钢厂
退火工艺对无取向硅钢磁性能的影响
分析总结退火工艺各参数对冷轧无取向硅钢磁性能的影响,结合设计和生产实践经验介绍退火工艺中各参数的实际生产取值,并针对现生产工艺过程中出现的典型问题提出解决办法。 It is analyzed and summarized the great influences on magnetism of cold rolled non-oriented silicon steel affected by various annealing process data in this article.The relevant settled ways is raised.According to the actual value presetting ways for various annealing process data based on design and production,as well as typical problems occurred during production.
晶界位向对硅钢立方/旋转立方取向双晶轧制取向变化的影响
晶界和{100}柱状晶在硅钢生产过程中对织构的遗传和演变有关键作用,因此本文利用晶体塑性有限元方法进行立方和旋转立方取向双晶在晶界不同位向时晶体取向演变的全场模拟。模拟显示,三种晶界位向下,晶界都具有诱发晶内产生S形状形变不均匀和缓解局部形变不均匀区取向转动的特点,立方和旋转立方取向双晶在带有剪切作用的轧制条件下都显示明显的取向稳定性。GB⊥RD(表示晶界垂直于轧向)晶界位向时,旋转立方取向晶粒优先在晶界中心位置发生取向转动,而立方取向则优先在远离晶界的端部发生取向转动。GB⊥TD(表示晶界垂直于横向)的晶界位向下,其晶界阻碍作用最小,双晶内产生的取向漫散度大,织构强度较低;除绕TD转动外,也具有复杂的绕RD、ND的取向转动。GB⊥ND(表示晶界垂直于法向)的晶界位向下,取向转动与GB⊥RD时相近,但有少量取向绕ND转动。 Grain boundaries and initial{100}columnar grains play a key role in the inheritance and evolution of texture in the production of electrical steels.In this paper,the crystal plasticity finite element method was used to simulate the grain orientation evolution of cube and rotated-cube oriented bicrystals when grain boundary was set to different orientations.It was shown that the grain boundary in three grain boundary orientations demonstrated the characteristics of inducing Sshape deformation inh...
无取向电工钢退火工艺研究现状
综述了退火温度、时间对无取向电工钢磁性的影响。退火温度主要影响无取向电工钢不同织构的占有率,退火时间主要影响晶粒尺寸的大小,晶粒尺寸的变化对织构的形成也有一定的影响。磁感最高点出现在纤维组织完全消失,(111)面织构组分较弱的组织状态。铁损的降低主要依赖于磁滞损耗的降低,织构的影响不大。 The effects of annealing temperature and time on the non-oriented electrical steel magnetic properties were reviewed.Annealing temperature and time mainly affects the different textures share and the grain sizes of non-oriented electrical steel respectively.Changes of the grain sizes also have a certain effect on textures formation.The highest point of the magnetic induction value in the fibrous tissue completely disappears and{111} plane texture has a lower state of the component content.Iron l...
低铁损高磁通密度无取向硅钢的应用与生产技术进展
分析了高转矩和高转速条件下高效驱动马达铁芯材料对无取向硅钢磁性能要求,讨论了无取向硅钢的高磁通密度和低铁损对电机转矩和效率的影响,介绍了国内外高磁感无取向硅钢发展情况。在生产工艺上,提高钢质纯净度,弱化夹杂物和第二相粒子对畴壁移动和再结晶晶粒长大的钉扎作用,添加微量晶界和带钢表面的偏析元素促使有利织构发展等技术可提高无取向硅钢的磁通密度。 The requirements of high efficient drive motor core materials under the conditions of high torque and high speed were analyzed.The effects of high magnetic flux density of non-oriented silicon steel on the torque and efficiency of the motor were discussed.The development of non-oriented silicon steel with high magnetic was introduced.The magnetic flux density of non-oriented silicon steel sheet can be obviously improved by some production technologies,such as purification steel,weakening the pin...
Cr对含Nb高强无取向硅钢组织、织构及性能的影响
高强无取向硅钢主要应用于高速电机,要求其具备高强度和优异磁性能,但目前无取向硅钢的磁性能和强度难以兼顾。因此,设计并制备了添加微量Cr的含Nb高强无取向硅钢,通过光学显微镜、EBSD、万能拉伸试验机、四探针测试仪和磁性能测量仪等研究了Cr对含Nb高强无取向硅钢微观组织、织构、力学性能及磁性能的影响。结果表明,添加质量分数为0.5%的Cr抑制了热轧组织的回复,使常化和退火组织再结晶减弱,常化和退火后有利织构面积分数增加,不利织构面积分数减小。添加质量分数为0.5%的Cr使含Nb无取向硅钢的屈服强度显著增大,磁感略升高,但对铁损几乎没有影响。Cr对屈服强度的影响一方面是由于Cr的固溶强化作用,另一方面Cr促进了Nb的析出而使Nb的析出强化效果增强;而Cr提高含Nb高强无取向硅钢的磁感主要是由于促进有利织构形成的同时抑制了不利织构的形成,使得织构因子增大;添加Cr使无取向硅钢的电阻率增加从而使铁损降低,同时Cr促进了Nb的析出,而这种富Nb析出相不仅抑制晶粒长大且会阻碍磁畴移动而使铁损增高,在两方面因素的综合作用下,添加质量分数为0.5%的Cr对含Nb高强无取向硅钢的铁损几乎没有影响。因此,... High strength non-oriented silicon steel is mainly used in high-speed motors, which requires good mechanical and magnetic properties. However, it is difficult for non-oriented silicon steel to obtain high strength and good magnetic properties at the same time. In this paper, the Cr-microalloyed Nb-containing high strength non-oriented silicon steel was designed and prepared. The effect of Cr on the microstructure, texture, mechanical properties and magnetic properties of Nb-containing high stren...
