以CaO-CaF2复合渣系为脱硫剂,在RH精炼过程采用真空投入法进行高牌号无取向电工钢深脱硫工业试验,采用KTH模型计算分析了RH炉渣成分对硫容量CS的影响。研究结果表明,炉渣成分控制在w((CaO))/w((SiO2))为5~7,w((CaO))/w((Al2O3))为1.5~1.8,w((Al2O3))为25%~30%,w((FeO+MnO))<5%,脱硫剂加入量为6~8kg/t时,钢中硫质量分数从平均0.003 1%降低到0.001 8%,最高脱硫率达到47.1%,平均脱硫率为41.7%。 The industrial trials on deep desulphurization of high grade non-oriented electrical steel were finished through using CaO-CaF2complex based fluxes in RH process.Using the KTH model,the effect of refining slag composition on the sulfide capacities was analyzed.The results show that the chemical composition of refining slag(mass fraction,%)is w((CaO/SiO2))between 5to 7,w((CaO))/w((Al2O3))beween 1.5to 1.8,w((Al2O3)) between 25%to 30%,w((FeO+MnO))less than 5%,and the desulphurizer addition level of... 
2014-02-28 136 5.8

研究表明,硅钢中的夹杂物对成品带钢的磁性能有显著影响。为研究冶炼过程硅钢中的夹杂物遗传变化,进而提出更有效的控制措施加以去除,本文结合典型的无取向硅钢生产炉次,采用非水溶液电解提取+扫描电镜观察方法分析冶炼过程中上述炉次典型试样的夹杂物。结果表明:转炉冶炼结束、RH精炼开始时,钢的氧化物夹杂总量最大,约为0.23%;RH精炼过程中,氧化物夹杂总量不断降低,并在脱碳结束时达到最低,约为0.02%;连铸过程中,氧化物夹杂总量仍有不断降低趋势,但夹杂物的平均尺寸变化不大。本试验条件下,中间包试样的夹杂物数量约为1.59×104个/mm3。 As we all know, the non-metallic inclusion effects magnetic properties of silicon steel sheets obviously. The article aims to study the heredity of non-metallic inclusion in non-oriented silicon steels during the steel making process, and then provides a more effective controlling measure to remove the inclusions. Based on the typical non-oriented silicon steel charges, the non-aqueous solution extraction and SEM observation were adopted to analyze the non-metallic inclusions. Results show that,... 
2014-05-28 137 5.8

通过对3%Si CGO硅钢进行恒变形速率、不同变形温度下的单道次压缩实验,结合Thermal-Calc软件,金相分析,SEM及EBSD技术,研究了取向硅钢热变形过程中组织和微观织构的变化规律。结果表明:实验钢是在双相区变形,变形后组织主要是铁素体和少量的珠光体。随变形温度的升高,晶粒由长条状变为等轴状,尺寸逐渐变大;CGO硅钢在热变形过程中立方{100}<001>取向是较为稳定存在的。随着变形温度的提高,{111}<110>等取向逐渐转向{110}<1 10>取向,且{110}<1 10>取向逐渐变得锋锐。 3% Si CGO silicon steel was studied at constant strain rate and different deformation temperatures by single-pass compression deformation experiments to reveal the evolution of microstructure and texture during thermal deformation in oriented silicon steel,and the Thermal-Calc software,metallurgical,SEM and EBSD technique was used in the experiment. The results show that experimental steel is deformed at the temperatures of two-phase zone. The microstructure of the deformed steel consists of fer... 
2014-05-28 147 5.8

研究了应用电感耦合等离子体质谱法(ICP-MS)测定硅钢中痕量铜和镍的分析方法。采用硝酸分解样品,通过内标校正和基体匹配消除了基体干扰的影响,同时根据测量时存在的质谱干扰情况,选择同位素65Cu和60Ni作为测定元素和通过调节仪器参数使双电荷离子的产率最低,以减少带来的干扰。该方法用于硅钢中痕量铜和镍的测定,所得的结果与ICP-AES法测定结果完全吻合,各元素测定结果的RSD值小于5%,加标回收率为97.3%~100.3%。 A method for the determination trace copper and nickel in silicon steel by inductively coupled plasma mass spectrometry(ICP-MS) was studied.The samples were dissolved in HNO3.The effect of matrix interference was eliminated by internal standard correction and matrix matching.Meanwhile,according to the mass spectral interferences in determination,the isotopes including 65Cu and 60Ni were used as measuring elements.The yield of double-charge ions were minimized by adjusting instrumental parameters... 
2011-05-28 145 5.8

