脉冲磁场热处理对CGO取向硅钢脱碳退火过程中组织和织构的影响
采用自主研发的脉冲磁场退火装置,在取向硅钢脱碳退火过程中分别施加不同强度的磁场,并采用光学显微镜和X射线衍射仪研究了脉冲磁场脱碳退火后试样的显微组织和宏观织构。结果表明,脱碳退火过程中施加脉冲磁场后取向硅钢的平均晶粒尺寸均增加,当磁场强度为40 mT时,平均晶粒尺寸最大,为13.06μm。此外,取向硅钢试样的立方织构{001}<100>强度减弱,高斯织构{110}<001>和{111}<112>织构增强,有利于获得更好的成品织构和磁性能。 Self-developed pulsed magnetic field annealing device was used to apply magnetic field of different intensities during decarburization annealing of an oriented silicon steel, and microstructure and macro-texture of the specimens after decarburization annealing in a pulsed magnetic field were studied by using optical microscope and X-ray diffractometer. The results show that the average grain size of the oriented silicon steel increases with the application of pulsed magnetic field during decarbu...
无取向硅钢中的夹杂物析出在线观察
借助高温激光共聚焦显微镜,在线观察了不同Mn含量的无取向硅钢中夹杂物的尺寸、类型、数量变化。结果表明,Mn含量(质量分数)为0.77%、0.32%时,试样中的夹杂物数量分别约为1000万个/mm3、1600万个/mm3。Mn含量较高的钢种,会优先析出球形、椭球形MnS夹杂物,其析出数量较少,尺寸相对较大,可以有效抑制AlN、CuxS夹杂物析出;Mn含量较低的钢种,会在试样再加热后冷却过程中,先析出相当数量MnS夹杂物,并作为AlN夹杂物析出核心,形成MnS+AlN复合夹杂物。这种复合夹杂物数量较多,尺寸也较大。 Based on the high temperature confocal microscope, the chage of size, type, and quantity of inclusions in non-oriented silicon steels with different Mn content were observed by in-situ SEM. Results show that the inclusion quantities are 10 million per mm3 and 16 million per mm3,while the mass fractions of Mn are 0.77% and 0.32%, respectively. In the silicon steel with higher Mn content, the spherical and ellipsoidal MnS inclusion will precipitate first, which can retard the precipitation of AlN ...
冷轧无取向硅钢产品标准浅析
聚焦无取向硅钢产品标准,从电磁性能、表面性能、机械性能以及尺寸公差与边部质量等维度对国际标准IEC、EN、JIS、ASTM以及国标GB进行了分析研究。分析得出,各类标准在电磁性能方面要求基本一致;ASTM标准的机械性能要求有别于其他几个标准。 In this paper,non-oriented silicon steel standards of EN,JIS,GB and ASTM were compared and analyzed. It is showed that,all types of standards in electromagnetic performance requirements are basically the same. Surface properties in ASTM standard are expressed in the most detailed. The mechanical properties requirements of the standards,except for ASTM,are basically the same.
高强无取向硅钢组织演变与强化机制
针对新能源汽车的发展,制备了含Ni固溶强化、含Cu析出强化以及含Ni+Cu复合强化3%Si无取向硅钢,研究了强化方式对无取向硅钢组织、织构和性能的影响。结果表明:固溶强化型无取向硅钢热轧板中形成了粗大{221}<221>晶粒,冷轧过程中剪切变形明显并在退火后形成良好再结晶织构。析出强化型无取向硅钢热轧板中心层形成γ取向粗大晶粒,在后续的加工中γ织构逐渐增强并最终得到相对细小的再结晶晶粒。复合强化型无取向硅钢热轧板中保留了强λ取向带状组织,退火后形成了有益的Goss织构和λ织构。固溶强化型与复合强化型无取向硅钢磁感应强度B50分别达到1.742、1.688 T,高于析出强化型无取向硅钢的1.645 T。同时,复合强化型无取向硅钢高频铁损最低,其P1.0/400和P1.0/1 000分别低至20.97、82.69 W/kg,这与其较小的晶粒尺寸和织构改善有关。强度计算结果表明:Ni元素固溶强化对强度的提高有限,屈服强度为468 MPa,纳米Cu析出可显著提高屈服强度(强度增量约200 MPa),且主要来自于模量强... For the development of new energy vehicles, 3%Si non-oriented silicon steel were processed by solid solution strengthening with Ni, precipitation strengthening with Cu, and composite strengthening with Ni and Cu. The effects of different strengthening methods on the microstructure, texture and properties of high-strength non oriented silicon steel were studied.The results show that coarse {221}<221> grains are formed in the hot rolled sheet of solution strengthened non-oriented silicon ste...
