所有分类
  • 所有分类
  • 未分类

对欧盟市场汽车压缩机专用产品进行技术解析,对比分析了其电磁性能、退火和发蓝处理、物理性能、化学成分、应用特点等参数。探讨国内外电工钢产品应用方式的不同特点,并结合鞍钢自身工艺装备和炼钢、热轧、冷轧工艺参数介绍了其生产可行性。提供了冶金工艺流程下,后工序电工钢专业生产线及传统冷轧系统生产线两种生产方式,均能满足用户最终使用要求。 The technology of automotive compressor accommodation manufacture of European Economic and Monetary Union market was described.The magnetic properties,annealing bluing,physical properties,chemical composition,application parameters were analysed.The different characteristics of the application of electrical steel products,the feasibility of manufacture on the existing technology and equipment,steelmaking,hot rolled,cold rolled technical parameters were discussed.The professional product line of ... 
2013-06-28 674 5.8

研究了罩式炉常化工艺对50W350硅钢热轧板组织、夹杂物和性能的影响。研究结果显示,罩式炉常化工艺在温度一定的情况下,随着保温时间延长,硅钢晶粒逐步再结晶并长大,同时析出物也在聚集长大。通过制定合理的罩式炉常化工艺,可以实现硅钢晶粒的再结晶和长大,从而达到连续退火炉常化工艺产品技术要求。 The influence of normalization process with a bell furnace on the structure,inclusions and properties of 50W350electrical steel hot-rolled sheet was studied.The research results showed that:when the steel was normalized at a certain temperature in the bell furnace,the silicon steel grains gradually recrystallized and grew up with the extension of the annealing holding time,and at the same time,the precipitates also gathered and grew up.The recrystallization and growth of the silicon steel grains... 
2022-02-28 252 5.8

【摘要】 <正>2014年5月9日,从武钢硅钢事业部获悉,...
2014-06-28 201 5.8

涂层技术在高磁感取向硅钢生产中起着重要的作用.根据生产实践,介绍了高磁感取向硅钢生产中涂层的种类和作用、涂料的成分和对产品性能的影响、涂层工艺质量控制要点和检验方法等,并提出了通过优化涂层工艺改善高磁感取向硅钢性能和外观质量的方法. Surface coating technique plays an important role in producing high magnetic inductivity grain-oriented silicon steel.Based on production practice,this paper describes the types and function of the coating,the composition of the coating and its effect on the product performance,the quality control and inspection method for the coatings,as well as proposes ways to improve the magnetic property and surface quality of the steel by optimizing the coating process. 
2012-06-28 213 5.8

硅钢是钢铁产品中的\"工艺品\",是高附加值产品,通过对我国主要硅钢生产厂家的工艺设备,市场情况分析,简要介绍了我国硅钢生产消费现状,未来生产能力预测及硅钢未来发展趋势。 Silicon steel is the \"crafts\" of steel products,also is high value-added product.By analyzing process equipment and market condition of major silicon steel-making plant of China,it briefly introduces our current production consumption status,future production capacity prediction and future development trend of silicon steel. 
2011-03-28 227 5.8

以市场上购买的取向硅钢成品板为原料,经不同压下率冷轧至0.23~0.08 mm不等。借助X射线衍射仪(XRD)检测了冷轧后样品中的织构组分及其含量,利用电子背散射技术(EBSD)测量了试样的取向因子分布情况。观察了孪晶的形貌与晶体学特征,分析了硅钢超薄带的塑性变形行为。结果发现,在平面压缩应力下,{112}<111>滑移系的取向因子较大。随冷轧压下率的增加,Goss织构的含量逐渐减少,{212}<141>织构组分的含量先增加后减少,{111}<112>织构组分的含量逐渐增加,织构组分以{110}<001>→{212}<141>→{111}<112>顺序演变。冷轧后样品中出现了孪晶,其晶体取向为{001}<110>,冷轧过程中孪晶取向没有发生变化。 The commercial finished oriented silicon steel plate as the raw material were rolled to 0.23-0.08 mm. With the X-ray diffractometer(XRD), the texture components and their volume fractions in the cold-rolled samples were detected. And the orientation factor distribution of the cross-section of the samples was measured by the electron backscattering technique(EBSD). The morphology and crystallographic characteristics of twins were observed, and the plastic deformation behaviors of the ultra-thin o... 
2022-02-28 475 5.8

介绍在取向硅钢生产中抑制剂的作用以及多元抑制剂的机理和应用情况,分析多元抑制剂方案中各种元素对高磁感取向硅钢性能的影响,并根据生产实践提出了进一步研究的方向. The role of an inhibitor in the production of grain oriented silicon steel,and the mechanism of multiplex inhibitor in the production are described in the present article.In addition,the influence of various elements in the multiplex inhibitor on the performance of grain oriented silicon steel with high magnetic induction is elucidated.Further work needed in this research is also indicated. 
2013-01-28 201 5.8

