所有分类
  • 所有分类
  • 未分类

冷轧中中低牌号的无取向硅钢多采用万能凸度轧机(Universal crown mill,UCM)生产,其板形好坏受制于UCM轧机板形调节手段的协调使用。为掌握UCM轧机的板形控制特点,建立基于二维变厚度有限元的辊系弹性变形和基于三维差分的轧件塑性变形的六辊轧机耦合模型,对UCM轧机的板形调控性能进行详尽的分析,包括工作辊和中间辊弯辊、中间辊窜辊的调控功效、辊间接触压力分布等。在此基础上,提出可用指导生产的板形控制策略,指出UCM轧机在横向厚差控制方面的不足。针对工业生产中UCM轧机轧制无取向硅钢横向厚差大的问题,在大量仿真计算的基础上,开发具有高次曲线函数的边部变凸度(Edge variable crown,EVC)的工作辊。采用该工作辊后,各种品种的无取向硅钢的横向厚差不大于10μm的百分比由24%提高到99%,横向厚差的均值小于6μm,远小于之前的13μm。 Medium-low grade non-oriented silicon steel is rolled often by universal crown mill(UCM) during cold rolling.Its shape quality is dependent on the coordinated control of several shape adjustment devices of UCM.In order to understand the shape control characteristics of UCM,coupling model of six-high rolling mill,based on two-dimensional varying thickness finite element rolls elastic deformation model and three-dimensional finite difference strip plastic deformation model,is setup for the detaile... 
2011-10-28 207 5.8

用Gleeble1500D模拟试验机在变形温度为950~1 200℃、应变速率为0.01~8s-1、最大变形程度为60%的条件下,对硅钢50A1300做单道次压缩试验,首先分析了不同参数对流变应力的影响,然后用回归法确定了应力模型中的变形激活能及材料常数,得到硅钢50A1300在峰值应力条件和稳态应力条件下的变形激活能分别为270.360和91.557kJ/mol,同时得到了流变峰值应力模型,模型的相关系数为0.997。最后通过作lnθ-ε图的方法找到了硅钢50A1300发生动态再结晶的临界应变量,并回归得到峰值应变量、临界应变量与参数Z/C的关系式。 To analyze the effects of different parameters on the flow stress and critical strain of the dynamic recrystallization,single-pass compression experiments were carried out with silicon steel 50A1300 specimens using a Gleeble1500D thermal simulator at a temperature range of 950-1 200 ℃ and strain rate range of 0.01-8 s-1 under the condition of maximum deformation of 60%.The average deformation activation energy is respectively 270.360 and 91.557 kJ/mol under the peak stress and steady-state stres... 
2012-11-28 228 5.8

取向硅钢因其高磁导率、低矫顽力和大电阻系数等特性,被广泛应用于大中型变压器和大型电动机铁芯的制造。因取向硅钢性能和成分控制严格,生产工艺复杂,故其产品代表了钢铁企业特殊钢生产的最高水平。本文介绍了新钢公司卷板厂1580热连轧线生产取向硅钢过程中出现的窄尺问题,研究了取向硅钢产品的特点,分析了热轧过程中的组织转变,并结合生产实际提出了改进措施。通过对加热炉钢坯加热模式、粗轧轧制策略、精轧轧制工艺、二级模型等方面的优化和改进,取向硅钢窄尺情况明显好转,提高了产品的成材率和市场口碑。 The oriented silicon steel is widely used in the iron core manufacture of large and mediumsized transformers and large motors because of its high permeability, low coercivity and large resistance coefficient. Due to the performance and composition control of oriented silicon steel is strict, the production process is complex,therefore, its products represent the highest level of special steel production in iron and steel enterprises. This paper introduces the problem of narrow gauge in the produ... 
2022-06-28 244 5.8

