钢厂
TSCR试制高强度无取向电工钢
采用固溶强化、细晶强化和位错强化方法,模拟TSCR流程试开发高强度无取向电工钢,试开发钢的主要合金成分为3%Si、0.83%Al和2.99%Mn。分析热轧、常化、退火后的钢板组织,并针对不同的成品板组织,详尽地分析了相应的力学性能和磁性能。试验电工钢平均晶粒直径为12.37μm时,R p0.2为530 MPa,R m为618 MPa;当退火制度为700℃×4 min,成品组织完全为未再结晶的回复组织时,R p0.2为853.5 MPa,R m为895.5 MPa。该成分的电工钢P15/50或P10/400最小时,对应的平均晶粒直径都大于59.67μm;P10/800或P10/1000最小时,对应的平均晶粒直径都处于12.37~59.67μm尺寸区间。 TSCR was simulated to develop high-strength non-oriented electrical steel with 3% of Si,0.83% of Al and 2.99% of Mn by solution strengthening,grain refinement strengthening and dislocation strengthening.The microstructures of hot rolled plates,normalized plates and annealed plates were analyzed.Furthermore,the mechanical properties and magnetic properties of products with different microstructures were detailedly studied.As the average grain diameter of the steel was 12.37 μm,the yield strength ...
取向硅钢中含铜抑制剂的固溶析出行为
含铜抑制剂作为取向硅钢的主抑制剂或辅助抑制剂不仅可以抑制初次晶粒的长大,促进二次再结晶,还可以降低铸坯的加热温度。取向硅钢中主要抑制剂为10~50 nm Cu2S,在钢的铸坯、热轧、冷轧、脱碳等工艺过程均可析出;(Cu,Mn)1.8S、Cu1.8S、ε-Cu等主要作为辅助抑制剂,尺寸一般为30~50 nm(或大于50 nm),主要在热轧阶段析出。总结了国内外有关取向硅钢中含铜抑制剂析出行为的研究进展,当前主要研究不同生产流程和工序中含铜抑制剂的析出行为和作用机理。 As main inhibitor or auxiliary inhibitor for grain-oriented silicon steel,the particles of inhibitor bearing copper not only inhibit the primary crystal growing and promote the secondary recrystallization,but also decrease the heat temperature of casting slab.The main inhibitor for grain-oriented silicon steel is 10~50 nm Cu2S,which precipitate in process and procedure including steel casting slab,hot rolling,cold rolling and decarburizing process,while the 30~50 nm or more than 50 nm...
硅钢连续退火机组的节能措施
针对硅钢连续退火机组的主要能源介质消耗现状,对现有生产工艺和设备研究采取机组循环用水、增加清洗段漂洗级数等措施可节约大概27 m3/h的过滤水量,并可减少78%的弱碱处理量;将炉子烟气换热系统增加一级余热回收,每年回收的余热相当于583 t标煤消耗,可节约蒸汽5 368 t。 The present situation of energy consumption for silicon steel annealing line is analyzed in this paper.In existing process and equipment conditions,increasing the number of cleaning series will lead to a saving of about 27 m3/h of filter water and reduce 78 % of weak base processing volume.For the flue gas heat-exchange system,adding a waste heat recovery device will recover waste heat equivalent to 583 tons of standard coal per year,corresponding to a saving of steam 5 368 t per year.
新日铁高强度无取向电工钢的研究进展
针对新日铁公开的相关专利,总结日本高强度无取向电工钢的研究进展,分析了各专利化学成分、生产工艺及产品性能的特点,指出固溶强化、细晶强化、析出强化、位错强化都有可能被用来提高无取向电工钢的强度。在高强度无取向电工钢的研发过程中,需要根据其具体用途确定目标性能,再采用合适的强化手段,从而实现力学性能、磁性能和生产性能之间的平衡。 Authors summarize the research progress of high strength non-oriented electrical steel in Japan by learning related patents brought into the public by Nippon Steel. Authors also analyze the characteristics of the chemical composition, production technology and properties of products in the patents and point out that any ones of solution strengthening method, fine-grain strengthening method, precipitation strengthening method or dislocations strengthening method may be used to improve the strengt...
