以马鞍山钢铁集团公司电工钢板形优化控制研究项目为背景,系统地研究了热轧、冷连轧和单机架轧机在电工钢生产过程中的边缘降控制问题。通过现场数据采集、工况数值模拟计算和工业化大生产试验,设计出适用、合理的电工钢板形控制的辊型优化曲线,满足了不同工序、不同机型的板形控制策略要求,解决了电工钢板形质量问题,取得了显著的经济效益。 Based on the project of electric steel strip shape optimization control,problem of edge drop control was systematically studied in production of electric steel of hot-rolling mill,cold-rolling mill and single stand mill.Roll optimization contour was designed out in point and reasonable by collection of work condition data,numerical simulation and test of industrial production.The shape control system can meet with the different working steps and difference mills,and quality problem of electric s... 
2011-02-28 182 5.8

以构建高磁感、低铁损、免轧制高硅电工钢铁芯为出发点,提出采用单辊甩带制备非晶铁硅合金薄带、微氧化法在铁硅合金粉末表面包覆高电阻率铁硅氧化物薄膜制备核壳异质结构高硅电工钢纳米粉末、放电等离子烧结快速成形制备颗粒间绝缘的高硅电工钢铁芯。研究了不同氧化包覆时间对SPS烧结试样密度、物相组成、微观结构和静磁性能的影响。研究表明,在氧化包覆5h烧结温度800℃工艺条件下,制备的6.5%Si高硅电工钢铁芯的静磁性能最佳,饱和磁化强度为128.84A.m2/kg、矫顽力为2.25kA/m、剩磁为3.47A.m2/kg。其饱和磁化强度与粉末压延法制备的高硅钢相当,但矫顽力降低了1/3。 The paper takes preparation 6.5%Si steel with high induction,low core loss and removing rolling as the starting point,amorphous Fe-Si ribbons was synthesized by melt spinning method,6.5%Si steel nanopowders with high resietivity core shell structure was prepared by the slight oxidation process and 6.5% Si steel iron core with evaluating internal was sintered by spark plasma sintering process(SPS).The essay focuses studies the effects of different oxidation cladding time on sample density,phase c... 
2013-10-28 151 5.8

【作者】 吴清; ...
2013-06-28 126 5.8

6.5%Si硅钢具有优异的磁学性能和广泛的应用前景。本文综述了6.5%Si硅钢的物理、机械及磁学特性,讨论了传统轧制、温轧、薄带连铸、快速凝固、CVD、粉末轧制等不同制备工艺的关键技术及特点,概括了6.5%Si硅钢在高效节能电机、汽车马达及磁屏蔽等领域中的主要应用,介绍了硅钢的制备技术取得的研究进展,并指出了其广阔的发展前景。 6.5% Si silicon steel has good magnetic properties and wide applications.In this paper physical and mechanical magnetic properties were summarized,and key technology and characteristic of several preparation methods,such as traditional rolling,warm rolling,thin strip continuous casting,rapid solidification,CVD and powder rolling,were discussed.Main applications of 6.5% Si steel in the fields of high-efficiency electrical motors,automobile motors,transformer cores and magnetic shielding were gene... 
2012-06-28 175 5.8

考虑剪应变对微孔洞损伤演化的影响,对GTN损伤模型的损伤演化机制进行修正,建立了适用于不同应力三轴度水平的损伤模型。结合隐式应力更新算法和显式有限元计算,采用VUMAT子程序实现了修正GTN模型在有限元软件ABAQUS中的数值计算。通过模拟纯剪切和剪切-拉伸两组试样的损伤演化和断裂行为,验证了修正GTN模型在不同应力三轴度承载条件下的有效性。运用修正GTN损伤模型模拟含边部缺口的带钢在轧制过程中裂纹的萌生和扩展行为,模拟结果与实验相一致,表明该模型可有效地用于带钢缺陷在轧制过程中扩展行为的分析和预测。模拟和实验结果表明,带钢边部缺口在轧制过程中,缺口前沿和后沿均会萌生裂纹,且后沿裂纹扩展更为明显。 Considering the effect of shear strain of micro-void on damage evolution, a modified GTN model applicable to various stress triaxiality conditions is proposed by modifying the damage evolution mechanism of the GTN damage model. The modified model is implemented in commercial finite element software ABAQUS by combining the implicit stress update method with an explicit finite element solving algorithm and through the user-defined material subroutine VUMAT. The damage evolution and the failure pro... 
2014-06-28 173 5.8

