  • 未分类

对欧盟市场汽车压缩机专用产品进行技术解析,对比分析了其电磁性能、退火和发蓝处理、物理性能、化学成分、应用特点等参数。探讨国内外电工钢产品应用方式的不同特点,并结合鞍钢自身工艺装备和炼钢、热轧、冷轧工艺参数介绍了其生产可行性。提供了冶金工艺流程下,后工序电工钢专业生产线及传统冷轧系统生产线两种生产方式,均能满足用户最终使用要求。 The technology of automotive compressor accommodation manufacture of European Economic and Monetary Union market was described.The magnetic properties,annealing bluing,physical properties,chemical composition,application parameters were analysed.The different characteristics of the application of electrical steel products,the feasibility of manufacture on the existing technology and equipment,steelmaking,hot rolled,cold rolled technical parameters were discussed.The professional product line of ... 
2013-06-28 123 5.8

研究了取向硅钢制备过程中常见的两种冷轧工艺,主要研究了一阶段冷轧与两阶段冷轧+中间退火工艺对初次再结晶组织及织构的影响.结果表明:采用两阶段冷轧+中间退火工艺制备以Cu2S为主抑制剂的取向硅钢,其初次再结晶平均晶粒尺寸为18.1μm,高斯晶粒的体积分数为0.6%,迁移性强的重位点阵晶界(Σ5+Σ9)和高能晶界(20°~45°取向偏差角)所占比例分别为1.8%和50.4%.与一阶段冷轧工艺相比,其初次再结晶晶粒较细,且高斯晶核与特征晶界所占的比例较高,有利于高斯晶粒发生二次再结晶. Two common cold-rolling processes of grain oriented silicon steel and the effects of the single stage cold rolling and tw o-stage cold rolling w ith intermediate annealing processes on the primary recrystallization microstructure and texture w ere investigated. The results revealed that for the grain oriented silicon steel prepared under the tw o-stage cold rolling process w ith intermediate annealing w ith Cu 2 S as the main inhibitor,the average grain size of the primary recrystallization micr... 
2014-02-28 139 5.8

通过金相分析和电子背散射衍射技术研究了一种新型含铜无取向电工钢在950℃退火不同时间(3~180s)空冷后的组织和织构取向的演变。结果表明:该钢在退火3s时的主要织构为α和γ线织构,{100}<110>织构最强;退火20s时织构以<111><112>、{111}<110>、{112}<110>、高斯织构和立方织构为主,随着退火时间的延长,高斯织构和立方织构强度呈减弱趋势;合理控制保温时间有利于提高{100}、{110}面织构的占有率。 Evolution of microstructure and texture oriented of a new non-oriented electrical steel during annealing at 950℃for different times(3-180) s and air cooling was studied by metallography and electron back-scattering diffraction analysis.The results show that after annealing for 3 s most of the texture oriented alongα-fibre andγ-fibre,the intensity of {100}〈110〉was the strongest.{111}〈112〉,{111}〈110〉,{112}〈110〉,Gauss texture and cube texture were the main texture after annealing for 20 s,with the ... 
2011-09-28 114 5.8

冷轧取向硅钢工程中有很多的超长、大体积以及薄壁的混凝土结构,裂缝控制是土建施工的关键。在工程中,按照\"抗放兼施、先放后抗、以抗为主\"的原则,采用\"无缝分块跳仓法\",防止超长混凝土结构收缩产生裂缝;在隧道和池体的底板与墙板施工中,采用\"整体浇筑\"法,避免了墙板因约束应力而产生的裂缝。 In the Cold-rolled grain-oriented silicon steel project,there are many overlength,bulk mass,thin-walled concretes structures,how to control the crack is the key of civil engineering construction.In these projects,according to the principle of\"release with resist,resist before release,resist is dominant \",the crack of the over-long structure and shrinkage can be prevented by the method of\"seamless block skip bin \".In the construction of the bottom plate and wall of the tunnel and the pool,the cra... 
2023-05-12 1.29k 5.8

利用FE-SEM、EDS分析了含不同抑制剂成分的成品取向硅钢中夹杂物的组成和形貌,统计其尺寸及数量分布;结合对磁性能测试的结果,分析了Sn、Cu、Nb和Cr对取向硅钢磁性能影响的机理。结果表明:含Sn的取向硅钢试样中夹杂物主要为块状的微米级Al-Ti-C-N-O复合物,还有少量的球形Al-N-O颗粒和块状Ti-C-N-O颗粒,棒状夹杂物较少;含Cr的取向硅钢试样中夹杂物主要为球形的微米级Al2O3,还有少量Cu-Al-N-O-S复合物,棒状夹杂物和不规则夹杂物均较少;含Cr试样中1~3μm夹杂物的平均尺寸较含Sn试样小,但数量多,而大于3μm夹杂物的平均尺寸较含Sn试样大,但数量很少。磁性能测试结果表明,外场为800A/m和2500A/m时,含Cr试样磁感应强度偏低,铁损值P1.7/50较含Sn试样高,为1.171W/kg。 The composition and morphology of inclusions in the finished grain-oriented silicon steels are analyzed by using FE-SEM and EDS, and the number density and size distribution of the inclusions are counted. The influence mechanism of Sn, Cu, Nb, and Cr on the magnetic properties of the steel is also discussed. Results show that the inclusions composition in the grain-oriented silicon steel samples containing Sn is mainly block Al-Ti-C-N-O, compounding with a few spherical Al-N-O and block Ti-C-N-O... 
2014-05-28 132 5.8