通过试验确定氩气分析流量为3.5L/min,静态流量为0.75L/min,冲洗时间为3s,预燃时间为12s,积分时间为5s的激发条件,采用火花源原子发射光谱法测定取向硅钢中碳、硅、锰、磷、硫。分别采用铣床铣样、砂轮磨样两种制样方式进行了精密度考察,发现制样方式对结果影响不大;讨论了取向硅钢样品中碳、硅、锰、磷、硫测定时可能存在的共存元素干扰,发现硅对锰元素的干扰不可忽略,采用干扰系数法进行了校正,据此拟合得到各元素校准曲线的相关系数均在0.999 0以上。精密度考察结果表明,碳、硅、锰、磷、硫的相对标准偏差(n=10)在0.71%~9.4%之间。对两块取向硅钢生产样品进行分析,并与钢铁研究总院进行比对分析,结果一致,且偏差均在允许范围内。 Carbon,silicon,manganese,phosphorus and sulfur in oriented silicon steel were determined by spark source atomic emission spectrometry.The selected excitation conditions were as follows:the analytical flow rate of argon was 3.5L/min,the static flow rate was 0.75L/min,the flush time was3s,the precombustion time was 12sand the integration time was 5s.Two sample preparation methods,including milling machine and grinding wheel,were investigated.The precision test results showed that,the determination... 
2013-10-28 141 5.8

通过微观组织表征、高温拉伸和断口形貌分析,研究了钇(Y)元素对6.5%Si无取向硅钢组织、高温拉伸及断裂机制的影响。研究结果表明,添加Y元素可以在钢液中形成YS和YP的复合析出。YS和YP可以充当异质形核基底,提高形核率,细化凝固组织。热轧组织不均匀,由表层至芯部分别形成等轴晶、等轴晶/拉长晶和拉长晶的混合组织。退火后,热轧变形组织转变为等轴晶,含Y实验钢的退火组织得到明显细化。500℃时效处理后,含Y实验钢具备较低的有序度,300℃的拉伸断口呈现韧性断裂特征,断后伸长率达到20.2%。相反,无Y实验钢发生脆性断裂,断后伸长率仅为2.1%。研究结果证实,Y元素可以通过组织细化和降低有序度提高6.5%Si无取向硅钢的中温塑性。 The effects of yttrium(Y)on microstructure,elevated-temperature tensile properties and fracture mechanism of 6.5% Si non-oriented electrical steel were investigated by means of microstructure characterization,high-temperature tensile test and fracture analysis.The results showed that the doping of Y introduced composite Y-rich precipitates(YS/YP)in the melt.YS and YP precipitates were qualified for heterogeneous nucleation agents,which thus raised the nucleation rate and refined the solidificati... 
2022-01-28 154 5.8

研究了CSP工艺生产≤0.005%C-1.1%Si的2.2mm无取向电工钢热轧板在800~1000℃常化对0.5mm冷轧板840℃退火后组织和磁性能的影响。结果表明,热轧板常化温度升高,冷轧板退火后的再结晶晶粒增大,铁损降低,磁感增加;热轧板常化温度超过900℃,因第二相固溶而后弥散析出,退火后冷轧晶粒细化,铁损增加,因此该无取向电工钢热轧板最佳常化温度为900℃。 The effect of normalizing at 800-1000℃ of CSP produced plate(≤0.005%C-1.1%Si) on the microstructure and magnetic properties of downstream cold-rolled non-oriented electrical steel annealed at 840℃ was studied.Results show that with increasing normalizing temperature of hot-rolled material the recrystallized grain size of annealed sheet increases,iron loss reduced and magnetic induction increases.As normalizing temperature excesses 900℃,grain is refined and iron loss increases after annealing due... 
2012-03-28 121 5.8

运用电子背散射衍射(EBSD)技术,研究了50W600无取向硅钢在热轧→冷轧→退火工序间织构的演变。结果表明:由于热轧板沿板厚方向的应力场和温度场存在差异,导致热轧板不同层织构类型和强度存在差异;热轧板表层主要存在铜型、黄铜和高斯织构,1/4层织构主要为α纤维织构和较弱的高斯织构,中心层织构较单一,主要为α纤维织构;和热轧板相比,冷轧板各层织构差异较小,为典型的轧制织构(α纤维织构和γ纤维织构);退火板各层都表现为γ纤维织构增强、α纤维织构减弱,旋转立方织构基本消失。 The texture evolution of 50W600non-oriented silicon steel in hot rolling,cold rolling and annealing process was investigated by electron back-scatter diffraction(EBSD)technology.Results show that the hot rolled plate texture types and intensities along thickness direction were different because of the different stress fields and temperature fields.The major texture types in the surface of hot rolled plate were copper,brass and Gauss texture.The texture was composed ofαfibre texture and weaker Ga... 
2014-08-28 129 5.8

