钢厂
高硅FeSi合金层对普通取向硅钢磁性能的影响
目的提高硅钢的磁性能。方法采用多弧离子镀技术,在普通取向硅钢薄板两面沉积高硅FeSi合金层制得高硅梯度硅钢,并进行热处理,观察其显微组织,测量磁性能。结果退火态高硅梯度硅钢表面的高硅FeSi合金层与基底结合紧密,均匀致密。高硅梯度硅钢中硅含量呈梯度分布,最表层硅质量分数为11.0%,随着深度增加,硅含量逐渐降低,在距表面20μm处硅质量分数仍能达到6.5%。沉积态高硅梯度硅钢的电阻率ρ、低频铁损P10/50、高频铁损P10/1k及磁感应强度B8分别为68.6μΩ·cm,0.82W/kg,83.3 W/kg和1.73 T,退火后分别为63.1μΩ·cm,0.44 W/kg,54.38 W/kg和1.89 T。结论由于表层高硅FeSi合金层的存在,梯度高硅钢的低频磁学性能良好,但高频损耗需进一步改善。 Objective To improve the magnetic properties of silicon steel. Methods FeSi alloy coatings with high-silicon content were deposited on the surface of common grain-oriented silicon steel by cathodic arc plasma evaporation,and then a kind of high silicon gradient steel was prepared. The morphologies,content and magnetic properties of the samples were tested. Results FeSi alloy coatings were featured with compact microstructures and excellent adhesive quality with the substrates. The silicon conten...
提高热轧硅钢凸度精度的工艺措施
以太钢热连轧厂的硅钢为研究对象,利用凸度仪测量热轧带钢出口凸度值,采用矩阵和失效模式的分析方法了解影响带钢凸度变化的主次因素。研究结果表明:通过有效控制轧制过程中的加热温度、时间及采用合理的辊型,硅钢凸度精度提高了4.34%左右。 In this paper,we take the hot-rolled silicon steelsheet of Taigang as the research symbol,exit profile was measured by convex instrument,the primary and secondary factors that affect the strip profile were measured by using matrix and failure mode analysis methed.The results indicate that convexity accuracy has significantly improved by nearly 4.34% through the effective control of the heating temperature,heating time and the use of correct roller type in the process of hot rolling.
湿H_2气氛下CGO硅钢初次再结晶织构演变行为
通过对湿H2气氛下,相同退火温度、不同退火时间的CGO硅钢初次再结晶样品进行金相组织观察,并进行了EBSD微观织构分析,研究了CGO硅钢初次再结晶过程中的组织及再结晶织构演变行为。结果表明,在湿H2气氛下,820℃保温,CGO硅钢初次再结晶过程约在120 s时完成。随着退火时间的延长,γ面上{111}<112>织构含量逐渐减少,{111}<110>织构先减少后增多,随着再结晶的完成,部分{111}<112>取向晶粒向高斯{110}<001>取向转化的同时,也向{111}<110>取向转化,高斯{110}<001>织构含量逐渐增多。高斯取向晶粒较多是由{111}<112>取向晶粒转化而来,同时也证明了CGO硅钢高斯取向晶粒的二次再结晶异常长大生长机制为择优形核。 Microstructure development and texture evolution of conventional grain oriented silicon steel,which were annealed at same annealing temperature and different annealing time under wet H2 atmosphere,were investigated through metallographic observation and electron backscattered diffraction analyzing.The results show that the primary recrystallization finishes in 120 s at 820 ℃ under wet H2 atmosphere.With the extending of annealing time,{111}<112> texture decreases,{111}<110> texture d...
冷轧无取向硅钢产品标准浅析
聚焦无取向硅钢产品标准,从电磁性能、表面性能、机械性能以及尺寸公差与边部质量等维度对国际标准IEC、EN、JIS、ASTM以及国标GB进行了分析研究。分析得出,各类标准在电磁性能方面要求基本一致;ASTM标准的机械性能要求有别于其他几个标准。 In this paper,non-oriented silicon steel standards of EN,JIS,GB and ASTM were compared and analyzed. It is showed that,all types of standards in electromagnetic performance requirements are basically the same. Surface properties in ASTM standard are expressed in the most detailed. The mechanical properties requirements of the standards,except for ASTM,are basically the same.
我国硅钢发展现状及发展趋势
硅钢是钢铁产品中的\"工艺品\",是高附加值产品,通过对我国主要硅钢生产厂家的工艺设备,市场情况分析,简要介绍了我国硅钢生产消费现状,未来生产能力预测及硅钢未来发展趋势。 Silicon steel is the \"crafts\" of steel products,also is high value-added product.By analyzing process equipment and market condition of major silicon steel-making plant of China,it briefly introduces our current production consumption status,future production capacity prediction and future development trend of silicon steel.
