钢厂
退火工艺对无取向硅钢磁性能的影响
分析总结退火工艺各参数对冷轧无取向硅钢磁性能的影响,结合设计和生产实践经验介绍退火工艺中各参数的实际生产取值,并针对现生产工艺过程中出现的典型问题提出解决办法。 It is analyzed and summarized the great influences on magnetism of cold rolled non-oriented silicon steel affected by various annealing process data in this article.The relevant settled ways is raised.According to the actual value presetting ways for various annealing process data based on design and production,as well as typical problems occurred during production.
球刻痕法对高磁感取向硅钢磁性的影响
试验研究了球刻痕法对高磁感取向硅钢的铁损、矫顽力、相对磁导率、巴克豪森噪声等磁学性能的影响.研究结果表明:经过球刻痕处理后,高磁感取向硅钢的铁损明显降低,矫顽力下降,8 mm球刻痕过后铁损值与矫顽力分别下降16.2%和14.7%,且铁损和矫顽力均随刻痕间距降低而减少.刻痕后的高磁感取向硅钢磁导率在高磁感应强度下明显上升,刻痕后巴克豪森噪声值明显降低,经过对比分析确定8 mm为球刻痕的最佳刻痕间距.从磁畴观察、细化磁畴的原理等方面解释了细化磁畴对高磁感取向硅钢性能的影响原因. The effects of the ball scribing on magnetic properties of high permeability grain-oriented silicon steels,including the iron loss,coercive force,relative permeability,and Barkhausen noise were investigated. The results showed that the iron loss and coercive force of the high permeability grain-oriented silicon steels apparently decreased 16. 2% and 14. 7% respectively after 8 mm ball scribing and they both decreased with the decrease of the scribing spacing at the same magnetic flux density. At...
晶粒尺寸对无取向硅钢磁性能影响的主成分回归分析
采用电子背散射衍射技术测定50SW1300冷轧无取向硅钢中不同尺寸范围晶粒的含量,利用主成分回归分析法,综合研究不同尺寸范围晶粒的含量对无取向硅钢磁性能的影响。结果表明:通过主成分回归分析法能够从不同尺寸范围晶粒的含量的多个影响因素中获取主要的因素,定量研究它们对无取向硅钢磁性能的影响规律。分析表明,无取向硅钢的铁损与不同尺寸范围晶粒的含量之间存在着可靠的多元线性关系,在一定范围内,较大尺寸晶粒的含量越多,其对铁损优化的作用越明显;而无取向硅钢的磁感与不同尺寸范围晶粒的含量之间并无线性关系。 Distribution of grain size in cold rolled non-oriented silicon steel 50SW1300 was measured by EBSD.The effects of the distribution of grain size on magnetic properties of the non-oriented silicon steel were comprehensively researched by means of principal component regression method.The results indicate that the main factors influencing the magnetic properties in the distribution of grain sizes,which can be used to guantitative study the magnetlic properies of the steel,are obtained by principal...
Fe-3.15%Si低温取向硅钢不同常化工艺下的组织及析出相研究
利用OM,TEM,EDS与XRD技术,对Fe-3.15%Si低温取向硅钢热轧板不同常化处理后的显微组织、析出相及最终产品的磁性能进行了分析研究,并对热轧板和常化板经过冷轧后的冷轧板织构进行了对比分析.结果表明,采用1120℃保温3 min二段式冷却的常化处理工艺,常化板表层显微组织均匀,沿板厚方向的显微组织的不均匀性显著,对后续过程中形成高取向的Goss织构最有利,取向硅钢的磁性能最高;采用二段式冷却的常化冷却工艺最优,在此冷却工艺下析出的细小的析出物数量最多,且弥散分布在基体中,抑制剂的抑制效果最好,对成品获得高磁性最有利;热轧板、常化板经过冷轧后的冷轧板织构均主要由{111}〈110〉和{111}〈112〉织构组成,但常化板较热轧板冷轧后的冷轧板γ取向线织构密度明显增高,由此可以证实常化处理有助于取向硅钢最终获得高取向的Goss织构. The decreasing of slab heating temperature for grain-oriented silicon steel will reduce the amount of precipitates in hot rolled plate,and be disadvantage to the formation of ultimate Goss texture.The aim of normalizing is to control and adjust the amount,size and distribution of precipitates.Microstructures,precipitates and magnetic characteristics of finished products with different normalizing technologies for Fe-3.15%Si low temperature hot rolled grain-oriented silicon steel are researched,a...
电工钢中柱状晶对热轧和退火时晶粒取向及组织的影响
利用EBSD技术研究了电工钢中长轴平行于轧向的柱状晶样品在热轧和退火过程中组织和取向的演变规律,并与长轴平行于板法向的样品的已有研究结果进行对比。结果表明,无论柱状晶按何种方向排列,只要表面存在剪切力,热轧后都可形成剪切织构,同时中心形成轧制织构,主要包括旋转立方织构和{112}<1-10>。柱状晶造成的影响主要体现在板中心层,长轴平行于轧向排列的样品热轧时形成的粗大旋转立方晶粒要到脱碳退火后才能完全消除,但破坏了正常的不同取向晶粒间的取向差分布及尺寸均匀性,导致二次再结晶不完全及磁性能降低。 The evolution of microstructure and grain orientation in an electrical steel containing columnar grains with its long axis being parallel to the rolling direction of sheet was studied during hot rolling and annealing by EBSD technique.The results are compared with those of samples containing columnar grains being parallel to normal direction of sheet reported in the reference [3].It was shown that,whether the long axis of columnar grains was arranged in RD or ND,shear textures can be formed in t...
