所有分类
  • 所有分类
  • 未分类

结合工业化生产的高效硅钢,进行了RH精炼稀土处理试验研究。针对不同的稀土处理条件,观察了夹杂物的形貌和尺寸分布,探讨了稀土处理后钢中的夹杂物形成、变化规律。结果表明:试验条件下,最佳的稀土合金添加数量为0.6~0.9 kg/t。经过合适的稀土处理后,可以有效抑制尺寸相对较小的、不规则的AlN、MnS复合夹杂生成,促进钢中微细夹杂物的聚合、上浮,钢质纯净度得到明显提高。此时,钢中全氧含量最低,脱硫效果最佳,钢中的夹杂物主要是尺寸相对较大的、近似球形或者椭球形的稀土类夹杂。 Based on the industrial production of non-oriented silicon steel,the experiment on RE treatment during the RH refining process was studied.The morphology and the size distribution were observed for the steel specimens treated with different RE treatment conditions.Further more,the formation and change of inclusions of final steel sheets after RE treatment were discussed.The results show that the suitable RE added amount was 0.6~0.9 kg/t.After the suitable RE treatment,the formation of AlN and Mn... 
2011-03-28 147 5.8

基于BOF→RH→CSP生产工艺,研究了RH精炼过程钢中夹杂物类型演变及MgO·Al2O3夹杂物形成规律,同时对MgO·Al2O3夹杂物的形成条件进行了热力学计算,借助CFD数值模拟软件研究了RH精炼过程卷渣行为。研究发现,RH精炼过程20和30 min时,w([MgO])/w([Al2O3])为0.005~0.020,未发现MgO·Al2O3夹杂物;RH出站后夹杂物w([MgO])/w([Al2O3])为0.3~0.5,且RH精炼结束后MgO·Al2O3夹杂物占夹杂物总量的58.4%;另外,RH精炼过程钢液表面速度CFD模拟结果为0.57 m/s,大于临界卷渣速度0.45 m/s,且顶渣成分与夹杂物成分相近,存在卷渣现象。热力学计算表明,钢液与炉渣平衡时钢中w([Al])为0.31%~0.37%,w([Mg])为0.00024%~0.00028%,在MgO·Al2O3生成区域之内。减少RH处理过程卷渣,浇铸过程下渣及控制顶渣和包衬相中MgO质量分数可抑制MgO·Al2O3夹杂物形成。 Based on the practical production of non-oriented silicon steel, the evolution of inclusion type and the formation of MgO·Al2O3inclusion were analyzed in the process of BOF→RH→CSP. The thermodynamic conditions for forming MgO·Al2O3inclusion were discussed and the behavior of slag entrapment of molten steel was also simulated by CFD software during RH refining. The results showed that the value of w([MgO])/w([Al2O3]) was in the range of 0.005-0.020 and no MgO · Al2O3 inclusion was observed at 20 ... 
2014-09-28 134 5.8

研究了冷轧大压下量,950℃退火时间对一种新型含铜无取向电工钢晶粒度和织构的影响。结果表明,大压下量冷轧,随压下量的增加,退火晶粒向γ线聚集,形成强{111}<112>织构。提高冷轧压下率,退火织构{111}<100>,{110}<001>强度减弱,增加退火时间,退火织构{111}<110>,{100}<001>,{110}<001>强度变弱。采用87.5%冷轧压下率和950℃退火60 s,有利织构{100},{110}占有率最大。 The effect of annealing(950 ℃) time with high cold rolling reduction on grain size and texture of a new non-oriented electrical steel containing copper was investigated.The results show that for high cold rolling reduction,most annealed grains are oriented along γ-fibre with increasing cold rolling reduction ratio and strong texture {111}<112> is formed.With increasing the cold rolling reduction ratio,the intensity of annealed texture {111}<110>,{011}<100> decreases.With increa... 
2011-01-28 135 5.8

