钢厂
低铁损高磁通密度无取向硅钢的应用与生产技术进展
分析了高转矩和高转速条件下高效驱动马达铁芯材料对无取向硅钢磁性能要求,讨论了无取向硅钢的高磁通密度和低铁损对电机转矩和效率的影响,介绍了国内外高磁感无取向硅钢发展情况。在生产工艺上,提高钢质纯净度,弱化夹杂物和第二相粒子对畴壁移动和再结晶晶粒长大的钉扎作用,添加微量晶界和带钢表面的偏析元素促使有利织构发展等技术可提高无取向硅钢的磁通密度。 The requirements of high efficient drive motor core materials under the conditions of high torque and high speed were analyzed.The effects of high magnetic flux density of non-oriented silicon steel on the torque and efficiency of the motor were discussed.The development of non-oriented silicon steel with high magnetic was introduced.The magnetic flux density of non-oriented silicon steel sheet can be obviously improved by some production technologies,such as purification steel,weakening the pin...
氧硫交互作用对硅钢中非金属夹杂物生成的影响
结合工业化生产的无取向硅钢,探讨了氧硫交互作用对钢中夹杂物生成的影响。借助非水溶液电解+扫描电镜法,研究了不同O、S含量下钢中夹杂物的变化规律。结果表明,本实验条件下,提高O含量、降低S含量,会劣化热轧组织再结晶效果。在劣化效果上,O的作用大于S;低Si、无Al硅钢中,应尽可能降低O含量、适当提高S含量,以粗化钢中微细夹杂物,减少尺寸小于1.0μm的夹杂物的数量;O、S含量与钢中夹杂物数量不具有关联性。生产过程中,不仅要严格控制O、S含量,还要严格控制生产工艺,以免生成较多的有害夹杂物。 Based on the industrial production of non-oriented silicon steel,the effects of interaction between oxygen and sulfur on the formation of inclusions were discussed.The change of non-metallic inclusions in steel sheets was investigated by means of electrolysis with non-aqueous solution under different oxygen and sulfur content.Results show that the recrystallization microstructure of hot rolled sheets will be deteriorated with the increase of oxygen content and the decrease of sulfur content.The ...
陶瓷辊除瘤方法在瑞致电工钢的应用
针对陶瓷辊表面结瘤清除时间长、清除效果差等缺陷,研究正反转陶瓷辊除瘤法,以缩短除瘤时间,增强除瘤效果。 The general removal of ceramic roller surface tumor costs a long time and the effect is poor.This paper probed into the ceramic roller tumor removal in order to shorten time and enhance the effect of eliminating.
我国硅钢发展现状及发展趋势
硅钢是钢铁产品中的\"工艺品\",是高附加值产品,通过对我国主要硅钢生产厂家的工艺设备,市场情况分析,简要介绍了我国硅钢生产消费现状,未来生产能力预测及硅钢未来发展趋势。 Silicon steel is the \"crafts\" of steel products,also is high value-added product.By analyzing process equipment and market condition of major silicon steel-making plant of China,it briefly introduces our current production consumption status,future production capacity prediction and future development trend of silicon steel.
薄板坯连铸连轧流程试制含钒钛取向硅钢中氮化物析出相
通过热力学计算与模拟试验研究了含钒钛取向硅钢中氮化物析出相的析出规律与析出行为,并探讨了含钒钛元素的氮化物析出相作为薄板坯连铸连轧流程制备取向硅钢中辅助抑制剂的可行性.研究表明,在所冶炼的含钒钛取向硅钢的成分范围内,Ti N在钢液凝固末期便具备析出的热力学条件,而Al N与VN只可能在凝固后的α+γ或α+Fe3C两相区内析出.含钒钛取向硅钢中氮化物析出相以成分复杂的复合析出相为主,且随着钒钛加入量的增加,钢中抑制剂析出相总的分布密度由于含钒钛元素的氮化物析出相的增加而明显提高,使抑制剂抑制初次再结晶晶粒正常长大的能力得以加强,最终成品的磁感应强度值B8由1.857 T提升至1.898 T.同时,加入不高于0.007%的Ti与不高于0.005%的V不会影响中间脱碳退火工序的脱碳效果以及高温退火净化阶段硫、氮的脱除效果,其形成的含钒钛元素的纳米级氮化物析出相适合作为薄板坯连铸连轧流程制备取向硅钢的辅助抑制剂. The precipitation behavior of nitride precipitates in grain-oriented silicon steel containing vanadium and titanium elements produced by thin slab casting and rolling process was studied by thermodynamic calculation and simulation experiment. The feasibility of nitride precipitates containing V and Ti elements as auxiliary inhibitors was also investigated. It is found that Ti N is likely to precipitate at the final stage of solidification in the grain-oriented silicon steel,but VN and Al N can p...
