钢厂
电解清洗装置在电工钢生产线上的应用
介绍了电工钢生产线连退机组的表面处理工艺,特别是电解清洗系统的工作机理、设备构造、生产工艺及各种影响因素。 This paper introduces the technology of surface treatment of continuous annealing unit in electrical steel production line,in particular the working mechanism,structure of equipment,production techniques and various influence factors of the electrolytic cleaning system.
资源节约型高强度电工钢SXRC的开发
日本住友金属成功地开发了一种资源节约型高强度无取向电工钢SXRC,这种电工钢是通过固溶铌适度抑制位错的合并对消而得到一种特殊的微观组织,因此兼具很高的力学性能和磁性,特别适用于HEV、EV驱动电机转子。而且,不使用昂贵的镍就可以达到期望的强度,合金成本可控,是一种优越的资源节约型产品。 Sumitomo metal industries ltd of Japan successfully developed a type of high strength non-orientation electrical steel SXRC of resources-saving.The steel has both high mechanical performance and good magnetic property thanks to the special microstructure produced by the formation of Nb solid solution serving to appropriately inhibit the combination and cancellation of dislocations.The material is,in particular,suitable for manufacturing rotors of HEV and EV driving motors.Besides,expected streng...
ICP-AES法测定硅钢中铌的不确定度评定
分析了电感耦合等离子体发射光谱法(ICP-AES)测定硅钢中铌的检测过程,讨论了该检测过程中不确定度的主要来源,建立了该方法的定量的数学模型,并根据这一模型计算出了检测结果的合成标准不确定度和扩展不确定度。 The measurement of niobium content in silicon steel by inductively coupled plasma atomic emission spectrometry(ICP-AES) was analyzed,by which the main factors affecting the uncertainty of the measurement were ascertained and the calculation formula was given.Finally,according to the formula the combined uncertainty and expanded uncertainty were obtained.
CSP流程试制50W270高牌号无取向硅钢织构的演变
研究了CSP流程试制50W270高牌号无取向硅钢热轧→常化→冷轧→退火过程中织构的演变.利用电子背散射衍射技术对全流程织构进行测量和分析.发现热轧板织构在厚度方向上存在较大差异,表层主要为铜型、黄铜和高斯织构,1/4层存在微弱的高斯织构和旋转立方织构,中心层以γ纤维织构和旋转立方织构为主,还含有较弱的α纤维织构.与热轧板相比,常化板表层和1/4层织构变化不大,中心层旋转立方织构和α纤维织构增强.冷轧板各层均具有α纤维织构和γ纤维织构.与冷轧板相比,成品板各层中α纤维织构基本消失,还出现了立方织构和高斯织构. This article focuses on texture evolution in 50W270 high-brand non-oriented silicon steel produced by CSP in hot rolling,normalizing,cold rolling,and annealing processes.The texture in the whole process was measured and analyzed by electron back-scatter diffraction.It is found that the texture along the thickness direction in hot-rolled strips changes obviously;there are mainly copper,brass,and Goss textures in the surface layer;the 1/4 layer has weak Goss texture and rotating cube texture;γ-fib...
电感耦合等离子体质谱法测定硅钢中痕量铝钼钒钛铌
研究了应用电感耦合等离子体质谱(ICP-MS)同时测定硅钢中痕量铝、钼、钒、钛、铌元素的分析方法。通过条件试验对测量参数进行了优化,确定RF功率1 400 W,泵速30rpm,采样深度140,雾化压力0.90。样品采用硝酸分解,以Be、Y混合内标校正了测量过程中高基体引起的信号漂移。根据测量时存在的质谱干扰情况,选择同位素27 Al、98 Mo、51 V、47 Ti和93 Nb作为测定同位素,同时通过调节仪器参数使得双电荷离子和氧化物离子的产率最低,以减少其带来的干扰。采用基体匹配法配制校准溶液,以标准加入法建立工作曲线,并扣除试剂空白。该方法各元素的测定下限均可达到1μg/g。用于硅钢标准样品的测定,所得结果与参考值完全吻合,各元素的RSD小于5.2%。 A method for the determination of trace aluminum,molybdenum,vanadium,titanium and niobium in silicon steel by inductively coupled plasma mass spectrometry(ICP-MS) was described.A series of single parameter condition experiment was conducted.The optimized operation parameters with RF power 1 400 W,turbo pump rate 30 rpm,sampling depth 140 and nebulizer pressure 0.90 were obtained.The samples were dissolved by HNO3,and the Be and Y mixing internal standard were used to eliminate the signal drift c...
