钢厂
电工钢生产中硫的控制
针对攀钢高硫铁水冶炼现状,结合不同生产工艺路线,论述了攀钢近年来为实现低硫电工钢的生产,在铁水预处理、转炉冶炼、钢水精炼过程中硫控制技术的开发与应用,形成了低硫洁净钢生产工艺技术,实现了低硫电工钢的生产。低硫电工钢RH脱硫率可达到20%左右,成品[S]控制在0.006%左右。 According to the smelting situations of hot metal with high sulphur content at Panzhihua Steel,combined with different produce processes,technologies for controlling the sulfur content during hot metal pretreatment,converter smelting,and second refining are developed. Technologies in low-sulfur clean steelmaking are formed. Low-sulfur electric steel are produced. As for the desulfurization rate of lowsulfur electric steel can reach about 20%,and the content of [S] in products is controlled to ab...
凝固速率对定向凝固50W600无取向硅钢固液界面稳定性和枝晶间距的影响
采用ZMLMC超高梯度定向凝固装置,研究了5种凝固速率(10、35、80、150和450μm/s)对定向凝固50W600无取向硅钢的固液界面稳定性转变规律和一次、二次枝晶间距的影响。研究结果表明,在特定的温度梯度下,随着凝固速率的增加,定向凝固的固液界面由胞状晶转变为胞状枝晶,再转变为细小的树枝晶。随着凝固速率的增加,定向凝固组织的枝晶形貌逐渐细化,一次和二次枝晶间距逐渐减小,且与冷却速率之间都符合指数关系:λ1=151.73×(G L·R)-0.31,λ2=22.07×(G L·R)-0.44。当冷却速率达到4.275℃/s时,一次、二次枝晶间距分别为112μm、14.1μm。 Under the conditions of certain temperature gradient and different solidification rate,the directional solidification experiment of non-oriented electrical steel 50W600 was carried out.The microstructure of 50W600 steel was also analyzed in different solidification rate.The result shows that the solid/liquid interface of the steel undergoes an evolution from cellular,cellular dendrite and finally to fine dendrite morphologies.The dendrite refines gradually and the distance between dendrites decr...
高强度无取向电工钢疲劳性能及断裂机制
测试了高强无取向电工钢的S-N曲线,并借助光学显微镜、扫描电子显微镜、透射电子显微镜分析了实验钢组织,疲劳断口形貌和位错结构。结果表明:室温条件下,频率为20Hz,应力比R为0.1,循环10~7周次时,实验钢的疲劳强度为360MPa,疲劳裂纹萌生于实验钢的次表面,裂纹萌生点附近有沿晶开裂现象,疲劳裂纹扩展区域有解理台阶与疲劳条纹,瞬间断裂区是韧性断裂,有大量韧窝。实验钢在循环应力作用下基体中产生了大量位错,并有驻留滑移带终止在晶界位置。 The S-N curve of a high strength non-oriented electrical steel was tested.The microstructure and fatigue fracture morphology and dislocation were analyzed by optical microscope,scanning electron microscope,transmission electron microscope.The results showed that:at room temperature and the frequency of 20 Hz and the stress ratio Rof 0.1,the fatigue strength of the experimental steel was 360 MPa when the cycle was 10~7 cycles.The fatigue crack initiation at the surface of the steel and the interg...
钒钛对取向硅钢组织、织构和析出物的影响
通过在实验室条件下模拟薄板坯连铸连轧流程,并在以Cu2S为主抑制剂制造普通取向硅钢(CGO)的基础上,加入适量钒钛,研究了钒钛对取向硅钢组织与磁性能的影响。结果表明,适量钒钛使热轧板和脱碳退火板组织更好,尤其使脱碳退火板的晶粒更加细小和均匀;加入适量钒钛不但使热轧板表面高斯织构强度更高,更使脱碳退火板中有利于高斯织构发展的γ织构强度更高;适量钒钛能形成Cu2S+(V,Ti)N等复合析出物,起到辅助抑制剂作用,加强抑制能力。细小均匀的晶粒、强度更高的有利织构和更强的抑制能力使CGO钢磁性能更佳。 Effect of V and Ti on microstructure and magnetic properties of conventional grain-oriented silicon steel(CGO) were investigated under simulated thin slab continuous casting and rolling process in laboratory with Cu2 S as the dominant inhibitor. The results show that appropriate amount V and Ti make the microstructures of the hot rolled sheet and the decarburizing annealed sheet better,especially make the grains of the decarburizing annealed sheet more tiny and uniform. Adding appropriate V and ...
