钢厂
硅钢连退机组辐射管加热段数值模拟
文章以国内某公司硅钢厂连续退火机组1号辐射管加热段为研究对象,分析炉内传热机理,建立并开发了辐射管加热段的传热模型。采用生产实际数据对模型进行了验证,以总燃料消耗量最小为目标,得出该炉段长度方向上燃料的最佳分配机制。所得结论为该公司连续退火机组节能控制提供理论依据。 Taking the radiant tube heating section of No.1 continuous annealing unit in a silicon steel plant of a domestic company as the research object, the heat transfer mechanism in the furnace is analyzed, and the heat transfer model of the radiant tube heating section is established and developed. The model is verified by the actual production data. Aiming at the minimum total fuel consumption, the optimal fuel distribution mechanism in the length direction of the furnace section is obtained. The co...
冷轧产线硅钢激光高速切边实验研究
为了解决目前冷轧产线硅钢现有切边技术存在的微裂纹、应力、毛刺和边浪等问题,采用光纤激光器进行了高速切割实验,对激光功率、切割速度、激光模式等影响因素进行了分析,同时对高速切割时的切割前沿形状进行了研究。结果表明,切割最高速度随着功率的增加而增加;随着离焦量的增加,切割质量下降,挂渣增多,切缝宽度增加,切割深度变浅;基模激光器能量密度更高,所以薄板切割时的切割速度高于多模激光器;切割前沿随着切割速度的增加会变得平缓,速度足够大时,切割前沿甚至接近与切割方向平行,此时切缝下部存在挂渣现象。 In order to solve the problems such as micro crack,stress,burr,edge waves and so on,existing in cold rolling production line of silicon steel side cutting,experimentsof high speed laser cutting using fiber laser were carried out.Laser power,cutting speed,laser mode and other factors were analyzed,at the same time,cutting front geometries were studied.The results show that the maximum speed increases with power.And the increases of defocus result in poor quality,wider kerf and shallowerkerf.Energ...
TSCR热轧工艺对3.2%Si无取向硅钢组织性能的影响
研究了薄板坯连铸连轧流程(TSCR)条件下热轧工艺对3.2%Si-0.7%Al无取向硅钢组织、织构演变及磁性能的影响规律。结果表明,提高均热温度和热轧温度有助于获得粗大的变形组织和强烈的{001}〈110〉织构,进而对后续的组织、织构演变进程及磁性能产生有利的遗传影响。与低温均热和低温热轧相比,高温均热和高温热轧得到的最终成品板的再结晶晶粒较粗大,λ纤维再结晶织构较强而γ纤维再结晶织构较弱,磁感应强度较高。 It was investigated that the effects of thin slab cast rolling(TSCR) hot rolling processes on microstructural,textural evolution and magnetic properties of 3.2%Si-0.7%Al non-oriented silicon steel.The results show that much larger hot rolling deformed microstructure and much stronger {001}〈110〉 texture could be obtained by increasing the soaking and hot rolling temperatures,which had good heritable effects on subsequent microstructural,textural evolution and magnetic properties.The final sheets ...
Si在纯Fe及低硅钢中扩散行为
采用磁控溅射方法,分别在纯Fe以及低硅钢基片上沉积富Si膜,并对其进行真空扩散热处理.通过能谱分析及X射线衍射研究了Si在纯Fe与低硅钢基体中的扩散特征,运用DICTRA软件建立了扩散模型.研究发现Si在纯Fe基体中扩散时发生γ-Fe(Si)→α-Fe(Si)相转变,扩散速率受控于相界面的迁移.当沿截面Si含量梯度不足以驱动相界面正向迁移时,延长扩散时间会发生相界面回迁现象,最终趋于单一相内均匀化扩散过程.Si在低硅钢基体中的扩散符合Fick扩散第二定律. Si-rich films were deposited on pure iron and low-Si steel substrates by direct current magnetron sputtering,and then were subjected to vacuum annealing.The distribution characteristics of Si across Fe and low-Si steel substrates were studied by energy spectrum analysis(EDS) and X-ray diffraction(XRD).DICTRA software was used to simulate the diffusion models.It is found that the diffusion behavior of Si in the Fe substrate is from γ-Fe(Si) phase to α-Fe(Si) phase and the rate of diffusion is con...
