6.5%Si硅钢具有优异的磁学性能和广泛的应用前景。本文综述了6.5%Si硅钢的物理、机械及磁学特性,讨论了传统轧制、温轧、薄带连铸、快速凝固、CVD、粉末轧制等不同制备工艺的关键技术及特点,概括了6.5%Si硅钢在高效节能电机、汽车马达及磁屏蔽等领域中的主要应用,介绍了硅钢的制备技术取得的研究进展,并指出了其广阔的发展前景。 6.5% Si silicon steel has good magnetic properties and wide applications.In this paper physical and mechanical magnetic properties were summarized,and key technology and characteristic of several preparation methods,such as traditional rolling,warm rolling,thin strip continuous casting,rapid solidification,CVD and powder rolling,were discussed.Main applications of 6.5% Si steel in the fields of high-efficiency electrical motors,automobile motors,transformer cores and magnetic shielding were gene... 
2012-06-28 158 5.8

取向硅钢成品的晶粒尺寸非常大,其易磁化方向[001]晶向对于轧向的偏差角度对其磁性能影响极大。本文介绍了取向硅钢二次再结晶后成品晶粒位向的几种测定方法,包括侵蚀法、劳厄法、OIM法、极图法和非对称X射线衍射法等,并对这几种测量方法进行了比较。 The finished product of grain-oriented silicon steel has immense grain size ranging from millimeters to centimeters and the deviation angles of easy magnetization direction from rolling direction plays a remarkable role in magnetic properties of grain-oriented silicon steel.The methods in common use for determining the deviation angles of crystal direction are introduced,which include the etch-figure method,the Laue method,the OIM method,the pole figure method and the asymmetrical X-Ray diffract... 
2011-04-28 167 5.8

采用磁控溅射方法,分别在纯Fe以及低硅钢基片上沉积富Si膜,并对其进行真空扩散热处理.通过能谱分析及X射线衍射研究了Si在纯Fe与低硅钢基体中的扩散特征,运用DICTRA软件建立了扩散模型.研究发现Si在纯Fe基体中扩散时发生γ-Fe(Si)→α-Fe(Si)相转变,扩散速率受控于相界面的迁移.当沿截面Si含量梯度不足以驱动相界面正向迁移时,延长扩散时间会发生相界面回迁现象,最终趋于单一相内均匀化扩散过程.Si在低硅钢基体中的扩散符合Fick扩散第二定律. Si-rich films were deposited on pure iron and low-Si steel substrates by direct current magnetron sputtering,and then were subjected to vacuum annealing.The distribution characteristics of Si across Fe and low-Si steel substrates were studied by energy spectrum analysis(EDS) and X-ray diffraction(XRD).DICTRA software was used to simulate the diffusion models.It is found that the diffusion behavior of Si in the Fe substrate is from γ-Fe(Si) phase to α-Fe(Si) phase and the rate of diffusion is con... 
2012-10-28 137 5.8

结合冶炼无取向硅钢的生产实际,对钢中硫的来源,以及炉渣性质、钢水温度、底吹强度对脱硫的影响进行了分析。研究表明,转炉钢中硫的主要来源为铁水、废钢、铁水渣及石灰带入;冶炼硅钢时,终渣碱度为3.0~3.5,w((FeO))≤20%,终点钢水温度大于等于1 680℃,加大底吹搅拌强度能提高转炉脱硫效果。硅钢平均出钢硫的质量分数为0.004 8%,能满足无取向硅钢对硫含量的要求。 With the actual production of non-oriented silicon steel,the source of sulphur and the effect of metallugic parameters like slag properties,temperature of molten steel and bottom stirring on desulphurizing ability were investigated.The results show that the main source of sulphur is molten metal,scrap,the remaining slag volume in hot metal and lime.The degree of desulphurization for smelting silicon steel can be increased through adopting the following measures,such as the basicity of finishing ... 
2011-02-28 174 5.8

对w(Si)=3%无取向硅钢进行表面机械研磨处理(SMAT)和异步轧制(CSR),获得表面纳米结构,再进行550~650℃、4 h固体粉末渗硅处理,用透射电镜(TEM)、扫描电镜(SEM)和X射线衍射仪(XRD)研究表层组织演变。结果表明:经过SMAT后,w(Si)=3%无取向硅钢表面形成了等轴状、取向呈随机分布的、晶粒尺寸为10 nm的纳米晶组织;异步轧制后,表面纳米晶组织保持不变;550~650℃、4 h渗硅处理后,SMAT+CSR样品表面形成化合物层,其厚度随着温度的升高由17μm增加到52μm;化合物层由Fe3Si和FeSi相组成. Nanostructured surface layer was fabricated on a 3%(mass fraction) non-grain oriented silicon steel by means of surface mechanical attrition treatment(SMAT) and cross-shear rolling(CSR),and then a solid powder siliconizing treatment was carried out for the SMAT+CSR sample at 550~650 ℃ for 4 h.The microstructural evolution was examined by using transmission electron microscopy(TEM),scanning electron microscopy(SEM) and X-ray diffraction(XRD).Experimental results show that: equiaxed nanocrystallin... 
2011-03-28 155 5.8