高牌号无取向电工钢技术发展及应用
对高牌号无取向电工钢国内生产情况、工艺技术、产品性能及应用领域等进行了阐述,并探讨了高牌号无取向电工钢产品的发展趋势。 This paper introduces basic facts on the production status,process technology and products’ properties and their applications of non-oriented electrical steel with high grade at home,and then discusses the development trend on technology for producing the non-oriented electrical steel with high grade.
硅钢级氧化镁颗粒度检测工艺的研究
通过对激光粒度分析仪测量硅钢级氧化镁(MgO)的分析条件进行优化,如分散介质、分散方式、样品预处理、仪器暗淡度等,探讨了硅钢级MgO粒度范围测量重现性较好的试验方法,满足硅钢生产过程控制对MgO粒度的要求。 The analysis condition of the laser particle size analyzer on grain oriented silicon-steel grade magnesium oxide is optimized,including the dispersion medium,dispersion methods,sample preparation,and instrument obscuration,etc.Therefore,particle size measurement with good reproducibility for silicon-steel magnesium oxide is discussed,which may meet the requirement of MgO particle size for silicon-steel process control.
CN202111662527.7一种低温高磁感取向硅钢的热轧方法
一种低温高磁感取向硅钢的热轧方法:经转炉冶炼并浇注成坯;对铸坯加热后进行粗轧:首先确定粗轧减宽量;根据所确定的粗轧减宽量进行粗轧;进行精轧;常规进行下工序。本发明采用低温板坯加热技术,降低了板坯烧损和修炉负担,且边裂发生率比现有技术的不低于18%的基础上能降低5%以上,由此节约资源及降低能耗。
CN202123179290.5一种新型冷轧硅钢片的剪切装置
本实用新型公开了一种新型冷轧硅钢片的剪切装置,包括支架,为装置主要的支撑安装结构,所述支架的顶表面设置有剪切机,所述支架的中端设置有轨道架,所述支架底表面设置有导轨;第一底座,位于所述导轨外表面,所述第一底座对立面设置有第二底座,所述第一底座与所述第二底座内部连接有双向螺杆;夹持板,位于所述第一底座顶部,所述夹持板内部分别设置有丝杆与滑杆。该新型冷轧硅钢片的剪切装置,通过调整硅钢片在硅钢片纵剪线上的夹持方式,可以实现硅钢片剪切时两边不留余边的剪切制作过程,剪切完成后的硅钢片经过横剪及叠装后,在试验中检测不会增加空载损耗,不会造成多余的浪费,也不需要调整后期工序的加工工艺。
CN202123152209.4一种硅钢卷切边防护装置
本实用新型公开了一种硅钢卷切边防护装置,包括从左到右依次设置的开卷机、分切机、张力调节机以及收卷机,所述张力调节机前后两侧均设置有通过电机驱动用于收拢切边废料的收料装置。本实用新型,通过两组滚轮的夹持能够对废料进行导向,使得废料准确的经过检测组件之间,通过上下触头相对设置,将切边废料夹在中间,当出现断料后,中间没有支撑,下触头通过第一弹簧带动与上触头接触,形成闭合电路,通过报警组件进行报警,断料时,报警组件工作的同时,收料装置上的电机断电,且第一电磁铁和第二电磁铁通电产生磁性,相互吸附,将上夹板向下带动,上下夹板通过两组防滑垫将料头夹住,避免被甩出,大大增加安全系数。
CN202122912214.4一种硅钢片绝缘测试装置
本实用新型公开了一种硅钢片绝缘测试装置,包括检测箱体、固定调节装置、探测装置和绝缘探测仪,所述固定调节装置、探测装置和绝缘探测仪设于检测箱体内,固定调节装置包括底座、支撑杆、放置板、夹板和夹持螺杆,所述支撑杆设于底座上,支撑杆上设有旋转腔,旋转腔内设有旋转电机,放置板旋转设于旋转腔上,旋转电机输出端设于放置板上,所述夹板滑动设于放置板两侧,夹持螺杆旋转设于放置板上;本实用新型属于绝缘测试领域,具体是一种通过固定调节装置可将硅钢片夹持固定,便于不同位置的调节,通过探测装置进行探测,并通过绝缘探测仪的检测于控制计算机将数据呈现和计算,减少手动操作,提高安全性的硅钢片绝缘测试装置。