钢厂
我国硅钢发展现状及发展趋势
硅钢是钢铁产品中的\"工艺品\",是高附加值产品,通过对我国主要硅钢生产厂家的工艺设备,市场情况分析,简要介绍了我国硅钢生产消费现状,未来生产能力预测及硅钢未来发展趋势。 Silicon steel is the \"crafts\" of steel products,also is high value-added product.By analyzing process equipment and market condition of major silicon steel-making plant of China,it briefly introduces our current production consumption status,future production capacity prediction and future development trend of silicon steel.
硅钢水溶性极厚绝缘涂层的热老化行为研究
对两种硅钢水溶性极厚绝缘涂层进行了不同温度的热老化实验。通过TG-DTA,GDS,FT-IR,SEM和光泽度仪等测试方法对老化的涂层进行分析表征,提出了评估硅钢水溶性极厚绝缘涂层热老化性能的合理温度区间,探讨了涂层热老化行为,并分析了两种涂层热老化性能的差异。结果表明,涂层附着性随着老化时间的延长逐渐下降。FT-IR表征结果显示,热老化过程中,涂料交联形成的化学键未发生断裂,交联剂氨基树脂的三嗪环被破坏是聚合物三维网络结构坍塌的主要原因。 Thermal aging expriments at different temperature were carried out on two types of water-soluble and extra-thick insulation coatings for non-oriented silicon steel,and a series of test methods such as glossmeters,TG-DTA,FT-IR,GDS,SEM were applied in analysis.For evaluating the thermal aging effect of this kind of insulation coating,the proper temperature range was proposed.The difference of aging performance between two coatings was been investigated and the related behaviors were been discussed...
稀土在无取向电工钢中应用的研究进展
稀土元素在许多钢中发挥着独特而且不可替代的重要作用。半个世纪以来,它的作用已经在各种低合金和特殊合金钢中的研究及应用中得到充分的证明;然而,作为具有稀土资源优势的中国,在属于重要功能材料的无取向电工钢中稀土的应用却落后于国外,本文就中国稀土在无取向电工钢中的应用研究作简要的评述,希望能够进一步推进此领域的研究,并且促进中国稀土在无取向电工钢中应用技术的发展,缩短与国外差距,并提出了在此应用领域今后需深入开展的研究方向。 Rare earth elements play a unique and irreplaceable role in a lot of steels,it has given the full proof by the practice of various low alloy steels and special alloy steels since half century.However,as our country has the advantage of rare earth resources,RE application technology in non-oriented electrical steels has lagged behind abroad.The application researches of rare earth in non-oriented electrical steel in our country are briefly reviewed in this paper,which hope to promote the research...
冲剪加工对无取向硅钢边缘组织和磁性能的影响
通过观察冲剪边缘组织,测量冲剪边缘的显微硬度、残余应力的分布情况和磁性能的变化研究了冲剪加工对无取向硅钢50WW800边缘组织和磁性能的影响。对冲剪后硅钢片进行750℃退火,分析退火对组织和磁性能的影响。结果表明,硅钢片剪切边缘会存在0.4 mm的形变硬化层,边缘应力大,铁损增加。退火后变形减小,形变硬化层变小,残余应力大幅度减少,铁损减少。 The influence of punching process on cutting edge microstructure and magnetic properties of non-oriented silicon steel 50WW800was studied by observing microstructure and measuring microhardness near cutting edge.The residual stress distribution in the silicon steel tooth and magnetic properties were measured.Effect of annealing at 750 ℃ on microstructure and magnetic properties of the silicon steel was analyzed.The results show that a cut-edge hardening layer up to 0.4 mm is observed,residual st...
无取向硅钢钙处理前后夹杂物的行为研究
研究了无取向硅钢钙处理前后夹杂物的行为,重点考察了钙处理前后夹杂物的成分、类型、形貌和尺寸研究的变化情况,为实际生产中无取向硅钢的钙处理提供理论指导。试验发现:钙处理前夹杂物主要以Al2O3、Al2O3-MgO为主,且在夹杂物表面有AlN析出,钙处理后夹杂物以Al2O3-MgO-CaS-CaO系复合夹杂物为主,还含有少量的SiO2或AlN;钙处理前后,夹杂物形貌由多边形或不规则形逐渐向球形或近似球形转变,并且夹杂物尺寸不断增大;钙处理前后,含钙夹杂物的比例发生突变,由10%增大到74.5%,且随着钙处理时间的延长,含钙夹杂物比例下降,表明钙处理使夹杂物变性后易聚集长大并上浮去除。 Behavior of inclusions before and after calcium treatment in non-oriented silicon steel was researched by investigating changes of compositions,types,shapes and sizes of inclusions before and after calcium treatment,for the purpose of providing theoretical guidance for calcium treatment of non-oriented silicon steel in actual situation. Results indicated that Al2O3 and Al2O3-MgO were main types of inclusions before calcium treatment,sometimes AlN maybe precipitate in the outer of inclusions. Al2...
