考虑剪应变对微孔洞损伤演化的影响,对GTN损伤模型的损伤演化机制进行修正,建立了适用于不同应力三轴度水平的损伤模型。结合隐式应力更新算法和显式有限元计算,采用VUMAT子程序实现了修正GTN模型在有限元软件ABAQUS中的数值计算。通过模拟纯剪切和剪切-拉伸两组试样的损伤演化和断裂行为,验证了修正GTN模型在不同应力三轴度承载条件下的有效性。运用修正GTN损伤模型模拟含边部缺口的带钢在轧制过程中裂纹的萌生和扩展行为,模拟结果与实验相一致,表明该模型可有效地用于带钢缺陷在轧制过程中扩展行为的分析和预测。模拟和实验结果表明,带钢边部缺口在轧制过程中,缺口前沿和后沿均会萌生裂纹,且后沿裂纹扩展更为明显。 Considering the effect of shear strain of micro-void on damage evolution, a modified GTN model applicable to various stress triaxiality conditions is proposed by modifying the damage evolution mechanism of the GTN damage model. The modified model is implemented in commercial finite element software ABAQUS by combining the implicit stress update method with an explicit finite element solving algorithm and through the user-defined material subroutine VUMAT. The damage evolution and the failure pro... 
2014-06-28 143 5.8

借助于EBSD对比研究了常化退火对高牌号无取向电工钢热轧组织和织构演变的影响,分析了常化退火对热轧板各厚度层织构的演变规律。结果表明,常化退火改善了热轧组织的均匀性,并弱化了热轧变形的γ纤维织构。升高常化退火温度,可增大热轧板的晶粒尺寸,提高{100}和{110}织构组分占有率,有利于提高无取向电工钢成品板的磁性能。 Effects of normalizing annealing on microstructure and texture of high-grade non-oriented electrical steel hot-rolled sheet were investigated by EBSD. Emphasis was put on the effects of normalizing annealing on texture evolution in the sheet thickness. The results show that the hot-rolled microstructure homogeneity is improved and the γ-fiber texture is weakened by normalizing annealing treatment. The grain size of hot-rolled sheet and intensity of the {100} and {110} favorable texture can be in... 
2014-02-28 144 5.8

为了提升新能源车用驱动电机的功率密度,各大电机厂商都在不断地提升电机转速,随之而来的问题就是电机的铁耗也在不断增高,如何降低电机铁耗成为了电机厂商必须要解决的难题。本文讨论了电机铁耗的组成部分及影响因素,并对1台8极48槽的永磁同步电机分别使用3种不同厚度的材料进行仿真,对比其效率及铁耗分布,推导出驱动电机中硅钢厚度、铁耗及成本的关系,最后对驱动电机选材提出建议。 In order to increase the power density of traction motor for new energy vehicles,major motor manufacturers have been constantly increasing the motor speed.The following problem that manufacturers have to solve is how to reduce the increasing iron loss when the motor speed is increased.The components and influencing factors of motors’ iron loss were discussed in this paper,and an 8-pole 48-slot permanent magnet synchronous motor using three different thickness materials was simulated.To compare i... 
2022-01-28 174 5.8

利用FE-SEM、EDS分析了含不同抑制剂成分的成品取向硅钢中夹杂物的组成和形貌,统计其尺寸及数量分布;结合对磁性能测试的结果,分析了Sn、Cu、Nb和Cr对取向硅钢磁性能影响的机理。结果表明:含Sn的取向硅钢试样中夹杂物主要为块状的微米级Al-Ti-C-N-O复合物,还有少量的球形Al-N-O颗粒和块状Ti-C-N-O颗粒,棒状夹杂物较少;含Cr的取向硅钢试样中夹杂物主要为球形的微米级Al2O3,还有少量Cu-Al-N-O-S复合物,棒状夹杂物和不规则夹杂物均较少;含Cr试样中1~3μm夹杂物的平均尺寸较含Sn试样小,但数量多,而大于3μm夹杂物的平均尺寸较含Sn试样大,但数量很少。磁性能测试结果表明,外场为800A/m和2500A/m时,含Cr试样磁感应强度偏低,铁损值P1.7/50较含Sn试样高,为1.171W/kg。 The composition and morphology of inclusions in the finished grain-oriented silicon steels are analyzed by using FE-SEM and EDS, and the number density and size distribution of the inclusions are counted. The influence mechanism of Sn, Cu, Nb, and Cr on the magnetic properties of the steel is also discussed. Results show that the inclusions composition in the grain-oriented silicon steel samples containing Sn is mainly block Al-Ti-C-N-O, compounding with a few spherical Al-N-O and block Ti-C-N-O... 
2014-05-28 168 5.8

针对新日铁公开的相关专利,总结日本高强度无取向电工钢的研究进展,分析了各专利化学成分、生产工艺及产品性能的特点,指出固溶强化、细晶强化、析出强化、位错强化都有可能被用来提高无取向电工钢的强度。在高强度无取向电工钢的研发过程中,需要根据其具体用途确定目标性能,再采用合适的强化手段,从而实现力学性能、磁性能和生产性能之间的平衡。 Authors summarize the research progress of high strength non-oriented electrical steel in Japan by learning related patents brought into the public by Nippon Steel. Authors also analyze the characteristics of the chemical composition, production technology and properties of products in the patents and point out that any ones of solution strengthening method, fine-grain strengthening method, precipitation strengthening method or dislocations strengthening method may be used to improve the strengt... 
2013-11-28 137 5.8

