CSP流程生产高磁感无取向电工钢磁各向异性研究
对CSP流程生产的高磁感无取向电工钢50W1300在偏离轧制方向不同角度处的磁性能进行了测试和分析。结果表明:在偏离轧向不同角度处,磁性能差异显著,尤其在α=60°时磁感最低;偏离轧制方向不同角度处的磁性能大小取决于织构类型、强度及分布状态;增强{100}<0vw>和α、η取向的有利织构组分,降低不利的γ取向织构组分,且使有利织构组分分布越漫散,磁各向异性越小。 Magnetic properties of high magnetic induction non-oriented electrical steel 50W1300 produced by CSP processes were investigated with different direction in relation to the rolling direction.The result shows that magnetic properties are significantly different in relation to the rolling direction,in particular,the minimum magnetic induction occurs at 60° in relation to the rolling direction.Magnetic properties of different directions in relation to rolling direction depend on type and distributi...
压下率对取向硅钢热轧板织构的影响
采用X-射线衍射分析技术测定了取向硅钢热轧板在不同压下率下不同厚度处的织构。结果表明,在压下率低于80%的情况下,几乎所有试样的不同厚度处的织构均为旋转立方织构类型{100}<011>,但不同压下率、不同厚度处的织构强度存在很大差异;在压下率大于80%的情况下,不同试样的不同厚度处的织构类型发生了变化,其织构类型为旋转立方织构或高斯织构{011}<100>,且当织构类型为旋转立方织构时,织构强度存在很大差异,而当织构类型为高斯织构时,织构强度差异相对较小。 The texture of the grain oriented silicon steel hot rolled plate at different compressibility has been measured.The experimental results have shown that the texture of all samples at different thickness is {100}<011> when the compressibility is below 80%,and its intensity at different compressibility and thickness is difference.The texture of all samples at different thickness is variable when the compressibility is above 80%,it is {100}<011> or {011}<100>,and the intensity of ...