钢厂
常化和退火工艺对冷轧无取向硅钢高频磁性能和强度的影响
冷轧无取向硅钢(/%:0.003C,2.35Si,0.22Mn,0.011P,0.002S,0.36A1,0.003 0N)经890℃或940℃3 min常化的2.3 mm热轧板冷轧成0.35 mm薄板。研究了常化温度和800920℃3 min退火对该钢高频(400Hz)磁性能和抗拉强度的影响。结果表明,830920℃退火时高频铁损P10/400值最低,随退火温度增加,晶粒尺寸增大,钢的抗拉强度降低;该钢的最佳热处理工艺为常化温度940℃,退火温度830℃,其抗拉强度Rm、高频铁损P10/400和磁感应强度J50分别为565 MPa,21.5 W/kg和1.69 T。 The cold-rolled non-oriented silicon steel(/%:0.003C,2.35Si,0.22Mn,0.011P,0.002S,0.36A1,0.003 0N) is cold-rolled to 0.35 mm sheet from 2.3 mm hot-rolled plate normalized at 890 ℃ or 940℃ for 3 min.The effect of normalizing temperature and annealing process at 800 920 °C for 3 min on high frequency(400 Hz) magnetic properties and tensile strength of the steel has been tested and studied.Results show that with annealing at 830 920 ℃the high frequency iron loss value P10...
B元素对高牌号无取向硅钢热轧板组织和性能的影响
借助实验室设备研究了B元素对高牌号无取向硅钢热轧板组织和磁性能的影响。结果表明,与无硼钢相比,含硼钢的热轧板晶粒尺寸略小,析出物的类型和尺寸没有区别,主要是AlN和(AlN+MnS)复合析出物,少量的MnS析出物,尺寸集中在1.0~2.5μm范围内。未发现BN析出物。在力学性能方面,B对钢的软化作用不明显。在磁性能方面,含硼钢的铁损为3.215W/kg,磁感为1.710T,综合磁性能比无硼钢差。 Influences of boron on microstructure and properties of hot rolled band in high-grade non-oriented silicon steel are researched in this paper by experimental equipments.Compared with boron-free steel,the result shows that boron-bearing steel has smaller grain size,but the type and size of precipitations have no differences.The main precipitates are AlN,(MnS + AlN) composite precipitate and few MnS,the range of which are between 1.0 μm and 2.5 μm.BN precipitation is not found.With reward to mecha...
稀土处理无取向硅钢中的夹杂物与电磁性能变化
结合工业化生产的无取向硅钢,进行了RH精炼添加稀土合金实验。结果表明,1.15%(质量分数)Si钢的脱硫反应,主要发生在添加稀土合金之后的前5min。最佳的稀土合金添加量为0.6~0.9kg/t钢。钢液经过稀土处理后,加入的稀土总量越多,稀土氧硫化物夹杂物的尺寸就越大,但热轧带钢再结晶效果会逐渐变差,成品带钢晶粒尺寸先是快速长大,而后逐渐减小。最佳的钢中存留稀土含量与钢的化学成分有关,应严格控制在2.0×10-3%~6.0×10-3%(质量分数)。在此范围内,钢的铁损先是快速降低,而后缓慢升高,钢的磁感应强度则单调降低。 Based on the industrial production of non-oriented electrical steel,rare earth(RE) alloy treatment during the RH refining process was studied.The results showed that the effects of desulfurization and total concentration of RE remained in steel mainly depended on the chemical compositions of different steel grades.For 1.15wt% Si steel grade,the desulfurization reaction mainly focused on the initial 5min after RE alloy added during the RH refining process.The suitable RE alloy addition was 0.6-0....
陶瓷辊除瘤方法在瑞致电工钢的应用
针对陶瓷辊表面结瘤清除时间长、清除效果差等缺陷,研究正反转陶瓷辊除瘤法,以缩短除瘤时间,增强除瘤效果。 The general removal of ceramic roller surface tumor costs a long time and the effect is poor.This paper probed into the ceramic roller tumor removal in order to shorten time and enhance the effect of eliminating.
