6.5%Si硅钢具有优异的磁学性能和广泛的应用前景。本文综述了6.5%Si硅钢的物理、机械及磁学特性,讨论了传统轧制、温轧、薄带连铸、快速凝固、CVD、粉末轧制等不同制备工艺的关键技术及特点,概括了6.5%Si硅钢在高效节能电机、汽车马达及磁屏蔽等领域中的主要应用,介绍了硅钢的制备技术取得的研究进展,并指出了其广阔的发展前景。 6.5% Si silicon steel has good magnetic properties and wide applications.In this paper physical and mechanical magnetic properties were summarized,and key technology and characteristic of several preparation methods,such as traditional rolling,warm rolling,thin strip continuous casting,rapid solidification,CVD and powder rolling,were discussed.Main applications of 6.5% Si steel in the fields of high-efficiency electrical motors,automobile motors,transformer cores and magnetic shielding were gene... 
2012-06-28 141 5.8

薄带连铸流程下取向硅钢粗大λ晶粒(〈100〉//ND,normal direction)的“遗传”会导致磁性能恶化.为解决这一问题,针对取向硅钢的热轧孪生行为开展研究,结果表明:凝固组织粗大的取向硅钢在650℃热轧时可产生大量{112}〈111〉形变孪晶,这与具有高层错能的硅钢在较高温度下难以孪生变形的传统认知不同.热轧过程中复杂的应力状态降低了变形孪晶的取向依赖性,由于具有更高的储存能,孪晶界/孪晶界及孪晶界/晶界交叉点成为再结晶形核的优先位置,大大提高了常化过程中的再结晶率,受沿孪晶界应变分布及孪晶间距离的限制,沿孪晶界形核的再结晶晶粒通常呈“饼状”,最终形成以细小且取向漫散的再结晶晶粒为主的常化组织,消除了初始凝固组织中有害的粗大λ晶粒. In strip casting grain-oriented silicon steels, the inheritance of coarse λ grains(〈100〉//ND, normal direction) can deteriorate their magnetic properties. To solve the problem, twinning behaviors in strip casting grain-oriented silicon steels during hot rolling were investigated in this work. It is found that after rolling at 650 ℃, a number of {112}〈111〉deformation twins are formed in the coarse solidification microstructure of the steels, in contrast to the well-accepted view that it is diffic... 
2022-02-28 179 5.8

提出了一种基于爱泼斯坦方圈族(包括标准25cm爱泼斯坦方圈、缩比的17.5cm和20cm爱泼斯坦方圈)和二级加权处理方法对爱泼斯坦测试数据,包括有效磁路长度、比损耗、励磁功率,进行处理的晶粒取向电工钢磁性能扩展模拟方法。详细地考察了励磁频率、试样剪切角度和环境温度对爱泼斯坦方圈测量结果的影响。研究结果表明,利用本文提出的爱泼斯坦方圈组合以及二级加权处理技术,可以有效地建立取向电工钢损耗模拟模型,从而更加准确地确定了取向电工钢的损耗,改善并提高了爱泼斯坦磁性能测试数据的应用价值。 The extended modeling of the magnetic properties of GO(grain oriented) electrical steel is presented in this paper which is based on a set of standard and scaled-down Epstein frames and a proposed two-level weighted processing of Epstein data, including the mean magnetic path length, specific magnetization loss and exciting power. The effects of excitation frequency, strip angle and ambient temperature on the results obtained from the Epstein frames are investigated. It is shown that using the p... 
2014-09-28 141 5.8

【摘要】 <正>编号:2012016获奖等级:特等完成单位:...
2012-11-28 144 5.8

对西昌钢钒炼钢厂200 t BOF(顶底复吹)-RH-CC工艺生产50PRW800无取向硅钢RH精炼过程中主要成份进行了分析。找出了目前工艺中影响钢液质量的主要因素是钢水脱氧处理不彻底,造成加入的部分硅元素烧损。操作工艺改为铝的脱氧即合金化操作一步完成,保证了钢水中氧处于一个较低的范围,从而减少对硅元素的烧损,提高合金收得率。 The factors of BOF-RH-CC process affecting the compositions of liquid steel were systematically investigated and studied of Xichang Steel and Vanadium Company. The main factors affecting the steel cleanliness were picked out. All results showed that the loss of silicon elements resulting from the deoxidization of liquid steel was not completely. It was suggested that the addition of aluminum for deoxidizing and alloying of molten steel was executed as one step in order to lower the oxygen potent... 
2014-03-28 152 5.8

