钢厂
电工钢反复弯曲试验的影响因素
电工钢反复弯曲次数是电工钢性能检验的重要指标之一,直接影响到用户在使用电工钢过程的机加工性能。主要分析了试样宽度、试样张力、晶粒取向、反复弯曲设备等因素对电工钢反复弯曲试验的影响,并对各个因素的影响程度进行量化以及原因探讨,从而归纳形成各影响因素的基本规律,以便为电工钢实际生产、用户使用提供科学指导。结果表明:试样宽度增加,反复弯曲次数也会不断增加,晶粒位向对取向电工钢的反复弯曲次数影响较大,当支座顶部到拨杆底部的距离减小或拉紧力增加时,反复弯曲次数会不断减小,但当拉紧力达到60N以上时,对反复弯曲次数影响不大,试样经退火后,反复弯曲次数略有上升。 The reverse bend number is an important performance of electrical steels′capabilities,affecting the machining performance directly when the customers used.It investigated some factors,such as sample′s width,sample′s tension load,grain orientation and equipment,how to effect the reverse bend test for electrical steel,measured the influence degree,and discussed the reason,in order to form basic rules which could be guided the manufacturing and using for electrical steel.Results showed that the rev...
融入结构张量和活动轮廓的硅钢表面缺陷分割
为了解决在纹理背景下冷轧硅钢表面缺陷的分割问题,提出了基于局部信息结构张量和活动轮廓模型的硅钢表面缺陷分割方法。将图像的局部信息引入到结构张量中;在结构张量提取的特征空间中,以KL距离作为区域的概率密度相似性度量建立分割图像的活动轮廓模型;采用Split-Bregman数值解法对模型进行求解。运用提出的分割方法对硅钢表面的一些常见缺陷如纵向划伤、横向划伤、异物和孔洞等进行分割实验。实验结果表明,该方法可以准确地分割出硅钢表面缺陷区域,验证了该方法的有效性。 In order to address the segmentation problem for cold rolled silicon steel surface defect based on the texture background,a novel method based on structure tensor and active contour model is proposed.Image local information is introduced to the structure tensor.In the extracted feature space of structure tensor,KL distance is treated as a regional similarity measure of the probability density to establish active contour model for image segmentation.The numerical solution of Split-Bregman is used...
高温硅钢加热炉双蓄热燃烧技术的探讨
介绍了双蓄热燃烧技术的特点和高温硅钢加热炉的特点,探讨了双蓄热燃烧技术在高温硅钢加热炉中使用的技术难点,分析了双蓄热燃烧技术在高温硅钢加热炉上使用的可能性。 Introduced characteristics of double regenerative combustion technology and high temperature silicon steel reheating furnace,discussed technical difficulties for using double regenerative combustion technology,analyzed the possibility of double regenerative combustion technology applied to high temperature silicon steel reheating furnace.
常化温度对含1.5%Si无取向电工钢磁性能的影响
研究了CSP工艺流程生产的硅含量为1.5%的无取向电工钢在不同常化温度下对磁性能的变化。研究结果表明:随着常化温度的提高,热轧板的晶粒尺寸增大,且组织均匀性提高;此外成品的有利织构组分{100}<0vw>、α、η增强,不利织构组分减弱;铁损P1.5/50呈下降趋势,磁感B50上升平缓。在常化工艺为970℃×2.5min下,对应的铁损P1.5/50<3.4W/kg,磁感B50>1.74T。 The effect of normalizing temperature on the magnetic properties of non-oriented electrical steel containing 1.5%silicon produced by CSP process was studied.The results show that with increasing normalizing temperature,the average grain size of hot-rolled plate increases and the microstructure uniformity is improved.Furthermore,the texture components of finished products are improved through enhancing of{100}<0vw>,αandηtextures and weakening of{111}<112>texture;the core loss P1.5/50 ...
取向硅钢初次再结晶退火工艺正交试验
以试验室模拟CSP工艺生产的Fe-3Si热轧钢带为研究对象,采用正交试验及方差分析的方法,研究了取向硅钢初次再结晶退火工艺对高温退火后获得锋锐的高斯织构的影响。结果表明:取向硅钢两段式初次再结晶脱碳退火工艺参数加热段保温时间及加热温度是高温退火后获得锋锐高斯织构的主要影响因素,其可信度分别在90%和85%以上;在本试验条件下,通过正交试验获得的最佳退火工艺为:冷硬板经600℃保温3 min和850℃保温6 min。 Fe-3Si hot rolled strip was produced by simulating CSP technology in the laboratory.Orthogonal experiment and analysis of variance were carried out to investigate the influence of primary recrystallization on the sharp Goss texture of the oriented silicon steel.The results show that holding time of the heating section and the heating temperature for a sharp Goss texture of the samples annealed has important implications in this experiment conditions,the two-step decarburization annealing process...
电力变压器用高磁感取向硅钢的发展及应用
阐述了国内外高磁感取向硅钢的生产研究水平与发展趋势,包括通过提高高斯晶粒取向度、细化磁畴、涂覆张力涂层、减薄钢片厚度进一步降低铁损以及低温加热技术和短流程技术新工艺。分析高磁感取向硅钢在我国大型电力变压器上的应用情况,结果表明,发展更薄规格高磁感、低铁损、低磁致伸缩取向硅钢可为大型变压器的安全性、节能性及环保性提供有效保障。 The research progress and development trend of high magnetic induction grain-oriented silicon steel at home and abroad are summarized,including the technology of improving the Goss alignment,refining domain wall,adding stress coating,decreasing thickness of sheet,and the new technique of reducing heating temperature of casting slab and shortening operational.Moreover,the application of high magnetic induction grain-oriented silicon in power transformer is presented.Developing grain-oriented sili...