【作者】 杨佳直; ...
2013-05-28 459 5.8

借助电子背散射衍射(EBSD)及ZEISS-200MAT金相显微镜对某钢厂普通取向硅钢(CGO)进行研究,研究结果表明:热轧板组织、织构沿板厚方向存在明显的不均匀性,在热轧板表层及次表层发生再结晶,同时存在强度较高的Goss织构,中心层存在较强的{001}<110>变形织构。冷轧组织均呈纤维状条带组织,一次冷轧后,热轧板中的Goss织构消失,织构主要为α、γ织构,经中间脱碳退火后,α、γ织构强度减弱,并出现一定强度的Goss织构和利于Goss织构发展的{554}<225>、{332}<113>等织构,经二次冷轧后,二次冷轧织构类型与一次冷轧织构一致,但织构强度不同。 The grain-oriented silicon steel produced by a steel factory was investigated by EBSD and ZEISS-200 MAT metallographic microscope.The results show that the textures and microstructures along thickness of hot rolled slab are inhomogeneous.The surface layer and the layer near that are recrystallized structure which has a high Goss texture,but there is deformation texture{001}<110>in the central layer.The structure after cold rolling is a structure like fiber strip.After the first cold rollin... 
2014-11-28 217 5.8

采用硅钢自动测量装置及X射线衍射仪检测出样品在实验前后的磁性能参数和织构强度.结果表明:较低的电压、9 Hz、较长的处理时间以及退火温度为650℃有利于增高铁损降低比例;较低的电压、较高的频率以及退火温度为650℃有利于增加磁感应强度增高比例.最佳的提高磁性能的实验参数是:频率为9 Hz,电压为500 V,处理时间为6 min,退火温度为650℃.通过织构分析可以验证:取向硅钢磁感应强度的变化取决于{110}<001>晶粒取向度值,而{110}<001>取向度值可看成是一个反映总体平均偏离角大小情况的综合值. An automatic measurement system for silicon steel and an X-ray diffraction meter were used for measuring the magnetic property parameters and texture of ex-processed samples and processed samples.It is shown that under the condition of a lower voltage,9Hz,a longer processed time and an annealing temperature of 650℃,the decrease rate of iron loss can be increased;a lower voltage,a higher frequency and an annealing temperature of 650℃ are in favor of improving the increase rate of magnetic inducti... 
2011-08-28 338 5.8

针对本钢薄板坯铸机在生产无取向电工硅钢的过程中存在的铸坯拉断、中包增碳、增氮等问题,进行了连铸工艺优化。通过采用新型无碳中间包覆盖剂、环保中间包干式料及专用结晶器保护渣后,降低了铸坯增碳量;通过控制钢包到中间包的增氮环节,降低钢水增氮;适当增大二冷水量,控制钢水过热度,防止铸坯拉断等生产事故的发生。改进工艺后,精炼后到成品铸坯的平均增碳量能控制在10×10-6以内,平均增氮量能控制在4×10-6以内。 The technology optimization has been adopted for preventing nitrogen increasing and carbon increasing in Benxi thin slab producing non-oriented silicon steel.Measures accordingly were adopted and satisfactory results were achieved. 
2011-05-28 360 5.8

采用EBSD检测技术,分析了50W800无取向电工钢在重要生产工序间织构的演变以及织构沿带钢宽度方向上的差异性。结果表明:热轧板织构沿带钢宽度方向上的差异性主要体现在表层织构。带钢边部表层织构主要由旋转立方织构、α纤维织构以及少量的γ纤维织构组成,带钢宽度1/4处的表层织构主要存在高斯织构,带钢宽度1/2处的表层织构主要为(110)面织构以及少量的铜型织构。各处的带钢宽度1/4处和1/2处的织构类型基本一致,都以α纤维织构和旋转立方织构为主。冷轧后,各处的表层织构类型差异较小,均为γ纤维织构和α纤维织构。由板宽边部至中心处织构强度值逐渐降低。退火后,各处织构的组分基本一致,为较强的γ纤维织构和较弱的(100)面织构。各处织构强度值差异较小,变化趋势与冷轧板一致。 The texture of non-oriented electrical steel 50W800 was detected by EBSD technique.The evolution of the texture between important processes and the difference of texture along the width direction of strip were analyzed.The result shows that the difference along the width direction of strip of texture at the surface of hot rolled plate is most obvious.The texture at the surface of strip edge is primarily made of rotating cube texture,αfiber texture and weakγfiber texture.Goss texture is mainly co... 
2014-09-28 318 5.8