火花源原子发射光谱法在线测定电工钢中的超低碳
采用火花源原子发射光谱分析测定电工钢中超低C,研究试样制备方法、Ar纯度和压力等条件对分析结果的影响,并对工作曲线进行了优化,实现了一次分析同时测定电工钢的多种元素,满足炉前和精炼在线分析的要求。 Ultra-low carbon in electrical steel is determined with spark-source atom emission spectrum.It is researched the influence of sample making method,purity of Ar,and pressure on analysis result.The work curve is optimized.The determination of many elements in electrical steel only in one analysis is realized.It meets demands of on-line analysis for blast furnace and refining.
硅钢脱硫影响因素分析研究
对RH法(真空循环脱气法)生产的冷轧硅钢的脱硫原理及影响因素进行了分析研究。研究表明:降低顶渣中FeO、MnO的含量,提高钢液温度,增加脱硫剂的加入量并延长其循环时间有利于提高脱硫效率。 The principles of desulfurization and its influence factors of cold rolling silicon steel during RH process have been studied in this paper.The result indicated that reducing contents of FeO and MnO,rising temperature of the liquid steel,increasing quantity of desulfurizer,lengthening cycle time of desulfurzer are benefit for desulfurization.
热轧工艺对TSCR流程生产取向硅钢组织和性能的影响
取向硅钢热轧板中组织、织构梯度对发展完善的二次再结晶十分关键,通过对2种不同热轧工艺生产取向硅钢的组织、织构进行研究,结果表明:采用后道次大压下热轧工艺时热轧板表层再结区晶粒平均尺寸增加,再结晶区厚度增加,高温退火后二次晶粒尺寸减小;采用后道次大压下热轧工艺热轧时,热轧板中平均等效应变高,热轧板厚度心部{100}〈011〉和{100}〈001〉位向取向强度降低,({111}~{113})〈110〉位向取向强度提高,高温退火后{110}〈001〉位向偏离角降低,磁性能提高。 The texture and microstructure gradient in hot rolled grain oriented silicon steel strip was one of the essential factors to achieve a perfect secondary recrystallization.The texture and microstructure of grain oriented silicon steel strip as-rolled with two different hot rolling parameters was investigated.The results show that with big reduction at the end rolling process,the intensity of {100}〈011〉 and {100}〈001〉 orientation reduces with({111}-{113})〈110〉 orientation intensity enhanced in hot...
退火温度对无取向电工钢组织和磁性能的影响
主要研究了0.7%Si无取向电工钢退火试样的组织、晶粒尺寸和织构对其磁性能的影响。结果表明,随着退火温度的升高,晶粒尺寸逐渐增大,组织的均匀性得到改善;ɑ取向线上的纤维织构多集中于{114}<110>和{223}<110>附近,再结晶结束后,织构含量变化不大。{111}<110>织构取向密度值随温度升高而下降,{112}<111>织构与{111}<110>织构变化相反。晶粒尺寸增大对磁感强度的影响较小,而对铁损的影响较大。 Influences of microstructure,grain size and texture on the magnetic properties of 0.7% Si non-oriented electrical steels annealed samples were studied.The results show that with annealing temperature increasing the average grain size is increased gradually.Uniformity of the microstructure is improved;the textures of ɑ-fiber gathered in the vicinity of the { 114} < 110 > and { 223 } < 110 > texture.After recrystallization,the volume fraction of texture changes small.{ 111} < 110 &g...