无铬无取向硅钢涂层烧结固化工艺
为进行磷酸盐系无铬无取向硅钢涂层烧结固化工艺研究,首先对磷酸盐系无铬无取向硅钢涂层进行热重-差示扫描量热(TG-DSC)分析;然后在不同烧结固化温度条件下,测定涂层板温随时间变化曲线;最终获得涂层烧结固化温度与时间(T-t)工艺曲线。通过中性盐雾试验、动电位极化、交流阻抗、涂层附着力以及扫描电子显微镜(SEM)和能谱(EDS)分析验证。结果表明,根据涂层烧结固化温度与时间(T-t)工艺曲线制备的涂层结构致密、性能优异,证明该工艺曲线具有合理性与正确性。 In order to study the curing process of chromium-free non-oriented silicon steel coatings,phosphatic chromium-free non-oriented silicon steel insulating coating was prepared and TG-DSC analysis of the coating was conducted,then the change of the actual temperature of the coated non-oriented silicon steel sheet with time at different curing temperatures was studied. Based on the experiments,the processing curves of curing temperature vs. curing time( T-t) for the chromium-free non-oriented silico...
表面机械研磨/异步轧制无取向硅钢薄带的渗硅行为
对w(Si)=3%无取向硅钢进行表面机械研磨处理(SMAT)和异步轧制(CSR),获得表面纳米结构,再进行550~650℃、4 h固体粉末渗硅处理,用透射电镜(TEM)、扫描电镜(SEM)和X射线衍射仪(XRD)研究表层组织演变。结果表明:经过SMAT后,w(Si)=3%无取向硅钢表面形成了等轴状、取向呈随机分布的、晶粒尺寸为10 nm的纳米晶组织;异步轧制后,表面纳米晶组织保持不变;550~650℃、4 h渗硅处理后,SMAT+CSR样品表面形成化合物层,其厚度随着温度的升高由17μm增加到52μm;化合物层由Fe3Si和FeSi相组成. Nanostructured surface layer was fabricated on a 3%(mass fraction) non-grain oriented silicon steel by means of surface mechanical attrition treatment(SMAT) and cross-shear rolling(CSR),and then a solid powder siliconizing treatment was carried out for the SMAT+CSR sample at 550~650 ℃ for 4 h.The microstructural evolution was examined by using transmission electron microscopy(TEM),scanning electron microscopy(SEM) and X-ray diffraction(XRD).Experimental results show that: equiaxed nanocrystallin...
预退火温度对高磁感取向硅钢初次再结晶织构的影响
对高磁感取向硅钢冷轧板分别进行800、950、1050和1120℃不脱碳的预退火处理,在800℃预退火,成品的磁性能较好。织构分析的结果表明,随着预退火温度升高,初次再结晶后有利织构组分{111}<112>与不利织构组分(118)[110]的比值f(111)/f(118)逐渐降低,初次再结晶织构的变化是成品磁性的影响因素之一。 Preliminary annealing process at different temperatures for cold-rolled strips of a high permeability grain-oriented silicon steel was investigated to study the effect of the annealing temperature on microstructure and magnetic performance of the steel.Results show that the magnetic performances of the products annealed at 800 ℃ are best.Analysis of primary recrystallization texture indicates that with rising temperature,f(111)/f(118) which is the ratio of the favorable component {111}<112>...
固溶处理对高牌号无取向硅钢磁性能的影响
对商用50W330型无取向硅钢成品在930℃下保温2 h固溶并以不同方式冷却处理,利用磁性检测仪检测分析了处理前后的磁感和铁损变化,应用光学显微镜、扫描电子显微镜、X射线衍射仪观测分析了显微组织结构的演变。考察了平均晶粒尺寸、织构组分比及第二相粒子状态对磁性能的影响规律,结果表明:固溶处理前后平均晶粒尺寸的变化对硅钢磁性能的影响非常显著;当平均晶粒尺寸相差不大时,织构组分比[Goss+{100}]/{111}越大,磁感会越高;固溶处理会将细小弥散的第二相粒子重新回溶到基体中,减小了其对磁畴壁的钉扎作用,铁损随之下降。 The commercial 50W330 non-oriented silicon steel samples were heat treated at 930℃ for 2 h and cooled in different ways,then the iron loss and the magnetic induction of the samples before and after solution treatment were measured with a magnetic detector.The evolution of microstructural texture was analyzed by optical microscopy,scanning electron microscopy and X-ray diffractometry.The effects of average grain size,texture composition ratio and the second phase particles on the magnetic propert...
