表面机械研磨/异步轧制无取向硅钢薄带的渗硅行为
对w(Si)=3%无取向硅钢进行表面机械研磨处理(SMAT)和异步轧制(CSR),获得表面纳米结构,再进行550~650℃、4 h固体粉末渗硅处理,用透射电镜(TEM)、扫描电镜(SEM)和X射线衍射仪(XRD)研究表层组织演变。结果表明:经过SMAT后,w(Si)=3%无取向硅钢表面形成了等轴状、取向呈随机分布的、晶粒尺寸为10 nm的纳米晶组织;异步轧制后,表面纳米晶组织保持不变;550~650℃、4 h渗硅处理后,SMAT+CSR样品表面形成化合物层,其厚度随着温度的升高由17μm增加到52μm;化合物层由Fe3Si和FeSi相组成. Nanostructured surface layer was fabricated on a 3%(mass fraction) non-grain oriented silicon steel by means of surface mechanical attrition treatment(SMAT) and cross-shear rolling(CSR),and then a solid powder siliconizing treatment was carried out for the SMAT+CSR sample at 550~650 ℃ for 4 h.The microstructural evolution was examined by using transmission electron microscopy(TEM),scanning electron microscopy(SEM) and X-ray diffraction(XRD).Experimental results show that: equiaxed nanocrystallin...
电感耦合等离子体质谱法测定硅钢中痕量铜和镍
研究了应用电感耦合等离子体质谱法(ICP-MS)测定硅钢中痕量铜和镍的分析方法。采用硝酸分解样品,通过内标校正和基体匹配消除了基体干扰的影响,同时根据测量时存在的质谱干扰情况,选择同位素65Cu和60Ni作为测定元素和通过调节仪器参数使双电荷离子的产率最低,以减少带来的干扰。该方法用于硅钢中痕量铜和镍的测定,所得的结果与ICP-AES法测定结果完全吻合,各元素测定结果的RSD值小于5%,加标回收率为97.3%~100.3%。 A method for the determination trace copper and nickel in silicon steel by inductively coupled plasma mass spectrometry(ICP-MS) was studied.The samples were dissolved in HNO3.The effect of matrix interference was eliminated by internal standard correction and matrix matching.Meanwhile,according to the mass spectral interferences in determination,the isotopes including 65Cu and 60Ni were used as measuring elements.The yield of double-charge ions were minimized by adjusting instrumental parameters...
无取向硅钢钙处理前后夹杂物的行为研究
研究了无取向硅钢钙处理前后夹杂物的行为,重点考察了钙处理前后夹杂物的成分、类型、形貌和尺寸研究的变化情况,为实际生产中无取向硅钢的钙处理提供理论指导。试验发现:钙处理前夹杂物主要以Al2O3、Al2O3-MgO为主,且在夹杂物表面有AlN析出,钙处理后夹杂物以Al2O3-MgO-CaS-CaO系复合夹杂物为主,还含有少量的SiO2或AlN;钙处理前后,夹杂物形貌由多边形或不规则形逐渐向球形或近似球形转变,并且夹杂物尺寸不断增大;钙处理前后,含钙夹杂物的比例发生突变,由10%增大到74.5%,且随着钙处理时间的延长,含钙夹杂物比例下降,表明钙处理使夹杂物变性后易聚集长大并上浮去除。 Behavior of inclusions before and after calcium treatment in non-oriented silicon steel was researched by investigating changes of compositions,types,shapes and sizes of inclusions before and after calcium treatment,for the purpose of providing theoretical guidance for calcium treatment of non-oriented silicon steel in actual situation. Results indicated that Al2O3 and Al2O3-MgO were main types of inclusions before calcium treatment,sometimes AlN maybe precipitate in the outer of inclusions. Al2...
初次再结晶退火工艺对3%Si取向硅钢组织和织构的影响
试验研究了0.3 mm取向硅钢冷轧板(/%:0.046C,3.07Si,0.09Mn,0.029P,0.004S,0.005A1)的退火温度(760~880℃7 min)和退火时间(820℃3~9 min)对该钢的晶粒尺寸,再结晶和织构的影响。结果表明,最佳初次再结晶退火工艺为820℃5 min,该钢的平均晶粒尺寸为14.20μm,完全再结晶率为92%,不利{111}<110>结构含量为3.16%,有利织构{111}<112>,{012}<001>和高斯织构含量分别0.40%,4.73%和2.46%。 The effect of annealing temperature(at 760 ~ 880 X.for 7 min) and time(at 820℃ for 3~9 min) on grain size,recrystallization rate and texture of 0.3 mm cold-rolled sheet of oriented silicon steel(/%:0.046C,3.07Si,0.09Mn,0.029P,0.004S,0.005Al) has been tested and studied.Results show that with optimum recrystallized annealing at 820℃ for 5 min,the silicon steel average grain size is 14.20 fun,the complete recrystaUization rate is 92%,the unfavourable-texture {111}< 110 > content in steel is ...
