钢厂
CSP流程试制50W270高牌号无取向硅钢织构的演变
研究了CSP流程试制50W270高牌号无取向硅钢热轧→常化→冷轧→退火过程中织构的演变.利用电子背散射衍射技术对全流程织构进行测量和分析.发现热轧板织构在厚度方向上存在较大差异,表层主要为铜型、黄铜和高斯织构,1/4层存在微弱的高斯织构和旋转立方织构,中心层以γ纤维织构和旋转立方织构为主,还含有较弱的α纤维织构.与热轧板相比,常化板表层和1/4层织构变化不大,中心层旋转立方织构和α纤维织构增强.冷轧板各层均具有α纤维织构和γ纤维织构.与冷轧板相比,成品板各层中α纤维织构基本消失,还出现了立方织构和高斯织构. This article focuses on texture evolution in 50W270 high-brand non-oriented silicon steel produced by CSP in hot rolling,normalizing,cold rolling,and annealing processes.The texture in the whole process was measured and analyzed by electron back-scatter diffraction.It is found that the texture along the thickness direction in hot-rolled strips changes obviously;there are mainly copper,brass,and Goss textures in the surface layer;the 1/4 layer has weak Goss texture and rotating cube texture;γ-fib...
基于人工神经网络-遗传算法的取向硅钢刻痕工艺优化
为了优化激光刻痕降低取向硅钢铁损的工艺,寻找刻痕速度、脉冲能量、扫描间距等重要刻痕参数的最佳匹配关系,提出了一种基于人工神经网络与遗传算法的优化模型,并利用这种模型对30Q130取向硅钢材料的刻痕工艺进行了优化实验,结果表明,这种模型稳定可靠,可以作为取向硅钢刻痕工艺优化的一种有效的措施。 A laser is often considered to scribe the grain-oriented silicon steel surfaces after cold-rolling and annealing to reduce the core loss.It is necessary to select the best scribing parameters to maximize the reduction in this process.This paper proposes an optimization method of genetic algorithm during laser scribing of 30Q130 steel,by developing an artificial neural network prediction model using a database form a designed orthogonal experiment.The objective is to determine the best combinatio...
加热温度对W470高硅钢连铸坯氧化铁皮的影响
采用SEM、EDS和XRD对不同加热温度下W470连铸坯氧化铁皮的微观形貌及相结构进行研究。结果表明,W470氧化铁皮难以除去的原因是氧化铁皮熔化,液相包裹着FeO,凝固时发生共晶反应,生成FeO/Fe2SiO4共晶混合物,并深嵌入基体。降低加热炉的加热温度,使连铸坯全程在FeO/Fe2SiO4共晶混合物熔点(1177℃)以下加热,可降低氧化铁皮与基体的结合力,能够有效解决W470除鳞困难问题。 The microstructure and phase structure of iron scale of W470 continuous casting billet at different heating temperatures were investigated by SEM,EDS,and XRD.The results show that the reason why the iron scale of W470 removes hardly is that iron scale is melted and the FeO is surrounded by the liquid phase,which forms FeO / Fe2SiO4eutectic mixture and is embedded into the matrix after solidification.Lowering the heating temperature and keeping the continuous casting billet heating under the melt...
无取向电工钢硫含量控制技术研究
针对采用含钒铁水生产无取向电工钢存在的铁水脱硫率低、转炉冶炼过程回硫量大、成品硫含量偏高的问题,通过对含钒钛铁水脱硫,减少转炉冶炼过程回硫以及RH脱硫技术等方面的研究,大幅度降低了电工钢成品硫含量。生产表明钢中w(S)=0.001 9%~0.006 9%,平均为0.004 2%;w(S)≤0.008%的比例达到了100%,且w(S)≤0.005%的比例也达到了91.43%。 In cognizance of the problems of low desulphurization rate for hot metal,large sulfur-recovery in converter as well as high sulfur content in products in producing non-orientation electrical steel with vanadium-content hot metal countermeasures have been carried out.Sulfur content in non-orientation electrical steel is decreased obviously by way of study on technologies of desulphurization for hot metal with vanadium & titanium,sulfur-recovery control in converter and desulphurization in RH ...
