钢厂
奥氏体化温度对高碳含硅钢等温转变的影响
采用XRD物相分析、金相组织观察及TEM精细组织分析研究了奥氏体组织结构状态对Fe-0.88C-1.35Si-1.03Cr-0.43Mn钢中温等温相变鼻温和孕育期的影响,以及不同温度奥氏体化后240℃等温20 min试样的组织结构特征。试验发现,随着奥氏体化温度的升高,中温等温开始转变的鼻温移向更低温度并且相变孕育期缩短;不同温度奥氏体化后同为240℃等温20 min处理,虽然均形成由贝氏体铁素体亚条平行排列构成的束状贝氏体组织,但贝氏体组织的精细结构状态不同,突出的差别在于对应低温奥氏体化贝氏体亚条端部边界具有凸起结构,而对应高温奥氏体化贝氏体亚条端部边界较为平齐且呈现楔形结构。不能简单地以马氏体切变机制认识试验钢中贝氏体组织的形成。 The influence of austenitization temperature on the incubation period and the bainitic phase transformation behaviour in high-carbon silicon steel has been investigated using X-ray diffraction(XRD), optical microscopy and transmission electron microscopy(TEM). The microstructure characteristics of the isothermal transformation(240 ℃, 20 min)products were also studied. It was found that the nose temperature of bainite transformation and incubation period decreased with the increasing austenitizin...
热轧卷取时间对新型冷轧无取向电工钢组织和性能的影响
研究了热轧卷取时间对无取向电工钢晶粒组织、织构演变、铁损和磁感的影响。结果表明,成品晶粒尺寸在120~140μm之间,随卷取时间的增加,成品晶粒尺寸增大。成品织构主要由γ纤维、а纤维和高斯织构等构成。随着保温时间的增加,{111}<110>和{112}<110>织构强度降低。随卷取时间的增加,成品P1.5降低。热轧板最佳的卷取工艺为550℃保温2~3 h,电工钢的综合磁性能优良。 The effects of hot-rolling coiling time on microstructure,texture,core loss and magnetic induction of a new cold-rolled non-oriented electrical steel containing copper were investigated.The test results showed that for final product the grain sizes are 120-140um,with the increase of coiling time,the grain size increase.For final product there are mainly γ-fibre,а-fibre,and {110}<001> texture,Coiling at 550℃ for hot rolled plate,the {111}<110>,{112}<110> texture was weaked with ...
冷轧无取向硅钢横向厚差控制
冷轧中中低牌号的无取向硅钢多采用万能凸度轧机(Universal crown mill,UCM)生产,其板形好坏受制于UCM轧机板形调节手段的协调使用。为掌握UCM轧机的板形控制特点,建立基于二维变厚度有限元的辊系弹性变形和基于三维差分的轧件塑性变形的六辊轧机耦合模型,对UCM轧机的板形调控性能进行详尽的分析,包括工作辊和中间辊弯辊、中间辊窜辊的调控功效、辊间接触压力分布等。在此基础上,提出可用指导生产的板形控制策略,指出UCM轧机在横向厚差控制方面的不足。针对工业生产中UCM轧机轧制无取向硅钢横向厚差大的问题,在大量仿真计算的基础上,开发具有高次曲线函数的边部变凸度(Edge variable crown,EVC)的工作辊。采用该工作辊后,各种品种的无取向硅钢的横向厚差不大于10μm的百分比由24%提高到99%,横向厚差的均值小于6μm,远小于之前的13μm。 Medium-low grade non-oriented silicon steel is rolled often by universal crown mill(UCM) during cold rolling.Its shape quality is dependent on the coordinated control of several shape adjustment devices of UCM.In order to understand the shape control characteristics of UCM,coupling model of six-high rolling mill,based on two-dimensional varying thickness finite element rolls elastic deformation model and three-dimensional finite difference strip plastic deformation model,is setup for the detaile...
取向硅钢成品晶粒的位向测定方法
取向硅钢成品的晶粒尺寸非常大,其易磁化方向[001]晶向对于轧向的偏差角度对其磁性能影响极大。本文介绍了取向硅钢二次再结晶后成品晶粒位向的几种测定方法,包括侵蚀法、劳厄法、OIM法、极图法和非对称X射线衍射法等,并对这几种测量方法进行了比较。 The finished product of grain-oriented silicon steel has immense grain size ranging from millimeters to centimeters and the deviation angles of easy magnetization direction from rolling direction plays a remarkable role in magnetic properties of grain-oriented silicon steel.The methods in common use for determining the deviation angles of crystal direction are introduced,which include the etch-figure method,the Laue method,the OIM method,the pole figure method and the asymmetrical X-Ray diffract...
