无取向硅钢夹杂物分析
采用非水溶液电解方法来提取无取向硅钢中夹杂物。通过扫描电镜(SEM)观察结果表明:无取向硅钢中主要夹杂物为六棱柱的AlN、不规则硅酸盐及球状的铁的硫化物和氧化物,其中AlN夹杂尺寸在1~5μm,数量较多,还有部分AlN的复合夹杂。进一步研究了AlN复合夹杂形成机理,采用了Thermo-Calc热力学计算软件计算出该钢样中AlN、MnS析出温度分别为1 240℃、1 200℃,而Al2O3析出温度大于1 800℃,从而为AlN复合夹杂形成机理提供了一个理论依据。 Extracting inclusions from non-oriented silicon steel in non-aqueous electrolysis is a nondestructive method to gain inclusions.Scanning electron microscopy shows that the main inclusions in non-oriented silicon steel were hexagonal AlN,which was of large quantity,irregular silicate,spherical iron sulfide and oxide.The size of AlN inclusions ranged from 1to 5μm,and there were some duplex inclusions of AlN.To further study the formation mechanism of AlN duplex inclusions,Thermo-Calc thermodynamic...
D21硅钢芯片冲压工艺分析及模具设计
变压器D21硅钢铁芯片采用冲压工艺生产。首先对其工艺进行了分析,确定了冲压方案。对产品进行了排样设计,计算了冲压力,确定了压力中心。然后,设计了单工序落料模具,完成了模具装配图。 D21 silicon steel chips for transformer are produced by stamping.First,its stamping process was analyzed and the scheme of the stamping process was determined.The product layout was designed,the punching pressure was calculated,the pressure center was determined.Then,the blanking die with single procedure was designed,the die assembly drawing was completed.
云边一体化系统架构下硅钢制造管理业务数字化融合应用
提出以“云边一体化架构”构建硅钢智慧决策系统,来解决原硅钢制造L1~L5系统架构模式下的数字信息孤岛、业务功能割裂等问题。在此基础上,开发了云边协同的自学习型控制模型及业务决策模型,构建起硅钢“智慧大脑”,形成了以研发、制造、服务等核心业务数字化融合的智能化决策支持新模式,探索出一条钢铁制造业数字化、智能化转型之路。 SIDS(Silicon-steel Intelligent Decision-making System)based on \"cloud-edge integration architecture\" was proposed to solve the problems of data silos and business function fragmentation in the original L1~L5 system architecture.On this basis,the self-learning control model and decision-making model of cloud-edge collaboration were developed,the \"smart brain\" of silicon steel department was constructed,and a new intelligent decision-making support model of digital integration of core businesses s...
高温卷取的热轧态原料与常化态原料生产高牌号无取向硅钢的比较
研究了采用高温卷取热轧态原料和常化态原料生产高牌号冷轧无取向电工钢组织、织构和磁性能。研究发现钢卷采用750℃高温卷取,下线后立即采用\"保温罩\"对钢卷进行保温,时间96h,然后空冷至100℃时上线生产的工艺可取代常化工艺生产高牌号冷轧无取向电工钢。冷轧上线前,热轧态原料的表层为大量的再结晶组织,这部分组织包括了热轧轧制时保留下来的动态再结晶组织,钢卷本身高温回复后产生再结晶晶粒,以及在保温罩内保温时形成的再结晶组织。高温卷取的热轧态和常化态的热轧卷作为原料时,试样织构类型相似,取向分布密度接近,再结晶后织构类型仍然相似,取向分布密度仍然接近。Goss织构对磁性能增加有促进作用。实验钢中较好的磁性能对应的织构[{100}+Goss]/{111}的比值较高,体现了织构的遗传性。 Microstructure,texture and magnetic properties of high grade cold rolled nonoriented electrical steel which made of hot rolled material with high temperature coiling and with normalization were studied.Steels coiled in high temperature(at 750 ℃),stacked with insulation cover for 96hand air cooled to 100 ℃ were using to manufacture high grade nonoriented electrical steel.The process can replace the normalization process.There are a lot of recrystallized grains in the surface layer of the coil wit...
CSP流程试制50W270高牌号无取向硅钢织构的演变
研究了CSP流程试制50W270高牌号无取向硅钢热轧→常化→冷轧→退火过程中织构的演变.利用电子背散射衍射技术对全流程织构进行测量和分析.发现热轧板织构在厚度方向上存在较大差异,表层主要为铜型、黄铜和高斯织构,1/4层存在微弱的高斯织构和旋转立方织构,中心层以γ纤维织构和旋转立方织构为主,还含有较弱的α纤维织构.与热轧板相比,常化板表层和1/4层织构变化不大,中心层旋转立方织构和α纤维织构增强.冷轧板各层均具有α纤维织构和γ纤维织构.与冷轧板相比,成品板各层中α纤维织构基本消失,还出现了立方织构和高斯织构. This article focuses on texture evolution in 50W270 high-brand non-oriented silicon steel produced by CSP in hot rolling,normalizing,cold rolling,and annealing processes.The texture in the whole process was measured and analyzed by electron back-scatter diffraction.It is found that the texture along the thickness direction in hot-rolled strips changes obviously;there are mainly copper,brass,and Goss textures in the surface layer;the 1/4 layer has weak Goss texture and rotating cube texture;γ-fib...
