针对新日铁公开的相关专利,总结日本高强度无取向电工钢的研究进展,分析了各专利化学成分、生产工艺及产品性能的特点,指出固溶强化、细晶强化、析出强化、位错强化都有可能被用来提高无取向电工钢的强度。在高强度无取向电工钢的研发过程中,需要根据其具体用途确定目标性能,再采用合适的强化手段,从而实现力学性能、磁性能和生产性能之间的平衡。 Authors summarize the research progress of high strength non-oriented electrical steel in Japan by learning related patents brought into the public by Nippon Steel. Authors also analyze the characteristics of the chemical composition, production technology and properties of products in the patents and point out that any ones of solution strengthening method, fine-grain strengthening method, precipitation strengthening method or dislocations strengthening method may be used to improve the strengt... 
2013-11-28 173 5.8

介绍了微合金元素锡、铌、稀土对无取向硅钢性能的影响,并扼要分析了这些元素对硅钢性能的影响机理:晶界偏聚元素Sn可细化晶粒提高硅钢磁性能;微合金元素Nb细化铁素体晶粒,提高硅钢的强度、韧性和塑性及磁性能;稀土元素(RE)在硅钢中的主要作用包括净化钢液、变质夹杂物、改善铸态组织和性能及微合金化,减少晶界上出现偏析的几率。 The influence of micro-alloy elements on properties of non-oriented silicon steel and the mechanism for effect of the micro-alloy elements including Sn、Nb and RE on the properties of steel are presented and analyzed in this paper.Grain boundary segregation elements Sn in steel can grain refinement and improve the magnetic properties;Micro-alloy elements Nb can refine the ferrite grain,increase the silicon steel strength,toughness and plastic;The main role of the RE in the silicon steel including... 
2013-03-28 195 5.8

结合工业化生产的50A1300牌号无取向硅钢,分析了化学成分、RH精炼脱氧方式、板坯装炉温度以及热轧平整工艺等对磁性能的影响,探讨成品钢磁性能的改善。结果表明,采取改善后,50A1300牌号无取向硅钢的磁性能得到明显改善。2012年,该钢种平均铁损、磁感应强度分别达到5.26 W/kg、1.762 T,能够较好地满足用户市场需求及同行对标需要。 Based on the industrial manufacture of 50A1300 grade non-oriented silicon steel sheets,effects of chemical composition,deoxidization method in RH vacuum refining,charging temperature of steel slabs,hot rolling and flattening progress on magnetic properties are analyzed.The optimization methods of magnetic properties of steels are discussed. Results show that the magnetic properties are obviously improved by the adopted measures above. In 2012,the average core loss and the magnetic induction of 5... 
2014-02-28 228 5.8

为了解决目前冷轧产线硅钢现有切边技术存在的微裂纹、应力、毛刺和边浪等问题,采用光纤激光器进行了高速切割实验,对激光功率、切割速度、激光模式等影响因素进行了分析,同时对高速切割时的切割前沿形状进行了研究。结果表明,切割最高速度随着功率的增加而增加;随着离焦量的增加,切割质量下降,挂渣增多,切缝宽度增加,切割深度变浅;基模激光器能量密度更高,所以薄板切割时的切割速度高于多模激光器;切割前沿随着切割速度的增加会变得平缓,速度足够大时,切割前沿甚至接近与切割方向平行,此时切缝下部存在挂渣现象。 In order to solve the problems such as micro crack,stress,burr,edge waves and so on,existing in cold rolling production line of silicon steel side cutting,experimentsof high speed laser cutting using fiber laser were carried out.Laser power,cutting speed,laser mode and other factors were analyzed,at the same time,cutting front geometries were studied.The results show that the maximum speed increases with power.And the increases of defocus result in poor quality,wider kerf and shallowerkerf.Energ... 
2013-04-28 139 5.8

