稀土元素在许多钢中发挥着独特而且不可替代的重要作用。半个世纪以来,它的作用已经在各种低合金和特殊合金钢中的研究及应用中得到充分的证明;然而,作为具有稀土资源优势的中国,在属于重要功能材料的无取向电工钢中稀土的应用却落后于国外,本文就中国稀土在无取向电工钢中的应用研究作简要的评述,希望能够进一步推进此领域的研究,并且促进中国稀土在无取向电工钢中应用技术的发展,缩短与国外差距,并提出了在此应用领域今后需深入开展的研究方向。 Rare earth elements play a unique and irreplaceable role in a lot of steels,it has given the full proof by the practice of various low alloy steels and special alloy steels since half century.However,as our country has the advantage of rare earth resources,RE application technology in non-oriented electrical steels has lagged behind abroad.The application researches of rare earth in non-oriented electrical steel in our country are briefly reviewed in this paper,which hope to promote the research... 
2014-05-28 123 5.8

研究了硅钢铸坯再加热过程中夹杂物的析出行为。采用非水溶液电解提取+扫描电镜观察方法,观察了试样的显微组织,统计了夹杂物的尺寸、种类、数量、分布。结果表明,均热温度为1 523 K时,水淬试样的夹杂物尺寸绝大部分小于0.5μm,0.5~5.0μm的夹杂物数量很少,没有发现5.0μm以上的夹杂物。此外,均热时间为10、30、60、90、120、240 min时,对应试样中0.05~0.2μm的夹杂物数量分别为4.04×104、4.73×104、3.70×104、3.33×104、3.10×104、1.56×104个/mm3。绝大部分夹杂物以MnS、AlN、CuxS类为主,并以三类夹杂物中的两类复合或三类复合居多。三类复合夹杂物总量占每组试样夹杂物总量的90%或以上。随均热时间延长,典型的夹杂物组成会发生如下变化:MnS+AlN+CuxS MnS+AlN AlN。与此同时,MnS、AlN、CuxS三者复合比例从45.2%(均热10 min)降为9.7%(均热240 min)。 The methods of electrolysis extraction from nonaqueous solution and scanning electron microscope were adopted to study the precipitation behavior of non-metallic inclusions in Si steel slabs during reheating processes.The morphologies,chemical compositions,quantity and size distribution of non-metallic inclusions in these steel samples were analyzed.Results show that,when the soaking temperature is 1 523 K,almost all of the non-metallic inclusions are smaller than 0.5 μm,few are in the range of ... 
2013-02-28 122 5.8

【作者】 吴玉美; 陆晔; ...
2023-05-09 157 5.8

【摘要】 <正>2012年3月29日中国钢铁工业协会在上...
2012-04-28 111 5.8

为了解决在纹理背景下冷轧硅钢表面缺陷的分割问题,提出了基于局部信息结构张量和活动轮廓模型的硅钢表面缺陷分割方法。将图像的局部信息引入到结构张量中;在结构张量提取的特征空间中,以KL距离作为区域的概率密度相似性度量建立分割图像的活动轮廓模型;采用Split-Bregman数值解法对模型进行求解。运用提出的分割方法对硅钢表面的一些常见缺陷如纵向划伤、横向划伤、异物和孔洞等进行分割实验。实验结果表明,该方法可以准确地分割出硅钢表面缺陷区域,验证了该方法的有效性。 In order to address the segmentation problem for cold rolled silicon steel surface defect based on the texture background,a novel method based on structure tensor and active contour model is proposed.Image local information is introduced to the structure tensor.In the extracted feature space of structure tensor,KL distance is treated as a regional similarity measure of the probability density to establish active contour model for image segmentation.The numerical solution of Split-Bregman is used... 
2023-05-09 162 5.8