对无取向电工钢中的夹杂进行了系统的分析。利用小样电解,采取不同电解液,不同的分离方法对无取向电工钢中稳定和不稳定夹杂物进行了提取、分离和收集。利用扫描电镜(SEM)、X-射线衍射、ICP等对电解分离收集的夹杂物进行了定性和定量分析。 The inclusion analysis of the non-oriented electrical steel has been investigated.By using small sample electrolytic analysis,with different electrolytes and different separation ways,the stable inclusions and unstable inclusions was drew,separated,and collected.With utilizing the methods of SEM,X-ray and ICP,the qualitative and quantitative analysis of inclusions in the non-oriented electrical steel was obtained. 
2023-05-09 224 5.8

采用XRD、SEM和激光粒度仪等手段,观察并研究了不同特性氧化镁在硅钢表面形成硅酸镁底层形貌特点,并结合热力学和差热-失重分析了MgO-SiO2的反应机理。研究结果表明:粒度小,活性值高的特种氧化镁在高温退火过程中与基体表面氧化物生成的硅酸镁底层,界面中硅酸镁底层嵌入基体较多,表面致密,颗粒细小,有利于形成附着性能优良的硅酸镁底层。 Surface microstructure of Mg2SiO4 coatings formed on the surface of oriented silicon steel coated with different kinds of MgO was investigated by XRD and SEM.The reaction mechanism between MgO and SiO2 was analyzed by TG-DSC and thermodynamic calculation.Results revealed that when the MgO with finer microstructure size and higher activity is employed,a dense Mg2SiO4 layer with finer microstructure and good binding to the steel substrate can be obtained.The results are very helpful for the prepar... 
2011-10-28 160 5.8

【作者】 朱一知; 陈山; ...
2011-06-28 129 5.8

采用传统的轧制和退火工艺制备了0.30mm厚的6.5%(质量分数)Si高硅电工钢薄板,采用X射线衍射技术对退火过程中的再结晶织构进行了研究。冷轧高硅钢薄板700℃退火形成以{111}〈112〉为峰值的γ织构(〈111〉∥ND)和以{001}〈210〉为峰值的{001}织构;而900℃以上温度退火则形成强{001}〈210〉织构。进一步的研究表明是在晶粒长大过程中{001}〈210〉发展成为主要再结晶织构组分。 High silicon steel thin sheets with thickness of 0.3mm were successfully produced by conventional rolling and annealing methods.Recrystallization texture was investigated by means of X-ray diffraction.It is found that recrystallization texture is mainly composed of γ fiber(〈111〉∥ND)with peak at {111}〈112〉 and {001} fiber with peak at {001}〈210〉 after annealing at 700℃,while strong {001}〈210〉 component dominates recrystallization texture after annealing above 900℃.It is during grain growth that {... 
2011-11-28 201 5.8

介绍了国内无底层取向电工钢生产技术水平、产量和用途,简述了无底层取向电工钢作为取向电工钢超/极薄带母料及应用于制作大型发电机组铁心、风电等电机铁心和变压器铁心等的情况。 The production technology level,output and application of domestic glassless grainoriented electrical steel were introduced,and the application of glassless grain-oriented electrical steel as parent material of ultra-thin strip of grain-oriented electrical steel and in making large-scale electric generator cores,wind power motor cores and transformer cores were briefly described. 
2022-02-28 192 5.8

叠片系数是冷轧无取向电工钢的重要质量指标。为了提高叠片系数,必须保证无取向电工钢板形良好以及横向厚差小。针对攀钢冷轧厂4机架HC轧机轧制无取向电工钢的边部减薄问题,以无取向电工钢横向厚差最小作为目标函数,建立了一套针对无取向电工钢边部减薄控制的辊型曲线优化数学模型,开发了无取向电工钢专用辊型曲线,使无取向电工钢横向厚差从25μm降低到10μm以下,取得了良好的控制效果。 The lamination factor is an important quality index of non-oriented silicon steel strip.Considering the lamination factor,the non-oriented silicon steel must have a good shape and a smaller transverse thickness difference.In order to solve the edge thinning of non-oriented silicon steel strip in Panzhihua Steel,a mathematic model for designing the roll shape is built.In the model,the transverse thickness difference of non-oriented silicon steel strip is taken as the objective function.Based on t... 
2011-01-28 196 5.8

介绍了烟气余热利用系统的工艺流程及控制思想,结合该系统在钢厂硅钢连续退火机组中的应用实践,估算出烟气余热利用系统每年可节约蒸汽5 040 t,经济效益良好,同时分析了该系统存在的问题及对策。 Introduced a method about the process and control of the application of waste heat system, which had been used into a silicon steel continuous annealing line and profiting a good economic benefit by saving a large number of steam every year, which has been estimated about 5 040 tons, and analyzed the problems and solutions existed in this system. 