钢厂
加热温度对W470高硅钢连铸坯氧化铁皮的影响
采用SEM、EDS和XRD对不同加热温度下W470连铸坯氧化铁皮的微观形貌及相结构进行研究。结果表明,W470氧化铁皮难以除去的原因是氧化铁皮熔化,液相包裹着FeO,凝固时发生共晶反应,生成FeO/Fe2SiO4共晶混合物,并深嵌入基体。降低加热炉的加热温度,使连铸坯全程在FeO/Fe2SiO4共晶混合物熔点(1177℃)以下加热,可降低氧化铁皮与基体的结合力,能够有效解决W470除鳞困难问题。 The microstructure and phase structure of iron scale of W470 continuous casting billet at different heating temperatures were investigated by SEM,EDS,and XRD.The results show that the reason why the iron scale of W470 removes hardly is that iron scale is melted and the FeO is surrounded by the liquid phase,which forms FeO / Fe2SiO4eutectic mixture and is embedded into the matrix after solidification.Lowering the heating temperature and keeping the continuous casting billet heating under the melt...
硅钢常化退火炉气-雾冷却技术及其特点分析
常化快冷是生产高牌号无取向硅钢和高磁感取向硅钢不可缺少的一个工艺环节,气-雾冷却则是实现常化快冷的关键方式之一。介绍了国内自主设计建设的常化酸洗机组气雾冷却系统的技术特性,并对其特点进行了系统分析,最后给出该系统在设计、运行参数的选择上若干注意事项,对气-雾冷却系统设计和使用具有一定的指导作用。 The normalizing rapid cooling is a indispensable process to high grade non-oriented silicon steel and high magnetic induction oriented silicon steel’ s production. The fog cooling is a key ways of coming true the normalizing rapid cooling. This paper introduces the technical features of the fog cooling system in normalizing pickling line which is the domestic independent design and construction. Meanwhile,the fog cooling system’s characteristic is analyzed systematacially. In the end,this paper ...
低温取向硅钢热轧析出物与织构的研究
采用低温板坯加热制备取向硅钢,通过透射电镜(TEM)观察并研究热轧板中的析出物,用ODF织构法研究热轧板距表面1/8、1/4和1/2处的织构分布。结果表明,热轧板中的析出物主要是密排六方AlN,AlN形貌呈规则长方形,AlN颗粒大小不等,分布密度低;热轧板中的织构沿板厚方向,由亚表层的{110}<001>织构向1/2中心层的α线织构变化,其中{110}<001>织构在热轧板距表面1/4层处最强。 The low temperature grain-oriented silicon steels were produced by acquired inhibitor method.The precipitates in hot rolling strip were observed and studied by transmission electron microscope,and the texture distribution in 1/8,1/4 and 1/2 layers of hot rolling strip were analyzed by ODF method.The results showed that the square shaped h-AlN is the main precipitates in hot rolling strip.The precipitates are varying in size and distribution.The texture of hot rolling strip in thick direction are...
电工钢检测方法及标准综述
综述了电工钢从生产到成品过程中涉及到的检测项目、检测方法及仪器,并通过对电工钢标准的发展改进,详细阐述了我国现有的电工钢技术标准体系,同时对代表企业的电工钢重点指标进行了摘录对比,为综合应用电工钢检测方法并促进电工钢的发展提供了一定的参考。 This article summarizes the testing items,methods,and instruments involved in the process from manufacturing to finished products of electric steel. The current electric steel technical standards system in our country is also elaborated in detail,along with the development and improvement of electric steel standards. Meanwhile,by comparison of electric steel KPI in representitive companies,this article provides references for comprehensive application of electric steels testing methods and promo...
二次冷轧中间退火对基于CSP工艺的取向硅钢组织及织构的影响
在实验室模拟CSP工艺条件下制备了取向硅钢,研究了二次冷轧中间退火工艺对组织和织构的影响。结果表明,中间退火温度对取向硅钢脱碳,高温退火组织及织构均产生明显影响。经940℃中间退火后,取向硅钢脱碳再结晶晶粒较850℃中间退火的多,且再经高温退火处理后,晶粒粗化,最大晶粒尺寸达4.8 mm;高斯织构组分密度达27.00,较850℃中间退火试样高。 Grain-oriented silicon steel was prepared by simulated CSP technology in laboratory. Effects of secondary cold-rolled intermediate annealing on microstructure and texture were studied. The results show that intermediate annealing has obvious effects on the microstructure and texture of the steels after decarburization annealing and high temperature annealing. After intermediate annealing at 940 ℃,recrystallized grain of decarburization annealed steel is more than that of intermediate annealed at...