【作者】 胡志强; 张文康; ...
2011-02-28 136 5.8

含铜抑制剂作为取向硅钢的主抑制剂或辅助抑制剂不仅可以抑制初次晶粒的长大,促进二次再结晶,还可以降低铸坯的加热温度。取向硅钢中主要抑制剂为10~50 nm Cu2S,在钢的铸坯、热轧、冷轧、脱碳等工艺过程均可析出;(Cu,Mn)1.8S、Cu1.8S、ε-Cu等主要作为辅助抑制剂,尺寸一般为30~50 nm(或大于50 nm),主要在热轧阶段析出。总结了国内外有关取向硅钢中含铜抑制剂析出行为的研究进展,当前主要研究不同生产流程和工序中含铜抑制剂的析出行为和作用机理。 As main inhibitor or auxiliary inhibitor for grain-oriented silicon steel,the particles of inhibitor bearing copper not only inhibit the primary crystal growing and promote the secondary recrystallization,but also decrease the heat temperature of casting slab.The main inhibitor for grain-oriented silicon steel is 10~50 nm Cu2S,which precipitate in process and procedure including steel casting slab,hot rolling,cold rolling and decarburizing process,while the 30~50 nm or more than 50 nm... 
2013-03-28 118 5.8

借助电子背散射(EBSD)技术对AlN为主抑制剂的Hi-B取向硅钢常化工艺的中间冷却制度进行了研究。结果表明:常化后试样均发生了完全再结晶,在60℃/s冷速下组织最均匀;在合适的冷却制度下常化板表层保留了强的Goss织构,它深入到1/4厚度处,并且形成对Goss织构有利的强{554}<225>织构。 The intermediate cooling system of Hi-B oriented silicon steel with AlN main inhibitor in normalizing process was studied by means of electron back diffraction(EBSD) technique. The results show that:the specimens after normalizing are fully recrystallization, and the microstructure is most uniform under the intermediate cooling rate of 60℃/s; under suitable cooling system, normalized plate surface retains strong Goss texture, it penetrates into the 1/4 thickness of the plate and forming strong {... 
2014-11-28 115 5.8

为提高无取向硅钢导磁性能,研究了不同剪切方式对无取向硅钢剪切处磁畴结构的影响。利用纳米磁流体观测无取向硅钢剪切后边部磁畴结构。结果表明,硅钢无论在机械剪切还是线切割后的边部磁畴都会发生不同程度的改变:线切割对边部磁畴结构改变较小,边部磁畴分布均匀且连续,在距边缘0~20μm范围内出现磁畴宽度变小现象;机械剪切对磁畴的改变较为严重,剪切处磁畴零乱且不连续,在距边缘20μm处仍难以观察到完整的磁畴结构。 The effects of different shearing modes on magnetic domain structure of cold rolled non-oriented silicon steel are studied in this paper.The magnetic domain of cold rolled non-oriented silicon steel is observed by nanometer magnetic fluid pattern method.The results show that the edge magnetic domain structure will be changed by mechanical shear and wire-electrode cutting,the variation of edge magnetic domain structure wire-electrode cutting edge is very small,the magnetic domain structure is wel... 
2012-04-28 114 5.8

介绍了电工钢生产线连退机组的表面处理工艺,特别是电解清洗系统的工作机理、设备构造、生产工艺及各种影响因素。 This paper introduces the technology of surface treatment of continuous annealing unit in electrical steel production line,in particular the working mechanism,structure of equipment,production techniques and various influence factors of the electrolytic cleaning system. 
2023-05-11 1.28k 5.8

针对硅钢连续退火机组的主要能源介质消耗现状,对现有生产工艺和设备研究采取机组循环用水、增加清洗段漂洗级数等措施可节约大概27 m3/h的过滤水量,并可减少78%的弱碱处理量;将炉子烟气换热系统增加一级余热回收,每年回收的余热相当于583 t标煤消耗,可节约蒸汽5 368 t。 The present situation of energy consumption for silicon steel annealing line is analyzed in this paper.In existing process and equipment conditions,increasing the number of cleaning series will lead to a saving of about 27 m3/h of filter water and reduce 78 % of weak base processing volume.For the flue gas heat-exchange system,adding a waste heat recovery device will recover waste heat equivalent to 583 tons of standard coal per year,corresponding to a saving of steam 5 368 t per year. 