高牌号无取向硅钢CSP流程铸坯及热轧板的组织和夹杂物分析
2.9 mm热轧3%Si高牌号无取向硅钢板(/%:0.004 6C、3.04Si、0.32Mn、0.49Als、0.004S、0.013P、0.0042N)由CSP(Compact Strip Production紧凑式带材生产线)流程:120 t BOF-70 mm CC-热轧工艺生产。热轧终轧温度872℃,卷取温度683℃。铸坯及热轧板的组织和夹杂物的分析结果表明,铸坯组织为典型的贯穿柱状晶组织;热轧板边部为再结晶组织,中部为纤维组织带有少量再结晶晶粒;高牌号无取向硅钢的主要夹杂物为铸坯-Al2O3,AlN和Cu2S+MnS;热轧板-Al2O3,AlN,AIN+MnS和Cu2S+MnS。 The 2.9 mm hot rolled 3%Si high grade non-oriented silicon steel plate(/%:0.004 6C,3.04Si, 0.32Mn,0.49Als,0.004S,0.013P,0.004 2N) is produced by CSP(Compact Strip Production) flow sheet i.e.120 t BOF-70 mm CC-hot rolling process with end rolling at 872℃and coiling at 683℃.The analysis results on structure and inclusions in casting slab and hot rolled plate show that the structure of slab is typical trans-columnar crystal,the structure of hot rolled plate at edge is recrystallized grain and in ce...
电感耦合等离子体质谱法测定硅钢中痕量铜和镍
研究了应用电感耦合等离子体质谱法(ICP-MS)测定硅钢中痕量铜和镍的分析方法。采用硝酸分解样品,通过内标校正和基体匹配消除了基体干扰的影响,同时根据测量时存在的质谱干扰情况,选择同位素65Cu和60Ni作为测定元素和通过调节仪器参数使双电荷离子的产率最低,以减少带来的干扰。该方法用于硅钢中痕量铜和镍的测定,所得的结果与ICP-AES法测定结果完全吻合,各元素测定结果的RSD值小于5%,加标回收率为97.3%~100.3%。 A method for the determination trace copper and nickel in silicon steel by inductively coupled plasma mass spectrometry(ICP-MS) was studied.The samples were dissolved in HNO3.The effect of matrix interference was eliminated by internal standard correction and matrix matching.Meanwhile,according to the mass spectral interferences in determination,the isotopes including 65Cu and 60Ni were used as measuring elements.The yield of double-charge ions were minimized by adjusting instrumental parameters...
冷轧电工钢森吉米尔轧机研究进展
森吉米尔二十辊轧机是冷轧电工钢的主要机型,具有整体刚度大,辊径小,轧制道次压下量大,产品精度高等特点,简要介绍了近年来冷轧电工钢森吉米尔二十辊轧机领域进展,在轧机结构、厚度自动控制、板形自动控制等方面的技术及研究。 20-h Sendzmir reversible mill is the main type of cold rolled electrical steel which has the characteristic of high integral stiffness,small roller diameter,high pass reduction and high product quality.In this paper,the recent progress of frame structure,automatic gauge control,automatic flatness control of Sendzmir mill is introduced.
免常化处理的耐酸蚀无取向电工钢的研制
在现普通冷轧无取向硅钢的基础上,降低Si含量,复合添加少量辅助元素,组合热轧板处理和成品退火加热技术,研制出了免常化处理的高磁感、低铁损并具有良好耐酸腐蚀性能的新系列无取向电工钢。 Based on existing common cold rolled non-oriented silicon steel,a new series of non-orientedelectrical steel with high induction,low core loss and excellent anti-corrosion property has been developed by reducing Si element,adding complexly a small amount of supplementary elements,and employing combined treatment of hot rolled sheet and finished product annealed heated technology.
国内外中低牌号无取向硅钢夹杂物控制效果解析
选用国内外无取向硅钢标杆企业A、B、C的产品,采用非水溶液电解提取+SEM(EDS)方法,分析了其典型牌号对应成品试样中的夹杂物。结果表明,从磁性能控制角度而言,受钢的化学成分及生产工艺影响,A、B、C企业成品试样的夹杂物尺寸、种类、数量存在差异,这些差异对其磁性能产生显著影响;从夹杂物控制角度而言,A、B、C企业对应成品试样的夹杂物,以MnS、CuxS复合或者AlN、MnS、CuxS复合为主,其中1.0μm以下的夹杂物数量分别为2.34×107个/mm3、2.98×107个/mm3和11.98×107个/mm3,1.0μm以上夹杂物数量均很少,夹杂物的平均尺寸从大到小依次为A企业、B企业、C企业。 According to the production of three benchmarking manufacture enterprises A,B and C of non-oriented silicon steel at home and abroad,the inclusions in finished steel samples with typical grades were investigated by electrolytic extraction from non-aqueous solution and SEM(EDS).Results show that,from the viewpoint of improving the magnetic properties,affected by chemical composition and production technique,the size,type and amount of inclusions in finished steel samples are various,which will af...