钢厂
化学气相沉积法制备6.5%Si高硅钢的研究
采用化学气相沉积(CVD)渗硅处理工艺连续制备6.5%Si高硅钢,具有优质的软磁性能,通过理论研究化学反应并且用简单的试验设备做进一步的探讨。根据试验的结果对连续制备6.5%Si高硅钢的CVD工艺构造提出全面、有效的建议,实现制备6.5%Si高硅钢系统。 CVD method for continuously manufacturing 6.5%Si Steel Sheet has excellent soft magnetic.Carried out a theoretical study of related chemical reaction and performing basic research with a simple test apparatus.Based on the results,finally proposed an overall process configuration to realize such a production-CVD method for continuously manufacturing 6.5%Si Steel Sheet.
酸溶铝对铸态取向硅钢中第二相粒子组成和形貌的影响
试验的铸态取向硅钢(/%:0.0440.056C,3.123.32Si,0.080.11Mn,0.0020.008S,0.002 90.029 1Als,0.006 20.010 9N)由30 kg高频真空感应炉熔炼。通过场发射扫描电子显微镜/能谱仪(FE-SEM/EDS)研究结果表明,0.002 9%Als钢中氧化物主要为SiO2,存在片状、棒状及近似球状的独立MnS,未发现含铝的氧化物或氮化物;0.0090%Als钢中出现以Al2O3为主的复合氧化夹杂物,存在MnS与AlN的复合析出物。钢中Als增加,复合析出物多呈簇状发展。氧化物容易成为MnS-AlN复合析出的核心,钢中Als含量越低,夹杂物中的MnS含量越高;作为核心的氧化物夹杂的尺寸越小,形成的复合夹杂物的形状越规则,尺寸也越小。热力学计算结果表明,钢中Als含量主要影响了钢中氧化物夹杂的组成和AlN的析出温度及析出量。 Test as-cast grain-oriented silicon steel(/%:0.044 0.056C,3.12 3.32Si,0.08 0.11Mn,0.0020.008S,0.002 90.029 1 Als,0.006 20.010 9N) is melted by a 30 kg high frequency vacuum induction furnace.The research results by using field emission-scanning electron microscope/energy dispersive spectrometer(FE-SEM/EDS) show that in 0.002 9%Als steel the main oxide is SiO2,and there is independent laminable,rod-like and approximate ...
普通冷轧取向硅钢中间完全脱碳退火工艺的确定
为了确定普通冷轧取向硅钢最优的中间完全脱碳退火工艺,在其一次冷轧后进行5种不同工艺的脱碳退火处理,借助扫描电镜及电子背散射衍射技术研究了不同工艺脱碳退火后的组织、织构和脱碳效果。结果表明:经5种工艺脱碳退火处理后,初次再结晶的平均晶粒尺寸均约为19μm,且不随退火温度和时间的变化而变化;经840℃×10min工艺退火后的晶粒最均匀,高斯织构位向更准确,高斯织构面积分数最多,为3.1%,可将碳脱至0.003 5%。 In order to determine the optimal intermediate complete decarburizing annealing processes for common grain-oriented(CGO)silicon steel,five kinds of intermediate decarburizing annealing processes were conducted,the microstructure,texture and decarbonization after different decarburizing annealing processes were studied by scanning electron microscopy and electro back-scattered diffraction(EBSD)technology.The results show that the average grains sizes of primary recrystallization were about 19μm a...
锰含量对无取向电工钢组织性能的影响
研究了锰含量对w(Si)=1.8%Si无取向电工钢组织和性能的影响。结果表明,钢中锰含量从0.3%增加到1.2%时,由于α_γ相变的产生,铸坯低倍组织、热轧板金相组织及成品织构等均发生了不同程度的变化,对成品表面质量及磁性能产生了明显的影响。 The effects of manganese content on structure and properties of w(Si)=1.8% non-oriented electrical steels have been studied.Results show that with increasing manganese content to 1.2% from 0.3%,macrostructure of continuous casting slab,hot rolled band metallurgical structure and finished product texture vary in some extent because of the occurrence of α-γ phase transformation,the surface quality and magnetic properties of finished product are affected greatly.
无取向硅钢表面环保涂层的发展
简述了无取向硅钢环保涂层发展背景,分析了硅钢环保涂层的特点及国内、外研究进展,提出了硅钢保涂层下一步的发展方向。 The back ground of environmental protection coating of non-oriented silicon steel was described in this paper.The characteristics and study progress in domestic and foreign of environmental protection coating of non-oriented silicon steel were analysised.The next development direction of environmental protection coating of non-oriented silicon steel was put forward.