两炉次无取向硅钢XG800WR(/%:0.003~0.004C、0.71~0.75Si、0.32~0.33Mn、0.004~0.007S、0.016P)的炼钢流程为铁水预处理(KR)-210 t顶底复吹转炉-钢包吹氩-RH脱碳精炼-230mm×1220 mm板坯连铸。53 t中间包钢水过热度为25~30℃,钢包到中间包采用长水口全程吹氩保护浇铸,中间包至结晶器采用浸入式水口浇铸。结果表明,在RH、中间包、结晶器过程中钢中总氧以及夹杂物数量和尺寸均明显降低;但在钢包到中间包过程T[O]、[N]和钢中夹杂物数量增加,说明长水口浇铸过程存在二次氧化。连铸坯中T[O]、[N]平均他分别为11×10-6和30×10-6,显微夹杂物数量平均为4个/mm2。铸坯中的显微夹杂物主要为3~5μm的AlN,同时存在少量的MnS、Al2O3·AlN和Al2O3·MgO·MnS。 The steelmaking flow sheet for two heats non-oriented silicon steel XG800WR(/%:0.003~0.004C. 0.71~0.75Si,0.32~0.33Mn,0.004~0.007S,0.016P) is hot metal pretreatment(KR)-210 t top and bottom combined blown converter-ladle argon blowing-RH decarburization refining-230 mm×1 220 mm slab casting.The superheating extent of liquid in 53 t tundish is 25~30℃,whole casting is shielded by blowing argon with long nozzle from ladle to tundish and the submerged nozzle is adopted in casting from tundish to mold... 
2011-05-28 188 5.8

【作者】 O.M.Гбанов; A.E.Чеглов; ...
2014-03-28 122 5.8

Fe-6.5%Si高硅钢是一种具有高磁导率、低矫顽力和低铁损等优异软磁性能的合金,但是其室温脆性和低的热加工性能严重影响了其在工业领域的应用。综述了Fe-6.5%Si高硅钢的性能,评述了合金的改性法、特殊轧制法、快速凝固法、沉积扩散法、粉末冶金法等制备工艺。 It is well known that 6.5%Si high silicon steel is one kind of soft magnetic materials with higher re-lative permeability,lower coercive force and iron loss than those of conventional industrial silicon steel.However,their room-temperature embrittleness and poor workability limit their practical applications in the industry.The pre-paration technique such as modification treatment on alloy,special rolling,rapid solidification,CVD and powder me-tallurgy is reviewed. 
2023-05-09 239 5.8

简述了无取向硅钢环保涂层发展背景,分析了硅钢环保涂层的特点及国内、外研究进展,提出了硅钢保涂层下一步的发展方向。 The back ground of environmental protection coating of non-oriented silicon steel was described in this paper.The characteristics and study progress in domestic and foreign of environmental protection coating of non-oriented silicon steel were analysised.The next development direction of environmental protection coating of non-oriented silicon steel was put forward. 
2013-04-28 186 5.8

分析了电感耦合等离子体发射光谱法(ICP-AES)测定硅钢中铌的检测过程,讨论了该检测过程中不确定度的主要来源,建立了该方法的定量的数学模型,并根据这一模型计算出了检测结果的合成标准不确定度和扩展不确定度。 The measurement of niobium content in silicon steel by inductively coupled plasma atomic emission spectrometry(ICP-AES) was analyzed,by which the main factors affecting the uncertainty of the measurement were ascertained and the calculation formula was given.Finally,according to the formula the combined uncertainty and expanded uncertainty were obtained. 
2023-05-12 1.4k 5.8

为了提升新能源车用驱动电机的功率密度,各大电机厂商都在不断地提升电机转速,随之而来的问题就是电机的铁耗也在不断增高,如何降低电机铁耗成为了电机厂商必须要解决的难题。本文讨论了电机铁耗的组成部分及影响因素,并对1台8极48槽的永磁同步电机分别使用3种不同厚度的材料进行仿真,对比其效率及铁耗分布,推导出驱动电机中硅钢厚度、铁耗及成本的关系,最后对驱动电机选材提出建议。 In order to increase the power density of traction motor for new energy vehicles,major motor manufacturers have been constantly increasing the motor speed.The following problem that manufacturers have to solve is how to reduce the increasing iron loss when the motor speed is increased.The components and influencing factors of motors’ iron loss were discussed in this paper,and an 8-pole 48-slot permanent magnet synchronous motor using three different thickness materials was simulated.To compare i... 
2022-01-28 199 5.8

硅钢连续退火线是无取向硅钢生产的成品线。由于受机组布置的影响,带钢经转向辊进出口活套后,当套量达到60%后就出现偏离生产线的情况,从而影响最终产品的质量及成材率,甚至损坏设备。针对某冷轧厂硅钢连续退火机组出口活套入口处带钢跑偏开展纠偏研究,利用Matlab对该纠偏系统进行动态仿真研究,分析系统的稳定性。 Silicon steel continuous annealing line is non oriented silicon steel production of finished product line.Due to the influence of unit layout,strip by roll Import & Export loop,when the set volume reached 60% after the emergence of deviation from the production line,thus affecting the quality of the final product and the rate of finished products,and even damage the equipment.For the export of continuous annealing line in cold rolling silicon steel strip deviation rectification loop at the e... 
2014-06-28 171 5.8