所有分类
  • 所有分类
  • 未分类

无取向硅钢的磁性能主要取决于铁素体的晶粒尺寸、晶体织构和钢中的夹杂物。通过合适的化学成分设计以及采用适宜的夹杂物控制技术,可以获得最佳的夹杂物控制效果,使其纯净度大幅度提高或者无害,最终获得磁性能优良的高级别无取向硅钢。同时,为满足节能、环保、高效需求,无取向硅钢正朝着节能降耗、环境友好以及多功能、高效率、易加工等方向发展。 The magnetic properties of non-oriented silicon steel mainly depend on the grain size of ferrite,the crystallographic texture,and the inclusions in the steel.The optimum inclusion control effects can be obtained through a suitable chemical composition design and an appropriate inclusion control technique,and then the liquid steel will get be clean or the inclusion will get be harmless,finally the excellent magnetic property of the non-oriented silicon steel can be obtained.Meanwhile,in order to ... 
2013-03-28 133 5.8

无氧化炉具有加热效率高、投资与运营成本低、作业率高、表面质量及板型良好、NOx排放相对低等优势,在硅钢热处理领域应用前景广泛。本文阐述了确定无氧化炉(NOF)加热能力详细过程,涵盖炉温、炉断面尺寸、炉长、热平衡结算、加热能力计算等,为今后无氧化炉(NOF)在硅钢热处理应用时的设计提供了借鉴,同时也为今后明火直接加热的工业炉设计提供了参考。 Non-oxidation furnace has the advantage s of high heating efficiency, low investment and operation cost, high operation rate, good surface quality and plate shape, and relatively low NOxemission,and it still has wide application prospect in the field of silicon steel heat treatment. The detailed process of determining the heating capacity of a non-oxidizing furnace(NOF) is described, covering furnace temperature, furnace section size, furnace length, heat balance settlement, heating capacity cal... 
2022-01-28 152 5.8

对两种硅钢水溶性极厚绝缘涂层进行了不同温度的热老化实验。通过TG-DTA,GDS,FT-IR,SEM和光泽度仪等测试方法对老化的涂层进行分析表征,提出了评估硅钢水溶性极厚绝缘涂层热老化性能的合理温度区间,探讨了涂层热老化行为,并分析了两种涂层热老化性能的差异。结果表明,涂层附着性随着老化时间的延长逐渐下降。FT-IR表征结果显示,热老化过程中,涂料交联形成的化学键未发生断裂,交联剂氨基树脂的三嗪环被破坏是聚合物三维网络结构坍塌的主要原因。 Thermal aging expriments at different temperature were carried out on two types of water-soluble and extra-thick insulation coatings for non-oriented silicon steel,and a series of test methods such as glossmeters,TG-DTA,FT-IR,GDS,SEM were applied in analysis.For evaluating the thermal aging effect of this kind of insulation coating,the proper temperature range was proposed.The difference of aging performance between two coatings was been investigated and the related behaviors were been discussed... 
2011-04-28 116 5.8

硅钢连续退火线是无取向硅钢生产的成品线。由于受机组布置的影响,带钢经转向辊进出口活套后,当套量达到60%后就出现偏离生产线的情况,从而影响最终产品的质量及成材率,甚至损坏设备。针对某冷轧厂硅钢连续退火机组出口活套入口处带钢跑偏开展纠偏研究,利用Matlab对该纠偏系统进行动态仿真研究,分析系统的稳定性。 Silicon steel continuous annealing line is non oriented silicon steel production of finished product line.Due to the influence of unit layout,strip by roll Import & Export loop,when the set volume reached 60% after the emergence of deviation from the production line,thus affecting the quality of the final product and the rate of finished products,and even damage the equipment.For the export of continuous annealing line in cold rolling silicon steel strip deviation rectification loop at the e... 
2014-06-28 118 5.8

【作者】 谌剑; ...
2011-09-28 83 5.8

借助高温激光共聚焦显微镜,在线观察了不同Mn含量的无取向硅钢中夹杂物的尺寸、类型、数量变化。结果表明,Mn含量(质量分数)为0.77%、0.32%时,试样中的夹杂物数量分别约为1000万个/mm3、1600万个/mm3。Mn含量较高的钢种,会优先析出球形、椭球形MnS夹杂物,其析出数量较少,尺寸相对较大,可以有效抑制AlN、CuxS夹杂物析出;Mn含量较低的钢种,会在试样再加热后冷却过程中,先析出相当数量MnS夹杂物,并作为AlN夹杂物析出核心,形成MnS+AlN复合夹杂物。这种复合夹杂物数量较多,尺寸也较大。 Based on the high temperature confocal microscope, the chage of size, type, and quantity of inclusions in non-oriented silicon steels with different Mn content were observed by in-situ SEM. Results show that the inclusion quantities are 10 million per mm3 and 16 million per mm3,while the mass fractions of Mn are 0.77% and 0.32%, respectively. In the silicon steel with higher Mn content, the spherical and ellipsoidal MnS inclusion will precipitate first, which can retard the precipitation of AlN ... 
2014-05-28 130 5.8