冷轧无取向硅钢表面麻面缺陷成因分析及其控制措施
针对某厂DMS森吉米尔轧机生产无取向硅钢表面麻面缺陷的问题,根据生产实际,对其形成原因从乳化液及工作辊两方面因素进行了分析。结果表明:乳化液对麻面缺陷的产生有一定影响,但不是主要因素,主要原因是由于二十辊森吉米尔轧机工作辊辊径较小,轧制相同长度带钢轧辊运转周期较大,容易产生疲劳失效而导致。为此,提出通过调整冷轧工序成品轧制道次的压下率以减小轧制力,从而减小工作辊的磨损疲劳;通过对轧制乳化液浓度、温度的合理控制,以改善润滑效果、提高轧制速度,而进一步缓解轧辊疲劳的改进措施,使该钢厂无取向硅钢麻面缺陷发生率由原来的18%降至0.8%,带钢表面质量明显改善。 For the problem of surface pockmarks of non-oriented silicon steel strip produced by a DMS Sendzimir mill, based on the production practice, the formation causes were analyzed from two aspects of emulsion and working roll. The results show that the emulsion has a certain effect on the formation of surface pockmarks defects, but it is not the main factor. The main reason is that the working roll diameter of the 20-high Sendzimir mill is small, and the running period of the roll rolling the same l...
冷轧压下量对取向硅钢极薄带显微组织的影响
观察了取向硅钢极薄带经冷轧至不同厚度,并经过不同工艺热处理后的显微组织及亚结构。结果表明:冷轧压下量越大,显微组织中位错密度越高,冷变形组织越多,等轴晶粒越少;增加冷轧压下量可以使试样的再结晶温度降低,当钢带厚度为0.08 mm时,在650℃退火时就能发生明显的再结晶。 Microstructure and substructure of the grain oriented ultra-thin silicon steel sheets is analyzed,which are rolled down to different thickness and treated with different heat treatment process.The result shows that there are higher dislocation density,more cold deformation structure and less equiaxed crystal grain in microstructure of the steel sheets with more cold rolled reduction.Increase of cold rolled reduction will decrease recrystallization temperature,and when thickness of the steel shee...
Nb微合金化Fe14Si2高硅钢温轧板织构演变规律
采用Nb对Fe-6.5%Si(质量分数)高硅钢进行微合金化处理,结果表明:Nb在高硅钢薄板制备过程中细晶效果明显.铸态、锻态和热轧态组织的晶粒分别细化了17.50%,24.51%和30.13%.铸态样品压缩强度由1365 MPa提高至1520 MPa,延伸率提高77.78%;温轧板试样室温拉伸强度由573 MPa提高至621 MPa,延伸率提高44.44%.利用XRD对厚度为0.30—1.68 mm的温轧板的板面织构演变过程进行跟踪测量,结果发现:初始织构以(011)〈100〉Goss织构为主,单道次变形量为26.2%的情况下,Goss织构完全转化为(100)〈011〉旋转立方织构,随后,在单道次变形为22.6%的情况下,旋转立方织构完全转化为{111}面织构,即纤维织构,并稳定保持至0.30 mm. Fe-6.5%Si(mass fraction) alloy possess perfect magnetic properties,though intermetallics of Fe14Si2 phase brought 6.5%Si leads to room temperature brittleness and hinder this significant materials industrialization.Nb was adopted into micro-alloying of Fe-6.5%Si high silicon steel. OM,thermal simulated test machine and XRD were employed to study the influence of Nb on high silicon steel in processing stages.Textures of warm-rolled high silicon steel strips were determined b...
多元抑制剂对高磁感取向硅钢性能的影响
介绍在取向硅钢生产中抑制剂的作用以及多元抑制剂的机理和应用情况,分析多元抑制剂方案中各种元素对高磁感取向硅钢性能的影响,并根据生产实践提出了进一步研究的方向. The role of an inhibitor in the production of grain oriented silicon steel,and the mechanism of multiplex inhibitor in the production are described in the present article.In addition,the influence of various elements in the multiplex inhibitor on the performance of grain oriented silicon steel with high magnetic induction is elucidated.Further work needed in this research is also indicated.
