钢厂
卷取工艺对新型冷轧无取向电工钢组织性能的影响
研究了卷取工艺对一种新型含铜无取向电工钢晶粒尺寸、织构演变、铁损和磁感应强度的影响。结果表明,试样织构组分主要为{111}、{112}、{100}和高斯织构,在550℃卷取、保温2~3h,{100}织构有增强趋势,磁感应强度较高,铁损较低。 The effects of coiling process on grain size,texture,core loss and magnetic induction of a new cold rolled non-oriented electrical steel with copper were investigated.The results show that there are mainly {111},{112},{100} and {110}<001> texture.Coiling at 550℃and keeping for 2~3 hours,the {100} texture is enhanced,magnetic induction is higher and core loss is lower.
Al含量对2.2%Si无取向硅钢组织、织构和磁性能的影响
通过实验室25 kg真空感应炉冶炼和锻轧研究了0.26%~0.95%Al含量对0.5 mm 2.2%Si无取向硅钢冷轧板组织、织构和磁性能的影响。试验结果表明,0.26%~0.81%Al含量时,随钢中Al含量的增加,成品退火钢板的晶粒尺寸增加同时铁损减少;当Al含量大于0.81%时,随Al含量增加,钢板的晶粒尺寸减小,同时铁损增加。Al含量对硅钢板磁感的影响没有明显的规律。2.2%Si无取向硅钢的合适Al含量为0.48%~0.81%。 The effect of 0.26%~0.95%Al content on structure,texture and magnetic performance of 0.5 mm cold rolled sheet of 2.2%Si non-oriented silicon steel has been studied by a 25 kg vacuum induction furnace smelting,and forging -rolling in laboratory.Results show that as 0.26%~0.81%Al,with increasing Al content in steel the grain size of annealed finished sheet increases while iron loss of sheet decreases,and as Al content in steel is more than 0.81%,the grain size of sheet decreases while iron loss in...
CGO硅钢各阶段织构遗传继承性的EBSD分析
利用EBSD技术对CGO硅钢热轧、中间退火、脱碳退火及二次再结晶退火组织及织构进行分析,研究了CGO硅钢各阶段加工制备过程中高斯{110}<001>晶粒的形状、尺寸及分布特点,分析了高斯取向晶粒在各工序过程中的遗传继承性特点。结果表明,CGO硅钢热轧板的次表层存在Goss取向晶粒,历经一次冷轧及中间退火后Goss取向晶粒基本消失,一次再结晶之后Goss织构仍不是主要织构,主要织构为{111}<110>和{111}<112>,说明Goss取向晶粒在二次再结晶退火前数量及尺寸上并不占优势,二次再结晶过程中Goss取向晶粒异常长大形成锋锐Goss织构。{111}<110>和{111}<112>织构组分的强度在一次冷轧中不断增加,{111}<112>织构组分的强度在二次冷轧后达到最大而{111}<110>织构组分是在初次再结晶后变强。 Grain shape,size and distribution of { 110} < 001 > Goss grains in CGO steel and the hereditary characteristics of Goss orientated grains during each processing period were investigated,based on the analysis of the microstructure and texture of the CGO silicon steel during hot rolling,intermediate annealing,decarburizing annealing and secondary recrystallization annealing by means of EBSD. The results show that Goss orientated grains exist in the subsurface of the hot rolled plate,and Goss...
硅钢连退机组辐射管加热段数值模拟
文章以国内某公司硅钢厂连续退火机组1号辐射管加热段为研究对象,分析炉内传热机理,建立并开发了辐射管加热段的传热模型。采用生产实际数据对模型进行了验证,以总燃料消耗量最小为目标,得出该炉段长度方向上燃料的最佳分配机制。所得结论为该公司连续退火机组节能控制提供理论依据。 Taking the radiant tube heating section of No.1 continuous annealing unit in a silicon steel plant of a domestic company as the research object, the heat transfer mechanism in the furnace is analyzed, and the heat transfer model of the radiant tube heating section is established and developed. The model is verified by the actual production data. Aiming at the minimum total fuel consumption, the optimal fuel distribution mechanism in the length direction of the furnace section is obtained. The co...
ICP-AES法测定硅钢中铌的不确定度评定
分析了电感耦合等离子体发射光谱法(ICP-AES)测定硅钢中铌的检测过程,讨论了该检测过程中不确定度的主要来源,建立了该方法的定量的数学模型,并根据这一模型计算出了检测结果的合成标准不确定度和扩展不确定度。 The measurement of niobium content in silicon steel by inductively coupled plasma atomic emission spectrometry(ICP-AES) was analyzed,by which the main factors affecting the uncertainty of the measurement were ascertained and the calculation formula was given.Finally,according to the formula the combined uncertainty and expanded uncertainty were obtained.