50W600无取向硅钢钙处理的热力学分析及实验研究
通过热力学计算及实验室研究,对钙处理前后50W600无取向硅钢退火冷轧板中夹杂物的类型、数量及尺寸进行了系统分析。结果表明,50W600无取向硅钢经钙处理后(w(Ca)=0.002 6%),钙在1 600℃的钢液中主要以固态的CaO·2Al2O3、CaO·6Al2O3及溶解钙的形式存在。在钢液的凝固过程中,钢中的溶解钙和硫反应生成了CaS和CaS-MnS复合夹杂,有效抑制了MnS的弥散析出,减少了钢中微细夹杂物的数量。同时钙处理促进了钢中微细夹杂物的聚合长大,导致显微夹杂物的数量增加。 Based on thermodynamic calculation and laboratory experiment,the type,quantity and size of inclusions in annealed cold-rolled steel sheets of 50W600 non-oriented silicon steel before and after calcium treatment were systematically studied.Results showed that after calcium treatment(w(Ca) = 0.002 6%),calcium was mainly in the form of CaO·2Al2O3,CaO·6Al2O3 and dissolved calcium in steel at 1 600 ℃.Dissolved calcium could combine with sulfur to form CaS inclusions and compound CaS-MnS inclusions du...
常化冷却工艺对低温取向硅钢组织及析出相的影响(英文)
利用OM、TEM与EDS技术,对Fe-3.2%Si低温取向硅钢热轧板进行不同常化冷却工艺处理后的显微组织、析出相及最终产品的磁性能进行分析,并与热轧板的组织和析出相进行对比。结果表明,常化板较热轧板的表层组织均匀,基体中再结晶比例增加,带状组织变窄;常化板中析出物的数量明显比热轧板的多,析出物主要有AlN、MnS及复合析出的(Cu,Mn)S等。在常化温度1120℃、保温3 min的条件下,采用二段式冷却较空冷、淬沸水、淬常温水的冷却工艺,常化板表层显微组织更均匀,沿板厚方向的显微组织的不均匀性显著,取向硅钢的磁性能最高;常化后采用二段式冷却工艺析出的细小析出物数量最多,且弥散分布在基体中,抑制剂的抑制效果最好,对成品获得高磁性最有利。 Microstructure, precipitate and magnetic characteristic of final products with different normalizing cooling processes for Fe-3.2%Si low-temperature hot-rolled grain-oriented silicon steel were analyzed and compared with the hot-rolled plate by optical microscopy(OM), transmission electron microscopy(TEM), and energy dispersive spectrometry(EDS). The results show that, the surface microstructure is uniform, the proportion of recrystallization in matrix increases, and the banding textures are nar...
还原分离-原子荧光光谱法分析硅钢中痕量汞的不确定度评定
用还原分离-原子荧光光谱法分析了硅钢中的痕量汞.分析方法的不确定度主要来自测量重复性,样品溶液浓度,工作曲线变动性,标准溶液,移取、配制标准溶液,仪器变动性等.文章分别对上述构成合成不确定度大小的分量进行了计算讨论. Trace mercury in silicon steel and galvanized sheet was analyzed by adopting reduced separation-atomic fluorescence spectrometry.The uncertainty of the analysis method mainly comes from measurement repeatability,sample concentration,working curve volatility,standard solution,pipetting and preparation of standard solution,and instrument variability,etc.The essay conducted all calculations and discussions on the above components that determine uncertainty.
无取向电工钢退火工艺研究现状
综述了退火温度、时间对无取向电工钢磁性的影响。退火温度主要影响无取向电工钢不同织构的占有率,退火时间主要影响晶粒尺寸的大小,晶粒尺寸的变化对织构的形成也有一定的影响。磁感最高点出现在纤维组织完全消失,(111)面织构组分较弱的组织状态。铁损的降低主要依赖于磁滞损耗的降低,织构的影响不大。 The effects of annealing temperature and time on the non-oriented electrical steel magnetic properties were reviewed.Annealing temperature and time mainly affects the different textures share and the grain sizes of non-oriented electrical steel respectively.Changes of the grain sizes also have a certain effect on textures formation.The highest point of the magnetic induction value in the fibrous tissue completely disappears and{111} plane texture has a lower state of the component content.Iron l...
电脉冲对取向硅钢凝固组织的影响研究
对取向硅钢熔融态钢液进行处理,对比研究了不同脉冲参数的作用效果。结果表明,电脉冲对钢锭晶粒组织具有明显的细化作用,凝固组织等轴晶比例大幅上升。在脉冲电容、频率、处理时间和电压中,影响等轴晶比例的最显著性因素为脉冲频率;最优正交实验参数为:电容1 200μF,脉冲频率1 Hz,处理时间5 s,脉冲电压800 V;随着输入能量的增大,等轴晶率先增大后减小,脉冲输入能量为某值时,等轴晶率最大,通过经典形核理论和热力学对这一现象进行了解释。 Research on the influence of the electric pulse on the solidification structure of oriented silicon steel was preformed.Electric pulses in different parameters were applied to molten steel and results were compared.The result shows that solidification structure of oriented silicon steel can be improved by the electric pulse,and the equiaxed crystal ratio increases obviously.Among the four parameter factors of electric capacity,frequency,applied time and voltage,the most effective factor is frequ...