钢厂
表面机械研磨/异步轧制无取向硅钢薄带的渗硅行为
对w(Si)=3%无取向硅钢进行表面机械研磨处理(SMAT)和异步轧制(CSR),获得表面纳米结构,再进行550~650℃、4 h固体粉末渗硅处理,用透射电镜(TEM)、扫描电镜(SEM)和X射线衍射仪(XRD)研究表层组织演变。结果表明:经过SMAT后,w(Si)=3%无取向硅钢表面形成了等轴状、取向呈随机分布的、晶粒尺寸为10 nm的纳米晶组织;异步轧制后,表面纳米晶组织保持不变;550~650℃、4 h渗硅处理后,SMAT+CSR样品表面形成化合物层,其厚度随着温度的升高由17μm增加到52μm;化合物层由Fe3Si和FeSi相组成. Nanostructured surface layer was fabricated on a 3%(mass fraction) non-grain oriented silicon steel by means of surface mechanical attrition treatment(SMAT) and cross-shear rolling(CSR),and then a solid powder siliconizing treatment was carried out for the SMAT+CSR sample at 550~650 ℃ for 4 h.The microstructural evolution was examined by using transmission electron microscopy(TEM),scanning electron microscopy(SEM) and X-ray diffraction(XRD).Experimental results show that: equiaxed nanocrystallin...
提高热轧硅钢凸度精度的工艺措施
以太钢热连轧厂的硅钢为研究对象,利用凸度仪测量热轧带钢出口凸度值,采用矩阵和失效模式的分析方法了解影响带钢凸度变化的主次因素。研究结果表明:通过有效控制轧制过程中的加热温度、时间及采用合理的辊型,硅钢凸度精度提高了4.34%左右。 In this paper,we take the hot-rolled silicon steelsheet of Taigang as the research symbol,exit profile was measured by convex instrument,the primary and secondary factors that affect the strip profile were measured by using matrix and failure mode analysis methed.The results indicate that convexity accuracy has significantly improved by nearly 4.34% through the effective control of the heating temperature,heating time and the use of correct roller type in the process of hot rolling.
脱碳温度和脱碳时间对CGO取向硅钢碳含量控制的试验研究
通过测试取向硅钢不同工艺条件下的碳含量,探讨了CGO取向硅钢碳含量控制的最优处理条件,研究了脱碳温度和脱碳时间对相同初始碳含量取向硅钢的脱碳效果的影响。结果表明,在气氛为(15%~20%)H2+(75%~80%)N2,炉压差为10~20 Pa的条件下,CGO取向硅钢合适的脱碳温度为1 073 K~1 123 K,脱碳时间为10~20 min。在该处理条件下,能取得较好的脱碳效果。 By means of testing carbon content of oriented silicon steel below the distinct technical conditions,inquires the excellent handle terms of carbon content controlling for CGO oriented silicon steel,studies effects of decarburization annealing temperature and decarburization annealing time to the oriented silicon steel decarburization efficiency in same initial carbon content.The results show that,under the condition of atmosphere(15% ~ 20%) H2+(75% ~ 80%)N2 and furnace pressure difference 10 ~ 2...
热轧辊冷却对冷轧无取向电工钢卷纵向磁性的影响及工艺优化
通过对35W300高牌号0.35 mm冷轧无取向电工钢卷(/%:0.002C、2.71Si、0.22Mn、0.015P、0.003S、0.0020N、0.55Als)头、中、尾组织、织构及对应的磁性能的试验研究,发现因热轧时12 MPa高压水连续冷却造成接触轧辊的钢卷头、中、尾在不同温度下轧制,卷取后钢卷头部处于卷心、温度略高而冷却速度略低于钢卷尾部,致使钢卷纵向组织、织构不同,成品卷头、尾各250 m内磁感逐渐增加,铁损逐渐降低,250 m外至钢卷中部磁性能稳定。通过将热轧辊的冷却方式改为周期冷却和卷取后的层流冷却改为钢卷70 m后开始冷却,至钢卷尾部70 m前停止冷却的方式使得钢卷纵向铁损差异明显减小,磁感差异略有改善。 According to the test research on structure and texture of head,meddle and end of 35W300 high grade 0.35 mm cold rolled non-oriented electrical steel strip coil(/%:0.002C,2.71Si,0.22Mn,0.015P,0.003S,0.002 0 N,0.55Als) and corresponding magnetic properties,It is found that due to 12 MPa high pressure water continuous cooling the roller in hot rolling process led to head,middle and tail of strip rolling at different temperature and after coiling the head of strip coil being in center of coil led t...
