钢厂
6.5%Si高硅钢铸锭凝固组织的CAFE法模拟研究
应用CAFE法对6.5%Si高硅钢铸锭凝固组织进行了模拟研究,确定出了适合高硅钢组织模拟的模型。进一步用该模型研究了过热度及冷却条件对凝固组织的影响,结果表明,随着过热度的降低,凝固组织中柱状晶比例和晶粒平均面积均减小。水冷条件下,高硅钢铸锭凝固组织几乎全是柱状晶,而且晶粒粗大。空冷条件下,等轴晶区扩大,但柱状晶仍占主要部分。缓冷条件下,等轴晶区占主要部分,晶粒平均面积和空冷条件下相当。 The solidification structure of 6. 5% Si steel ingot was simulated based on CAFE method and the model suitable for simulating the structure of high silicon steel wad ascertained. The influence of superheat and cooling condition on the solidification structure were studied. It was shown that with the superheat decreasing,the proportion of columnar crystals decrease,and the average grain size become smaller. Under water cooling condition,the solidification structure of casting was composed of almo...
Fe-6.5%Si高硅钢的性能及制备技术
Fe-6.5%Si高硅钢是一种具有高磁导率、低矫顽力和低铁损等优异软磁性能的合金,但是其室温脆性和低的热加工性能严重影响了其在工业领域的应用。综述了Fe-6.5%Si高硅钢的性能,评述了合金的改性法、特殊轧制法、快速凝固法、沉积扩散法、粉末冶金法等制备工艺。 It is well known that 6.5%Si high silicon steel is one kind of soft magnetic materials with higher re-lative permeability,lower coercive force and iron loss than those of conventional industrial silicon steel.However,their room-temperature embrittleness and poor workability limit their practical applications in the industry.The pre-paration technique such as modification treatment on alloy,special rolling,rapid solidification,CVD and powder me-tallurgy is reviewed.
余热利用系统在硅钢连续退火机组中的应用
介绍了烟气余热利用系统的工艺流程及控制思想,结合该系统在钢厂硅钢连续退火机组中的应用实践,估算出烟气余热利用系统每年可节约蒸汽5 040 t,经济效益良好,同时分析了该系统存在的问题及对策。 Introduced a method about the process and control of the application of waste heat system, which had been used into a silicon steel continuous annealing line and profiting a good economic benefit by saving a large number of steam every year, which has been estimated about 5 040 tons, and analyzed the problems and solutions existed in this system.
冷轧硅钢废水处理现状、问题及对策浅析
就冷轧硅钢废水处理生产中面临的主要问题进行分析,从技术角度及运行管理角度提出工艺优化升级改进措施及应对策略;同时从后续深度处理,逐步实现零排放目标的角度进行探讨,为冷轧硅钢废水减量化、出路乃至废水零排放提供一些思路。 The main problems in the wastewater treatment process of cold-rolled silicon steel lines are analyzed and process upgrading measures and optimization strategy are put forward from both technical and management views.At the same time,downstream deep treatment to gradually achieve the target of zero discharge is discussed,to provide some ideas for reduction or even zero discharge of wastewater from cold-rolled silicon steel lines.
初次再结晶退火工艺对3%Si取向硅钢组织和织构的影响
试验研究了0.3 mm取向硅钢冷轧板(/%:0.046C,3.07Si,0.09Mn,0.029P,0.004S,0.005A1)的退火温度(760~880℃7 min)和退火时间(820℃3~9 min)对该钢的晶粒尺寸,再结晶和织构的影响。结果表明,最佳初次再结晶退火工艺为820℃5 min,该钢的平均晶粒尺寸为14.20μm,完全再结晶率为92%,不利{111}<110>结构含量为3.16%,有利织构{111}<112>,{012}<001>和高斯织构含量分别0.40%,4.73%和2.46%。 The effect of annealing temperature(at 760 ~ 880 X.for 7 min) and time(at 820℃ for 3~9 min) on grain size,recrystallization rate and texture of 0.3 mm cold-rolled sheet of oriented silicon steel(/%:0.046C,3.07Si,0.09Mn,0.029P,0.004S,0.005Al) has been tested and studied.Results show that with optimum recrystallized annealing at 820℃ for 5 min,the silicon steel average grain size is 14.20 fun,the complete recrystaUization rate is 92%,the unfavourable-texture {111}< 110 > content in steel is ...
无取向硅钢钢液增钛原因分析
对无取向硅钢炼钢全流程钢液增钛的原因进行了分析,认为铁水钛含量、转炉出钢温度、转炉下渣量、精炼渣TiO2含量、钢水罐及RH浸入管混钢种生产是影响钢液增钛的主要原因。通过采取低钛铁水冶炼,减少转炉下渣量,提高出钢温度,添加白灰改质精炼渣等措施,均能够降低钢液中的钛含量。 After analyzing the causes leading to increased content of titanium in molten nonoriented silicon steel during whole steelmaking process, it was concluded that such factors as content of titanium in hot metal, tapping temperature from converter, quantity of roughing slag entered into the ladle from converter, content of TiO2 in refining slag, molten steel ladle car,carrying out the steelmaking of different steel grades by the same ladle and same RH immersion tube were the main causes ...
电力系统绝缘子防污闪纳米硅钢涂层应用研究
为了更好的解决电力系统防污闪涂料RTV-Ⅰ长期应用暴露出来的问题以及目前RTV-Ⅱ防污闪涂料存在的一些不足,结合具体实际需求,在电力系统外绝缘领域,应用新型防污闪硬质涂层——防污闪纳米硅钢涂层,并对分别喷涂了防污闪纳米硅钢涂层以及RTV涂料的绝缘子进行对比运行情况研究分析。研究结果表明,防污闪纳米硅钢涂层是一种同时具有优异憎水性迁移性能和自洁性能的新型涂层,具有良好的应用前景。 In order to solve the problem exposed of anti-pollution flashover coating RTV-Ⅰwhich has been used long-term in power system,as well as to better solve some shortcomings of the current anti-pollution flashover coating RTV-Ⅱ,in this paper,a new anti-pollution flashover hard coating — anti-pollution flashover nanometer silicon hard coating(NSHC) is applied in the field of power system insulation for the specific practical needs.At the same time insulators which are separately sprayed by the NSHC a...
