高牌号无取向电工钢RH深脱硫
以CaO-CaF2复合渣系为脱硫剂,在RH精炼过程采用真空投入法进行高牌号无取向电工钢深脱硫工业试验,采用KTH模型计算分析了RH炉渣成分对硫容量CS的影响。研究结果表明,炉渣成分控制在w((CaO))/w((SiO2))为5~7,w((CaO))/w((Al2O3))为1.5~1.8,w((Al2O3))为25%~30%,w((FeO+MnO))<5%,脱硫剂加入量为6~8kg/t时,钢中硫质量分数从平均0.003 1%降低到0.001 8%,最高脱硫率达到47.1%,平均脱硫率为41.7%。 The industrial trials on deep desulphurization of high grade non-oriented electrical steel were finished through using CaO-CaF2complex based fluxes in RH process.Using the KTH model,the effect of refining slag composition on the sulfide capacities was analyzed.The results show that the chemical composition of refining slag(mass fraction,%)is w((CaO/SiO2))between 5to 7,w((CaO))/w((Al2O3))beween 1.5to 1.8,w((Al2O3)) between 25%to 30%,w((FeO+MnO))less than 5%,and the desulphurizer addition level of...
PDSOFT在硅钢退火炉管道设计中的应用
结合硅钢退火炉项目中应用PDSOFT软件进行三维配管设计的案例,描述PDSOFT软件的应用过程,总结其使用要点,分析其优缺点,并提出了推广三维设计软件的思路,对今后PDSOFT在相似项目中的推广应用有参考和借鉴价值。 Combining the case of using PDSOFT software to design the three-dimensional piping,the application process of the PDSOFT software is described,the using points are summarized,the advantages and disadvantages are analyzed,and the ideas of promoting the three-dimensional design software are put forward,which have a strong reference value for the promotion and application of PDSOFT in similar projects in the future.
双辊薄带连铸3.98%Si-0.71%Al无取向硅钢的组织、织构和磁性能
采用双辊薄带连铸工艺制备了厚度为2.4mm的3.98%Si-0.71%Al无取向硅钢带,经常化、冷轧、不同温度退火后,对其显微组织、析出物、织构和磁性能进行了检测分析。结果表明:随着退火温度的提高,退火板晶粒尺寸增大,组织均匀性提高;退火板析出物主要是AlN和MnS与AlN复合析出物,尺寸较粗大,达0.5~2.5μm;退火板织构沿厚度方向变化明显,表层和1/2层存在较强的{100}织构,1/2层还存在较强的{111}织构,1/4层主要是{112}织构;随退火温度的升高相应的铁损和磁感应强度均降低。 Using twin roll thin strip continuous casting technique,the 3.98%Si-0.71%Al no-oriented silicon steel strip in thickness of 2.4mm was produced.The microstructure,precipitates,texture,and magnetic properties of the sheet after normalizing,cold rolling and annealing at different temperatures were studied.The results show that with annealing temperature increase,the grain size and uniformity of annealed sheet increased.The main precipitates in coarse size of 0.5-2.5μm in annealed sheet were AlN and...
基于GTN损伤模型对含边部缺陷硅钢薄板冷轧时边裂的预测
采用拉伸试验和显微组织观测的方法确定了GTN损伤模型中的9个损伤参数,运用GTN损伤模型对冷轧硅钢薄板边部缺陷的扩展及边裂的产生进行了有限元模拟,并与预置缺口的钢板轧制试验进行对比。结果表明:轧制过程中边部缺陷是造成钢板边部裂纹萌生和扩展的一个重要原因,GTN损伤模型可用来预测含边部缺陷硅钢薄板在冷轧过程中边裂的产生;预测结果与试验结果基本一致。 The crack initiation and propagation of silicon steel strip with edge defect during cold rolling process was studied by using GTN damage model in this paper.Nine damage parameters in GTN model were identified by tensile testing and microstructure observing,and then the FE simulation of edge defect evolution of silicon steel strip during rolling process was conducted on the base of GTN damage model,and then the results were compared with rolling experimental results.The results show that the edge...
