无取向硅钢的磁性能主要取决于铁素体的晶粒尺寸、晶体织构和钢中的夹杂物。通过合适的化学成分设计以及采用适宜的夹杂物控制技术,可以获得最佳的夹杂物控制效果,使其纯净度大幅度提高或者无害,最终获得磁性能优良的高级别无取向硅钢。同时,为满足节能、环保、高效需求,无取向硅钢正朝着节能降耗、环境友好以及多功能、高效率、易加工等方向发展。 The magnetic properties of non-oriented silicon steel mainly depend on the grain size of ferrite,the crystallographic texture,and the inclusions in the steel.The optimum inclusion control effects can be obtained through a suitable chemical composition design and an appropriate inclusion control technique,and then the liquid steel will get be clean or the inclusion will get be harmless,finally the excellent magnetic property of the non-oriented silicon steel can be obtained.Meanwhile,in order to ... 
2013-03-28 182 5.8

综述了退火温度、时间对无取向电工钢磁性的影响。退火温度主要影响无取向电工钢不同织构的占有率,退火时间主要影响晶粒尺寸的大小,晶粒尺寸的变化对织构的形成也有一定的影响。磁感最高点出现在纤维组织完全消失,(111)面织构组分较弱的组织状态。铁损的降低主要依赖于磁滞损耗的降低,织构的影响不大。 The effects of annealing temperature and time on the non-oriented electrical steel magnetic properties were reviewed.Annealing temperature and time mainly affects the different textures share and the grain sizes of non-oriented electrical steel respectively.Changes of the grain sizes also have a certain effect on textures formation.The highest point of the magnetic induction value in the fibrous tissue completely disappears and{111} plane texture has a lower state of the component content.Iron l... 
2013-10-28 157 5.8

常化快冷是生产高牌号无取向硅钢和高磁感取向硅钢不可缺少的一个工艺环节,气-雾冷却则是实现常化快冷的关键方式之一。介绍了国内自主设计建设的常化酸洗机组气雾冷却系统的技术特性,并对其特点进行了系统分析,最后给出该系统在设计、运行参数的选择上若干注意事项,对气-雾冷却系统设计和使用具有一定的指导作用。 The normalizing rapid cooling is a indispensable process to high grade non-oriented silicon steel and high magnetic induction oriented silicon steel’ s production. The fog cooling is a key ways of coming true the normalizing rapid cooling. This paper introduces the technical features of the fog cooling system in normalizing pickling line which is the domestic independent design and construction. Meanwhile,the fog cooling system’s characteristic is analyzed systematacially. In the end,this paper ... 
2014-03-28 165 5.8

利用OM,TEM,EDS与XRD技术,对Fe-3.15%Si低温取向硅钢热轧板不同常化处理后的显微组织、析出相及最终产品的磁性能进行了分析研究,并对热轧板和常化板经过冷轧后的冷轧板织构进行了对比分析.结果表明,采用1120℃保温3 min二段式冷却的常化处理工艺,常化板表层显微组织均匀,沿板厚方向的显微组织的不均匀性显著,对后续过程中形成高取向的Goss织构最有利,取向硅钢的磁性能最高;采用二段式冷却的常化冷却工艺最优,在此冷却工艺下析出的细小的析出物数量最多,且弥散分布在基体中,抑制剂的抑制效果最好,对成品获得高磁性最有利;热轧板、常化板经过冷轧后的冷轧板织构均主要由{111}〈110〉和{111}〈112〉织构组成,但常化板较热轧板冷轧后的冷轧板γ取向线织构密度明显增高,由此可以证实常化处理有助于取向硅钢最终获得高取向的Goss织构. The decreasing of slab heating temperature for grain-oriented silicon steel will reduce the amount of precipitates in hot rolled plate,and be disadvantage to the formation of ultimate Goss texture.The aim of normalizing is to control and adjust the amount,size and distribution of precipitates.Microstructures,precipitates and magnetic characteristics of finished products with different normalizing technologies for Fe-3.15%Si low temperature hot rolled grain-oriented silicon steel are researched,a... 
2013-05-28 156 5.8

结合硅钢退火炉项目中应用PDSOFT软件进行三维配管设计的案例,描述PDSOFT软件的应用过程,总结其使用要点,分析其优缺点,并提出了推广三维设计软件的思路,对今后PDSOFT在相似项目中的推广应用有参考和借鉴价值。 Combining the case of using PDSOFT software to design the three-dimensional piping,the application process of the PDSOFT software is described,the using points are summarized,the advantages and disadvantages are analyzed,and the ideas of promoting the three-dimensional design software are put forward,which have a strong reference value for the promotion and application of PDSOFT in similar projects in the future. 
2014-04-28 130 5.8

