钢厂
脉冲磁场热处理对CGO取向硅钢脱碳退火过程中组织和织构的影响
采用自主研发的脉冲磁场退火装置,在取向硅钢脱碳退火过程中分别施加不同强度的磁场,并采用光学显微镜和X射线衍射仪研究了脉冲磁场脱碳退火后试样的显微组织和宏观织构。结果表明,脱碳退火过程中施加脉冲磁场后取向硅钢的平均晶粒尺寸均增加,当磁场强度为40 mT时,平均晶粒尺寸最大,为13.06μm。此外,取向硅钢试样的立方织构{001}<100>强度减弱,高斯织构{110}<001>和{111}<112>织构增强,有利于获得更好的成品织构和磁性能。 Self-developed pulsed magnetic field annealing device was used to apply magnetic field of different intensities during decarburization annealing of an oriented silicon steel, and microstructure and macro-texture of the specimens after decarburization annealing in a pulsed magnetic field were studied by using optical microscope and X-ray diffractometer. The results show that the average grain size of the oriented silicon steel increases with the application of pulsed magnetic field during decarbu...
高效电机用冷轧无取向电工钢退火板析出物的析出特征研究
通过热力学计算,分析了实验钢中主要析出物析出的可能性。结果表明:在液相和固液两相区中,AlN和MnS均不能析出;在奥氏体区,AlN和MnS具备热力学析出条件,平衡析出温度分别为1547、1582 K。成品退火板中的析出物主要为AlN和MnS。扫描电镜下观察到的AlN形貌多为长条状,MnS形貌多为棒状或近似球形。这两种析出物占了析出物总量的85%以上,尺寸集中分布在400~800nm;复合析出物主要是(Al2O3+MnS)和(AlN+MnS),形貌不规则,尺寸集中在0.7~1.5μm;透射电镜下观察到了少量100nm以下独立的AlN析出。 According to thermodynamic calculation, the precipitation probability of precipitates was analyzed, AlN and MnS can not precipitate in liquid phase area and solid-liquid two-phase area. In austenite area, both the AlN and MnS have precipitation condition in thermodynamics and precipitates at 1547 K and 1582 K, respectively. The precipitates in annealing plate are mainly AlN and MnS. The shape of AlN is mostly strip, and MnS is stick or near sphericity. They accounted for over 85% of the total qu...
低温取向硅钢热轧析出物与织构的研究
采用低温板坯加热制备取向硅钢,通过透射电镜(TEM)观察并研究热轧板中的析出物,用ODF织构法研究热轧板距表面1/8、1/4和1/2处的织构分布。结果表明,热轧板中的析出物主要是密排六方AlN,AlN形貌呈规则长方形,AlN颗粒大小不等,分布密度低;热轧板中的织构沿板厚方向,由亚表层的{110}<001>织构向1/2中心层的α线织构变化,其中{110}<001>织构在热轧板距表面1/4层处最强。 The low temperature grain-oriented silicon steels were produced by acquired inhibitor method.The precipitates in hot rolling strip were observed and studied by transmission electron microscope,and the texture distribution in 1/8,1/4 and 1/2 layers of hot rolling strip were analyzed by ODF method.The results showed that the square shaped h-AlN is the main precipitates in hot rolling strip.The precipitates are varying in size and distribution.The texture of hot rolling strip in thick direction are...
CSP流程生产高磁感无取向电工钢磁各向异性研究
对CSP流程生产的高磁感无取向电工钢50W1300在偏离轧制方向不同角度处的磁性能进行了测试和分析。结果表明:在偏离轧向不同角度处,磁性能差异显著,尤其在α=60°时磁感最低;偏离轧制方向不同角度处的磁性能大小取决于织构类型、强度及分布状态;增强{100}<0vw>和α、η取向的有利织构组分,降低不利的γ取向织构组分,且使有利织构组分分布越漫散,磁各向异性越小。 Magnetic properties of high magnetic induction non-oriented electrical steel 50W1300 produced by CSP processes were investigated with different direction in relation to the rolling direction.The result shows that magnetic properties are significantly different in relation to the rolling direction,in particular,the minimum magnetic induction occurs at 60° in relation to the rolling direction.Magnetic properties of different directions in relation to rolling direction depend on type and distributi...
低温高磁感取向硅钢常化工艺中间冷却制度的研究
借助电子背散射(EBSD)技术对AlN为主抑制剂的Hi-B取向硅钢常化工艺的中间冷却制度进行了研究。结果表明:常化后试样均发生了完全再结晶,在60℃/s冷速下组织最均匀;在合适的冷却制度下常化板表层保留了强的Goss织构,它深入到1/4厚度处,并且形成对Goss织构有利的强{554}<225>织构。 The intermediate cooling system of Hi-B oriented silicon steel with AlN main inhibitor in normalizing process was studied by means of electron back diffraction(EBSD) technique. The results show that:the specimens after normalizing are fully recrystallization, and the microstructure is most uniform under the intermediate cooling rate of 60℃/s; under suitable cooling system, normalized plate surface retains strong Goss texture, it penetrates into the 1/4 thickness of the plate and forming strong {...