高牌号无取向电工钢RH深脱硫
以CaO-CaF2复合渣系为脱硫剂,在RH精炼过程采用真空投入法进行高牌号无取向电工钢深脱硫工业试验,采用KTH模型计算分析了RH炉渣成分对硫容量CS的影响。研究结果表明,炉渣成分控制在w((CaO))/w((SiO2))为5~7,w((CaO))/w((Al2O3))为1.5~1.8,w((Al2O3))为25%~30%,w((FeO+MnO))<5%,脱硫剂加入量为6~8kg/t时,钢中硫质量分数从平均0.003 1%降低到0.001 8%,最高脱硫率达到47.1%,平均脱硫率为41.7%。 The industrial trials on deep desulphurization of high grade non-oriented electrical steel were finished through using CaO-CaF2complex based fluxes in RH process.Using the KTH model,the effect of refining slag composition on the sulfide capacities was analyzed.The results show that the chemical composition of refining slag(mass fraction,%)is w((CaO/SiO2))between 5to 7,w((CaO))/w((Al2O3))beween 1.5to 1.8,w((Al2O3)) between 25%to 30%,w((FeO+MnO))less than 5%,and the desulphurizer addition level of...
EB5325涂层液在冷轧无取向电工钢中的应用
介绍了EB5325涂层液的主要性能和中冶新材生产冷轧无取向电工钢所用的涂层设备,通过多次试验摸索出使用EB5325涂层液的工艺,对涂层出现的缺陷进行分析研究,并提出解决方法,使中冶新材生产的冷轧无取向电工钢的涂层质量满足了用户的要求。 This article introduces the main properties of EB5325 and the coating equipments for cold-rolled non-oriented electrical steel. A process using EB5325 coating liquid is made through many time experiments and exploration. The appeared defects in the coating are studied and analyzed,and the solutions are proposed. The coating quality meets clients’ requirements of cold rolled non-oriented electrical steel.
硅钢级氧化镁的研究进展
随着中国电工钢产量的增加,硅钢级氧化镁需求量不断增加,传统的以白云石为原料制备氧化镁的工艺已经无法满足市场需求。中国是一个卤水资源丰富的国家,因此,研究如何资源化综合利用盐湖资源变得越来越重要。硅钢级氧化镁是一种制备取向硅钢的涂层材料,主要用于取向硅钢高温退火处理阶段,起到隔离剂、绝缘膜层、脱硫、脱磷等作用。综述了制备硅钢级氧化镁的方法、工艺流程、研究进展及存在的问题,指出了硅钢级氧化镁制备技术的发展方向,并对中国卤水资源的利用提出了建议。 With the increasing output of electric steel,the demand for silicon steel grade magnesium oxide(MgO) is larger and larger in China,and the traditional MgO production process with dolomite as raw material has been unable to meet market demand.China is a brine resource-rich country,the study of how to comprehensively utilize salt lake resources has become increasingly important.As a coating material used for preparing oriented silicon steel,silicon steel grade MgO is mainly used in the process of ...
ZnO对无铬无取向硅钢绝缘涂层性能的影响研究
主要研究了氧化锌对以Al(H2PO4)3为基料的无铬无取向硅钢绝缘涂层各项性能的影响.用盐雾实验和动电位极化研究了不同氧化锌含量对硅钢绝缘涂层的耐蚀性和电化学行为的影响.采用SEM和体视显微镜对涂层的表面形貌和附着性能进行研究.结果表明,氧化锌含量为4.0%时,氧化锌能完全中和涂层表面的游离磷酸,涂层的耐蚀性和附着性最好;氧化锌含量过少或过多时,涂层的耐蚀性和附着性都较差. This paper studies the influence of zinc oxide on the performance of chromium-free non-oriented silicon steel insulating coating which based on aluminum dihydrogen phosphate.Salt spray experiment and potentiodynamic polarization were used to study the influence of zinc oxide content on the corrosion resistance and electrochemical behavior of the insulation coating of silicon steel.The surface morphology and adhesion of coating were tested by SEM and stereo microscope.The results show that when t...