采用双辊薄带连铸工艺试制了2.6 mm厚5.28%Si-1.11%Al高硅钢薄带,对比了1050℃×5 min正火及不正火铸带280℃冷轧至0.5 mm后,再经900~1100℃退火的磁性能。结果表明,高硅钢铸带显微组织为等轴晶组织,正火后铸带边部晶粒长大,中心层晶粒变化较小。成品中析出物主要为较粗大的AlN和AlN+MnS复合析出物,尺寸为0.5~2.5μm。与不正火试样相比,正火试样成品铁损大幅降低,磁感小幅下降;随退火温度的升高,两种工艺下铁损和磁感都是先降低后升高,在1050℃出现最低值。 2.6 mm thickness 5.28% Si-1.11% Al non-oriented high silicon steel was produced by twin roll thin strip casting.Magnetic property of the strip un-normalized and normalized at 1050 ℃×5 min was contrasted after cold rolled to 0.5 mm at 280 ℃ and 900-1100 ℃ final annealing.The results show that microstructure of the strip is equiaxed crystal.The surface grain is coarsened and the center layer grain has little change of the normalized strip.The main precipitates are AlN and MnS+AlN with 0.5-2.5 μm s... 
2013-06-28 289 5.8

综述了退火温度、时间对无取向电工钢磁性的影响。退火温度主要影响无取向电工钢不同织构的占有率,退火时间主要影响晶粒尺寸的大小,晶粒尺寸的变化对织构的形成也有一定的影响。磁感最高点出现在纤维组织完全消失,(111)面织构组分较弱的组织状态。铁损的降低主要依赖于磁滞损耗的降低,织构的影响不大。 The effects of annealing temperature and time on the non-oriented electrical steel magnetic properties were reviewed.Annealing temperature and time mainly affects the different textures share and the grain sizes of non-oriented electrical steel respectively.Changes of the grain sizes also have a certain effect on textures formation.The highest point of the magnetic induction value in the fibrous tissue completely disappears and{111} plane texture has a lower state of the component content.Iron l... 
2013-10-28 205 5.8

日本住友金属成功地开发了一种资源节约型高强度无取向电工钢SXRC,这种电工钢是通过固溶铌适度抑制位错的合并对消而得到一种特殊的微观组织,因此兼具很高的力学性能和磁性,特别适用于HEV、EV驱动电机转子。而且,不使用昂贵的镍就可以达到期望的强度,合金成本可控,是一种优越的资源节约型产品。 Sumitomo metal industries ltd of Japan successfully developed a type of high strength non-orientation electrical steel SXRC of resources-saving.The steel has both high mechanical performance and good magnetic property thanks to the special microstructure produced by the formation of Nb solid solution serving to appropriately inhibit the combination and cancellation of dislocations.The material is,in particular,suitable for manufacturing rotors of HEV and EV driving motors.Besides,expected streng... 
2011-06-28 303 5.8

从取向硅钢生产路线的选择、工艺技术的改进和生产设备的改造三方面进行了生产取向硅钢的节能降耗技术改造.通过完善多元抑制剂配方生产低温取向硅钢,通过加抛丸的酸洗、带面超声波清洗、改进连续退火炉以及余热循环利用等技术改造,使2012年取向硅钢的产量与未进行技术改造前的2009年相比提高了2.5倍,产品磁性上升了一个半牌号,能耗下降了8.9%,成材率提高了6.4%,生产成本下降了22%,综合效益显著. Energy saving technological transformation was carried out in the production of grain oriented silicon steel from three aspects of the oriented silicon steel production process route selection,technology improvement and equipment renovation.Through the improvement of multiple inhibitor formulations for producing low-temperature grain-oriented silicon steel,and by adding the blasting pickling,the belt surface ultrasonic cleaning,improvement of continuous annealing furnace,waste heat recycling tec... 
2013-02-28 252 5.8

站点公告

网站试运行,请大家关注本站公众号,多提宝贵意见!

显示验证码
没有账号?注册  忘记密码?