钢厂
电工钢热连轧宽度自适应模型优化及应用
某厂对电工钢的轧制策略进行了优化,粗轧道次由“1+5”改为“1+3”。在优化后的生产过程中,每次变换钢种,烫辊材就会出现窄尺现象,而紧随其后的电工钢板则出现超宽现象。文中针对该问题,介绍了宽度设定模型和宽度自适应模型的原理,阐述了该问题出现的原因及解决方案,并通过对宽度自适应模型的应用研究及优化攻关,有效地解决了问题,大幅提升了实物质量,降低了宽度封锁率。 The rolling strategy of electrical steel was optimized in a factory,and the rough rolling pass was changed from “1+5”to“1+3”.Subsequently,the following problems were occurred in the production process:when the steel grade changed,the roasting roller steel before the electrical steel appeared the narrow width phenomenon,and then the electrical steel appeared the ultra-wide phenomenon.This paper introduced the principle of width setting model and width adaptive model,and expounded the causes and s...
国产化高牌号无取向硅钢退火、涂层炉新技术
从影响高牌号无取向硅钢退火工艺的主要参数入手,介绍高牌号无取向硅钢退火炉在加热、气氛控制、冷却、涂层烘烤方面的新技术,并展望无取向硅钢退火炉的发展方向。 Based on the technology parameters of high-grade non-oriented silicon steel annealing,the new technology of the annealing line,which includes heating,atmosphere control,cooling,coating baking,is introduced,and the development direction of non-oriented silicon steel annealing furnace is pointed out.
轧制力优化对20辊冷轧硅钢厚度精度的影响
轧制力是影响冷轧带钢厚度精度的关键因素。为实现高精度的冷轧带钢厚度控制,通过优化变形抗力模型参数和摩擦系数模型参数提高冷轧轧制力模型计算精度,并使用指数平滑法的自学习算法保证轧制力精度的稳定性。在首钢股份公司迁安钢铁公司20辊森基米尔轧机生产线进行S12硅钢钢种轧制力优化试验,将优化的模型参数应用于L2并投入现场生产,结果表明该优化方法不仅提高了轧制力设定精度,而且减小了冷轧硅钢的厚度超差长度,提高了成材率。 The rolling force is the key factor which influences the accuracy of cold-rolling strip thickness. To implement high precision control of cold-rolling strip thickness,we optimize the deformation resistance model parameters and friction coefficient model parameters to improve the calculation precision of cold-rolling force model,and use exponential smoothing self-learn algorithm to ensure the stability of rolling force accuracy. In Shougang Qiangang 20-high Sendzimir mill single stand production ...
本钢高硬度无取向电工钢50BW600的研发
目前随着电工钢用户冲压设备的升级,冲压速度逐步提高,对电工钢产品的硬度和强度指标提出了更高的要求。与普通硬度级别的无取向硅钢相比,高硬度50BW600的Hv硬度提高15~20,达到125以上,同时对电磁性能指标也有较高要求。本钢通过化学成份和热轧及冷轧连退生产工艺的设计,经过小批量生产试验,满足用户要求。通过对工艺的严格控制,在大批量生产过程中,保证了产品的力学性能和电磁性的检验合格率。 Currently with upgrading of stamping equipment of silicon steel user, gradually increasing of stamping speed, propose higher demand for hardness and strength of silicon steel. Compared with conventional 50BW600, high hardness 50BW600 have higher hardness, reach greater than 125Hv. Through design of chemical composition with hot mill and annealing, production test of small quantities, stamping performance meet user request.
典型半工艺电工钢产品M660-50K5生产及应用技术解析
对欧盟市场汽车压缩机专用产品进行技术解析,对比分析了其电磁性能、退火和发蓝处理、物理性能、化学成分、应用特点等参数。探讨国内外电工钢产品应用方式的不同特点,并结合鞍钢自身工艺装备和炼钢、热轧、冷轧工艺参数介绍了其生产可行性。提供了冶金工艺流程下,后工序电工钢专业生产线及传统冷轧系统生产线两种生产方式,均能满足用户最终使用要求。 The technology of automotive compressor accommodation manufacture of European Economic and Monetary Union market was described.The magnetic properties,annealing bluing,physical properties,chemical composition,application parameters were analysed.The different characteristics of the application of electrical steel products,the feasibility of manufacture on the existing technology and equipment,steelmaking,hot rolled,cold rolled technical parameters were discussed.The professional product line of ...