分析了冲裁硅钢芯片时出现的质量问题,针对影响硅钢芯片冲裁质量的4大因素——人、原材料状态、工艺和工装进行了工艺试验和分析,根据原材料状态的差异,采用不同工艺方案,特别是如何合理选择冲裁模具间隙,解决了硅钢芯片冲裁时产生的主要质量问题,使冲裁的硅钢芯片达到最佳质量状态,并满足硅钢芯片的使用性能。 The problems occurred during silicon steel chip punching and the factors that affect the quality of silicon steel chip punching were analyzed,the factors include 4aspects,that is,people,raw material status,process and frock,at the same time,process tests and analysis aimed at the factors that affect punching quality were did,according to the difference of raw material status,corresponding process schedules wee taken,especially in how to reasonably select punching dies clearance,which solved the ... 
2013-10-28 70 5.8

通过对35W300高牌号0.35 mm冷轧无取向电工钢卷(/%:0.002C、2.71Si、0.22Mn、0.015P、0.003S、0.0020N、0.55Als)头、中、尾组织、织构及对应的磁性能的试验研究,发现因热轧时12 MPa高压水连续冷却造成接触轧辊的钢卷头、中、尾在不同温度下轧制,卷取后钢卷头部处于卷心、温度略高而冷却速度略低于钢卷尾部,致使钢卷纵向组织、织构不同,成品卷头、尾各250 m内磁感逐渐增加,铁损逐渐降低,250 m外至钢卷中部磁性能稳定。通过将热轧辊的冷却方式改为周期冷却和卷取后的层流冷却改为钢卷70 m后开始冷却,至钢卷尾部70 m前停止冷却的方式使得钢卷纵向铁损差异明显减小,磁感差异略有改善。 According to the test research on structure and texture of head,meddle and end of 35W300 high grade 0.35 mm cold rolled non-oriented electrical steel strip coil(/%:0.002C,2.71Si,0.22Mn,0.015P,0.003S,0.002 0 N,0.55Als) and corresponding magnetic properties,It is found that due to 12 MPa high pressure water continuous cooling the roller in hot rolling process led to head,middle and tail of strip rolling at different temperature and after coiling the head of strip coil being in center of coil led t... 
2013-05-28 129 5.8

硅钢工业退火炉温度控制具有强耦合、纯滞后、多扰动等特点,它的控制方法代表着一类非线性系统控制的解决方法。以硅钢工业退火炉温度为控制对象,在双交叉限幅控制的基础上引入了智能学习系统,形成了基于智能学习系统的双交叉限幅控制方法来解决此类非线性系统的控制问题,并通过模块化的编程来实现其功能。结果表明:与传统的PID控制相比,该控制方法的控制精度、抗扰性等控制指标有明显提高,是解决此类非线性控制的一种有效方法。 The temperature control of silicon steel industrial annealing furnace has the features of strong coupling,pure lag,multidisturbance. The control method represents the solution of a class of nonlinear control systems. The control object is the temperature control of silicon steel industrial an-nealing furnace, the intelligent learning system based on Double Across Limit Control is introducedand used to solve control problem of this kind of nonlinear system, and the module programming isused to re... 
2014-05-28 109 5.8

变压器D21硅钢铁芯片采用冲压工艺生产。首先对其工艺进行了分析,确定了冲压方案。对产品进行了排样设计,计算了冲压力,确定了压力中心。然后,设计了单工序落料模具,完成了模具装配图。 D21 silicon steel chips for transformer are produced by stamping.First,its stamping process was analyzed and the scheme of the stamping process was determined.The product layout was designed,the punching pressure was calculated,the pressure center was determined.Then,the blanking die with single procedure was designed,the die assembly drawing was completed. 
2013-07-28 73 5.8

考虑剪应变对微孔洞损伤演化的影响,对GTN损伤模型的损伤演化机制进行修正,建立了适用于不同应力三轴度水平的损伤模型。结合隐式应力更新算法和显式有限元计算,采用VUMAT子程序实现了修正GTN模型在有限元软件ABAQUS中的数值计算。通过模拟纯剪切和剪切-拉伸两组试样的损伤演化和断裂行为,验证了修正GTN模型在不同应力三轴度承载条件下的有效性。运用修正GTN损伤模型模拟含边部缺口的带钢在轧制过程中裂纹的萌生和扩展行为,模拟结果与实验相一致,表明该模型可有效地用于带钢缺陷在轧制过程中扩展行为的分析和预测。模拟和实验结果表明,带钢边部缺口在轧制过程中,缺口前沿和后沿均会萌生裂纹,且后沿裂纹扩展更为明显。 Considering the effect of shear strain of micro-void on damage evolution, a modified GTN model applicable to various stress triaxiality conditions is proposed by modifying the damage evolution mechanism of the GTN damage model. The modified model is implemented in commercial finite element software ABAQUS by combining the implicit stress update method with an explicit finite element solving algorithm and through the user-defined material subroutine VUMAT. The damage evolution and the failure pro... 
2014-06-28 107 5.8

