森吉米尔二十辊轧机是冷轧电工钢的主要机型,具有整体刚度大,辊径小,轧制道次压下量大,产品精度高等特点,简要介绍了近年来冷轧电工钢森吉米尔二十辊轧机领域进展,在轧机结构、厚度自动控制、板形自动控制等方面的技术及研究。 20-h Sendzmir reversible mill is the main type of cold rolled electrical steel which has the characteristic of high integral stiffness,small roller diameter,high pass reduction and high product quality.In this paper,the recent progress of frame structure,automatic gauge control,automatic flatness control of Sendzmir mill is introduced. 
2023-05-06 255 5.8

运用EBSD和光学显微镜,研究了0.25%~0.45%Cu对无取向电工钢热轧板显微组织,成品板显微组织、织构和磁性能的影响。实验结果表明:卷取过程中Cu元素在热轧板表层的偏聚作用显著阻碍了热轧板表层再结晶晶粒长大,导致热轧板表层晶粒尺寸随着Cu含量增加而逐渐较小,但热轧板中间晶粒尺寸变化不大。同时发现Cu元素能够明显改善织构类型,使有利织构组分增加,不利织构组分减少,同时减弱织构强度。从实验结果可知0.35%Cu能够显著改善电工钢的磁性能,铁损P15/50最低达到4.1 W/kg,磁感B50最高值达到1.8 T。 Effects of high content Cu on microstructure of hot rolled plates and microstructure,texture and magnetic properties of annealed finish product plates of non-oriented electrical steel were examined by means of EBSD technique and optical microscope. The results show that surface segregation of Cu significantly hindered recrystallized grain growth of surface layer in hot rolled plate during the coiling,as a result,the surface grain sizes of the hot-rohed plates decrease with the increase of Cu con... 
2013-11-28 178 5.8

阐述了国内外高磁感取向硅钢的生产研究水平与发展趋势,包括通过提高高斯晶粒取向度、细化磁畴、涂覆张力涂层、减薄钢片厚度进一步降低铁损以及低温加热技术和短流程技术新工艺。分析高磁感取向硅钢在我国大型电力变压器上的应用情况,结果表明,发展更薄规格高磁感、低铁损、低磁致伸缩取向硅钢可为大型变压器的安全性、节能性及环保性提供有效保障。 The research progress and development trend of high magnetic induction grain-oriented silicon steel at home and abroad are summarized,including the technology of improving the Goss alignment,refining domain wall,adding stress coating,decreasing thickness of sheet,and the new technique of reducing heating temperature of casting slab and shortening operational.Moreover,the application of high magnetic induction grain-oriented silicon in power transformer is presented.Developing grain-oriented sili... 
2014-11-28 215 5.8

采用硅钢自动测量装置及X射线衍射仪检测出样品在实验前后的磁性能参数和织构强度.结果表明:较低的电压、9 Hz、较长的处理时间以及退火温度为650℃有利于增高铁损降低比例;较低的电压、较高的频率以及退火温度为650℃有利于增加磁感应强度增高比例.最佳的提高磁性能的实验参数是:频率为9 Hz,电压为500 V,处理时间为6 min,退火温度为650℃.通过织构分析可以验证:取向硅钢磁感应强度的变化取决于{110}<001>晶粒取向度值,而{110}<001>取向度值可看成是一个反映总体平均偏离角大小情况的综合值. An automatic measurement system for silicon steel and an X-ray diffraction meter were used for measuring the magnetic property parameters and texture of ex-processed samples and processed samples.It is shown that under the condition of a lower voltage,9Hz,a longer processed time and an annealing temperature of 650℃,the decrease rate of iron loss can be increased;a lower voltage,a higher frequency and an annealing temperature of 650℃ are in favor of improving the increase rate of magnetic inducti... 
2011-08-28 170 5.8

【机构】 宝山钢铁股份有限公司规划与科技部; ...
2022-06-28 209 5.8

在Gleeble-3500热/力模拟试验机上对HW600钢进行高温压缩试验,研究在不同试验条件下的变形抗力。试验结果表明:变形温度对变形抗力的影响最为显著,在相同的变形速率下,随着变形温度的升高,变形抗力降低;在同一变形温度下,变形速率增大,变形抗力增加;在同一变形温度、变形速率下,随着变形程度的增加,变形抗力急剧增大,真应变达到0.1后,变形抗力增加趋势变缓。 The high-temperature compression test is done for HW600 steel with Gleeble-3500 thermal simulation testing machine to research its resistance to deformation under different test conditions.It is showed from result that deformation temperature has greatest effect on the resistance,and along with the temperature getting higher the resistance lowered under same deformation rate;the resistance increases along with deformation rate getting greater under same temperature;and under same deformation tem... 
2013-04-28 156 5.8