研究了卷取工艺对一种新型含铜无取向电工钢晶粒尺寸、织构演变、铁损和磁感应强度的影响。结果表明,试样织构组分主要为{111}、{112}、{100}和高斯织构,在550℃卷取、保温2~3h,{100}织构有增强趋势,磁感应强度较高,铁损较低。 The effects of coiling process on grain size,texture,core loss and magnetic induction of a new cold rolled non-oriented electrical steel with copper were investigated.The results show that there are mainly {111},{112},{100} and {110}<001> texture.Coiling at 550℃and keeping for 2~3 hours,the {100} texture is enhanced,magnetic induction is higher and core loss is lower. 
2011-03-28 293 5.8

【作者】 谌剑; ...
2011-09-28 281 5.8

通过后天抑制剂获得法制备了取向硅钢,对渗氮前后和高温退火升温阶段析出物的析出和转化规律进行了研究。研究结果表明,渗氮前脱碳退火态基体中存在少量的粗大AlN颗粒和细小AlN颗粒,渗氮处理后新析出大量的Si3N4析出物,高温退火升温阶段Si3N4将转化为(Al,Si)N,随着温度的继续升高(Al,Si)N颗粒将发生粗化,(Al,Si)N是后天抑制剂获得法制备取向硅钢的主要抑制剂。 Grain-oriented silicon steels were produced by acquired inhibitor method.The rule of precipitate transformation was studied after nitriding treatment and high-temperature finishing annealing.The results show that a small amount of large AlN and fine AlN are found in matrix before nitriding treatment,and a large amount of Si3N4 is precipitated in matrix after nitriding treatment.During the temperature rising period of high-temperature finishing annealing,Si3N4 would transform into(Al,Si)N,and(Al,... 
2011-12-28 232 5.8

本文中简要介绍了武汉钢铁有限公司采用薄板坯连铸连轧CSP(compact strip production, CSP)工艺生产中低牌号无取向硅钢的实践情况.CSP工艺生产的硅钢具有成品磁性均匀、板形好的优势,但是在利用该技术生产中低牌号无取向硅钢时,常存在成品板表面瓦楞状缺陷严重、连铸生产效率低等问题.通过优化炼钢成分、热轧等相关工艺,可消除热轧板厚度方向中心的粗大形变组织,从源头上避免了粗大{100}<011>纤维组织的出现,消除了瓦楞状缺陷;通过提升冶炼效率和控制钢中夹杂物总量,可优化隧道炉的加热温度与在炉时间,大幅度提升了连铸生产效率,实现了中低牌号无取向硅钢的批量稳定制造,使CSP产线成为中低牌号无取向硅钢热轧板原料的主要供给生产线.如何进一步提升钢水纯洁度、提高连铸生产效率、降低生产成本,以及挖掘该产线生产薄带钢的技术优点,是未来工作的重点. This paper briefly introduces the practice of producing medium and low grade non oriented silicon steel(NGO) with CSP(compact strip production, CSP)technology in Wuhan Iron and Steel Co., Ltd.. This technology has the inherent advantages of uniform magnetic properties and good shape for silicon steel finished strip. However, in the actual production process, there are serious corrugated defects on the surface of silicon steel finished strip, and production efficiency of continuous casting is low... 
2023-01-28 255 5.8

研究了组织和析出物对高效电机用无取向硅钢退火板磁性能的影响。结果表明:随着退火温度升高,退火板平均晶粒尺寸增加,P15/50明显降低,B50略有升高。退火温度在1 000℃时,退火板的综合性能较好。析出物主要是AlN、(MnS+AlN)和(MnS+Al2O3)复合析出物,尺寸较粗大,主要集中在1.0~2.5μm,还发现少量百纳米以下的细小AlN和TiN。实验室模拟TSCR流程试制的高效电机用无取向硅钢,铁损平均值小于4.00 W/kg,磁感应强度大于1.75 T,适合作中小型高效电机铁芯材料。 Effects of microstructure and precipitation on magnetic property of non-oriented silicon steel sheets after annealing for high-efficiency motor are studied in the paper by experiments.The annealed sheet exhibits a larger average grain size,obviously decreasing iron loss and slightly raising magnetic induction with increasing temperature.The annealed sheet has better comprehensive properties at a annealing temperature of 1 000 ℃.The main precipitates are compounds of AlN、(MnS+AlN)and(MnS+Al2O3) w... 
2011-04-28 267 5.8

站点公告

网站试运行,请大家关注本站公众号,多提宝贵意见!

显示验证码
没有账号?注册  忘记密码?