针对新日铁公开的相关专利,总结日本高强度无取向电工钢的研究进展,分析了各专利化学成分、生产工艺及产品性能的特点,指出固溶强化、细晶强化、析出强化、位错强化都有可能被用来提高无取向电工钢的强度。在高强度无取向电工钢的研发过程中,需要根据其具体用途确定目标性能,再采用合适的强化手段,从而实现力学性能、磁性能和生产性能之间的平衡。 Authors summarize the research progress of high strength non-oriented electrical steel in Japan by learning related patents brought into the public by Nippon Steel. Authors also analyze the characteristics of the chemical composition, production technology and properties of products in the patents and point out that any ones of solution strengthening method, fine-grain strengthening method, precipitation strengthening method or dislocations strengthening method may be used to improve the strengt... 
2013-11-28 132 5.8

提出一种基于粒子群优化算法实现的硅钢涂层厚度近红外光谱检测新方法。首先,采用近红外光谱仪采集获得了硅钢表面绝缘涂层的近红外光谱,然后,采用离散粒子群算法筛选出近红外光谱数据的最佳波长变量并组成新的光谱数据,最后,建立涂层厚度的核偏最小二乘定量分析模型。实验显示,所建定量分析模型对检验样本分析的绝对误差范围为-0.12~0.19μm,最大相对误差为14.31%,完全符合现场检验需要。研究表明,离散粒子群算法可以有效地筛选出携带更多有用信息的波长变量,提高定量分析模型的分析准确度和速度,是一种有效的近红外光谱波长筛选方法,同时,近红外光谱法也是一种有效的硅钢绝缘涂层厚度检测方法。 A novel thickness measurement NIR spectrometry for surface insulation coating of silicon steel based on discrete binary particle swarm optimization(DBPSO) algorithm is presented.First,we used NIR spectrometer to collect the NIR spectra of insulation coating of silicon steel,and then,DBPSO algorithm was used to select the optimal wavelength variates and composed a new spectra set.Last,the authors created the thickness quantitative analysis model using kernel partial least square algorithm.The exp... 
2011-09-28 116 5.8

利用EBSD技术研究了电工钢中不同的柱状晶尺寸及退火工艺下{100}织构的演变规律。结果表明,初始晶粒尺寸的影响最显著。细小柱状晶热轧后经过常化处理,组织已均匀,但中心层有强{100}织构。粗大柱状晶中{100}织构的遗传性强,常化及中间退火后,中心层仍有粗大的以{100}取向为主的晶粒;脱碳退火后才能完成组织均匀化和织构梯度的弱化。常化时的升温速度也对织构演变存在影响,低的升温速度有利于{100}织构的保留,但升温速度的影响没有初始晶粒尺寸及退火次数的影响显著。细小柱状晶样品经过热轧及三次退火工艺适合制备取向电工钢。 Evolution of {100} texture of different columnar grains and annealing process was investigated in electrical steels with the help of EBSD technique.The results show that the effect of initial grain size is the strongest.The initial fine-grained specimen shows uniform microstructure after the normalizing process,while {100} grains appear preferentially in the central layer of sheets.The heredity of {100} texture in the initial coarse-grained specimen is more significant.{100} mainly-oriented coar... 
2013-08-28 153 5.8

针对攀钢高硫铁水冶炼现状,结合不同生产工艺路线,论述了攀钢近年来为实现低硫电工钢的生产,在铁水预处理、转炉冶炼、钢水精炼过程中硫控制技术的开发与应用,形成了低硫洁净钢生产工艺技术,实现了低硫电工钢的生产。低硫电工钢RH脱硫率可达到20%左右,成品[S]控制在0.006%左右。 According to the smelting situations of hot metal with high sulphur content at Panzhihua Steel,combined with different produce processes,technologies for controlling the sulfur content during hot metal pretreatment,converter smelting,and second refining are developed. Technologies in low-sulfur clean steelmaking are formed. Low-sulfur electric steel are produced. As for the desulfurization rate of lowsulfur electric steel can reach about 20%,and the content of [S] in products is controlled to ab... 
2013-03-28 148 5.8

采用ZMLMC超高梯度定向凝固装置,研究了5种凝固速率(10、35、80、150和450μm/s)对定向凝固50W600无取向硅钢的固液界面稳定性转变规律和一次、二次枝晶间距的影响。研究结果表明,在特定的温度梯度下,随着凝固速率的增加,定向凝固的固液界面由胞状晶转变为胞状枝晶,再转变为细小的树枝晶。随着凝固速率的增加,定向凝固组织的枝晶形貌逐渐细化,一次和二次枝晶间距逐渐减小,且与冷却速率之间都符合指数关系:λ1=151.73×(G L·R)-0.31,λ2=22.07×(G L·R)-0.44。当冷却速率达到4.275℃/s时,一次、二次枝晶间距分别为112μm、14.1μm。 Under the conditions of certain temperature gradient and different solidification rate,the directional solidification experiment of non-oriented electrical steel 50W600 was carried out.The microstructure of 50W600 steel was also analyzed in different solidification rate.The result shows that the solid/liquid interface of the steel undergoes an evolution from cellular,cellular dendrite and finally to fine dendrite morphologies.The dendrite refines gradually and the distance between dendrites decr... 
2013-11-28 130 5.8