冷轧硅钢废水处理现状、问题及对策浅析
就冷轧硅钢废水处理生产中面临的主要问题进行分析,从技术角度及运行管理角度提出工艺优化升级改进措施及应对策略;同时从后续深度处理,逐步实现零排放目标的角度进行探讨,为冷轧硅钢废水减量化、出路乃至废水零排放提供一些思路。 The main problems in the wastewater treatment process of cold-rolled silicon steel lines are analyzed and process upgrading measures and optimization strategy are put forward from both technical and management views.At the same time,downstream deep treatment to gradually achieve the target of zero discharge is discussed,to provide some ideas for reduction or even zero discharge of wastewater from cold-rolled silicon steel lines.
“双碳”大背景下的中国电工钢走势
阐述了电工钢在\"双碳\"中的作用,强调了电工钢的生产工艺技术及在减少碳排放、降低能耗中的作用,对下游能效升级带来明显的节能及降碳成果。同时,分析了2021年电工钢的生产运行情况,介绍了电工钢的未来发展,并针对如何减少碳排放以及生产更多的更低铁损、更高磁感的电工钢谈了几点启示。 The effects of electrical steels on carbon peak and carbon neutralization were expounded,especially on the achievements of obvious energy saving and carbon reduction to the downstream energy efficiency upgrading bringing from the production technology of electrical steels and their effects to reducing carbon emission and energy consumption.Meanwhile the production situation of electrical steels in 2021 was analyzed,and the future development of electrical steels was introduced,and some advices w...
硅钢连续退火生产线设备改造
针对硅钢连续生产线设备存在的故障、隐患以及精度等影响产品质量的问题进行分析及改造,实现保证生产线设备稳定运行、提高设备精度及硅钢产品质量的目的。 This paper analyzes and transforms the electrical equipment failures, risks existed in slicon continuous production line, and the effect of accuracy to product quality, in order to ensure stable operation of equipment in production line and improve the accuracy of device, quality of silicon.
高硫硅钢的硫化物析出行为及其微观组织和电磁性能变化
为了弄清楚高硫硅钢中的硫化物析出行为及其对钢的微观组织和电磁性能的影响,以便为工业化生产制定更为合理的硫含量控制标准和采取更为有效措施减轻炼钢生产的硫含量控制压力,结合0.25% Si 无取向硅钢 ,采用非水溶液电解提取 + 扫描电镜/透射电镜观察相结合的方法 ,研究了0.006 8%、0.010 2%、0.025 5% 和 0.035 3% 硫含量条件下,钢中的硫化物夹杂物组成和存在形式及其形貌、种类、尺寸、数量变化,以及相应的热轧、成品试样的微观组织和电磁性能变化。结果表明,随着钢中硫含量的增加,钢中的硫化物逐渐由 MnS→MnS+Cu2S→Cu2S转变,数量逐渐增多,尺寸向高低两个方向发展。相应地,导致热轧再结晶组织劣化和抑制了成品晶粒尺寸长大。随着钢中硫含量的增加,钢的磁感、铁损劣化程度逐渐增大。钢中的硫含量平均每增加 0.01%,涡流损耗、磁滞损耗分别劣化0.24 W/kg 和 0.41 W/kg,而磁感会劣化 0.009 T。但是 ,在硫含量为 0.010 2% 时 ,铁损可以低于 6.0W/kg,而在硫含量为 0.025 5% ... In order to find out the precipitation behavior of sulfide inclusions and the corresponding changes of microstructure and electromagnetic properties of high sulfur silicon steel sheets, so that to design more suitable sulfur concentration controlling limit for industrial manufacture and to release the steel-making difficulty effectively, Based on the change of given sulfur concentration 0.006 8%, 0.010 2%0.025 3% and 0.035 3%, the type and composition, the size and number, and the size distribut...
Fe-6.5%Si高硅钢铁芯与Epstein Square标准单片铁损检测结果对比及数据差异分析
作为一种具有优异高频铁磁性能的合金,Fe-6.5%Si(质量分数)高硅钢在高频工况条件下降损效果明显,对电气行业应用器件高频化、小型化、节能等具有十分重要的意义。通过与取向硅钢测量B-P数据对比,验证了高硅钢高频超低损特性,且轧制高硅钢与日本CVD法生产高硅钢存在基本相同的铁损值。采用国标Epstein Square法对0.30mm高硅钢薄板进行单片测试,并对由0.30mm高硅钢薄板首次装配成的电感器进行铁损测试,对比测试结果表明,元件测试与单片测试数据基本吻合,高磁感应强度条件下,元件测试结果略低于单片测试,分析原因为:线圈引起励磁压降;元件叠片间出现短路,电流增大,损耗增加;气隙板厚度过大。 As one core material with excellent high-frequency ferromagnetism,Fe-6.5%Si performs obviously reduction on core loss in high field frequency which means much to high frequency,minimization,energy conservation in electric industry.Super low loss was verified by drawing B-P curves based on detected experimental data,and which went equal to Fe-6.5%Si thin strip fabricated by CVD in Japan.Fe-6.5%Si was firstly fabricated as inductor in this research,and its core loss was determined for comparison w...