所有分类
  • 所有分类
  • 未分类

在50Kg氧化镁坩埚真空感应炉上进行高硅电工钢的脱氧试验。结果表明,通过控制原料的成分、高真空下的碳氧反应和炉衬分解向钢液中的供氧,可使钢液的总氧含量≤15×10-6;在维持高温高真空条件下,当钢液中的反应达到一定程度后,延长精炼时间并不能降低钢液的总氧含量;完成精炼后加入硅钙合金沉淀脱氧可进一步降低钢液的总含氧量,但脱氧效果有限。 The test of high-silicon electric steel deoxidation has been carried out in 50Kg vacuum induction furnace with magnesium oxide crucible.Results show that the total oxygen could be ≤15×10-6in molten steel by controlling material components,carbon-oxygen reaction in high vacuum and oxygen contamination from crucible materials on molten steel;And when the reaction was carried through to a certain extent,total oxygen in molten steel could not be reduced by the extension of refining period in high va... 
2011-02-28 290 5.8

采用XRD、SEM和激光粒度仪等手段,观察并研究了不同特性氧化镁在硅钢表面形成硅酸镁底层形貌特点,并结合热力学和差热-失重分析了MgO-SiO2的反应机理。研究结果表明:粒度小,活性值高的特种氧化镁在高温退火过程中与基体表面氧化物生成的硅酸镁底层,界面中硅酸镁底层嵌入基体较多,表面致密,颗粒细小,有利于形成附着性能优良的硅酸镁底层。 Surface microstructure of Mg2SiO4 coatings formed on the surface of oriented silicon steel coated with different kinds of MgO was investigated by XRD and SEM.The reaction mechanism between MgO and SiO2 was analyzed by TG-DSC and thermodynamic calculation.Results revealed that when the MgO with finer microstructure size and higher activity is employed,a dense Mg2SiO4 layer with finer microstructure and good binding to the steel substrate can be obtained.The results are very helpful for the prepar... 
2011-10-28 357 5.8

介绍了攀钢冶炼电工钢过程硫含量变化以及过程回硫、增硫情况,采取针对性措施,如:提高铁水装入量、转炉采用石英砂代替复合造渣剂造渣、RH脱硫等,降低钢中硫含量。结果表明:采取相应措施后,电工钢炼成率大幅提高,成品w[S]≤0.008%的比例由改进前的62%提高到92.4%,取得了明显的冶金效果。 The resulfurization and the change of sulphur content in production of electrical steel is analyzed.The targeted measures have been taken,such as increase the loaded quantity of liquid iron,quartz sand replaces the composite slagging agent in the converter and RH desulfurization to decrease the sulphur content of the steel.The result shows,after the measures have been taken,the finished product ratio of electrical steel increase a lot.The ratio of sulfur content of finished product no more than ... 
2011-02-28 669 5.8

对RH法(真空循环脱气法)生产的冷轧硅钢的脱硫原理及影响因素进行了分析研究。研究表明:降低顶渣中FeO、MnO的含量,提高钢液温度,增加脱硫剂的加入量并延长其循环时间有利于提高脱硫效率。 The principles of desulfurization and its influence factors of cold rolling silicon steel during RH process have been studied in this paper.The result indicated that reducing contents of FeO and MnO,rising temperature of the liquid steel,increasing quantity of desulfurizer,lengthening cycle time of desulfurzer are benefit for desulfurization. 
2011-06-28 371 5.8

研究了冷轧大压下量,950℃退火时间对一种新型含铜无取向电工钢晶粒度和织构的影响。结果表明,大压下量冷轧,随压下量的增加,退火晶粒向γ线聚集,形成强{111}<112>织构。提高冷轧压下率,退火织构{111}<100>,{110}<001>强度减弱,增加退火时间,退火织构{111}<110>,{100}<001>,{110}<001>强度变弱。采用87.5%冷轧压下率和950℃退火60 s,有利织构{100},{110}占有率最大。 The effect of annealing(950 ℃) time with high cold rolling reduction on grain size and texture of a new non-oriented electrical steel containing copper was investigated.The results show that for high cold rolling reduction,most annealed grains are oriented along γ-fibre with increasing cold rolling reduction ratio and strong texture {111}<112> is formed.With increasing the cold rolling reduction ratio,the intensity of annealed texture {111}<110>,{011}<100> decreases.With increa... 
2011-01-28 551 5.8

