研究了电工钢SXRC的显微结构和疲劳性能,并与DP钢进行了比较。结果表明,退火温度低温化能够有效的抑制电工钢的再结晶。该钢在固溶铌的作用下,能够在保证电机磁性的同时具有一定的强度。与DP钢相比,SXRC钢的抗疲劳性能更好。 The microstructures and fatigue properties of the electrical steel SXRC we re investigated, and the properties were also compared with the steel DP. The results show that the recrystallization of the electrical steel can be suppressed at lower annealing temperature. The steel presents favorable motor magnetic and also a compatible strength with the help of solid-solution Nb. Compared with the steel DP, the fatigue resistance of the steel SXRC is preferable. 
2014-09-28 201 5.8

采用扫描电镜、场发射扫描电镜、能谱仪等对50SW1300冷轧无取向硅钢中的夹杂物分不同尺寸区间进行数量统计,利用主成分回归分析法,即数据的标准化处理—主成分分析—回归分析—标准化的变量还原成原始变量—确定显著影响因素,综合分析夹杂物总量及各尺寸区间的夹杂物数量对无取向硅钢磁性能的影响。结果表明:主成分回归分析能够从夹杂物尺寸区间及数量的多个影响因素中提取主要的因素,定量研究其对磁性能的影响。分析表明,显著影响无取向硅钢铁损的夹杂物为100~500nm的AlN、AlN+MnS、MnS、Al2O3、AlN+Al2O3,而劣化磁感最明显的夹杂物尺寸区间为100~200nm。 Different size intervals of inclusions in cold rolled non-oriented silicon steel 50SW1300 were counted by scanning electron microscope(SEM),field emission scanning electron microscope(FESEM)and energy disperse spectroscopy(EDS).With principal component regression method:standardization for experimental data,principal component analysis,regression analysis,transform standardized variables into original variables,determination of significant factor,effects of the total number of inclusions and the... 
2014-10-28 231 5.8

对CSP流程生产的高磁感无取向电工钢50W1300在偏离轧制方向不同角度处的磁性能进行了测试和分析。结果表明:在偏离轧向不同角度处,磁性能差异显著,尤其在α=60°时磁感最低;偏离轧制方向不同角度处的磁性能大小取决于织构类型、强度及分布状态;增强{100}<0vw>和α、η取向的有利织构组分,降低不利的γ取向织构组分,且使有利织构组分分布越漫散,磁各向异性越小。 Magnetic properties of high magnetic induction non-oriented electrical steel 50W1300 produced by CSP processes were investigated with different direction in relation to the rolling direction.The result shows that magnetic properties are significantly different in relation to the rolling direction,in particular,the minimum magnetic induction occurs at 60° in relation to the rolling direction.Magnetic properties of different directions in relation to rolling direction depend on type and distributi... 
2011-04-28 197 5.8

采用光学显微镜、X射线衍射仪等分析了宁波钢铁有限公司生产的取向硅钢不同工序下的组织及织构演变规律。结果表明:铸坯经过热轧后,沿着厚度方向组织不均匀;一次冷轧并经脱碳退火后,组织由条状纤维状变成等轴状的初次再结晶晶粒,初次再结晶平均晶粒尺寸为18.17μm,织构主要以α织构和γ织构为主;在二次冷轧后,晶粒再次被压缩,转变为纤维状,织构主要为γ织构;经过高温退火后,发生二次再结晶,晶粒异常长大,晶粒尺寸达到厘米级,织构成分为单一且锋锐的Goss织构。 The microstructure and texture evolution of oriented silicon steel produced by Ningbo Iron and Steel Co.,Ltd.were analyzed by optical microscope and X-ray diffraction.The results showed that the microstructure of the slab was inhomogenous along the thickness direction after hot rolling.After first cold rolling and decarburizing annealing,the microstructure changed from strip fibrous to equiaxed primary recrystallized grains,and the average grain size of the primary recrystallization microstructu... 
2022-01-28 203 5.8

【摘要】 <正>3月15日,随着第5754卷HiB钢下线,武钢...
2011-02-28 170 5.8

【摘要】 <正>近日,世界上最先进的硅钢冷连轧酸轧...
2014-05-28 143 5.8

以马鞍山钢铁集团公司电工钢板形优化控制研究项目为背景,系统地研究了热轧、冷连轧和单机架轧机在电工钢生产过程中的边缘降控制问题。通过现场数据采集、工况数值模拟计算和工业化大生产试验,设计出适用、合理的电工钢板形控制的辊型优化曲线,满足了不同工序、不同机型的板形控制策略要求,解决了电工钢板形质量问题,取得了显著的经济效益。 Based on the project of electric steel strip shape optimization control,problem of edge drop control was systematically studied in production of electric steel of hot-rolling mill,cold-rolling mill and single stand mill.Roll optimization contour was designed out in point and reasonable by collection of work condition data,numerical simulation and test of industrial production.The shape control system can meet with the different working steps and difference mills,and quality problem of electric s... 
2011-02-28 184 5.8