铬、锰及退火温度对无取向硅钢组织性能影响
为探究铬、锰元素及退火温度对高强无取向硅钢性能的影响规律,借助OM、SEM、EBSD与万能拉伸试验机等分析不同制造工艺下3组不同含量铬、锰元素的无取向硅钢热轧、常化及退火处理后组织与性能。结果表明,试验钢热轧后组织不均匀,心部为沿轧向分布纤维状组织,边部为少量再结晶晶粒,常化处理能显著改善热轧板组织均匀性,消除热轧板中心部位的纤维状组织。经冷轧及退火后得到多边形铁素体晶粒,其中960℃退火,晶粒尺寸偏大,有利织构{100}组分体积分数减少,不利织构{111}组分体积分数增加,成分为0.2Mn-1Cr的1号试验钢960℃退火后铁损最大,磁感强度偏小;成分为0.5Mn-1Cr的2号试验钢930℃退火后,磁性能与强度等综合性能最佳,工频铁损P1.5/50为2.41W/kg,高频铁损P1.0/400为17.36W/kg,磁感应强度B5 000为1.638T,抗拉强度为685MPa。 In order to study the effect of Cr,Mn and annealing temperature on the properties of high-strength non-oriented silicon steel,the microstructure and properties of three groups of non-oriented silicon steel with different Cr,Mn content under different manufacturing processes were analyzed by means of OM,SEM,EBSD and universal tensile tester.The results show that the structure of experimental steel is not uniform after hot rolling,and the core is distributed in fibrous structure along the rolling ...
电工钢边缘降控制研究
以马鞍山钢铁集团公司电工钢板形优化控制研究项目为背景,系统地研究了热轧、冷连轧和单机架轧机在电工钢生产过程中的边缘降控制问题。通过现场数据采集、工况数值模拟计算和工业化大生产试验,设计出适用、合理的电工钢板形控制的辊型优化曲线,满足了不同工序、不同机型的板形控制策略要求,解决了电工钢板形质量问题,取得了显著的经济效益。 Based on the project of electric steel strip shape optimization control,problem of edge drop control was systematically studied in production of electric steel of hot-rolling mill,cold-rolling mill and single stand mill.Roll optimization contour was designed out in point and reasonable by collection of work condition data,numerical simulation and test of industrial production.The shape control system can meet with the different working steps and difference mills,and quality problem of electric s...
脉冲磁场退火对取向硅钢磁性能的影响
通过对取向硅钢进行脉冲磁场退火实验,发现在相同的退火时间(6.0 min)内,低于1 T的脉冲磁场可以在一定程度上提高取向硅钢的磁感(B8),而高于1 T的脉冲磁场则会使取向硅钢的磁性能急剧恶化.同时发现,脉冲直流电加热方式会使取向硅钢的磁性能恶化.研究表明,脉冲磁场退火有望成为一种调控材料微观结构的有效手段. We have carried out experiments of annealing by pulse magnetic field.The results show that a pulse magnetic field with intensity lower than 1 T can promote magnetic induction density(B8) of grain-oriented silicon steel,while the magnetic properties deteriorate sharply when intensity is higher than 1 T.It has also been found that heating by using pulse direct current can cause the magnetic properties to deteriorate,in contrast to the traditional heating using resistance furnace.Our research shows...
硅钢氧化镁的制备进展
介绍了硅钢氧化镁制备方法及高质量硅钢氧化镁制备技术的研究进展,并对利用我国丰富的卤水资源制备硅钢氧化镁进行了展望。 The preparation methods of silicon steel magnesium oxide and research progress of high quality silicon steel magnesium oxide preparation technology were introduced.The use of abundant brine resources in the preparation of silicon steel magnesium oxide was prospected.