利用光学显微镜(OM)和扫描电镜(SEM)研究了不同稀土Ce含量的50W470无取向硅钢的铸坯、热轧板和冷轧退火板的宏观和微观组织,并采用磁性能测试仪测定其磁性能。结果表明:当稀土Ce的加入量从0增加到66×10-6(质量分数)时,铸坯的柱状晶平均宽度从3.82 mm减小到3.24 mm,等轴晶率从43.1%增加到51.3%;热轧板的平均晶粒尺寸逐渐增加,从26.2μm增加到33.3μm,再结晶百分数从24%增加到37%;退火板的平均晶粒尺寸从36.2μm增加到39.3μm;磁性能测试表明,微观组织的变化有利于50W470无取向硅钢铁损降低和磁感提高。 Macro-structure and microstructure of as-cast plate, hot rolled plate and cold rolled annealed plate of 50 W470 non-oriented silicon steel with different rare earth Ce content was studied by optical microscope(OM) and scanning electron microscopy(SEM), and their magnetic properties were measured by magnetic property tester. The results show that when the addition amount of rare earth Ce increases from 0 to 66×10-6(mass fraction), the average width of columnar crystal of the as-cast pl... 
2022-03-28 269 5.8

采用铸坯低倍组织检验和化学分析的方法,研究板坯连铸机二冷区电磁搅拌器电流和频率参数对无取向电工钢XG800WR板坯中心偏析和等轴晶率的影响,结果表明:铸坯等轴晶率随着搅拌器电流强度和电流频率的增大而增加。采用二冷区电磁搅拌可减小中心易偏析元素S的偏析,试验得出:减小铸坯S偏析效果最好的电磁搅拌参数为电流380~400A,频率6Hz。 The effect of electromagnetic stirring current and frequency parameter at secondary cooling area on the central segregation and equiaxed crystal ratio of XG800WR non - oriented electrical steels slab was investigated through the methods of chemical and macrostructure analysis.The results shows that the rate of equiaxed crystal zone is going up with increasing of current intensity and current frequency.Electromagnetic stirring in the secondary cooling area can be easily reduced segregation caused... 
2011-01-28 229 5.8

采用XRD物相分析、金相组织观察及TEM精细组织分析研究了奥氏体组织结构状态对Fe-0.88C-1.35Si-1.03Cr-0.43Mn钢中温等温相变鼻温和孕育期的影响,以及不同温度奥氏体化后240℃等温20 min试样的组织结构特征。试验发现,随着奥氏体化温度的升高,中温等温开始转变的鼻温移向更低温度并且相变孕育期缩短;不同温度奥氏体化后同为240℃等温20 min处理,虽然均形成由贝氏体铁素体亚条平行排列构成的束状贝氏体组织,但贝氏体组织的精细结构状态不同,突出的差别在于对应低温奥氏体化贝氏体亚条端部边界具有凸起结构,而对应高温奥氏体化贝氏体亚条端部边界较为平齐且呈现楔形结构。不能简单地以马氏体切变机制认识试验钢中贝氏体组织的形成。 The influence of austenitization temperature on the incubation period and the bainitic phase transformation behaviour in high-carbon silicon steel has been investigated using X-ray diffraction(XRD), optical microscopy and transmission electron microscopy(TEM). The microstructure characteristics of the isothermal transformation(240 ℃, 20 min)products were also studied. It was found that the nose temperature of bainite transformation and incubation period decreased with the increasing austenitizin... 
2014-07-28 201 5.8