氢氧化镁煅烧制备硅钢级氧化镁的研究
以青海盐湖氯化镁为初级原料,采用喷雾热解法制备原料氧化镁。原料氧化镁通过水化制备氢氧化镁。将氢氧化镁过滤、洗涤、烘干、粉碎、煅烧,制备硅钢级氧化镁。本文重点考察煅烧温度、煅烧时间、料层厚度等因素对氧化镁水化率的影响,采用均匀实验设计和DPS数据处理,确定最优煅烧实验条件为:煅烧温度1250℃,煅烧保温时间4小时,料层厚度0.5cm。在此条件下得到的硅钢级氧化镁完全满足硅钢及氧化镁的行业标准。 The magnesium oxide is prepared by Spray pyrolysis process,which magnesium chloride from Qinghai Salt Lake is used as primary raw material,and hydrated to magnesium hydroxide,then obtained silicon steel magnesia through filtering,washing,drying,crushing and calcinations.In this paper,influences of some factors on magnesia hydration rate are studied,such as calcination temperature,calcination time and material thickness.After average experimental design and DPS data processing,optimal calcination...
退火工艺对3.15%Si冷轧无取向硅钢组织和织构的影响
试验研究了退火温度(850~950℃)和时间(5~18 min)对2.3 mm热轧硅钢板(/%:0.036C,3.15Si,0.21Mn,0.005P,0.007S,0.032A1)6道次轧制的0.35 mm冷轧板组织和织构的影响。结果表明,退火温度越高,晶粒平均尺寸越大,900℃5 min退火时平均晶粒尺寸41.39μm,试样织构主要集中在γ取向线上的{111}<112>织构组分和{111}<110>织构组分;900℃18 min退火时平均晶粒尺寸为48.08μm,试样的{111}面织构和{112}面织构密度都明显减弱,{001}面织构增强,磁性能较优。 The effect of annealing temperature(850 ~950 ℃) and holding time(5 ~ 18 min) on structure and texture of 0.35 mm sheet by 6 passes cold-rolling from 2.3 mm hot-rolled plate of silicon steel(/%:0.036 C,3.15 Si,0.21 Mn,0.005 P,0.007 S,0.032A1) has been tested and studied.Results show that the higher the annealing temperature the coarser the average grain size;As annealing at 900 ℃ for 5 min the average grain size of steel sheet is 41.39 μm,and the texture in sample is mainly concentrated in y orie...
钙处理对无取向硅钢中非金属夹杂物的影响
采用电解法和扫描电镜研究了300 t转炉-RH精炼钙处理对无取向硅钢板(%:≤0.005C、1.2~2.2Si、0.2~0.6Mn、≤0.20P、≤0.005S、0.2~0.6Al、0~0.01Ca)中夹杂物的影响。结果表明,钢中Al含量为0.25%和0.35%时,钢中溶解氧均小于1×10-4%,钙处理后都会产生CaS夹杂物,尤其是含0.35%Al的钢水;钙处理可以有效减少钢中的夹杂物数量,尤其是0.5μm以下的微细夹杂物数量;钙处理后夹杂物的种类以AlN、CaS为主,同时还含有少量的氧化物夹杂物以及AlN-CaS复合夹杂物,尺寸主要为1.5~5.0μm。 The effect of 300 t converter-RH refining calcium treatment on inclusions in non-oriented silicon steel sheet (%:≤0.005C,1.2~2.2Si,0.2~0.6Mn,≤0.20P,≤0.005S,0.2~0.6A1,0~0.01Ca) has been studied by electrolysis and scanning electron microscope.Results show that with 0.25%and 0.35%Al content in steel,all the dissolved oxygen in liquid is less than 1×10-4%,and the CaS inclusions are produced after calcium treatment,especial for the liquid containing 0.35%Al;the amount of inclusions in ste...
基于CSP工艺取向硅钢初次再结晶晶界特征对宏观织构的影响
利用背散射衍射技术(EBSD)和XRD,研究了两段式脱碳退火工艺对取向硅钢纵截面初次再结晶的微区取向、取向差分布、特殊晶界(CSL)及高温退火试样高斯织构。分析了初次再结晶晶界特征对取向硅钢高温退火后宏观织构的影响。结果表明:初次再结晶的纵截面基体中Σ3和Σ5晶界使得高斯晶粒有着较高的迁移率,在高温退火时借助20o~45°的大角度晶界的界面能吞并周围{111}<112>晶粒迅速长大,形成密度水平较高的高斯织构。 Micro area orientation of primary recrystallization,the misorientation distribution,special boundaries under different two-stage decarburization annealing and the Goss texture under high temperature annealing the longitudinal section of grain-oriented silicon steel were detected by electron back scattering diffraction(EBSD) and X-ray diffraction(XRD).The effect of primary recrystallization grain boundary on macrotexture after high temperature annealing was analyzed.The results show that the Σ3 a...