无取向硅钢C6厚涂层性能的影响因素
本文介绍了无取向硅钢C6涂液的性能,研究了配水量、固化程度和涂层厚度等因素对无取向硅钢C6涂层性能的影响。结果表明,随着配水量的增加,完全固化所需的时间增加,涂液固体含量降低,涂层厚度减小;随着固化程度的提高,涂层硬度先增大然后趋于恒定,而柔韧性逐渐变差,在过固化后急剧恶化;涂层厚度对涂层的表面外观、附着性和绝缘层间电阻均有显著影响。 Based on the introduction about the performance of C6 varnish for non-oriented silicon steel sheets,effects of water amount,curing degree and coating thickness are discussed. Results show that with the increase of water amount,the time required to cure completely extends,and both the solid content of C6 varnish and the coating thickness decrease. As the curing degree increases,the hardness of the coating increases first and then tends to be constant,however the flexibility degenerates,especially...
退火温度和时间对用电沉积法制备的高硅钢性能的影响
研究了退火温度和退火时间对电沉积硅钢试样中的断面层组织、硅在试样中的分布情况、织构分布和磁性能的影响。结果表明:退火温度为1000℃、退火时间为210 min时得到的试样晶粒分布均匀、硅在试样中分布均匀、硅平均浓度为6.3715%(接近6.5%)。试样的织构分析及磁性能检测的结果表明,在较高温度下延长退火时间可增加{100}和{110}面织构,降低铁损,所得试样的磁性能较为良好。 The effect of annealing temperature and time on the microstructure, distribution of silicon,texture and magnetism of the high silicon steel prepared by electrodeposition was investigated. The results showed that after annealing at 1000℃ for 210 min, the mean grain size of steel was about 190 μm with a uniform grain size distribution, and the silicon is also uniformly distributed on the entire cross section with an average Si concentration 6.3715%(close to 6.5%); With the increasing annealing tim...
两段式正火对含Sb冷轧无取向电工钢磁性能的影响
利用OM、EBSD等手段研究了热轧板两段式正火时在700℃保温不同时间(0、10、30、60 min)对含Sb冷轧无取向电工钢磁性能的影响。结果表明,700℃保温10 min处理的样品铁损最小,磁感最高。对成品板的组织分析结果表明,试样的晶粒尺寸随700℃保温时间的延长先增大后减小,保温10 min时晶粒尺寸达到最大;分析成品试样织构发现,有利织构组分随700℃保温时间的延长先增加后减少,保温10 min时有利织构组分所占百分比最高。因此,含Sb冷轧无取向电工钢两段式正火时在700℃保温10 min时磁性能最好。 Effect of two-stage normalization on magnetic property of non-oriented electrical steel containing antimony was investigated by using optical microscope(OM) and electron back-scattered diffraction technology(EBSD).The experimental results show that the iron loss and magnetic permeability of the specimen insulated at 700 ℃ for 10 min are lowest and highest respectively.The grain size of the finish specimens increases first and then decreases with the increase of holding time.Similarly,the advanta...
取向硅钢成品晶粒的位向测定方法
取向硅钢成品的晶粒尺寸非常大,其易磁化方向[001]晶向对于轧向的偏差角度对其磁性能影响极大。本文介绍了取向硅钢二次再结晶后成品晶粒位向的几种测定方法,包括侵蚀法、劳厄法、OIM法、极图法和非对称X射线衍射法等,并对这几种测量方法进行了比较。 The finished product of grain-oriented silicon steel has immense grain size ranging from millimeters to centimeters and the deviation angles of easy magnetization direction from rolling direction plays a remarkable role in magnetic properties of grain-oriented silicon steel.The methods in common use for determining the deviation angles of crystal direction are introduced,which include the etch-figure method,the Laue method,the OIM method,the pole figure method and the asymmetrical X-Ray diffract...
普通冷轧取向硅钢中间完全脱碳退火工艺的确定
为了确定普通冷轧取向硅钢最优的中间完全脱碳退火工艺,在其一次冷轧后进行5种不同工艺的脱碳退火处理,借助扫描电镜及电子背散射衍射技术研究了不同工艺脱碳退火后的组织、织构和脱碳效果。结果表明:经5种工艺脱碳退火处理后,初次再结晶的平均晶粒尺寸均约为19μm,且不随退火温度和时间的变化而变化;经840℃×10min工艺退火后的晶粒最均匀,高斯织构位向更准确,高斯织构面积分数最多,为3.1%,可将碳脱至0.003 5%。 In order to determine the optimal intermediate complete decarburizing annealing processes for common grain-oriented(CGO)silicon steel,five kinds of intermediate decarburizing annealing processes were conducted,the microstructure,texture and decarbonization after different decarburizing annealing processes were studied by scanning electron microscopy and electro back-scattered diffraction(EBSD)technology.The results show that the average grains sizes of primary recrystallization were about 19μm a...