钢厂
硅钢高温退火环形炉炉壳制作与安装技术
硅钢高温退火环形炉炉壳制作与安装精度要求较高,施工时通过对壳体原材料矫正、炉壳板拼焊、下料切割、型钢骨架组装及焊接、骨架及炉壳板矫正、骨架与炉壳板组装及焊接、炉壳矫正、零配件装置、定位钻孔、报验检查、出厂、内侧板安装、外侧板安装、顶板安装等环节的工艺技术控制,能保质高效地完成硅钢高温退火环形炉炉壳制作与安装,为以后同类工程的施工提供可借鉴经验。 The required precision of manufacture and installation technique of the silicon steel high temperature annealing annular-furnace shell is high.During construction , manufacture and installation of the silicon steel high temperature annealing annular-furnace shell could be finished high efficiently through correcting the raw materials of shell , furnace shell plate welding , material cutting , steel frame assembly and welding , skeleton and shell plate correction , skeleton and furnace shell asse...
无取向电工钢环保绝缘处理液试验研究
针对目前大部分无取向电工钢处理液为含铬处理液、且需在较高温度下固化的情况,在分析成膜物质性质的基础上,试验研究了一种可低温快速固化的电工钢环保绝缘处理液,研究了其涂装工艺,并测定了涂层的附着性、绝缘性、耐热性、耐蚀性等性能。试验结果表明:该处理液可在150~250℃下快速烘干固化,涂层表面光滑且致密均匀,性能优良,可满足中小电机的使用要求。 At present,most of the insulating fluid for non-oriented electrical steel contains chromium,and should be cured at high temperature.On the basis of analyzing the characteristics of the film-forming substance,a kind of eco-friendly insulating fluid with lower curing temperature for non-oriented electrical steel sheet was developed in the experiments.Then its coating process was studied,and the adhesiveness,insulativity,heat resistance,corrosion resistance and other properties of the coating was m...
双辊连铸法制备硅钢薄带的组织和性能
采用双辊连铸工艺制备了硅的质量分数分别为0.5%,1.0%,3.0%,4.5%的硅钢薄带,用光学显微镜观察其组织,并研究了后处理工艺对薄带组织和性能的影响。结果表明:硅含量为0.5%和1.0%的薄带适合采用一次冷轧+850~950℃退火的后处理工艺,而硅含量在3.0%以上的薄带适合采用二次冷轧+950℃退火的后处理工艺;硅含量为3.0%和4.5%的薄带在冷轧并950℃退火后,其磁性能最佳,铁芯损耗约为4.30 W·kg-1,磁感应强度约为1.68T。 Silicon steel thin strips with silicon content of 0.5wt%,1.0wt%,3.0wt%and 4.5wt%were prepared by twin-roll continuous casting process,and the microstructure of the strips were observed by means of optical microscopy,and on the basis,the effect of post-treatment process on microstructure and properties of the strips was studied.The results show that the post-treatment process of one-time cold rolling and annealing between 850—950℃was suitable for the strips with silicon content of 0.5wt%and 1.0wt...
压下率对6.5%Si电工钢温轧板织构的影响规律
6.5%Si电工钢是一种优异的软磁材料,织构对其磁性能影响很大。利用温轧工艺对6.5%Si电工钢热轧板进行不同压下率轧制,研究了温轧板织构随压下率的变化规律。实验结果显示,随着压下率的增大,{100}〈110〉、{110}〈100〉和γ纤维织构在薄板表层中的强度先增强后减弱,当压下率达到75%时,沿板厚方向形成3个组织区域:表层细晶粒区({110}〈100〉取向为主)、过渡层({111}〈110〉和{111}〈112〉变形晶粒区)和中心层(以拉长的γ纤维织构和{100}〈110〉取向晶粒为主),这种组织和织构不均性对后期织构的发展有重大影响。 6.5wt% Si electric steel has excellent soft magnetic properties,on which texture play important role.In this experiment,warm rolling technique was employed to investigate the effect of rolling reduction on texture.It was found that the density of {100}〈110〉,{110}〈100〉 and γ-fiber textures first increased and then decreased with increasing of the rolling reduction.At 75% reduction,the microstructure along the thickness of the sheet formed three zones,containing surface layer with {110}〈100〉 orien...
