钢厂
TSCR热轧工艺对3.2%Si无取向硅钢组织性能的影响
研究了薄板坯连铸连轧流程(TSCR)条件下热轧工艺对3.2%Si-0.7%Al无取向硅钢组织、织构演变及磁性能的影响规律。结果表明,提高均热温度和热轧温度有助于获得粗大的变形组织和强烈的{001}〈110〉织构,进而对后续的组织、织构演变进程及磁性能产生有利的遗传影响。与低温均热和低温热轧相比,高温均热和高温热轧得到的最终成品板的再结晶晶粒较粗大,λ纤维再结晶织构较强而γ纤维再结晶织构较弱,磁感应强度较高。 It was investigated that the effects of thin slab cast rolling(TSCR) hot rolling processes on microstructural,textural evolution and magnetic properties of 3.2%Si-0.7%Al non-oriented silicon steel.The results show that much larger hot rolling deformed microstructure and much stronger {001}〈110〉 texture could be obtained by increasing the soaking and hot rolling temperatures,which had good heritable effects on subsequent microstructural,textural evolution and magnetic properties.The final sheets ...
冷轧无取向硅钢的边缘降控制优化研究
某冷连轧机生产无取向硅钢板材时,其边缘降的长度合格率频繁超标。为满足用户的叠片厚度精度要求,这类产品必须以增大切边量的方式来保证交货质量,而这种方式又直接降低了金属收得率,提高了生产成本。基于此,以该产线现有设备特性为基础,详细分析其软、硬件功能模式,分别对辊形与反馈控制进行全面分析与优化改进。通过现场试验论证,充分明确依托辊形优化与反馈控制程序的改进能显著提高边缘降的控制水平,该技术的使用为生产现场的边缘降控制提供了合理的技术支撑。 A cold rolling mill production of non-oriented silicon steel sheet,the thickness difference of the edge( edge-drop) is usually exceed the preset standard value,In order to meet the accuracy requirements of the user flatness,these production must be trimed wider length to meet the delivery quality of the user need, which directly reduce the metal yield and increase the manufacturing cost. Therefor,the software and hardware of the production line has been analyzed, and the work roll shape and feed...
无取向电工钢退火工艺研究现状
综述了退火温度、时间对无取向电工钢磁性的影响。退火温度主要影响无取向电工钢不同织构的占有率,退火时间主要影响晶粒尺寸的大小,晶粒尺寸的变化对织构的形成也有一定的影响。磁感最高点出现在纤维组织完全消失,(111)面织构组分较弱的组织状态。铁损的降低主要依赖于磁滞损耗的降低,织构的影响不大。 The effects of annealing temperature and time on the non-oriented electrical steel magnetic properties were reviewed.Annealing temperature and time mainly affects the different textures share and the grain sizes of non-oriented electrical steel respectively.Changes of the grain sizes also have a certain effect on textures formation.The highest point of the magnetic induction value in the fibrous tissue completely disappears and{111} plane texture has a lower state of the component content.Iron l...
无取向电工钢边部减薄控制技术研究
叠片系数是冷轧无取向电工钢的重要质量指标。为了提高叠片系数,必须保证无取向电工钢板形良好以及横向厚差小。针对攀钢冷轧厂4机架HC轧机轧制无取向电工钢的边部减薄问题,以无取向电工钢横向厚差最小作为目标函数,建立了一套针对无取向电工钢边部减薄控制的辊型曲线优化数学模型,开发了无取向电工钢专用辊型曲线,使无取向电工钢横向厚差从25μm降低到10μm以下,取得了良好的控制效果。 The lamination factor is an important quality index of non-oriented silicon steel strip.Considering the lamination factor,the non-oriented silicon steel must have a good shape and a smaller transverse thickness difference.In order to solve the edge thinning of non-oriented silicon steel strip in Panzhihua Steel,a mathematic model for designing the roll shape is built.In the model,the transverse thickness difference of non-oriented silicon steel strip is taken as the objective function.Based on t...
初次再结晶退火工艺对3%Si取向硅钢组织和织构的影响
试验研究了0.3 mm取向硅钢冷轧板(/%:0.046C,3.07Si,0.09Mn,0.029P,0.004S,0.005A1)的退火温度(760~880℃7 min)和退火时间(820℃3~9 min)对该钢的晶粒尺寸,再结晶和织构的影响。结果表明,最佳初次再结晶退火工艺为820℃5 min,该钢的平均晶粒尺寸为14.20μm,完全再结晶率为92%,不利{111}<110>结构含量为3.16%,有利织构{111}<112>,{012}<001>和高斯织构含量分别0.40%,4.73%和2.46%。 The effect of annealing temperature(at 760 ~ 880 X.for 7 min) and time(at 820℃ for 3~9 min) on grain size,recrystallization rate and texture of 0.3 mm cold-rolled sheet of oriented silicon steel(/%:0.046C,3.07Si,0.09Mn,0.029P,0.004S,0.005Al) has been tested and studied.Results show that with optimum recrystallized annealing at 820℃ for 5 min,the silicon steel average grain size is 14.20 fun,the complete recrystaUization rate is 92%,the unfavourable-texture {111}< 110 > content in steel is ...
取向硅钢用特种氧化镁的应用研究
采用XRD、SEM和激光粒度仪等手段,观察并研究了不同特性氧化镁在硅钢表面形成硅酸镁底层形貌特点,并结合热力学和差热-失重分析了MgO-SiO2的反应机理。研究结果表明:粒度小,活性值高的特种氧化镁在高温退火过程中与基体表面氧化物生成的硅酸镁底层,界面中硅酸镁底层嵌入基体较多,表面致密,颗粒细小,有利于形成附着性能优良的硅酸镁底层。 Surface microstructure of Mg2SiO4 coatings formed on the surface of oriented silicon steel coated with different kinds of MgO was investigated by XRD and SEM.The reaction mechanism between MgO and SiO2 was analyzed by TG-DSC and thermodynamic calculation.Results revealed that when the MgO with finer microstructure size and higher activity is employed,a dense Mg2SiO4 layer with finer microstructure and good binding to the steel substrate can be obtained.The results are very helpful for the prepar...