无取向硅钢晶粒长大过程中应力对织构和晶界变化的影响
采用EBSD技术研究了有、无拉应力作用下无取向硅钢在晶粒长大过程中织构转变及晶界变化的规律。结果表明:在晶粒生长期间,无应力作用下的硅钢中,{111}〈112〉,{111}〈110〉织构组分强化,而{100}〈001〉织构组分弱化;与无拉应力作用下的情况相比,施加5MPa的拉应力时,{111}〈112〉,{111}〈110〉织构组分强化的速率下降,{100}〈001〉织构组分变化不明显。对于在晶粒生长期间持续变化的{111}〈112〉,{111}〈110〉和{100}〈001〉织构组分而言,虽然有、无拉应力作用下硅钢的{111}〈112〉和{111}〈110〉织构组分的高取向差角度晶界频率均下降,而{100}〈001〉织构组分的高取向差角度晶界频率则上升,但当有拉应力作用后,{111}〈112〉和{111}〈110〉织构组分的高取向差角度晶界频率下降的速率变小,{100}〈001〉织构组分的高取向差角度晶界频率上升的速率稍有变小。通过对无取向硅钢在晶粒长大过程中织构转变及晶界变化规律的研究,分析了合金原子在晶界的偏聚行为。 The rules of texture and grain boundary transformation in the nonoriented silicon steel under applied stress or without applied stress during grain growth were investigated by EBSD.The results show that the {111}〈112〉 and {111}〈110〉 components in the nonoriented silicon steel without stress are strengthened during grain growth whereas {100}〈001〉 component is weakened,but the growth rate of {111}〈112〉 and {111}〈110〉 component decreases,while the area fraction of {100}〈001〉 component doesn’t chang...
资源节约型高强度电工钢SXRC的开发
日本住友金属成功地开发了一种资源节约型高强度无取向电工钢SXRC,这种电工钢是通过固溶铌适度抑制位错的合并对消而得到一种特殊的微观组织,因此兼具很高的力学性能和磁性,特别适用于HEV、EV驱动电机转子。而且,不使用昂贵的镍就可以达到期望的强度,合金成本可控,是一种优越的资源节约型产品。 Sumitomo metal industries ltd of Japan successfully developed a type of high strength non-orientation electrical steel SXRC of resources-saving.The steel has both high mechanical performance and good magnetic property thanks to the special microstructure produced by the formation of Nb solid solution serving to appropriately inhibit the combination and cancellation of dislocations.The material is,in particular,suitable for manufacturing rotors of HEV and EV driving motors.Besides,expected streng...
云边一体化系统架构下硅钢制造管理业务数字化融合应用
提出以“云边一体化架构”构建硅钢智慧决策系统,来解决原硅钢制造L1~L5系统架构模式下的数字信息孤岛、业务功能割裂等问题。在此基础上,开发了云边协同的自学习型控制模型及业务决策模型,构建起硅钢“智慧大脑”,形成了以研发、制造、服务等核心业务数字化融合的智能化决策支持新模式,探索出一条钢铁制造业数字化、智能化转型之路。 SIDS(Silicon-steel Intelligent Decision-making System)based on \"cloud-edge integration architecture\" was proposed to solve the problems of data silos and business function fragmentation in the original L1~L5 system architecture.On this basis,the self-learning control model and decision-making model of cloud-edge collaboration were developed,the \"smart brain\" of silicon steel department was constructed,and a new intelligent decision-making support model of digital integration of core businesses s...
高效电机用冷轧无取向电工钢退火板析出物的析出特征研究
通过热力学计算,分析了实验钢中主要析出物析出的可能性。结果表明:在液相和固液两相区中,AlN和MnS均不能析出;在奥氏体区,AlN和MnS具备热力学析出条件,平衡析出温度分别为1547、1582 K。成品退火板中的析出物主要为AlN和MnS。扫描电镜下观察到的AlN形貌多为长条状,MnS形貌多为棒状或近似球形。这两种析出物占了析出物总量的85%以上,尺寸集中分布在400~800nm;复合析出物主要是(Al2O3+MnS)和(AlN+MnS),形貌不规则,尺寸集中在0.7~1.5μm;透射电镜下观察到了少量100nm以下独立的AlN析出。 According to thermodynamic calculation, the precipitation probability of precipitates was analyzed, AlN and MnS can not precipitate in liquid phase area and solid-liquid two-phase area. In austenite area, both the AlN and MnS have precipitation condition in thermodynamics and precipitates at 1547 K and 1582 K, respectively. The precipitates in annealing plate are mainly AlN and MnS. The shape of AlN is mostly strip, and MnS is stick or near sphericity. They accounted for over 85% of the total qu...