高硫硅钢的硫化物析出行为及其微观组织和电磁性能变化
为了弄清楚高硫硅钢中的硫化物析出行为及其对钢的微观组织和电磁性能的影响,以便为工业化生产制定更为合理的硫含量控制标准和采取更为有效措施减轻炼钢生产的硫含量控制压力,结合0.25% Si 无取向硅钢 ,采用非水溶液电解提取 + 扫描电镜/透射电镜观察相结合的方法 ,研究了0.006 8%、0.010 2%、0.025 5% 和 0.035 3% 硫含量条件下,钢中的硫化物夹杂物组成和存在形式及其形貌、种类、尺寸、数量变化,以及相应的热轧、成品试样的微观组织和电磁性能变化。结果表明,随着钢中硫含量的增加,钢中的硫化物逐渐由 MnS→MnS+Cu2S→Cu2S转变,数量逐渐增多,尺寸向高低两个方向发展。相应地,导致热轧再结晶组织劣化和抑制了成品晶粒尺寸长大。随着钢中硫含量的增加,钢的磁感、铁损劣化程度逐渐增大。钢中的硫含量平均每增加 0.01%,涡流损耗、磁滞损耗分别劣化0.24 W/kg 和 0.41 W/kg,而磁感会劣化 0.009 T。但是 ,在硫含量为 0.010 2% 时 ,铁损可以低于 6.0W/kg,而在硫含量为 0.025 5% ... In order to find out the precipitation behavior of sulfide inclusions and the corresponding changes of microstructure and electromagnetic properties of high sulfur silicon steel sheets, so that to design more suitable sulfur concentration controlling limit for industrial manufacture and to release the steel-making difficulty effectively, Based on the change of given sulfur concentration 0.006 8%, 0.010 2%0.025 3% and 0.035 3%, the type and composition, the size and number, and the size distribut...
提高硅钢卷材下料利用率的几种方法
阐述了影响硅钢卷材下料利用率的因素,并结合具体事例利用计算机排样系统进行了详细分析,对提高硅钢卷材的利用率具有一定的指导作用。 It describes the factors influenceing the the utilization ratio of the roll of Silicon steel,and analyzes it in detail combined with concrete examples by a computer arrangement system,which can give a guide for increasing the utilization ratio of the roll of Silicon steel.
辉光放电发射光谱法测定硅钢薄板中微量硼元素
通过对辉光放电发射光谱参数的优化,以铁元素为内标来消除基体效应,建立了测定硅钢薄板中微量硼元素的方法。优化的实验参数为:放电电压1200 V,放电电流50 mA,预溅射时间40 s,积分时间10 s。校准曲线硼元素含量范围0.0001%~0.022%,相关系数大于0.999,测量结果与认定值一致,相对标准偏差小于10%。完全能够满足日常分析测试的要求。 A glow discharge optical emission spectrometry(GD-OES) method for determining trace boron element in silicon steel sheets were established through optimization of instrumental parameters and using Fe element as an internal standard to eliminate the matrix effect.The optimized instrumental parameters included discharge voltage,discharge current,pre-sputtering time and integration time,which are 1200 V,50 mA,40 s,and 10 s,respectively.The content of boron element that can be determined from the ca...