以取向电工钢成分为基础,制备了含C或Mn和S的4种实验钢。观察了接近平衡析出状态实验钢经60%冷轧后在600~1000℃范围再结晶退火过程中微观组织演变,统计分析了再结晶体积分数随退火时间的变化规律,进而计算了各实验钢静态再结晶的激活能。观察了高含C实验钢退火初期再结晶晶粒优先出现的部位。结果表明900~1000℃范围内各实验钢铁素体的化学成分相似,因而其再结晶激活能基本一致。在600~800℃范围内铁素体内会有阻碍再结晶进程的三次渗碳体析出,从而使再结晶激活能明显提高。高C含量实验钢中还会有从奥氏体转变而来的粗大珠光体或渗碳体,轧制过程中其附近形成的变形区会促进600~800℃加热时该区域附近率先发生再结晶形核、降低再结晶激活能。固溶的Mn、S元素可微弱提高再结晶激活能,但高Mn、S含量会改变粗渗碳体从奥氏体析出时的形态。 Four experimental steels based on grain oriented electrical steel containing C,or Mn and S were prepared.Microstructure evolution of the steels close to a state of equilibrium precipitation were observed during annealing processes at 600-1000 ℃after 60% cold rolling,the changes of recrystallization volume fraction were analyzed statistically as the annealing was prolonged,and the activation energy for static recrystallization of the steels were calculated.The locations,where the recrystallizatio... 
2011-12-28 204 5.8

采用EBSD检测技术,分析了50W800无取向电工钢在重要生产工序间织构的演变以及织构沿带钢宽度方向上的差异性。结果表明:热轧板织构沿带钢宽度方向上的差异性主要体现在表层织构。带钢边部表层织构主要由旋转立方织构、α纤维织构以及少量的γ纤维织构组成,带钢宽度1/4处的表层织构主要存在高斯织构,带钢宽度1/2处的表层织构主要为(110)面织构以及少量的铜型织构。各处的带钢宽度1/4处和1/2处的织构类型基本一致,都以α纤维织构和旋转立方织构为主。冷轧后,各处的表层织构类型差异较小,均为γ纤维织构和α纤维织构。由板宽边部至中心处织构强度值逐渐降低。退火后,各处织构的组分基本一致,为较强的γ纤维织构和较弱的(100)面织构。各处织构强度值差异较小,变化趋势与冷轧板一致。 The texture of non-oriented electrical steel 50W800 was detected by EBSD technique.The evolution of the texture between important processes and the difference of texture along the width direction of strip were analyzed.The result shows that the difference along the width direction of strip of texture at the surface of hot rolled plate is most obvious.The texture at the surface of strip edge is primarily made of rotating cube texture,αfiber texture and weakγfiber texture.Goss texture is mainly co... 
2014-09-28 184 5.8

通过对3%Si CGO硅钢进行恒变形速率、不同变形温度下的单道次压缩实验,结合Thermal-Calc软件,金相分析,SEM及EBSD技术,研究了取向硅钢热变形过程中组织和微观织构的变化规律。结果表明:实验钢是在双相区变形,变形后组织主要是铁素体和少量的珠光体。随变形温度的升高,晶粒由长条状变为等轴状,尺寸逐渐变大;CGO硅钢在热变形过程中立方{100}<001>取向是较为稳定存在的。随着变形温度的提高,{111}<110>等取向逐渐转向{110}<1 10>取向,且{110}<1 10>取向逐渐变得锋锐。 3% Si CGO silicon steel was studied at constant strain rate and different deformation temperatures by single-pass compression deformation experiments to reveal the evolution of microstructure and texture during thermal deformation in oriented silicon steel,and the Thermal-Calc software,metallurgical,SEM and EBSD technique was used in the experiment. The results show that experimental steel is deformed at the temperatures of two-phase zone. The microstructure of the deformed steel consists of fer... 
2014-05-28 208 5.8

变压器D21硅钢铁芯片采用冲压工艺生产。首先对其工艺进行了分析,确定了冲压方案。对产品进行了排样设计,计算了冲压力,确定了压力中心。然后,设计了单工序落料模具,完成了模具装配图。 D21 silicon steel chips for transformer are produced by stamping.First,its stamping process was analyzed and the scheme of the stamping process was determined.The product layout was designed,the punching pressure was calculated,the pressure center was determined.Then,the blanking die with single procedure was designed,the die assembly drawing was completed. 
2013-07-28 131 5.8

