稀土元素在许多钢中发挥着独特而且不可替代的重要作用。半个世纪以来,它的作用已经在各种低合金和特殊合金钢中的研究及应用中得到充分的证明;然而,作为具有稀土资源优势的中国,在属于重要功能材料的无取向电工钢中稀土的应用却落后于国外,本文就中国稀土在无取向电工钢中的应用研究作简要的评述,希望能够进一步推进此领域的研究,并且促进中国稀土在无取向电工钢中应用技术的发展,缩短与国外差距,并提出了在此应用领域今后需深入开展的研究方向。 Rare earth elements play a unique and irreplaceable role in a lot of steels,it has given the full proof by the practice of various low alloy steels and special alloy steels since half century.However,as our country has the advantage of rare earth resources,RE application technology in non-oriented electrical steels has lagged behind abroad.The application researches of rare earth in non-oriented electrical steel in our country are briefly reviewed in this paper,which hope to promote the research... 
2014-05-28 151 5.8

介绍了普通取向硅钢(CGO)和高磁感取向硅钢(Hi-B)铸坯高温加热两次冷轧、一次冷轧和铸坯低温加热两次冷轧、一次冷轧法4种成熟生产工艺的主要技术参数,取向硅钢理论研究(Goss晶核和抑制剂)和生产技术现状。取向钢的发展趋势为:提高(110)[001]晶粒取向度,降低取向硅钢铁损,发展铸坯低温加热(≤1 300℃)和薄板坯连铸连轧流程生产取向硅钢工艺。 Main technology parameters of four developed process:cast bloom higher temperature heating-double cold rolling or single cold rolling,lower temperature heating-double cold rolling or single rolling process for production of common grain oriented silicon steel(CGO) and high magnetic induction grain oriented silicon steel(Hi-B),theory research on grain oriented steel(Goss nucleus and inhibitor) and present situation of process are summarized in this paper.The development trend of grain oriented si... 
2013-05-28 165 5.8

从取向硅钢生产路线的选择、工艺技术的改进和生产设备的改造三方面进行了生产取向硅钢的节能降耗技术改造.通过完善多元抑制剂配方生产低温取向硅钢,通过加抛丸的酸洗、带面超声波清洗、改进连续退火炉以及余热循环利用等技术改造,使2012年取向硅钢的产量与未进行技术改造前的2009年相比提高了2.5倍,产品磁性上升了一个半牌号,能耗下降了8.9%,成材率提高了6.4%,生产成本下降了22%,综合效益显著. Energy saving technological transformation was carried out in the production of grain oriented silicon steel from three aspects of the oriented silicon steel production process route selection,technology improvement and equipment renovation.Through the improvement of multiple inhibitor formulations for producing low-temperature grain-oriented silicon steel,and by adding the blasting pickling,the belt surface ultrasonic cleaning,improvement of continuous annealing furnace,waste heat recycling tec... 
2013-02-28 182 5.8

采用自主研发的脉冲磁场退火装置,在取向硅钢脱碳退火过程中分别施加不同强度的磁场,并采用光学显微镜和X射线衍射仪研究了脉冲磁场脱碳退火后试样的显微组织和宏观织构。结果表明,脱碳退火过程中施加脉冲磁场后取向硅钢的平均晶粒尺寸均增加,当磁场强度为40 mT时,平均晶粒尺寸最大,为13.06μm。此外,取向硅钢试样的立方织构{001}<100>强度减弱,高斯织构{110}<001>和{111}<112>织构增强,有利于获得更好的成品织构和磁性能。 Self-developed pulsed magnetic field annealing device was used to apply magnetic field of different intensities during decarburization annealing of an oriented silicon steel, and microstructure and macro-texture of the specimens after decarburization annealing in a pulsed magnetic field were studied by using optical microscope and X-ray diffractometer. The results show that the average grain size of the oriented silicon steel increases with the application of pulsed magnetic field during decarbu... 
2022-02-28 184 5.8

依据GB/T 15616—2008《金属及合金的电子探针定量分析方法》,采用电子探针波谱仪对某W600硅钢中的硅含量进行了定量测定,对影响其定量测定结果的不确定度分量进行了分析,并对不确定度的各个分量进行了计算和合成,最后给出了硅钢中硅含量测定结果的不确定度报告:该硅钢中的硅含量(质量分数)为1.50%,扩展不确定度U=0.20%,取包含因子k=2。 According to GB/T 15616-2008\"Quantitative Method for Electron Prohe Microanalysis of Metals and Alloys\",the quantitative results of Si content in some W600 silicon steel was measured hy EPMA-WDS.The uncertainty components which might affect the measurement results were considered,calculated and synthesized. Finally the uncertainty result for the quantitative value of Si content in the silicon steel was got.The mass content of Si was 1.50%,and expanded uncertainty U=0.20%under the condition of co... 
2011-06-28 149 5.8

概述了无抑制剂法生产取向电工钢的特性及其用途;总结无抑制剂生产取向电工钢的原理及工艺方案.重点讨论了成分方案,即元素对磁性能的影响和最终高温退火方案对二次再结晶的影响.研究结果表明,无抑制剂取向硅钢化学成分范围没有普通取向硅钢和高磁感取向硅钢严格,提高了成材率;最终高温退火决定了二次再结晶的好坏,从而最终决定成品磁性能,最佳的高温退火温度在850~950℃之间. This article provides an overview on the characteristics and uses of inhibitorless process producing grain-oriented electrical steels.The mechanism of inhibitorless process and technology programs were discussed.The results show that the chemical composition and final annealing were determined according to magnetic properties.The inhibitor-free grain oriented silicon steel has loose range of chemical composition;Secondary recrystallization occurs mainly in the final annealing and the best anneal... 
2012-04-28 158 5.8

