钢厂
无取向硅钢晶粒长大过程中应力对织构和晶界变化的影响
采用EBSD技术研究了有、无拉应力作用下无取向硅钢在晶粒长大过程中织构转变及晶界变化的规律。结果表明:在晶粒生长期间,无应力作用下的硅钢中,{111}〈112〉,{111}〈110〉织构组分强化,而{100}〈001〉织构组分弱化;与无拉应力作用下的情况相比,施加5MPa的拉应力时,{111}〈112〉,{111}〈110〉织构组分强化的速率下降,{100}〈001〉织构组分变化不明显。对于在晶粒生长期间持续变化的{111}〈112〉,{111}〈110〉和{100}〈001〉织构组分而言,虽然有、无拉应力作用下硅钢的{111}〈112〉和{111}〈110〉织构组分的高取向差角度晶界频率均下降,而{100}〈001〉织构组分的高取向差角度晶界频率则上升,但当有拉应力作用后,{111}〈112〉和{111}〈110〉织构组分的高取向差角度晶界频率下降的速率变小,{100}〈001〉织构组分的高取向差角度晶界频率上升的速率稍有变小。通过对无取向硅钢在晶粒长大过程中织构转变及晶界变化规律的研究,分析了合金原子在晶界的偏聚行为。 The rules of texture and grain boundary transformation in the nonoriented silicon steel under applied stress or without applied stress during grain growth were investigated by EBSD.The results show that the {111}〈112〉 and {111}〈110〉 components in the nonoriented silicon steel without stress are strengthened during grain growth whereas {100}〈001〉 component is weakened,but the growth rate of {111}〈112〉 and {111}〈110〉 component decreases,while the area fraction of {100}〈001〉 component doesn’t chang...
高温硅钢加热炉双蓄热燃烧技术的探讨
介绍了双蓄热燃烧技术的特点和高温硅钢加热炉的特点,探讨了双蓄热燃烧技术在高温硅钢加热炉中使用的技术难点,分析了双蓄热燃烧技术在高温硅钢加热炉上使用的可能性。 Introduced characteristics of double regenerative combustion technology and high temperature silicon steel reheating furnace,discussed technical difficulties for using double regenerative combustion technology,analyzed the possibility of double regenerative combustion technology applied to high temperature silicon steel reheating furnace.
低温板坯加热取向硅钢形变和初次再结晶织构的演变规律
采用取向分布函数和取向线分析方法对低温板坯加热取向硅钢从热轧到初次再结晶工艺阶段的织构进行了研究。研究表明:一次冷轧后各层的织构组分与热轧板各层面的织构组分存在着继承关系,次表层存在很强的{001}<110>织构,中心层的织构和热轧板的中心层相似,存在强的{001}<110>和{112}<110>织构;中间退火后发生再结晶,各织构组分的强度有所减弱,Goss织构组分再次出现;二次冷轧后沿厚度方向上的织构不均匀性不明显,{111}<112>织构强度最高,几乎是其他织构组分的1倍,{001}<110>织构大幅降低;初次再结晶后织构沿厚度方向没有明显的不均匀性,{111}<110>为最强的织构组分,并且具有一定强度的Goss位向。 The texture from the first cold rolling to the primary recrystallization of low temperature slab reheating grain-oriented electrical steel were researched by orientation distribution function and orientation distribution intensity technique.The results show that after the first stage of cold rolling,there is a strong {001}<110> texture in the subsurface and the texture in center layer is very similar to the center layer of hot band which has strong {001}<110> and {112}<110> tex...
云边一体化系统架构下硅钢制造管理业务数字化融合应用
提出以“云边一体化架构”构建硅钢智慧决策系统,来解决原硅钢制造L1~L5系统架构模式下的数字信息孤岛、业务功能割裂等问题。在此基础上,开发了云边协同的自学习型控制模型及业务决策模型,构建起硅钢“智慧大脑”,形成了以研发、制造、服务等核心业务数字化融合的智能化决策支持新模式,探索出一条钢铁制造业数字化、智能化转型之路。 SIDS(Silicon-steel Intelligent Decision-making System)based on \"cloud-edge integration architecture\" was proposed to solve the problems of data silos and business function fragmentation in the original L1~L5 system architecture.On this basis,the self-learning control model and decision-making model of cloud-edge collaboration were developed,the \"smart brain\" of silicon steel department was constructed,and a new intelligent decision-making support model of digital integration of core businesses s...