温度及扩散时间对CVD法制备高硅钢的影响
采用CVD法制备6.5%Si高硅钢,介绍了具体的制备工艺过程,研究了温度对渗硅速率和试样质量减轻的影响,同时分析了扩散时间对高硅钢中硅分布的影响。结果表明:在CVD反应过程中,反应温度高于1050℃将大大提高渗硅速率,但当温度大于1200℃后,渗硅速率趋于稳定;渗硅后,试样会减轻、减薄,随着温度升高,试样质量减轻的速率逐渐增大,在1200℃左右趋于稳定;扩散时间越长,硅分布越均匀,结合制备效率进行考虑,满足Δw表-中/b≤5的时间为适宜的扩散时间。 6.5%Si high silicon steel was manufactured by using CVD method and the process was introduced,the influence of temperature on the siliconizing rate and quality reducing rate,diffusion time on silicon distribution were investigated.Results as follows: the siliconizing rate will increase quickly when the temperature is higher than 1050 ℃,but the siliconizing rate will become steadily as the temperature up to 1200 ℃;The quality reducing rate will increase with the elevating of temperature and the r...
低铁损高磁通密度无取向硅钢的应用与生产技术进展
分析了高转矩和高转速条件下高效驱动马达铁芯材料对无取向硅钢磁性能要求,讨论了无取向硅钢的高磁通密度和低铁损对电机转矩和效率的影响,介绍了国内外高磁感无取向硅钢发展情况。在生产工艺上,提高钢质纯净度,弱化夹杂物和第二相粒子对畴壁移动和再结晶晶粒长大的钉扎作用,添加微量晶界和带钢表面的偏析元素促使有利织构发展等技术可提高无取向硅钢的磁通密度。 The requirements of high efficient drive motor core materials under the conditions of high torque and high speed were analyzed.The effects of high magnetic flux density of non-oriented silicon steel on the torque and efficiency of the motor were discussed.The development of non-oriented silicon steel with high magnetic was introduced.The magnetic flux density of non-oriented silicon steel sheet can be obviously improved by some production technologies,such as purification steel,weakening the pin...
无取向硅钢磁性能提升技术进步及其发展动向
无取向硅钢的磁性能主要取决于铁素体的晶粒尺寸、晶体织构和钢中的夹杂物。通过合适的化学成分设计以及采用适宜的夹杂物控制技术,可以获得最佳的夹杂物控制效果,使其纯净度大幅度提高或者无害,最终获得磁性能优良的高级别无取向硅钢。同时,为满足节能、环保、高效需求,无取向硅钢正朝着节能降耗、环境友好以及多功能、高效率、易加工等方向发展。 The magnetic properties of non-oriented silicon steel mainly depend on the grain size of ferrite,the crystallographic texture,and the inclusions in the steel.The optimum inclusion control effects can be obtained through a suitable chemical composition design and an appropriate inclusion control technique,and then the liquid steel will get be clean or the inclusion will get be harmless,finally the excellent magnetic property of the non-oriented silicon steel can be obtained.Meanwhile,in order to ...
本钢高硬度无取向电工钢50BW600的研发
目前随着电工钢用户冲压设备的升级,冲压速度逐步提高,对电工钢产品的硬度和强度指标提出了更高的要求。与普通硬度级别的无取向硅钢相比,高硬度50BW600的Hv硬度提高15~20,达到125以上,同时对电磁性能指标也有较高要求。本钢通过化学成份和热轧及冷轧连退生产工艺的设计,经过小批量生产试验,满足用户要求。通过对工艺的严格控制,在大批量生产过程中,保证了产品的力学性能和电磁性的检验合格率。 Currently with upgrading of stamping equipment of silicon steel user, gradually increasing of stamping speed, propose higher demand for hardness and strength of silicon steel. Compared with conventional 50BW600, high hardness 50BW600 have higher hardness, reach greater than 125Hv. Through design of chemical composition with hot mill and annealing, production test of small quantities, stamping performance meet user request.
电工钢检测方法及标准综述
综述了电工钢从生产到成品过程中涉及到的检测项目、检测方法及仪器,并通过对电工钢标准的发展改进,详细阐述了我国现有的电工钢技术标准体系,同时对代表企业的电工钢重点指标进行了摘录对比,为综合应用电工钢检测方法并促进电工钢的发展提供了一定的参考。 This article summarizes the testing items,methods,and instruments involved in the process from manufacturing to finished products of electric steel. The current electric steel technical standards system in our country is also elaborated in detail,along with the development and improvement of electric steel standards. Meanwhile,by comparison of electric steel KPI in representitive companies,this article provides references for comprehensive application of electric steels testing methods and promo...