广泛应用于电子电力行业的取向硅钢材料的磁性能与其晶体取向密切关联,对取向硅钢晶体衍射花样的研究非常重要.采用理论计算的方式研究了取向硅钢的晶体衍射花样特征,并绘制了取向硅钢的高斯织构理论极图、理论单晶透射电子衍射斑点花样和理论电子背散射衍射(Electron backscatter diffraction, EBSD)菊池花样.取向硅钢理论单晶衍射花样不仅可以为以后标定样品实测晶体衍射花样提供一种简单快捷的方法,也可以为样品检测提供一种标准.这种研究方法不仅限于取向硅钢,也被期待应用于其他材料晶体衍射花样研究. The magnetic properties of oriented silicon steels which are widely used in electronic and power industries are closely related to their crystal orientations, so it is very important to study the crystal diffraction patterns of oriented silicon steels. The characteristics of crystal diffraction patterns of oriented silicon steels are studied by means of theoretical calculation. The theoretical pole figures, theoretical single crystal transmitted electron diffraction patterns and theoretical elec... 
2022-03-28 139 5.8

冷轧无取向硅钢是高技术含量、高附加值产品,工艺复杂,生产周期长,过程控制难度大,被誉为钢铁产品中的\"工艺品\"。热轧生产工艺又是无取向硅钢生产的重中之重,直接决定了硅钢的铁损和电磁性等多项指标。 Cold rolled non-oriented silicon steel is high technology content 、high added value product. Its process is complex, its production cycle is of length, and its process control is difficult, which is known as the iron and steel products \" Arts and crafts\". Hot rolling production process is the top priority of non-oriented silicon steel, which directly determines iron loss of the silicon steel and electromagnetic property,as well as other many index. 
2014-02-28 140 5.8

对硅钢板材分别进行异步和同步轧制,研究了轧制参数包括速比、压下量和道次对板材表面显微组织的演变的作用.结果表明,异步轧制硅钢板材表面形成了晶粒尺寸为10~50 nm,取向接近随机分布的纳米晶,而同步轧制板材的表面只形成了位错胞,证明异步轧制可以诱发表面纳米化.异步轧制板材表面纳米晶的形成过程为:在剪切力的反复作用下,高密度位错形成、滑移、湮灭和重组形成亚微米尺度的亚微晶/位错胞.随着压下量和轧制道次增加,高密度位错重复以上过程使晶粒尺寸减小、取向差增大,最终形成取向接近随机分布的纳米晶组织.大压下量和多道次是异步轧制诱发板材表面纳米化的关键,而速比的增加可以加快纳米化进程. Surface nanocrystallization(SNC) can effectively enhance the surface and global properties of the metallic materials,such as microhardness,intensity,fatigue,wear and corrosion resistances,therefore provides more promising practical industrial applicability.Up to now,several SNC treatment methods were developed based either on the principles of ball impactions or friction sliding,however,difficulty still exists for the surface treatment of large-dimensional samples with high efficiency.Recently,m... 
2014-09-28 152 5.8

对新能源汽车以及驱动电机的现有市场和未来市场规模进行梳理分析,通过自建计算公式推导出我国2021年1-11月份驱动电机用电工钢的总量,进而预测未来10年中国新能源汽车驱动电机用电工钢情况,为无取向电工钢的生产和在电机中的应用提供有价值的参考。 The current market and future market size of new energy vehicles and traction motors were analyzed,and the total amount of electrical steels used in traction motors in China from January to November 2021 was derived by using self-built calculation formulas,and then the situation in the next ten years of electrical steel used in traction motors of new energy vehicles in China was predicted.It will provide a valuable reference for the production of non-grain oriented electrical steel and its appli... 
2022-02-28 144 5.8

取向硅钢热轧板中织构梯度对发展完善的二次再结晶十分关键,通过添加铜可以显著降低取向硅钢板坯加热温度,从而影响热轧板织构分布。利用X射线衍射仪,分析了实验室模拟薄板坯连铸连轧(TSCR)工艺的3种不同铜含量的取向硅钢热轧板织构。结果表明:不同铜含量热轧板表面到厚度1/4处均为弱的热轧织构,热轧板心部主要为{100}面织构;铜含量约在0.4%时,热轧板次表层的{110}<001>织构比例最高,而热轧板心部的{100}<110>织构比例最低;铜含量对热轧织构中{114}<110>和{001}<100>织构发展有显著影响。 The texture gradient in hot rolled grain oriented silicon steel strip is one of the essential factors to achieve a perfect secondary recrystallization.The addition of copper can significantly reduce the slab reheating temperature of grain oriented silicon steel,so as to impact the texture distribution in the hot rolled strip.The texture of hot rolled grain oriented silicon steel strip as-rolled by thin slab casting and rolling process(TSCR) in laboratory with three different copper contents was ... 
2011-01-28 139 5.8

结合工业化生产的无取向硅钢,探讨了氧硫交互作用对钢中夹杂物生成的影响。借助非水溶液电解+扫描电镜法,研究了不同O、S含量下钢中夹杂物的变化规律。结果表明,本实验条件下,提高O含量、降低S含量,会劣化热轧组织再结晶效果。在劣化效果上,O的作用大于S;低Si、无Al硅钢中,应尽可能降低O含量、适当提高S含量,以粗化钢中微细夹杂物,减少尺寸小于1.0μm的夹杂物的数量;O、S含量与钢中夹杂物数量不具有关联性。生产过程中,不仅要严格控制O、S含量,还要严格控制生产工艺,以免生成较多的有害夹杂物。 Based on the industrial production of non-oriented silicon steel,the effects of interaction between oxygen and sulfur on the formation of inclusions were discussed.The change of non-metallic inclusions in steel sheets was investigated by means of electrolysis with non-aqueous solution under different oxygen and sulfur content.Results show that the recrystallization microstructure of hot rolled sheets will be deteriorated with the increase of oxygen content and the decrease of sulfur content.The ... 
2012-04-28 114 5.8

站点公告

网站试运行,请大家关注本站公众号,多提宝贵意见!

显示验证码