采用Nb对Fe-6.5%Si(质量分数)高硅钢进行微合金化处理,结果表明:Nb在高硅钢薄板制备过程中细晶效果明显.铸态、锻态和热轧态组织的晶粒分别细化了17.50%,24.51%和30.13%.铸态样品压缩强度由1365 MPa提高至1520 MPa,延伸率提高77.78%;温轧板试样室温拉伸强度由573 MPa提高至621 MPa,延伸率提高44.44%.利用XRD对厚度为0.30—1.68 mm的温轧板的板面织构演变过程进行跟踪测量,结果发现:初始织构以(011)〈100〉Goss织构为主,单道次变形量为26.2%的情况下,Goss织构完全转化为(100)〈011〉旋转立方织构,随后,在单道次变形为22.6%的情况下,旋转立方织构完全转化为{111}面织构,即纤维织构,并稳定保持至0.30 mm. Fe-6.5%Si(mass fraction) alloy possess perfect magnetic properties,though intermetallics of Fe14Si2 phase brought 6.5%Si leads to room temperature brittleness and hinder this significant materials industrialization.Nb was adopted into micro-alloying of Fe-6.5%Si high silicon steel. OM,thermal simulated test machine and XRD were employed to study the influence of Nb on high silicon steel in processing stages.Textures of warm-rolled high silicon steel strips were determined b... 
2013-11-28 169 5.8

考虑剪应变对微孔洞损伤演化的影响,对GTN损伤模型的损伤演化机制进行修正,建立了适用于不同应力三轴度水平的损伤模型。结合隐式应力更新算法和显式有限元计算,采用VUMAT子程序实现了修正GTN模型在有限元软件ABAQUS中的数值计算。通过模拟纯剪切和剪切-拉伸两组试样的损伤演化和断裂行为,验证了修正GTN模型在不同应力三轴度承载条件下的有效性。运用修正GTN损伤模型模拟含边部缺口的带钢在轧制过程中裂纹的萌生和扩展行为,模拟结果与实验相一致,表明该模型可有效地用于带钢缺陷在轧制过程中扩展行为的分析和预测。模拟和实验结果表明,带钢边部缺口在轧制过程中,缺口前沿和后沿均会萌生裂纹,且后沿裂纹扩展更为明显。 Considering the effect of shear strain of micro-void on damage evolution, a modified GTN model applicable to various stress triaxiality conditions is proposed by modifying the damage evolution mechanism of the GTN damage model. The modified model is implemented in commercial finite element software ABAQUS by combining the implicit stress update method with an explicit finite element solving algorithm and through the user-defined material subroutine VUMAT. The damage evolution and the failure pro... 
2014-06-28 168 5.8

针对硅钢连续生产线设备存在的故障、隐患以及精度等影响产品质量的问题进行分析及改造,实现保证生产线设备稳定运行、提高设备精度及硅钢产品质量的目的。 This paper analyzes and transforms the electrical equipment failures, risks existed in slicon continuous production line, and the effect of accuracy to product quality, in order to ensure stable operation of equipment in production line and improve the accuracy of device, quality of silicon. 
2014-04-28 158 5.8

介绍了国内无底层取向电工钢生产技术水平、产量和用途,简述了无底层取向电工钢作为取向电工钢超/极薄带母料及应用于制作大型发电机组铁心、风电等电机铁心和变压器铁心等的情况。 The production technology level,output and application of domestic glassless grainoriented electrical steel were introduced,and the application of glassless grain-oriented electrical steel as parent material of ultra-thin strip of grain-oriented electrical steel and in making large-scale electric generator cores,wind power motor cores and transformer cores were briefly described. 
2022-02-28 203 5.8

综述了国内外大钢铁企业与研究机构采用获得抑制剂法生产低温高磁感取向硅钢的开发及应用情况,分析了以该法生产高磁感取向硅钢过程中抑制剂的控制技术,包括固有抑制剂组成方案、气态渗氮方式与工艺及高温退火工艺的制定.研究表明,固有抑制剂组成方案的设计思路大体一致,化合物抑制剂以AlN为主、硫化物为辅,同时添加少量Sn,Sb等单元素抑制剂,但组成元素含量存在一定差别;在脱碳退火后用NH3进行非平衡渗氮处理已成为气态渗氮的主要方式,但最佳方式仍未明确,具体选择需依据实际生产条件,相应脱碳及渗氮工艺的控制条件差别较大;高温退火工艺中升温制度差别不大,升温阶段退火气氛中N2含量的选择存在差别.此外,分析了抑制剂控制技术目前存在的关键问题,并指出了进一步的研究方向. The current application and exploitation on production of low-temperature high magnetic induction grain-oriented silicon steel with acquired inhibitor method at both iron and steel enterprises and research institutions in the world are reviewed. The control techniques of inhibitors, which include the composition design for inherent inhibitors, nitriding method and process, and secondary recrystallization annealing, are thoroughly analyzed and proposed. It is indicated that the design ideas for i... 
2014-01-28 180 5.8

【作者】 罗海文; 向睿; ...
2014-10-28 182 5.8

以试验室模拟CSP工艺生产的Fe-3Si热轧钢带为研究对象,采用正交试验及方差分析的方法,研究了取向硅钢初次再结晶退火工艺对高温退火后获得锋锐的高斯织构的影响。结果表明:取向硅钢两段式初次再结晶脱碳退火工艺参数加热段保温时间及加热温度是高温退火后获得锋锐高斯织构的主要影响因素,其可信度分别在90%和85%以上;在本试验条件下,通过正交试验获得的最佳退火工艺为:冷硬板经600℃保温3 min和850℃保温6 min。 Fe-3Si hot rolled strip was produced by simulating CSP technology in the laboratory.Orthogonal experiment and analysis of variance were carried out to investigate the influence of primary recrystallization on the sharp Goss texture of the oriented silicon steel.The results show that holding time of the heating section and the heating temperature for a sharp Goss texture of the samples annealed has important implications in this experiment conditions,the two-step decarburization annealing process... 
2013-02-28 171 5.8