二次冷轧法对薄带连铸无取向高硅钢组织和磁性能的影响
采用双辊薄带连铸技术试制了3.98%Si-0.71%Al无取向硅钢铸带,研究了二次冷轧法对硅钢组织和磁性能的影响。结果表明:硅钢铸带显微组织为等轴晶组织,铸带再结晶较完全,常化对铸带显微组织影响较小。二次冷轧工艺和一次冷轧工艺下,最终退火后成品显微组织为等轴晶组织,二次冷轧法最终退火后的晶粒尺寸小于一次冷轧法。二次冷轧法能够提高成品磁性能. Effect of double cold rolling on magnetic properties and microstructure of 3.98%Si-0.71%Al non-oriented silicon Steel Sheets cast by twin-roll thin strip casting process were investigated.The results show that the structure of the thin strip is equiaxed crystal,the recrystallization is complete and normalizing has lesser effect on microstructure.Using both cold rolled and double cold rolled process,the microstructure is equiaxed grain after final annealing.The average grain size of annealed shee...
Fe-6.5%Si高硅钢的性能及制备技术
Fe-6.5%Si高硅钢是一种具有高磁导率、低矫顽力和低铁损等优异软磁性能的合金,但是其室温脆性和低的热加工性能严重影响了其在工业领域的应用。综述了Fe-6.5%Si高硅钢的性能,评述了合金的改性法、特殊轧制法、快速凝固法、沉积扩散法、粉末冶金法等制备工艺。 It is well known that 6.5%Si high silicon steel is one kind of soft magnetic materials with higher re-lative permeability,lower coercive force and iron loss than those of conventional industrial silicon steel.However,their room-temperature embrittleness and poor workability limit their practical applications in the industry.The pre-paration technique such as modification treatment on alloy,special rolling,rapid solidification,CVD and powder me-tallurgy is reviewed.
高温硅钢加热炉双蓄热燃烧技术的探讨
介绍了双蓄热燃烧技术的特点和高温硅钢加热炉的特点,探讨了双蓄热燃烧技术在高温硅钢加热炉中使用的技术难点,分析了双蓄热燃烧技术在高温硅钢加热炉上使用的可能性。 Introduced characteristics of double regenerative combustion technology and high temperature silicon steel reheating furnace,discussed technical difficulties for using double regenerative combustion technology,analyzed the possibility of double regenerative combustion technology applied to high temperature silicon steel reheating furnace.
无取向硅钢钙处理前后夹杂物的行为研究
研究了无取向硅钢钙处理前后夹杂物的行为,重点考察了钙处理前后夹杂物的成分、类型、形貌和尺寸研究的变化情况,为实际生产中无取向硅钢的钙处理提供理论指导。试验发现:钙处理前夹杂物主要以Al2O3、Al2O3-MgO为主,且在夹杂物表面有AlN析出,钙处理后夹杂物以Al2O3-MgO-CaS-CaO系复合夹杂物为主,还含有少量的SiO2或AlN;钙处理前后,夹杂物形貌由多边形或不规则形逐渐向球形或近似球形转变,并且夹杂物尺寸不断增大;钙处理前后,含钙夹杂物的比例发生突变,由10%增大到74.5%,且随着钙处理时间的延长,含钙夹杂物比例下降,表明钙处理使夹杂物变性后易聚集长大并上浮去除。 Behavior of inclusions before and after calcium treatment in non-oriented silicon steel was researched by investigating changes of compositions,types,shapes and sizes of inclusions before and after calcium treatment,for the purpose of providing theoretical guidance for calcium treatment of non-oriented silicon steel in actual situation. Results indicated that Al2O3 and Al2O3-MgO were main types of inclusions before calcium treatment,sometimes AlN maybe precipitate in the outer of inclusions. Al2...
Cr对含Nb高强无取向硅钢组织、织构及性能的影响
高强无取向硅钢主要应用于高速电机,要求其具备高强度和优异磁性能,但目前无取向硅钢的磁性能和强度难以兼顾。因此,设计并制备了添加微量Cr的含Nb高强无取向硅钢,通过光学显微镜、EBSD、万能拉伸试验机、四探针测试仪和磁性能测量仪等研究了Cr对含Nb高强无取向硅钢微观组织、织构、力学性能及磁性能的影响。结果表明,添加质量分数为0.5%的Cr抑制了热轧组织的回复,使常化和退火组织再结晶减弱,常化和退火后有利织构面积分数增加,不利织构面积分数减小。添加质量分数为0.5%的Cr使含Nb无取向硅钢的屈服强度显著增大,磁感略升高,但对铁损几乎没有影响。Cr对屈服强度的影响一方面是由于Cr的固溶强化作用,另一方面Cr促进了Nb的析出而使Nb的析出强化效果增强;而Cr提高含Nb高强无取向硅钢的磁感主要是由于促进有利织构形成的同时抑制了不利织构的形成,使得织构因子增大;添加Cr使无取向硅钢的电阻率增加从而使铁损降低,同时Cr促进了Nb的析出,而这种富Nb析出相不仅抑制晶粒长大且会阻碍磁畴移动而使铁损增高,在两方面因素的综合作用下,添加质量分数为0.5%的Cr对含Nb高强无取向硅钢的铁损几乎没有影响。因此,... High strength non-oriented silicon steel is mainly used in high-speed motors, which requires good mechanical and magnetic properties. However, it is difficult for non-oriented silicon steel to obtain high strength and good magnetic properties at the same time. In this paper, the Cr-microalloyed Nb-containing high strength non-oriented silicon steel was designed and prepared. The effect of Cr on the microstructure, texture, mechanical properties and magnetic properties of Nb-containing high stren...