无铬无取向硅钢涂层烧结固化工艺
为进行磷酸盐系无铬无取向硅钢涂层烧结固化工艺研究,首先对磷酸盐系无铬无取向硅钢涂层进行热重-差示扫描量热(TG-DSC)分析;然后在不同烧结固化温度条件下,测定涂层板温随时间变化曲线;最终获得涂层烧结固化温度与时间(T-t)工艺曲线。通过中性盐雾试验、动电位极化、交流阻抗、涂层附着力以及扫描电子显微镜(SEM)和能谱(EDS)分析验证。结果表明,根据涂层烧结固化温度与时间(T-t)工艺曲线制备的涂层结构致密、性能优异,证明该工艺曲线具有合理性与正确性。 In order to study the curing process of chromium-free non-oriented silicon steel coatings,phosphatic chromium-free non-oriented silicon steel insulating coating was prepared and TG-DSC analysis of the coating was conducted,then the change of the actual temperature of the coated non-oriented silicon steel sheet with time at different curing temperatures was studied. Based on the experiments,the processing curves of curing temperature vs. curing time( T-t) for the chromium-free non-oriented silico...
无取向电工钢边部减薄控制技术研究
叠片系数是冷轧无取向电工钢的重要质量指标。为了提高叠片系数,必须保证无取向电工钢板形良好以及横向厚差小。针对攀钢冷轧厂4机架HC轧机轧制无取向电工钢的边部减薄问题,以无取向电工钢横向厚差最小作为目标函数,建立了一套针对无取向电工钢边部减薄控制的辊型曲线优化数学模型,开发了无取向电工钢专用辊型曲线,使无取向电工钢横向厚差从25μm降低到10μm以下,取得了良好的控制效果。 The lamination factor is an important quality index of non-oriented silicon steel strip.Considering the lamination factor,the non-oriented silicon steel must have a good shape and a smaller transverse thickness difference.In order to solve the edge thinning of non-oriented silicon steel strip in Panzhihua Steel,a mathematic model for designing the roll shape is built.In the model,the transverse thickness difference of non-oriented silicon steel strip is taken as the objective function.Based on t...
成品第二次退火工艺对高牌号无取向电工钢35W300组织和性能的影响
对高牌号无取向电工钢35W300的成品进行了第二次退火,对第二次退火后的成品性能、纵横向磁性能差异和组织变化进行了分析。结果表明,随着第二次退火温度的升高,晶粒长大,磁性能优化。铁损平均值下降0.087 5W/kg,磁感平均值升高0.008T。第二次退火温度为820℃的产品的磁性能能够满足用户使用要求。 The product of high grade non-oriented electrical steel 35W300 was annealed at the second time.Microstructure,the difference of magnetic properties in the vertical and horizontal and were studied.The results show that the grain grew up and magnetic properties optimized with the increase of annealing temperature for the second time.Iron loss average declines in 0.0875 W/kg,magnetic induction average increases 0.008 T.The magnetic properties can meet the requirements of users at the second anneali...
400mm硅钢自动轧制试验轧机
西安重型机械研究所为武钢开发了目前国内第一台自动化水平较高的先进可靠的硅钢热轧试验轧机。本文介绍了该轧机的工艺参数、设备组成,技术特点及轧制流程,该轧机在规定的终轧温度范围内,实现了2.5 m/s的快速轧制速度,保证了控制系统准确及时的采集到轧件进出轧辊时的信号,缩短道次间隙时间,实现了自动控制,保证了产品板形及精度的高水平要求,对于硅钢尤其是对其取向硅钢新产品、新工艺的开发具有深远意义。 An experimental prototype of 400 mm silicon steel hot rolling mill was developed by Xi’an Heavy Machinery Research Institue for Wu Gang.The technological parameters,configuration and characteristic of advanced control system in the experimental prototype are introduced in detail.The experimental prototype was realized the fast rolling of 2.5 m/s in the range of specified rolling temperature.Its automatic rolling control system can acquisite the signals that a rolled piece enters in and exits fro...