叠片系数是冷轧无取向电工钢的重要质量指标。为了提高叠片系数,必须保证无取向电工钢板形良好以及横向厚差小。针对攀钢冷轧厂4机架HC轧机轧制无取向电工钢的边部减薄问题,以无取向电工钢横向厚差最小作为目标函数,建立了一套针对无取向电工钢边部减薄控制的辊型曲线优化数学模型,开发了无取向电工钢专用辊型曲线,使无取向电工钢横向厚差从25μm降低到10μm以下,取得了良好的控制效果。 The lamination factor is an important quality index of non-oriented silicon steel strip.Considering the lamination factor,the non-oriented silicon steel must have a good shape and a smaller transverse thickness difference.In order to solve the edge thinning of non-oriented silicon steel strip in Panzhihua Steel,a mathematic model for designing the roll shape is built.In the model,the transverse thickness difference of non-oriented silicon steel strip is taken as the objective function.Based on t... 
2011-01-28 169 5.8

稀土元素在许多钢中发挥着独特而且不可替代的重要作用。半个世纪以来,它的作用已经在各种低合金和特殊合金钢中的研究及应用中得到充分的证明;然而,作为具有稀土资源优势的中国,在属于重要功能材料的无取向电工钢中稀土的应用却落后于国外,本文就中国稀土在无取向电工钢中的应用研究作简要的评述,希望能够进一步推进此领域的研究,并且促进中国稀土在无取向电工钢中应用技术的发展,缩短与国外差距,并提出了在此应用领域今后需深入开展的研究方向。 Rare earth elements play a unique and irreplaceable role in a lot of steels,it has given the full proof by the practice of various low alloy steels and special alloy steels since half century.However,as our country has the advantage of rare earth resources,RE application technology in non-oriented electrical steels has lagged behind abroad.The application researches of rare earth in non-oriented electrical steel in our country are briefly reviewed in this paper,which hope to promote the research... 
2014-05-28 132 5.8

常化快冷是生产高牌号无取向硅钢和高磁感取向硅钢不可缺少的一个工艺环节,气-雾冷却则是实现常化快冷的关键方式之一。介绍了国内自主设计建设的常化酸洗机组气雾冷却系统的技术特性,并对其特点进行了系统分析,最后给出该系统在设计、运行参数的选择上若干注意事项,对气-雾冷却系统设计和使用具有一定的指导作用。 The normalizing rapid cooling is a indispensable process to high grade non-oriented silicon steel and high magnetic induction oriented silicon steel’ s production. The fog cooling is a key ways of coming true the normalizing rapid cooling. This paper introduces the technical features of the fog cooling system in normalizing pickling line which is the domestic independent design and construction. Meanwhile,the fog cooling system’s characteristic is analyzed systematacially. In the end,this paper ... 
2014-03-28 125 5.8

采用RH精炼添加钙合金方式对硅钢进行钙处理,结果表明,钙合金添加量为0.67、1.00和1.67 kg/t钢时,钢中Ca含量分别为0、2×10-6和4×10-(6质量分数);随着钙合金添加量的增加,钢中夹杂物粒度逐渐由0~2μm向2~4μm、4~6μm偏移;不同钙处理条件下,钢中均存在粒径小于1μm和粒径为1~5μm的MnS、CuxS夹杂物,后者或单独存在,或与AlN、CaS夹杂复合;钢中粒径为5~10μm的夹杂物基本以Ca的氧化物和硫化物为主。与未经钙处理的炉次相比,钙合金添加量为0.67、1.00和1.67 kg/t钢时,粒径小于1.0μm的夹杂物减少幅度分别为68.06%、87.50%和94.94%。钙合金添加量为1.67 kg/t钢时,可以去除钢中绝大部分的微细夹杂物。 In order to improve the properties of final silicon steels,the calcium treatment was adopted by adding Ca alloys into the liquid steel during the RH refining process.Results show that when the addition of Ca alloys is 0.67 kg/t,1.00 kg/t and 1.67 kg/t,the corresponding Ca content in silicon steels is 0,2 × 10-6 and 4 × 10-6 respectively.With the increase of Ca alloy addition,the particle sizes of inclusions in steels become 2~4 μm and 4~6 μm,from 0~2 μm.Under different calcium treatments,there e... 