硅钢事业部获悉,...
2014-06-28 154 5.8

为了弄清楚高硫硅钢中的硫化物析出行为及其对钢的微观组织和电磁性能的影响,以便为工业化生产制定更为合理的硫含量控制标准和采取更为有效措施减轻炼钢生产的硫含量控制压力,结合0.25% Si 无取向硅钢 ,采用非水溶液电解提取 + 扫描电镜/透射电镜观察相结合的方法 ,研究了0.006 8%、0.010 2%、0.025 5% 和 0.035 3% 硫含量条件下,钢中的硫化物夹杂物组成和存在形式及其形貌、种类、尺寸、数量变化,以及相应的热轧、成品试样的微观组织和电磁性能变化。结果表明,随着钢中硫含量的增加,钢中的硫化物逐渐由 MnS→MnS+Cu2S→Cu2S转变,数量逐渐增多,尺寸向高低两个方向发展。相应地,导致热轧再结晶组织劣化和抑制了成品晶粒尺寸长大。随着钢中硫含量的增加,钢的磁感、铁损劣化程度逐渐增大。钢中的硫含量平均每增加 0.01%,涡流损耗、磁滞损耗分别劣化0.24 W/kg 和 0.41 W/kg,而磁感会劣化 0.009 T。但是 ,在硫含量为 0.010 2% 时 ,铁损可以低于 6.0W/kg,而在硫含量为 0.025 5% ... In order to find out the precipitation behavior of sulfide inclusions and the corresponding changes of microstructure and electromagnetic properties of high sulfur silicon steel sheets, so that to design more suitable sulfur concentration controlling limit for industrial manufacture and to release the steel-making difficulty effectively, Based on the change of given sulfur concentration 0.006 8%, 0.010 2%0.025 3% and 0.035 3%, the type and composition, the size and number, and the size distribut... 
2022-02-28 179 5.8

利用光学显微镜(OM)和扫描电镜(SEM)研究了不同稀土Ce含量的50W470无取向硅钢的铸坯、热轧板和冷轧退火板的宏观和微观组织,并采用磁性能测试仪测定其磁性能。结果表明:当稀土Ce的加入量从0增加到66×10-6(质量分数)时,铸坯的柱状晶平均宽度从3.82 mm减小到3.24 mm,等轴晶率从43.1%增加到51.3%;热轧板的平均晶粒尺寸逐渐增加,从26.2μm增加到33.3μm,再结晶百分数从24%增加到37%;退火板的平均晶粒尺寸从36.2μm增加到39.3μm;磁性能测试表明,微观组织的变化有利于50W470无取向硅钢铁损降低和磁感提高。 Macro-structure and microstructure of as-cast plate, hot rolled plate and cold rolled annealed plate of 50 W470 non-oriented silicon steel with different rare earth Ce content was studied by optical microscope(OM) and scanning electron microscopy(SEM), and their magnetic properties were measured by magnetic property tester. The results show that when the addition amount of rare earth Ce increases from 0 to 66×10-6(mass fraction), the average width of columnar crystal of the as-cast pl... 
2022-03-28 198 5.8

取向硅钢热轧板中织构梯度对发展完善的二次再结晶十分关键,通过添加铜可以显著降低取向硅钢板坯加热温度,从而影响热轧板织构分布。利用X射线衍射仪,分析了实验室模拟薄板坯连铸连轧(TSCR)工艺的3种不同铜含量的取向硅钢热轧板织构。结果表明:不同铜含量热轧板表面到厚度1/4处均为弱的热轧织构,热轧板心部主要为{100}面织构;铜含量约在0.4%时,热轧板次表层的{110}<001>织构比例最高,而热轧板心部的{100}<110>织构比例最低;铜含量对热轧织构中{114}<110>和{001}<100>织构发展有显著影响。 The texture gradient in hot rolled grain oriented silicon steel strip is one of the essential factors to achieve a perfect secondary recrystallization.The addition of copper can significantly reduce the slab reheating temperature of grain oriented silicon steel,so as to impact the texture distribution in the hot rolled strip.The texture of hot rolled grain oriented silicon steel strip as-rolled by thin slab casting and rolling process(TSCR) in laboratory with three different copper contents was ... 
2011-01-28 191 5.8

研究了冷轧大压下量,950℃退火时间对一种新型含铜无取向电工钢晶粒度和织构的影响。结果表明,大压下量冷轧,随压下量的增加,退火晶粒向γ线聚集,形成强{111}<112>织构。提高冷轧压下率,退火织构{111}<100>,{110}<001>强度减弱,增加退火时间,退火织构{111}<110>,{100}<001>,{110}<001>强度变弱。采用87.5%冷轧压下率和950℃退火60 s,有利织构{100},{110}占有率最大。 The effect of annealing(950 ℃) time with high cold rolling reduction on grain size and texture of a new non-oriented electrical steel containing copper was investigated.The results show that for high cold rolling reduction,most annealed grains are oriented along γ-fibre with increasing cold rolling reduction ratio and strong texture {111}<112> is formed.With increasing the cold rolling reduction ratio,the intensity of annealed texture {111}<110>,{011}<100> decreases.With increa... 
2011-01-28 178 5.8

【作者】 陶永根; ...
2011-06-28 147 5.8

对商用50W330型无取向硅钢成品在930℃下保温2 h固溶并以不同方式冷却处理,利用磁性检测仪检测分析了处理前后的磁感和铁损变化,应用光学显微镜、扫描电子显微镜、X射线衍射仪观测分析了显微组织结构的演变。考察了平均晶粒尺寸、织构组分比及第二相粒子状态对磁性能的影响规律,结果表明:固溶处理前后平均晶粒尺寸的变化对硅钢磁性能的影响非常显著;当平均晶粒尺寸相差不大时,织构组分比[Goss+{100}]/{111}越大,磁感会越高;固溶处理会将细小弥散的第二相粒子重新回溶到基体中,减小了其对磁畴壁的钉扎作用,铁损随之下降。 The commercial 50W330 non-oriented silicon steel samples were heat treated at 930℃ for 2 h and cooled in different ways,then the iron loss and the magnetic induction of the samples before and after solution treatment were measured with a magnetic detector.The evolution of microstructural texture was analyzed by optical microscopy,scanning electron microscopy and X-ray diffractometry.The effects of average grain size,texture composition ratio and the second phase particles on the magnetic propert... 