硅钢脱硫影响因素分析研究
对RH法(真空循环脱气法)生产的冷轧硅钢的脱硫原理及影响因素进行了分析研究。研究表明:降低顶渣中FeO、MnO的含量,提高钢液温度,增加脱硫剂的加入量并延长其循环时间有利于提高脱硫效率。 The principles of desulfurization and its influence factors of cold rolling silicon steel during RH process have been studied in this paper.The result indicated that reducing contents of FeO and MnO,rising temperature of the liquid steel,increasing quantity of desulfurizer,lengthening cycle time of desulfurzer are benefit for desulfurization.
CSP流程热轧板常化温度对冷轧无取向电工钢退火组织和磁性能的影响
研究了CSP工艺生产≤0.005%C-1.1%Si的2.2mm无取向电工钢热轧板在800~1000℃常化对0.5mm冷轧板840℃退火后组织和磁性能的影响。结果表明,热轧板常化温度升高,冷轧板退火后的再结晶晶粒增大,铁损降低,磁感增加;热轧板常化温度超过900℃,因第二相固溶而后弥散析出,退火后冷轧晶粒细化,铁损增加,因此该无取向电工钢热轧板最佳常化温度为900℃。 The effect of normalizing at 800-1000℃ of CSP produced plate(≤0.005%C-1.1%Si) on the microstructure and magnetic properties of downstream cold-rolled non-oriented electrical steel annealed at 840℃ was studied.Results show that with increasing normalizing temperature of hot-rolled material the recrystallized grain size of annealed sheet increases,iron loss reduced and magnetic induction increases.As normalizing temperature excesses 900℃,grain is refined and iron loss increases after annealing due...
硅钢CSP工程辊底式均热炉技术特点
介绍了硅钢CSP工程辊底式均热炉的技术特性,详细阐述了辊底式均热炉工艺特点。根据硅钢均热要求,通过采取不同烧嘴布置方法和燃烧控制技术,选用耐火纤维模块和绝热材料等相关技术措施,满足了出钢温度要求。 The technical specialty for roller hearth furnace of silicon steel CSP Plant was introduced,and the technology characteristics of the roller hearth furnace were illuminated in detail.According to the reheating require of the silicon steel,different burner arrangement and combustion control methods were applied,and technology measures such as selecting refractory fiber module and insulation material and so on were taken,the temperature requirement of silicon steel was met.
RH精炼添加钙合金去除硅钢夹杂物研究
采用RH精炼添加钙合金方式对硅钢进行钙处理。结果表明,钙合金添加量为0.67、1.00、1.67kg/t钢时,钢中钙含量分别为0、2×10-6、4×10-6;随着钙合金添加量增大,钢中夹杂物粒度逐渐由0~2μm向2~4、4~6μm偏移;不同钙处理条件下,钢中均存在粒径小于1μm和粒径为1~5μm的MnS、CuxS夹杂物,后者或单独存在,或同AlN、CaS夹杂复合;粒径为5~10μm区间,钢中的夹杂物基本以钙的氧、硫化物为主。与钙处理前相比,钙合金添加量为0.67、1.00、1.67kg/t钢时,粒径小于1.0μm的微细夹杂物减少幅度分别为68.06%、87.50%、94.94%。钙合金添加量为1.67kg/t钢时,可以去除钢中绝大部分的微细夹杂物。 Ca alloy was added into the liquid steel during RH refining,and the results show that Ca concentration in final Si steel sheets is insignificant,about 0,2×10-6 and 4×10-6 when the added amount of Ca is 0.67,1.00 and 1.67 kg/t steel,respectively.With the increase in the added Ca alloy amount,the inclusions in the steel gradually change from those of 0~2 μm to those of 2~4 and 4~6 μm.Under different Ca treatments,there exist MnS and CuxS inclusions whose size is below 1 μm as well as MnS and CuxS ...
云边一体化系统架构下硅钢制造管理业务数字化融合应用
提出以“云边一体化架构”构建硅钢智慧决策系统,来解决原硅钢制造L1~L5系统架构模式下的数字信息孤岛、业务功能割裂等问题。在此基础上,开发了云边协同的自学习型控制模型及业务决策模型,构建起硅钢“智慧大脑”,形成了以研发、制造、服务等核心业务数字化融合的智能化决策支持新模式,探索出一条钢铁制造业数字化、智能化转型之路。 SIDS(Silicon-steel Intelligent Decision-making System)based on \"cloud-edge integration architecture\" was proposed to solve the problems of data silos and business function fragmentation in the original L1~L5 system architecture.On this basis,the self-learning control model and decision-making model of cloud-edge collaboration were developed,the \"smart brain\" of silicon steel department was constructed,and a new intelligent decision-making support model of digital integration of core businesses s...