钢厂
取向硅钢成品晶粒的位向测定方法
取向硅钢成品的晶粒尺寸非常大,其易磁化方向[001]晶向对于轧向的偏差角度对其磁性能影响极大。本文介绍了取向硅钢二次再结晶后成品晶粒位向的几种测定方法,包括侵蚀法、劳厄法、OIM法、极图法和非对称X射线衍射法等,并对这几种测量方法进行了比较。 The finished product of grain-oriented silicon steel has immense grain size ranging from millimeters to centimeters and the deviation angles of easy magnetization direction from rolling direction plays a remarkable role in magnetic properties of grain-oriented silicon steel.The methods in common use for determining the deviation angles of crystal direction are introduced,which include the etch-figure method,the Laue method,the OIM method,the pole figure method and the asymmetrical X-Ray diffract...
我国硅钢发展现状及发展趋势
硅钢是钢铁产品中的\"工艺品\",是高附加值产品,通过对我国主要硅钢生产厂家的工艺设备,市场情况分析,简要介绍了我国硅钢生产消费现状,未来生产能力预测及硅钢未来发展趋势。 Silicon steel is the \"crafts\" of steel products,also is high value-added product.By analyzing process equipment and market condition of major silicon steel-making plant of China,it briefly introduces our current production consumption status,future production capacity prediction and future development trend of silicon steel.
常化温度对TSCR流程制备低碳低硅无取向硅钢组织和性能的影响
在实验室试制了TSCR流程的低碳低硅无取向硅钢,研究了在850~1050℃不同温度常化对冷轧量0.5mm厚钢板再经950℃×7min退火后的组织、织构和磁性能的影响。结果表明:随常化温度的升高,使热轧板晶粒尺寸增大,晶界更清晰,组织均匀性更好;由于第二相AlN和MnS析出物尺寸比较大,使冷轧退火后钢板晶粒也随常化温度升高呈单调增大趋势;γ有利织构和{111}、{112}不利织构与常化温度升高同时增强,但前者增强更多;冷轧板退火后铁损随常化温度升高呈单调下降,磁感呈单调上升趋势。 The low-carbon and low-silicon non-oriented silicon steel was prepared by thin slab casting and rolling(TSCR) in lab.The effect of normalizing at different temperatures in 850-1 050℃on microstructure, texture and magnetic properties of 0.5 mm cold-rolled sheets after annealing at 950℃for 7 min was researched. The results show that with increasing the normalizing temperature,the grain size of hot-rolled sheets increased,the grain boundaries were more clear and the rnicrostructure uniformity was b...
二次冷轧压下率对高牌号无取向硅钢组织结构和磁性能的影响
研究二次冷轧压下率对于硅的质量分数为3.0%的无取向硅钢组织结构和磁性能的影响。结果表明:当第二次冷轧压下率从0变化至16.7%时,铁损逐渐增加,磁感逐渐降低。当第二次冷轧压下率大于16.7%时,随压下率的增加,铁损逐渐减小,磁感逐渐增加。当第二次冷轧压下率大于38%时,二次冷轧法所能获得的磁性能明显优于一次冷轧法。 Effect of double cold reduction on magnetic,microstructure and texture of 3.0% Si non-oriented silicon steel sheets was investigated.The results show that the iron loss increases and magnetic induction reduces as the percentage redcution in secondary cold rolling changes from 0 to 16.7%.The core loss can be reduced remarkably,and magnetic induction can get a little benefit if the percentage redcution in double cold reduction is higher 16.7%.In case of higher than 38% of the percentage redcution ...
稀土在无取向电工钢中应用的研究进展
稀土元素在许多钢中发挥着独特而且不可替代的重要作用。半个世纪以来,它的作用已经在各种低合金和特殊合金钢中的研究及应用中得到充分的证明;然而,作为具有稀土资源优势的中国,在属于重要功能材料的无取向电工钢中稀土的应用却落后于国外,本文就中国稀土在无取向电工钢中的应用研究作简要的评述,希望能够进一步推进此领域的研究,并且促进中国稀土在无取向电工钢中应用技术的发展,缩短与国外差距,并提出了在此应用领域今后需深入开展的研究方向。 Rare earth elements play a unique and irreplaceable role in a lot of steels,it has given the full proof by the practice of various low alloy steels and special alloy steels since half century.However,as our country has the advantage of rare earth resources,RE application technology in non-oriented electrical steels has lagged behind abroad.The application researches of rare earth in non-oriented electrical steel in our country are briefly reviewed in this paper,which hope to promote the research...
无取向电工钢表面线状缺陷的影响因素分析
结合扫描电镜和大样电解研究了CSP流程W800牌号无取向电工钢表面线状缺陷中夹杂物成分及来源,采用SPSS软件回归分析了生产过程各因素对表面线状缺陷的影响。研究表明:稳态浇铸过程铸坯中大型夹杂物含量为5.39 mg/10 kg。引起无取向电工钢表面线状缺陷的大型夹杂物主要为脱氧产物、镁铝尖晶石和钢包顶渣,主要类型为Al2O3、MgO-Al2O3、CaO-Al2O3-MgO和CaO-Al2O3-SiO2。非稳态浇铸过程钢水洁净度明显降低,热轧板表面线状缺陷比例上升。影响表面线状缺陷的主要因素为RH出站时顶渣的w(CaO)/w(Al2O3)、RH脱氧结束氧位及中间包最低吨位。 Combining scanning electron microscopy and large sample electrolysis, the composition and source of inclusions in the surface linear defects of W800 grade non-oriented electrical steel in the CSP process were studied. SPSS software was used to regress and analyze the main factors which affected the surface linear defects in the steelmaking process. Research shows that the content of large inclusions in the steady state casting process is 5.39 mg/10 kg. The large inclusions which cause linear def...
硅钢连续退火生产线设备改造
针对硅钢连续生产线设备存在的故障、隐患以及精度等影响产品质量的问题进行分析及改造,实现保证生产线设备稳定运行、提高设备精度及硅钢产品质量的目的。 This paper analyzes and transforms the electrical equipment failures, risks existed in slicon continuous production line, and the effect of accuracy to product quality, in order to ensure stable operation of equipment in production line and improve the accuracy of device, quality of silicon.