所有分类
  • 所有分类
  • 未分类

晶界和{100}柱状晶在硅钢生产过程中对织构的遗传和演变有关键作用,因此本文利用晶体塑性有限元方法进行立方和旋转立方取向双晶在晶界不同位向时晶体取向演变的全场模拟。模拟显示,三种晶界位向下,晶界都具有诱发晶内产生S形状形变不均匀和缓解局部形变不均匀区取向转动的特点,立方和旋转立方取向双晶在带有剪切作用的轧制条件下都显示明显的取向稳定性。GB⊥RD(表示晶界垂直于轧向)晶界位向时,旋转立方取向晶粒优先在晶界中心位置发生取向转动,而立方取向则优先在远离晶界的端部发生取向转动。GB⊥TD(表示晶界垂直于横向)的晶界位向下,其晶界阻碍作用最小,双晶内产生的取向漫散度大,织构强度较低;除绕TD转动外,也具有复杂的绕RD、ND的取向转动。GB⊥ND(表示晶界垂直于法向)的晶界位向下,取向转动与GB⊥RD时相近,但有少量取向绕ND转动。 Grain boundaries and initial{100}columnar grains play a key role in the inheritance and evolution of texture in the production of electrical steels.In this paper,the crystal plasticity finite element method was used to simulate the grain orientation evolution of cube and rotated-cube oriented bicrystals when grain boundary was set to different orientations.It was shown that the grain boundary in three grain boundary orientations demonstrated the characteristics of inducing Sshape deformation inh... 
2022-01-28 152 5.8

对低温加热工艺生产的普通取向(common grain-oriented,CGO)硅钢的高温退火过程进行了中断实验,材料为含3.0%Si、0.5%Cu、0.009 8%S(均为质量分数)的以Cu2S为主抑制剂的普通取向CGO钢。原始板坯厚度为230 mm,于1 200℃均热后经4道次粗轧、7道次精轧至2.3mm;热轧板采用两次冷轧法轧至0.3mm,中间完全脱碳退火,最后于1 200℃高温退火。最后样品的磁性能:铁损P17/50为1.182W/kg,磁感应强度B8为1.897T。借助配有EDAX OIM电子背散射衍射(EBSD)系统的ZEISS SUPRA 55VP扫描电子显微镜,对高温退火过程中高斯晶粒的演变进行了研究,结果表明:升温过程中晶粒尺寸增长缓慢,650℃时取向分布函数(ODF)图出现高斯织构组分,但强度很弱,高斯晶粒偏离角小于9°;950℃时高斯晶粒平均生长速度超过其他晶粒;950~1 000℃时高斯晶粒异常长大,偏离角降至约3°;在950℃之前高斯取向晶粒相比于其他晶粒没有尺寸优势。 The high-temperature annealing process of common grain-oriented(CGO)silicon steel was investigated by interrupting test.The samples were rolled from CGO silicon steel slab under low reheating temperature.The CGO silicon steel,taking Cu2S as the main inhibitor,contains3.0%Si,0.5%Cu,and 0.0098%S.The original casting slab is 230mm in thickness.After 1 200℃reheating,four-pass rough rolling and seven-pass finish rolling were conducted to make the thickness of the slab get to 2.3mm.Then the hot rolled... 
2013-11-28 149 5.8

采用双辊连铸工艺制备了硅的质量分数分别为0.5%,1.0%,3.0%,4.5%的硅钢薄带,用光学显微镜观察其组织,并研究了后处理工艺对薄带组织和性能的影响。结果表明:硅含量为0.5%和1.0%的薄带适合采用一次冷轧+850~950℃退火的后处理工艺,而硅含量在3.0%以上的薄带适合采用二次冷轧+950℃退火的后处理工艺;硅含量为3.0%和4.5%的薄带在冷轧并950℃退火后,其磁性能最佳,铁芯损耗约为4.30 W·kg-1,磁感应强度约为1.68T。 Silicon steel thin strips with silicon content of 0.5wt%,1.0wt%,3.0wt%and 4.5wt%were prepared by twin-roll continuous casting process,and the microstructure of the strips were observed by means of optical microscopy,and on the basis,the effect of post-treatment process on microstructure and properties of the strips was studied.The results show that the post-treatment process of one-time cold rolling and annealing between 850—950℃was suitable for the strips with silicon content of 0.5wt%and 1.0wt... 
2011-08-28 130 5.8