电工钢中柱状晶对热轧和退火时晶粒取向及组织的影响
利用EBSD技术研究了电工钢中长轴平行于轧向的柱状晶样品在热轧和退火过程中组织和取向的演变规律,并与长轴平行于板法向的样品的已有研究结果进行对比。结果表明,无论柱状晶按何种方向排列,只要表面存在剪切力,热轧后都可形成剪切织构,同时中心形成轧制织构,主要包括旋转立方织构和{112}<1-10>。柱状晶造成的影响主要体现在板中心层,长轴平行于轧向排列的样品热轧时形成的粗大旋转立方晶粒要到脱碳退火后才能完全消除,但破坏了正常的不同取向晶粒间的取向差分布及尺寸均匀性,导致二次再结晶不完全及磁性能降低。 The evolution of microstructure and grain orientation in an electrical steel containing columnar grains with its long axis being parallel to the rolling direction of sheet was studied during hot rolling and annealing by EBSD technique.The results are compared with those of samples containing columnar grains being parallel to normal direction of sheet reported in the reference [3].It was shown that,whether the long axis of columnar grains was arranged in RD or ND,shear textures can be formed in t...
低温高磁感取向硅钢高温退火过程高斯晶粒的演变
对低温加热工艺生产的以AlN为主抑制剂的高磁感取向硅钢高温退火过程进行中断实验,借助电子背散射衍射技术对高温退火过程中高斯晶粒的演变进行了研究.在升温过程中高斯晶粒平均尺寸先减小再增大.800℃时取向分布函数图出现高斯织构组分,但强度很弱,高斯晶粒偏离角在10°以上;900℃时高斯晶粒平均生长速率超过其他晶粒;950~1000℃时高斯晶粒异常长大,偏离角3°~6°;在1000℃之前高斯取向晶粒相比于其他晶粒没有尺寸优势. The high-temperature annealing process of high permeability grain-oriented silicon steel with AlN as an inhibitor was studied by interrupting test.The evolution of Goss texture in this process was analyzed by electron back-scattered diffraction.It is found that the Goss grain size first decreases and then increases with the rise of temperature.Goss texture appears in the orientation distribution function at 800 ℃,but the intensity is very weak and the deviation angle is more than 10°.The average...
中低牌号无取向电工钢轧制工艺研究
热轧轧制工艺对产品性能和轧制稳定性影响很大,对中低牌号无取向电工钢,当在两相区轧制时,热轧塑性明显降低,板形变坏,易出现边裂等情况。以50W1000为例,通过对其变形抗力进行研究,得出把两相区控制在F4与F5之间为最佳轧制工艺的结论。在此基础上制定了一套较为合理的热轧工艺制度。采用新的轧制工艺后,50W1000热轧精轧的稳定性明显改善,热轧产品合格率由开发初期的40%左右提高到95%以上。 The hot rolling process has great influence on product′s performance and rolling stability.For the low medium grade non-oriented electrical steel,when non-oriented electrical steel is rolled in tow phase region,the hot rolling plasticity reduces obviously,the shape of strip goes bad and easily to crack at the edge.The deformation resistance of 50W1000 steel was investigated.The results show that the optimal rolling process is to control the two phase region between F4 and F5.Based on the results...