承钢无取向电工钢CGW800的研发
承钢采用铁水预处理(脱硫)→转炉提钒→转炉冶炼→RH精炼→连铸→轧制工艺,成功研发了无取向电工钢CGW800。试制的CGW800钢碳含量≤0.006 0%、氮含量<0.004 0%,热轧后的金相组织为铁素体和少量渗碳体,晶粒度5.5级,获得了较粗大、均匀的晶粒,钢板的成分和力学性能达到了标准要求。 In Cheng Steel,the CGW800 non- oriented electrical steel is successfully developed with process of hot metal pre- treating,vanadium extracting with converter,smelting with converter,RH refining,continuous casting and rolling. In the steel,the carbon content is not higher than 0. 006 0%,nitrogen less than0. 004 0%,the metallographic structure after hot rolling is ferrite and a little amount of cementite,grain size is 5. 5 degree,relative large and even grain got. The composition and mechanical pr...
无取向硅钢铬酸镁绝缘涂层结构与耐蚀性能研究
采用扫描电镜、原子力显微镜研究了铬酸镁半无机绝缘涂层的微观结构。结果表明,涂层厚度为数微米,涂层中的有机树脂乳液颗粒均匀分布在无机涂层的表面,从而保证了涂层具有良好的冲片性能。采用极化曲线研究了涂层的耐蚀性能,发现铬酸镁与铬酸锌绝缘涂层的耐蚀性能相当。 In this paper,the microstructure and anti-corrosion property of magnesium chromate coating on non-oriented silicon steel were studied.The microstructure was observed by SEM and AFM.The anti-corrosion properties were evaluated by polarization curves.The results show that the thickness of coating is several microns and the polymer particles were scattered on the surface of inorganic coating,which is the guarantee for lamination property.The corrosion resistance of the magnesium chromate film was e...
钇元素对6.5%Si无取向硅钢组织、高温拉伸及断裂机制的影响
通过微观组织表征、高温拉伸和断口形貌分析,研究了钇(Y)元素对6.5%Si无取向硅钢组织、高温拉伸及断裂机制的影响。研究结果表明,添加Y元素可以在钢液中形成YS和YP的复合析出。YS和YP可以充当异质形核基底,提高形核率,细化凝固组织。热轧组织不均匀,由表层至芯部分别形成等轴晶、等轴晶/拉长晶和拉长晶的混合组织。退火后,热轧变形组织转变为等轴晶,含Y实验钢的退火组织得到明显细化。500℃时效处理后,含Y实验钢具备较低的有序度,300℃的拉伸断口呈现韧性断裂特征,断后伸长率达到20.2%。相反,无Y实验钢发生脆性断裂,断后伸长率仅为2.1%。研究结果证实,Y元素可以通过组织细化和降低有序度提高6.5%Si无取向硅钢的中温塑性。 The effects of yttrium(Y)on microstructure,elevated-temperature tensile properties and fracture mechanism of 6.5% Si non-oriented electrical steel were investigated by means of microstructure characterization,high-temperature tensile test and fracture analysis.The results showed that the doping of Y introduced composite Y-rich precipitates(YS/YP)in the melt.YS and YP precipitates were qualified for heterogeneous nucleation agents,which thus raised the nucleation rate and refined the solidificati...
取向硅钢中含铜抑制剂的固溶析出行为
含铜抑制剂作为取向硅钢的主抑制剂或辅助抑制剂不仅可以抑制初次晶粒的长大,促进二次再结晶,还可以降低铸坯的加热温度。取向硅钢中主要抑制剂为10~50 nm Cu2S,在钢的铸坯、热轧、冷轧、脱碳等工艺过程均可析出;(Cu,Mn)1.8S、Cu1.8S、ε-Cu等主要作为辅助抑制剂,尺寸一般为30~50 nm(或大于50 nm),主要在热轧阶段析出。总结了国内外有关取向硅钢中含铜抑制剂析出行为的研究进展,当前主要研究不同生产流程和工序中含铜抑制剂的析出行为和作用机理。 As main inhibitor or auxiliary inhibitor for grain-oriented silicon steel,the particles of inhibitor bearing copper not only inhibit the primary crystal growing and promote the secondary recrystallization,but also decrease the heat temperature of casting slab.The main inhibitor for grain-oriented silicon steel is 10~50 nm Cu2S,which precipitate in process and procedure including steel casting slab,hot rolling,cold rolling and decarburizing process,while the 30~50 nm or more than 50 nm...