硅钢车间ST机组粉尘调质与除尘系统改造
针对某硅钢车间ST机组的除尘系统除尘效率较低、排放浓度不达标、二次污染较严重的问题,通过现场调研,对除尘系统、含尘气体组分与物性参数等进行测试和分析,运用管道伴热技术改善粉尘黏性后,再选取合适的除尘器对粉尘进行除尘处理,大大地提高了系统的除尘效率。 To solve the problems of low dust removal efficiency, substandard emission concentration and severe secondary pollution, some investigations are conducted to test and analyze the dust removal system,dust-gas composition and relevant physical parameters.Moreover, dust removal efficiency is greatly improved by the use of pipe heat tracing technology and by choosing appropriate dust remover.
高牌号无取向硅钢CSP流程铸坯及热轧板的组织和夹杂物分析
2.9 mm热轧3%Si高牌号无取向硅钢板(/%:0.004 6C、3.04Si、0.32Mn、0.49Als、0.004S、0.013P、0.0042N)由CSP(Compact Strip Production紧凑式带材生产线)流程:120 t BOF-70 mm CC-热轧工艺生产。热轧终轧温度872℃,卷取温度683℃。铸坯及热轧板的组织和夹杂物的分析结果表明,铸坯组织为典型的贯穿柱状晶组织;热轧板边部为再结晶组织,中部为纤维组织带有少量再结晶晶粒;高牌号无取向硅钢的主要夹杂物为铸坯-Al2O3,AlN和Cu2S+MnS;热轧板-Al2O3,AlN,AIN+MnS和Cu2S+MnS。 The 2.9 mm hot rolled 3%Si high grade non-oriented silicon steel plate(/%:0.004 6C,3.04Si, 0.32Mn,0.49Als,0.004S,0.013P,0.004 2N) is produced by CSP(Compact Strip Production) flow sheet i.e.120 t BOF-70 mm CC-hot rolling process with end rolling at 872℃and coiling at 683℃.The analysis results on structure and inclusions in casting slab and hot rolled plate show that the structure of slab is typical trans-columnar crystal,the structure of hot rolled plate at edge is recrystallized grain and in ce...
硅钢50A1300的流变应力和临界动态再结晶行为
用Gleeble1500D模拟试验机在变形温度为950~1 200℃、应变速率为0.01~8s-1、最大变形程度为60%的条件下,对硅钢50A1300做单道次压缩试验,首先分析了不同参数对流变应力的影响,然后用回归法确定了应力模型中的变形激活能及材料常数,得到硅钢50A1300在峰值应力条件和稳态应力条件下的变形激活能分别为270.360和91.557kJ/mol,同时得到了流变峰值应力模型,模型的相关系数为0.997。最后通过作lnθ-ε图的方法找到了硅钢50A1300发生动态再结晶的临界应变量,并回归得到峰值应变量、临界应变量与参数Z/C的关系式。 To analyze the effects of different parameters on the flow stress and critical strain of the dynamic recrystallization,single-pass compression experiments were carried out with silicon steel 50A1300 specimens using a Gleeble1500D thermal simulator at a temperature range of 950-1 200 ℃ and strain rate range of 0.01-8 s-1 under the condition of maximum deformation of 60%.The average deformation activation energy is respectively 270.360 and 91.557 kJ/mol under the peak stress and steady-state stres...
微合金元素Sn、Nb、Re对无取向硅钢性能的影响
介绍了微合金元素锡、铌、稀土对无取向硅钢性能的影响,并扼要分析了这些元素对硅钢性能的影响机理:晶界偏聚元素Sn可细化晶粒提高硅钢磁性能;微合金元素Nb细化铁素体晶粒,提高硅钢的强度、韧性和塑性及磁性能;稀土元素(RE)在硅钢中的主要作用包括净化钢液、变质夹杂物、改善铸态组织和性能及微合金化,减少晶界上出现偏析的几率。 The influence of micro-alloy elements on properties of non-oriented silicon steel and the mechanism for effect of the micro-alloy elements including Sn、Nb and RE on the properties of steel are presented and analyzed in this paper.Grain boundary segregation elements Sn in steel can grain refinement and improve the magnetic properties;Micro-alloy elements Nb can refine the ferrite grain,increase the silicon steel strength,toughness and plastic;The main role of the RE in the silicon steel including...