硅钢连续退火机组的节能措施
针对硅钢连续退火机组的主要能源介质消耗现状,对现有生产工艺和设备研究采取机组循环用水、增加清洗段漂洗级数等措施可节约大概27 m3/h的过滤水量,并可减少78%的弱碱处理量;将炉子烟气换热系统增加一级余热回收,每年回收的余热相当于583 t标煤消耗,可节约蒸汽5 368 t。 The present situation of energy consumption for silicon steel annealing line is analyzed in this paper.In existing process and equipment conditions,increasing the number of cleaning series will lead to a saving of about 27 m3/h of filter water and reduce 78 % of weak base processing volume.For the flue gas heat-exchange system,adding a waste heat recovery device will recover waste heat equivalent to 583 tons of standard coal per year,corresponding to a saving of steam 5 368 t per year.
CSP流程试制50W270高牌号无取向硅钢织构的演变
研究了CSP流程试制50W270高牌号无取向硅钢热轧→常化→冷轧→退火过程中织构的演变.利用电子背散射衍射技术对全流程织构进行测量和分析.发现热轧板织构在厚度方向上存在较大差异,表层主要为铜型、黄铜和高斯织构,1/4层存在微弱的高斯织构和旋转立方织构,中心层以γ纤维织构和旋转立方织构为主,还含有较弱的α纤维织构.与热轧板相比,常化板表层和1/4层织构变化不大,中心层旋转立方织构和α纤维织构增强.冷轧板各层均具有α纤维织构和γ纤维织构.与冷轧板相比,成品板各层中α纤维织构基本消失,还出现了立方织构和高斯织构. This article focuses on texture evolution in 50W270 high-brand non-oriented silicon steel produced by CSP in hot rolling,normalizing,cold rolling,and annealing processes.The texture in the whole process was measured and analyzed by electron back-scatter diffraction.It is found that the texture along the thickness direction in hot-rolled strips changes obviously;there are mainly copper,brass,and Goss textures in the surface layer;the 1/4 layer has weak Goss texture and rotating cube texture;γ-fib...
基于CSP工艺取向硅钢初次再结晶晶界特征对宏观织构的影响
利用背散射衍射技术(EBSD)和XRD,研究了两段式脱碳退火工艺对取向硅钢纵截面初次再结晶的微区取向、取向差分布、特殊晶界(CSL)及高温退火试样高斯织构。分析了初次再结晶晶界特征对取向硅钢高温退火后宏观织构的影响。结果表明:初次再结晶的纵截面基体中Σ3和Σ5晶界使得高斯晶粒有着较高的迁移率,在高温退火时借助20o~45°的大角度晶界的界面能吞并周围{111}<112>晶粒迅速长大,形成密度水平较高的高斯织构。 Micro area orientation of primary recrystallization,the misorientation distribution,special boundaries under different two-stage decarburization annealing and the Goss texture under high temperature annealing the longitudinal section of grain-oriented silicon steel were detected by electron back scattering diffraction(EBSD) and X-ray diffraction(XRD).The effect of primary recrystallization grain boundary on macrotexture after high temperature annealing was analyzed.The results show that the Σ3 a...
提高热轧硅钢凸度精度的工艺措施
以太钢热连轧厂的硅钢为研究对象,利用凸度仪测量热轧带钢出口凸度值,采用矩阵和失效模式的分析方法了解影响带钢凸度变化的主次因素。研究结果表明:通过有效控制轧制过程中的加热温度、时间及采用合理的辊型,硅钢凸度精度提高了4.34%左右。 In this paper,we take the hot-rolled silicon steelsheet of Taigang as the research symbol,exit profile was measured by convex instrument,the primary and secondary factors that affect the strip profile were measured by using matrix and failure mode analysis methed.The results indicate that convexity accuracy has significantly improved by nearly 4.34% through the effective control of the heating temperature,heating time and the use of correct roller type in the process of hot rolling.
中低牌号无取向硅钢冷轧工艺优化生产实践
无取向硅钢特别是中牌号以上的无取向硅钢,随着含硅量的提高,常温下塑性较差,冷轧过程中轧制力明显提高,如果存在原料质量问题,极易发生断带事故,影响硅钢冷轧过程的成材率和生产效率。通过优化冷轧工艺参数,可提高冷轧稳定性。生产中通过合理分配冷轧各道次压下量和轧制速度,保证了轧制过程的稳定,很大程度减少了冷轧断带事故的发生。 Non-oriented silicon steel, especially in the low and middle grade, with the increase of silicon content, plasticity is poor at room temperature, rolling force in cold rolling process significantly improved .If there is the quality defect of raw materials , easily sheet is rolling off. Affect finished product rate and production efficiency in process of cold-rolled silicon steel. Through optimization of cold rolled process parameter , improve the stability of cold-rolling process. Through reason...
硅钢高温氧化铁皮的显微结构表征
利用电子探针面分析、状态分析及电子背散射衍射相分析技术研究硅钢高温氧化铁皮的显微结构。电子探针面分析可以直观的看出元素的分布状态,初步判断氧化铁皮的结构,而状态分析可以准确表征常规氧化铁皮中铁元素的状态,对于合金元素富集区域则通过电子背散射衍射相分析技术来标定。结果表明,高温氧化铁皮的结构主要有4层,即最外层为厚度约为10μm的Fe2O3相,次外层为Fe3O4相,中间层为FeO相上分布有颗粒状的Fe3O4相,最内层为FeO相和Si元素富集的Fe2SiO4相。其中Fe2SiO4层的分布特征与加热温度密切相关:1 100℃时,Fe2SiO4相呈颗粒状,弥散分布在FeO层;1 200℃时,Fe2SiO4相呈液态,侵入基体和疏松的FeO层,且沿着FeO晶界呈网状分布。 The microstructure of high temperature oxide scale on silicon steel was characterized by electron probe microanalyzer(EPMA)mapping analysis,state analysis and electron backscatter diffraction(EBSD)phase analysis.The element distribution and the initial structure of the oxide scale could be detected by EPMA mapping analysis apparently.And the state of iron in the conventional oxide scales could be determined by state analysis.Meanwhile,the alloy-rich region could be identified by EBSD phase analy...