利用加热炉模拟、动态再结晶以及热模拟等试验方法以及扫描电镜、金相显微镜等分析观察手段对无取向硅钢边裂的成因进行了探讨。结果表明,长时间加热使得板坯边部晶粒异常长大,晶界氧化并脱碳,轧制过程中边部温度过低,动态再结晶过程变弱,使得板坯边部延伸性能变差,是导致硅钢边裂的主要原因。建议通过适当降低铸坯加热温度、缩短保温时间、提高终轧温度来改善硅钢边裂缺陷。 The behaviors of high temperature oxidation,dynamic recrystallization,and hot ductility,microstructure evolution were investigated on the non-oriented electrical steel sheets to discuss the formation of edge crack.The key causes of cracking was found to be the coarse as-cast microstructure,grain boundary oxidation and decarburization in reheating furnace,as well as reduced temperature at strip edge region during hot rolling process resulting in reduced hot ductility and lack of enough dynamic re... 
2013-02-28 177 5.8

采用热模拟方法及EBSD技术,研究Fe-3 wt%Si电工钢在不同温度下组织的动、静态再结晶及晶粒取向特征,特别是少量奥氏体对铁素体动、静态再结晶组织及取向的影响。结果表明,不同温度形变的组织主要分三类:形变长条铁素体、珠光体和等轴细小铁素体。长条形变铁素体内发生动态回复或连续式的动态再结晶,奥氏体周围的铁素体动态再结晶加速,部分以传统的不连续方式动态再结晶。铁素体、奥氏体都可发生静态再结晶。奥氏体的静态再结晶在1050℃以上明显,铁素体的静态再结晶随温度的升高逐渐进行,最显著的再结晶发生在1050℃。不同温度形变的样品,其形变晶粒取向主要以<111>和<100>为主,小等轴铁素体晶粒除与大形变铁素体取向相近外,出现了<110>取向及其它取向。 Static and dynamic recrystallization and grain orientations in a hot-compressed Fe-3 wt% Si electrical steels were studied at different temperatures using Gleeble simulator and EBSD technique,particularly focusing on the effect of small amount of austenite on ferritic microstructure and orientations.The results show that microstructure of the compressed steel,depending on deformation temperature,consisted of elongated and deformed ferrite,pearlite and fine equal-axed ferrite.The elongated ferrit... 
2011-01-28 191 5.8

【作者】 罗海文; 向睿; ...
2014-10-28 157 5.8

某厂对电工钢的轧制策略进行了优化,粗轧道次由“1+5”改为“1+3”。在优化后的生产过程中,每次变换钢种,烫辊材就会出现窄尺现象,而紧随其后的电工钢板则出现超宽现象。文中针对该问题,介绍了宽度设定模型和宽度自适应模型的原理,阐述了该问题出现的原因及解决方案,并通过对宽度自适应模型的应用研究及优化攻关,有效地解决了问题,大幅提升了实物质量,降低了宽度封锁率。 The rolling strategy of electrical steel was optimized in a factory,and the rough rolling pass was changed from “1+5”to“1+3”.Subsequently,the following problems were occurred in the production process:when the steel grade changed,the roasting roller steel before the electrical steel appeared the narrow width phenomenon,and then the electrical steel appeared the ultra-wide phenomenon.This paper introduced the principle of width setting model and width adaptive model,and expounded the causes and s... 
2022-02-28 151 5.8

利用OM、EBSD等手段研究了热轧板两段式正火时在700℃保温不同时间(0、10、30、60 min)对含Sb冷轧无取向电工钢磁性能的影响。结果表明,700℃保温10 min处理的样品铁损最小,磁感最高。对成品板的组织分析结果表明,试样的晶粒尺寸随700℃保温时间的延长先增大后减小,保温10 min时晶粒尺寸达到最大;分析成品试样织构发现,有利织构组分随700℃保温时间的延长先增加后减少,保温10 min时有利织构组分所占百分比最高。因此,含Sb冷轧无取向电工钢两段式正火时在700℃保温10 min时磁性能最好。 Effect of two-stage normalization on magnetic property of non-oriented electrical steel containing antimony was investigated by using optical microscope(OM) and electron back-scattered diffraction technology(EBSD).The experimental results show that the iron loss and magnetic permeability of the specimen insulated at 700 ℃ for 10 min are lowest and highest respectively.The grain size of the finish specimens increases first and then decreases with the increase of holding time.Similarly,the advanta... 
2013-11-28 160 5.8