中、厚板坯生产的取向硅钢组织及织构特征
采用中、厚板坯生产技术对取向硅钢进行了研制和开发,对热轧及后工序样品进行了金相组织观察和EBSD分析,探讨了两种组织及织构的差异性,研究结果表明:除高温退火样品外,中板坯生产的取向硅钢各工序样品平均晶粒尺寸大;厚板坯生产的取向硅钢热轧和常化样品亚表层Goss织构强;中板坯和厚板坯的脱碳退火板织构没有明显区别。中板坯生产的取向硅钢成本低,产品磁性能和质量与厚板坯相当。 Grain oriented silicon steel was researched and developed by medium thickness slab and thick slab.Microstructures observation and EBSD analysis to the samples of hot rolling and following processes were carried out,respectively.The differences between the two kinds of microstructures and textures were discussed.The results show that the average grain sizes of every process samples are larger except that of high temperature annealing samples of grain oriented silicon steel produced by medium thic...
轧制法制备低铁损高磁感6.4%(质量分数)硅钢及其织构演变
采用轧制法制备出具有低铁损高磁感0.23mm厚6.4%(质量分数)Si高硅钢。沿轧制方向的最终磁性能为B8=1.474 T,B50=1.714 T;P10/50=0.30W/kg,P15/50=0.88W/kg。利用X射线衍射及背散射电子衍射(EBSD)技术分析了高硅钢在轧制及退火过程中的织构演变过程。结果表明,通过采用大压下率热轧,确保热轧板次表层中产生更多的高斯织构,随后进行遗传;温轧板中粗大的晶粒有利于冷轧剪切带的形成;冷轧板经脱碳退火后生成强{210}〈001〉织构及次表层较强的高斯织构是在轧向上获得高磁感的原因,归因于其在{111}〈112〉冷轧形变晶粒内的剪切带优先形核并长大;最终退火后虽出现了随机取向,但以{310}〈001〉织构为代表的η织构得以保留并且增强,进一步提高了磁感。随着退火温度的升高及保温时间的延长,高硅钢薄板晶粒尺寸不断增大,铁损明显降低。 6.4wt%Si high silicon steel sheets(0.23mm thick)with low iron loss and high magnetic induction were successfully produced by rolling process.The final magnetic properties along the rolling direction(RD) were:B8=1.474T,B50=1.714T;P10/50=0.30 W/kg,P15/50=0.88 W/kg.The texture evolution during rolling and annealing was investigated by means of X-ray diffraction and electron backscatter diffraction(EBSD).It was found that more Goss textures formed in the subsurface of hot rolled plates by using larg...
50W600无取向硅钢钙处理的热力学分析及实验研究
通过热力学计算及实验室研究,对钙处理前后50W600无取向硅钢退火冷轧板中夹杂物的类型、数量及尺寸进行了系统分析。结果表明,50W600无取向硅钢经钙处理后(w(Ca)=0.002 6%),钙在1 600℃的钢液中主要以固态的CaO·2Al2O3、CaO·6Al2O3及溶解钙的形式存在。在钢液的凝固过程中,钢中的溶解钙和硫反应生成了CaS和CaS-MnS复合夹杂,有效抑制了MnS的弥散析出,减少了钢中微细夹杂物的数量。同时钙处理促进了钢中微细夹杂物的聚合长大,导致显微夹杂物的数量增加。 Based on thermodynamic calculation and laboratory experiment,the type,quantity and size of inclusions in annealed cold-rolled steel sheets of 50W600 non-oriented silicon steel before and after calcium treatment were systematically studied.Results showed that after calcium treatment(w(Ca) = 0.002 6%),calcium was mainly in the form of CaO·2Al2O3,CaO·6Al2O3 and dissolved calcium in steel at 1 600 ℃.Dissolved calcium could combine with sulfur to form CaS inclusions and compound CaS-MnS inclusions du...