硅钢高温退火环形炉炉壳制作与安装技术
硅钢高温退火环形炉炉壳制作与安装精度要求较高,施工时通过对壳体原材料矫正、炉壳板拼焊、下料切割、型钢骨架组装及焊接、骨架及炉壳板矫正、骨架与炉壳板组装及焊接、炉壳矫正、零配件装置、定位钻孔、报验检查、出厂、内侧板安装、外侧板安装、顶板安装等环节的工艺技术控制,能保质高效地完成硅钢高温退火环形炉炉壳制作与安装,为以后同类工程的施工提供可借鉴经验。 The required precision of manufacture and installation technique of the silicon steel high temperature annealing annular-furnace shell is high.During construction , manufacture and installation of the silicon steel high temperature annealing annular-furnace shell could be finished high efficiently through correcting the raw materials of shell , furnace shell plate welding , material cutting , steel frame assembly and welding , skeleton and shell plate correction , skeleton and furnace shell asse...
高强度无取向电工钢的研究进展
针对宝钢集团、日本新日铁住金和JFE公司公开的相关专利等资料,总结了国内外高强度无取向电工钢的研究进展,分析了不同电工钢的化学成分、生产工艺及产品性能,指出固溶强化、细晶强化、析出强化、位错强化都有可能被用来提高无取向电工钢的强度,并阐述了四种强化方式的优缺点;指出在高强度无取向电工钢的研发过程中,需根据其具体用途确定目标性能,再采用合适的强化手段,最终实现力学性能、磁性能和生产性能之间的平衡。 The research progress of high strength non-oriented electrical steels at home and abroad is summarized according to related patents brought into the public by Baosteel,Nippon Steel & Sumitomo Metal corporation and JFE corporation.The characteristics of chemical composition,production technology and properties of products in the patents are analyzed.Each of solution strengthening method,fine-grain strengthening method, precipitation strengthening method or dislocations strengthening method ma...
火花源原子发射光谱法在线测定电工钢中的超低碳
采用火花源原子发射光谱分析测定电工钢中超低C,研究试样制备方法、Ar纯度和压力等条件对分析结果的影响,并对工作曲线进行了优化,实现了一次分析同时测定电工钢的多种元素,满足炉前和精炼在线分析的要求。 Ultra-low carbon in electrical steel is determined with spark-source atom emission spectrum.It is researched the influence of sample making method,purity of Ar,and pressure on analysis result.The work curve is optimized.The determination of many elements in electrical steel only in one analysis is realized.It meets demands of on-line analysis for blast furnace and refining.
ICP-AES法测定硅钢中铌的不确定度评定
分析了电感耦合等离子体发射光谱法(ICP-AES)测定硅钢中铌的检测过程,讨论了该检测过程中不确定度的主要来源,建立了该方法的定量的数学模型,并根据这一模型计算出了检测结果的合成标准不确定度和扩展不确定度。 The measurement of niobium content in silicon steel by inductively coupled plasma atomic emission spectrometry(ICP-AES) was analyzed,by which the main factors affecting the uncertainty of the measurement were ascertained and the calculation formula was given.Finally,according to the formula the combined uncertainty and expanded uncertainty were obtained.
锡或锑在无取向电工钢中的研究进展
近年来,在节能减排背景之下,国内外众多研究者对无取向电工钢磁性能的提升做了大量研究。为了探索无取向电工钢磁性能提升的方法,对锡或锑对无取向电工钢磁性能的作用机制(晶粒尺寸和晶体织构的控制)进行分析。基于该作用机制,介绍锡或锑的添加对无取向电工钢磁性能的影响。经研究发现,适量的锡或锑在晶界偏聚,不会阻碍晶界的移动并且致使晶粒尺寸降低;与此同时,锡或锑在晶界偏聚不仅抑制{111}织构在原始晶界处形核及生长,还降低(100)晶粒表面能,促进(100)晶粒生长。因此,适量添加锡或锑,可使无取向电工钢铁损下降、磁感提升。最后结合生产工艺,建议无取向电工钢的研究方向应为稀土含量对高牌号无取向硅钢夹杂物尺寸和数量分布的影响,锡或锑的添加量和常化工艺参数(常化时间、常化温度)对常化晶粒尺寸的影响。 In recent years, due to the background of energy saving and emission reduction, numerous researchers all around the world have done a lot of investigations on the improvement of magnetic properties for non-oriented electrical steel. In order to explore the method of improving the magnetic properties of non-oriented electrical steel, the mechanism of tin or antimony on the magnetic properties(the control of grain size and crystallographic texture) of non-oriented electrical steel is illuminated. ...