钙处理对无取向硅钢中非金属夹杂物的影响
采用电解法和扫描电镜研究了300 t转炉-RH精炼钙处理对无取向硅钢板(%:≤0.005C、1.2~2.2Si、0.2~0.6Mn、≤0.20P、≤0.005S、0.2~0.6Al、0~0.01Ca)中夹杂物的影响。结果表明,钢中Al含量为0.25%和0.35%时,钢中溶解氧均小于1×10-4%,钙处理后都会产生CaS夹杂物,尤其是含0.35%Al的钢水;钙处理可以有效减少钢中的夹杂物数量,尤其是0.5μm以下的微细夹杂物数量;钙处理后夹杂物的种类以AlN、CaS为主,同时还含有少量的氧化物夹杂物以及AlN-CaS复合夹杂物,尺寸主要为1.5~5.0μm。 The effect of 300 t converter-RH refining calcium treatment on inclusions in non-oriented silicon steel sheet (%:≤0.005C,1.2~2.2Si,0.2~0.6Mn,≤0.20P,≤0.005S,0.2~0.6A1,0~0.01Ca) has been studied by electrolysis and scanning electron microscope.Results show that with 0.25%and 0.35%Al content in steel,all the dissolved oxygen in liquid is less than 1×10-4%,and the CaS inclusions are produced after calcium treatment,especial for the liquid containing 0.35%Al;the amount of inclusions in ste...
硅钢级氧化镁反应行为的研究
利用DSC、XRD,结合热焓分析对硅钢级氧化镁和二氧化硅的固相反应行为进行了研究。比较了不同二氧化硅原料及混合方法对硅钢级氧化镁反应性的影响,找到了一种更为有效的硅钢级氧化镁反应性的评估方法,克服了传统柠檬酸活性法在比较不同厂家生产的氧化镁的反应性上的局限性。进一步研究了Na2B4O7添加剂、TiO2添加剂对氧化镁和二氧化硅反应行为的影响,结果表明,Na2B4O7添加剂含量的增加对反应有利,而TiO2添加剂对反应有阻碍作用。 The solid-state reaction behavior between silicon-steel grade MgO and SiO2 was investigated by DSC and XRD combined with enthalpimetric analysis.The influence of different kinds of SiO2 and different preparation methods were studied and a specifical measurement that is more reliable was proposed to evaluate reactivity of silicon steel grade MgO.It overcomes the limitation of the traditional citric acid activity(CAA) method,which can not be used to evaluate the reactivity of...
Fe-6.5%Si高硅钢铁芯与Epstein Square标准单片铁损检测结果对比及数据差异分析
作为一种具有优异高频铁磁性能的合金,Fe-6.5%Si(质量分数)高硅钢在高频工况条件下降损效果明显,对电气行业应用器件高频化、小型化、节能等具有十分重要的意义。通过与取向硅钢测量B-P数据对比,验证了高硅钢高频超低损特性,且轧制高硅钢与日本CVD法生产高硅钢存在基本相同的铁损值。采用国标Epstein Square法对0.30mm高硅钢薄板进行单片测试,并对由0.30mm高硅钢薄板首次装配成的电感器进行铁损测试,对比测试结果表明,元件测试与单片测试数据基本吻合,高磁感应强度条件下,元件测试结果略低于单片测试,分析原因为:线圈引起励磁压降;元件叠片间出现短路,电流增大,损耗增加;气隙板厚度过大。 As one core material with excellent high-frequency ferromagnetism,Fe-6.5%Si performs obviously reduction on core loss in high field frequency which means much to high frequency,minimization,energy conservation in electric industry.Super low loss was verified by drawing B-P curves based on detected experimental data,and which went equal to Fe-6.5%Si thin strip fabricated by CVD in Japan.Fe-6.5%Si was firstly fabricated as inductor in this research,and its core loss was determined for comparison w...