无取向硅钢中的夹杂物析出在线观察
借助高温激光共聚焦显微镜,在线观察了不同Mn含量的无取向硅钢中夹杂物的尺寸、类型、数量变化。结果表明,Mn含量(质量分数)为0.77%、0.32%时,试样中的夹杂物数量分别约为1000万个/mm3、1600万个/mm3。Mn含量较高的钢种,会优先析出球形、椭球形MnS夹杂物,其析出数量较少,尺寸相对较大,可以有效抑制AlN、CuxS夹杂物析出;Mn含量较低的钢种,会在试样再加热后冷却过程中,先析出相当数量MnS夹杂物,并作为AlN夹杂物析出核心,形成MnS+AlN复合夹杂物。这种复合夹杂物数量较多,尺寸也较大。 Based on the high temperature confocal microscope, the chage of size, type, and quantity of inclusions in non-oriented silicon steels with different Mn content were observed by in-situ SEM. Results show that the inclusion quantities are 10 million per mm3 and 16 million per mm3,while the mass fractions of Mn are 0.77% and 0.32%, respectively. In the silicon steel with higher Mn content, the spherical and ellipsoidal MnS inclusion will precipitate first, which can retard the precipitation of AlN ...
高牌号无取向电工钢RH深脱硫
以CaO-CaF2复合渣系为脱硫剂,在RH精炼过程采用真空投入法进行高牌号无取向电工钢深脱硫工业试验,采用KTH模型计算分析了RH炉渣成分对硫容量CS的影响。研究结果表明,炉渣成分控制在w((CaO))/w((SiO2))为5~7,w((CaO))/w((Al2O3))为1.5~1.8,w((Al2O3))为25%~30%,w((FeO+MnO))<5%,脱硫剂加入量为6~8kg/t时,钢中硫质量分数从平均0.003 1%降低到0.001 8%,最高脱硫率达到47.1%,平均脱硫率为41.7%。 The industrial trials on deep desulphurization of high grade non-oriented electrical steel were finished through using CaO-CaF2complex based fluxes in RH process.Using the KTH model,the effect of refining slag composition on the sulfide capacities was analyzed.The results show that the chemical composition of refining slag(mass fraction,%)is w((CaO/SiO2))between 5to 7,w((CaO))/w((Al2O3))beween 1.5to 1.8,w((Al2O3)) between 25%to 30%,w((FeO+MnO))less than 5%,and the desulphurizer addition level of...
高硅钢温轧过程压下率及中间退火对组织、织构的影响
传统轧制法制备6.5wt.%高硅钢过程中温轧工艺具有显著不同于3 wt.%Si的电工钢的特点及组织织构特征,是开发新型基于织构优化的高硅钢的关键环节。采用EBSD技术对通过热轧、温轧、冷轧及退火工艺制备0.3mm厚的6.5wt.%Si电工钢板的组织和织构进行分析,重点研究温轧过程中的中间退火和大、小压下率组合以控制织构。结果表明,在热轧退火板是部分再结晶组织的情况下,一次性温轧或先小形变量、中间退火后再大形变量的工艺可得到更多的Goss晶粒;经过最终退火后Goss取向会发生偏转,形成部分黄铜取向,而{111}〈112〉取向的晶粒内形核生成近Goss取向的再结晶晶粒;大压下量轧制是最终组织中{111}取向晶粒较多的主要原因。 Warm rolling,a key process of developing new type high-Si electrical steel based on texture optimization,has significant different characteristics from 3wt% Si steel in conventional preparing process. 0. 3mm thickness 6. 5wt. % Si steel,obtained by a series of processes including hot and warm rolling,intermediate annealing and then cold rolling,was analyzed from microstructure and texture by EBSD,which are utilized mainly for investigating the intermediate annealing process and the combination o...
PDSOFT在硅钢退火炉管道设计中的应用
结合硅钢退火炉项目中应用PDSOFT软件进行三维配管设计的案例,描述PDSOFT软件的应用过程,总结其使用要点,分析其优缺点,并提出了推广三维设计软件的思路,对今后PDSOFT在相似项目中的推广应用有参考和借鉴价值。 Combining the case of using PDSOFT software to design the three-dimensional piping,the application process of the PDSOFT software is described,the using points are summarized,the advantages and disadvantages are analyzed,and the ideas of promoting the three-dimensional design software are put forward,which have a strong reference value for the promotion and application of PDSOFT in similar projects in the future.
常化退火处理对无取向硅钢组织和织构的影响
采用光学显微镜和X射线衍射仪研究了常化退火处理对无取向硅钢热轧板和成品退火板显微组织和织构的影响。结果表明:常化退火处理消除了热轧板中的变形组织,促使变形晶粒完成再结晶;常化退火处理使高斯织构和立方织构易通过再结晶在变形带内形核和长大,可显著降低成品退火板的{111}和{112}不利织构组分的占有率,提高{100}和{110}有利织构组分的占有率,从而有利于提高无取向硅钢成品板的磁性能。 The effect of normalizing annealing treatment on microstructure and texture of non-oriented silicon steel hot rolled plates and final products were investigated by means of optical microscope and X-ray diffractometer analysis.The results show that the deformed microstructure of the hot rolled plates transformed into recrystallized grain after normalizing annealing treatment.The grains of Goss texture and cubic texture crystallographic orientation were formed and grown by recrystallization in the...