  • 未分类

利用OM、SEM、TEM等实验方法研究了卷取工艺对一种新型含铜无取向电工钢晶粒度和析出相的影响。结果表明,该电工钢热轧带卷取后的晶粒尺寸为18~24μm,在卷取过程中,热轧带中有一定数量的第二相析出,经EDS能谱及选区电子衍射分析,这些析出相主要为AlN。随着卷取工艺的变化,该电工钢的晶粒度大小变化不明显,析出相的类型、尺寸大小不发生改变,体积分数发生一定的改变。 The effects of coiling process on grain size and precipitates of a new copper-bearing non-oriented electrical steel were investigated by OM,TEM and other experimental method.The results show that the grain size of hot-rolled bands after coiling is 18~24 μm.The second phases precipitate during coiling process.They are mainly AlN by EDS spectra and selected area electron diffraction.With the change of coiling process,the grain size of the electrical steel does not change significantly;the type and... 
2011-06-28 154 5.8

借助于EBSD对比研究了常化退火对高牌号无取向电工钢热轧组织和织构演变的影响,分析了常化退火对热轧板各厚度层织构的演变规律。结果表明,常化退火改善了热轧组织的均匀性,并弱化了热轧变形的γ纤维织构。升高常化退火温度,可增大热轧板的晶粒尺寸,提高{100}和{110}织构组分占有率,有利于提高无取向电工钢成品板的磁性能。 Effects of normalizing annealing on microstructure and texture of high-grade non-oriented electrical steel hot-rolled sheet were investigated by EBSD. Emphasis was put on the effects of normalizing annealing on texture evolution in the sheet thickness. The results show that the hot-rolled microstructure homogeneity is improved and the γ-fiber texture is weakened by normalizing annealing treatment. The grain size of hot-rolled sheet and intensity of the {100} and {110} favorable texture can be in... 
2014-02-28 148 5.8

研究了取向硅钢制备过程中常见的两种冷轧工艺,主要研究了一阶段冷轧与两阶段冷轧+中间退火工艺对初次再结晶组织及织构的影响.结果表明:采用两阶段冷轧+中间退火工艺制备以Cu2S为主抑制剂的取向硅钢,其初次再结晶平均晶粒尺寸为18.1μm,高斯晶粒的体积分数为0.6%,迁移性强的重位点阵晶界(Σ5+Σ9)和高能晶界(20°~45°取向偏差角)所占比例分别为1.8%和50.4%.与一阶段冷轧工艺相比,其初次再结晶晶粒较细,且高斯晶核与特征晶界所占的比例较高,有利于高斯晶粒发生二次再结晶. Two common cold-rolling processes of grain oriented silicon steel and the effects of the single stage cold rolling and tw o-stage cold rolling w ith intermediate annealing processes on the primary recrystallization microstructure and texture w ere investigated. The results revealed that for the grain oriented silicon steel prepared under the tw o-stage cold rolling process w ith intermediate annealing w ith Cu 2 S as the main inhibitor,the average grain size of the primary recrystallization micr... 
2014-02-28 169 5.8

分析了影响脱碳效果和结晶行为的各种要素及其相互制约关系,提出了Hi-B连续退火工艺曲线,总结得出快速加热及合理稳态气氛是实现工艺制度的关键。结合实际工程,介绍了在连续退火炉设计中快速加热和气氛设计的考虑方法,并指出随着Hi-B产品的发展,如何改进这些方法将是连退工程研发的方向之一。 The factors which affect decarbonization and crystallization and the mutual restriction between them were analyzed.A complete continuous annealing process for Hi-B was put forward.As a result,the rapid heating and the proper steady atmosphere were two important factors.According to an actual project,the consider methods for designing rapid heating and proper steady atmosphere were introduced,and it is pointed that with the development of Hi-B technique,how to improve these techniques would be on... 
2011-02-28 181 5.8

介绍了烟气余热利用系统的工艺流程及控制思想,结合该系统在钢厂硅钢连续退火机组中的应用实践,估算出烟气余热利用系统每年可节约蒸汽5 040 t,经济效益良好,同时分析了该系统存在的问题及对策。 Introduced a method about the process and control of the application of waste heat system, which had been used into a silicon steel continuous annealing line and profiting a good economic benefit by saving a large number of steam every year, which has been estimated about 5 040 tons, and analyzed the problems and solutions existed in this system. 
2014-02-28 119 5.8

采用节能、环保、经济型的生产技术与工艺来制造高磁感取向硅钢目前已成为世界各大取向硅钢生产厂的研发热点。总结了国内外各大钢铁企业与研究机构采用低温板坯加热技术生产高磁感取向硅钢的开发及应用情况,概括了传统流程实现低温板坯加热技术的方法。介绍了薄板坯连铸连轧与双辊薄带连铸等短流程工艺生产高磁感取向硅钢的研发现状。在此基础上,探讨了高磁感取向硅钢生产技术与工艺的发展趋势及方向。 Utilizing energy-efficient,environmentally friendly,economic production processes and technologies to manufacture high magnetic induction grain-oriented silicon steel has become the focus of current research work.Based on using low-temperature slab reheating techniques to produce high magnetic induction grain-oriented silicon steel at both iron and steel enterprises and research institutions all over the world,the current application and exploitation was thoroughly generalized;the implementation... 
2013-03-28 135 5.8

