钢厂
取向硅钢初次再结晶退火工艺正交试验
以试验室模拟CSP工艺生产的Fe-3Si热轧钢带为研究对象,采用正交试验及方差分析的方法,研究了取向硅钢初次再结晶退火工艺对高温退火后获得锋锐的高斯织构的影响。结果表明:取向硅钢两段式初次再结晶脱碳退火工艺参数加热段保温时间及加热温度是高温退火后获得锋锐高斯织构的主要影响因素,其可信度分别在90%和85%以上;在本试验条件下,通过正交试验获得的最佳退火工艺为:冷硬板经600℃保温3 min和850℃保温6 min。 Fe-3Si hot rolled strip was produced by simulating CSP technology in the laboratory.Orthogonal experiment and analysis of variance were carried out to investigate the influence of primary recrystallization on the sharp Goss texture of the oriented silicon steel.The results show that holding time of the heating section and the heating temperature for a sharp Goss texture of the samples annealed has important implications in this experiment conditions,the two-step decarburization annealing process...
冷轧无取向硅钢产品标准浅析
聚焦无取向硅钢产品标准,从电磁性能、表面性能、机械性能以及尺寸公差与边部质量等维度对国际标准IEC、EN、JIS、ASTM以及国标GB进行了分析研究。分析得出,各类标准在电磁性能方面要求基本一致;ASTM标准的机械性能要求有别于其他几个标准。 In this paper,non-oriented silicon steel standards of EN,JIS,GB and ASTM were compared and analyzed. It is showed that,all types of standards in electromagnetic performance requirements are basically the same. Surface properties in ASTM standard are expressed in the most detailed. The mechanical properties requirements of the standards,except for ASTM,are basically the same.
夹杂物尺寸及数量对无取向硅钢磁性能影响的主成分回归分析
采用扫描电镜、场发射扫描电镜、能谱仪等对50SW1300冷轧无取向硅钢中的夹杂物分不同尺寸区间进行数量统计,利用主成分回归分析法,即数据的标准化处理—主成分分析—回归分析—标准化的变量还原成原始变量—确定显著影响因素,综合分析夹杂物总量及各尺寸区间的夹杂物数量对无取向硅钢磁性能的影响。结果表明:主成分回归分析能够从夹杂物尺寸区间及数量的多个影响因素中提取主要的因素,定量研究其对磁性能的影响。分析表明,显著影响无取向硅钢铁损的夹杂物为100~500nm的AlN、AlN+MnS、MnS、Al2O3、AlN+Al2O3,而劣化磁感最明显的夹杂物尺寸区间为100~200nm。 Different size intervals of inclusions in cold rolled non-oriented silicon steel 50SW1300 were counted by scanning electron microscope(SEM),field emission scanning electron microscope(FESEM)and energy disperse spectroscopy(EDS).With principal component regression method:standardization for experimental data,principal component analysis,regression analysis,transform standardized variables into original variables,determination of significant factor,effects of the total number of inclusions and the...
常化和退火工艺对冷轧无取向硅钢高频磁性能和强度的影响
冷轧无取向硅钢(/%:0.003C,2.35Si,0.22Mn,0.011P,0.002S,0.36A1,0.003 0N)经890℃或940℃3 min常化的2.3 mm热轧板冷轧成0.35 mm薄板。研究了常化温度和800920℃3 min退火对该钢高频(400Hz)磁性能和抗拉强度的影响。结果表明,830920℃退火时高频铁损P10/400值最低,随退火温度增加,晶粒尺寸增大,钢的抗拉强度降低;该钢的最佳热处理工艺为常化温度940℃,退火温度830℃,其抗拉强度Rm、高频铁损P10/400和磁感应强度J50分别为565 MPa,21.5 W/kg和1.69 T。 The cold-rolled non-oriented silicon steel(/%:0.003C,2.35Si,0.22Mn,0.011P,0.002S,0.36A1,0.003 0N) is cold-rolled to 0.35 mm sheet from 2.3 mm hot-rolled plate normalized at 890 ℃ or 940℃ for 3 min.The effect of normalizing temperature and annealing process at 800 920 °C for 3 min on high frequency(400 Hz) magnetic properties and tensile strength of the steel has been tested and studied.Results show that with annealing at 830 920 ℃the high frequency iron loss value P10...
硅钢芯片冲裁工艺分析与对策
分析了冲裁硅钢芯片时出现的质量问题,针对影响硅钢芯片冲裁质量的4大因素——人、原材料状态、工艺和工装进行了工艺试验和分析,根据原材料状态的差异,采用不同工艺方案,特别是如何合理选择冲裁模具间隙,解决了硅钢芯片冲裁时产生的主要质量问题,使冲裁的硅钢芯片达到最佳质量状态,并满足硅钢芯片的使用性能。 The problems occurred during silicon steel chip punching and the factors that affect the quality of silicon steel chip punching were analyzed,the factors include 4aspects,that is,people,raw material status,process and frock,at the same time,process tests and analysis aimed at the factors that affect punching quality were did,according to the difference of raw material status,corresponding process schedules wee taken,especially in how to reasonably select punching dies clearance,which solved the ...
