研究了冷轧大压下量,950℃退火时间对一种新型含铜无取向电工钢晶粒度和织构的影响。结果表明,大压下量冷轧,随压下量的增加,退火晶粒向γ线聚集,形成强{111}<112>织构。提高冷轧压下率,退火织构{111}<100>,{110}<001>强度减弱,增加退火时间,退火织构{111}<110>,{100}<001>,{110}<001>强度变弱。采用87.5%冷轧压下率和950℃退火60 s,有利织构{100},{110}占有率最大。 The effect of annealing(950 ℃) time with high cold rolling reduction on grain size and texture of a new non-oriented electrical steel containing copper was investigated.The results show that for high cold rolling reduction,most annealed grains are oriented along γ-fibre with increasing cold rolling reduction ratio and strong texture {111}<112> is formed.With increasing the cold rolling reduction ratio,the intensity of annealed texture {111}<110>,{011}<100> decreases.With increa... 
2011-01-28 583 5.8

借助于EBSD对比研究了常化退火对高牌号无取向电工钢热轧组织和织构演变的影响,分析了常化退火对热轧板各厚度层织构的演变规律。结果表明,常化退火改善了热轧组织的均匀性,并弱化了热轧变形的γ纤维织构。升高常化退火温度,可增大热轧板的晶粒尺寸,提高{100}和{110}织构组分占有率,有利于提高无取向电工钢成品板的磁性能。 Effects of normalizing annealing on microstructure and texture of high-grade non-oriented electrical steel hot-rolled sheet were investigated by EBSD. Emphasis was put on the effects of normalizing annealing on texture evolution in the sheet thickness. The results show that the hot-rolled microstructure homogeneity is improved and the γ-fiber texture is weakened by normalizing annealing treatment. The grain size of hot-rolled sheet and intensity of the {100} and {110} favorable texture can be in... 
2014-02-28 194 5.8

借助实验室设备研究了B元素对高牌号无取向硅钢热轧板组织和磁性能的影响。结果表明,与无硼钢相比,含硼钢的热轧板晶粒尺寸略小,析出物的类型和尺寸没有区别,主要是AlN和(AlN+MnS)复合析出物,少量的MnS析出物,尺寸集中在1.0~2.5μm范围内。未发现BN析出物。在力学性能方面,B对钢的软化作用不明显。在磁性能方面,含硼钢的铁损为3.215W/kg,磁感为1.710T,综合磁性能比无硼钢差。 Influences of boron on microstructure and properties of hot rolled band in high-grade non-oriented silicon steel are researched in this paper by experimental equipments.Compared with boron-free steel,the result shows that boron-bearing steel has smaller grain size,but the type and size of precipitations have no differences.The main precipitates are AlN,(MnS + AlN) composite precipitate and few MnS,the range of which are between 1.0 μm and 2.5 μm.BN precipitation is not found.With reward to mecha... 
2011-05-28 462 5.8

应用CAFE法对6.5%Si高硅钢铸锭凝固组织进行了模拟研究,确定出了适合高硅钢组织模拟的模型。进一步用该模型研究了过热度及冷却条件对凝固组织的影响,结果表明,随着过热度的降低,凝固组织中柱状晶比例和晶粒平均面积均减小。水冷条件下,高硅钢铸锭凝固组织几乎全是柱状晶,而且晶粒粗大。空冷条件下,等轴晶区扩大,但柱状晶仍占主要部分。缓冷条件下,等轴晶区占主要部分,晶粒平均面积和空冷条件下相当。 The solidification structure of 6. 5% Si steel ingot was simulated based on CAFE method and the model suitable for simulating the structure of high silicon steel wad ascertained. The influence of superheat and cooling condition on the solidification structure were studied. It was shown that with the superheat decreasing,the proportion of columnar crystals decrease,and the average grain size become smaller. Under water cooling condition,the solidification structure of casting was composed of almo... 
2023-05-06 405 5.8

【机构】 中国金属学会电工钢分会; ...
2011-06-28 322 5.8

本文介绍了无取向硅钢C6涂液的性能,研究了配水量、固化程度和涂层厚度等因素对无取向硅钢C6涂层性能的影响。结果表明,随着配水量的增加,完全固化所需的时间增加,涂液固体含量降低,涂层厚度减小;随着固化程度的提高,涂层硬度先增大然后趋于恒定,而柔韧性逐渐变差,在过固化后急剧恶化;涂层厚度对涂层的表面外观、附着性和绝缘层间电阻均有显著影响。 Based on the introduction about the performance of C6 varnish for non-oriented silicon steel sheets,effects of water amount,curing degree and coating thickness are discussed. Results show that with the increase of water amount,the time required to cure completely extends,and both the solid content of C6 varnish and the coating thickness decrease. As the curing degree increases,the hardness of the coating increases first and then tends to be constant,however the flexibility degenerates,especially... 
2014-02-28 368 5.8