对取向硅钢熔融态钢液进行处理,对比研究了不同脉冲参数的作用效果。结果表明,电脉冲对钢锭晶粒组织具有明显的细化作用,凝固组织等轴晶比例大幅上升。在脉冲电容、频率、处理时间和电压中,影响等轴晶比例的最显著性因素为脉冲频率;最优正交实验参数为:电容1 200μF,脉冲频率1 Hz,处理时间5 s,脉冲电压800 V;随着输入能量的增大,等轴晶率先增大后减小,脉冲输入能量为某值时,等轴晶率最大,通过经典形核理论和热力学对这一现象进行了解释。 Research on the influence of the electric pulse on the solidification structure of oriented silicon steel was preformed.Electric pulses in different parameters were applied to molten steel and results were compared.The result shows that solidification structure of oriented silicon steel can be improved by the electric pulse,and the equiaxed crystal ratio increases obviously.Among the four parameter factors of electric capacity,frequency,applied time and voltage,the most effective factor is frequ... 
2011-01-28 152 5.8

以构建高磁感、低铁损、免轧制高硅电工钢铁芯为出发点,提出采用单辊甩带制备非晶铁硅合金薄带、微氧化法在铁硅合金粉末表面包覆高电阻率铁硅氧化物薄膜制备核壳异质结构高硅电工钢纳米粉末、放电等离子烧结快速成形制备颗粒间绝缘的高硅电工钢铁芯。研究了不同氧化包覆时间对SPS烧结试样密度、物相组成、微观结构和静磁性能的影响。研究表明,在氧化包覆5h烧结温度800℃工艺条件下,制备的6.5%Si高硅电工钢铁芯的静磁性能最佳,饱和磁化强度为128.84A.m2/kg、矫顽力为2.25kA/m、剩磁为3.47A.m2/kg。其饱和磁化强度与粉末压延法制备的高硅钢相当,但矫顽力降低了1/3。 The paper takes preparation 6.5%Si steel with high induction,low core loss and removing rolling as the starting point,amorphous Fe-Si ribbons was synthesized by melt spinning method,6.5%Si steel nanopowders with high resietivity core shell structure was prepared by the slight oxidation process and 6.5% Si steel iron core with evaluating internal was sintered by spark plasma sintering process(SPS).The essay focuses studies the effects of different oxidation cladding time on sample density,phase c... 
2013-10-28 120 5.8

测试了高强无取向电工钢的S-N曲线,并借助光学显微镜、扫描电子显微镜、透射电子显微镜分析了实验钢组织,疲劳断口形貌和位错结构。结果表明:室温条件下,频率为20Hz,应力比R为0.1,循环10~7周次时,实验钢的疲劳强度为360MPa,疲劳裂纹萌生于实验钢的次表面,裂纹萌生点附近有沿晶开裂现象,疲劳裂纹扩展区域有解理台阶与疲劳条纹,瞬间断裂区是韧性断裂,有大量韧窝。实验钢在循环应力作用下基体中产生了大量位错,并有驻留滑移带终止在晶界位置。 The S-N curve of a high strength non-oriented electrical steel was tested.The microstructure and fatigue fracture morphology and dislocation were analyzed by optical microscope,scanning electron microscope,transmission electron microscope.The results showed that:at room temperature and the frequency of 20 Hz and the stress ratio Rof 0.1,the fatigue strength of the experimental steel was 360 MPa when the cycle was 10~7 cycles.The fatigue crack initiation at the surface of the steel and the interg... 
2022-01-28 149 5.8

冷轧无取向硅钢是高技术含量、高附加值产品,工艺复杂,生产周期长,过程控制难度大,被誉为钢铁产品中的\"工艺品\"。热轧生产工艺又是无取向硅钢生产的重中之重,直接决定了硅钢的铁损和电磁性等多项指标。 Cold rolled non-oriented silicon steel is high technology content、high addedvalue product. Its process is complex, Its production cycle is of Length, and Its Process control is difficult. Which is known as the iron and steel products \" Arts and crafts\". Hot rolling production process is the top priority of non-oriented silicon steel, Which Directly determines iron loss of the silicon steel and electromagnetic property, etc many index. 
2023-05-09 209 5.8

站点公告

网站试运行,请大家关注本站公众号,多提宝贵意见!

显示验证码
没有账号?注册  忘记密码?