稀土处理无取向硅钢中夹杂物的控制
结合工业化生产的高效硅钢,进行了RH精炼稀土处理试验研究。针对不同的稀土处理条件,观察了夹杂物的形貌和尺寸分布,探讨了稀土处理后钢中的夹杂物形成、变化规律。结果表明:试验条件下,最佳的稀土合金添加数量为0.6~0.9 kg/t。经过合适的稀土处理后,可以有效抑制尺寸相对较小的、不规则的AlN、MnS复合夹杂生成,促进钢中微细夹杂物的聚合、上浮,钢质纯净度得到明显提高。此时,钢中全氧含量最低,脱硫效果最佳,钢中的夹杂物主要是尺寸相对较大的、近似球形或者椭球形的稀土类夹杂。 Based on the industrial production of non-oriented silicon steel,the experiment on RE treatment during the RH refining process was studied.The morphology and the size distribution were observed for the steel specimens treated with different RE treatment conditions.Further more,the formation and change of inclusions of final steel sheets after RE treatment were discussed.The results show that the suitable RE added amount was 0.6~0.9 kg/t.After the suitable RE treatment,the formation of AlN and Mn...
热卷箱在取向硅钢生产中的应用
热卷箱位于热连轧带钢生产线粗轧与精轧机之间,是热连轧生产中比较理想的中间保温设备。由于取向硅钢变形温度区间较窄,在生产中易出现边裂现象,同时中间坯的边部温度难于得到保证,因此一般不采用热卷箱设备生产,限制了传统热连轧生产线产品开发的品种。通过合理优化热卷箱控制工艺参数,解决了某厂传统热连轧生产线用热卷箱生产取向硅钢的边部质量问题,成功地生产出取向硅钢带。 The hot coil-box is an ideal heat retaining apparatus for hot rolling,lined between roughing mill and finishing mill. But oriented silicon steel has a narrow deformation temperature range,so that the edge crack easily occurs and it is difficult to insure the temperature of the intermediate blank. Therefore,the hot coil-box is rarely used in producing oriented silicon steel,which restricts the product development of the traditional hot rolling line. The article reasonable optimized process parame...
ICP-AES法测定硅钢中铌的不确定度评定
分析了电感耦合等离子体发射光谱法(ICP-AES)测定硅钢中铌的检测过程,讨论了该检测过程中不确定度的主要来源,建立了该方法的定量的数学模型,并根据这一模型计算出了检测结果的合成标准不确定度和扩展不确定度。 The measurement of niobium content in silicon steel by inductively coupled plasma atomic emission spectrometry(ICP-AES) was analyzed,by which the main factors affecting the uncertainty of the measurement were ascertained and the calculation formula was given.Finally,according to the formula the combined uncertainty and expanded uncertainty were obtained.
电工钢反复弯曲试验的影响因素
电工钢反复弯曲次数是电工钢性能检验的重要指标之一,直接影响到用户在使用电工钢过程的机加工性能。主要分析了试样宽度、试样张力、晶粒取向、反复弯曲设备等因素对电工钢反复弯曲试验的影响,并对各个因素的影响程度进行量化以及原因探讨,从而归纳形成各影响因素的基本规律,以便为电工钢实际生产、用户使用提供科学指导。结果表明:试样宽度增加,反复弯曲次数也会不断增加,晶粒位向对取向电工钢的反复弯曲次数影响较大,当支座顶部到拨杆底部的距离减小或拉紧力增加时,反复弯曲次数会不断减小,但当拉紧力达到60N以上时,对反复弯曲次数影响不大,试样经退火后,反复弯曲次数略有上升。 The reverse bend number is an important performance of electrical steels′capabilities,affecting the machining performance directly when the customers used.It investigated some factors,such as sample′s width,sample′s tension load,grain orientation and equipment,how to effect the reverse bend test for electrical steel,measured the influence degree,and discussed the reason,in order to form basic rules which could be guided the manufacturing and using for electrical steel.Results showed that the rev...