研究了铝和铬元素在无取向电工钢晶粒长大过程中对织构及晶界变化的影响规律。试验结果表明:电工钢在晶粒长大过程中的主要织构组分均为{111}<112>。在晶粒生长期间,不加铝的1号试样中,{111}<112>、{111}<110>织构组分强化,而{100}<001>织构组分弱化;与1号试样相比,在加入0.2%的铝(质量分数,下同)的2号试样中,{111}<112>、{111}<110>织构组分强化(增加)的速率下降,{100}<001>织构组分变化不明显,甚至稍有增加。在含铝的试样中再加入0.3 5%的铬之后(3号试样),{111}<112>{、111}<110>和{100}<001>织构组分的变化规律与1号试样相似,但当电工钢中加入0.72%的铬之后(4号试样),上述3种织构组分的变化规律与2号试样相似。对于在晶粒生长期间持续变化的3种织构组分而言,1号试样的{1 1 1}<112>和{111}<110>织构组分的高(低)取向差角度晶界频率下降(... The effect rule of Aluminm and Chromium on texture and grain boundary transformation in the nonoriented electrical steel during grain growth was investigated.The experimental result shows that the main texture component is {111}<112> in the electrical steel.The {111}<112> and {111}<110> components in specimen 1 without Alumium were strengthened during grain growth whereas {100}<001> component was weakened.But the growth rate of {111}<112> and {111}<110> compon... 
2011-06-28 485 5.8

利用加热炉模拟、动态再结晶以及热模拟等试验方法以及扫描电镜、金相显微镜等分析观察手段对无取向硅钢边裂的成因进行了探讨。结果表明,长时间加热使得板坯边部晶粒异常长大,晶界氧化并脱碳,轧制过程中边部温度过低,动态再结晶过程变弱,使得板坯边部延伸性能变差,是导致硅钢边裂的主要原因。建议通过适当降低铸坯加热温度、缩短保温时间、提高终轧温度来改善硅钢边裂缺陷。 The behaviors of high temperature oxidation,dynamic recrystallization,and hot ductility,microstructure evolution were investigated on the non-oriented electrical steel sheets to discuss the formation of edge crack.The key causes of cracking was found to be the coarse as-cast microstructure,grain boundary oxidation and decarburization in reheating furnace,as well as reduced temperature at strip edge region during hot rolling process resulting in reduced hot ductility and lack of enough dynamic re... 
2013-02-28 240 5.8

为了确保硅钢铬酸盐涂料的环保性,需要严格控制涂料的固化工艺,保证涂料固化过程中涂料中的六价铬充分转化为三价铬。对涂料及原料进行热重分析(TG)及差示扫描量热法分析(DSC)。结果表明,MgO与铬酐混合转化为MgCrO4,使六价铬稳定性增强,其中大部分Cr6+转变为Cr3+发生在620~700℃,在450~500℃高于铬酐发生大量失重,因此必须加入还原剂保证涂料中六价铬被充分还原;超过360℃后树脂会发生分解,因此实际板温不能超过360℃;加入了还原剂的整体涂料的失重温度区间主要在260~320℃,因此涂料固化时钢板的实际温度最佳区间为320~360℃。 Because of the silicon steel chromate coating’s environmental requirements,the paint curing process must be controlled strictly to ensure all Cr( Ⅵ) transforms to Cr( Ⅲ). The TG and DSC analyses of the paint are studied. The reaction of MgO and CrO3 would generate MgCrO4,enhancing the stability of Cr( Ⅵ). The most r( Ⅵ) in MgCrO4 changes to Cr( Ⅲ) at 620-700 ℃,while the CrO3 has a large weight loss at 450-500 ℃. The reductant must be added in the paint to make sure the Cr( Ⅵ) could transform suf... 
2014-09-28 591 5.8

主要研究了0.7%Si无取向电工钢退火试样的组织、晶粒尺寸和织构对其磁性能的影响。结果表明,随着退火温度的升高,晶粒尺寸逐渐增大,组织的均匀性得到改善;ɑ取向线上的纤维织构多集中于{114}<110>和{223}<110>附近,再结晶结束后,织构含量变化不大。{111}<110>织构取向密度值随温度升高而下降,{112}<111>织构与{111}<110>织构变化相反。晶粒尺寸增大对磁感强度的影响较小,而对铁损的影响较大。 Influences of microstructure,grain size and texture on the magnetic properties of 0.7% Si non-oriented electrical steels annealed samples were studied.The results show that with annealing temperature increasing the average grain size is increased gradually.Uniformity of the microstructure is improved;the textures of ɑ-fiber gathered in the vicinity of the { 114} < 110 > and { 223 } < 110 > texture.After recrystallization,the volume fraction of texture changes small.{ 111} < 110 &g... 
2013-07-28 224 5.8

通过制备磷酸二氢铝硅钢涂层,研究了氧化锌对无铬涂层耐盐雾性能、电化学性能和附着性的影响。结果表明,硅钢表面涂层含有4.0%的氧化锌时,涂层具有最高的耐腐蚀性能和电化学性能,而且其致密表面最为平整,没有裂纹出现。 The effects of ZnO on the salt spray resistance property, electrochemical performance and adhesiveness of silicon steel insulating coating were studied. The results show that the best corrosion resistance and electrochemical properties can be obtained when the coating contains 4.0% oxide zinc, and the dense surface is smooth without cracks. 
2014-07-28 242 5.8

对高牌号无取向电工钢国内生产情况、工艺技术、产品性能及应用领域等进行了阐述,并探讨了高牌号无取向电工钢产品的发展趋势。 This paper introduces basic facts on the production status,process technology and products’ properties and their applications of non-oriented electrical steel with high grade at home,and then discusses the development trend on technology for producing the non-oriented electrical steel with high grade. 
2011-02-28 224 5.8