【作者】 谌剑; ...
2011-09-28 110 5.8

森吉米尔二十辊轧机是冷轧电工钢的主要机型,具有整体刚度大,辊径小,轧制道次压下量大,产品精度高等特点,简要介绍了近年来冷轧电工钢森吉米尔二十辊轧机领域进展,在轧机结构、厚度自动控制、板形自动控制等方面的技术及研究。 20-h Sendzmir reversible mill is the main type of cold rolled electrical steel which has the characteristic of high integral stiffness,small roller diameter,high pass reduction and high product quality.In this paper,the recent progress of frame structure,automatic gauge control,automatic flatness control of Sendzmir mill is introduced. 
2023-05-06 207 5.8

利用场发射电镜及能谱仪研究了取向电工钢薄、厚板坯铸锭中不同区域的析出相差异,确定了MnS、AlN及Fe3C的析出顺序和形貌特征。结果表明AlN以先析出的MnS为形核核心,形成粗大微米级的复合析出相。针状Fe3C既可以在复合析出相表面形成也可以在基体中单独出现,主要受冷却速度的影响。在1250℃保温1~2 h,AlN、Fe3C均可完全回溶,但部分MnS仍不回溶。MnS尺寸随着保温时间延长而增大。导致热轧板中沿轧向分布的粗大MnS,减弱了粒子钉扎力。 Precipitates in thin and thick slabs of electrical silicon steel were investigated by means of field emission SEM and EDS analysis.The precipitation sequence and the morphology of MnS,AlN and Fe3C particles were identified.AlN particles are observed to be nucleated on surface of MnS forming micron-meter-sized complex particles.Acicular Fe3C can precipitate on surface of the complex MnS/AlN particles or directly from matrix depending on cooling rate of the slabs.After holding at 1250 ℃ for 1-2 h,... 
2011-08-28 139 5.8

绝缘涂层可以有效提高硅钢片的耐蚀、耐腐、磁、绝缘等性能,因此取向硅钢涂装绝缘涂层是取向硅钢生产过程中重要的一环。本文对取向硅钢含铬无机绝缘涂层以及氮化铬涂层的性能优缺点进行了介绍,并对国内无机含铬取向硅钢绝缘涂层及氮化铬涂层的研究现状进行了综述。最后对未来含铬无机绝缘涂层的研发方向进行了展望。 Insulation coating can effectively improve the corrosion resistance of silicon steel sheet, such as corrosion, magnetic, insulation performance, thus oriented silicon steel insulation coating is the important part of oriented silicon steel production process. In this paper, the inorganic insulation coating oriented silicon steel containing chromium and chromium nitride coating performance advantages and disadvantages are introduced.In addition, the research status of insulation coating and chrom... 
2022-02-28 166 5.8

对w(Si)=3%无取向硅钢进行表面机械研磨处理(SMAT)和异步轧制(CSR),获得表面纳米结构,再进行550~650℃、4 h固体粉末渗硅处理,用透射电镜(TEM)、扫描电镜(SEM)和X射线衍射仪(XRD)研究表层组织演变。结果表明:经过SMAT后,w(Si)=3%无取向硅钢表面形成了等轴状、取向呈随机分布的、晶粒尺寸为10 nm的纳米晶组织;异步轧制后,表面纳米晶组织保持不变;550~650℃、4 h渗硅处理后,SMAT+CSR样品表面形成化合物层,其厚度随着温度的升高由17μm增加到52μm;化合物层由Fe3Si和FeSi相组成. Nanostructured surface layer was fabricated on a 3%(mass fraction) non-grain oriented silicon steel by means of surface mechanical attrition treatment(SMAT) and cross-shear rolling(CSR),and then a solid powder siliconizing treatment was carried out for the SMAT+CSR sample at 550~650 ℃ for 4 h.The microstructural evolution was examined by using transmission electron microscopy(TEM),scanning electron microscopy(SEM) and X-ray diffraction(XRD).Experimental results show that: equiaxed nanocrystallin... 
2011-03-28 140 5.8

以马鞍山钢铁集团公司电工钢板形优化控制研究项目为背景,系统地研究了热轧、冷连轧和单机架轧机在电工钢生产过程中的边缘降控制问题。通过现场数据采集、工况数值模拟计算和工业化大生产试验,设计出适用、合理的电工钢板形控制的辊型优化曲线,满足了不同工序、不同机型的板形控制策略要求,解决了电工钢板形质量问题,取得了显著的经济效益。 Based on the project of electric steel strip shape optimization control,problem of edge drop control was systematically studied in production of electric steel of hot-rolling mill,cold-rolling mill and single stand mill.Roll optimization contour was designed out in point and reasonable by collection of work condition data,numerical simulation and test of industrial production.The shape control system can meet with the different working steps and difference mills,and quality problem of electric s... 
2011-02-28 148 5.8

针对硅钢连续生产线设备存在的故障、隐患以及精度等影响产品质量的问题进行分析及改造,实现保证生产线设备稳定运行、提高设备精度及硅钢产品质量的目的。 This paper analyzes and transforms the electrical equipment failures, risks existed in slicon continuous production line, and the effect of accuracy to product quality, in order to ensure stable operation of equipment in production line and improve the accuracy of device, quality of silicon. 