50A1300牌号无取向硅钢磁性能改善工业实践
结合工业化生产的50A1300牌号无取向硅钢,分析了化学成分、RH精炼脱氧方式、板坯装炉温度以及热轧平整工艺等对磁性能的影响,探讨成品钢磁性能的改善。结果表明,采取改善后,50A1300牌号无取向硅钢的磁性能得到明显改善。2012年,该钢种平均铁损、磁感应强度分别达到5.26 W/kg、1.762 T,能够较好地满足用户市场需求及同行对标需要。 Based on the industrial manufacture of 50A1300 grade non-oriented silicon steel sheets,effects of chemical composition,deoxidization method in RH vacuum refining,charging temperature of steel slabs,hot rolling and flattening progress on magnetic properties are analyzed.The optimization methods of magnetic properties of steels are discussed. Results show that the magnetic properties are obviously improved by the adopted measures above. In 2012,the average core loss and the magnetic induction of 5...
异步轧制硅钢的表面纳米化及轧制参数的影响
对硅钢板材分别进行异步和同步轧制,研究了轧制参数包括速比、压下量和道次对板材表面显微组织的演变的作用.结果表明,异步轧制硅钢板材表面形成了晶粒尺寸为10~50 nm,取向接近随机分布的纳米晶,而同步轧制板材的表面只形成了位错胞,证明异步轧制可以诱发表面纳米化.异步轧制板材表面纳米晶的形成过程为:在剪切力的反复作用下,高密度位错形成、滑移、湮灭和重组形成亚微米尺度的亚微晶/位错胞.随着压下量和轧制道次增加,高密度位错重复以上过程使晶粒尺寸减小、取向差增大,最终形成取向接近随机分布的纳米晶组织.大压下量和多道次是异步轧制诱发板材表面纳米化的关键,而速比的增加可以加快纳米化进程. Surface nanocrystallization(SNC) can effectively enhance the surface and global properties of the metallic materials,such as microhardness,intensity,fatigue,wear and corrosion resistances,therefore provides more promising practical industrial applicability.Up to now,several SNC treatment methods were developed based either on the principles of ball impactions or friction sliding,however,difficulty still exists for the surface treatment of large-dimensional samples with high efficiency.Recently,m...
浅谈无底层取向电工钢的多种应用
介绍了国内无底层取向电工钢生产技术水平、产量和用途,简述了无底层取向电工钢作为取向电工钢超/极薄带母料及应用于制作大型发电机组铁心、风电等电机铁心和变压器铁心等的情况。 The production technology level,output and application of domestic glassless grainoriented electrical steel were introduced,and the application of glassless grain-oriented electrical steel as parent material of ultra-thin strip of grain-oriented electrical steel and in making large-scale electric generator cores,wind power motor cores and transformer cores were briefly described.
提高硅钢卷材下料利用率的几种方法
阐述了影响硅钢卷材下料利用率的因素,并结合具体事例利用计算机排样系统进行了详细分析,对提高硅钢卷材的利用率具有一定的指导作用。 It describes the factors influenceing the the utilization ratio of the roll of Silicon steel,and analyzes it in detail combined with concrete examples by a computer arrangement system,which can give a guide for increasing the utilization ratio of the roll of Silicon steel.
熔盐电沉积过程温度对1.6Si无取向硅钢Si扩散的影响
试验了通过NaCl-KCl-NaF-SiO2熔盐在电流密度50 mA/cm2、电沉积脉冲电流正反向比9:1和750850℃60min电沉积下阴极(/mm)20×20×0.5的1.6Si无取向冷轧硅钢片断面层硅的分布,并通过计算得出Si的扩散系数。结果表明,电沉积温度由750℃提高至850℃时,试样中Si含量增加,扩散的深度由18μm提高到40μm;电沉积温度与Si在钢中的扩散系数近似符合Arrhenius指数关系。 The distribution of silicon at cross section of cathode(/mm) 20 × 20 × 0.5 sheet of 1.6Si non-oriented cold rolled silicon steel after electro-deposit treatment by NaCl-KCl-NaF-SiO2 molten salt with current intensity 50 mA/cm2,electro-deposit pulse current positive-negative ratio 9:1 at 750 850 ℃ for 60 min has been tested and the diffusion coefficient of Si is obtained by calculation.Results show that with increasing electro-deposit temperature from 750 ℃ to 85...