高效电机用无取向电工钢组织和析出物研究及产品开发
为开发高效电机用冷轧无取向电工钢,借助实验室薄板坯连铸连轧模拟设备及扫描电镜、透射电镜等检验手段研究了成分、组织、织构和析出物等对无取向电工钢磁性能的影响规律;结果表明:常化处理使组织均匀化并增加有利于磁性提高的织构组分;采用CSP流程开发的高效电机用无取向电工钢铁损平均值3.4 0 W/kg,磁感≥1.68 T。 In order to develop electrical steel for high efficiency motor,effect of components,microstructure,texture and precipitation on magnetic property of electrical steel are analyzed.From the result,normalizing treatment makes microstructure uniform and increases component of favorable texture.Iron loss of electrical steel developed by CSP line is 3.40W/kg and magnetic induction is more than 1.68T.
CSP工艺生产无取向电工钢
介绍了CSP工艺生产无取向电工钢各工序的设备特点、采用的工艺控制手段和电工钢产品质量情况,结合生产实践证明了马钢CSP工艺开发的无取向电工钢产品丰富了薄板坯连铸连轧的品种结构,发挥了薄板坯连铸连轧生产无取向电工钢性能均一、稳定的特点。 The equipment characteristic,the process control method and the quality of non-orientated silicon steel by CSP process were introduced.Combined with the production situation,it is proved that production of non-orientated silicon steel developed on Masteel CSP line would enrich product structure of thin slab continuous casting and rolling,and it exerts stable performance of non-orientated silicon steel.
冷轧无取向硅钢表面麻面缺陷成因分析及其控制措施
针对某厂DMS森吉米尔轧机生产无取向硅钢表面麻面缺陷的问题,根据生产实际,对其形成原因从乳化液及工作辊两方面因素进行了分析。结果表明:乳化液对麻面缺陷的产生有一定影响,但不是主要因素,主要原因是由于二十辊森吉米尔轧机工作辊辊径较小,轧制相同长度带钢轧辊运转周期较大,容易产生疲劳失效而导致。为此,提出通过调整冷轧工序成品轧制道次的压下率以减小轧制力,从而减小工作辊的磨损疲劳;通过对轧制乳化液浓度、温度的合理控制,以改善润滑效果、提高轧制速度,而进一步缓解轧辊疲劳的改进措施,使该钢厂无取向硅钢麻面缺陷发生率由原来的18%降至0.8%,带钢表面质量明显改善。 For the problem of surface pockmarks of non-oriented silicon steel strip produced by a DMS Sendzimir mill, based on the production practice, the formation causes were analyzed from two aspects of emulsion and working roll. The results show that the emulsion has a certain effect on the formation of surface pockmarks defects, but it is not the main factor. The main reason is that the working roll diameter of the 20-high Sendzimir mill is small, and the running period of the roll rolling the same l...
新能源车驱动电机用电工钢用量解析计算及预测方法
对新能源汽车以及驱动电机的现有市场和未来市场规模进行梳理分析,通过自建计算公式推导出我国2021年1-11月份驱动电机用电工钢的总量,进而预测未来10年中国新能源汽车驱动电机用电工钢情况,为无取向电工钢的生产和在电机中的应用提供有价值的参考。 The current market and future market size of new energy vehicles and traction motors were analyzed,and the total amount of electrical steels used in traction motors in China from January to November 2021 was derived by using self-built calculation formulas,and then the situation in the next ten years of electrical steel used in traction motors of new energy vehicles in China was predicted.It will provide a valuable reference for the production of non-grain oriented electrical steel and its appli...
轧制法制备低铁损高磁感6.4%(质量分数)硅钢及其织构演变
采用轧制法制备出具有低铁损高磁感0.23mm厚6.4%(质量分数)Si高硅钢。沿轧制方向的最终磁性能为B8=1.474 T,B50=1.714 T;P10/50=0.30W/kg,P15/50=0.88W/kg。利用X射线衍射及背散射电子衍射(EBSD)技术分析了高硅钢在轧制及退火过程中的织构演变过程。结果表明,通过采用大压下率热轧,确保热轧板次表层中产生更多的高斯织构,随后进行遗传;温轧板中粗大的晶粒有利于冷轧剪切带的形成;冷轧板经脱碳退火后生成强{210}〈001〉织构及次表层较强的高斯织构是在轧向上获得高磁感的原因,归因于其在{111}〈112〉冷轧形变晶粒内的剪切带优先形核并长大;最终退火后虽出现了随机取向,但以{310}〈001〉织构为代表的η织构得以保留并且增强,进一步提高了磁感。随着退火温度的升高及保温时间的延长,高硅钢薄板晶粒尺寸不断增大,铁损明显降低。 6.4wt%Si high silicon steel sheets(0.23mm thick)with low iron loss and high magnetic induction were successfully produced by rolling process.The final magnetic properties along the rolling direction(RD) were:B8=1.474T,B50=1.714T;P10/50=0.30 W/kg,P15/50=0.88 W/kg.The texture evolution during rolling and annealing was investigated by means of X-ray diffraction and electron backscatter diffraction(EBSD).It was found that more Goss textures formed in the subsurface of hot rolled plates by using larg...