研究了锰含量对w(Si)=1.8%Si无取向电工钢组织和性能的影响。结果表明,钢中锰含量从0.3%增加到1.2%时,由于α_γ相变的产生,铸坯低倍组织、热轧板金相组织及成品织构等均发生了不同程度的变化,对成品表面质量及磁性能产生了明显的影响。 The effects of manganese content on structure and properties of w(Si)=1.8% non-oriented electrical steels have been studied.Results show that with increasing manganese content to 1.2% from 0.3%,macrostructure of continuous casting slab,hot rolled band metallurgical structure and finished product texture vary in some extent because of the occurrence of α-γ phase transformation,the surface quality and magnetic properties of finished product are affected greatly. 
2011-03-28 121 5.8

晶界和{100}柱状晶在硅钢生产过程中对织构的遗传和演变有关键作用,因此本文利用晶体塑性有限元方法进行立方和旋转立方取向双晶在晶界不同位向时晶体取向演变的全场模拟。模拟显示,三种晶界位向下,晶界都具有诱发晶内产生S形状形变不均匀和缓解局部形变不均匀区取向转动的特点,立方和旋转立方取向双晶在带有剪切作用的轧制条件下都显示明显的取向稳定性。GB⊥RD(表示晶界垂直于轧向)晶界位向时,旋转立方取向晶粒优先在晶界中心位置发生取向转动,而立方取向则优先在远离晶界的端部发生取向转动。GB⊥TD(表示晶界垂直于横向)的晶界位向下,其晶界阻碍作用最小,双晶内产生的取向漫散度大,织构强度较低;除绕TD转动外,也具有复杂的绕RD、ND的取向转动。GB⊥ND(表示晶界垂直于法向)的晶界位向下,取向转动与GB⊥RD时相近,但有少量取向绕ND转动。 Grain boundaries and initial{100}columnar grains play a key role in the inheritance and evolution of texture in the production of electrical steels.In this paper,the crystal plasticity finite element method was used to simulate the grain orientation evolution of cube and rotated-cube oriented bicrystals when grain boundary was set to different orientations.It was shown that the grain boundary in three grain boundary orientations demonstrated the characteristics of inducing Sshape deformation inh... 
2022-01-28 128 5.8

通过测试取向硅钢不同工艺条件下的碳含量,探讨了CGO取向硅钢碳含量控制的最优处理条件,研究了脱碳温度和脱碳时间对相同初始碳含量取向硅钢的脱碳效果的影响。结果表明,在气氛为(15%~20%)H2+(75%~80%)N2,炉压差为10~20 Pa的条件下,CGO取向硅钢合适的脱碳温度为1 073 K~1 123 K,脱碳时间为10~20 min。在该处理条件下,能取得较好的脱碳效果。 By means of testing carbon content of oriented silicon steel below the distinct technical conditions,inquires the excellent handle terms of carbon content controlling for CGO oriented silicon steel,studies effects of decarburization annealing temperature and decarburization annealing time to the oriented silicon steel decarburization efficiency in same initial carbon content.The results show that,under the condition of atmosphere(15% ~ 20%) H2+(75% ~ 80%)N2 and furnace pressure difference 10 ~ 2... 
2013-03-28 120 5.8

分析了高转矩和高转速条件下高效驱动马达铁芯材料对无取向硅钢磁性能要求,讨论了无取向硅钢的高磁通密度和低铁损对电机转矩和效率的影响,介绍了国内外高磁感无取向硅钢发展情况。在生产工艺上,提高钢质纯净度,弱化夹杂物和第二相粒子对畴壁移动和再结晶晶粒长大的钉扎作用,添加微量晶界和带钢表面的偏析元素促使有利织构发展等技术可提高无取向硅钢的磁通密度。 The requirements of high efficient drive motor core materials under the conditions of high torque and high speed were analyzed.The effects of high magnetic flux density of non-oriented silicon steel on the torque and efficiency of the motor were discussed.The development of non-oriented silicon steel with high magnetic was introduced.The magnetic flux density of non-oriented silicon steel sheet can be obviously improved by some production technologies,such as purification steel,weakening the pin... 
2023-05-11 1.3k 5.8

利用OM、SEM、TEM等实验方法研究了卷取工艺对一种新型含铜无取向电工钢晶粒度和析出相的影响。结果表明,该电工钢热轧带卷取后的晶粒尺寸为18~24μm,在卷取过程中,热轧带中有一定数量的第二相析出,经EDS能谱及选区电子衍射分析,这些析出相主要为AlN。随着卷取工艺的变化,该电工钢的晶粒度大小变化不明显,析出相的类型、尺寸大小不发生改变,体积分数发生一定的改变。 The effects of coiling process on grain size and precipitates of a new copper-bearing non-oriented electrical steel were investigated by OM,TEM and other experimental method.The results show that the grain size of hot-rolled bands after coiling is 18~24 μm.The second phases precipitate during coiling process.They are mainly AlN by EDS spectra and selected area electron diffraction.With the change of coiling process,the grain size of the electrical steel does not change significantly;the type and... 
2011-06-28 121 5.8

【机构】 中国金属学会电工钢分会; ...
2011-06-28 89 5.8

结合硅钢退火炉项目中应用PDSOFT软件进行三维配管设计的案例,描述PDSOFT软件的应用过程,总结其使用要点,分析其优缺点,并提出了推广三维设计软件的思路,对今后PDSOFT在相似项目中的推广应用有参考和借鉴价值。 Combining the case of using PDSOFT software to design the three-dimensional piping,the application process of the PDSOFT software is described,the using points are summarized,the advantages and disadvantages are analyzed,and the ideas of promoting the three-dimensional design software are put forward,which have a strong reference value for the promotion and application of PDSOFT in similar projects in the future. 