轧制裂纹及热处理工艺对高硅电工钢复合板磁性能的影响
对3层高硅电工钢复合板铸坯进行热轧及温轧变形加工后,采用正火、退火两种热处理方式处理,并观察轧制过程中产生的裂纹,研究不同状态下复合板的磁性能。对不同状态下的试样进行扩散退火处理,研究复合板中裂纹变化及其对磁性能的影响。结果表明:不同热处理工艺下合金内部的裂纹尺寸差异明显,裂纹尺寸对复合板的磁性能影响显著,相对于深裂纹,其他因素的影响较小;温轧变形加工后,复合板内层出现有序组织,但该有序组织在合金存在深裂纹的前提下并不能从本质上提高合金的磁性能;扩散退火工艺可以消除复合板内部的浅裂纹及微裂纹,但不能消除尺寸较大的裂纹,故而不能显著提高存在深裂纹的复合板的磁性能。 After hot rolling and warm rolling deformation processing of casting billet for three-layer high silicon electrical steel composite plate, it was normalized and annealed for heat treatment. Then, the cracks produced during the rolling process were observed, and the magnetic properties of composite plate in different states were also investigated. Furthermore, the samples in different states were subjected to diffusion annealing treatment, and the changes of crack in composite plate and their eff...
冷轧大压下量下新型无取向电工钢的退火组织演变
研究了冷轧大压下量,950℃退火时间对一种新型含铜无取向电工钢晶粒度和织构的影响。结果表明,大压下量冷轧,随压下量的增加,退火晶粒向γ线聚集,形成强{111}<112>织构。提高冷轧压下率,退火织构{111}<100>,{110}<001>强度减弱,增加退火时间,退火织构{111}<110>,{100}<001>,{110}<001>强度变弱。采用87.5%冷轧压下率和950℃退火60 s,有利织构{100},{110}占有率最大。 The effect of annealing(950 ℃) time with high cold rolling reduction on grain size and texture of a new non-oriented electrical steel containing copper was investigated.The results show that for high cold rolling reduction,most annealed grains are oriented along γ-fibre with increasing cold rolling reduction ratio and strong texture {111}<112> is formed.With increasing the cold rolling reduction ratio,the intensity of annealed texture {111}<110>,{011}<100> decreases.With increa...
铸坯热装温度对无取向硅钢中AlN和MnS析出行为的影响
通过固溶度积公式计算及热模拟实验,对不同热装和加热温度条件下的无取向硅钢铸坯中析出相进行了研究.在低于950℃热装时,铸坯中AlN的析出量和尺寸不再变化,但MnS和AlN-MnS的数量及平均尺寸随着热装温度降低而进一步增加,并在温度低于600℃时达到最大值后保持不变.与1200℃相比,1100℃加热的铸坯中AlN、MnS的总固溶量相对更少.相比850℃热装,600℃热装再加热到1100℃的铸坯中AlN和MnS的总固溶量更少,且AlN和MnS尺寸更大.合适的热装温度和加热温度分别为600℃和1100℃. Based on solubility product calculation and thermal simulation experiments,precipitated phases in continuous casting slabs of non-oriented silicon steel were systematically studied at different hot charging and heating temperatures.When the hot charging temperature is below 950 ℃,the content and size of AlN remain unchanged,but the quantity and size of MnS and AlN-MnS increase when the hot charging temperature decreases,reach maximum and remain unchanged when the hot charging temperature is belo...
取向硅钢超大高斯晶粒取向偏离角的X射线衍射测量
介绍了一种适用于超大晶粒取向硅钢的高斯晶粒取向偏离角的X射线衍射测量方法,提出了将试探法和探测器扫描法相结合的方式进行测量。结果表明:该方法可以同时获得准确的实际衍射角度和取向偏离角度,试样制备方式简单,对设备的要求低且测量结果准确。 This paper introduces a X-ray diffraction measurement method of Gaussian grain orientation deviation angle for ultra-large grain oriented silicon steel, and puts forward a method of combining the test method with the detector scanning. The results show that this method can obtain accurate actual diffraction angle and orientation deviation angle at the same time. The sample preparation method is simple, the requirements for equipment are low, and the measurement results are accurate.
无取向硅钢热轧边裂的形成原因
利用加热炉模拟、动态再结晶以及热模拟等试验方法以及扫描电镜、金相显微镜等分析观察手段对无取向硅钢边裂的成因进行了探讨。结果表明,长时间加热使得板坯边部晶粒异常长大,晶界氧化并脱碳,轧制过程中边部温度过低,动态再结晶过程变弱,使得板坯边部延伸性能变差,是导致硅钢边裂的主要原因。建议通过适当降低铸坯加热温度、缩短保温时间、提高终轧温度来改善硅钢边裂缺陷。 The behaviors of high temperature oxidation,dynamic recrystallization,and hot ductility,microstructure evolution were investigated on the non-oriented electrical steel sheets to discuss the formation of edge crack.The key causes of cracking was found to be the coarse as-cast microstructure,grain boundary oxidation and decarburization in reheating furnace,as well as reduced temperature at strip edge region during hot rolling process resulting in reduced hot ductility and lack of enough dynamic re...
硅钢连续退火生产线设备改造
针对硅钢连续生产线设备存在的故障、隐患以及精度等影响产品质量的问题进行分析及改造,实现保证生产线设备稳定运行、提高设备精度及硅钢产品质量的目的。 This paper analyzes and transforms the electrical equipment failures, risks existed in slicon continuous production line, and the effect of accuracy to product quality, in order to ensure stable operation of equipment in production line and improve the accuracy of device, quality of silicon.