无氧化炉具有加热效率高、投资与运营成本低、作业率高、表面质量及板型良好、NOx排放相对低等优势,在硅钢热处理领域应用前景广泛。本文阐述了确定无氧化炉(NOF)加热能力详细过程,涵盖炉温、炉断面尺寸、炉长、热平衡结算、加热能力计算等,为今后无氧化炉(NOF)在硅钢热处理应用时的设计提供了借鉴,同时也为今后明火直接加热的工业炉设计提供了参考。 Non-oxidation furnace has the advantage s of high heating efficiency, low investment and operation cost, high operation rate, good surface quality and plate shape, and relatively low NOxemission,and it still has wide application prospect in the field of silicon steel heat treatment. The detailed process of determining the heating capacity of a non-oxidizing furnace(NOF) is described, covering furnace temperature, furnace section size, furnace length, heat balance settlement, heating capacity cal... 
2022-01-28 200 5.8

测试了高强无取向电工钢的S-N曲线,并借助光学显微镜、扫描电子显微镜、透射电子显微镜分析了实验钢组织,疲劳断口形貌和位错结构。结果表明:室温条件下,频率为20Hz,应力比R为0.1,循环10~7周次时,实验钢的疲劳强度为360MPa,疲劳裂纹萌生于实验钢的次表面,裂纹萌生点附近有沿晶开裂现象,疲劳裂纹扩展区域有解理台阶与疲劳条纹,瞬间断裂区是韧性断裂,有大量韧窝。实验钢在循环应力作用下基体中产生了大量位错,并有驻留滑移带终止在晶界位置。 The S-N curve of a high strength non-oriented electrical steel was tested.The microstructure and fatigue fracture morphology and dislocation were analyzed by optical microscope,scanning electron microscope,transmission electron microscope.The results showed that:at room temperature and the frequency of 20 Hz and the stress ratio Rof 0.1,the fatigue strength of the experimental steel was 360 MPa when the cycle was 10~7 cycles.The fatigue crack initiation at the surface of the steel and the interg... 
2022-01-28 187 5.8

【作者】 王桦; 舒子龙; ...
2013-01-28 132 5.8

【作者】 严伟明; ...
2013-09-28 155 5.8

在现普通冷轧无取向硅钢的基础上,降低Si含量,复合添加少量辅助元素,组合热轧板处理和成品退火加热技术,研制出了免常化处理的高磁感、低铁损并具有良好耐酸腐蚀性能的新系列无取向电工钢。 Based on existing common cold rolled non-oriented silicon steel,a new series of non-orientedelectrical steel with high induction,low core loss and excellent anti-corrosion property has been developed by reducing Si element,adding complexly a small amount of supplementary elements,and employing combined treatment of hot rolled sheet and finished product annealed heated technology. 
2013-02-28 163 5.8

【作者】 姚昌国; ...
2011-05-28 182 5.8

通过微观组织表征、高温拉伸和断口形貌分析,研究了钇(Y)元素对6.5%Si无取向硅钢组织、高温拉伸及断裂机制的影响。研究结果表明,添加Y元素可以在钢液中形成YS和YP的复合析出。YS和YP可以充当异质形核基底,提高形核率,细化凝固组织。热轧组织不均匀,由表层至芯部分别形成等轴晶、等轴晶/拉长晶和拉长晶的混合组织。退火后,热轧变形组织转变为等轴晶,含Y实验钢的退火组织得到明显细化。500℃时效处理后,含Y实验钢具备较低的有序度,300℃的拉伸断口呈现韧性断裂特征,断后伸长率达到20.2%。相反,无Y实验钢发生脆性断裂,断后伸长率仅为2.1%。研究结果证实,Y元素可以通过组织细化和降低有序度提高6.5%Si无取向硅钢的中温塑性。 The effects of yttrium(Y)on microstructure,elevated-temperature tensile properties and fracture mechanism of 6.5% Si non-oriented electrical steel were investigated by means of microstructure characterization,high-temperature tensile test and fracture analysis.The results showed that the doping of Y introduced composite Y-rich precipitates(YS/YP)in the melt.YS and YP precipitates were qualified for heterogeneous nucleation agents,which thus raised the nucleation rate and refined the solidificati... 
2022-01-28 209 5.8

结合实际生产0.4%Si无取向硅钢,统计了不含Sn和0.025%Sn无取向硅钢的磁性能变化,利用金相显微镜、X射线衍射仪观察分析不同成分下试样的显微组织和微观织构。试验结果表明:Sn元素可以显著降低无取向硅钢的晶粒尺寸,0.025%Sn试样的平均晶粒尺寸比不含Sn减小28.4%;加入Sn元素后抑制了无取向硅钢中不利于磁性能的{111}面织构组分强度,提高了对磁性能有利的{100}面织构组分强度,0.025%Sn与不含Sn相比磁感均值从1.756 T提升至1.768 T,铁损均值从5.476 W/kg降低至5.204 W/kg,明显改善了无取向硅钢磁性能。 In this paper combined with the actual production of 0.4% Si non oriented silicon steel, the magnetic properties of non oriented silicon steel without Sn and 0.025% Sn were counted. The microstructure and microtexture of samples with different compositions were observed and analyzed by metallographic microscope and X-ray diffraction. The results show that: Sn can significantly reduce the grain size of non oriented silicon steel, and the average grain size of 0.025% Sn sample is 28.4% smaller tha... 
2022-01-28 188 5.8

研究了无取向硅钢钙处理前后夹杂物的行为,重点考察了钙处理前后夹杂物的成分、类型、形貌和尺寸研究的变化情况,为实际生产中无取向硅钢的钙处理提供理论指导。试验发现:钙处理前夹杂物主要以Al2O3、Al2O3-MgO为主,且在夹杂物表面有AlN析出,钙处理后夹杂物以Al2O3-MgO-CaS-CaO系复合夹杂物为主,还含有少量的SiO2或AlN;钙处理前后,夹杂物形貌由多边形或不规则形逐渐向球形或近似球形转变,并且夹杂物尺寸不断增大;钙处理前后,含钙夹杂物的比例发生突变,由10%增大到74.5%,且随着钙处理时间的延长,含钙夹杂物比例下降,表明钙处理使夹杂物变性后易聚集长大并上浮去除。 Behavior of inclusions before and after calcium treatment in non-oriented silicon steel was researched by investigating changes of compositions,types,shapes and sizes of inclusions before and after calcium treatment,for the purpose of providing theoretical guidance for calcium treatment of non-oriented silicon steel in actual situation. Results indicated that Al2O3 and Al2O3-MgO were main types of inclusions before calcium treatment,sometimes AlN maybe precipitate in the outer of inclusions. Al2... 