硅钢高温氧化铁皮的显微结构表征
利用电子探针面分析、状态分析及电子背散射衍射相分析技术研究硅钢高温氧化铁皮的显微结构。电子探针面分析可以直观的看出元素的分布状态,初步判断氧化铁皮的结构,而状态分析可以准确表征常规氧化铁皮中铁元素的状态,对于合金元素富集区域则通过电子背散射衍射相分析技术来标定。结果表明,高温氧化铁皮的结构主要有4层,即最外层为厚度约为10μm的Fe2O3相,次外层为Fe3O4相,中间层为FeO相上分布有颗粒状的Fe3O4相,最内层为FeO相和Si元素富集的Fe2SiO4相。其中Fe2SiO4层的分布特征与加热温度密切相关:1 100℃时,Fe2SiO4相呈颗粒状,弥散分布在FeO层;1 200℃时,Fe2SiO4相呈液态,侵入基体和疏松的FeO层,且沿着FeO晶界呈网状分布。 The microstructure of high temperature oxide scale on silicon steel was characterized by electron probe microanalyzer(EPMA)mapping analysis,state analysis and electron backscatter diffraction(EBSD)phase analysis.The element distribution and the initial structure of the oxide scale could be detected by EPMA mapping analysis apparently.And the state of iron in the conventional oxide scales could be determined by state analysis.Meanwhile,the alloy-rich region could be identified by EBSD phase analy...
火花源原子发射光谱法测定取向硅钢中碳硅锰磷硫
通过试验确定氩气分析流量为3.5L/min,静态流量为0.75L/min,冲洗时间为3s,预燃时间为12s,积分时间为5s的激发条件,采用火花源原子发射光谱法测定取向硅钢中碳、硅、锰、磷、硫。分别采用铣床铣样、砂轮磨样两种制样方式进行了精密度考察,发现制样方式对结果影响不大;讨论了取向硅钢样品中碳、硅、锰、磷、硫测定时可能存在的共存元素干扰,发现硅对锰元素的干扰不可忽略,采用干扰系数法进行了校正,据此拟合得到各元素校准曲线的相关系数均在0.999 0以上。精密度考察结果表明,碳、硅、锰、磷、硫的相对标准偏差(n=10)在0.71%~9.4%之间。对两块取向硅钢生产样品进行分析,并与钢铁研究总院进行比对分析,结果一致,且偏差均在允许范围内。 Carbon,silicon,manganese,phosphorus and sulfur in oriented silicon steel were determined by spark source atomic emission spectrometry.The selected excitation conditions were as follows:the analytical flow rate of argon was 3.5L/min,the static flow rate was 0.75L/min,the flush time was3s,the precombustion time was 12sand the integration time was 5s.Two sample preparation methods,including milling machine and grinding wheel,were investigated.The precision test results showed that,the determination...
低温高磁感取向硅钢高温退火过程织构及析出物的演变行为
对低温法生产的以AlN为主抑制剂的Hi-B取向硅钢高温退火过程进行了中断实验,借助EBSD及TEM技术对高温退火连续升温过程中织构与析出物的演变进行了研究。实验结果表明,800℃时ODF图出现高斯织构组分,但强度很弱,高斯晶粒偏离角在10°以上;950~1 000℃时高斯晶粒异常长大,偏离角3~6°;高温退火过程析出物主要有球形、规则立方形及不规则多面体形3种形貌,由于渗N的影响,Zener因子先增大再减小,并且析出物在高斯晶界前沿优先粗化。 The annealing process at high temperature of Hi-B silicon steel using low slab reheat temperature and with AlN as the inhibitor has been studied by interrupting test,and the evolution of texture and precipitates during continuous heating-up in the annealing process at high temperature was analyzed by EBSD and TEM. The results showed that Goss texture appears in ODF at 800 ℃,but the intensity of Goss texture was very weak and the deviation angle was more than10°. Goss grains grow abnormally durin...