硅钢轧制过程中乳化液流量数学模型研究及应用
目前高磁感冷轧硅钢生产过程中,采用经验方法确定的乳化液流量设定值往往会造成硅钢产品的磁感性能达不到预期目标,针对此情况,基于轧机轧制机理研究了的乳化液流量数学模型,确定了乳化液流量设定值。实践表明,使用该数学模型输出的乳化液流量设定值,可提高轧制过程中乳化液流量控制精度,从而提高高磁感冷轧硅钢的轧制性能。 In view of the current production process of high magnetically inductive cold-rolled silicon steel, the mathematical model of emulsified fluid flow based on mill rolling mechanism is studied in view of the situation in which the magnetic sensing performance of silicon steel products is often not up to the expected target by using empirical method to determine the emulsified liquid flow setting. Practice shows that the emulsified fluid flow setting value output from this mathematical model improv...
硅钢水溶性极厚绝缘涂层的热老化行为研究
对两种硅钢水溶性极厚绝缘涂层进行了不同温度的热老化实验。通过TG-DTA,GDS,FT-IR,SEM和光泽度仪等测试方法对老化的涂层进行分析表征,提出了评估硅钢水溶性极厚绝缘涂层热老化性能的合理温度区间,探讨了涂层热老化行为,并分析了两种涂层热老化性能的差异。结果表明,涂层附着性随着老化时间的延长逐渐下降。FT-IR表征结果显示,热老化过程中,涂料交联形成的化学键未发生断裂,交联剂氨基树脂的三嗪环被破坏是聚合物三维网络结构坍塌的主要原因。 Thermal aging expriments at different temperature were carried out on two types of water-soluble and extra-thick insulation coatings for non-oriented silicon steel,and a series of test methods such as glossmeters,TG-DTA,FT-IR,GDS,SEM were applied in analysis.For evaluating the thermal aging effect of this kind of insulation coating,the proper temperature range was proposed.The difference of aging performance between two coatings was been investigated and the related behaviors were been discussed...
晶界位向对硅钢立方/旋转立方取向双晶轧制取向变化的影响
晶界和{100}柱状晶在硅钢生产过程中对织构的遗传和演变有关键作用,因此本文利用晶体塑性有限元方法进行立方和旋转立方取向双晶在晶界不同位向时晶体取向演变的全场模拟。模拟显示,三种晶界位向下,晶界都具有诱发晶内产生S形状形变不均匀和缓解局部形变不均匀区取向转动的特点,立方和旋转立方取向双晶在带有剪切作用的轧制条件下都显示明显的取向稳定性。GB⊥RD(表示晶界垂直于轧向)晶界位向时,旋转立方取向晶粒优先在晶界中心位置发生取向转动,而立方取向则优先在远离晶界的端部发生取向转动。GB⊥TD(表示晶界垂直于横向)的晶界位向下,其晶界阻碍作用最小,双晶内产生的取向漫散度大,织构强度较低;除绕TD转动外,也具有复杂的绕RD、ND的取向转动。GB⊥ND(表示晶界垂直于法向)的晶界位向下,取向转动与GB⊥RD时相近,但有少量取向绕ND转动。 Grain boundaries and initial{100}columnar grains play a key role in the inheritance and evolution of texture in the production of electrical steels.In this paper,the crystal plasticity finite element method was used to simulate the grain orientation evolution of cube and rotated-cube oriented bicrystals when grain boundary was set to different orientations.It was shown that the grain boundary in three grain boundary orientations demonstrated the characteristics of inducing Sshape deformation inh...
硅钢连续退火生产线设备改造
针对硅钢连续生产线设备存在的故障、隐患以及精度等影响产品质量的问题进行分析及改造,实现保证生产线设备稳定运行、提高设备精度及硅钢产品质量的目的。 This paper analyzes and transforms the electrical equipment failures, risks existed in slicon continuous production line, and the effect of accuracy to product quality, in order to ensure stable operation of equipment in production line and improve the accuracy of device, quality of silicon.
轧制裂纹及热处理工艺对高硅电工钢复合板磁性能的影响
对3层高硅电工钢复合板铸坯进行热轧及温轧变形加工后,采用正火、退火两种热处理方式处理,并观察轧制过程中产生的裂纹,研究不同状态下复合板的磁性能。对不同状态下的试样进行扩散退火处理,研究复合板中裂纹变化及其对磁性能的影响。结果表明:不同热处理工艺下合金内部的裂纹尺寸差异明显,裂纹尺寸对复合板的磁性能影响显著,相对于深裂纹,其他因素的影响较小;温轧变形加工后,复合板内层出现有序组织,但该有序组织在合金存在深裂纹的前提下并不能从本质上提高合金的磁性能;扩散退火工艺可以消除复合板内部的浅裂纹及微裂纹,但不能消除尺寸较大的裂纹,故而不能显著提高存在深裂纹的复合板的磁性能。 After hot rolling and warm rolling deformation processing of casting billet for three-layer high silicon electrical steel composite plate, it was normalized and annealed for heat treatment. Then, the cracks produced during the rolling process were observed, and the magnetic properties of composite plate in different states were also investigated. Furthermore, the samples in different states were subjected to diffusion annealing treatment, and the changes of crack in composite plate and their eff...