含铜无取向电工钢中析出相及其析出机理
研究了含铜低碳低硅无取向电工钢中的析出相及其析出机理.由能谱(EDS)及选区电子衍射(SAED)分析可知,铁素体基体上存在的大量弥散分布的等轴状析出相为类B2结构的铜.这些铜析出相的析出机理可以是一般析出、位错析出、台阶机理相间析出和弓出机理相间析出:一般析出在550、650和750℃三个等温温度均可发生;位错析出只发生在较低的等温温度(550℃),此时析出相呈特殊的平行短列状;台阶机理相间析出也可在上述三个等温温度下发生,但650℃等温时最有利于台阶机理相间析出,此时析出相平直列状分布;弓出机理相间析出只发生在较高的等温温度(750℃),析出相弯曲列状分布. Precipitates in low-carbon low-silicon non-oriented electrical steel containing Cu were studied and the precipitation mechanism was analyzed by means of energy dispersive spectrometry(EDS) and selected area electron diffraction(SAED).It is found that the equiaxed precipitates of Cu with B2-like structure distribute dispersively in the non-oriented electrical steel.The precipitation mechanism involves general precipitation,dislocation precipitation,interphase precipitations formed by the ledge me...
无取向硅钢铬酸镁绝缘涂层高温固化工艺
为了确保硅钢铬酸盐涂料的环保性,需要严格控制涂料的固化工艺,保证涂料固化过程中涂料中的六价铬充分转化为三价铬。对涂料及原料进行热重分析(TG)及差示扫描量热法分析(DSC)。结果表明,MgO与铬酐混合转化为MgCrO4,使六价铬稳定性增强,其中大部分Cr6+转变为Cr3+发生在620~700℃,在450~500℃高于铬酐发生大量失重,因此必须加入还原剂保证涂料中六价铬被充分还原;超过360℃后树脂会发生分解,因此实际板温不能超过360℃;加入了还原剂的整体涂料的失重温度区间主要在260~320℃,因此涂料固化时钢板的实际温度最佳区间为320~360℃。 Because of the silicon steel chromate coating’s environmental requirements,the paint curing process must be controlled strictly to ensure all Cr( Ⅵ) transforms to Cr( Ⅲ). The TG and DSC analyses of the paint are studied. The reaction of MgO and CrO3 would generate MgCrO4,enhancing the stability of Cr( Ⅵ). The most r( Ⅵ) in MgCrO4 changes to Cr( Ⅲ) at 620-700 ℃,while the CrO3 has a large weight loss at 450-500 ℃. The reductant must be added in the paint to make sure the Cr( Ⅵ) could transform suf...
多元抑制剂对高磁感取向硅钢性能的影响
介绍在取向硅钢生产中抑制剂的作用以及多元抑制剂的机理和应用情况,分析多元抑制剂方案中各种元素对高磁感取向硅钢性能的影响,并根据生产实践提出了进一步研究的方向. The role of an inhibitor in the production of grain oriented silicon steel,and the mechanism of multiplex inhibitor in the production are described in the present article.In addition,the influence of various elements in the multiplex inhibitor on the performance of grain oriented silicon steel with high magnetic induction is elucidated.Further work needed in this research is also indicated.
压下率对取向硅钢热轧板织构的影响
采用X-射线衍射分析技术测定了取向硅钢热轧板在不同压下率下不同厚度处的织构。结果表明,在压下率低于80%的情况下,几乎所有试样的不同厚度处的织构均为旋转立方织构类型{100}<011>,但不同压下率、不同厚度处的织构强度存在很大差异;在压下率大于80%的情况下,不同试样的不同厚度处的织构类型发生了变化,其织构类型为旋转立方织构或高斯织构{011}<100>,且当织构类型为旋转立方织构时,织构强度存在很大差异,而当织构类型为高斯织构时,织构强度差异相对较小。 The texture of the grain oriented silicon steel hot rolled plate at different compressibility has been measured.The experimental results have shown that the texture of all samples at different thickness is {100}<011> when the compressibility is below 80%,and its intensity at different compressibility and thickness is difference.The texture of all samples at different thickness is variable when the compressibility is above 80%,it is {100}<011> or {011}<100>,and the intensity of ...
辉光放电发射光谱法测定硅钢薄板中微量硼元素
通过对辉光放电发射光谱参数的优化,以铁元素为内标来消除基体效应,建立了测定硅钢薄板中微量硼元素的方法。优化的实验参数为:放电电压1200 V,放电电流50 mA,预溅射时间40 s,积分时间10 s。校准曲线硼元素含量范围0.0001%~0.022%,相关系数大于0.999,测量结果与认定值一致,相对标准偏差小于10%。完全能够满足日常分析测试的要求。 A glow discharge optical emission spectrometry(GD-OES) method for determining trace boron element in silicon steel sheets were established through optimization of instrumental parameters and using Fe element as an internal standard to eliminate the matrix effect.The optimized instrumental parameters included discharge voltage,discharge current,pre-sputtering time and integration time,which are 1200 V,50 mA,40 s,and 10 s,respectively.The content of boron element that can be determined from the ca...