硅钢常化炉段工艺特征及问题分析
连续酸洗退火机组(CPAL)对于当前生产高磁感取向硅钢和高牌号无取向硅钢是必不可少的一个环节。常化炉是常化酸洗机组关键的组成部分。本文对国内自主建造的两条退火酸洗机组的工艺流程,特别是常化炉段进行了对比分析。总结出了常化炉的工艺及组成特点,对生产过程中暴露的问题进行了仔细的分析并提出了改进的意见,对于以后新建常化炉具有一定的提示作用。 The continous pickling annealing line(CPAL) is an essential step in producing high magnetic induction grain-oriented silicon steel and high grade non-oriented silicon steel.The normalizing furnace is a very important part of the CAPL.In this paper,the process flows of two CAPL with independent manufacture in our country have been compared,especially the part of normalizing furnaces.The characteristics of process and component are summarized and problems of the normalizing furnace during the prod...
常化温度对TSCR流程制备低碳低硅无取向硅钢组织和性能的影响
在实验室试制了TSCR流程的低碳低硅无取向硅钢,研究了在850~1050℃不同温度常化对冷轧量0.5mm厚钢板再经950℃×7min退火后的组织、织构和磁性能的影响。结果表明:随常化温度的升高,使热轧板晶粒尺寸增大,晶界更清晰,组织均匀性更好;由于第二相AlN和MnS析出物尺寸比较大,使冷轧退火后钢板晶粒也随常化温度升高呈单调增大趋势;γ有利织构和{111}、{112}不利织构与常化温度升高同时增强,但前者增强更多;冷轧板退火后铁损随常化温度升高呈单调下降,磁感呈单调上升趋势。 The low-carbon and low-silicon non-oriented silicon steel was prepared by thin slab casting and rolling(TSCR) in lab.The effect of normalizing at different temperatures in 850-1 050℃on microstructure, texture and magnetic properties of 0.5 mm cold-rolled sheets after annealing at 950℃for 7 min was researched. The results show that with increasing the normalizing temperature,the grain size of hot-rolled sheets increased,the grain boundaries were more clear and the rnicrostructure uniformity was b...
获得抑制剂法生产低温高磁感取向硅钢的抑制剂控制研究进展
综述了国内外大钢铁企业与研究机构采用获得抑制剂法生产低温高磁感取向硅钢的开发及应用情况,分析了以该法生产高磁感取向硅钢过程中抑制剂的控制技术,包括固有抑制剂组成方案、气态渗氮方式与工艺及高温退火工艺的制定.研究表明,固有抑制剂组成方案的设计思路大体一致,化合物抑制剂以AlN为主、硫化物为辅,同时添加少量Sn,Sb等单元素抑制剂,但组成元素含量存在一定差别;在脱碳退火后用NH3进行非平衡渗氮处理已成为气态渗氮的主要方式,但最佳方式仍未明确,具体选择需依据实际生产条件,相应脱碳及渗氮工艺的控制条件差别较大;高温退火工艺中升温制度差别不大,升温阶段退火气氛中N2含量的选择存在差别.此外,分析了抑制剂控制技术目前存在的关键问题,并指出了进一步的研究方向. The current application and exploitation on production of low-temperature high magnetic induction grain-oriented silicon steel with acquired inhibitor method at both iron and steel enterprises and research institutions in the world are reviewed. The control techniques of inhibitors, which include the composition design for inherent inhibitors, nitriding method and process, and secondary recrystallization annealing, are thoroughly analyzed and proposed. It is indicated that the design ideas for i...
退火温度对无取向电工钢组织和磁性能的影响
主要研究了0.7%Si无取向电工钢退火试样的组织、晶粒尺寸和织构对其磁性能的影响。结果表明,随着退火温度的升高,晶粒尺寸逐渐增大,组织的均匀性得到改善;ɑ取向线上的纤维织构多集中于{114}<110>和{223}<110>附近,再结晶结束后,织构含量变化不大。{111}<110>织构取向密度值随温度升高而下降,{112}<111>织构与{111}<110>织构变化相反。晶粒尺寸增大对磁感强度的影响较小,而对铁损的影响较大。 Influences of microstructure,grain size and texture on the magnetic properties of 0.7% Si non-oriented electrical steels annealed samples were studied.The results show that with annealing temperature increasing the average grain size is increased gradually.Uniformity of the microstructure is improved;the textures of ɑ-fiber gathered in the vicinity of the { 114} < 110 > and { 223 } < 110 > texture.After recrystallization,the volume fraction of texture changes small.{ 111} < 110 &g...