基于简化的取向硅钢片模型,系统地对不同的交流激励下的硅钢叠片内铁损、交链磁通和空气中指定位置的法向漏磁的分布进行了\"单片级\"的测量,并建立了相应的硅钢叠片级问题的三维有限元分析模型,进行了大规模的数值计算分析。模型实验和数值分析的结果表明垂直进入硅钢片的漏磁通和损耗呈现浅透入的特点,在硅钢片内引起的涡流损耗在总铁损中占据了\"举足轻重\"的份额。用电磁场有限元分析软件MagNet瞬态场时步法计算结果与测量结果相吻合,说明本文方法研究复杂的硅钢叠片问题的有效性。 The measurement and 3D finite element analysis of the iron loss,interlinkage flux inside the laminated silicon steel sheets and the magnetic flux densities at the specified positions are carried out based on a verifying silicon steel sheet model.The modeling results show that the leakage flux vertically through the silicon steel sheets has the peculiarity of shin effect,and the eddy current loss caused by the AC leakage flux is a significant component of the total iron loss.The calculated result... 
2013-05-28 173 5.8

采用电子背散射衍射技术测定50SW1300冷轧无取向硅钢中不同尺寸范围晶粒的含量,利用主成分回归分析法,综合研究不同尺寸范围晶粒的含量对无取向硅钢磁性能的影响。结果表明:通过主成分回归分析法能够从不同尺寸范围晶粒的含量的多个影响因素中获取主要的因素,定量研究它们对无取向硅钢磁性能的影响规律。分析表明,无取向硅钢的铁损与不同尺寸范围晶粒的含量之间存在着可靠的多元线性关系,在一定范围内,较大尺寸晶粒的含量越多,其对铁损优化的作用越明显;而无取向硅钢的磁感与不同尺寸范围晶粒的含量之间并无线性关系。 Distribution of grain size in cold rolled non-oriented silicon steel 50SW1300 was measured by EBSD.The effects of the distribution of grain size on magnetic properties of the non-oriented silicon steel were comprehensively researched by means of principal component regression method.The results indicate that the main factors influencing the magnetic properties in the distribution of grain sizes,which can be used to guantitative study the magnetlic properies of the steel,are obtained by principal... 
2014-11-28 206 5.8

采用X射线衍射仪分析无取向硅钢冷轧织构和再结晶退火织构的演化,研究了热轧组织对无取向硅钢织构以及磁性能的影响。结果表明,具有均匀、粗大晶粒组织的热轧板,冷轧形成更多的剪切带,导致成品板形成高的高斯织构组分,并提高了{100}织构强度,降低了γ纤维织构,最终导致成品磁感应强度升高,铁损下降。 The texture evolution of non-oriented silicon steel during cold-rolling and recrystallization annealing was investigated by X-ray diffractometer.The effects of hot band microstructure on the texture and magnetic properties of non-oriented silicon steel were analyzed.The results show that more shear bands appear during cold rolling due to homogeneous coarse grain in hot band.So strong{110}<001> texture after recrystallization annealing forms.At the same time,the {100} texture components inc... 
2023-05-09 239 5.8

采用X-射线衍射分析技术测定了取向硅钢热轧板在不同压下率下不同厚度处的织构。结果表明,在压下率低于80%的情况下,几乎所有试样的不同厚度处的织构均为旋转立方织构类型{100}<011>,但不同压下率、不同厚度处的织构强度存在很大差异;在压下率大于80%的情况下,不同试样的不同厚度处的织构类型发生了变化,其织构类型为旋转立方织构或高斯织构{011}<100>,且当织构类型为旋转立方织构时,织构强度存在很大差异,而当织构类型为高斯织构时,织构强度差异相对较小。 The texture of the grain oriented silicon steel hot rolled plate at different compressibility has been measured.The experimental results have shown that the texture of all samples at different thickness is {100}<011> when the compressibility is below 80%,and its intensity at different compressibility and thickness is difference.The texture of all samples at different thickness is variable when the compressibility is above 80%,it is {100}<011> or {011}<100>,and the intensity of ... 
2011-04-28 194 5.8

介绍在取向硅钢生产中抑制剂的作用以及多元抑制剂的机理和应用情况,分析多元抑制剂方案中各种元素对高磁感取向硅钢性能的影响,并根据生产实践提出了进一步研究的方向. The role of an inhibitor in the production of grain oriented silicon steel,and the mechanism of multiplex inhibitor in the production are described in the present article.In addition,the influence of various elements in the multiplex inhibitor on the performance of grain oriented silicon steel with high magnetic induction is elucidated.Further work needed in this research is also indicated. 