Fe-6.5%Si高硅钢是一种具有高磁导率、低矫顽力和低铁损等优异软磁性能的合金,但是其室温脆性和低的热加工性能严重影响了其在工业领域的应用。综述了Fe-6.5%Si高硅钢的性能,评述了合金的改性法、特殊轧制法、快速凝固法、沉积扩散法、粉末冶金法等制备工艺。 It is well known that 6.5%Si high silicon steel is one kind of soft magnetic materials with higher re-lative permeability,lower coercive force and iron loss than those of conventional industrial silicon steel.However,their room-temperature embrittleness and poor workability limit their practical applications in the industry.The pre-paration technique such as modification treatment on alloy,special rolling,rapid solidification,CVD and powder me-tallurgy is reviewed. 
2023-05-09 250 5.8

取向硅钢常化工序主要采用现场实测带钢温度的方式测定冷却速率,并通过稳定冷却水温、调整冷却水量及喷梁运行数量等方式保证合理的冷却速率,给常化工艺设计和生产带来诸多不便。通过对常化工艺水冷过程带钢的传热分析求解,在建立带钢水冷温度模型的基础上,研究了不同冷却工艺参数对带钢温度及冷却速率的影响规律以及冷却工艺的交互作用结果。结果表明:模型计算结果能够较好地反映取向硅钢在常化水冷过程中的温度及冷却速率的变化,其计算误差为0.80%~4.11%;在特定取向硅钢厚度规格和常化工艺下,随着常化冷却水量及有效冷却长度的增加,带钢水冷温度及冷却速率与呈非线性变化;常化水冷工艺主要通过调控带钢与冷却水之间热交换量和交换时间实现对带钢温度的控制,实际生产中需综合考虑机组速度、冷却水量及有效冷却长度之间的交互作用,选定喷梁投入数量和冷却水量以获得稳定的冷却速率。 The cooling rate of normalization process mainly determined by measuring the grain oriented silicon steel strip temperature on site, and ensures the cooling rate by stabilizing the cooling water temperature, adjusting the cooling water volume and the operation quantity of spray beam, which brings inconvenience to the normalization process design and production. Based on the heat transfer of strip in the water cooling section of normalization process, the water cooling temperature model for the n... 
2022-01-28 233 5.8

连续酸洗退火机组(CPAL)对于当前生产高磁感取向硅钢和高牌号无取向硅钢是必不可少的一个环节。常化炉是常化酸洗机组关键的组成部分。本文对国内自主建造的两条退火酸洗机组的工艺流程,特别是常化炉段进行了对比分析。总结出了常化炉的工艺及组成特点,对生产过程中暴露的问题进行了仔细的分析并提出了改进的意见,对于以后新建常化炉具有一定的提示作用。 The continous pickling annealing line(CPAL) is an essential step in producing high magnetic induction grain-oriented silicon steel and high grade non-oriented silicon steel.The normalizing furnace is a very important part of the CAPL.In this paper,the process flows of two CAPL with independent manufacture in our country have been compared,especially the part of normalizing furnaces.The characteristics of process and component are summarized and problems of the normalizing furnace during the prod... 
2013-03-28 169 5.8

【机构】 武钢研究院; ...
2013-06-28 143 5.8

以构建高磁感、低铁损、免轧制高硅电工钢铁芯为出发点,提出采用单辊甩带制备非晶铁硅合金薄带、微氧化法在铁硅合金粉末表面包覆高电阻率铁硅氧化物薄膜制备核壳异质结构高硅电工钢纳米粉末、放电等离子烧结快速成形制备颗粒间绝缘的高硅电工钢铁芯。研究了不同氧化包覆时间对SPS烧结试样密度、物相组成、微观结构和静磁性能的影响。研究表明,在氧化包覆5h烧结温度800℃工艺条件下,制备的6.5%Si高硅电工钢铁芯的静磁性能最佳,饱和磁化强度为128.84A.m2/kg、矫顽力为2.25kA/m、剩磁为3.47A.m2/kg。其饱和磁化强度与粉末压延法制备的高硅钢相当,但矫顽力降低了1/3。 The paper takes preparation 6.5%Si steel with high induction,low core loss and removing rolling as the starting point,amorphous Fe-Si ribbons was synthesized by melt spinning method,6.5%Si steel nanopowders with high resietivity core shell structure was prepared by the slight oxidation process and 6.5% Si steel iron core with evaluating internal was sintered by spark plasma sintering process(SPS).The essay focuses studies the effects of different oxidation cladding time on sample density,phase c... 