电工钢热压缩时动、静态再结晶组织及取向分析
采用热模拟方法及EBSD技术,研究Fe-3 wt%Si电工钢在不同温度下组织的动、静态再结晶及晶粒取向特征,特别是少量奥氏体对铁素体动、静态再结晶组织及取向的影响。结果表明,不同温度形变的组织主要分三类:形变长条铁素体、珠光体和等轴细小铁素体。长条形变铁素体内发生动态回复或连续式的动态再结晶,奥氏体周围的铁素体动态再结晶加速,部分以传统的不连续方式动态再结晶。铁素体、奥氏体都可发生静态再结晶。奥氏体的静态再结晶在1050℃以上明显,铁素体的静态再结晶随温度的升高逐渐进行,最显著的再结晶发生在1050℃。不同温度形变的样品,其形变晶粒取向主要以<111>和<100>为主,小等轴铁素体晶粒除与大形变铁素体取向相近外,出现了<110>取向及其它取向。 Static and dynamic recrystallization and grain orientations in a hot-compressed Fe-3 wt% Si electrical steels were studied at different temperatures using Gleeble simulator and EBSD technique,particularly focusing on the effect of small amount of austenite on ferritic microstructure and orientations.The results show that microstructure of the compressed steel,depending on deformation temperature,consisted of elongated and deformed ferrite,pearlite and fine equal-axed ferrite.The elongated ferrit...
火花源原子发射光谱法测定取向硅钢中碳硅锰磷硫
通过试验确定氩气分析流量为3.5L/min,静态流量为0.75L/min,冲洗时间为3s,预燃时间为12s,积分时间为5s的激发条件,采用火花源原子发射光谱法测定取向硅钢中碳、硅、锰、磷、硫。分别采用铣床铣样、砂轮磨样两种制样方式进行了精密度考察,发现制样方式对结果影响不大;讨论了取向硅钢样品中碳、硅、锰、磷、硫测定时可能存在的共存元素干扰,发现硅对锰元素的干扰不可忽略,采用干扰系数法进行了校正,据此拟合得到各元素校准曲线的相关系数均在0.999 0以上。精密度考察结果表明,碳、硅、锰、磷、硫的相对标准偏差(n=10)在0.71%~9.4%之间。对两块取向硅钢生产样品进行分析,并与钢铁研究总院进行比对分析,结果一致,且偏差均在允许范围内。 Carbon,silicon,manganese,phosphorus and sulfur in oriented silicon steel were determined by spark source atomic emission spectrometry.The selected excitation conditions were as follows:the analytical flow rate of argon was 3.5L/min,the static flow rate was 0.75L/min,the flush time was3s,the precombustion time was 12sand the integration time was 5s.Two sample preparation methods,including milling machine and grinding wheel,were investigated.The precision test results showed that,the determination...
电动汽车电机用电工钢疲劳性能测试技术研究
电动汽车电机在高速旋转时承受离心力和电磁力的作用,在进行电机转子设计时,既要考虑电磁性能,还要考虑机械性能。对电机转子受力情况进行了综述,分析了转子用电工钢疲劳性能参数的重要性,详细阐述了试样抛光、表面处理、试样的对中和安装对测试结果的影响。 The motor of electric vehicle bears big force for high speed rotors,mainly including centrifugal and electromagnetic forces.The magnetic and mechanical aspects of the electrical steel are crucial to machine design.In this paper,the forces applied on the motor were summarized and importance of fatigue properties was analyzed.The influence of specimen polish,surface treatment,alignment and installation on fatigue testing result were represented in detail.
ICP-AES法测定硅钢中铌的不确定度评定
分析了电感耦合等离子体发射光谱法(ICP-AES)测定硅钢中铌的检测过程,讨论了该检测过程中不确定度的主要来源,建立了该方法的定量的数学模型,并根据这一模型计算出了检测结果的合成标准不确定度和扩展不确定度。 The measurement of niobium content in silicon steel by inductively coupled plasma atomic emission spectrometry(ICP-AES) was analyzed,by which the main factors affecting the uncertainty of the measurement were ascertained and the calculation formula was given.Finally,according to the formula the combined uncertainty and expanded uncertainty were obtained.
高硅钢薄板退火过程中的织构演变
采用传统的轧制和退火工艺制备了0.30mm厚的6.5%(质量分数)Si高硅电工钢薄板,采用X射线衍射技术对退火过程中的再结晶织构进行了研究。冷轧高硅钢薄板700℃退火形成以{111}〈112〉为峰值的γ织构(〈111〉∥ND)和以{001}〈210〉为峰值的{001}织构;而900℃以上温度退火则形成强{001}〈210〉织构。进一步的研究表明是在晶粒长大过程中{001}〈210〉发展成为主要再结晶织构组分。 High silicon steel thin sheets with thickness of 0.3mm were successfully produced by conventional rolling and annealing methods.Recrystallization texture was investigated by means of X-ray diffraction.It is found that recrystallization texture is mainly composed of γ fiber(〈111〉∥ND)with peak at {111}〈112〉 and {001} fiber with peak at {001}〈210〉 after annealing at 700℃,while strong {001}〈210〉 component dominates recrystallization texture after annealing above 900℃.It is during grain growth that {...