压下率对取向硅钢热轧板织构的影响
采用X-射线衍射分析技术测定了取向硅钢热轧板在不同压下率下不同厚度处的织构。结果表明,在压下率低于80%的情况下,几乎所有试样的不同厚度处的织构均为旋转立方织构类型{100}<011>,但不同压下率、不同厚度处的织构强度存在很大差异;在压下率大于80%的情况下,不同试样的不同厚度处的织构类型发生了变化,其织构类型为旋转立方织构或高斯织构{011}<100>,且当织构类型为旋转立方织构时,织构强度存在很大差异,而当织构类型为高斯织构时,织构强度差异相对较小。 The texture of the grain oriented silicon steel hot rolled plate at different compressibility has been measured.The experimental results have shown that the texture of all samples at different thickness is {100}<011> when the compressibility is below 80%,and its intensity at different compressibility and thickness is difference.The texture of all samples at different thickness is variable when the compressibility is above 80%,it is {100}<011> or {011}<100>,and the intensity of ...
球刻痕法对高磁感取向硅钢磁性的影响
试验研究了球刻痕法对高磁感取向硅钢的铁损、矫顽力、相对磁导率、巴克豪森噪声等磁学性能的影响.研究结果表明:经过球刻痕处理后,高磁感取向硅钢的铁损明显降低,矫顽力下降,8 mm球刻痕过后铁损值与矫顽力分别下降16.2%和14.7%,且铁损和矫顽力均随刻痕间距降低而减少.刻痕后的高磁感取向硅钢磁导率在高磁感应强度下明显上升,刻痕后巴克豪森噪声值明显降低,经过对比分析确定8 mm为球刻痕的最佳刻痕间距.从磁畴观察、细化磁畴的原理等方面解释了细化磁畴对高磁感取向硅钢性能的影响原因. The effects of the ball scribing on magnetic properties of high permeability grain-oriented silicon steels,including the iron loss,coercive force,relative permeability,and Barkhausen noise were investigated. The results showed that the iron loss and coercive force of the high permeability grain-oriented silicon steels apparently decreased 16. 2% and 14. 7% respectively after 8 mm ball scribing and they both decreased with the decrease of the scribing spacing at the same magnetic flux density. At...
电脉冲对取向硅钢凝固组织的影响
对熔融态钢液进行处理,研究了电脉冲对于取向硅钢凝固组织的影响作用,利用正交试验法研究了脉冲电容、频率、处理时间和电压等脉冲参数的作用效果。结果表明:电脉冲对钢锭晶粒组织具有明显的细化作用,凝固组织的等轴晶比例大幅上升,影响等轴晶比例的最显著性因素为脉冲频率,最优正交试验参数为电容1 200μF,脉冲频率1 Hz,处理时间5 s,脉冲电压800 V。随着输入能量的增大等轴晶率先增大后减小,脉冲输入能量为某值时,等轴晶率最大,利用经典形核理论和热力学对这一现象进行了解释。 The influence of electric pulse on the solidification structure of oriented silicon steel was investigated by applying electric pulse in molten steel.The affection due to different electric pulse parameters such as electric capacity,frequency,applied time and voltage was studied by orthogonal design test.The result showed that solidification structure of oriented silicon steel could be improved by the electric pulse,and the equiaxed crystal ratio increased obviously.The most influential paramete...
50W600无取向硅钢在轧制与退火工序间的织构演变
运用电子背散射衍射(EBSD)技术,研究了50W600无取向硅钢在热轧→冷轧→退火工序间织构的演变。结果表明:由于热轧板沿板厚方向的应力场和温度场存在差异,导致热轧板不同层织构类型和强度存在差异;热轧板表层主要存在铜型、黄铜和高斯织构,1/4层织构主要为α纤维织构和较弱的高斯织构,中心层织构较单一,主要为α纤维织构;和热轧板相比,冷轧板各层织构差异较小,为典型的轧制织构(α纤维织构和γ纤维织构);退火板各层都表现为γ纤维织构增强、α纤维织构减弱,旋转立方织构基本消失。 The texture evolution of 50W600non-oriented silicon steel in hot rolling,cold rolling and annealing process was investigated by electron back-scatter diffraction(EBSD)technology.Results show that the hot rolled plate texture types and intensities along thickness direction were different because of the different stress fields and temperature fields.The major texture types in the surface of hot rolled plate were copper,brass and Gauss texture.The texture was composed ofαfibre texture and weaker Ga...