根据现场实际的生产控制情况,指出了热轧原料断面轮廓缺陷以一定的比列遗传给了冷轧带钢,分析了不同热轧原料断面轮廓对冷轧电工钢尺寸精度的具体影响,提出了相应的规律。并阐明了严格控制热轧原料断面轮廓形貌,对保证冷轧电工钢尺寸精度具有重大意义,对于中国现行的冷轧电工钢生产具有指导意义。 Based on the actual situation of production control,it was pointed out that the section profile defects of hot-rolled raw materials were geneticed to the cold-rolled strip.The specific impact analysis for the profile of different hot-rolled raw materials to the dimensional accuracy of cold-rolled silicon steel was analyzed.As a result, the corresponding orderliness are given;And the strict control to section profile of the hot-rolled material is of great significance to ensure the dimensional ac... 
2014-01-28 220 5.8

对欧盟市场汽车压缩机专用产品进行技术解析,对比分析了其电磁性能、退火和发蓝处理、物理性能、化学成分、应用特点等参数。探讨国内外电工钢产品应用方式的不同特点,并结合鞍钢自身工艺装备和炼钢、热轧、冷轧工艺参数介绍了其生产可行性。提供了冶金工艺流程下,后工序电工钢专业生产线及传统冷轧系统生产线两种生产方式,均能满足用户最终使用要求。 The technology of automotive compressor accommodation manufacture of European Economic and Monetary Union market was described.The magnetic properties,annealing bluing,physical properties,chemical composition,application parameters were analysed.The different characteristics of the application of electrical steel products,the feasibility of manufacture on the existing technology and equipment,steelmaking,hot rolled,cold rolled technical parameters were discussed.The professional product line of ... 
2013-06-28 670 5.8

取向硅钢热轧板中织构梯度对发展完善的二次再结晶十分关键,通过添加铜可以显著降低取向硅钢板坯加热温度,从而影响热轧板织构分布。利用X射线衍射仪,分析了实验室模拟薄板坯连铸连轧(TSCR)工艺的3种不同铜含量的取向硅钢热轧板织构。结果表明:不同铜含量热轧板表面到厚度1/4处均为弱的热轧织构,热轧板心部主要为{100}面织构;铜含量约在0.4%时,热轧板次表层的{110}<001>织构比例最高,而热轧板心部的{100}<110>织构比例最低;铜含量对热轧织构中{114}<110>和{001}<100>织构发展有显著影响。 The texture gradient in hot rolled grain oriented silicon steel strip is one of the essential factors to achieve a perfect secondary recrystallization.The addition of copper can significantly reduce the slab reheating temperature of grain oriented silicon steel,so as to impact the texture distribution in the hot rolled strip.The texture of hot rolled grain oriented silicon steel strip as-rolled by thin slab casting and rolling process(TSCR) in laboratory with three different copper contents was ... 
2011-01-28 586 5.8

试验研究了退火温度(850~950℃)和时间(5~18 min)对2.3 mm热轧硅钢板(/%:0.036C,3.15Si,0.21Mn,0.005P,0.007S,0.032A1)6道次轧制的0.35 mm冷轧板组织和织构的影响。结果表明,退火温度越高,晶粒平均尺寸越大,900℃5 min退火时平均晶粒尺寸41.39μm,试样织构主要集中在γ取向线上的{111}<112>织构组分和{111}<110>织构组分;900℃18 min退火时平均晶粒尺寸为48.08μm,试样的{111}面织构和{112}面织构密度都明显减弱,{001}面织构增强,磁性能较优。 The effect of annealing temperature(850 ~950 ℃) and holding time(5 ~ 18 min) on structure and texture of 0.35 mm sheet by 6 passes cold-rolling from 2.3 mm hot-rolled plate of silicon steel(/%:0.036 C,3.15 Si,0.21 Mn,0.005 P,0.007 S,0.032A1) has been tested and studied.Results show that the higher the annealing temperature the coarser the average grain size;As annealing at 900 ℃ for 5 min the average grain size of steel sheet is 41.39 μm,and the texture in sample is mainly concentrated in y orie... 
2014-06-28 215 5.8

站点公告