介绍在取向硅钢生产中抑制剂的作用以及多元抑制剂的机理和应用情况,分析多元抑制剂方案中各种元素对高磁感取向硅钢性能的影响,并根据生产实践提出了进一步研究的方向. The role of an inhibitor in the production of grain oriented silicon steel,and the mechanism of multiplex inhibitor in the production are described in the present article.In addition,the influence of various elements in the multiplex inhibitor on the performance of grain oriented silicon steel with high magnetic induction is elucidated.Further work needed in this research is also indicated. 
2013-01-28 150 5.8

【作者】 凌健; ...
2011-03-28 145 5.8

采用X射线衍射仪分析无取向硅钢冷轧织构和再结晶退火织构的演化,研究了热轧组织对无取向硅钢织构以及磁性能的影响。结果表明,具有均匀、粗大晶粒组织的热轧板,冷轧形成更多的剪切带,导致成品板形成高的高斯织构组分,并提高了{100}织构强度,降低了γ纤维织构,最终导致成品磁感应强度升高,铁损下降。 The texture evolution of non-oriented silicon steel during cold-rolling and recrystallization annealing was investigated by X-ray diffractometer.The effects of hot band microstructure on the texture and magnetic properties of non-oriented silicon steel were analyzed.The results show that more shear bands appear during cold rolling due to homogeneous coarse grain in hot band.So strong{110}<001> texture after recrystallization annealing forms.At the same time,the {100} texture components inc... 
2023-05-09 207 5.8

在50Kg氧化镁坩埚真空感应炉上进行高硅电工钢的脱氧试验。结果表明,通过控制原料的成分、高真空下的碳氧反应和炉衬分解向钢液中的供氧,可使钢液的总氧含量≤15×10-6;在维持高温高真空条件下,当钢液中的反应达到一定程度后,延长精炼时间并不能降低钢液的总氧含量;完成精炼后加入硅钙合金沉淀脱氧可进一步降低钢液的总含氧量,但脱氧效果有限。 The test of high-silicon electric steel deoxidation has been carried out in 50Kg vacuum induction furnace with magnesium oxide crucible.Results show that the total oxygen could be ≤15×10-6in molten steel by controlling material components,carbon-oxygen reaction in high vacuum and oxygen contamination from crucible materials on molten steel;And when the reaction was carried through to a certain extent,total oxygen in molten steel could not be reduced by the extension of refining period in high va... 
2011-02-28 172 5.8

利用电子背散射衍射(EBSD)技术和场发射电子扫描显微镜(FESEM)研究了电工钢中柱状晶不同初始取向50%热压缩变形后的演变规律及其对粒子析出行为的影响。结果表明:〈100〉晶粒形变后仍为〈100〉取向,只发生绕ND∥〈100〉方向的转动,具有遗传性,粒子析出数量少。柱状晶长轴与压缩轴的偏转度增加,取向的稳定性变差,超过40°,可形成〈111〉取向,期间发生复杂的滑移系交互作用,产生较高的缺陷密度,促进粒子析出。MnS粒子主要在晶内析出,变形温度高、形变量低,粒子均无法充分析出。回复时,形变晶粒内高的储能和缺陷密度是促进粒子进一步析出的必要条件。 The evolution of initial orientations and their influence on precipitation of columnar-grained electrical steel after 50% hot compression deformation were investigated by electron backscatter diffraction technique and field emission scanning electron microscopy.The results indicate that the〈100〉orientated columnar grains remain still〈100〉after hot compression deformation,with only rotation around ND parallel to〈100〉direction,with heredity,and less precipitation.As the deviation angle between the... 
2014-10-28 155 5.8

借助光学显微镜、扫描电镜、交流磁性能测量仪和万能拉伸试验机研究了0.3 mm厚高强无取向电工钢冷轧板在780、820、860和900℃退火保温2 min后的组织、织构和性能。结果表明:在退火温度范围内,试验钢均发生了完全再结晶,得到等轴状的铁素体晶粒;随着退火温度的升高,平均晶粒尺寸从9.2μm增长到41.3μm,工频铁损和400 Hz高频铁损均先大幅减小后趋于平缓,磁感应强度先升高后降低。在820℃退火时,铁损P1.5/50=5.51 W/kg,P1.0/400=33.22 W/kg均处于较低值,磁感应强度B5000最大,为1.649 T。试验钢的屈服强度和抗拉强度均随退火温度的升高而降低,780℃退火时屈服强度为496 MPa, 900℃退火时降低至407 MPa。综合磁性能和力学性能考虑,试验钢的最佳退火温度是820℃。 Microstructure, texture and properties of 0.3 mm thick high strength non-oriented electrical steel cold rolled sheet annealed at 780 ℃, 820 ℃, 860 ℃ and 900 ℃ for 2 min were studied by means of optical microscope, scanning electron microscopy, AC magnetic property tester and universal tensile testing machine. The results show that in the annealing temperature range, complete recrystallization of the experimental steel occurs and equiaxed ferrite grains are obtained. With the increase of annealin... 