剪切方式对冷轧无取向硅钢边部磁畴的影响
为提高无取向硅钢导磁性能,研究了不同剪切方式对无取向硅钢剪切处磁畴结构的影响。利用纳米磁流体观测无取向硅钢剪切后边部磁畴结构。结果表明,硅钢无论在机械剪切还是线切割后的边部磁畴都会发生不同程度的改变:线切割对边部磁畴结构改变较小,边部磁畴分布均匀且连续,在距边缘0~20μm范围内出现磁畴宽度变小现象;机械剪切对磁畴的改变较为严重,剪切处磁畴零乱且不连续,在距边缘20μm处仍难以观察到完整的磁畴结构。 The effects of different shearing modes on magnetic domain structure of cold rolled non-oriented silicon steel are studied in this paper.The magnetic domain of cold rolled non-oriented silicon steel is observed by nanometer magnetic fluid pattern method.The results show that the edge magnetic domain structure will be changed by mechanical shear and wire-electrode cutting,the variation of edge magnetic domain structure wire-electrode cutting edge is very small,the magnetic domain structure is wel...
云边一体化系统架构下硅钢制造管理业务数字化融合应用
提出以“云边一体化架构”构建硅钢智慧决策系统,来解决原硅钢制造L1~L5系统架构模式下的数字信息孤岛、业务功能割裂等问题。在此基础上,开发了云边协同的自学习型控制模型及业务决策模型,构建起硅钢“智慧大脑”,形成了以研发、制造、服务等核心业务数字化融合的智能化决策支持新模式,探索出一条钢铁制造业数字化、智能化转型之路。 SIDS(Silicon-steel Intelligent Decision-making System)based on \"cloud-edge integration architecture\" was proposed to solve the problems of data silos and business function fragmentation in the original L1~L5 system architecture.On this basis,the self-learning control model and decision-making model of cloud-edge collaboration were developed,the \"smart brain\" of silicon steel department was constructed,and a new intelligent decision-making support model of digital integration of core businesses s...
无取向电工钢退火工艺研究现状
综述了退火温度、时间对无取向电工钢磁性的影响。退火温度主要影响无取向电工钢不同织构的占有率,退火时间主要影响晶粒尺寸的大小,晶粒尺寸的变化对织构的形成也有一定的影响。磁感最高点出现在纤维组织完全消失,(111)面织构组分较弱的组织状态。铁损的降低主要依赖于磁滞损耗的降低,织构的影响不大。 The effects of annealing temperature and time on the non-oriented electrical steel magnetic properties were reviewed.Annealing temperature and time mainly affects the different textures share and the grain sizes of non-oriented electrical steel respectively.Changes of the grain sizes also have a certain effect on textures formation.The highest point of the magnetic induction value in the fibrous tissue completely disappears and{111} plane texture has a lower state of the component content.Iron l...
新能源车驱动电机用电工钢用量解析计算及预测方法
对新能源汽车以及驱动电机的现有市场和未来市场规模进行梳理分析,通过自建计算公式推导出我国2021年1-11月份驱动电机用电工钢的总量,进而预测未来10年中国新能源汽车驱动电机用电工钢情况,为无取向电工钢的生产和在电机中的应用提供有价值的参考。 The current market and future market size of new energy vehicles and traction motors were analyzed,and the total amount of electrical steels used in traction motors in China from January to November 2021 was derived by using self-built calculation formulas,and then the situation in the next ten years of electrical steel used in traction motors of new energy vehicles in China was predicted.It will provide a valuable reference for the production of non-grain oriented electrical steel and its appli...
高Cu无取向电工钢的制备
运用EBSD和光学显微镜,研究了0.25%~0.45%Cu对无取向电工钢热轧板显微组织,成品板显微组织、织构和磁性能的影响。实验结果表明:卷取过程中Cu元素在热轧板表层的偏聚作用显著阻碍了热轧板表层再结晶晶粒长大,导致热轧板表层晶粒尺寸随着Cu含量增加而逐渐较小,但热轧板中间晶粒尺寸变化不大。同时发现Cu元素能够明显改善织构类型,使有利织构组分增加,不利织构组分减少,同时减弱织构强度。从实验结果可知0.35%Cu能够显著改善电工钢的磁性能,铁损P15/50最低达到4.1 W/kg,磁感B50最高值达到1.8 T。 Effects of high content Cu on microstructure of hot rolled plates and microstructure,texture and magnetic properties of annealed finish product plates of non-oriented electrical steel were examined by means of EBSD technique and optical microscope. The results show that surface segregation of Cu significantly hindered recrystallized grain growth of surface layer in hot rolled plate during the coiling,as a result,the surface grain sizes of the hot-rohed plates decrease with the increase of Cu con...