取向硅钢常化工序主要采用现场实测带钢温度的方式测定冷却速率,并通过稳定冷却水温、调整冷却水量及喷梁运行数量等方式保证合理的冷却速率,给常化工艺设计和生产带来诸多不便。通过对常化工艺水冷过程带钢的传热分析求解,在建立带钢水冷温度模型的基础上,研究了不同冷却工艺参数对带钢温度及冷却速率的影响规律以及冷却工艺的交互作用结果。结果表明:模型计算结果能够较好地反映取向硅钢在常化水冷过程中的温度及冷却速率的变化,其计算误差为0.80%~4.11%;在特定取向硅钢厚度规格和常化工艺下,随着常化冷却水量及有效冷却长度的增加,带钢水冷温度及冷却速率与呈非线性变化;常化水冷工艺主要通过调控带钢与冷却水之间热交换量和交换时间实现对带钢温度的控制,实际生产中需综合考虑机组速度、冷却水量及有效冷却长度之间的交互作用,选定喷梁投入数量和冷却水量以获得稳定的冷却速率。 The cooling rate of normalization process mainly determined by measuring the grain oriented silicon steel strip temperature on site, and ensures the cooling rate by stabilizing the cooling water temperature, adjusting the cooling water volume and the operation quantity of spray beam, which brings inconvenience to the normalization process design and production. Based on the heat transfer of strip in the water cooling section of normalization process, the water cooling temperature model for the n... 
2022-01-28 138 5.8

选用国内外无取向硅钢标杆企业A、B、C的产品,采用非水溶液电解提取+SEM(EDS)方法,分析了其典型牌号对应成品试样中的夹杂物。结果表明,从磁性能控制角度而言,受钢的化学成分及生产工艺影响,A、B、C企业成品试样的夹杂物尺寸、种类、数量存在差异,这些差异对其磁性能产生显著影响;从夹杂物控制角度而言,A、B、C企业对应成品试样的夹杂物,以MnS、CuxS复合或者AlN、MnS、CuxS复合为主,其中1.0μm以下的夹杂物数量分别为2.34×107个/mm3、2.98×107个/mm3和11.98×107个/mm3,1.0μm以上夹杂物数量均很少,夹杂物的平均尺寸从大到小依次为A企业、B企业、C企业。 According to the production of three benchmarking manufacture enterprises A,B and C of non-oriented silicon steel at home and abroad,the inclusions in finished steel samples with typical grades were investigated by electrolytic extraction from non-aqueous solution and SEM(EDS).Results show that,from the viewpoint of improving the magnetic properties,affected by chemical composition and production technique,the size,type and amount of inclusions in finished steel samples are various,which will af... 
2013-01-28 119 5.8

磁性能指标是硅钢产品最关键的质量指标之一,但是目前磁性能判定100%依赖于样品的离线实验室检测结果,生产线配置的在线检测仪的测量结果由于精度问题,不宜直接用于成品牌号判级。本文在现有硅钢产品质量管控体系基础上,利用大数据技术对生产数据进行分析与建模,构建不同磁性能指标在线检测模型,并在现有信息系统上完成模型库的集成部署,实现硅钢产品全长、多指标磁性能结果的拟合数据输出,支撑取样优化、精准分切、辅助综合判定等功能应用,进一步优化硅钢产品质量管控体系。 The magnetic performance index of silicon steel products is one of the most critical quality indexes.However,at present,100%determination of magnetic performance depends on the offline laboratory test results of samples,and the measurement results of the online detector configured in the production line cannot be applied in practice due to the accuracy problem.Based on the existing quality control system of silicon steel products,big data technology was used to analyze and model the production d... 
2022-02-28 183 5.8