稀土元素Ce含量对50W470无取向硅钢显微组织及性能的影响
利用光学显微镜(OM)和扫描电镜(SEM)研究了不同稀土Ce含量的50W470无取向硅钢的铸坯、热轧板和冷轧退火板的宏观和微观组织,并采用磁性能测试仪测定其磁性能。结果表明:当稀土Ce的加入量从0增加到66×10-6(质量分数)时,铸坯的柱状晶平均宽度从3.82 mm减小到3.24 mm,等轴晶率从43.1%增加到51.3%;热轧板的平均晶粒尺寸逐渐增加,从26.2μm增加到33.3μm,再结晶百分数从24%增加到37%;退火板的平均晶粒尺寸从36.2μm增加到39.3μm;磁性能测试表明,微观组织的变化有利于50W470无取向硅钢铁损降低和磁感提高。 Macro-structure and microstructure of as-cast plate, hot rolled plate and cold rolled annealed plate of 50 W470 non-oriented silicon steel with different rare earth Ce content was studied by optical microscope(OM) and scanning electron microscopy(SEM), and their magnetic properties were measured by magnetic property tester. The results show that when the addition amount of rare earth Ce increases from 0 to 66×10-6(mass fraction), the average width of columnar crystal of the as-cast pl...
无取向电工钢织构的演变及其沿带钢宽度方向上的差异
采用EBSD检测技术,分析了50W800无取向电工钢在重要生产工序间织构的演变以及织构沿带钢宽度方向上的差异性。结果表明:热轧板织构沿带钢宽度方向上的差异性主要体现在表层织构。带钢边部表层织构主要由旋转立方织构、α纤维织构以及少量的γ纤维织构组成,带钢宽度1/4处的表层织构主要存在高斯织构,带钢宽度1/2处的表层织构主要为(110)面织构以及少量的铜型织构。各处的带钢宽度1/4处和1/2处的织构类型基本一致,都以α纤维织构和旋转立方织构为主。冷轧后,各处的表层织构类型差异较小,均为γ纤维织构和α纤维织构。由板宽边部至中心处织构强度值逐渐降低。退火后,各处织构的组分基本一致,为较强的γ纤维织构和较弱的(100)面织构。各处织构强度值差异较小,变化趋势与冷轧板一致。 The texture of non-oriented electrical steel 50W800 was detected by EBSD technique.The evolution of the texture between important processes and the difference of texture along the width direction of strip were analyzed.The result shows that the difference along the width direction of strip of texture at the surface of hot rolled plate is most obvious.The texture at the surface of strip edge is primarily made of rotating cube texture,αfiber texture and weakγfiber texture.Goss texture is mainly co...
硅钢常化退火炉气-雾冷却技术及其特点分析
常化快冷是生产高牌号无取向硅钢和高磁感取向硅钢不可缺少的一个工艺环节,气-雾冷却则是实现常化快冷的关键方式之一。介绍了国内自主设计建设的常化酸洗机组气雾冷却系统的技术特性,并对其特点进行了系统分析,最后给出该系统在设计、运行参数的选择上若干注意事项,对气-雾冷却系统设计和使用具有一定的指导作用。 The normalizing rapid cooling is a indispensable process to high grade non-oriented silicon steel and high magnetic induction oriented silicon steel’ s production. The fog cooling is a key ways of coming true the normalizing rapid cooling. This paper introduces the technical features of the fog cooling system in normalizing pickling line which is the domestic independent design and construction. Meanwhile,the fog cooling system’s characteristic is analyzed systematacially. In the end,this paper ...
ZnO对硅钢绝缘涂层组织与性能的影响
通过制备磷酸二氢铝硅钢涂层,研究了氧化锌对无铬涂层耐盐雾性能、电化学性能和附着性的影响。结果表明,硅钢表面涂层含有4.0%的氧化锌时,涂层具有最高的耐腐蚀性能和电化学性能,而且其致密表面最为平整,没有裂纹出现。 The effects of ZnO on the salt spray resistance property, electrochemical performance and adhesiveness of silicon steel insulating coating were studied. The results show that the best corrosion resistance and electrochemical properties can be obtained when the coating contains 4.0% oxide zinc, and the dense surface is smooth without cracks.