研究了热处理工艺(退火温度、保温时间、冷却方式)对含Mn的Fe-6.5wt%Si高硅钢热轧带的显微组织及硬度的影响。结果表明,退火温度对Fe-6.5wt%Si合金的组织和显微硬度均有较大影响,随退火温度升高,平均晶粒尺寸和显微硬度均明显增大。小于1 h退火时,晶粒长大缓慢,而长时间(>1 h)退火时,一些次表层晶粒将发生异常长大。水冷组织比空冷组织略细小,但水冷显著降低了显微硬度。Mn含量提高能抑制850℃退火时晶粒的长大,并且促进退火后高硅钢的软化。 The influences of heat treatment process(annealing temperature,heating time,cooling methods) on the microstructure and microhardness of Fe-6.5wt%Si high silicon steel containing manganese for hot rolled strip were studied.The results show that the annealing temperature has a great effect on the microstructure and microhardness of Fe-6.5wt%Si alloy,and as the annealing temperature increases,the average grain sizes and microhardness will significantly increase.When annealing time for less than 1 h... 
2023-05-12 1.34k 5.8

研究了应用电感耦合等离子体质谱(ICP-MS)同时测定硅钢中痕量铝、钼、钒、钛、铌元素的分析方法。通过条件试验对测量参数进行了优化,确定RF功率1 400 W,泵速30rpm,采样深度140,雾化压力0.90。样品采用硝酸分解,以Be、Y混合内标校正了测量过程中高基体引起的信号漂移。根据测量时存在的质谱干扰情况,选择同位素27 Al、98 Mo、51 V、47 Ti和93 Nb作为测定同位素,同时通过调节仪器参数使得双电荷离子和氧化物离子的产率最低,以减少其带来的干扰。采用基体匹配法配制校准溶液,以标准加入法建立工作曲线,并扣除试剂空白。该方法各元素的测定下限均可达到1μg/g。用于硅钢标准样品的测定,所得结果与参考值完全吻合,各元素的RSD小于5.2%。 A method for the determination of trace aluminum,molybdenum,vanadium,titanium and niobium in silicon steel by inductively coupled plasma mass spectrometry(ICP-MS) was described.A series of single parameter condition experiment was conducted.The optimized operation parameters with RF power 1 400 W,turbo pump rate 30 rpm,sampling depth 140 and nebulizer pressure 0.90 were obtained.The samples were dissolved by HNO3,and the Be and Y mixing internal standard were used to eliminate the signal drift c... 
2013-01-28 159 5.8

本文中简要介绍了武汉钢铁有限公司采用薄板坯连铸连轧CSP(compact strip production, CSP)工艺生产中低牌号无取向硅钢的实践情况.CSP工艺生产的硅钢具有成品磁性均匀、板形好的优势,但是在利用该技术生产中低牌号无取向硅钢时,常存在成品板表面瓦楞状缺陷严重、连铸生产效率低等问题.通过优化炼钢成分、热轧等相关工艺,可消除热轧板厚度方向中心的粗大形变组织,从源头上避免了粗大{100}<011>纤维组织的出现,消除了瓦楞状缺陷;通过提升冶炼效率和控制钢中夹杂物总量,可优化隧道炉的加热温度与在炉时间,大幅度提升了连铸生产效率,实现了中低牌号无取向硅钢的批量稳定制造,使CSP产线成为中低牌号无取向硅钢热轧板原料的主要供给生产线.如何进一步提升钢水纯洁度、提高连铸生产效率、降低生产成本,以及挖掘该产线生产薄带钢的技术优点,是未来工作的重点. This paper briefly introduces the practice of producing medium and low grade non oriented silicon steel(NGO) with CSP(compact strip production, CSP)technology in Wuhan Iron and Steel Co., Ltd.. This technology has the inherent advantages of uniform magnetic properties and good shape for silicon steel finished strip. However, in the actual production process, there are serious corrugated defects on the surface of silicon steel finished strip, and production efficiency of continuous casting is low... 
2023-01-28 180 5.8

采用扫描电镜、场发射扫描电镜、能谱仪等对50SW1300冷轧无取向硅钢中的夹杂物分不同尺寸区间进行数量统计,利用主成分回归分析法,即数据的标准化处理—主成分分析—回归分析—标准化的变量还原成原始变量—确定显著影响因素,综合分析夹杂物总量及各尺寸区间的夹杂物数量对无取向硅钢磁性能的影响。结果表明:主成分回归分析能够从夹杂物尺寸区间及数量的多个影响因素中提取主要的因素,定量研究其对磁性能的影响。分析表明,显著影响无取向硅钢铁损的夹杂物为100~500nm的AlN、AlN+MnS、MnS、Al2O3、AlN+Al2O3,而劣化磁感最明显的夹杂物尺寸区间为100~200nm。 Different size intervals of inclusions in cold rolled non-oriented silicon steel 50SW1300 were counted by scanning electron microscope(SEM),field emission scanning electron microscope(FESEM)and energy disperse spectroscopy(EDS).With principal component regression method:standardization for experimental data,principal component analysis,regression analysis,transform standardized variables into original variables,determination of significant factor,effects of the total number of inclusions and the... 
2014-10-28 183 5.8

研究了锰含量对w(Si)=1.8%Si无取向电工钢组织和性能的影响。结果表明,钢中锰含量从0.3%增加到1.2%时,由于α_γ相变的产生,铸坯低倍组织、热轧板金相组织及成品织构等均发生了不同程度的变化,对成品表面质量及磁性能产生了明显的影响。 The effects of manganese content on structure and properties of w(Si)=1.8% non-oriented electrical steels have been studied.Results show that with increasing manganese content to 1.2% from 0.3%,macrostructure of continuous casting slab,hot rolled band metallurgical structure and finished product texture vary in some extent because of the occurrence of α-γ phase transformation,the surface quality and magnetic properties of finished product are affected greatly. 
2011-03-28 149 5.8