利用光学显微镜、TEM和EBSD研究了退火温度对双辊连铸无取向硅钢再结晶组织的影响。结果表明,900℃退火后组织分布不均匀,有大量带状组织,平均晶粒尺寸29.5μm。提高退火温度,晶粒尺寸增大,组织均匀化程度增加,1050℃退火时,带状组织基本消失,平均晶粒尺寸42.2μm。 Effect of annealing temperature on recrystallization microstructure of non-oriented electrical steel produced by twin-roll casting process was investigated using OM,TEM and EBSD.The results show that the recrystallization microstructure is uneven because of many banded grains existing,average grain size is 29.5 μm.With annealing temperature increasing,the recrystallization grain size increases,microstructure becomes more homogeneous.When 1050 ℃ annealing,the banded structure almost disappear and... 
2013-03-28 149 5.8

利用X-射线衍射织构分析和线形分析技术测定了交叉轧制双取向硅钢在制备工艺各阶段的织构及微结构,进而探讨了立方织构({100}<001>)的形成过程。通过对实验结果的分析可知,二次冷轧和交叉轧制工艺为立方织构提供了内能优势和有利的形变织构,而低温预退火工艺既强化了立方织构的内能优势,又为立方织构的异常长大提供了有利的组织保证,最终在抑制剂(AlN和MnS)的协同作用下,硅钢在二次再结晶退火后形成了强烈的立方织构。 The texture and substructure of the double oriented electrical steels produced by the cross rolling technology during the difference process has been measured by means of the X-ray texture and diffraction peak profile analysis technology,and research the formation mechanism of cube texture,{100}<001>.The results show that the dominances of inner energy and deformation texture were supplied by secondary cold rolling and the cross rolling technology and strengthened by pre-annealing at a low... 
2011-02-28 171 5.8

选用国内外无取向硅钢标杆企业A、B、C的产品,采用非水溶液电解提取+SEM(EDS)方法,分析了其典型牌号对应成品试样中的夹杂物。结果表明,从磁性能控制角度而言,受钢的化学成分及生产工艺影响,A、B、C企业成品试样的夹杂物尺寸、种类、数量存在差异,这些差异对其磁性能产生显著影响;从夹杂物控制角度而言,A、B、C企业对应成品试样的夹杂物,以MnS、CuxS复合或者AlN、MnS、CuxS复合为主,其中1.0μm以下的夹杂物数量分别为2.34×107个/mm3、2.98×107个/mm3和11.98×107个/mm3,1.0μm以上夹杂物数量均很少,夹杂物的平均尺寸从大到小依次为A企业、B企业、C企业。 According to the production of three benchmarking manufacture enterprises A,B and C of non-oriented silicon steel at home and abroad,the inclusions in finished steel samples with typical grades were investigated by electrolytic extraction from non-aqueous solution and SEM(EDS).Results show that,from the viewpoint of improving the magnetic properties,affected by chemical composition and production technique,the size,type and amount of inclusions in finished steel samples are various,which will af... 
2013-01-28 154 5.8

日本住友金属成功地开发了一种资源节约型高强度无取向电工钢SXRC,这种电工钢是通过固溶铌适度抑制位错的合并对消而得到一种特殊的微观组织,因此兼具很高的力学性能和磁性,特别适用于HEV、EV驱动电机转子。而且,不使用昂贵的镍就可以达到期望的强度,合金成本可控,是一种优越的资源节约型产品。 Sumitomo metal industries ltd of Japan successfully developed a type of high strength non-orientation electrical steel SXRC of resources-saving.The steel has both high mechanical performance and good magnetic property thanks to the special microstructure produced by the formation of Nb solid solution serving to appropriately inhibit the combination and cancellation of dislocations.The material is,in particular,suitable for manufacturing rotors of HEV and EV driving motors.Besides,expected streng... 
2011-06-28 139 5.8

介绍了电工钢生产线连退机组的表面处理工艺,特别是电解清洗系统的工作机理、设备构造、生产工艺及各种影响因素。 This paper introduces the technology of surface treatment of continuous annealing unit in electrical steel production line,in particular the working mechanism,structure of equipment,production techniques and various influence factors of the electrolytic cleaning system. 
2023-05-11 1.34k 5.8

采用光学显微镜、X射线衍射仪等分析了宁波钢铁有限公司生产的取向硅钢不同工序下的组织及织构演变规律。结果表明:铸坯经过热轧后,沿着厚度方向组织不均匀;一次冷轧并经脱碳退火后,组织由条状纤维状变成等轴状的初次再结晶晶粒,初次再结晶平均晶粒尺寸为18.17μm,织构主要以α织构和γ织构为主;在二次冷轧后,晶粒再次被压缩,转变为纤维状,织构主要为γ织构;经过高温退火后,发生二次再结晶,晶粒异常长大,晶粒尺寸达到厘米级,织构成分为单一且锋锐的Goss织构。 The microstructure and texture evolution of oriented silicon steel produced by Ningbo Iron and Steel Co.,Ltd.were analyzed by optical microscope and X-ray diffraction.The results showed that the microstructure of the slab was inhomogenous along the thickness direction after hot rolling.After first cold rolling and decarburizing annealing,the microstructure changed from strip fibrous to equiaxed primary recrystallized grains,and the average grain size of the primary recrystallization microstructu... 
2022-01-28 176 5.8

【摘要】 <正>编号:2012016获奖等级:特等完成单位:...