观察了取向硅钢极薄带经冷轧至不同厚度,并经过不同工艺热处理后的显微组织及亚结构。结果表明:冷轧压下量越大,显微组织中位错密度越高,冷变形组织越多,等轴晶粒越少;增加冷轧压下量可以使试样的再结晶温度降低,当钢带厚度为0.08 mm时,在650℃退火时就能发生明显的再结晶。 Microstructure and substructure of the grain oriented ultra-thin silicon steel sheets is analyzed,which are rolled down to different thickness and treated with different heat treatment process.The result shows that there are higher dislocation density,more cold deformation structure and less equiaxed crystal grain in microstructure of the steel sheets with more cold rolled reduction.Increase of cold rolled reduction will decrease recrystallization temperature,and when thickness of the steel shee... 
2012-11-28 170 5.8

组织和织构是影响无取向硅钢性能的重要因素。为改善产品性能,研究了冷轧压下率(71.7%~87.0%)对高牌号无取向硅钢组织、织构、磁性能和力学性能的影响。结果表明,随冷轧压下率的增加,退火晶粒平均尺寸先减小后增大;高斯和立方织构强度减弱,γ纤维织构增强,α纤维织构转变为较强的α*({h, 1, 1}〈1/h, 1, 2〉)织构,并随冷轧压下率的增加而增强,同时其峰值逐渐向{111}面移动;工频铁损P1.5/50、高频铁损P1.0/400和磁极化强度J5000同时降低,屈服强度变化不大,表面硬度逐渐增加。当冷轧压下率由84.7%增至87.0%、厚度减至0.30 mm时,高频铁损降幅是工频铁损的11倍,表面硬度增幅变大。以上研究成果对硅钢减薄后织构及组织的优化提供了很好的指导。 Microstructure and texture are critical factors on non-oriented silicon steel properties. In order to improve product properties, this paper studied the effect of cold rolling reduction rate(71.7%-87.0%) on microstructure, texture, magnetic properties and mechanical properties of high-grade non-oriented silicon steel. The results show that with the increase of cold rolling reduction rate, the average size of annealing grain decreases first and then increases. The intensity of Goss and λ fiber te... 
2022-05-28 186 5.8

介绍在取向硅钢生产中抑制剂的作用以及多元抑制剂的机理和应用情况,分析多元抑制剂方案中各种元素对高磁感取向硅钢性能的影响,并根据生产实践提出了进一步研究的方向. The role of an inhibitor in the production of grain oriented silicon steel,and the mechanism of multiplex inhibitor in the production are described in the present article.In addition,the influence of various elements in the multiplex inhibitor on the performance of grain oriented silicon steel with high magnetic induction is elucidated.Further work needed in this research is also indicated. 
2013-01-28 150 5.8

对3层高硅电工钢复合板铸坯进行热轧及温轧变形加工后,采用正火、退火两种热处理方式处理,并观察轧制过程中产生的裂纹,研究不同状态下复合板的磁性能。对不同状态下的试样进行扩散退火处理,研究复合板中裂纹变化及其对磁性能的影响。结果表明:不同热处理工艺下合金内部的裂纹尺寸差异明显,裂纹尺寸对复合板的磁性能影响显著,相对于深裂纹,其他因素的影响较小;温轧变形加工后,复合板内层出现有序组织,但该有序组织在合金存在深裂纹的前提下并不能从本质上提高合金的磁性能;扩散退火工艺可以消除复合板内部的浅裂纹及微裂纹,但不能消除尺寸较大的裂纹,故而不能显著提高存在深裂纹的复合板的磁性能。 After hot rolling and warm rolling deformation processing of casting billet for three-layer high silicon electrical steel composite plate, it was normalized and annealed for heat treatment. Then, the cracks produced during the rolling process were observed, and the magnetic properties of composite plate in different states were also investigated. Furthermore, the samples in different states were subjected to diffusion annealing treatment, and the changes of crack in composite plate and their eff... 
2022-02-28 187 5.8

【作者】 严伟明; ...
2013-09-28 132 5.8

通过实验室25 kg真空感应炉冶炼和锻轧研究了0.26%~0.95%Al含量对0.5 mm 2.2%Si无取向硅钢冷轧板组织、织构和磁性能的影响。试验结果表明,0.26%~0.81%Al含量时,随钢中Al含量的增加,成品退火钢板的晶粒尺寸增加同时铁损减少;当Al含量大于0.81%时,随Al含量增加,钢板的晶粒尺寸减小,同时铁损增加。Al含量对硅钢板磁感的影响没有明显的规律。2.2%Si无取向硅钢的合适Al含量为0.48%~0.81%。 The effect of 0.26%~0.95%Al content on structure,texture and magnetic performance of 0.5 mm cold rolled sheet of 2.2%Si non-oriented silicon steel has been studied by a 25 kg vacuum induction furnace smelting,and forging -rolling in laboratory.Results show that as 0.26%~0.81%Al,with increasing Al content in steel the grain size of annealed finished sheet increases while iron loss of sheet decreases,and as Al content in steel is more than 0.81%,the grain size of sheet decreases while iron loss in... 