二次冷轧的中间退火温度对2.3Si无取向硅钢组织和性能的影响
试验2.3Si无取向硅钢(/%:0.003C,2.30Si,0.16Mn,≤0.020P,≤0.005S,0.54Al)冷轧板由常化和未常化的2.5 mm热轧板冷轧至0.6 mm(压下率76%),经750~950℃2.5 min中间退火后再冷轧至0.5 mm(压下率16.7%),成品板经890℃+960℃2.5 min退火。研究了中间退火温度对该钢晶粒尺寸、织构和磁性能的影响。结果表明,随中间退火温度的升高,二次冷轧前晶粒和成品晶粒增大,成品中不利织构组分{111}和{112}减弱,磁性能得到改善。热轧板经过常化时的磁性能明显好于未经常化时的磁性能,但中间退火温度较高时常化对磁性能的有利作用减弱。 The test cold sheet of 2.3Si non-oriented silicon steel(/%:0.003C,2.30Si,0.16Mn,≤0.020P,≤0.005S,0.54Al) is first cold-rolled from normalized and un-normalizing 2.5 mm hot-rolled plate to 0.6 mm sheet(reduction 76%),then intermediate annealed at 750~950℃ for 2.5 min and double cold-rolled to 0.5 mm sheet(reduction16.7%),the finished sheet annealed at 890℃+960℃ for 2.5 min.Effect of the intermediate annealing temperature on grain size,texture and magnetic performance of the steel has been studied....
稀土元素Ce含量对50W470无取向硅钢显微组织及性能的影响
利用光学显微镜(OM)和扫描电镜(SEM)研究了不同稀土Ce含量的50W470无取向硅钢的铸坯、热轧板和冷轧退火板的宏观和微观组织,并采用磁性能测试仪测定其磁性能。结果表明:当稀土Ce的加入量从0增加到66×10-6(质量分数)时,铸坯的柱状晶平均宽度从3.82 mm减小到3.24 mm,等轴晶率从43.1%增加到51.3%;热轧板的平均晶粒尺寸逐渐增加,从26.2μm增加到33.3μm,再结晶百分数从24%增加到37%;退火板的平均晶粒尺寸从36.2μm增加到39.3μm;磁性能测试表明,微观组织的变化有利于50W470无取向硅钢铁损降低和磁感提高。 Macro-structure and microstructure of as-cast plate, hot rolled plate and cold rolled annealed plate of 50 W470 non-oriented silicon steel with different rare earth Ce content was studied by optical microscope(OM) and scanning electron microscopy(SEM), and their magnetic properties were measured by magnetic property tester. The results show that when the addition amount of rare earth Ce increases from 0 to 66×10-6(mass fraction), the average width of columnar crystal of the as-cast pl...
大压下率冷轧无取向硅钢再结晶织构演变
研究了冷轧95%变形量无取向硅钢不同退火温度(710~1 050℃)下再结晶织构特征.再结晶刚完成时(710℃退火),呈现强γ({111<112>~<134>)与弱{114}<481>织构特征;随退火温度升高至900℃,γ明显减弱,{114}<481>组分持续增强,形成典型的{h,1,1}<1/h,1,2>织构;进一步升温至1 050℃,再结晶织构不再发生明显变化.基于EBSD分析,{114}<481>组分的持续强化可归因于其明显的尺寸优势以及较高频率的高能晶界(取向差角为20°~45°). A non-oriented silicon steel was heavily rolled to 95% reduction and subsequently annealed at 710~1 050 ℃ to investigate recrystallization texture evolution.When annealed at 710 ℃ with complete recrystallization,the texture is characterized by a strong partial γ fiber spreading from {111}<112> to {111}<134> and a weak {114}<481> component.As annealing at 900 ℃,γ fiber is decreased significantly while {114}<481> is increased consistently,producing a typical {h,1,1}<1/h,...
无取向硅钢铬酸镁绝缘涂层结构与耐蚀性能研究
采用扫描电镜、原子力显微镜研究了铬酸镁半无机绝缘涂层的微观结构。结果表明,涂层厚度为数微米,涂层中的有机树脂乳液颗粒均匀分布在无机涂层的表面,从而保证了涂层具有良好的冲片性能。采用极化曲线研究了涂层的耐蚀性能,发现铬酸镁与铬酸锌绝缘涂层的耐蚀性能相当。 In this paper,the microstructure and anti-corrosion property of magnesium chromate coating on non-oriented silicon steel were studied.The microstructure was observed by SEM and AFM.The anti-corrosion properties were evaluated by polarization curves.The results show that the thickness of coating is several microns and the polymer particles were scattered on the surface of inorganic coating,which is the guarantee for lamination property.The corrosion resistance of the magnesium chromate film was e...