提出以“云边一体化架构”构建硅钢智慧决策系统,来解决原硅钢制造L1~L5系统架构模式下的数字信息孤岛、业务功能割裂等问题。在此基础上,开发了云边协同的自学习型控制模型及业务决策模型,构建起硅钢“智慧大脑”,形成了以研发、制造、服务等核心业务数字化融合的智能化决策支持新模式,探索出一条钢铁制造业数字化、智能化转型之路。 SIDS(Silicon-steel Intelligent Decision-making System)based on \"cloud-edge integration architecture\" was proposed to solve the problems of data silos and business function fragmentation in the original L1~L5 system architecture.On this basis,the self-learning control model and decision-making model of cloud-edge collaboration were developed,the \"smart brain\" of silicon steel department was constructed,and a new intelligent decision-making support model of digital integration of core businesses s... 
2022-02-28 184 5.8

结合硅钢退火炉项目中应用PDSOFT软件进行三维配管设计的案例,描述PDSOFT软件的应用过程,总结其使用要点,分析其优缺点,并提出了推广三维设计软件的思路,对今后PDSOFT在相似项目中的推广应用有参考和借鉴价值。 Combining the case of using PDSOFT software to design the three-dimensional piping,the application process of the PDSOFT software is described,the using points are summarized,the advantages and disadvantages are analyzed,and the ideas of promoting the three-dimensional design software are put forward,which have a strong reference value for the promotion and application of PDSOFT in similar projects in the future. 
2014-04-28 109 5.8

针对硅钢连续退火机组的主要能源介质消耗现状,对现有生产工艺和设备研究采取机组循环用水、增加清洗段漂洗级数等措施可节约大概27 m3/h的过滤水量,并可减少78%的弱碱处理量;将炉子烟气换热系统增加一级余热回收,每年回收的余热相当于583 t标煤消耗,可节约蒸汽5 368 t。 The present situation of energy consumption for silicon steel annealing line is analyzed in this paper.In existing process and equipment conditions,increasing the number of cleaning series will lead to a saving of about 27 m3/h of filter water and reduce 78 % of weak base processing volume.For the flue gas heat-exchange system,adding a waste heat recovery device will recover waste heat equivalent to 583 tons of standard coal per year,corresponding to a saving of steam 5 368 t per year. 
2011-05-28 147 5.8

组织和织构是影响无取向硅钢性能的重要因素。为改善产品性能,研究了冷轧压下率(71.7%~87.0%)对高牌号无取向硅钢组织、织构、磁性能和力学性能的影响。结果表明,随冷轧压下率的增加,退火晶粒平均尺寸先减小后增大;高斯和立方织构强度减弱,γ纤维织构增强,α纤维织构转变为较强的α*({h, 1, 1}〈1/h, 1, 2〉)织构,并随冷轧压下率的增加而增强,同时其峰值逐渐向{111}面移动;工频铁损P1.5/50、高频铁损P1.0/400和磁极化强度J5000同时降低,屈服强度变化不大,表面硬度逐渐增加。当冷轧压下率由84.7%增至87.0%、厚度减至0.30 mm时,高频铁损降幅是工频铁损的11倍,表面硬度增幅变大。以上研究成果对硅钢减薄后织构及组织的优化提供了很好的指导。 Microstructure and texture are critical factors on non-oriented silicon steel properties. In order to improve product properties, this paper studied the effect of cold rolling reduction rate(71.7%-87.0%) on microstructure, texture, magnetic properties and mechanical properties of high-grade non-oriented silicon steel. The results show that with the increase of cold rolling reduction rate, the average size of annealing grain decreases first and then increases. The intensity of Goss and λ fiber te... 
2022-05-28 179 5.8

介绍了CSP工艺生产无取向电工钢各工序的设备特点、采用的工艺控制手段和电工钢产品质量情况,结合生产实践证明了马钢CSP工艺开发的无取向电工钢产品丰富了薄板坯连铸连轧的品种结构,发挥了薄板坯连铸连轧生产无取向电工钢性能均一、稳定的特点。 The equipment characteristic,the process control method and the quality of non-orientated silicon steel by CSP process were introduced.Combined with the production situation,it is proved that production of non-orientated silicon steel developed on Masteel CSP line would enrich product structure of thin slab continuous casting and rolling,and it exerts stable performance of non-orientated silicon steel. 
2013-06-28 165 5.8

【摘要】 <正>含6.5%Si的电工钢是软磁特性最佳的电...
2014-04-28 111 5.8

运用EBSD和光学显微镜,研究了0.25%~0.45%Cu对无取向电工钢热轧板显微组织,成品板显微组织、织构和磁性能的影响。实验结果表明:卷取过程中Cu元素在热轧板表层的偏聚作用显著阻碍了热轧板表层再结晶晶粒长大,导致热轧板表层晶粒尺寸随着Cu含量增加而逐渐较小,但热轧板中间晶粒尺寸变化不大。同时发现Cu元素能够明显改善织构类型,使有利织构组分增加,不利织构组分减少,同时减弱织构强度。从实验结果可知0.35%Cu能够显著改善电工钢的磁性能,铁损P15/50最低达到4.1 W/kg,磁感B50最高值达到1.8 T。 Effects of high content Cu on microstructure of hot rolled plates and microstructure,texture and magnetic properties of annealed finish product plates of non-oriented electrical steel were examined by means of EBSD technique and optical microscope. The results show that surface segregation of Cu significantly hindered recrystallized grain growth of surface layer in hot rolled plate during the coiling,as a result,the surface grain sizes of the hot-rohed plates decrease with the increase of Cu con... 