热轧无取向低硅钢SGG的研制开发及生产
针对川威950的工艺现状,结合无取向低硅钢SGG生产的工艺特点,主要从控制其钢坯加热和轧制以及终轧温度和卷曲温度几方面入手,进行无取向低硅钢生产的工艺控制研究。同时根据近6000吨的生产实践表明,该工艺措施能很好的满足该钢种的需要。 950 process Chuanwei status quo,with non-oriented silicon steel production process features low,mainly from the control of billet heating and rolling and finish rolling temperature and coiling temperature of several aspects,for non-oriented silicon steel production process of low control at the same time According to nearly 6,000 tons of production practice shows that the process measures could well meet the needs of the steel.
冷轧无取向电工钢的试制
利用本钢技术中心试验厂技术手段,并与北京钢铁研究院合作,试制了用作家电用电机、微电机、小电机或部分中型电机铁芯的冷轧无取向电工钢。试制钢硅含量小于0.5%,钢板表面平滑,公称厚度0.5mm,且厚度均匀偏差小,性能测定结果表明,产品的磁性能、力学性能满足其使用要求。 BX STEELTechnology Center pilot plant using technical means,and with Beijing Iron and Steel Research Institute,trial cold rolled non-oriented electrical steel that has been used as appliance motor core,micro motor core,small motor core,or part of the medium-sized motor core。Trial steel of silicon content is less than 0.5%,steel plate surface is smooth,the nominal thickness of 0.5mm,and the thickness deviation is small,performance measurement results show that the magnetic properties,mechanical p...
余热利用系统在硅钢连续退火机组中的应用
介绍了烟气余热利用系统的工艺流程及控制思想,结合该系统在钢厂硅钢连续退火机组中的应用实践,估算出烟气余热利用系统每年可节约蒸汽5 040 t,经济效益良好,同时分析了该系统存在的问题及对策。 Introduced a method about the process and control of the application of waste heat system, which had been used into a silicon steel continuous annealing line and profiting a good economic benefit by saving a large number of steam every year, which has been estimated about 5 040 tons, and analyzed the problems and solutions existed in this system.
冲剪加工对无取向硅钢边缘组织和磁性能的影响
通过观察冲剪边缘组织,测量冲剪边缘的显微硬度、残余应力的分布情况和磁性能的变化研究了冲剪加工对无取向硅钢50WW800边缘组织和磁性能的影响。对冲剪后硅钢片进行750℃退火,分析退火对组织和磁性能的影响。结果表明,硅钢片剪切边缘会存在0.4 mm的形变硬化层,边缘应力大,铁损增加。退火后变形减小,形变硬化层变小,残余应力大幅度减少,铁损减少。 The influence of punching process on cutting edge microstructure and magnetic properties of non-oriented silicon steel 50WW800was studied by observing microstructure and measuring microhardness near cutting edge.The residual stress distribution in the silicon steel tooth and magnetic properties were measured.Effect of annealing at 750 ℃ on microstructure and magnetic properties of the silicon steel was analyzed.The results show that a cut-edge hardening layer up to 0.4 mm is observed,residual st...
稀土处理无取向硅钢中夹杂物的控制
结合工业化生产的高效硅钢,进行了RH精炼稀土处理试验研究。针对不同的稀土处理条件,观察了夹杂物的形貌和尺寸分布,探讨了稀土处理后钢中的夹杂物形成、变化规律。结果表明:试验条件下,最佳的稀土合金添加数量为0.6~0.9 kg/t。经过合适的稀土处理后,可以有效抑制尺寸相对较小的、不规则的AlN、MnS复合夹杂生成,促进钢中微细夹杂物的聚合、上浮,钢质纯净度得到明显提高。此时,钢中全氧含量最低,脱硫效果最佳,钢中的夹杂物主要是尺寸相对较大的、近似球形或者椭球形的稀土类夹杂。 Based on the industrial production of non-oriented silicon steel,the experiment on RE treatment during the RH refining process was studied.The morphology and the size distribution were observed for the steel specimens treated with different RE treatment conditions.Further more,the formation and change of inclusions of final steel sheets after RE treatment were discussed.The results show that the suitable RE added amount was 0.6~0.9 kg/t.After the suitable RE treatment,the formation of AlN and Mn...