【作者】 彭志华; ...
2023-05-09 187 5.8

通过微观组织表征、高温拉伸和断口形貌分析,研究了钇(Y)元素对6.5%Si无取向硅钢组织、高温拉伸及断裂机制的影响。研究结果表明,添加Y元素可以在钢液中形成YS和YP的复合析出。YS和YP可以充当异质形核基底,提高形核率,细化凝固组织。热轧组织不均匀,由表层至芯部分别形成等轴晶、等轴晶/拉长晶和拉长晶的混合组织。退火后,热轧变形组织转变为等轴晶,含Y实验钢的退火组织得到明显细化。500℃时效处理后,含Y实验钢具备较低的有序度,300℃的拉伸断口呈现韧性断裂特征,断后伸长率达到20.2%。相反,无Y实验钢发生脆性断裂,断后伸长率仅为2.1%。研究结果证实,Y元素可以通过组织细化和降低有序度提高6.5%Si无取向硅钢的中温塑性。 The effects of yttrium(Y)on microstructure,elevated-temperature tensile properties and fracture mechanism of 6.5% Si non-oriented electrical steel were investigated by means of microstructure characterization,high-temperature tensile test and fracture analysis.The results showed that the doping of Y introduced composite Y-rich precipitates(YS/YP)in the melt.YS and YP precipitates were qualified for heterogeneous nucleation agents,which thus raised the nucleation rate and refined the solidificati... 
2022-01-28 163 5.8

【机构】 中国金属学会电工钢分会; ...
2011-06-28 111 5.8

综述了电工钢从生产到成品过程中涉及到的检测项目、检测方法及仪器,并通过对电工钢标准的发展改进,详细阐述了我国现有的电工钢技术标准体系,同时对代表企业的电工钢重点指标进行了摘录对比,为综合应用电工钢检测方法并促进电工钢的发展提供了一定的参考。 This article summarizes the testing items,methods,and instruments involved in the process from manufacturing to finished products of electric steel. The current electric steel technical standards system in our country is also elaborated in detail,along with the development and improvement of electric steel standards. Meanwhile,by comparison of electric steel KPI in representitive companies,this article provides references for comprehensive application of electric steels testing methods and promo... 
2014-05-28 139 5.8

本文介绍了无取向硅钢C6涂液的性能,研究了配水量、固化程度和涂层厚度等因素对无取向硅钢C6涂层性能的影响。结果表明,随着配水量的增加,完全固化所需的时间增加,涂液固体含量降低,涂层厚度减小;随着固化程度的提高,涂层硬度先增大然后趋于恒定,而柔韧性逐渐变差,在过固化后急剧恶化;涂层厚度对涂层的表面外观、附着性和绝缘层间电阻均有显著影响。 Based on the introduction about the performance of C6 varnish for non-oriented silicon steel sheets,effects of water amount,curing degree and coating thickness are discussed. Results show that with the increase of water amount,the time required to cure completely extends,and both the solid content of C6 varnish and the coating thickness decrease. As the curing degree increases,the hardness of the coating increases first and then tends to be constant,however the flexibility degenerates,especially... 
2014-02-28 166 5.8

无取向硅钢的磁性能主要取决于铁素体的晶粒尺寸、晶体织构和钢中的夹杂物。通过合适的化学成分设计以及采用适宜的夹杂物控制技术,可以获得最佳的夹杂物控制效果,使其纯净度大幅度提高或者无害,最终获得磁性能优良的高级别无取向硅钢。同时,为满足节能、环保、高效需求,无取向硅钢正朝着节能降耗、环境友好以及多功能、高效率、易加工等方向发展。 The magnetic properties of non-oriented silicon steel mainly depend on the grain size of ferrite,the crystallographic texture,and the inclusions in the steel.The optimum inclusion control effects can be obtained through a suitable chemical composition design and an appropriate inclusion control technique,and then the liquid steel will get be clean or the inclusion will get be harmless,finally the excellent magnetic property of the non-oriented silicon steel can be obtained.Meanwhile,in order to ... 
2013-03-28 156 5.8

试验研究了0.3 mm取向硅钢冷轧板(/%:0.046C,3.07Si,0.09Mn,0.029P,0.004S,0.005A1)的退火温度(760~880℃7 min)和退火时间(820℃3~9 min)对该钢的晶粒尺寸,再结晶和织构的影响。结果表明,最佳初次再结晶退火工艺为820℃5 min,该钢的平均晶粒尺寸为14.20μm,完全再结晶率为92%,不利{111}<110>结构含量为3.16%,有利织构{111}<112>,{012}<001>和高斯织构含量分别0.40%,4.73%和2.46%。 The effect of annealing temperature(at 760 ~ 880 X.for 7 min) and time(at 820℃ for 3~9 min) on grain size,recrystallization rate and texture of 0.3 mm cold-rolled sheet of oriented silicon steel(/%:0.046C,3.07Si,0.09Mn,0.029P,0.004S,0.005Al) has been tested and studied.Results show that with optimum recrystallized annealing at 820℃ for 5 min,the silicon steel average grain size is 14.20 fun,the complete recrystaUization rate is 92%,the unfavourable-texture {111}< 110 > content in steel is ... 