硅钢高温氧化铁皮的显微结构表征
利用电子探针面分析、状态分析及电子背散射衍射相分析技术研究硅钢高温氧化铁皮的显微结构。电子探针面分析可以直观的看出元素的分布状态,初步判断氧化铁皮的结构,而状态分析可以准确表征常规氧化铁皮中铁元素的状态,对于合金元素富集区域则通过电子背散射衍射相分析技术来标定。结果表明,高温氧化铁皮的结构主要有4层,即最外层为厚度约为10μm的Fe2O3相,次外层为Fe3O4相,中间层为FeO相上分布有颗粒状的Fe3O4相,最内层为FeO相和Si元素富集的Fe2SiO4相。其中Fe2SiO4层的分布特征与加热温度密切相关:1 100℃时,Fe2SiO4相呈颗粒状,弥散分布在FeO层;1 200℃时,Fe2SiO4相呈液态,侵入基体和疏松的FeO层,且沿着FeO晶界呈网状分布。 The microstructure of high temperature oxide scale on silicon steel was characterized by electron probe microanalyzer(EPMA)mapping analysis,state analysis and electron backscatter diffraction(EBSD)phase analysis.The element distribution and the initial structure of the oxide scale could be detected by EPMA mapping analysis apparently.And the state of iron in the conventional oxide scales could be determined by state analysis.Meanwhile,the alloy-rich region could be identified by EBSD phase analy...
无取向硅钢冶炼过程中的夹杂物遗传变化
研究表明,硅钢中的夹杂物对成品带钢的磁性能有显著影响。为研究冶炼过程硅钢中的夹杂物遗传变化,进而提出更有效的控制措施加以去除,本文结合典型的无取向硅钢生产炉次,采用非水溶液电解提取+扫描电镜观察方法分析冶炼过程中上述炉次典型试样的夹杂物。结果表明:转炉冶炼结束、RH精炼开始时,钢的氧化物夹杂总量最大,约为0.23%;RH精炼过程中,氧化物夹杂总量不断降低,并在脱碳结束时达到最低,约为0.02%;连铸过程中,氧化物夹杂总量仍有不断降低趋势,但夹杂物的平均尺寸变化不大。本试验条件下,中间包试样的夹杂物数量约为1.59×104个/mm3。 As we all know, the non-metallic inclusion effects magnetic properties of silicon steel sheets obviously. The article aims to study the heredity of non-metallic inclusion in non-oriented silicon steels during the steel making process, and then provides a more effective controlling measure to remove the inclusions. Based on the typical non-oriented silicon steel charges, the non-aqueous solution extraction and SEM observation were adopted to analyze the non-metallic inclusions. Results show that,...
球刻痕法对高磁感取向硅钢磁性的影响
试验研究了球刻痕法对高磁感取向硅钢的铁损、矫顽力、相对磁导率、巴克豪森噪声等磁学性能的影响.研究结果表明:经过球刻痕处理后,高磁感取向硅钢的铁损明显降低,矫顽力下降,8 mm球刻痕过后铁损值与矫顽力分别下降16.2%和14.7%,且铁损和矫顽力均随刻痕间距降低而减少.刻痕后的高磁感取向硅钢磁导率在高磁感应强度下明显上升,刻痕后巴克豪森噪声值明显降低,经过对比分析确定8 mm为球刻痕的最佳刻痕间距.从磁畴观察、细化磁畴的原理等方面解释了细化磁畴对高磁感取向硅钢性能的影响原因. The effects of the ball scribing on magnetic properties of high permeability grain-oriented silicon steels,including the iron loss,coercive force,relative permeability,and Barkhausen noise were investigated. The results showed that the iron loss and coercive force of the high permeability grain-oriented silicon steels apparently decreased 16. 2% and 14. 7% respectively after 8 mm ball scribing and they both decreased with the decrease of the scribing spacing at the same magnetic flux density. At...
不同尺寸电工钢样品磁性能检测对比分析
对CSP流程生产的无取向电工钢M50W800不同尺寸样品的磁性能进行了测试和分析,结果表明:采用不同单片检测的磁性能结果与标准的Epstein方圈样品检测对比,存在明显的偏差;且同一尺寸的单片纵横向样品之间相比较,对应的磁性能差异性也较大。几种不同尺寸的单片样品,以320mm×30mm尺寸的纵横向平均值最接近标准Epstein方圈样的性能值,其铁损偏差最小。 The magnetic properties of M50W800 non-oriented electrical steel produced by CSP process were tested and analyzed with samples of different sizes,showing that significant deviation existed compared to that of Epstein square circle sample.In particular,obvious difference in magnetic properties also existed between longitudinal and transverse samples of the same size.For test samples of different sizes,the average magnetic properties of 320mm×30mm samples are the closest to that of Epstein square ...