对熔融态钢液进行处理,研究了电脉冲对于取向硅钢凝固组织的影响作用,利用正交试验法研究了脉冲电容、频率、处理时间和电压等脉冲参数的作用效果。结果表明:电脉冲对钢锭晶粒组织具有明显的细化作用,凝固组织的等轴晶比例大幅上升,影响等轴晶比例的最显著性因素为脉冲频率,最优正交试验参数为电容1 200μF,脉冲频率1 Hz,处理时间5 s,脉冲电压800 V。随着输入能量的增大等轴晶率先增大后减小,脉冲输入能量为某值时,等轴晶率最大,利用经典形核理论和热力学对这一现象进行了解释。 The influence of electric pulse on the solidification structure of oriented silicon steel was investigated by applying electric pulse in molten steel.The affection due to different electric pulse parameters such as electric capacity,frequency,applied time and voltage was studied by orthogonal design test.The result showed that solidification structure of oriented silicon steel could be improved by the electric pulse,and the equiaxed crystal ratio increased obviously.The most influential paramete... 
2011-01-28 200 5.8

研究了应用电感耦合等离子体质谱法(ICP-MS)测定硅钢中痕量铜和镍的分析方法。采用硝酸分解样品,通过内标校正和基体匹配消除了基体干扰的影响,同时根据测量时存在的质谱干扰情况,选择同位素65Cu和60Ni作为测定元素和通过调节仪器参数使双电荷离子的产率最低,以减少带来的干扰。该方法用于硅钢中痕量铜和镍的测定,所得的结果与ICP-AES法测定结果完全吻合,各元素测定结果的RSD值小于5%,加标回收率为97.3%~100.3%。 A method for the determination trace copper and nickel in silicon steel by inductively coupled plasma mass spectrometry(ICP-MS) was studied.The samples were dissolved in HNO3.The effect of matrix interference was eliminated by internal standard correction and matrix matching.Meanwhile,according to the mass spectral interferences in determination,the isotopes including 65Cu and 60Ni were used as measuring elements.The yield of double-charge ions were minimized by adjusting instrumental parameters... 
2011-05-28 192 5.8

抑制回硅是低硅品种钢冶炼的重点和难点,南钢中厚板卷厂通过转炉出钢弱脱氧操作,精炼炉弱脱氧升温,脱氧、脱硫造渣,连铸严格的保护浇注及吹氩塞棒、吹氩浸入式上水口的应用等一系列工艺优化和操作的改进,使整个冶炼过程钢水回硅量稳定控制在200×10-6以内,钢水终点成分完全满足低硅钢要求。 Control of increasing silicon is the emphasis and difficulty in low silicon varieties steel smelting.The Nisco Wide Plate/Coil Plant can control the silicon content in molten steel keeping within 200×10-6 through whole steelmaking process by using oxygen residual operation in converter tapping,oxygen residual and increasing temperature,deoxidation,desulfurization,slag refining,protection cast,blowing argon by plugged nozzle,blowing argon by submerged entry nozzle in continuous casting,and other ... 
2013-05-28 154 5.8

{100}织构因具有两个易磁化方向能够明显的提高磁性能,因此如何在表面获得具有{100}织构一直是无取向电工钢研究焦点。本文主要介绍了获得{100}织构的主要工艺方法及其基本原理,并结合实际生产过程对各工艺方法的优缺点进行了分析;一方面,优化无取向电工钢的成分,降低碳、锰元素含量以避免脱碳退火和真空退火,简化生产工艺;另一方面,调节升温速度、降温速度和退火气氛,使{100}晶面的表面能或弹性应变能最低,制备具有{100}织构柱状晶组织的无取向电工钢是今后的发展方向。 Because { 100} texture has two easy magnetization directions,which can significantly improve magnetization properfies,how to develop { 100} texture is a focus for researchers and manufactures. In the paper,main manufacturing processes and basic principle are introdued,and their advantages and disadvantages in practical production are analyzed. On the one hand,the production process can be simplified by optimizing chemical compositions,such as reducing the content of C and Mn,which can avoid deca... 
2013-12-28 176 5.8